Electrochemical device and electric equipment comprising same
By using multiple spaced isolation films and insulating layers in the electrochemical device, the internal short circuit and electrolyte infiltration problems of the electrochemical device under abnormal conditions are solved, and its circulation performance and safety are improved.
Patent Information
- Application Number
- CN202380034178.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2023-06-12
- Publication Date
- 2024-11-19
- Estimated Expiration
- 2043-06-12
AI Technical Summary
Electrochemical devices may catch fire when subjected to abnormal conditions such as extrusion, collision or puncture, and there is a risk of internal short circuit, which affects its cycling performance and safety.
Using an electrochemical device design with a first isolation film and a first insulation layer arranged at a plurality of intervals, the electrode assembly is bound in the first direction by the first insulation layer, and the risk of internal short circuit caused by the shrinkage of the isolation film is reduced, and the plurality of The first coating and the second coating arranged at intervals increase the electrolyte transmission space, improve the electrolyte infiltration effect, and enhance the resistance to deformation of the electrode assembly.
It effectively reduces the risk of internal short circuit and poor electrolyte infiltration problems, improves the circulation and safety performance of electrochemical devices, and extends its service life.
Smart Images

Figure CN118985059A_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the field of energy storage devices, and in particular to an electrochemical device and an electrical device comprising the same. Background Art
[0002] Electrochemical devices (such as lithium-ion batteries) are widely used in electric vehicles and consumer electronics due to their high energy density, high output power, long cycle life and low environmental pollution. However, electrochemical devices may catch fire or have safety issues when subjected to abnormal conditions such as squeezing, collision or puncture. Summary of the invention
[0003] One object of the present application is to provide a battery having good cycle performance and reducing the risk of internal short circuit in an electrochemical device.
[0004] The present application provides an electrochemical device, comprising a housing, an electrode assembly, a first insulating layer and an electrolyte, wherein the electrode assembly and the electrolyte are contained in the housing. The electrode assembly comprises a plurality of pole pieces stacked along a first direction and a first isolation membrane disposed between the plurality of pole pieces. The electrode assembly also comprises a first surface and a second surface opposite to each other in the first direction and a first end face connected between the first surface and the second surface. The first insulating layer is bonded to the first surface, the second surface and the first end face. The first isolation membrane comprises a substrate layer and a first coating disposed at intervals on the surface of the substrate layer facing adjacent pole pieces.
[0005] The present application sets a first insulating layer connecting the first surface, the second surface and the first end face of the electrode assembly. The first insulating layer constrains the electrode assembly in the first direction, reduces the risk of internal short circuit caused by the shrinkage of the first isolation membrane, and improves safety performance. However, the use of the first insulating layer to constrain the electrode assembly in the first direction may reduce the gap between the first isolation membrane and the adjacent pole piece, thereby reducing the space available for electrolyte transmission and causing poor electrolyte infiltration. The present application sets the first isolation membrane to include a plurality of first coatings arranged at intervals. The gap between two adjacent first coatings reserves space for electrolyte transmission, improves the electrolyte infiltration effect, improves the problem of lithium plating on the pole piece caused by poor electrolyte infiltration, and improves the cycle performance. Therefore, the electrochemical device of the present application has high cyclability while maintaining safety.
[0006] In some possible implementations, the first coating is in a strip shape, the substrate layer includes two sides opposite to each other in a second direction perpendicular to the first direction, and the first coatings are arranged obliquely relative to the sides. Therefore, the bonding force between the first coating and the adjacent electrode sheets is continuously distributed on each edge of the electrode assembly, thereby improving the ability of the electrode assembly to resist deformation and improving the cycle performance.
[0007] In some possible implementations, when viewed along the first direction, the angle between the first coating and the side edge is θ1, 25°≤θ1≤65°. When the angle θ1 is within this range, the adhesion between the first coating and the edge of the pole piece can be maintained, and the edge deformation of the pole piece can be suppressed, thereby improving the cycle performance.
[0008] In some possible implementations, when observed along the first direction, the width of the first coating is D1, the spacing between two adjacent first coatings is D2, and 0.3D2≤D1≤0.5D2. When D1>0.5D2, under the condition of a certain electrode area, D2 is small, which reduces the space available for electrolyte transmission, and poor electrolyte infiltration worsens the problem of lithium precipitation in the electrode, affecting the cycle performance; when D1<0.3D2, the bonding area between the first coating and the electrode is reduced, the bonding force is reduced, and the anti-deformation ability is correspondingly reduced, affecting the cycle performance.
[0009] In some possible implementations, the first isolation film further includes a plurality of second coatings, which are spaced apart on the surface of the substrate layer away from the plurality of first coatings. The gap between two adjacent second coatings is reserved for electrolyte transmission, thereby improving the electrolyte infiltration effect, further improving the problem of lithium deposition on the pole piece caused by poor electrolyte infiltration, and improving the cycle performance.
[0010] In some possible implementations, the first coating and the second coating intersect at different surfaces, so that the gaps between two adjacent first coatings and the gaps between two adjacent second coatings are staggered, further improving the electrolyte infiltration effect, further improving the problem of lithium plating on the electrode caused by poor electrolyte infiltration, and improving the cycle performance.
[0011] In some possible implementations, the first isolation membrane also includes a plurality of first portions located in the plurality of pole pieces and a second portion and a third portion located outside the plurality of pole pieces and opposite to each other in a first direction, each first portion being arranged between two adjacent pole pieces, and the plurality of first portions, second portions and third portions being arranged as a whole and forming a winding structure. The first isolation membrane is configured as a winding structure, which restrains the plurality of pole pieces in a plurality of different directions, without the need to configure an additional insulating layer to restrain the plurality of pole pieces in a specific direction. Furthermore, the first insulating layer is connected to the second portion and the third portion of the first isolation membrane, thereby increasing the bonding force between the first insulating layer and the electrode assembly, reducing the risk of the first insulating layer falling off, and thereby reducing the risk of internal short circuit caused by shrinkage of the first isolation membrane.
[0012] In some possible implementations, in a third direction perpendicular to both the first direction and the second direction, the width of the electrode assembly is W1, the width of the first insulating layer is W2, and 0.7W1≤W2≤W1. When the width W1 of the electrode assembly and the width W2 of the first insulating layer are within this range, the adhesion between the first insulating layer and the first end surface can be maintained, reducing the risk of internal short circuit caused by shrinkage of the first isolation film, and improving safety performance.
[0013] In some possible implementations, 0.7W1≤W2≤0.95W1. In some possible implementations, 0.85W1≤W2≤0.95W1.
[0014] In some possible implementations, the first coating layer includes a first inorganic particle layer and a first bonding layer, the first inorganic particle layer is connected to the substrate layer, and the bonding layer is arranged on the surface of the inorganic particle layer away from the substrate layer and is bonded to the adjacent pole piece. The first bonding layer is bonded to the pole piece to improve the interfacial bonding force between the first isolation film and the pole piece, reduce the expansion deformation when the electrochemical device produces gas, and improve the cycle performance.
[0015] In some possible implementations, the first coating layer includes inorganic particles and a binder.
[0016] In some possible implementations, the electrochemical device further includes a second insulating layer, the electrode assembly further includes a second end face connected between the first surface and the second surface, the length direction of the electrode assembly is defined as the second direction, the first surface and the second surface are opposite in the second direction, and the second insulating layer is connected to the first surface, the second surface, and the second end face. The second insulating layer connecting the first surface, the second surface, and the second end face of the electrode assembly is provided to reduce the risk of internal short circuit caused by shrinkage of one end of the first isolation membrane close to the second end face.
[0017] In some possible implementations, the first insulating layer is single-sided tape or double-sided tape.
[0018] In some possible implementations, the second insulating layer is single-sided tape or double-sided tape.
[0019] In some possible implementations, the electrochemical device also includes a first metal plate and a second metal plate, both of which are connected to the electrode assembly; in a third direction perpendicular to the first direction, the electrode assembly also includes a second end face opposite to the first end face, and the first metal plate and the second metal plate extend out of the electrode assembly from the second end face.
[0020] In some possible implementations, the shell is a packaging bag.
[0021] The present application also provides an electrical equipment, comprising any of the above-mentioned electrochemical devices. BRIEF DESCRIPTION OF THE DRAWINGS
[0022] The above and / or additional aspects and advantages of the present application will become apparent and easily understood from the description of the embodiments in conjunction with the following drawings, in which: Figure 1 A first direction view of an electrochemical device provided in one embodiment of the present application; Figure 2 for Figure 1 The electrode assembly of the electrochemical device shown is a first direction view observed from the side where the first surface is located; Figure 3 for Figure 2 The electrode assembly shown is a first direction view observed from the side where the second surface is located; Figure 4 for Figure 2 A second directional view of the electrode assembly shown; Figure 5 for Figure 2 A cross-sectional view of the electrode assembly along VV is shown; Figure 6 for Figure 4 A cross-sectional view of the electrode assembly shown along VI-VI; Figure 7 for Figure 6 The first isolation film of the electrode assembly is shown in a first direction view from a side close to the first surface of the electrode assembly; Figure 8 for Figure 7 The first isolation film is shown as a first direction view from the side close to the second surface of the electrode assembly; Fig. 9 A first direction view of a first isolation film provided by another embodiment of the present application; Fig.10 A second direction view of an electrode assembly provided in another embodiment of the present application; Fig.11 A second direction view of an electrode assembly provided in yet another embodiment of the present application; Fig.12 A schematic diagram of the structure of an electrical device provided in one embodiment of the present application.
[0023] Main component symbols Electrochemical device 100 Housing 10 Electrode assembly 20 First metal plate 30 Second metal plate 40 First isolation film 23 The first pole piece 21 The second pole piece 22 First current collector 211 First active material layer 212 Second fluid collector 221 Second active material layer 222 First surface 201 Second surface 202 Second end surface 203 First end surface 204 First side 205 Second side 206 The first insulating layer 50 Fourth insulating layer 60 The third insulating layer 70 The second insulating layer 80 Base material layer 231 First coating 232 Gap G1, G2, G3 First inorganic particle layer 232a First adhesive layer 232b Side 231a Second coating 233 Second inorganic particle layer 233a Second adhesive layer 233b Part 23b Part III 23c Second isolation film 24 Electrical equipment 1 First direction Z Second direction Y The third direction X. DETAILED DESCRIPTION
[0024] The technical scheme in the embodiment of the present application is described clearly and in detail below. Obviously, the described embodiment is a part of the embodiment of the present application, rather than all the embodiments. Unless otherwise defined, all technical and scientific terms used herein have the same meaning as those generally understood by those skilled in the art of the present application. The terms used in the specification of the present application are only for the purpose of describing specific embodiments and are not intended to limit the present application.
[0025] Hereinafter, the embodiments of the present application will be described in detail. However, the present application can be embodied in many different forms and should not be construed as being limited to the exemplary embodiments illustrated herein. Rather, these exemplary embodiments are provided so that the present application is thoroughly and in detail communicated to those skilled in the art.
[0026] In addition, for simplicity and clarity, in the accompanying drawings, the size or thickness of various components, layers may be amplified. Throughout the entire text, the same numerical value refers to the same element. In addition, it should be understood that when element A is referred to as "connecting" element B, element A may be directly connected to element B, or there may be an intermediate element C and element A and element B may be indirectly connected to each other.
[0027] Further, the use of “may” when describing embodiments of the present application means “one or more embodiments of the present application”. The professional terms used herein are for the purpose of describing specific embodiments and are not intended to limit the application. As used herein, the singular form is intended to also include the plural form, unless the context clearly indicates otherwise. It should be understood that the term "comprising", when used in this specification, refers to the existence of narrated features, numerical values, steps, operations, elements and / or components, but does not exclude the existence or increase of one or more other features, numerical values, steps, operations, elements, components and / or combinations thereof. It should be understood that although the terms first, second, third, etc. can be used to describe various elements, components, regions, layers and / or parts herein, these elements, components, regions, layers and / or parts should not be limited by these terms. These terms are used to distinguish an element, component, region, layer or part from another element, component, region, layer or part. Therefore, the first element, component, region, layer or part discussed below can be referred to as the second element, component, region, layer or part, without departing from the teaching of exemplary embodiments.
[0028] The term "plurality" in this application refers to two or more.
[0029] In the present application, an electrochemical device includes any device that generates an electrochemical reaction, and its specific examples include all kinds of primary batteries, secondary batteries, fuel cells, solar cells or capacitors. Exemplarily, the electrochemical device is a lithium secondary battery, which may include a lithium metal secondary battery, a lithium ion secondary battery, a lithium polymer secondary battery or a lithium ion polymer secondary battery.
[0030] See also Figure 1 In one embodiment of the present application, an electrochemical device 100 is provided, comprising a housing 10, an electrode assembly 20 (in Figure 2 , Figure 3 ) and electrolyte, a first metal plate 30 and a second metal plate 40. In some embodiments, the housing 10 is a metal housing, such as a steel housing or an aluminum housing. In other embodiments, the housing 10 is a packaging bag obtained by packaging with a packaging film, that is, the electrochemical device 100 can be a soft pack battery. Figure 2 and Figure 3The electrochemical device 100 is shown to include one electrode assembly 20. In other embodiments, the electrochemical device 100 includes a plurality of electrode assemblies 20 in order to achieve a high voltage output.
[0031] like Figure 4 As shown, the electrode assembly 20 includes a plurality of pole pieces and a first isolation film 23 disposed between the plurality of pole pieces. The plurality of pole pieces are stacked along a first direction Z to form a laminate structure. In this embodiment, the first direction Z refers to the thickness direction of the electrode assembly 20. The plurality of pole pieces include a first pole piece 21 and a second pole piece 22 with opposite polarities. The first isolation film 23 is disposed between adjacent first pole pieces 21 and second pole pieces 22 to reduce the risk of short circuit caused by direct contact between the first pole piece 21 and the second pole piece 22.
[0032] The first metal plate 30 and the second metal plate 40 are electrically connected to the electrode assembly 20, respectively, and extend from the housing 10 to connect to external elements (not shown). Specifically, the first pole piece 21 includes a first current collector 211 and a first active material layer 212, the first active material layer 212 is disposed on at least one surface of the first current collector 211, and the first metal plate 30 is electrically connected to the first current collector 211. The second pole piece 22 includes a second current collector 221 and a second active material layer 222, the second active material layer 222 is disposed on at least one surface of the second current collector 221, and the second metal plate 40 is electrically connected to the second current collector 221.
[0033] In some embodiments, the first pole piece 21 is a positive pole piece, and the second pole piece 22 is a negative pole piece. Specifically, the first current collector 211 includes at least one of Ni, Ti, Cu, Ag, Au, Pt, Fe, Al and their combinations, and the first active material layer 212 includes a positive active material, which may include lithium cobaltate, lithium manganate, lithium nickelate, lithium nickel cobalt manganate, lithium iron phosphate, lithium manganese iron phosphate, lithium vanadium phosphate, lithium vanadium phosphate, lithium rich manganese-based materials, lithium nickel cobalt aluminum oxide and their combinations. The second current collector 221 includes at least one of Ni, Ti, Cu, Ag, Au, Pt, Fe, Al and their combinations. The second active material layer 222 includes a negative active material, which may be selected from at least one of graphite materials, alloy materials, lithium metal and their alloys. The graphite material may be selected from at least one of artificial graphite and natural graphite; the alloy material may be selected from at least one of silicon, silicon oxide, tin and titanium sulfide.
[0034] See also Figures 2 to 4The electrode assembly 20 further includes a first surface 201, a second surface 202, a second end surface 203, a first end surface 204, a first side surface 205, and a second side surface 206. The first surface 201 and the second surface 202 are opposite in the first direction Z. In the first direction Z, the surfaces of the two outermost pole pieces among the plurality of pole pieces are respectively used as the first surface 201 and the second surface 202. In some embodiments, the surfaces of the current collectors of the two outermost pole pieces among the plurality of pole pieces are used as the first surface 201 and the second surface 202. The second end surface 203 and the first end surface 204 are opposite in the second direction Y and are connected between the first surface 201 and the second surface 202. The first metal plate 30 and the second metal plate 40 extend from the second end surface 203. The first metal plate 30 and the second metal plate 40 can extend directly from the housing 10, or can be connected to another metal plate, which extends from the housing 10. The first side surface 205 and the second side surface 206 are opposite in the third direction X and are connected between the first surface 201 and the second surface 202. In the present application, the third direction X refers to the width direction of the electrode assembly 20, and the second direction Y refers to the length direction of the electrode assembly 20, wherein the second direction Y is also the direction in which the first metal plate 30 and the second metal plate 40 extend, and the first direction Z, the third direction X and the second direction Y are perpendicular to each other.
[0035] The first isolation film 23 includes at least one first portion 23a disposed in a plurality of pole pieces. In some embodiments, the first isolation film 23 includes a plurality of first portions 23a, each of which is used to separate adjacent first pole pieces 21 and second pole pieces 22. The plurality of first portions 23a are disposed separately, that is, the plurality of first portions 23a are configured as independent diaphragms. At this time, the electrode assembly 20 is obtained by alternately stacking the first pole piece 21, the first portion 23a, and the second pole piece 22. The edge of the first portion 23a of the first isolation film 23 exceeds the edge of the pole piece in both the third direction X and the second direction Y to separate the adjacent first pole piece 21 and the second pole piece 22. Among them, the end faces of the first portion 23a of the first isolation film 23 on both sides of the second direction Y are respectively used as the second end face 203 and the first end face 204, and the end faces of the first portion 23a of the first isolation film 23 on both sides of the third direction X are respectively used as the first side face 205 and the second side face 206.
[0036] See also Figure 2 , Figure 3 and Figure 5 The electrochemical device 100 further includes a first insulating layer 50. The first insulating layer 50 is generally in the form of a sheet, which covers at least a portion of the first surface 201, at least a portion of the second surface 202, and at least a portion of the first end surface 204, and is bonded to the first surface 201, the second surface 202, and the first end surface 204. Figure 5In the embodiment, the first insulating layer 50 is connected to the surfaces of the current collectors of the two pole pieces used as the first surface 201 and the second surface 202. The first insulating layer 50 constrains the electrode assembly 20 in the first direction Z and the second direction Y, reducing the risk of the first portion 23a of the first isolation film 23 near the first end face 204 shrinking in the second direction Y during thermal and mechanical abuse, resulting in a short circuit between the first pole piece 21 and the second pole piece 22, and can also reduce the stress on the first end face 204 during a fall, reducing the risk of pole piece damage.
[0037] See also Figure 2 and Figure 3 , define the width of the electrode assembly 20 in the third direction X as W1, define the width of the first insulating layer 50 in the third direction X as W2, where 0.7W1≤W2≤W1. In the case of W2<0.7W1, the width of the first insulating layer 50 is small, and the connection area between the first insulating layer 50 and the first end face 204 is small, that is, the connection area between the first insulating layer 50 and the first isolation film 23 is small, so the first isolation film 23 is prone to shrinkage during the hot box and drop process, resulting in an internal short circuit. In some embodiments, W2≤0.95W1, which is used to balance the tolerance of setting the first insulating layer 50 during the manufacturing process and improve the electrolyte infiltration effect of the first end face 204.
[0038] See also Figures 2 to 4 In some embodiments, the electrochemical device 100 further includes a fourth insulating layer 60 and a third insulating layer 70. The fourth insulating layer 60 is generally in the form of a sheet, and covers at least a portion of the first surface 201, at least a portion of the second surface 202, and at least a portion of the first side surface 205, and is connected to the first surface 201, the second surface 202, and the first side surface 205. The fourth insulating layer 60 constrains the electrode assembly 20 in the first direction Z and the third direction X, and reduces the risk of shrinking the end of the first portion 23a of the first isolation film 23 close to the first side surface 205 in the third direction X. The third insulating layer 70 is generally in the form of a sheet, and covers at least a portion of the first surface 201, at least a portion of the second surface 202, and at least a portion of the second side surface 206, and is connected to the first surface 201, the second surface 202, and the second side surface 206. The third insulating layer 70 constrains the electrode assembly 20 in the first direction Z and the third direction X, and reduces the risk of shrinking the end of the first portion 23a of the first isolation film 23 close to the second side surface 206 in the third direction X.
[0039] See also Figure 2 , Figure 3 and Figure 5In some embodiments, the electrochemical device 100 further includes a second insulating layer 80. The second insulating layer 80 is generally in the form of a sheet, which covers at least a portion of the first surface 201, at least a portion of the second surface 202, and a portion of the second end surface 203, and is connected to the first surface 201, the second surface 202, and the second end surface 203. The second insulating layer 80 constrains the electrode assembly 20 in the first direction Z and the second direction Y, reducing the risk of shrinkage in the second direction Y at one end of the first portion 23a of the first isolation film 23 close to the second end surface 203. In this embodiment, the electrochemical device 100 includes three second insulating layers 80, wherein one second insulating layer 80 is disposed between the first metal plate 30 and the second metal plate 40, one second insulating layer 80 is disposed between the first metal plate 30 and the first side surface 205, and one second insulating layer 80 is disposed between the second metal plate 40 and the second side surface 206. This increases the connection area between the second insulating layer 80 and the second end surface 203, maintains the adhesion between the second insulating layer 80 and the second end surface 203, and further reduces the risk of shrinkage of the first portion 23a of the first isolation membrane 23 close to the second end surface 203.
[0040] In some embodiments, the first insulating layer 50, the fourth insulating layer 60, the third insulating layer 70 and the second insulating layer 80 are all adhesive and bonded to the electrode assembly 20. The materials of the first insulating layer 50, the fourth insulating layer 60, the third insulating layer 70 and the second insulating layer 80 can be single-sided adhesive or double-sided adhesive.
[0041] See also Figure 6 , the first isolation membrane 23 has a laminated membrane structure. Specifically, the first isolation membrane includes a substrate layer 231 and a plurality of first coatings 232 spaced apart on a surface of the substrate layer 231, and the first coating 232 bonds the first pole piece 21. In another embodiment, the first coating 232 may also bond the second pole piece 22. There is a gap G1 between two adjacent first coatings 232. The gap G1 between the plurality of first coatings 232 is a reserved space for electrolyte transmission, and after injection, the electrolyte can flow through the gap G1 and fully infiltrate the pole piece. In this case, even if the first insulating layer 50 is provided to constrain the electrode assembly 20 in the first direction Z and the second direction Y, the electrolyte can still infiltrate the pole piece through the gap G1.
[0042] In one embodiment, the first coating 232 includes a first inorganic particle layer 232a and a first bonding layer 232b which are stacked. The first inorganic particle layer 232a is connected to the substrate layer 231, and the first bonding layer 232b is arranged on the surface of the first inorganic particle layer 232a away from the substrate layer 231, and the first isolation film 23 is bonded to the adjacent pole piece through the first bonding layer 232b. The first bonding layer 232b can bond the pole piece, improve the interfacial bonding force between the first isolation film 23 and the pole piece, reduce the expansion deformation when the electrochemical device 100 produces gas, that is, improve the anti-deformation ability of the electrochemical device 100, reduce the risk of deformation and structural damage of the electrode assembly 20, and thus improve the cycle performance of the electrochemical device 100.
[0043] See also Figure 7 , the first coating 232 is arranged in strips on the surface of the substrate layer 231, and a plurality of first coatings 232 are arranged parallel to each other. The substrate layer 231 includes two side edges 231a opposite to each other in the second direction Y. The angle between the first coating 232 and the side edge 231a is θ1. The first coating 232 is arranged obliquely relative to the side edge 231a, that is, 0°<θ1<90°, so the bonding force between the first coating 232 and the pole piece is continuously distributed on the edge of the electrode assembly in the second direction Y and the third direction X, thereby improving the ability of the electrode assembly to resist deformation and improving the cycle performance. In some embodiments, 25°≤θ1≤65°, so as to maintain the bonding force between the first coating 232 and the edge of the pole piece, curb the edge deformation of the pole piece, and thus improve the cycle performance. In the case of θ1<25°, since the first coating 232 is relatively flush with the third direction X, the adhesion between the first isolation film 23 and the pole piece in the second direction Y may be reduced, resulting in the edge of the electrode assembly 20 in the third direction X may be deformed, affecting the cycle life. When θ1>65°, since the first coating 232 is relatively flush with the second direction Y, the adhesion between the first isolation film 23 and the electrode sheet in the third direction X may be reduced, causing the edge of the electrode assembly 20 in the second direction Y to deform, affecting the cycle life.
[0044] like Figure 7 As shown, in some embodiments, when observed along the first direction Z, the width of the first coating 232 is D1, and the distance between two adjacent first coatings 232 is D2, wherein D1 and D2 satisfy: 0.3D2≤D1≤0.5D2. When D1>0.5D2, under the condition of a certain pole piece area, D2 is small, so that the space available for electrolyte transmission is reduced, and poor electrolyte infiltration causes lithium precipitation problems in the pole piece, affecting the cycle performance. When D1<0.3D2, the bonding area between the first coating 232 and the pole piece is reduced, the bonding force is reduced, and the anti-deformation ability is correspondingly reduced, affecting the cycle performance.
[0045] like Figure 6As shown, in some embodiments, the first isolation film 23 also includes a plurality of second coatings 233 spaced apart on a surface of the substrate layer 231, and the substrate layer 231 is located between the first coating 232 and the second coating 233. When the first coating 232 is bonded to the first pole piece 21, the second coating 233 is bonded to the second pole piece 22. There is also a gap G2 between two adjacent second coatings 233, which serves as a channel for electrolyte transmission. Therefore, the provision of the second coating 233 further improves the wetting effect of the electrolyte, further reduces the problem of lithium precipitation of the pole piece caused by poor electrolyte wetting, and thus improves the cycle performance.
[0046] The second coating layer 233 includes a second inorganic particle layer 233a and a second adhesive layer 233b which are stacked. The second inorganic particle layer 233a is in contact with the substrate layer 231 , and the second adhesive layer 233b is disposed on the surface of the second inorganic particle layer 233a which is away from the substrate layer 231 .
[0047] In some embodiments, the substrate layer 231 includes a polymer film, a multilayer polymer film, or a non-woven fabric formed by any one of the following polymers or a mixture of two or more thereof: polyolefin, polyvinylidene fluoride, polyethylene terephthalate, cellulose, polyimide, polyamide, spandex, and polyphenylene phthalamide. Such polymers have high thermal stability and are easy to surface treat, so that the first coating 232 and the second coating 233 are easy to coat on the substrate layer 231. In addition, such polymers have good toughness and are easy to bend.
[0048] The first inorganic particle layer 232a and the second inorganic particle layer 233a both include inorganic particle materials, and the inorganic particle materials include at least one of boehmite, aluminum hydroxide or magnesium hydroxide particles. The first inorganic particle layer 232a and the second inorganic particle layer 233a may also include a binder, and the binder bonds the inorganic particle materials together. The binder may include a copolymer of polyvinylidene fluoride or vinylidene fluoride-hexafluoropropylene.
[0049] The first adhesive layer 232b and the second adhesive layer 233b both include adhesive materials, and the adhesive materials include at least one of the following polymers: copolymers of vinylidene fluoride and hexafluoropropylene, copolymers of vinylidene fluoride and trichloroethylene, polymethyl methacrylate, polyacrylic acid, polyacrylic acid salt, polyacrylonitrile, polyvinyl pyrrolidone, polyvinyl acetate, copolymers of ethylene-vinyl acetate, polyimide, polyethylene oxide, cellulose acetate, cellulose acetate butyrate, cellulose acetate propionate, cyanoethyl amylopectin, cyanoethyl polyvinyl alcohol, cyanoethyl cellulose, cyanoethyl sucrose, amylopectin, sodium carboxymethyl cellulose, lithium carboxymethyl cellulose, copolymers of acrylonitrile-styrene-butadiene, polyvinyl alcohol, polyvinyl ether, polytetrafluoroethylene, polyhexafluoropropylene, copolymers of styrene-butadiene or polyvinylidene fluoride. These polymers can produce a strong bonding effect to bond the first isolation membrane 23 and the first pole piece 21 or the second pole piece 22 together.
[0050] Please also read Figure 8 In some embodiments, the second coating 233 is arranged in a strip shape, and a plurality of second coatings 233 are arranged parallel to each other. The angle between the second coating 233 and the side 231a is θ2. The second coating 233 is arranged obliquely relative to the side 231a, that is, 0°<θ2<90°. In some embodiments, 25°≤θ2≤65°, so as to maintain the adhesion between the second coating 233 and the edge of the pole piece, further curb the edge deformation of the pole piece, thereby improving the cycle performance. In the case of θ2<25°, since the second coating 233 is relatively flush with the third direction X, the adhesion between the first isolation film 23 and the pole piece in the second direction Y may be reduced, resulting in the possible deformation of the edge of the electrode assembly 20 in the third direction X, affecting the cycle life. In the case of θ2>65°, since the second coating 233 is relatively flush with the second direction Y, the adhesion between the first isolation film 23 and the pole piece in the third direction X may be reduced, resulting in the possible deformation of the edge of the electrode assembly 20 in the second direction Y, affecting the cycle life.
[0051] like Figure 8 As shown, the first coating 232 and the second coating 233 intersect each other at different planes, and the angle between the first coating 232 and the second coating 233 is θ3, 0°<θ3<180°. In this way, the gaps G1 between the first coatings 232 and the gaps G2 between the second coatings 233 are staggered, further improving the electrolyte infiltration effect. Fig. 9 As shown, in another embodiment, the first coating 232 and the second coating 233 may also be arranged in parallel, and in this case, the angle θ1 between the first coating 232 and the side 231 a is equal to the angle θ2 between the second coating 233 and the side 231 a .
[0052] See also Fig. 9, each first coating layer 232 or each second coating layer 233 can be intermittently arranged, such as being arranged in a plurality of blocks or a plurality of islands on the surface of the substrate layer 231. At this time, the angle θ1 between the first coating layer 232 and the side 231a is the angle between the line connecting the plurality of block parts or the plurality of island parts and the side 231a, and the angle θ2 between the second coating layer 233 and the side 231a is the angle between the line connecting the plurality of block parts or the plurality of island parts and the side 231a. Among them, each intermittently arranged first coating layer 232 or each intermittently arranged second coating layer 233 is also provided with a gap G3, which can serve as a channel for electrolyte transmission, further improving the electrolyte transmission performance.
[0053] See also Fig.10 In another embodiment, the plurality of first portions 23a of the first isolation film 23 are configured as one body, that is, the first isolation film 23 is provided as one body. The first isolation film 23 has a Z-shaped folding structure. Specifically, in the first direction Z, the first isolation film 23 is bent in a Z-shape to form a Z-shaped folding structure. The first isolation film 23 having the Z-shaped folding structure includes only two end portions, which reduces the risk of internal short circuit caused by the contraction of the first isolation film 23, thereby improving safety performance.
[0054] See also Fig.11 In another embodiment, the first isolation film 23 further includes a second portion 23b and a third portion 23c located outside the plurality of pole pieces and opposite to each other in the first direction Z, wherein the surface of the second portion 23b facing away from the pole piece is connected to the first insulating layer as the first surface 201 of the electrode assembly 20, and the surface of the third portion 23c facing away from the pole piece is connected to the first insulating layer as the second surface 202 of the electrode assembly 20. The plurality of first portions 23a, the second portion 23b and the third portion 23c of the first isolation film 23 are configured as a whole and form a winding structure, in which the plurality of pole pieces are located. Specifically, the first isolation film 23 is wound around the second direction Y with one end thereof as the center to form a winding structure with every n pole pieces in sequence, wherein n is an integer greater than or equal to 1. That is, n pole pieces are provided between each two adjacent first portions 23a. Fig.11 3 pole pieces are provided between two adjacent first parts 23a. When n is greater than or equal to 2, a second isolation film 24 is also provided between the plurality of pole pieces between two adjacent first parts 23a. The second isolation film 24 is made of an insulating material and is used to prevent the plurality of pole pieces between two adjacent first parts 23a from directly contacting and short-circuiting. The material of the second isolation film 24 may include at least one of polyolefin, polyvinylidene fluoride, polyethylene terephthalate, cellulose, polyimide, polyamide, spandex or polyphenylene phthalate.
[0055] The first isolation film 23 provided as an integral body is configured as a winding structure, and the first isolation film 23 as a whole binds a plurality of pole pieces in the first direction Z and the third direction X, and there is no need to additionally configure the second insulating layer and the third insulating layer that bind the electrode assembly 20 in the first direction Z and the third direction X. Compared with the second insulating layer and the third insulating layer configured to bind the electrode assembly 20 in the first direction Z and the third direction X, the first isolation film 23 configured as a winding structure has a weaker binding on the edge of the pole piece in the third direction X, which is conducive to the electrolyte flowing through the edge of the pole piece in the third direction X and fully infiltrating the pole piece. Furthermore, the first isolation film 23 includes a second portion 23b and a third portion 23c located outside the plurality of pole pieces, and the first insulating layer 50 is connected to the second portion 23b and the third portion 23c of the first isolation film 23. The surface roughness of the first isolation film 23 is greater than the surface roughness of the current collector of the pole piece, which increases the bonding force between the first insulating layer 50 and the electrode assembly 20 and reduces the risk of the first insulating layer 50 falling off.
[0056] See also Fig.12 In one embodiment of the present application, there is also provided an electric device 1, which includes the electrochemical device 100 as described above. The electric device 1 of the present application can be, but is not limited to, a laptop computer, a pen-input computer, a mobile computer, an electronic book player, a portable phone, a portable fax machine, a portable copier, a portable printer, a head-mounted stereo headset, a video recorder, an LCD TV, a portable cleaner, a portable CD player, a mini disc, a transceiver, an electronic notepad, a calculator, a memory card, a portable recorder, a radio, a backup electronic source, a motor, a car, a motorcycle, a power bicycle, a bicycle, a lighting fixture, a toy, a game console, a clock, an electric tool, a flashlight, a camera, a large household battery and a lithium ion capacitor, etc.
[0057] The present application is described in detail below through specific embodiments and comparative examples. Among them, the present application is described by taking the electrochemical device as a soft-pack battery as an example and combining the specific preparation process and testing method. Those skilled in the art should understand that the preparation method described in the present application is only an example, and any other suitable preparation method is within the scope of the present application.
[0058] Example 1 The slurry formed by mixing the inorganic particle material and the binder is coated at intervals on the surface of the substrate layer to form a plurality of first inorganic particle layers spaced apart, and then the binder is coated on the surface of the plurality of first inorganic particle layers to form a plurality of first bonding layers to obtain a plurality of first coating layers spaced apart, and then the slurry formed by mixing the inorganic particle material and the binder is coated at intervals on the other surface of the substrate layer to form a plurality of second inorganic particle layers spaced apart, and then the binder is coated on the surface of the plurality of second inorganic particle layers to form a plurality of second bonding layers to obtain a plurality of second coating layers spaced apart, thereby obtaining a first isolation film. The relationship between the width D1 of the first coating layer and the distance D2 between two adjacent first coating layers is D1=0.3D2, and the angle θ1 between the first coating layer and the side of the substrate layer is 45° The first isolation film and a plurality of pole pieces are stacked to obtain an electrode assembly, wherein the first isolation film has a winding structure, three pole pieces are arranged between the first parts of two adjacent first isolation films, and the surfaces of the second part and the third part of the first isolation film away from the pole pieces serve as the first surface and the second surface of the electrode assembly. The first insulating layer is bonded to the first surface, the second surface and the second end face of the electrode assembly, wherein the relationship between the width W2 of the first insulating layer and the width W1 of the electrode assembly is: W2=0.8W1.
[0059] The electrode assembly and the electrolyte are packaged in an aluminum-plastic film to obtain an electrochemical device.
[0060] Example 2-13 The difference from the first embodiment is that at least one of the value of D1 / D2, the value of W2 / W1, and the value of the angle θ1 is different.
[0061] Comparative Example 1 The difference from Example 1 is that the slurry is continuously coated on the surface of the substrate layer to form the first inorganic particle layer and the second inorganic particle layer, and the slurry is continuously coated on the surface of the first inorganic particle layer and the surface of the second inorganic particle layer to form the first bonding layer. That is, the plurality of first coating layers and the plurality of second coating layers spaced apart in Example 1 are connected as one.
[0062] The electrochemical devices of Comparative Example 1 and Examples 1-10, 12-13 were subjected to cycle tests, and the test results are recorded in Table 1. The cycle test steps include: charging the electrochemical device to 4.43 V at a constant current of 1 C at 45 degrees Celsius, then charging to 0.05 C at a constant voltage, then standing for 5 minutes, and then discharging to 3.0V at 0.7 C. The discharge capacity at this time is measured by a commercially available battery performance tester as the first discharge capacity of the electrochemical device, which is calculated as 100%; the above charge and discharge steps are cycled for 1000 times in sequence, and the ratio of the discharge capacity of the electrochemical device after the cycle to the first capacity multiplied by 100% is the capacity retention rate; the electrochemical device is fully charged according to the charging process, and the negative electrode plate interface and lithium precipitation are disassembled to observe.
[0063] Table 1 Comparing Comparative Example 1 with Examples 1-10, 12-13, it can be seen that when a first insulating layer with a relatively wide width is used to constrain the electrode assembly in the first direction, when the first coating and the second coating are continuously coated on the two surfaces of the substrate layer, it will cause serious electrolyte infiltration failure, and a large amount of purple spot lithium precipitation will be generated in the main area of the pole piece (the area near the center of the pole piece), affecting the life of the electrochemical device; and when the first coating and the second coating are intermittently coated on the two surfaces of the substrate layer, the gap between the adjacent first coating and the adjacent second coating is reserved for electrolyte transmission, improving the electrolyte infiltration effect and the life of the electrochemical device. Therefore, the cycle capacity retention rate of Comparative Example 1 is the lowest.
[0064] By comparing Examples 1-3 and 9-10, it can be seen that when 0.3D2≤D1≤0.5 is satisfied, the interface of the negative electrode plate is good after cycling, and the electrochemical device has a high capacity retention rate; when D1 is too small, the bonding area between the first isolation membrane and the electrode is too small, resulting in a low overall mechanical strength of the electrochemical device, and deformation is easily generated during the cycle, resulting in a poor interface; when D1 is too large, the reserved space for electrolyte transmission on the first isolation membrane is too small, resulting in poor wetting, and then causing a poor interface.
[0065] By comparing Examples 2, 7, 8, and 12-13, it can be seen that when 25°≤θ1≤65° is satisfied, the interface of the negative electrode plate is good after cycling, and the electrochemical device has a high capacity retention rate; when θ1 is too small or too large, the edge of the plate is easily deformed, resulting in a poor interface.
[0066] By comparing Examples 2 and 4-6, it can be seen that when 0.7W1≤W2 is satisfied, the interface of the negative electrode plate is good after cycling, and the electrochemical device has a high capacity retention rate; and as W2 / W2 increases, the cycle capacity retention rate shows a trend of first increasing and then remaining unchanged, and the electrochemical device has a higher capacity retention rate when W2≥0.85W1.
[0067] The electrochemical devices of Comparative Example 1 and Examples 2 and 14 were subjected to a hot box test, and the test results are recorded in Table 2. The steps of the hot box test include: charging the electrochemical device to 4.43 V at a constant current of 0.2C at 25±5°C, and then charging to 0.01 C at a constant voltage. The electrochemical device was heated to 140±2°C at a rate of 5±2°C / min, and then maintained for 60 minutes. The electrochemical device was observed to see if there were any failure phenomena such as fire and explosion. If not, the hot box test was passed, otherwise it was not passed. The hot box test pass rate of 20 electrochemical devices was counted. After the test, the electrochemical device was disassembled to observe whether the diaphragm shrank.
[0068] Table 2 By comparing Comparative Example 1 and Example 2, it can be seen that when the surfaces of the second part and the third part of the first isolation membrane are used as the first surface and the second surface of the electrode assembly, that is, when the electrode assembly is finished with the first isolation membrane, the first coating and the second coating are alternately coated on the two surfaces of the substrate layer, thereby improving the pass rate of the hot box test and improving the shrinkage of the first isolation membrane.
[0069] The electrochemical devices of Examples 1-6, 9, and 11 were subjected to a drop test, and the test results are recorded in Table 3. The steps of the drop test include: charging the electrochemical device to 4.43 V at a constant current of 0.2C at 25±5°C, and then charging to 0.01 C at a constant voltage. The electrochemical device was fixed in a drop test fixture, and dropped 6 times in sequence on the 6 sides of the drop test fixture at a height of 1.8m. After each drop, the electrochemical device was observed for damage, and the open circuit voltage of the electrochemical device was measured. If the voltage was less than 3.0V, the electrochemical device was judged to have failed. If there was no damage, the open circuit voltage was higher than 3.0V, which was judged to be non-failure. The test was continued until failure, and the number of drops performed when the electrochemical device failed was recorded. The electrochemical device was then disassembled and analyzed to observe whether the diaphragm shrank.
[0070] Table 3 Comparing Examples 1-3 and 9, it can be seen that when 0.3D2≤D1≤0.5D2 is satisfied, the electrochemical device has a high number of drops and a good drop resistance. When D1 is too small, the bonding area between the first isolation film and the pole piece is small, the first isolation film has a limited binding effect on the electrode assembly as a whole, and the mutual impact between the pole pieces and between the electrode assembly and the shell increases, which can easily lead to shell damage. Therefore, the electrochemical device of Example 9 has the worst drop resistance.
[0071] Comparing Examples 2, 4-6, and 11, it can be seen that when 0.7W1≤W2 is satisfied, the electrochemical device has a large number of drops and a good drop resistance. In Example 11, W2 is too small, and failure caused by shrinkage of the first isolation film occurs during the drop process, resulting in the least number of drops and the worst drop resistance.
[0072] The above disclosure is only a preferred implementation mode of the present application, and certainly cannot be used to limit the present application. Therefore, equivalent changes made according to the present application are still within the scope covered by the present application.
Claims
1. An electrochemical device, characterized in that include: case; an electrode assembly, contained in the housing, the electrode assembly comprising a plurality of electrode sheets stacked along a first direction and a first isolation film disposed between the plurality of electrode sheets, the electrode assembly further comprising a first surface and a second surface opposite to each other in the first direction, and a first end surface connected between the first surface and the second surface; A first insulating layer is bonded to the first surface, the second surface and the first end surface; and an electrolyte contained in the shell; The first isolation film includes a substrate layer and a first coating layer spaced apart on the surface of the substrate layer facing the adjacent pole piece.
2. The electrochemical device according to claim 1, characterized in that The first coating layer is in a strip shape, the substrate layer includes two side edges that are opposite to each other in a second direction that is perpendicular to the first direction, and the plurality of first coating layers are arranged obliquely relative to the side edges.
3. The electrochemical device according to claim 2, characterized in that When observed along the first direction, an included angle between the first coating and the side edge is θ1, and 25°≤θ1≤65°.
4. The electrochemical device according to claim 2, characterized in that When observed along the first direction, the width of the first coating layer is D1, the distance between two adjacent first coating layers is D2, and 0.3D2≤D1≤0.5D2.
5. The electrochemical device according to claim 2, characterized in that The first isolation film further includes a plurality of second coating layers, and the plurality of second coating layers are disposed at intervals on a surface of the substrate layer away from the plurality of first coating layers.
6. The electrochemical device according to claim 5, characterized in that The first coating layer and the second coating layer intersect each other in different planes.
7. The electrochemical device according to claim 1, characterized in that The first isolation membrane includes a plurality of first parts located in the plurality of pole pieces and a second part and a third part located outside the plurality of pole pieces and opposite to each other in the first direction, each of the first parts being arranged between two adjacent pole pieces, and the plurality of first parts, the second parts and the third part being arranged as a whole and forming a winding structure.
8. The electrochemical device according to claim 1, wherein In a third direction perpendicular to the first direction, the width of the electrode assembly is W1, the width of the first insulating layer is W2, and 0.7W1≤W2≤W1.
9. The electrochemical device according to claim 8, characterized in that 0.7W1≤W2≤0.95W1.
10. The electrochemical device according to claim 9, characterized in that 0.85W1≤W2≤0.95W1.
11. The electrochemical device according to claim 1, wherein The first coating layer includes a first inorganic particle layer and a first bonding layer. The first inorganic particle layer is connected to the substrate layer. The bonding layer is arranged on the surface of the inorganic particle layer away from the substrate layer and is bonded to the adjacent pole piece.
12. The electrochemical device according to claim 1, wherein The first coating layer includes inorganic particles and a binder.
13. The electrochemical device according to claim 1, wherein: The electrochemical device also includes a second insulating layer, and the electrode assembly also includes a second end face connected between the first surface and the second surface, defining the length direction of the electrode assembly as a second direction, the first surface and the second surface are opposite to each other in the second direction, and the second insulating layer is connected to the first surface, the second surface and the second end face.
14. The electrochemical device according to claim 13, characterized in that The first insulating layer is a single-sided adhesive tape or a double-sided adhesive tape, and / or the second insulating layer is a single-sided adhesive tape or a double-sided adhesive tape.
15. The electrochemical device according to claim 1, wherein The electrochemical device also includes a first metal plate and a second metal plate, and the first metal plate and the second metal plate are both connected to the electrode assembly; in a third direction perpendicular to the first direction, the electrode assembly also includes a second end face opposite to the first end face, and the first metal plate and the second metal plate extend out of the electrode assembly from the second end face.
16. The electrochemical device according to claim 1, wherein: The shell is a packaging bag.
17. An electrical equipment, characterized in that: Comprising the electrochemical device according to any one of claims 1 to 16.
Citation Information
Patent Citations
Electrochemical device and electronic apparatus
CN114420993A
Electrochemical device and electronic device
CN115149108A