Stress liner in semiconductor devices

By introducing stress lining and multi-patterning processes into semiconductor devices, the problem of insufficient hole mobility in the channel region during semiconductor device manufacturing is solved, thereby improving device performance.

CN118983337APending Publication Date: 2024-11-19TAIWAN SEMICONDUCTOR MANUFACTURING CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410109793.4
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2023-11-17
Filing Date
2024-01-26
Publication Date
2024-11-19

AI Technical Summary

Technical Problem

As semiconductor device sizes shrink and manufacturing processes become more complex, existing technologies struggle to effectively improve hole mobility in the channel region, impacting device performance.

Method used

Introducing stress liner into semiconductor devices enhances hole mobility in the channel region by providing compressive stress in the nanostructured channel region or fin structure. Gate and fin structures are formed using multi-patterning and self-aligned processes, and stress liner is set in ESL and ILD layers to transfer compressive stress.

Benefits of technology

By introducing compressive stress into the channel region, hole mobility is significantly improved, thereby enhancing the performance of semiconductor devices.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118983337A_ABST
    Figure CN118983337A_ABST
Patent Text Reader

Abstract

The invention discloses a stress liner in a semiconductor device. The invention discloses a semiconductor device and a manufacturing method of the semiconductor device. The semiconductor device includes a substrate, a nanostructured channel region disposed on the substrate, a gate structure surrounding the nanostructured channel region, a source / drain (S / D) region disposed adjacent to the nanostructured channel region, an etch stop layer (ESL) disposed on the S / D region, a stress liner disposed on the etch stop layer and configured to provide a compressive stress in the nanostructure channel region, an interlayer dielectric (ILD) layer disposed on the stress liner, and a contact structure disposed in the S / D region, the ESL, the stress liner, and the ILD layer.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present disclosure relates to stressed liners in semiconductor devices. Background Art

[0002] As semiconductor technology advances, there is an increasing demand for higher storage capacity, faster processing systems, higher performance, and lower costs. To meet these demands, the semiconductor industry continues to shrink the size of semiconductor devices, such as metal oxide semiconductor field effect transistors (MOSFETs), including planar MOSFETs and fin field effect transistors (finFETs). This shrinking increases the complexity of semiconductor manufacturing processes. Summary of the invention

[0003] According to a first aspect of the present disclosure, a semiconductor device is provided, comprising: a substrate; a nanostructure channel region disposed on the substrate; a gate structure surrounding the nanostructure channel region; a source / drain (S / D) region disposed adjacent to the nanostructure channel region; an etch stop layer (ESL) disposed on the S / D region; a stress liner disposed on the etch stop layer and configured to provide compressive stress in the nanostructure channel region; an interlayer dielectric (ILD) layer disposed on the stress liner; and a contact structure disposed in the S / D region, the ESL, the stress liner, and the ILD layer.

[0004] According to a second aspect of the present disclosure, a semiconductor device is provided, comprising: a substrate; a fin structure disposed on the substrate; a gate structure disposed on the fin structure; a source / drain (S / D) region disposed adjacent to the fin structure; and a dielectric layer stack disposed on the S / D region, comprising: a first dielectric layer disposed on the S / D region; a second dielectric layer disposed on the first dielectric layer and configured to provide compressive stress in the fin region of the fin structure; and a third dielectric layer disposed on the second dielectric layer, wherein the materials of the first dielectric layer, the second dielectric layer, and the third dielectric layer are different from each other.

[0005] According to a third aspect of the present disclosure, a method for forming a semiconductor device is provided, comprising: forming a first nanosheet stack and a second nanosheet stack on a substrate; forming a first polysilicon structure and a second polysilicon structure on the first nanosheet stack and the second nanosheet stack, respectively; forming a first source / drain (S / D) region adjacent to the first nanosheet stack and a second source / drain (S / D) region adjacent to the second nanosheet stack; depositing a semiconductor layer on the first polysilicon structure and the second polysilicon structure and on the first S / D region and the second S / D region; depositing a dielectric layer on the semiconductor layer; performing a thermal annealing process on the dielectric layer and the semiconductor layer; and replacing the first polysilicon structure and the sacrificial layer in the first nanosheet stack with a first gate structure, and replacing the second polysilicon structure and the sacrificial layer in the second nanosheet stack with a second gate structure. BRIEF DESCRIPTION OF THE DRAWINGS

[0006] Aspects of the present disclosure are best understood from the following detailed description when read with the accompanying figures.

[0007] Figure 1A An isometric view of a semiconductor device having a stressed liner is shown in accordance with some embodiments.

[0008] Figures 1B to 1G Different cross-sectional views of a semiconductor device having a stressed liner according to some embodiments are shown.

[0009] Figure 2 is a flow chart of a method for fabricating a semiconductor device having a stressed liner according to some embodiments.

[0010] FIG. 3A to FIG. 11A and 3B to Fig. 11B Cross-sectional views of a semiconductor device with a stressed liner at various stages of its fabrication process are shown in accordance with some embodiments.

[0011] Illustrative embodiments will now be described with reference to the drawings.In the drawings, like reference numbers generally indicate identical, functionally similar, and / or structurally similar elements. DETAILED DESCRIPTION

[0012] The following disclosure provides many different embodiments or examples for implementing the different features of the provided subject matter. Specific examples of components and arrangements are described below to simplify the present disclosure. Of course, these are only examples and are not intended to be limiting. For example, in the following description, a process for forming a first feature on a second feature may include an embodiment in which the first feature and the second feature are formed in direct contact, and may also include an embodiment in which an additional feature may be formed between the first feature and the second feature so that the first feature and the second feature may not be in direct contact. As used herein, forming a first feature on a second feature means that the first feature and the second feature are formed in direct contact. In addition, the present disclosure may repeat reference numerals and / or letters in various examples. The repetition itself does not indicate the relationship between the various embodiments and / or configurations discussed.

[0013] Spatially relative terms (e.g., "below," "lower," "above," "higher," etc.) may be used herein to facilitate describing the relationship of one element or feature illustrated in a figure relative to another element(s) or feature(s). These spatially relative terms are also intended to encompass different orientations of the device in use or operation in addition to the orientation illustrated in the figures. The device may be oriented in other orientations (rotated 90 degrees or at other orientations), and the spatially relative descriptors used herein should be similarly interpreted accordingly.

[0014] It should be noted that references in the specification to "one embodiment," "an embodiment," "an example embodiment," "exemplary," etc. indicate that the described embodiment may include a particular feature, structure, or characteristic, but not every embodiment may include the particular feature, structure, or characteristic. Furthermore, such phrases do not necessarily refer to the same embodiment. In addition, when a particular feature, structure, or characteristic is described in conjunction with an embodiment, whether or not explicitly described, it is within the knowledge of those skilled in the art to implement such feature, structure, or characteristic in conjunction with other embodiments.

[0015] It should be understood that the phraseology or terminology herein is for the purpose of description rather than limitation, so that the phraseology or terminology of the specification is interpreted by persons skilled in the relevant art(s) based on the teachings herein.

[0016] In some embodiments, the terms "about" and "substantially" may indicate that the value of a given amount varies within 5% to 20% of the value (e.g., ±1%, ±2%, ±3%, ±4%, ±5%, ±10%, ±10% to ±15%, ±15% to ±20% of the value). These values ​​are examples only and are not intended to be limiting. The terms "about" and "substantially" may refer to a percentage of a value as interpreted by one or more persons skilled in the relevant art(s) in accordance with the teachings herein.

[0017] The gate-all-around (GAA) transistor structure can be patterned by any suitable method. For example, one or more photolithography processes (including double patterning processes or multi-patterning processes) can be used to pattern these structures. The double patterning process or the multi-patterning process can combine the photolithography process and the self-alignment process, thereby allowing the generation of patterns with, for example, a spacing smaller than the spacing obtainable using a single direct photolithography process. For example, in one embodiment, a sacrificial layer is formed on the substrate and patterned using a photolithography process. Spacers are formed along the patterned sacrificial layer using a self-alignment process. The sacrificial layer is then removed, and the remaining spacers can then be used to pattern the GAA structure.

[0018] The fin structure disclosed herein can be patterned by any suitable method. For example, the fin structure can be patterned using one or more photolithography processes (including double patterning processes or multi-patterning processes). The double patterning process or the multi-patterning process can combine the photolithography process and the self-alignment process, thereby allowing the generation of patterns with, for example, a pitch smaller than that obtainable using a single direct photolithography process. For example, a sacrificial layer is formed on a substrate and patterned using a photolithography process. Spacers are formed along the patterned sacrificial layer using a self-alignment process. The sacrificial layer is then removed, and the remaining spacers can then be used to pattern the fin structure.

[0019] The present disclosure provides an example structure of a p-type FET (PFET) with a stress liner to enhance hole mobility in a channel region between adjacent source / drain (S / D) regions. By using a stress liner, longitudinal compressive stress in the channel region can be increased, which can increase the mobility of holes flowing in the channel region. Increasing hole mobility in the channel region can improve device performance.

[0020] In some embodiments, the PFET may include a channel region of a nanostructure, a gate structure surrounding the channel region of the nanostructure, and an S / D region on either side of the channel region of the nanostructure. The PFET may also include an etch stop layer (ESL), a stress liner, and an interlayer dielectric (ILD) layer. In some embodiments, the ESL may be disposed on the S / D region and disposed along the sidewall of the gate structure. In some embodiments, the stress liner may be disposed on the ESL, and the ILD layer may be disposed on the stress liner. The stress liner applies pressure to the gate structure, which is transmitted as a longitudinal compressive stress in the nanostructure channel region. In some embodiments, the stress liner may include a semiconductor material of silicon oxide, silicon germanium oxide, germanium oxide, or other suitable oxides.

[0021] Figure 1A An isometric view of a semiconductor device 100 having an NFET 102N and a PFET 102P is shown in accordance with some embodiments. Figure 1B , Figure 1D and Figure 1F shows the NFET 102N along Figure 1A Different cross-sectional views of line AA. Figure 1C , Figure 1E and Figure 1G shows the PFET 102P along Figure 1A Different cross-sectional views of line BB. Figures 1B to 1G A cross-sectional view with additional structures is shown. Figure 1A are not shown for simplicity purposes. Unless otherwise specified, Figures 1A to 1G Discussions of elements with the same annotation apply to each other.

[0022] The semiconductor device 100 may be formed on a substrate 104, wherein the NFET 102N and the PFET 102P are formed on different regions of the substrate 104. Other FETs and / or structures (e.g., isolation structures) may be formed between the NFET 102N and the PFET 102P on the substrate 104. In some embodiments, the substrate 104 may be a semiconductor material, such as silicon, germanium (Ge), silicon germanium (SiGe), a silicon on insulator (SOI) structure, and combinations thereof. In addition, the substrate 104 may be doped with a p-type dopant (e.g., boron, indium, aluminum, or gallium) or an n-type dopant (e.g., phosphorus or arsenic). The semiconductor device 100 may also include a shallow trench isolation (STI) region 105 disposed on the substrate 104. The STI region 105 may include an insulating material, such as silicon oxide (SiO2), silicon nitride (SiN), silicon oxynitride (SiON), silicon oxycarbide (SiOC), silicon carbon nitride (SiCN), silicon oxycarbon nitride (SiOCN), silicon germanium oxide (SiGeO2), or a combination thereof. x ).

[0023] refer to Figure 1A and Figure 1B In some embodiments, the NFET 102N may include: (i) a fin substrate or a sheet substrate 106N disposed on the substrate 104; (ii) an S / D region 108N disposed on the fin substrate or the sheet substrate 106N; (iii) a nanostructure channel region 110N disposed adjacent to the S / D region 108N; (iv) a gate structure 112N surrounding the nanostructure channel region 110N; (v) an external gate spacer 114N disposed along a sidewall of the gate structure 112N; (vi) an internal gate spacer 116 disposed along a sidewall of the S / D region 108N; (vii) an ESL 120N disposed directly on the S / D region 108N; and (viii) an ILD layer 124N disposed directly on the ESL 120N.

[0024] Similarly, refer to Figure 1A and Figure 1C In some embodiments, the PFET 102P may include: (i) a fin substrate or a sheet substrate 106P disposed on the substrate 104; (ii) an S / D region 108P disposed on the fin substrate or the sheet substrate 106P; (iii) a nanostructure channel region 110P disposed adjacent to the S / D region 108P; (iv) a gate structure 112P surrounding the nanostructure channel region 110P; (v) an external gate spacer 114P disposed along a sidewall of the gate structure 112P; (vi) an internal gate spacer 116 disposed along a sidewall of the S / D region 108P; (vii) an ESL 120P disposed directly on the S / D region 108N; (viii) a stress liner 122 disposed directly on the ESL 120P; and (ix) an ILD layer 124N disposed directly on the stress liner 122. S / D regions 108N and S / D regions 108P may be referred to individually or collectively as sources or drains, depending on the context.

[0025] In some embodiments, the fin base or sheet base 106N may include a material similar to that of the substrate 104. The fin base or sheet base 106N may have elongated sides extending along the X-axis. The S / D region 108N may include an epitaxially grown semiconductor material (e.g., Si) and an n-type dopant (e.g., phosphorus and other suitable n-type dopants). The S / D region 108P may include an epitaxially grown semiconductor material (e.g., Si and SiGe) and a p-type dopant (e.g., boron and other suitable p-type dopants).

[0026] As used herein, the term "nanostructure" defines a structure, layer, and / or region as having a horizontal dimension (e.g., along the X-axis and / or Y-axis) and / or a vertical dimension (e.g., along the Z-axis) of less than about 100 nm (e.g., about 90 nm, about 50 nm, about 10 nm, or other values ​​less than about 100 nm). In some embodiments, the nanostructure channel region 110N and the nanostructure channel region 110P may be in the form of a nanosheet, a nanowire, a nanorod, a nanotube, or other suitable nanostructure shape. The nanostructure channel region 110N and the nanostructure channel region 110P may include a semiconductor material similar to or different from the material of the substrate 104. In some embodiments, the nanostructure channel region 110N and the nanostructure channel region 110P may include Si, silicon arsenide (SiAs), silicon phosphide (SiP), silicon carbide (SiC), silicon phosphide carbon (SiCP), silicon germanium (SiGe), silicon germanium boron (SiGeB), germanium boron (GeB), silicon germanium tin boron (SiGeSnB), III-V semiconductor compounds, or other suitable semiconductor materials. In some embodiments, each of the nanostructure channel regions 110N and the nanostructure channel regions 110P may have a thickness of about 3 nm to about 15 nm along the Z axis. Although two nanostructure channel regions 110N are shown under each gate structure 112N, and two nanostructure channel regions 110P are shown under each gate structure 112P, the number of nanostructure channel regions 110N may be 1 to 5, and the number of nanostructure channel regions 110P may be 1 to 5. Although the nanostructure channel regions 110N and the nanostructure channel regions 110P are shown as rectangular cross-sections, the nanostructure channel regions 110N and the nanostructure channel regions 110P may have cross-sections of other geometric shapes (e.g., circular, elliptical, triangular, or polygonal).

[0027] Each of the gate structure 112N and the gate structure 112P may be a multilayer structure and may surround the channel region 110N of the nanostructure and the channel region 110P of the nanostructure, respectively, for which the gate structure 112N and the gate structure 112P may be referred to as a "GAA structure". In some embodiments, the gate pitch may be about 30 nm to about 100 nm. The gate pitch is defined as the sum of the distance along the X-axis between adjacent gate structures having equal gate lengths and the gate length of one of the adjacent gate structures. In some embodiments, each of the gate structure 112N and the gate structure 112P may include: (i) an interfacial oxide (IL) layer 126; (ii) a high-k (HK) gate dielectric layer 128 disposed on the IL layer 126; (iii) a work function metal (WFM) layer 130 disposed on the HK gate dielectric layer 128; (iv) a gate metal filling layer 132 disposed on the WFM layer 130; (v) a conductive cap layer 134 disposed on the gate metal filling layer 132; and (vi) an insulating cap layer 136 disposed on the conductive cap layer 136.

[0028] In some embodiments, the IL layer 126 may include SiO2, SiGeO x or germanium oxide (GeO x In some embodiments, the HK gate dielectric layer 128 may include a high-k dielectric material, such as hafnium oxide (HfO2), titanium oxide (TiO2), hafnium zirconium oxide (HfZrO), tantalum oxide (Ta2O3), hafnium silicate (HfSiO4), zirconium oxide (ZrO2), and zirconium silicate (ZrSiO2). In some embodiments, the WFM layer 130 may include titanium aluminum (TiAl), titanium aluminum carbide (TiAlC), tantalum aluminum (TaAl), tantalum aluminum carbide (TaAlC), Al-doped Ti, Al-doped TiN, Al-doped Ta, Al-doped TaN, or other suitable Al-based materials for the NFET 102N. In some embodiments, the WFM layer 130 may include a Ti-based or Ta-based nitride or alloy that is substantially free of Al (e.g., without Al), such as titanium nitride (TiN), titanium silicon nitride (TiSiN), titanium gold (Ti-Au) alloy, titanium copper (Ti-Cu) alloy, tantalum nitride (TaN), tantalum silicon nitride (TaSiN), tantalum gold (Ta-Au) alloy, and tantalum copper (Ta-Cu) for the PFET 102P. In some embodiments, the gate metal fill layer 132 may include a suitable conductive material, such as tungsten (W), titanium (Ti), silver (Ag), ruthenium (Ru), molybdenum (Mo), copper (Cu), cobalt (Co), Al, iridium (Ir), nickel (Ni), metal alloys, and combinations thereof.

[0029] The insulating capping layer 136 may protect the underlying conductive capping layer 134 from structural and / or compositional degradation during subsequent processing of the semiconductor device 100. In some embodiments, the insulating capping layer 136 may include a nitride material (e.g., SiN) and may have a thickness of about 5 nm to about 10 nm to adequately protect the underlying conductive capping layer 134.

[0030] The conductive cap layer 134 can provide a conductive interface between the gate metal filling layer 132 and the gate contact structure (not shown) to electrically connect the gate metal filling layer 132 to the gate contact structure without directly forming the gate contact structure on or in the gate metal filling layer 132. The gate contact structure is not formed directly on or in the gate metal filling layer 132 to prevent contamination by any processing materials used when the gate contact structure is formed. Contamination of the gate metal filling layer 132 may cause degradation of device performance. Therefore, by using the conductive cap layer 134, the gate structure 112N and the gate structure 112P can be electrically connected to the gate contact structure without compromising the integrity of the gate structure 112N and the gate structure 112P. In some embodiments, the conductive cap layer 134 may include a metal material, such as W, Ru, Mo, Co, other suitable metal materials, and combinations thereof.

[0031] In some embodiments, the gate structure 112N may be electrically isolated from the adjacent S / D region 108N by an external gate spacer 114N, and the gate structure 112P may be electrically isolated from the adjacent S / D region 108P by an external gate spacer 114P. In some embodiments, the external gate spacer 114N and the external gate spacer 114P may include an insulating material, such as SiO2, SiN, SiCN, SiOCN, and combinations thereof. In some embodiments, a portion of the gate structure 112N surrounding the nanostructure channel region 110N may be electrically isolated from the adjacent S / D region 108N by an internal spacer 116. Similarly, a portion of the gate structure 112P surrounding the nanostructure channel region 110P may be electrically isolated from the adjacent S / D region 108P by an internal spacer 116. The internal spacer 116 may include an insulating material, such as SiO2, SiN, SiCN, SiOCN, and combinations thereof. x , SiN, SiCN, SiOCN and combinations thereof.

[0032] In some embodiments, ESL 120N and ESL 120P can have a dielectric constant of about 4 to about 7. In some embodiments, ESL 120N and ESL 120P can include dielectric materials such as lanthanum oxide (LaO), aluminum oxide (Al2O3), yttrium oxide (Y2O3), tantalum carbon nitride (TaCN), zirconium silicide (ZrSi), SiOCN, SiOC, SiCN, zirconium nitride (ZrN), zirconium aluminum oxide (ZrAlO), TiO2, Ta2O3, ZrO2, HfO2, SiN, hafnium silicide (HfSi), aluminum oxynitride (AlON), SiO2, SiC, SiN, and zinc oxide (ZnO).

[0033] In some embodiments, the stress liner 122 may be disposed directly on the ESL 120P and may be configured to provide longitudinal compressive stress in the nanostructure channel region 110P during formation of the stress liner 122, which will be described in detail below. In some embodiments, the stress liner 122 may include a dielectric material, such as SiO x 、SiGeO x ,GeO x Or other oxide semiconductor materials. In some embodiments, the stress liner 122 may also include carbon, nitrogen and / or fluorine atoms, and the concentration of each of the carbon, nitrogen and / or fluorine atoms may be about 0.1 atomic % to about 5 atomic %. In some embodiments, the stress liner 122 may include a germanium-free silicon-based oxide layer or a germanium-free silicon-based oxide layer. In some embodiments, the stress liner 122 may include a silicon-germanium-based oxide layer having a Ge atomic concentration of about 1 atomic % to about 50 atomic %.

[0034] In some embodiments, the concentration of silicon and / or germanium atoms in liner portion 122P1 may be greater than the concentration of silicon and / or germanium atoms in liner portion 122P2. In some embodiments, the concentration of oxygen atoms in liner portion 122P2 may be greater than the concentration of oxygen atoms in liner portion 122P1. In some embodiments, the concentration of silicon and / or germanium atoms in liner portion 122P1 may be greater than the concentration of oxygen atoms in liner portion 122P1, and the concentration of oxygen atoms in liner portion 122P2 may be greater than the concentration of silicon and / or germanium atoms in liner portion 122P2. In some embodiments, liner portion 122P1 may include a non-oxidized Si, Ge, or SiGe layer (e.g., an oxygen-free Si, Ge, or SiGe layer), and liner portion 122P2 may include an oxidized Si, Ge, or SiGe layer (e.g., SiO x 、SiGeO x or GeO x ).

[0035] In some embodiments, the stress liner 122 may have a height H1 of about 5 nm to about 30 nm and a thickness T1 of about 2 nm to about 10 nm. In some embodiments, the bottom surface of the stress liner 122 may be disposed at a distance D1 of about 15 nm to about 25 nm above the top surface of the topmost nanostructure channel region 110P. In some embodiments, the stress liner 122 may be laterally spaced apart from the external gate spacer 114P by a distance D2 of about 2 nm to about 10 nm. Within these ranges of height H1, thickness T1, and distances D1 and D2, the stress liner 122 may provide sufficient longitudinal compressive stress in the nanostructure channel region 110P to enhance hole mobility in the nanostructure channel region 110P, thereby improving the performance of the PFET 102P. Although Figure 1C The sidewalls of the stress liner 122 are shown to form an angle A of about 90 degrees with the horizontal bottom of the stress liner, but according to some embodiments, the angle A may range from about 90 degrees to about 165 degrees.

[0036] In some embodiments, the ILD layer 124N may be disposed directly on the ESL 120N (eg, Figure 1B ), and the ILD layer 124P may be disposed directly on the stress liner 122 (as shown Figure 1C 120P, and the insulating cap layer 136 may be substantially coplanar with each other. In some embodiments, the materials of the ESL 120P, the stress liner 122, and the ILD layer 124P may be different from each other. In some embodiments, the materials of the ESL 120P and the ILD layer 124P may be the same, but different from the material of the stress liner 122. In some embodiments, the stress liner 122 may include a Ge-based oxide layer. According to some embodiments, the ESL 120P and the ILD layer 124P may include a germanium-free oxide or nitride layer.

[0037] refer to Figure 1D and Figure 1EIn some embodiments, the NFET 102N and the PFET 102P may further include an S / D contact structure 138N and an S / D contact structure 138P, respectively. The S / D contact structure 138N and the S / D contact structure 138P may include: (i) a silicide layer 140A and (ii) a contact plug 140B disposed on the silicide layer 140A. The silicide layer 140A may be disposed in the S / D region 108N and the S / D region 108P. The contact plug 140B of the S / D contact structure 138N may extend through the ILD layer 124N and the ESL 120N, and may be disposed on the silicide layer 140A, as shown in FIG. Figure 1D The contact plug 140B of the S / D contact structure 138P may extend through the ILD layer 124P, the stress liner 122, and the ESL 120P, and may be disposed on the silicide layer 140A, as shown. Figure 1E The sidewall of the stress liner 122 may be in contact with the contact plug 140B of the S / D contact structure 138P.

[0038] In some embodiments, the silicide layer 140A in the NFET 102N may include titanium silicide (Ti x Si y ), Tantalum silicide (Ta x Si y ), molybdenum silicide (Mo x Si y ), zirconium silicide (Zr x Si y ), Hafnium Silicide (Hf x Si y ), Scandium Silicate (Sc x Si y ), yttrium silicide (Y x Si y ), terbium silicide (Tb x Si y ), Lutetium silicide (Lu x Si y ), Erbium Silicide (Er x Si y ), Ytterbium silicide (Yb x Si y ), europium silicide (Eu x Si y ), Thorium Silicide (Th x Si y ), other suitable metal silicide materials, or combinations thereof. In some embodiments, the silicide layer 140A in the PFET 102P may include nickel silicide (Ni x Si y ), cobalt silicide (Co x Siy ), manganese silicide (Mn x Si y ), tungsten silicide (W x Si y ), iron silicide (Fe x Si y ), rhodium silicide (Rh x Si y ), palladium silicide (Pd x Si y ), ruthenium silicide (Ru x Si y ), platinum silicide (Pt x Si y ), iridium silicide (Ir x Si y ), Os x Si y ), other suitable metal silicide materials or combinations thereof.

[0039] In some embodiments, the contact plug 140B may include a conductive material having a low resistivity (e.g., a resistivity of about 50 μΩ-cm, about 40 μΩ-cm, about 30 μΩ-cm, about 20 μΩ-cm, or about 10 μΩ-cm), for example, Co, W, Ru, Al, Mo, iridium (Ir), nickel (Ni), osmium (Os), rhodium (Rh), other suitable conductive materials having a low resistivity, and combinations thereof.

[0040] refer to Figure 1F and Figure 1G In some embodiments, NFET 102N and PFET 102P may be finFETs instead of GAA FETs (eg, Figures 1B to 1E ) and may have fin structures 107N and fin structures 107P instead of nanostructure channel regions 110N and nanostructure channel regions 110P and fin substrates 106N and fin substrates 106P. Unlike GAA FETs, finFETs may have gate structures 112N and 112P, which are disposed on fin structures 107N and 107P, respectively. The fin region of the fin structure 107N located below the gate structure 112N and adjacent to the S / D region 106N and the fin region of the fin structure 107P located below the gate structure 112P and adjacent to the S / D region 106P may be used as a channel region. The stress liner 122 may provide longitudinal compressive stress in the fin region of the fin structure 107P.

[0041] Figure 2 According to some embodiments, a method for manufacturing a Figures 1A to 1C102N and PFET 102P as described herein. For purposes of illustration, reference will be made to an exemplary method 200 for fabricating a semiconductor device 100 such as a NFET 102N and a PFET 102P. FIG. 3A to FIG. 11A and FIG. 3B to FIG. 11B An example manufacturing process of the semiconductor device 100 is described as follows. Figure 2 The operation shown. FIG. 3A to FIG. 11A According to some embodiments, NFET 102N is manufactured at various stages along the Figure 1A Cross-sectional view along line AA. FIG. 3B to FIG. 11B According to some embodiments, PFET 102P is manufactured at various stages along the Figure 1A BB. The operations may be performed in a different order or not performed, depending on the particular application. It should be noted that method 200 may not produce a complete semiconductor device 100. Therefore, it should be understood that additional processes may be provided before, during, and after method 200, and only some of the other processes are briefly described herein. Unless otherwise stated, the Figures 1A to 1C , FIG. 3A to FIG. 11A and FIG. 3B to FIG. 11B Discussions of elements with the same annotation apply to each other.

[0042] refer to Figure 2 In operation 205, a superlattice structure is formed on the fin substrate, and a polysilicon structure is formed on the superlattice structure of the NFET and the PFET. Figure 3A and Figure 3BAs described, the superlattice structure 309N and the superlattice structure 309P (also referred to as "nanosheet stack 309N and nanosheet stack 309P") are formed on the fin substrate 106N and the fin substrate 106P, respectively, and the polysilicon structure 312N and the polysilicon structure 312P are formed on the superlattice structure 309N and the superlattice structure 309P, respectively. In some embodiments, the hard mask layer 344A and the hard mask layer 344B may be formed during the formation of the polysilicon structure 312N and the polysilicon structure 312P. The superlattice structure 309N may include the nanostructure layer 110N and the nanostructure layer 311N arranged in an alternating configuration. Similarly, the superlattice structure 309P may include the nanostructure layer 110P and the nanostructure layer 311P arranged in an alternating configuration. In some embodiments, the nanostructure layer 110N and the nanostructure layer 110P may include Si, and the nanostructure layer 311N and the nanostructure layer 311P may include SiGe. In some embodiments, each of the nanostructure layer 110N, the nanostructure layer 311N, the nanostructure layer 110P, and the nanostructure layer 311P may have a thickness along the Z axis of about 3 nm to about 15 nm. The nanostructure layer 311N and the nanostructure layer 311P are also referred to as "sacrificial layer 311N and sacrificial layer 311P". During subsequent processing, the polysilicon structure 312N and the sacrificial layer 311N may be replaced with the gate structure 112N in a gate replacement process, and the polysilicon structure 312P and the sacrificial layer 311P may be replaced with the gate structure 112P.

[0043] Reference Figure 2 In operation 210, S / D regions are formed on the fin substrates of the NFET and the PFET and in the superlattice structure. For example, as shown in FIG. Figure 3A and Figure 3B As described, S / D regions 108N and 108P are formed in superlattice structures 309N and 309P and on fin substrates 106N and 106P. Forming S / D regions 108N and 108P may include the following sequential operations: (i) forming S / D openings (not shown) in superlattice structures 309N and 309P; (ii) depositing a first hard mask layer (not shown) on NFET 102N and PFET 102P; (iii) removing the first hard mask layer from PFET 102P; (iv) epitaxially growing a semiconductor material (e.g., a p-type dopant) in the S / D openings of PFET 102P; and (v) epitaxially growing a semiconductor material (e.g., a p-type dopant) in the S / D openings of PFET 102P. Figure 3B(as shown); (v) removing the first hard mask layer from NFET 102N; (vi) depositing a second hard mask layer (not shown) on NFET 102N and PFET 102P; (vii) removing the second hard mask layer from NFET 102N; (viii) epitaxially growing a semiconductor material having an n-type dopant (e.g., Figure 3A and (ix) removing the second hard mask layer from PFET 102P. In some embodiments, inner spacer 116 may be formed after forming S / D openings in NFET 102N and PFET 102P and before depositing the first hard mask layer on NFET 102N and PFET 102P.

[0044] refer to Figure 2 In operation 215, an ESL is formed on the polysilicon structure and S / D regions of the NFET and PFET. Figure 4A and Figure 4B As described, ESL 120N and ESL 120P are formed on polysilicon structures 312N and polysilicon structures 312P and on S / D regions 108N and S / D regions 108P. Forming ESL 120N and ESL 120P may include: Figure 3A and Figure 3B A dielectric layer of LaO, Al2O3, Y2O3, TaCN, ZrSi, SiOCN, SiOC, SiCN, ZrN, ZrAlO, TiO2, Ta2O3, ZrO2, HfO2, SiN, HfSi, AlON, SiO2, SiC, SiN or ZnO is deposited on the structure to form Figure 4A and Figure 4B structure.

[0045] refer to Figure 2 In operation 220, a stress liner is formed on the ESL of the PFET. FIG. 5A to FIG. 10A and FIG. 5B to FIG. 10B As described above, the stress liner 122 is selectively formed on the ESL 120P of the PFET 102P but not on the ESL 120N of the NFET 102N. Forming the stress liner 122 may include the following sequential operations: (i) Figure 5A and Figure 5B As shown, a semiconductor layer 522 having a thickness of T3 is deposited directly on ESL 120N and ESL 120P; (ii) as shown Figure 6B As shown, a mask layer 646 is formed on a portion of the semiconductor layer 522 in the PFET 102P; (iii) as shown Fig. 7A As shown, a portion of the semiconductor layer 522 is etched from the NFET 102N; (iv) as shown Figure 8B As shown, the mask layer 646 is removed from the PFET 102P; (v) a flowable dielectric layer 824 is deposited directly on the ESL 120N and the semiconductor layer 522, as shown in FIG. Fig. 8A and Figure 8B As shown; (vi) Fig. 8A and Figure 8B A thermal annealing process is performed on the structure to form a stress liner 122 and an ILD layer 124N and an ILD layer 124P. Fig. 9A and Fig. 9B as shown; and (vii) in Fig. 9A and Fig. 9B A chemical mechanical polishing (CMP) process is performed on the structure to make the top surfaces of the ESL 120P, the ESL 120N, the stress liner 122, the ILD layer 124P and the ILD layer 124N and the top surfaces of the polysilicon structure 312P and the polysilicon structure 312P substantially coplanar together, as shown in FIG. Fig. 10A and 10B shown.

[0046] In some embodiments, the semiconductor layer 522 may include an amorphous Si layer, an amorphous Ge layer, or a SiGe layer. In some embodiments, the semiconductor layer 522 may include a silicon germanium layer with a Ge atomic concentration of about 1 atomic % to about 50 atomic %. In some embodiments, one or more of silane (SiH4), disilane (Si2H6), germanium (GeH4), dichlorosilane (SiH2Cl2), or other suitable higher silanes (Si x H 2x+2 ) to deposit the semiconductor layer 522. In some embodiments, the semiconductor layer 522 may be deposited at a temperature of about 300° C. to about 600° C. and a pressure of about 0.1 torr to about 10 torr.

[0047] In some embodiments, the thermal annealing process may be performed at a temperature of about 400° C. to about 700° C. During the thermal annealing process, the flowable dielectric layer 824 may be densified to form the ILD layer 124N and the ILD layer 124P, as shown in FIG. Fig. 9A and Fig. 9B At the same time, oxygen atoms from the flowable dielectric layer 824 may oxidize the semiconductor layer 522 during the thermal annealing process to form the stress liner 122, as shown in FIG. Fig. 9BAs shown. Due to the oxidation of the semiconductor layer 522, the volume of the semiconductor layer 522 may expand. As a result, the stress liner 122 may have a thickness T1 that is greater than the thickness T3 of the semiconductor layer 522. In addition, because of the volume expansion, the stress liner 122 may apply longitudinal and lateral pressure to the polysilicon structure 312P of the PFET 102P. The longitudinal and lateral pressure on the polysilicon structure 312P may be transmitted as a longitudinal compressive stress in the nanostructure channel region 110P.

[0048] Reference Figure 2 In operation 225, the polysilicon structure and the sacrificial layer of the superlattice structure are replaced with the gate structure. Fig.11A and Fig. 11B As described above, the polysilicon structures 312N and 312P and the sacrificial layers 311N and 311P are replaced with the gate structures 112N and 112P. The formation of the gate structures 112N and 112P may include: Fig. 10A and Fig. 10B The polysilicon structure 312N and the polysilicon structure 312P and the sacrificial layer 311N and the sacrificial layer 311P are removed from the structure to form a gate opening (not shown), and the gate structure 112N and the gate structure 112P are formed in the gate opening, as shown in FIG. Fig.11A and Fig. 11B In some embodiments, the gate structure 112N and the gate structure 112P may be formed after the S / D contact structure 138N and the S / D contact structure 138P are formed. Figure 1D and Figure 1E shown.

[0049] In some embodiments, operations similar to operations 205 to 225 of method 200 may be used to manufacture Figure 1F and Figure 1G finFET, except that (i) fin structures 107N and 107P are formed on fin substrates 106N and 106P in operation 205 instead of superlattice structures 309N and 309P; (ii) S / D regions 108N and 108P are formed in fin structures 107N and 107P in operation 210 instead of superlattice structures 309N and 309P; and (ii) sacrificial layers 311N and 311P are not provided and are not replaced with gate structures 112N and 112P in operation 225.

[0050] The present disclosure provides an example structure of a PFET (e.g., PFET 102P) having a stress liner (e.g., stress liner 122) to enhance hole mobility in a channel region (e.g., nanostructure channel region 110P) between adjacent S / D regions (e.g., S / D region 108). By using a stress liner, longitudinal compressive stress in the channel region can be increased, which can increase the mobility of holes flowing in the channel region. Increasing hole mobility in the channel region can improve device performance.

[0051] In some embodiments, the PFET may include a channel region of a nanostructure, a gate structure (e.g., gate structure 112P) surrounding the channel region of the nanostructure, and an S / D region on either side of the channel region of the nanostructure. The PFET may also include an ESL (e.g., ESL 120P), a stress liner, and an ILD layer (e.g., ILD layer 124P). In some embodiments, the ESL may be disposed on the S / D region and disposed along the sidewall of the gate structure. In some embodiments, the stress liner may be disposed on the ESL, and the ILD layer may be disposed on the stress liner. The stress liner applies pressure to the gate structure, which is transmitted as a longitudinal compressive stress in the channel region of the nanostructure. In some embodiments, the stress liner may include a semiconductor material of silicon oxide, silicon germanium oxide, germanium oxide, or other suitable oxides.

[0052] In some embodiments, a semiconductor device includes a substrate, a nanostructure channel region disposed on the substrate, a gate structure surrounding the nanostructure channel region, an S / D region disposed adjacent to the nanostructure channel region, an ESL disposed on the S / D region, a stress liner disposed on the etch stop layer and configured to provide compressive stress in the nanostructure channel region, an ILD layer disposed on the stress liner, and contact structures disposed in the S / D region, the ESL, the stress liner, and the ILD layer.

[0053] In some embodiments, a semiconductor device includes a substrate, a fin structure disposed on the substrate, a gate structure disposed on the fin structure, an S / D region disposed adjacent to the fin structure, and a dielectric layer stack disposed on the S / D region. The dielectric layer stack includes a first dielectric layer disposed on the S / D region, a second dielectric layer disposed on the first dielectric layer and configured to provide compressive stress in the fin region of the fin structure, and a third dielectric layer disposed on the second dielectric layer. The materials of the first dielectric layer, the second dielectric layer, and the third dielectric layer are different from each other.

[0054] In some embodiments, a method includes: forming a first nanosheet stack and a second nanosheet stack on a substrate; forming a first polysilicon structure and a second polysilicon structure on the first nanosheet stack and the second nanosheet stack, respectively; forming a first S / D region adjacent to the first nanosheet stack and a second S / D region adjacent to the second nanosheet stack; depositing a semiconductor layer on the first polysilicon structure and the second polysilicon structure and on the first S / D region and the second S / D region; performing a thermal annealing process on the dielectric layer and the semiconductor layer; and replacing the first polysilicon structure and the sacrificial layer in the first nanosheet stack with a first gate structure, and replacing the second polysilicon structure and the sacrificial layer in the second nanosheet stack with a second gate structure.

[0055] The foregoing disclosure summarizes the features of several embodiments so that those skilled in the art can better understand the various aspects of the present disclosure. It should be appreciated by those skilled in the art that they can easily use the present disclosure as a basis for designing or modifying other processes and structures for performing the same purpose and / or achieving the same advantages of the embodiments described herein. It should also be appreciated by those skilled in the art that these equivalent constructions do not depart from the spirit and scope of the present disclosure, and that they can make various changes, substitutions and modifications without departing from the spirit and scope of the present disclosure.

[0056] Example

[0057] Example 1. A semiconductor device, comprising: a substrate; a nanostructure channel region disposed on the substrate; a gate structure surrounding the nanostructure channel region; a source / drain (S / D) region disposed adjacent to the nanostructure channel region; an etch stop layer (ESL) disposed on the S / D region; a stress liner disposed on the etch stop layer and configured to provide compressive stress in the nanostructure channel region; an interlayer dielectric (ILD) layer disposed on the stress liner; and a contact structure disposed in the S / D region, the ESL, the stress liner, and the ILD layer.

[0058] Example 2. The semiconductor device of Example 1, wherein the stress liner comprises an oxide of the semiconductor layer.

[0059] Example 3. The semiconductor device of Example 1, wherein the stress liner comprises a silicon oxide layer, a germanium oxide layer, or a silicon germanium oxide layer.

[0060] Example 4. The semiconductor device of Example 1, wherein the stress liner comprises germanium atoms at a concentration of about 1 atomic % to about 50 atomic %.

[0061] Example 5. The semiconductor device of Example 1, wherein the stress liner comprises carbon, nitrogen, or fluorine atoms at a concentration of about 0.1 atomic % to about 5 atomic %.

[0062] Example 6. A semiconductor device according to Example 1, wherein the stress liner includes: a first liner portion, which contacts the ESL and includes a first concentration of oxygen atoms; and a second liner portion, which contacts the ILD layer and includes a second concentration of oxygen atoms, the second concentration of oxygen atoms being higher than the first concentration of oxygen atoms.

[0063] Example 7. A semiconductor device according to Example 1, wherein the stress liner includes: a first liner portion, which is in contact with the ESL and includes a first concentration of silicon or germanium atoms; and a second liner portion, which is in contact with the ILD layer and includes a second concentration of silicon or germanium atoms, the second concentration of silicon or germanium atoms being lower than the first concentration of silicon or germanium atoms.

[0064] Example 8. The semiconductor device of Example 1, wherein the stress liner comprises: a first liner portion comprising an oxygen-free silicon, germanium, or silicon germanium layer; and a second liner portion comprising a silicon oxide layer, a germanium oxide layer, or a silicon germanium oxide layer.

[0065] Example 9. A semiconductor device according to Example 1, wherein the stress liner includes: a first liner portion, including a first concentration of silicon or germanium atoms, the first concentration of silicon or germanium atoms being higher than a first concentration of oxygen atoms; and a second liner portion, including a second concentration of silicon or germanium atoms, the second concentration of silicon or germanium atoms being lower than a second concentration of oxygen atoms.

[0066] Example 10. The semiconductor device of Example 1, wherein a bottom surface of the stress liner is disposed at a distance of about 15 nm to about 25 nm above a top surface of the nanostructure channel region.

[0067] Example 11. A semiconductor device, comprising: a substrate; a fin structure disposed on the substrate; a gate structure disposed on the fin structure; a source / drain (S / D) region disposed adjacent to the fin structure; and a dielectric layer stack disposed on the S / D region, comprising: a first dielectric layer disposed on the S / D region; a second dielectric layer, disposed on the first dielectric layer and configured to provide compressive stress in the fin region of the fin structure; and a third dielectric layer disposed on the second dielectric layer, wherein the materials of the first dielectric layer, the second dielectric layer, and the third dielectric layer are different from each other.

[0068] Example 12. The semiconductor device of Example 11, wherein the first dielectric layer and the third dielectric layer include germanium-free oxide layers; and the second dielectric layer includes a germanium-based oxide layer.

[0069] Example 13. The semiconductor device of Example 11, wherein the second dielectric layer includes germanium atoms at a concentration of about 1 atomic % to about 50 atomic %.

[0070] Example 14. The semiconductor device of Example 11, wherein the second dielectric layer includes carbon, nitrogen, or fluorine atoms at a concentration of about 0.1 atomic % to about 5 atomic %.

[0071] Example 15. A semiconductor device according to Example 11, wherein the second dielectric layer includes: a first portion including a first concentration of oxygen atoms; and a second portion including a second concentration of oxygen atoms, the second concentration of oxygen atoms being higher than the first concentration of oxygen atoms.

[0072] Example 16. The semiconductor device of Example 11, wherein the second dielectric layer comprises a thickness of about 2 nm to about 10 nm.

[0073] Example 17. A method for forming a semiconductor device, comprising: forming a first nanosheet stack and a second nanosheet stack on a substrate; forming a first polysilicon structure and a second polysilicon structure on the first nanosheet stack and the second nanosheet stack, respectively; forming a first source / drain (S / D) region adjacent to the first nanosheet stack and a second source / drain (S / D) region adjacent to the second nanosheet stack; depositing a semiconductor layer on the first polysilicon structure and the second polysilicon structure and on the first S / D region and the second S / D region; depositing a dielectric layer on the semiconductor layer; performing a thermal annealing process on the dielectric layer and the semiconductor layer; and replacing the first polysilicon structure and the sacrificial layer in the first nanosheet stack with a first gate structure, and replacing the second polysilicon structure and the sacrificial layer in the second nanosheet stack with a second gate structure.

[0074] Example 18. The method of Example 17, wherein depositing the semiconductor layer comprises depositing an amorphous silicon layer, an amorphous germanium layer, or a silicon germanium layer.

[0075] Example 19. The method of Example 17, further comprising removing a portion of the semiconductor layer from the first polysilicon layer and the first S / D region.

[0076] Example 20. The method of Example 17 further includes: before depositing the semiconductor layer, depositing an etch stop layer on the first polysilicon structure and the second polysilicon structure and on the first S / D region and the second S / D region.

Claims

1. A semiconductor device, comprising: substrate; A nanostructured channel region is disposed on the substrate; a gate structure surrounding the nanostructure channel region; a source / drain (S / D) region disposed adjacent to the nanostructure channel region; an etch stop layer (ESL) disposed on the S / D region; a stress liner disposed on the etch stop layer and configured to provide a compressive stress in the nanostructure channel region; an interlayer dielectric (ILD) layer disposed on the stressed liner; as well as A contact structure is disposed in the S / D region, the ESL, the stress liner and the ILD layer.

2. The semiconductor device according to claim 1, wherein The stressed liner includes an oxide of the semiconductor layer.

3. The semiconductor device according to claim 1, wherein The stress liner includes a silicon oxide layer, a germanium oxide layer or a silicon germanium oxide layer.

4. The semiconductor device according to claim 1, wherein: The stress liner includes germanium atoms at a concentration of about 1 atomic % to about 50 atomic %.

5. The semiconductor device according to claim 1, wherein The stress liner includes carbon, nitrogen, or fluorine atoms at a concentration of about 0.1 atomic % to about 5 atomic %.

6. The semiconductor device according to claim 1, wherein The stress liner comprises: a first liner portion in contact with the ESL and comprising a first concentration of oxygen atoms; and A second liner portion contacts the ILD layer and includes a second concentration of oxygen atoms, the second concentration of oxygen atoms being higher than the first concentration of oxygen atoms.

7. The semiconductor device according to claim 1, wherein The stress liner comprises: a first liner portion contacting the ESL and comprising a first concentration of silicon or germanium atoms; and A second liner portion contacts the ILD layer and includes a second concentration of silicon or germanium atoms, the second concentration of silicon or germanium atoms being lower than the first concentration of silicon or germanium atoms.

8. The semiconductor device according to claim 1, wherein The stress liner comprises: a first liner portion including an oxygen-free silicon, germanium, or silicon germanium layer; and The second liner portion includes a silicon oxide layer, a germanium oxide layer or a silicon germanium oxide layer.

9. A semiconductor device comprising: substrate; A fin structure is disposed on the substrate; A gate structure, disposed on the fin structure; a source / drain (S / D) region disposed adjacent to the fin structure; as well as A dielectric layer stack disposed on the S / D region, the dielectric layer stack comprising: A first dielectric layer, disposed on the S / D region; a second dielectric layer disposed on the first dielectric layer and configured to provide compressive stress in a fin region of the fin structure; and A third dielectric layer is disposed on the second dielectric layer, wherein materials of the first dielectric layer, the second dielectric layer and the third dielectric layer are different from each other.

10. A method for forming a semiconductor device, comprising: forming a first nanosheet stack and a second nanosheet stack on a substrate; forming a first polysilicon structure and a second polysilicon structure on the first nanosheet stack and the second nanosheet stack, respectively; forming a first source / drain (S / D) region adjacent to the first nanosheet stack and a second source / drain (S / D) region adjacent to the second nanosheet stack; depositing a semiconductor layer on the first polysilicon structure and the second polysilicon structure and on the first S / D region and the second S / D region; depositing a dielectric layer on the semiconductor layer; performing a thermal annealing process on the dielectric layer and the semiconductor layer; as well as The first polysilicon structure and the sacrificial layer in the first nanosheet stack are replaced with a first gate structure, and the second polysilicon structure and the sacrificial layer in the second nanosheet stack are replaced with a second gate structure.