Macro-micro progressive failure analysis method for composite material

Through the finite element RVE mesoporative model and stress amplification coefficient method, combined with the failure model of fiber, matrix and interface, the macromechanical properties of composite materials were analyzed, and the failure analysis problem of composite materials under complex stress in the prior art was solved, and the failure analysis problem of composite materials under complex stress was achieved. Considerations on metal matrix yield and interface damage improve analysis accuracy and efficiency.

CN118983028AActive Publication Date: 2024-11-19NANJING UNIV OF AERONAUTICS & ASTRONAUTICS +1

Patent Information

Application Number
CN202410968125.7
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-18
Publication Date
2024-11-19
Estimated Expiration
2044-07-18

Smart Images

  • Figure CN118983028A_ABST
    Figure CN118983028A_ABST
Patent Text Reader

Abstract

The invention discloses a macroscopic and microscopic progressive failure analysis method for a composite material. The method comprises the following steps: establishing a finite element RVE microscopic model according to performance parameters of the composite material; the macroscopic stress of the macroscopic component made of the composite material is converted into local stress on the microcosmic level through an improved stress amplification coefficient method; and based on the performance parameters of each component of the composite material, establishing a corresponding failure model, and carrying out progressive failure analysis on the macroscopic component of the composite material. The method can be applied to progressive failure simulation analysis of the macroscopic component of the composite material under the forms of stretching, bending, torsional load and combined load, and has important significance on research and design of the macroscopic component of the composite material.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of progressive failure of metal matrix composite materials, in particular to a macroscopic and microscopic progressive failure analysis method of composite materials. Background Art

[0002] Fiber-reinforced metal matrix composites have the following advantages: (1) high specific strength and large specific modulus; (2) designable material properties; (3) good corrosion resistance and durability; (4) small thermal expansion coefficient. Brittle fibers such as silicon carbide fibers, carbon fibers, and boron fibers have the advantages of high hardness and high specific modulus and are widely used as the reinforcement phase of composite materials.

[0003] As a new material in the aviation field, SiC / Ti composites have been applied to low-pressure turbine shafts, integral blade rings, and blades of aircraft engines. Due to the addition of reinforcement phases and the existence of interfaces, the damage evolution of SiC / Ti composites is complex and may involve multiple failure modes, such as fiber breakage, matrix yielding, matrix cracking, fiber-matrix interface debonding, etc. There is a strong interaction between them, which makes its failure analysis more difficult. In addition, in actual engineering applications, due to the diversity of composite structures (such as layer structures and open-pore structures) and the complexity of loads, composite structures are inevitably subject to complex loads. Therefore, considering the geometric inhomogeneity of the composite microstructure and the complex load state of actual working conditions, the fiber and matrix will play different roles under different conditions, and it becomes more difficult to analyze the failure behavior of composite materials under complex stress states.

[0004] The commonly used macroscopic structural failure analysis treats the composite single-layer plate as a homogenized material for failure judgment, which cannot accurately reflect the macroscopic material failure process caused by the damage evolution of the microscopic component materials. The existing macro-micro combined progressive damage analysis method does not take into account the structural characteristics of metal matrix composites and is not suitable for cross-scale analysis of complex stress states. Summary of the invention

[0005] In order to solve the above problems, the present invention proposes a composite material macro-micro progressive failure analysis method which takes into account the composite material stiffness reduction caused by metal matrix yielding.

[0006] In order to achieve the above object, the present invention is implemented by the following technical solutions:

[0007] The present invention is a macro-micro progressive failure analysis method for composite materials, comprising the following operations:

[0008] Step 1, obtaining performance parameters of each component of the composite material according to a composite material component performance test;

[0009] Step 2, establishing a finite element RVE microscopic model according to the performance parameters of the composite material;

[0010] Step 3: Select reference points of each component on the composite material finite element RVE micro-model, and calculate the mechanical stress magnification coefficient M of the reference points of each component on the finite element RVE micro-model by using the improved stress magnification coefficient method and ABAQUS finite element software. σ and thermal stress amplification factor A σ ;

[0011] Step 4, using the finite element RVE microscopic model to simulate the macroscopic mechanical properties of the composite material, predicting the initial macroscopic elastic constants of the orthotropic composite material, including E11, E22, E33, μ12, μ13, μ23, G12, G13, G23;

[0012] Step 5, assigning the initial macro elastic constant to the macro component and applying a macro load increment to perform calculations to obtain the stress state of each unit of the macro component;

[0013] Step 6, taking the stress state of each unit of the macroscopic component as the stress boundary condition of the finite element RVE microscopic model, substituting the temperature change value ΔT, and solving to obtain the microscopic stress of each component reference point;

[0014] Step 7, bringing the microscopic stress of each component reference point into the corresponding failure criterion, judging the failure condition of the reference point, reducing the macroscopic elastic constant of the composite material according to the failure condition, and replacing the initial macroscopic elastic constant in step 4, and returning to step 4 until the macroscopic component completely fails;

[0015] Step 8, the failure analysis process of the macroscopic component from step 1 to step 7 is written into a composite material macro-micro progressive failure analysis VUMAT subroutine using Fortran language.

[0016] A further improvement of the present invention is that the composite material component performance test in step 1 includes a composite material nanoindentation test and a fiber push-out test.

[0017] The further improvement of the present invention is that the composite material includes fibers, a matrix, and a coating, and the established finite element RVE microscopic model includes a fiber failure model, a matrix failure model, and an interface damage failure model of the interface between the coating and the matrix.

[0018] Among them, the fiber failure model adopts the three-dimensional Hashin criterion, which includes:

[0019] Fiber axial tensile failure, σ 11 ≥0:

[0020]

[0021] Fiber axial compression failure, σ 11 <0:

[0022]

[0023] Among them, X T is the fiber tensile strength, X C is the fiber compression strength, S 12 is the fiber shear strength, σ 11 is the axial stress on the fiber, σ 12 and σ 13 is the shear stress on the fiber;

[0024] The matrix failure model adopts the Mise criterion, where the Mises equivalent stress is expressed as:

[0025]

[0026] in, is the macro stress at the integration point in the finite element analysis, σ x , σ y , σ z is the normal stress on the matrix in the three coordinate axis directions, τ xy , τ yz , τ zx is the shear stress on the matrix in the directions of the three coordinate axes;

[0027] Interface damage failure models include:

[0028] The secondary failure criterion is used to evaluate the interface damage;

[0029] When the cohesive element meets the secondary failure criterion, the Benzeggagh-Kenane criterion is used to define the damage evolution under the mixed stress mode.

[0030] A further improvement of the present invention is that: in step 3, the mechanical stress amplification coefficient M of the reference point of each component on the finite element RVE microscopic model is calculated and solved by using ABAQUS finite element software σ and thermal stress amplification factor A σ , the calculation expression is:

[0031]

[0032] in, is the macro stress at the integration point in the finite element analysis, σ k is the micro stress at the microscopic reference point k, M σ is the mechanical stress amplification factor of the reference point k, A σis the thermal stress amplification coefficient of the reference point k, and ΔT is the difference between the zero thermal stress temperature and the ambient temperature.

[0033] A further improvement of the present invention is that the failure conditions in step 7 include interface debonding, matrix yielding, interface cracking, and fiber breakage.

[0034] A further improvement of the present invention is that the composite material is a SiC / Ti composite material.

[0035] The beneficial effects of the present invention are as follows: the composite material macro-micro progressive failure analysis method proposed by the present invention can be applied to the calculation and analysis of various torsion, tension, bending loads and composite load forms, and the compiled subroutine analysis module is highly efficient.

[0036] The composite material macro-micro progressive failure analysis method proposed in the present invention improves the stress magnification factor method: (1) the composite material stiffness reduction caused by metal matrix yielding is considered; (2) the composite material stiffness reduction caused by interface damage is considered; (3) the effect of interface damage on the stress magnification factor is considered. The improved stress magnification factor method can be better applied to the progressive failure prediction analysis of metal matrix composite materials. BRIEF DESCRIPTION OF THE DRAWINGS

[0037] Figure 1 is a flow chart of the macro-micro progressive failure analysis method of the present invention;

[0038] Figure 2 is a schematic diagram of a finite element RVE mesoscopic model in an embodiment of the present invention;

[0039] Figure 3 is a cohesion-displacement schematic diagram of a bilinear cohesion model under tension in an embodiment of the present invention;

[0040] Figure 4 is a schematic diagram of stress amplification factor reference points in an embodiment of the present invention, wherein a is a fiber reference point, b is an interface reference point, and c is a matrix reference point;

[0041] Figure 5 Schematic diagram of RVE response under unit macroscopic stress in all directions in an embodiment of the present invention;

[0042] FIG6( a ) is a schematic diagram showing the initial evolution of interfacial debonding damage in an embodiment of the present invention;

[0043] FIG6( b ) is an enlarged schematic diagram of the evolution of interfacial debonding damage in an embodiment of the present invention;

[0044] FIG. 7( a ) is a schematic diagram of the onset of matrix yield failure evolution in an embodiment of the present invention;

[0045] FIG. 7( b ) is a schematic diagram of the enlarged evolution of the matrix yield failure in an embodiment of the present invention;

[0046] FIG8( a ) is a schematic diagram of the initiation of matrix crack failure evolution in an embodiment of the present invention;

[0047] FIG8( b ) is a schematic diagram of the enlarged evolution of matrix crack failure in an embodiment of the present invention;

[0048] FIG9( a ) is a schematic diagram of the initiation of fiber fracture damage evolution in an embodiment of the present invention;

[0049] FIG9( b ) is a schematic diagram of the fiber fracture damage evolution expansion T=203400 N·m in an embodiment of the present invention;

[0050] FIG9( c ) is a schematic diagram of the fiber fracture damage evolution expansion T=207200 N·m in an embodiment of the present invention. DETAILED DESCRIPTION

[0051] In order to make the purpose, technical solutions and advantages of the present invention more clearly understood, the present invention is further described in detail below in conjunction with the accompanying drawings and embodiments. It should be understood that the specific embodiments described herein are only used to explain the present invention and are not intended to limit the present invention. In addition, the technical features involved in the various embodiments of the present invention described below can be combined with each other as long as they do not conflict with each other.

[0052] like Figure 1 As shown, the composite macro-micro progressive failure analysis method of this embodiment, combined with the micromechanical failure theory, selects the failure criteria of each component of the composite material to evaluate the damage type of SiC / Ti composite material in asymptotic failure, and the damage type of SiC / Ti composite material in progressive failure, takes into account the influence of interface damage evolution and nonlinear behavior of the matrix on the macroscopic properties of the composite material, as well as the composite material stiffness degradation caused by interface debonding and matrix yielding, improves the stress amplification factor, and can use Fortran language to write the composite macro-micro progressive failure analysis method into a SiC / Ti composite material macro-micro progressive failure analysis VUMAT subroutine module, thereby improving the efficiency of composite material progressive failure analysis prediction.

[0053] This embodiment performs macro-micro progressive failure analysis on SiC / Ti-6Al-4V composite material, including the following steps:

[0054] Step 1, obtain the performance parameters of each microscopic component of the SiC / Ti-6Al-4V composite material through SiC / Ti-6Al-4V composite material component performance test experiments or literature data. Tables 1 and 2 are the material properties of the SiC / Ti composite material components obtained from the SiC / Ti-6Al-4V composite material component performance test experiments;

[0055] Table 1 Test values ​​of Young's modulus of each component of SiC / Ti composite materials

[0056]

[0057] Table 2 Material properties of each component of SiC / Ti composite material

[0058]

[0059] Step 2: Use ABAQUS finite element software to establish a finite element RVE microscopic model, such as Figure 2 As shown in the figure. Reduced integration elements (C3D8R) are used for the fiber, matrix, and coating, and eight-node cohesive elements (COH3D8) are used for the interface between the coating and the matrix. The fiber and matrix are isotropic materials in the global Cartesian coordinate system, and the fiber coating and interface are transversely isotropic materials in the cylindrical coordinate system. A callable periodic boundary condition program is written in Python to apply boundary conditions to the finite element RVE microscopic model to ensure deformation coordination and correct stress transfer during loading.

[0060] The fiber failure model uses the three-dimensional Hashin criterion:

[0061] Fiber axial tensile failure, σ 11 ≥0:

[0062]

[0063] Fiber axial compression failure, σ 11 <0:

[0064]

[0065] Among them, X T is the fiber tensile strength, X C is the fiber compression strength, S 12 is the fiber shear strength, σ 11 is the axial stress on the fiber, σ 12 and σ 13 is the shear stress on the fiber.

[0066] The matrix failure model adopts the Mise criterion, and the Mises equivalent stress can be expressed as:

[0067]

[0068] in, is the macro stress at the integration point in the finite element analysis, σ x , σ y , σ zis the normal stress on the matrix in the three coordinate axis directions, τ xy , τ yz , τ zx is the shear stress on the matrix in the directions of the three coordinate axes.

[0069] The interface damage failure model adopts a bilinear cohesive force model. Figure 3 This is a schematic diagram of the cohesion-displacement of the bilinear cohesion model under tension. The selection of the interface damage failure model is explained as follows:

[0070] Before damage occurs at the composite interface, the relationship between cohesion and displacement is linear elastic, and the strain relationship between stress and opening displacement can be expressed as:

[0071]

[0072] Among them, σ n is the stress value in the normal direction, σ s is the stress value in the first shear direction, σ t is the stress value in the second shear direction, δ n , δ s , δ t is the opening displacement in the normal direction, the first shear direction, and the second shear direction, K nn , K ss , K tt They are the stiffness corresponding to the opening, sliding and tearing crack forms respectively.

[0073] Taking an opening crack as an example, when the interface begins to be damaged, the stress of the interface is expressed as:

[0074] σ=(1-D)N max

[0075] Where, σ is the stress at the interface, N max is the maximum value of the interface bonding force of the cohesive force unit, and the damage variable D represents the degree of damage to the interface. Before the damage begins to occur, the damage variable D is equal to 0. After the damage begins to occur, the expression of the damage variable D is:

[0076]

[0077] Where δ is the opening displacement of the interface, δ 0 The displacement when the interface starts to be damaged, δ f is the displacement when the interface is completely damaged. The secondary damage criterion is used to evaluate the interface damage, and the expression of the secondary damage criterion is:

[0078]

[0079] Among them, <σ n> indicates that pure compressive stress will not cause interface damage, N max , S max , and T max are the interface bonding strengths corresponding to the opening type, sliding type, and tearing type cracks. The interface normal bonding strength N of the composite material in the interface damage failure model max Take 120MPa, S max , and T max Take 170MPa.

[0080] When the cohesive element meets the secondary failure criterion, the Benzeggagh-Kenane criterion (BK criterion) is used to define the damage evolution under the mixed stress mode. The stress after the interface is damaged under the complex stress state can be expressed as:

[0081]

[0082] in, and are the stress values ​​when the interface begins to be damaged in the normal direction, the first shear direction, and the second shear direction, respectively. At this time, the damage variable D can be expressed as:

[0083]

[0084] in, is the equivalent displacement corresponding to the beginning of damage, is the equivalent displacement corresponding to the complete damage, is the maximum value of the equivalent displacement during the entire loading process. The equivalent displacement can be defined as

[0085] Step 3: By improving the stress magnification factor method, the mechanical stress magnification factor M of the reference point of each material component of the finite element RVE microscopic model is calculated using ABAQUS finite element software. σ and thermal stress amplification factor A σ The stress magnification factor can convert the macroscopic stress of the macroscopic component of the composite material into the local stress of the fiber, matrix, and fiber-matrix interface at the microscopic level. The relationship between macroscopic and microscopic stress conversion achieved by the stress magnification factor is expressed as:

[0086]

[0087] in, is the macro stress at the integration point in the finite element analysis, σ k is the micro stress at the microscopic reference point k, M σ is the mechanical stress amplification factor of the reference point k, A σ is the thermal stress amplification factor of the reference point k, where M σis a 6×6 matrix, A σ is a 6×1 vector, ΔT is the difference between the zero thermal stress temperature and the ambient temperature, and its expanded form is:

[0088] σ k =[σ11σ22σ33τ12τ13τ23] T

[0089]

[0090] A σ =[A1 A2 A3 A4 A5 A6] T

[0091] Among them, σ11, σ22, and σ33 are the positive microstresses on the microscopic reference point k in the directions of the three coordinate axes, and τ12, τ13, and τ23 are the shear stresses on the microscopic reference point k in the directions of the three coordinate axes. is the positive macroscopic stress on the reference point k in the three coordinate axis directions in the finite element analysis, is the shear stress on the reference point k in the three coordinate axis directions in the finite element analysis, and A1, A2, A3, A4, A5, and A6 are the thermal stress amplifications of the reference point k in the six directions.

[0092] Applying the unit macroscopic stress component and the unit temperature difference distribution to the RVE, the mechanical stress and thermal stress amplification coefficient of each reference point can be calculated based on the stress response. The reference points should be selected to include the locations where damage may occur in the RVE. In this example, reference points are selected on the fiber, matrix, and interface, such as Figure 4 As shown, the reference points in the fiber are F1-F14, the reference points on the matrix are M1-M15, and the interface reference points are I1-I14.

[0093] The stress magnification factor is solved by the finite element RVE microscopic model. Taking the mechanical stress magnification factor as an example, the stress load is first applied Mesoscopic stress σ at the mesoscopic reference point k in the finite element RVE mesoscopic model k =[σ 11 σ 22 σ 33 τ 12 τ 13 τ 23 ] T It can be calculated by finite element method. And ΔT=0. σ k and ΔT into the expression In the above equation, we can solve for M σThe six parameters in the matrix are M11, M21, M31, M41, M51, and M61. Therefore, the mechanical stress amplification matrix M σ All unknown parameters in can be solved by applying unit loads in six degrees of freedom to the RVE, such as Figure 5 As shown. For the thermal stress amplification factor A σ , select and ΔT = 1, and the microscopic stress value σ of each reference point on the RVE is calculated by the finite element method k Similarly, the thermal stress amplification factor A is solved σ .

[0094] Step 4, use the RVE finite element model to simulate the macroscopic mechanical properties of the composite material and predict the initial elastic constants of the orthotropic composite material, including E11, E22, E33, μ12, μ13, μ23, G12, G13, and G23.

[0095] Step 5, assigning the initial macro elastic constant to the macro component and applying a macro load increment for calculation to obtain the stress state of each unit of the macro component.

[0096] Step 6: Use the stress state of each unit of the macroscopic component as the stress boundary condition of the finite element RVE microscopic model, substitute the temperature change value ΔT, and solve to obtain the microscopic stress of each component reference point.

[0097] Step 7, bring the microscopic stress of each component reference point into the corresponding failure criterion, judge the failure condition of the reference point, and reduce the macro elastic constant of the composite material according to the failure condition, such as interface debonding or matrix yield, combined with the fiber failure model, matrix failure model, interface damage failure model and stiffness reduction matrix, and replace the initial macro elastic constant in step 4, and return to step 4 until the macro component fails completely.

[0098] The metal matrix composite material of this embodiment will produce four failure modes during the loading process: interface debonding, matrix yielding, matrix cracking, and fiber breakage. When the material produces any one or several of the above damages, the material as a whole will produce a reduction in stiffness. When the metal matrix composite material is subjected to load, the fiber mainly bears the axial load, and the matrix mainly bears the lateral load, shear load, and part of the axial load. Therefore, matrix yielding and fiber breakage will affect the axial stiffness of the composite material, matrix yielding and matrix cracking will affect the lateral stiffness of the composite material, and damage to the fiber, matrix, and interface will affect the shear stiffness of the composite material. The stiffness degradation matrix of the composite material after damage is as follows:

[0099]

[0100] In the stiffness degradation matrix:

[0101] dC11=(1-d y )(1-d f )C11

[0102] dC22=(1-d i,y,m )C22

[0103] dC33=(1-d i,y,m )C33

[0104] dC12=(1-d f )(1-d i,y,m )C12

[0105] dC13=(1-d f )(1-d i,y,m )C13

[0106] dC23=(1-d f )(1-d i,y,m )C23

[0107] dG12=(1-d i,y,m )(1-d f )

[0108] dG13=(1-d i,y,m )(1-d f )

[0109] Among them, Cij (i, j = 1, 2, 3) and Gij (i, j = 1, 2, 3) are the elastic constants of the material components, dCij (i, j = 1, 2, 3) and dGij (i, j = 1, 2, 3) are the elastic constants of the material components after damage degradation, and d f is the fiber stiffness degradation index, d m is the matrix cracking stiffness degradation index, d i is the interface stiffness degradation index, d y is the matrix yield stiffness degradation index, d i,y,m =max{d i ,d y ,d m} is the maximum value of stiffness degradation caused by current interface damage, matrix yielding, and matrix cracking. When the composite material is in the non-destructive stage, all stiffness degradation indexes are 0. When matrix cracking or fiber damage occurs, the stiffness reduction is an instantaneous degradation type, and the fiber stiffness degradation index and matrix cracking stiffness degradation index are 0.99. When interface debonding and matrix yielding occur, the stiffness reduction is related to the number of failure reference points of the material components and the area of ​​the damaged area. The interface stiffness degradation index is 0.58, and the matrix yield stiffness degradation index is 0.28 in the axial direction and 0.33 in the transverse and shear directions.

[0110] Step 8, the failure analysis process of the macroscopic component from step 1 to step 7 is written into a composite material macro-micro progressive failure analysis VUMAT subroutine using Fortran language.

[0111] Figure 6(a) to Figure 9(c) The results of the progressive damage analysis of the 0° ply of the SiC / Ti turbine shaft under torsional load are shown, taking a certain type of aircraft engine turbine shaft as a prototype. The turbine shaft is the main load-bearing component of the turbine engine under high-speed rotation. It supports rotating components such as the wheel disc and blades and transmits loads during operation. The loads borne by the engine main shaft are relatively complex, and the loads borne mainly include torsional loads, axial loads, bending loads, radial loads and other types. This embodiment takes the progressive failure under torsional load as an example, and the analysis process of axial load and bending load is the same as this example. Among them, SDV20 is the matrix cracking damage index, SDV23 is the matrix yield damage index, SDV25 is the interface debonding damage index, and SDV27 is the fiber breakage damage index. When the damage index is greater than or equal to 1, it is considered that the unit has produced the corresponding damage form. The larger the SDV value, the earlier the belt unit produces the damage form.

[0112] It will be understood by those skilled in the art that, unless otherwise defined, all terms (including technical and scientific terms) used herein have the same meaning as those generally understood by those skilled in the art in the art to which the present invention belongs. It should also be understood that terms such as those defined in common dictionaries should be understood to have the same meaning as in the context of the prior art, and will not be interpreted with an idealized or overly formal meaning unless defined similarly here.

[0113] The specific implementation methods described above further illustrate the objectives, technical solutions and beneficial effects of the present invention in detail. It should be understood that the above description is only a specific implementation method of the present invention and is not intended to limit the present invention. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principles of the present invention should be included in the scope of protection of the present invention.

Claims

1. Macro- and micro-progressive failure analysis method for composite materials, characterized by: The following operations are included: Step 1, obtaining performance parameters of each component of the composite material according to a composite material component performance test; Step 2, establishing a finite element RVE microscopic model according to the performance parameters of the composite material; Step 3: Select reference points of each component on the composite material finite element RVE micro-model, and calculate the mechanical stress magnification coefficient M of the reference points of each component on the finite element RVE micro-model by using the improved stress magnification coefficient method and ABAQUS finite element software. σ and thermal stress amplification factor A σ ; Step 4, using the finite element RVE microscopic model to simulate the macroscopic mechanical properties of the composite material, predicting the initial macroscopic elastic constants of the orthotropic composite material, including E11, E22, E33, μ12, μ13, μ23, G12, G13, G23; Step 5, assigning the initial macro elastic constant to the macro component and applying a macro load increment to perform calculations to obtain the stress state of each unit of the macro component; Step 6, taking the stress state of each unit of the macroscopic component as the stress boundary condition of the finite element RVE microscopic model, substituting the temperature change value ΔT, and solving to obtain the microscopic stress of each component reference point; Step 7, bringing the microscopic stress of each component reference point into the corresponding failure criterion, judging the failure condition of the reference point, reducing the macroscopic elastic constant of the composite material according to the failure condition, and replacing the initial macroscopic elastic constant in step 4, and returning to step 4 until the macroscopic component completely fails; Step 8, the failure analysis process of the macroscopic component from step 1 to step 7 is written into a composite material macro-micro progressive failure analysis VUMAT subroutine using Fortran language.

2. The composite material macro-micro progressive failure analysis method according to claim 1, characterized in that: The composite material component performance test in step 1 includes a composite material nanoindentation test and a fiber push-out test.

3. The composite material macro-micro progressive failure analysis method according to claim 1, characterized in that: The composite material includes fibers, a matrix, and a coating. The established finite element RVE microscopic model includes a fiber failure model, a matrix failure model, and an interface damage failure model of the interface between the coating and the matrix. Among them, the fiber failure model adopts the three-dimensional Hashin criterion, which includes: Fiber axial tensile failure, σ 11 ≥0: Fiber axial compression failure, σ 11 <0: Among them, X T is the fiber tensile strength, X C is the fiber compression strength, S 12 is the fiber shear strength, σ 11 is the axial stress on the fiber, σ 12 and σ 13 is the shear stress on the fiber; The matrix failure model adopts the Mise criterion, where the Mises equivalent stress is expressed as: in, is the macro stress at the integration point in the finite element analysis, σ x , σ y , σ z is the normal stress on the matrix in the three coordinate axis directions, τ xy , τ yz , τ zx is the shear stress on the matrix in the directions of the three coordinate axes; Interface damage failure models include: The secondary failure criterion is used to evaluate the interface damage; When the cohesive element meets the secondary failure criterion, the Benzeggagh-Kenane criterion is used to define the damage evolution under the mixed stress mode.

4. The composite material macro-micro progressive failure analysis method according to claim 1, characterized in that: In step 3, ABAQUS finite element software is used to calculate and solve the mechanical stress magnification coefficient M of the reference point of each component on the finite element RVE microscopic model. σ and thermal stress amplification factor A σ , the calculation expression is: in, is the macro stress at the integration point in the finite element analysis, σ k is the micro stress at the microscopic reference point k, M σ is the mechanical stress amplification factor of the reference point k, A σ is the thermal stress amplification coefficient of the reference point k, and ΔT is the difference between the zero thermal stress temperature and the ambient temperature.

5. The composite material macro-micro progressive failure analysis method according to claim 1, characterized in that: The failure conditions in step 7 include interface debonding, matrix yielding, interface cracking, and fiber breakage.

6. The composite material macro-micro progressive failure analysis method according to claim 1, characterized in that: The composite material is a SiC / Ti composite material.

Citation Information

Patent Citations

  • Random damage morphology prediction method and system for fiber reinforced composite material structure

    CN113987895A

  • Multi-scale simulation method for vibration fatigue damage of 2.5 D woven composite material

    CN114912309A

  • Composite material structure multi-scale analysis method and application thereof

    CN117316358A

  • Dynamic Progressive Failure Analysis Method For Composite Multi-Scale Model

    US20220284150A1

Cited By

  • Method for analyzing dynamic performance degradation of protective coating-composite sheet in thermal vibration environment

    CN120102619A