Multi-phase flow erosion test device and test method thereof
By using the venturi mixer and recovery unit in the multiphase flow erosion test device, the problems of high corrosion resistance, high cost and low mixing efficiency of the power plant in the existing device are solved, and more efficient mixing and safety are achieved multiphase flow test reduces equipment costs and experimental costs.
Patent Information
- Application Number
- CN202411157419.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-22
- Publication Date
- 2024-11-19
AI Technical Summary
The existing multiphase flow erosion test device has high corrosion resistance, high economic cost, uneven mixing, low mixing efficiency and poor safety.
The venturi pipe mixer is used instead of the conventional stirring mixer. The venturi pipe drainage effect realizes the flow of water and oil and the mixing of oil, gas and water. Only a single compressor can realize the flow and mixing of three fluids, reducing power. Mechanical use reduces system costs, improves system reliability, and realizes media separation and reuse through recycling units and cooling devices to avoid contact between power machinery and corrosive media.
It improves mixing efficiency and safety, reduces equipment costs and experimental costs, simplifies the system process, achieves better gas-liquid mixing effect and media separation, and enhances the reliability and safety of the experimental device.
Smart Images

Figure CN118980599A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of multiphase flow erosion test devices, in particular to a multiphase flow erosion test device and an experimental method thereof. Background Art
[0002] In recent years, with the increase in the proportion of heavy oil and high-sulfur crude oil in the petrochemical industry, the failure of petrochemical industry pipelines and equipment (heat exchangers, air coolers, etc.) has become increasingly serious. The failure of petrochemical equipment is diverse and the mechanism is complex, such as material defects, various forms of corrosion creep, external force damage, etc. Among them, corrosion failure caused by erosion damage is the most common failure damage of petrochemical equipment. It is a process in which the material is subjected to the combined effects of erosion and corrosion. Erosion damage is obviously local, sudden, destructive and risky. Especially under the action of multiphase flow containing oil, gas, water, and various corrosive media, it is more likely to cause erosion perforation, and the situation is complicated and it is difficult to predict its occurrence. This has become a key technical issue that plagues the safe operation of fluid equipment and is increasingly attracting people's attention.
[0003] In response to the multiphase flow erosion problem in the petrochemical industry, a series of multiphase flow erosion test devices have been proposed, attempting to analyze the failure mechanism of pipelines through experimental research, in order to be used in engineering practice and improve the stability of industrial pipeline systems. However, most of the current multiphase flow erosion test devices are ring-type erosion test devices, and the disadvantage of ring-type erosion test devices is that they require corrosion-resistant power devices and mixing tanks, have high economic costs, uneven mixing, low mixing efficiency, and poor safety. Summary of the invention
[0004] The technical problem to be solved by the present invention is: in order to solve the problem that most of the current multiphase flow erosion test devices are ring-type erosion test devices, and the disadvantages of the ring-type erosion test devices are that they require corrosion-resistant power devices and mixing tanks, have high economic costs, uneven mixing, low mixing efficiency, and poor safety, a multiphase flow erosion test device and an experimental method thereof are now provided.
[0005] The technical solution adopted by the present invention to solve its technical problems is: a multiphase flow erosion test device, including an air storage tank, a compressor, a pressure-stabilizing tank, a venturi tube mixer, a water tank, an oil tank, a test section and a cooling device, wherein the air storage tank is used to store the required corrosive gas, the air storage tank is connected to the input end of the compressor, the output end of the compressor is connected to the pressure-stabilizing tank, the pressure-stabilizing tank is connected to the input end of the venturi tube mixer, the output end of the venturi tube mixer is connected to the input end of the test section, the output end of the test section is connected to a recovery unit, the recovery unit is used to separate the recovered mixed gas and liquid and store them separately, the water tank and the oil tank are respectively connected to the venturi tube mixer via the throat section of the venturi tube mixer. Compared with the prior art, this solution adopts a Venturi tube mixer instead of a conventional stirring mixer. The flow of water and oil and the mixing of oil, gas and water are achieved through the drainage effect of the Venturi tube. Only a single compressor is required to achieve the flow and mixing of the three fluids, and the gas-liquid mixing effect is better than the conventional stirring mixing effect, reducing the use of power machinery in the system, reducing the investment cost of the system device, simplifying the system process, and improving the system reliability. At the same time, the corrosive medium in the erosion experiment will dissolve in water. In the conventional erosion experiment system, a pump is required to transport the aqueous solution containing the corrosive medium, and the corrosion resistance and sealing of the pump are relatively high. However, the present invention does not need to use power machinery such as pumps to transport the corrosive solution. All the equipment in contact with the corrosive solution is static equipment, and there is no need to consider the corrosion resistance of the power machinery, which further improves the safety of the experimental device and reduces the equipment cost.
[0006] In order to recycle the medium after the test, some embodiments are preferred, wherein the recovery unit includes a three-phase separation tank, a first liquid storage tank, and a second liquid storage tank, and the output end of the test section is connected to the three-phase separation tank, and the three-phase separation tank is respectively connected to the gas storage tank, the first liquid storage tank, and the second liquid storage tank. By connecting the three-phase separation tank at the output end of the test section to separate the medium after the test, the gas is stored in the gas storage tank, the oil is stored in the first liquid storage tank, and the water is stored in the second liquid storage tank, respectively, so as to separate the medium after the test and recycle it, thereby greatly reducing the experimental cost.
[0007] Since the medium of the test is heated in advance, part of the water will be vaporized. In order to better recycle the medium after the experiment, some embodiments are preferably provided with a cooling device between the output end of the test section and the three-phase separation tank. By providing a cooling device at the output end of the test section, the cooling device cools the medium after the experiment, which facilitates the separation of water, oil and gas and improves the separation efficiency. In addition, the experimental temperature of some experimental conditions may be very high. If the high-temperature gas directly flows back to the compressor, the performance and life of the compressor may be reduced. Therefore, it needs to be cooled by the cooling device before reuse.
[0008] In order to facilitate the control of gas, oil and water and to facilitate the test section test, some preferred embodiments are wherein valves are provided between the gas storage tank and the three-phase separation tank, between the first liquid storage tank and the three-phase separation tank, between the second liquid storage tank and the three-phase separation tank, between the water tank and the throat section of the venturi tube mixer, between the oil tank and the throat section of the venturi tube mixer, and between the pressure stabilizing tank and the input end of the venturi tube mixer.
[0009] In order to study the erosion effect of gas-liquid multiphase flow on the test section under different flow rates, pressures and other conditions under the same working conditions, some preferred embodiments are provided with a first flow meter between the pressure stabilizing tank and the input end of the venturi mixer, and a second flow meter and a third flow meter are provided between the throat section of the water tank and the oil tank venturi mixer and between the throat section of the oil tank and the venturi mixer.
[0010] In order to facilitate the testing of media at different temperatures, in some preferred embodiments, a heating device is provided between the output end of the venturi mixer and the input end of the test section.
[0011] In order to better control the test requirements of the medium in the test section, in some preferred embodiments, a temperature sensor is provided between the output end of the venturi mixer and the heating device, and a temperature sensor and a pressure sensor are provided between the heating device and the input end of the test section.
[0012] In some preferred embodiments, a filter is provided between the gas storage tank and the compressor.
[0013] In some preferred embodiments, a valve is provided between the gas storage tank and the filter.
[0014] An experimental method using a multiphase flow erosion test device as described above, the specific operating steps are as follows:
[0015] S1. First close the valve between the gas storage tank and the filter, and the valve between the gas storage tank and the three-phase separation tank, and inject process gas and corrosive gas into the gas storage tank according to the required proportion;
[0016] S2. After the gas filling is completed, the valve between the gas storage tank and the filter, and the valve between the gas storage tank and the three-phase separation tank are opened, and the prepared gas is filtered through the filter. After the impurities are effectively filtered, the gas passes through the compressor, and the gas is compressed and the pressure is increased. The gas is buffered by the pressure-stabilizing tank. The flow rate of the gas flowing into the venturi tube mixer can be controlled by adjusting the valve opening between the pressure-stabilizing tank and the input end of the venturi tube mixer, and the water in the water tank and the oil in the oil tank are introduced into the venturi tube mixer through the drainage effect of the venturi tube mixer, and the oil phase, the water phase and the gas phase are mixed. After the mixture is evenly mixed, it is heated by the heating device to reach the specified working condition. The mixed liquid is passed into the test section of the test for erosion test, and the mixed liquid after the test is subsequently cooled by the cooling device. After the cooling is completed, the mixed liquid enters the three-phase separation tank for separation, and the gas phase flows back to the gas storage tank for reuse, the oil phase flows into the first liquid storage tank, and the water phase flows into the second liquid storage tank;
[0017] S3. After the test is completed, close the valves at the front and rear ends of the test section, disassemble the test section and perform anatomical testing and analysis on the test section.
[0018] The beneficial effects of the present invention are as follows: when a multiphase flow erosion test device and an experimental method thereof are used, a venturi tube mixer is used to replace a conventional stirring mixer, and the flow of water and oil and the mixing of oil, gas and water are realized through the drainage effect of the venturi tube. Only a single compressor is required to realize the flow and mixing of the three fluids, and the gas-liquid mixing effect is better than the conventional stirring mixing effect, thereby reducing the use of power machinery in the system, reducing the investment cost of the system device, simplifying the system process, and improving the system reliability. At the same time, the corrosive medium in the erosion experiment is generally dissolved in water. In the conventional erosion experiment system, a pump is required to transport an aqueous solution containing the corrosive medium, and high requirements are placed on the corrosion resistance and sealing of the pump. However, in the present invention, there is no need to use power machinery such as a pump to transport the corrosive solution, and all equipment in contact with the corrosive solution is static equipment, and there is no need to consider the corrosion resistance of the power machinery, thereby further improving the safety of the experimental device and reducing the equipment cost, thereby avoiding the current multiphase flow erosion test device, which is mostly a ring-type erosion test device, and the ring-type erosion test device requires a corrosion-resistant power device and a mixing tank, has high economic cost, uneven mixing, low mixing efficiency, and poor safety. BRIEF DESCRIPTION OF THE DRAWINGS
[0019] The present invention is further described below in conjunction with the accompanying drawings and embodiments.
[0020] Figure 1 It is a structural schematic diagram of the present invention.
[0021] In the figure: 1. gas storage tank, 2. filter, 3. compressor, 4. pressure regulating tank, 5. first flow meter, 6. water tank, 7. oil tank, 8. venturi mixer, 9. temperature sensor, 10. heating device, 11. pressure sensor, 12. test section, 13. cooling device, 14. three-phase separation tank, 15. first liquid storage tank, 16. second liquid storage tank. DETAILED DESCRIPTION
[0022] The present invention is further described in detail below in conjunction with embodiments:
[0023] The present invention is not limited to the following specific embodiments. A person skilled in the art can implement the present invention in various other specific embodiments according to the contents disclosed in the present invention, or any simple changes or modifications made to the design structure and ideas of the present invention fall within the protection scope of the present invention. It should be noted that the embodiments and features in the embodiments of the present invention can be combined with each other without conflict.
[0024] In the description of the present invention, it should be understood that the terms "center", "longitudinal", "lateral", "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside", "outside" and the like indicate positions or positional relationships based on the positions or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present invention and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as limiting the present invention. In addition, the terms "first", "second", and the like are only used for descriptive purposes, and cannot be understood as indicating or implying relative importance or implicitly indicating the number of technical features indicated. Thus, features defined as "first", "second", and the like may explicitly or implicitly include one or more of the features. In the description of the present invention, unless otherwise specified, "multiple" means two or more.
[0025] In the description of the present invention, it should be noted that, unless otherwise clearly specified and limited, the terms "installed", "connected", and "connected" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection, or it can be indirectly connected through an intermediate medium, or it can be the internal communication of two components. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood by specific circumstances.
[0026] Example 1
[0027] like Figure 1As shown, a multiphase flow erosion test device includes an air storage tank 1, a compressor 3, a pressure-suppressing tank 4, a venturi tube mixer 8, a water tank 6, an oil tank 7, a test section 12, a cooling device 13 and a computer. The computer is not shown in the figure. The air storage tank 1 is used to store the required process gas and corrosive gas. The air storage tank 1 is connected to the input end of the compressor 3, the output end of the compressor 3 is connected to the pressure-suppressing tank 4, the pressure-suppressing tank 4 is connected to the input end of the venturi tube mixer 8, the output end of the venturi tube mixer 8 is connected to the input end of the test section 12, the output end of the test section 12 is connected to the recovery unit, the recovery unit is used to separate the recovered mixed gas and liquid and store them separately, the water tank 6 and the oil tank 7 are connected to the venturi tube mixer 8 via the throat section of the venturi tube mixer 8 respectively.
[0028] The recovery unit includes a three-phase separation tank 14, a first liquid storage tank 15 and a second liquid storage tank 16. The output end of the test section 12 is connected to the three-phase separation tank 14, and the three-phase separation tank 14 is connected to the gas storage tank 1, the first liquid storage tank 15 and the second liquid storage tank 16 respectively.
[0029] Valves are provided between the gas storage tank 1 and the three-phase separation tank 14, between the first liquid storage tank 15 and the three-phase separation tank 14, between the second liquid storage tank 16 and the three-phase separation tank 14, between the water tank 6 and the throat section of the venturi tube mixer 8 of the oil tank 7, between the oil tank 7 and the throat section of the venturi tube mixer 8 of the oil tank 7, and between the pressure stabilizing tank 4 and the input end of the venturi tube mixer 8, and a valve is provided between the gas storage tank 1 and the filter 2.
[0030] A cooling device 13 is arranged between the output end of the test section 12 and the three-phase separation tank 14, a first flowmeter 5 is arranged between the pressure stabilizing tank 4 and the input end of the venturi tube mixer 8, a second flowmeter and a third flowmeter are arranged between the water tank 6 and the throat section of the venturi tube mixer 8, and between the oil tank 7 and the throat section of the venturi tube mixer 8, a heating device 10 is arranged between the output end of the venturi tube mixer 8 and the input end of the test section 12, a temperature sensor 9 is arranged between the output end of the venturi tube mixer 8 and the heating device 10, a temperature sensor 9 and a pressure sensor 11 are arranged between the heating device 10 and the input end of the test section 12, and a filter 2 is arranged between the air storage tank 1 and the compressor 3.
[0031] Example 2
[0032] Example 2 is an implementation of Example 1, specifically: an experimental method using a multiphase flow erosion test device as described above, and the specific operating steps are as follows:
[0033] S1. First, close the valve between the gas storage tank 1 and the filter 2, and the valve between the gas storage tank 1 and the three-phase separation tank 14, and inject process gas and corrosive gas into the gas storage tank 1 according to the required proportion;
[0034] S2. After the gas filling is completed, the valve between the gas storage tank 1 and the filter 2 and the valve between the gas storage tank 1 and the three-phase separation tank 14 are opened, and the prepared gas is filtered through the filter 2. After the impurities are effectively filtered, the gas passes through the compressor 3, the gas is compressed and the pressure is increased, and the gas is buffered by the pressure stabilizing tank 4. The flow rate of the gas flowing into the venturi mixer 8 can be controlled by adjusting the valve opening between the pressure stabilizing tank 4 and the input end of the venturi mixer 8, and the water in the water tank 6 and the oil in the oil tank 7 are introduced into the venturi mixer 8 through the drainage effect of the venturi mixer 8, and the mixing of the oil phase, the water phase and the gas phase is achieved. After the mixing is uniform, the mixed liquid is heated by the heating device 10 to reach the specified working condition, and the mixed liquid is passed into the test section 12 for erosion test. The tested mixed liquid then enters the cooling device 13 for cooling. After the cooling is completed, the mixed liquid enters the three-phase separation tank 14 for separation, and the gas phase flows back to the gas storage tank 1 for reuse, the oil phase flows into the first liquid storage tank 15, and the water phase flows into the second liquid storage tank 16;
[0035] S3. After the test is completed, the valves at the front and rear ends of the test section 12 are closed, the test section 12 is disassembled, and the test section 12 is anatomically tested and analyzed.
[0036] When the multiphase flow erosion test device and the experimental method are used, at the initial stage of the experiment, the two valves connecting the gas storage tank 1 and the filter 2 and the two valves connecting the gas storage tank 1 and the three-phase separation tank 14 are closed, and the process gas and the corrosive gas are injected into the gas storage tank 1 according to the required proportion. After the gas filling is completed, the two valves of the gas storage tank 1 and all the valves behind are opened, and the prepared gas is filtered through the filter 2. After the impurities are effectively filtered, the gas passes through the compressor 3, and the gas is compressed and the pressure increases. The gas is buffered by the voltage regulator tube. The gas flow rate flowing into the venturi tube mixer 8 can be controlled by adjusting the valve opening between the voltage regulator tank 4 and the input end of the venturi tube mixer 8. The gas is introduced into the venturi tube mixer 8 and mixed with the oil phase through the drainage effect of the venturi tube mixer 8. , water phase mixing, three valves connected to the venturi tube mixer 8 can control the mixing ratio of oil, gas and water. After mixing evenly, the mixed liquid is heated by the heating device 10 to reach the specified working condition. The mixed liquid is passed into the test section 12 for erosion test, and then enters the cooling device 13 for cooling. After cooling, the mixed liquid enters the three-phase separation tank 14 for separation, and the gas phase flows back to the gas storage tank 1 for reuse, the oil phase flows into the first liquid storage tank 15, and the water phase flows into the second liquid storage tank 16. The oil and water in the first liquid storage tank 15 and the second liquid storage tank 16 can be re-transported to the oil tank 7 and the water tank 6 for recycling. If it is necessary to replace the test tube at the test site and perform anatomical test and analysis on the test tube, the valves at the front and rear ends of the test tube can be closed, and the test tube can be disassembled and replaced for research.
[0037] The present invention only requires a single gas compressor 3 to realize the erosion characteristics test of gas-liquid multiphase flow, and there is no need to use other corrosion-resistant power devices such as corrosion-resistant pumps, which can save equipment costs to a great extent. At the same time, since the power device does not need to be in direct contact with the corrosive solution, the safety is improved. The experimental device can provide technical guarantee for pipeline safety in the petrochemical field.
[0038] The above-mentioned ideal embodiments of the present invention are for inspiration. Through the above-mentioned description, relevant staff can make various changes and modifications without departing from the technical idea of the present invention. The technical scope of the present invention is not limited to the contents of the specification, and its technical scope must be determined according to the scope of the claims.
Claims
1. A multiphase flow erosion test device, characterized in that: The invention comprises an air storage tank (1), a compressor (3), a pressure stabilizing tank (4), a venturi tube mixer (8), a water tank (6), an oil tank (7), a test section (12) and a cooling device (13); the air storage tank (1) is used to store required process gas and corrosive gas; the air storage tank (1) is connected to the input end of the compressor (3); the output end of the compressor (3) is connected to the pressure stabilizing tank (4); the pressure stabilizing tank (4) is connected to the input end of the venturi tube mixer (8); the output end of the venturi tube mixer (8) is connected to the input end of the test section (12); the output end of the test section (12) is connected to a recovery unit; the recovery unit is used to separate the recovered mixed gas and liquid and store them separately; the water tank (6) and the oil tank (7) are respectively connected to the venturi tube mixer (8) via the throat section of the venturi tube mixer (8).
2. A multiphase flow erosion test device according to claim 1, characterized in that: The recovery unit comprises a three-phase separation tank (14), a first liquid storage tank (15) and a second liquid storage tank (16); the output end of the test section (12) is connected to the three-phase separation tank (14); and the three-phase separation tank (14) is respectively connected to the gas storage tank (1), the first liquid storage tank (15) and the second liquid storage tank (16).
3. A multiphase flow erosion test device according to claim 2, characterized in that: A cooling device (13) is provided between the output end of the test section (12) and the three-phase separation tank (14).
4. A multiphase flow erosion test device according to claim 2 or 3, characterized in that: Valves are provided between the gas storage tank (1) and the three-phase separation tank (14), between the first liquid storage tank (15) and the three-phase separation tank (14), between the second liquid storage tank (16) and the three-phase separation tank (14), between the water tank (6) and the throat section of the venturi tube mixer (8), between the oil tank (7) and the throat section of the venturi tube mixer (8), and between the pressure stabilizing tank (4) and the input end of the venturi tube mixer (8).
5. A multiphase flow erosion test device according to claim 4, characterized in that: A first flow meter (5) is provided between the pressure stabilizing tank (4) and the input end of the venturi tube mixer (8), and a second flow meter and a third flow meter are provided between the water tank (6) and the throat section of the venturi tube mixer (8), and between the oil tank (7) and the throat section of the venturi tube mixer (8).
6. The multiphase flow erosion test device according to claim 1, characterized in that: A heating device (10) is provided between the output end of the venturi mixer (8) and the input end of the test section (12).
7. A multiphase flow erosion test device according to claim 6, characterized in that: A temperature sensor (9) is provided between the output end of the venturi mixer (8) and the heating device (10), and a temperature sensor (9) and a pressure sensor (11) are provided between the heating device (10) and the input end of the test section (12).
8. The multiphase flow erosion test device according to claim 1, characterized in that: A filter (2) is provided between the gas storage tank (1) and the compressor (3).
9. A multiphase flow erosion test device according to claim 8, characterized in that: A valve is provided between the gas storage tank (1) and the filter (2).
10. An experimental method using a multiphase flow erosion test device as claimed in any one of claims 1 to 9, characterized in that: The specific steps are as follows: S1. First, close the valve between the gas storage tank (1) and the filter (2), and the valve between the gas storage tank (1) and the three-phase separation tank (14), and inject process gas and corrosive gas into the gas storage tank (1) in the required proportion; S2. After the gas filling is completed, the valve between the gas storage tank (1) and the filter (2) and the valve between the gas storage tank (1) and the three-phase separation tank (14) are opened, and the prepared gas is filtered through the filter (2). After the impurities are effectively filtered, the gas passes through the compressor (3), and the gas is compressed and the pressure is increased. The gas is buffered by the pressure stabilizing tank (4) and the valve opening between the pressure stabilizing tank (4) and the input end of the venturi mixer (8) can be adjusted to control the flow rate of the gas into the venturi mixer (8), and the water tank (6) is drained by the drainage effect of the venturi mixer (8). The water in the tank (7) and the oil in the oil tank (7) are introduced into the venturi mixer (8) to achieve mixing of the oil phase, the water phase and the gas phase. After being evenly mixed, the mixed liquid is heated by a heating device (10) to reach a specified working condition. The mixed liquid is passed into a test section (12) for erosion testing. The tested mixed liquid then enters a cooling device (13) for cooling. After cooling, the mixed liquid enters a three-phase separation tank (14) for separation. The gas phase flows back to the gas storage tank (1) for reuse. The oil phase flows into a first liquid storage tank (15), and the water phase flows into a second liquid storage tank (16). S3. After the test is completed, the valves at the front and rear ends of the test section (12) are closed, the test section (12) is disassembled, and the test section (12) is dissected and tested for analysis.
Citation Information
Cited By
Sample quick-changing unit, deep-sea mining riser erosion resistance testing system and testing method thereof
CN120971148A