Aluminum flat tube brazed joint temperature control device and control method thereof
Through real-time temperature monitoring and adjustment of the temperature control device of aluminum flat tube brazing joint, the problem of inaccurate welding temperature control in the prior art is solved, and the welding quality and accuracy are improved.
Patent Information
- Application Number
- CN202411198626.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-29
- Publication Date
- 2024-11-22
AI Technical Summary
The existing induction brazing welding process is not accurate enough to control the welding process, resulting in the welded part temperature, especially the internal temperature, which does not meet expectations, affecting the welding quality.
The temperature control device of aluminum flat tube brazing joint is adopted, including external and internal temperature measurement devices, which monitors the temperature field of the workpiece to be welded in real time, and adjusts the heating parameters in real time according to the monitoring data, so as to realize the temperature field through the design of the driver parts and the temperature measurement device. Accurate acquisition and adjustment.
The welding quality is improved, and the welded parts meet the expected temperature field through accurate temperature control, which improves the accuracy and stability of welding.
Smart Images

Figure CN118989508A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of building construction, and in particular to a temperature control device and a control method for a brazing joint of an aluminum flat tube. Background Art
[0002] Brazing is a metal joining technology. It is a welding method in which the brazing material and the weldment are heated to the melting temperature of the brazing material at the same time, and the gap between the solid workpieces is filled with liquid brazing material to connect the metals. It is a green, efficient and low-energy welding method. The new liquid carbon dioxide freezing technology uses parallel flow aluminum flat tubes as heat exchangers inside the freezing tubes. The flat tubes need to be welded to the joints before use.
[0003] The current induction brazing process mainly uses the method of manually pre-setting welding parameters for automatic welding. This method does not accurately control the welding process. The preset welding parameters may not be well adapted to factors such as the environment, brazing material, and processing position, resulting in the weldment temperature, especially the internal temperature, not meeting expectations, thus affecting the welding quality. Summary of the invention
[0004] The purpose of the present invention is to overcome the defects of the prior art and provide a temperature control device and a control method for an aluminum flat tube brazing joint, which can detect the temperature field of the workpiece to be welded in real time during the brazing process so as to adjust the heating parameters in time and improve the welding quality.
[0005] To achieve the above purpose, the technical solution adopted by the present invention is a temperature control device for brazing joints of aluminum flat tubes, wherein the flat tube body is placed on the top of the joint body and together with the joint body forms a workpiece to be welded, and the temperature control device comprises:
[0006] A base, the base being located above the workpiece to be welded;
[0007] A limiting assembly for detachably mounting the base to an existing structure, wherein the limiting assembly is connected to two sides of the base;
[0008] An external temperature measuring device for monitoring the external temperature of the workpiece to be welded, wherein the external temperature measuring device is slidably connected to the bottom of the base;
[0009] An internal temperature measuring device for monitoring the internal temperature of the workpiece to be welded, the internal temperature measuring device comprising a thermometer placed on the top of the base and a plurality of thermocouple wires spaced apart and connected to the bottom of the thermometer, the base being provided with a first through hole for the plurality of thermocouple wires to pass through together, and the flat tube body being provided with a plurality of temperature measuring holes vertically penetrating therethrough for the plurality of thermocouple wires to be inserted one by one.
[0010] A further improvement of the temperature control device for brazing joints of aluminum flat tubes of the present invention is that the external temperature measuring device comprises:
[0011] A connecting plate arranged in the horizontal direction, wherein both sides of the bottom of the connecting plate are connected to first vertical plates, and a mounting box is connected to the middle of the bottom of the connecting plate, and the mounting box is located between the two first vertical plates;
[0012] Two one-way screw rods, the first ends of the two one-way screw rods are respectively rotatably connected to the opposite inner sides of the two first vertical plates, and the second ends of the two one-way screw rods are inserted into the installation box;
[0013] Two screw sleeves, the two screw sleeves are respectively threadedly sleeved on the two one-way screw rods, the top of each screw sleeve is connected to a limit slider, and the bottom of the connecting plate is provided with a limit slide groove for sliding the limit slider along the length direction of the one-way screw rod;
[0014] Two clamping plates for clamping the workpiece to be welded, the two clamping plates are respectively connected to the bottom of the two screw sleeves;
[0015] Two infrared thermometers, the two infrared thermometers are respectively connected to the opposite inner sides of the two clamping plates, and the opposite inner sides of the two clamping plates are each provided with a mounting groove for connecting the corresponding infrared thermometers;
[0016] A driving member is used for driving the two one-way screw rods to rotate, wherein the driving member is connected to the top of the connecting plate, and the driving member is connected to the base.
[0017] A further improvement of the temperature control device for brazing joints of aluminum flat tubes of the present invention is that the driving member is a first motor, a motor shaft of the first motor is inserted in the mounting box, a second through hole for the motor shaft to pass through is provided on the connecting plate and the mounting box, an active umbrella-shaped bevel gear is connected to the motor shaft, the second ends of the two one-way screw rods are connected to driven umbrella-shaped bevel gears, and the active umbrella-shaped bevel gear is meshingly connected with the two driven umbrella-shaped bevel gears.
[0018] A further improvement of the temperature control device for brazing joints of aluminum flat tubes of the present invention is that a sliding block is connected between the driving member and the base, a sliding rail is connected to the bottom of the base, and the sliding block slidably cooperates with the sliding rail.
[0019] A further improvement of the temperature control device for brazing joints of aluminum flat tubes of the present invention is that the height of the internal temperature measuring device is adjustable, and a hanging device for adjusting the height of the internal temperature measuring device is connected to the top of the base, and the hanging device includes:
[0020] Two second vertical plates, the two second vertical plates are connected to the top of the base at intervals and are located at two opposite sides of the first through hole;
[0021] A winding roller arranged in the horizontal direction, wherein the winding roller is rotatably connected between the two second vertical plates;
[0022] a second motor for driving the winding roller to rotate, the second motor being connected to the relatively outer side of one of the second vertical plates, and a third through hole for allowing the motor shaft of the second motor to pass through and being coaxially connected to the winding roller being provided on the corresponding second vertical plate;
[0023] Two hanging ropes are used for hanging the internal temperature measuring device, and the two hanging ropes are both wound on the winding roller and the free ends are connected to the top of the thermometer.
[0024] A further improvement of the temperature control device for brazing joints of aluminum flat tubes of the present invention is that the limit assembly comprises:
[0025] Two ear plates are arranged in a horizontal direction, and the two ear plates are respectively connected to opposite sides of the base;
[0026] Two vertically arranged pressure rods, and two ear plates are respectively provided with insertion holes for the two pressure rods to be inserted;
[0027] Two suction cups, the two suction cups are respectively connected to the bottoms of the two pressure rods;
[0028] Two buffer springs are respectively located at the top of the two ear plates and are respectively sleeved outside the two pressure rods. The first end of each buffer spring is connected to the top of the corresponding pressure rod, and the second end is connected to the top of the corresponding ear plate.
[0029] A method for controlling the temperature of an aluminum flat tube brazing joint comprises the following steps:
[0030] Step 1: Provide the above-mentioned aluminum flat tube brazing joint temperature control device and install it above the workpiece to be welded;
[0031] Step 2: Provide a welding device and weld the workpiece to be welded using the designed heating parameters, and at the same time slide the external temperature measuring device to monitor the external temperature of each external point of the workpiece to be welded, and insert multiple thermocouple wires into the corresponding temperature measuring holes on the flat tube body to monitor the internal temperature of each internal point of the workpiece to be welded;
[0032] Step 3: Based on all the monitored external temperatures and all the monitored internal temperatures, the temperature field of the workpiece to be welded is obtained, and it is determined whether the temperature field meets the welding requirements:
[0033] Step 3.1: If satisfied, continue welding using the designed heating parameters;
[0034] Step 3.2: If not satisfied, adjust the designed heating parameters and then return to the above step 2.
[0035] A further improvement of the temperature control method of the aluminum flat tube brazing joint of the present invention is that, when executing the above step 3, the temperature field is obtained by using the Kriging interpolation method.
[0036] Compared with the prior art, the advantages of the present invention are:
[0037] By combining an external temperature measuring device with an internal temperature measuring device, the temperature field of the workpiece to be welded can be accurately obtained, which facilitates real-time adjustment of heating parameters and improves welding quality. BRIEF DESCRIPTION OF THE DRAWINGS
[0038] In order to more clearly illustrate the technical solutions in the embodiments of the present invention, the following briefly introduces the drawings required for use in the description of the embodiments. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without creative work.
[0039] Figure 1 It is a schematic structural diagram of the use state of the temperature control device for the brazing joint of the aluminum flat tube of the present invention.
[0040] Figure 2 This is a detailed structural diagram of the external temperature measuring device of the temperature control device for the brazing joint of the aluminum flat tube of the present invention.
[0041] Figure 3 The figure is a schematic diagram of the flat tube body structure of the temperature control device for the brazing joint of the aluminum flat tube of the present invention.
[0042] Figure 4 The present invention is a schematic diagram of the structure of the hanging device of the temperature control device for the brazing joint of the aluminum flat tube.
[0043] In the figure: 1. base; 2. flat tube body; 3. joint body; 4. external temperature measuring device; 401. connecting plate; 402. first vertical plate; 403. mounting box; 404. one-way screw; 405. screw sleeve; 406. clamping plate; 407. mounting groove; 408. infrared thermometer; 409. first motor; 410. active umbrella-shaped bevel gear; 411. driven umbrella-shaped bevel gear; 5. sliding block; 6. hanging device; 601. second vertical plate; 602. winding roller; 603. second motor; 604. hanging rope; 7. thermometer; 8. thermocouple wire; 9. ear plate; 10. pressure rod; 11. suction cup; 12. buffer spring; 13. temperature measuring hole; 14. first through hole. DETAILED DESCRIPTION
[0044] The following describes the embodiments of the present invention through specific examples, and those skilled in the art can easily understand other advantages and effects of the present invention from the contents disclosed in this specification. The present invention can also be implemented or applied through other different specific embodiments, and the details in this specification can also be modified or changed in various ways based on different viewpoints and applications without departing from the spirit of the present invention.
[0045] The temperature control device and control method of the aluminum flat tube brazing joint of the present invention are further described in detail below in conjunction with the accompanying drawings and specific embodiments.
[0046] See also Figure 1 to Figure 4 As shown, the temperature control device for brazing an aluminum flat tube joint, the flat tube body 2 is placed on the top of the joint body 3, and together with the joint body 3 forms a workpiece to be welded, the temperature control device includes:
[0047] A base 1, the base 1 is located above the workpiece to be welded;
[0048] A limiting assembly for detachably mounting the base 1 to an existing structure, the limiting assembly being connected to two sides of the base 1;
[0049] An external temperature measuring device 4 for monitoring the external temperature of the workpiece to be welded, wherein the external temperature measuring device 4 is slidably connected to the bottom of the base 1;
[0050] An internal temperature measuring device for monitoring the internal temperature of the workpiece to be welded, the internal temperature measuring device comprises a thermometer 7 placed on the top of the base 1 and a plurality of thermocouple wires 8 connected at intervals to the bottom of the thermometer 7, the base 1 is provided with a first through hole 14 for the plurality of thermocouple wires 8 to pass through together, and the flat tube body 2 is provided with a plurality of temperature measuring holes 13 vertically penetrating therethrough for the plurality of thermocouple wires 8 to be inserted one by one.
[0051] An internal temperature measuring device is provided and temperature measuring holes 13 are provided at intervals on the flat tube body 2 so that the thermocouple wire 8 can extend into the temperature measuring hole 13 to monitor the internal temperature of the workpiece to be welded.
[0052] By combining the external temperature measuring device 4 with the internal temperature measuring device, the temperature field of the workpiece to be welded can be accurately obtained, which facilitates real-time adjustment of heating parameters and improves welding quality.
[0053] Preferably, the external temperature measuring device 4 comprises:
[0054] A connecting plate 401 arranged in the horizontal direction, both sides of the bottom of the connecting plate 401 are connected to first vertical plates 402, and a mounting box 403 is connected to the middle of the bottom of the connecting plate 401, and the mounting box 403 is located between the two first vertical plates 402;
[0055] Two one-way screw rods 404, the first ends of the two one-way screw rods 404 are respectively rotatably connected to the opposite inner sides of the two first vertical plates 402, and the second ends are both inserted into the installation box 403;
[0056] Two screw sleeves 405, the two screw sleeves 405 are respectively screwed and sleeved on the two one-way screw rods 404, the top of each screw sleeve 405 is connected to a limit slider, and the bottom of the connecting plate 401 is provided with a limit slide groove along the length direction of the one-way screw rod 404 for the limit slider to slide;
[0057] Two clamping plates 406 for clamping the workpiece to be welded, the two clamping plates 406 are respectively connected to the bottom of the two screw sleeves 405;
[0058] Two infrared thermometers 408, the two infrared thermometers 408 are respectively connected to the opposite inner sides of the two clamping plates 406, and the opposite inner sides of the two clamping plates 406 are both provided with mounting grooves 407 for connecting the corresponding infrared thermometers 408;
[0059] A driving member is used to drive the two one-way screw rods 404 to rotate. The driving member is connected to the top of the connecting plate 401 and is connected to the base 1 .
[0060] The two one-way screw rods 404 are driven to rotate by a driving member, so that the two screw sleeves 405 are relatively close to or relatively far away from each other, so as to adjust the distance between the two clamping plates 406, so as to facilitate clamping of workpieces to be welded of different sizes and improve practicality.
[0061] By providing the installation groove 407 for the infrared thermometer 408 to be installed, it is avoided that when the two clamps are arranged on the opposite outer sides of the workpiece to be welded, the infrared thermometer 408 is not directly in contact with the high-temperature workpiece to be welded, causing damage to the infrared thermometer 408.
[0062] Preferably, the driving member is a first motor 409, the motor shaft of the first motor 409 is inserted in the installation box 403, the connecting plate 401 and the installation box 403 are provided with a second through hole for the motor shaft to pass through, the motor shaft is connected to an active umbrella-shaped bevel gear 410, the second ends of the two one-way screw rods 404 are connected to driven umbrella-shaped bevel gears 411, and the active umbrella-shaped bevel gear 410 is meshingly connected with the two driven umbrella-shaped bevel gears 411.
[0063] Preferably, a sliding block 5 is connected between the driving member and the base 1 , a sliding rail is connected to the bottom of the base 1 , and the sliding block 5 is slidably matched with the sliding rail.
[0064] By providing the sliding block 5, the construction personnel can push the external temperature measuring device 4 to slide, so as to facilitate monitoring of the external temperature of each point on the workpiece to be welded, thereby improving the construction efficiency.
[0065] Preferably, the height of the internal temperature measuring device is adjustable, and the top of the base 1 is connected with a hanging device 6 for adjusting the height of the internal temperature measuring device, and the hanging device 6 includes:
[0066] Two second vertical plates 601 , the two second vertical plates 601 are connected to the top of the base 1 at intervals and are located at opposite sides of the first through hole 14 ;
[0067] A winding roller 602 arranged in the horizontal direction, the winding roller 602 is rotatably connected between the two second vertical plates 601;
[0068] A second motor 603 for driving the winding roller 602 to rotate, the second motor 603 being connected to the relatively outer side of one of the second vertical plates 601, and a third through hole for the motor shaft of the second motor 603 to pass through and coaxially connected to the winding roller 602 is provided on the corresponding second vertical plate 601;
[0069] Two hanging ropes 604 are used to hang the internal temperature measuring device. Both of the hanging ropes 604 are wound on the winding roller 602 and the free ends are connected to the top of the thermometer 7.
[0070] By setting the hanging device 6, the height of the internal temperature measuring device can be adjusted, so that the position of the internal temperature measuring point can be adjusted to correspond to the external temperature measuring point, so as to obtain a more accurate temperature field.
[0071] Specifically, the height of the second vertical plate 601 is adjustable. The second vertical plate 601 includes a sleeve connected to the top of the base and a core plate inserted in the sleeve. The sleeve and the core plate are connected by a pin. A first socket for inserting the pin is provided on the sleeve, and a plurality of second sockets for selectively inserting the pin are vertically spaced apart on the core plate.
[0072] By designing the second vertical plate 601 to be height-adjustable, it is suitable for workpieces to be welded of various heights, thereby improving practicality.
[0073] Preferably, the limit assembly comprises:
[0074] Two ear plates 9 are arranged in the horizontal direction, and the two ear plates 9 are respectively connected to opposite sides of the base 1;
[0075] Two vertically arranged pressure rods 10, and two ear plates 9 are respectively provided with insertion holes for the two pressure rods 10 to be inserted;
[0076] Two suction cups 11, the two suction cups 11 are respectively connected to the bottoms of the two pressure rods 10;
[0077] Two buffer springs 12 are respectively located at the top of the two ear plates 9 and are respectively sleeved outside the two pressure rods 10. The first end of each buffer spring 12 is connected to the top of the corresponding pressure rod 10, and the second end is connected to the top of the corresponding ear plate 9.
[0078] A method for controlling the temperature of an aluminum flat tube brazing joint comprises the following steps:
[0079] Step 1: Provide the above-mentioned aluminum flat tube brazing joint temperature control device and install it above the workpiece to be welded;
[0080] Step 2: Provide a welding device and weld the workpiece to be welded using the designed heating parameters, while sliding the external temperature measuring device 4 to monitor the external temperature of each point on the outside of the workpiece to be welded, and insert multiple thermocouple wires 8 into the corresponding temperature measuring holes 13 on the flat tube body 2 to monitor the internal temperature of each point on the inside of the workpiece to be welded;
[0081] Step 3: Based on all the monitored external temperatures and all the internal temperatures, the temperature field of the workpiece to be welded is obtained to determine whether the temperature field meets the welding requirements:
[0082] Step 3.1: If satisfied, continue welding using the designed heating parameters;
[0083] Step 3.2: If not satisfied, adjust the design heating parameters and then return to the above step 2.
[0084] Preferably, when executing the above step 3, the temperature field is obtained by using the Kriging interpolation method.
[0085] It should be noted that the structures, proportions, sizes, etc. illustrated in the drawings of this specification are only used to match the contents disclosed in the specification for people familiar with this technology to understand and read, and are not used to limit the limiting conditions for the implementation of the present invention, so they have no substantial technical significance. Any modification of the structure, change of the proportion relationship or adjustment of the size should still fall within the scope of the technical content disclosed by the present invention without affecting the effects and purposes that can be achieved by the present invention. At the same time, the terms such as "upper", "lower", "left", "right", "middle" and "one" quoted in this specification are only for the convenience of description, and are not used to limit the scope of the implementation of the present invention. The change or adjustment of their relative relationship should also be regarded as the scope of the implementation of the present invention without substantially changing the technical content.
[0086] The above is only a preferred embodiment of the present invention, and does not limit the present invention in any form. Although the present invention has been disclosed as a preferred embodiment as above, it is not used to limit the present invention. Any technician familiar with this profession can make some changes or modifications to equivalent embodiments of equivalent changes using the technical contents disclosed above without departing from the scope of the technical solution of the present invention. However, any simple modification, equivalent change and modification made to the above embodiments based on the technical essence of the present invention without departing from the content of the technical solution of the present invention still fall within the scope of the technical solution of the present invention.
Claims
1. A temperature control device for brazing an aluminum flat tube joint, wherein the flat tube body is placed on the top of the joint body and together with the joint body forms a workpiece to be welded. It is characterized in that The temperature control device comprises: A base, the base being located above the workpiece to be welded; A limiting assembly for detachably mounting the base to an existing structure, wherein the limiting assembly is connected to two sides of the base; An external temperature measuring device for monitoring the external temperature of the workpiece to be welded, wherein the external temperature measuring device is slidably connected to the bottom of the base; An internal temperature measuring device for monitoring the internal temperature of the workpiece to be welded, the internal temperature measuring device comprising a thermometer placed on the top of the base and a plurality of thermocouple wires spaced apart and connected to the bottom of the thermometer, the base being provided with a first through hole for the plurality of thermocouple wires to pass through together, and the flat tube body being provided with a plurality of temperature measuring holes vertically penetrating therethrough for the plurality of thermocouple wires to be inserted one by one.
2. The temperature control device for brazing joint of aluminum flat tube according to claim 1, It is characterized in that The external temperature measuring device comprises: A connecting plate arranged in the horizontal direction, wherein both sides of the bottom of the connecting plate are connected to first vertical plates, and a mounting box is connected to the middle of the bottom of the connecting plate, and the mounting box is located between the two first vertical plates; Two one-way screw rods, the first ends of the two one-way screw rods are respectively rotatably connected to the opposite inner sides of the two first vertical plates, and the second ends of the two one-way screw rods are inserted into the installation box; Two screw sleeves, the two screw sleeves are respectively threadedly sleeved on the two one-way screw rods, the top of each screw sleeve is connected to a limit slider, and the bottom of the connecting plate is provided with a limit slide groove for sliding the limit slider along the length direction of the one-way screw rod; Two clamping plates for clamping the workpiece to be welded, the two clamping plates are respectively connected to the bottom of the two screw sleeves; Two infrared thermometers, the two infrared thermometers are respectively connected to the opposite inner sides of the two clamping plates, and the opposite inner sides of the two clamping plates are each provided with a mounting groove for connecting the corresponding infrared thermometers; A driving member is used for driving the two one-way screws to rotate, wherein the driving member is connected to the top of the connecting plate, and the driving member is connected to the base.
3. The temperature control device for brazing joint of aluminum flat tube according to claim 2, It is characterized in that The driving member is a first motor, a motor shaft of the first motor is inserted in the mounting box, a second through hole for the motor shaft to pass through is provided on the connecting plate and the mounting box, an active umbrella-shaped bevel gear is connected to the motor shaft, the second ends of the two one-way screws are connected to driven umbrella-shaped bevel gears, and the active umbrella-shaped bevel gear is meshedly connected with the two driven umbrella-shaped bevel gears.
4. The temperature control device for brazing joint of aluminum flat tube according to claim 2, It is characterized in that A sliding block is connected between the driving member and the base, a sliding rail is connected to the bottom of the base, and the sliding block is slidably matched with the sliding rail.
5. The temperature control device for brazing joint of aluminum flat tube according to claim 1, It is characterized in that The height of the internal temperature measuring device is adjustable, and a hanging device for adjusting the height of the internal temperature measuring device is connected to the top of the base, and the hanging device includes: Two second vertical plates, the two second vertical plates are connected to the top of the base at intervals and are located at two opposite sides of the first through hole; A winding roller arranged in the horizontal direction, wherein the winding roller is rotatably connected between the two second vertical plates; a second motor for driving the winding roller to rotate, the second motor being connected to the relatively outer side of one of the second vertical plates, and a third through hole for allowing the motor shaft of the second motor to pass through and being coaxially connected to the winding roller being provided on the corresponding second vertical plate; Two hanging ropes are used for hanging the internal temperature measuring device, and the two hanging ropes are both wound on the winding roller and the free ends are connected to the top of the thermometer.
6. The temperature control device for brazing joint of aluminum flat tube according to claim 1, It is characterized in that The limiting component comprises: Two ear plates are arranged in a horizontal direction, and the two ear plates are respectively connected to opposite sides of the base; Two vertically arranged pressure rods, and two ear plates are respectively provided with insertion holes for the two pressure rods to be inserted; Two suction cups, the two suction cups are respectively connected to the bottoms of the two pressure rods; Two buffer springs are respectively located at the top of the two ear plates and are respectively sleeved outside the two pressure rods. The first end of each buffer spring is connected to the top of the corresponding pressure rod, and the second end is connected to the top of the corresponding ear plate.
7. A temperature control method for brazing joints of aluminum flat tubes, It is characterized in that Includes steps: Step 1: Provide the temperature control device for brazing joint of aluminum flat tube as claimed in claim 1 and install it above the workpiece to be welded; Step 2: Provide a welding device and weld the workpiece to be welded using the designed heating parameters, and at the same time slide the external temperature measuring device to monitor the external temperature of each external point of the workpiece to be welded, and insert multiple thermocouple wires into the corresponding temperature measuring holes on the flat tube body to monitor the internal temperature of each internal point of the workpiece to be welded; Step 3: Based on all the monitored external temperatures and all the monitored internal temperatures, the temperature field of the workpiece to be welded is obtained, and it is determined whether the temperature field meets the welding requirements: Step 3.1: If satisfied, continue welding using the designed heating parameters; Step 3.2: If not satisfied, adjust the designed heating parameters and then return to the above step 2.
8. The temperature control method of the aluminum flat tube brazing joint according to claim 7, It is characterized in that When executing the above step 3, the temperature field is obtained by using the Kriging interpolation method.