Adjusting material and online grinding method for annealing furnace roller
By designing the adjustment material including transition section A, grinding section and transition section B, the material loss and complexity problems in online grinding of annealing furnace rollers are solved, and the efficient grinding process is realized, reducing the grinding cost and belt The impact of steel production.
Patent Information
- Application Number
- CN202411158864.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-22
- Publication Date
- 2024-11-22
- Estimated Expiration
- 2044-08-22
AI Technical Summary
In the prior art, during the online grinding process of the annealing furnace furnace roller, the material loss of the adjustment material is more, and the grinding process is complicated, which leads to an increase in the grinding time and cost, and affects the production quality of the strip.
It provides an adjustment material including transition section A, grinding section and transition section B. The length of transition section A is matched with the annealing furnace production line, for replacing strip steel, grinding section for grinding, and transition section B is for Temperature recovery ensures temperature stability and reduces material waste and grinding time.
By optimizing the design of the adjustment material, grinding can be completed with only one roll of adjustment material, reducing material loss and online time, reducing grinding costs, simplifying production order, and avoiding the impact of strip quality.
Smart Images

Figure CN118990168A_ABST
Abstract
Description
Technical Field
[0001] The present application belongs to the technical field of furnace roller grinding, and specifically relates to an adjustment material and an online grinding method for an annealing furnace roller. Background Art
[0002] When the annealing furnace rollers are nodulated (foreign matter adheres to the rollers), they are usually treated by online grinding. The grinding principle is to create a large speed difference between the running speed of the strip and the linear speed of the rollers. The strip and the rollers will be relatively displaced, and the friction between the strip and the rollers is used to grind away foreign matter on the roller surface.
[0003] The above-mentioned grinding method will cause serious wear on the surface of the strip steel. Therefore, when grinding the furnace rollers, the annealing furnace production line will arrange adjustment materials (a relatively low-priced steel coil) to be put online to reduce the grinding cost of the furnace rollers.
[0004] The thicker the adjustment material is, the greater the pressure on the furnace roller is, and the better the grinding effect is. Therefore, the thickness of the adjustment material generally used for grinding furnace rollers is 0.6mm (greater than the thickness of the strip steel).
[0005] The thickness of the strip steel normally produced by the production line is relatively thin (below 0.35mm). Directly putting 0.6mm thick adjustment materials on the line will cause large fluctuations in the furnace temperature. Large fluctuations in the furnace temperature will directly affect the quality of the strip steel that has not yet come off the line.
[0006] To solve the above problems, the existing method is to put a roll of thinner adjustment material on line for transition when grinding the furnace roller nodules online, and replace the uncut strip steel to avoid affecting the quality of the strip steel due to temperature changes during the grinding process; then put a roll of 0.6mm thick adjustment material on line to grind the furnace roller, and after completing the grinding of the furnace roller, put another roll of thinner adjustment material on line to restore the production process of the strip steel. This method requires three rolls of adjustment material to complete the online grinding of the furnace roller without affecting the production of the strip steel. However, the length of the existing roll of adjustment material is much longer than the length of the annealing furnace production line, and a large amount of adjustment material used to replace and restore the production process will be wasted. At the same time, when putting the adjustment material on line, the operator needs to carry and weld the strip steel and the adjustment material or the adjustment material and the adjustment material many times, which makes the entire grinding process more complicated and the grinding time is greatly increased, resulting in an increase in the grinding cost of the furnace roller. Summary of the invention
[0007] In order to solve the above technical problems, the present application provides an adjustment material on the one hand to solve the technical problems in the prior art that the material loss in the online grinding of furnace rollers is large, the grinding process is relatively complicated, the grinding time is greatly increased, and the grinding cost is increased.
[0008] The technical solution adopted to achieve the purpose of this application is:
[0009] An adjustment material, comprising a transition section A, a grinding section and a transition section B;
[0010] The transition section A, the grinding section and the transition section B are connected in sequence; the length of the transition section A matches the length of the annealing furnace production line, and the time for the transition section B to pass through the annealing furnace production line can restore the working temperature of the annealing furnace production line to the production temperature;
[0011] In the process of grinding the furnace rollers of the annealing furnace, the transition section A is used to replace the strip steel on the annealing furnace production line, and the transition section B is used for the transition of temperature recovery of the annealing furnace production line.
[0012] In order to better achieve the purpose of the present application, further optimization is made in the above structure, and the thickness of the transition section A and the thickness of the transition section B are matched with the thickness of the strip processed by the annealing furnace production line.
[0013] In order to better achieve the purpose of the present application, further optimization is made in the above structure. When the length of the annealing furnace production line is greater than 400m, the length of the transition section A(1) is 0-200m shorter than the length of the annealing furnace production line.
[0014] In order to better achieve the purpose of the present application, further optimization is made in the above structure, and the thickness of the transition section A is 0.3-0.4 mm.
[0015] In order to better achieve the purpose of the present application, further optimization is made in the above structure, and the length of the transition section B (3) is 1-1.5 times the length of the annealing furnace production line.
[0016] In order to better achieve the purpose of the present application, further optimization is made in the above structure, and the thickness of the transition section B is 0.3-0.4 mm.
[0017] In order to better achieve the purpose of the present application, further optimization is made in the above structure, and the length of the grinding section (2) is 3-4 times the length of the annealing furnace production line.
[0018] In order to better achieve the purpose of the present application, further optimization is made in the above structure, and the thickness of the grinding section is 0.5-0.65 mm.
[0019] In order to better achieve the purpose of the present application, the above structure is further optimized, the transition section A, the grinding section and the transition section B are integrally formed components, or,
[0020] The transition section A, the grinding section and the transition section B are connected in sequence by welding.
[0021] On the other hand, the present application also provides an online grinding method for an annealing furnace roller, the method being performed using the above-mentioned adjustment material, the method comprising:
[0022] Obtain the surface condition information of the furnace rollers on the annealing furnace production line;
[0023] When nodules appear on the surface of the furnace roller, the adjustment material is put on the feeding end of the annealing furnace production line, and the end of the transition section A in the adjustment material away from the grinding section enters the annealing furnace production line along with the end of the strip at the feeding end of the annealing furnace production line;
[0024] The transition section A replaces the strip steel on the annealing furnace production line, and introduces the grinding section into the annealing furnace production line, and realizes the grinding of the furnace roller by using the relative displacement between the surface of the grinding section and the surface of the furnace roller;
[0025] The end of the grinding section away from the transition section A introduces the transition section B into the annealing furnace production line. When the transition section B passes through the annealing furnace production line, the working temperature of the annealing furnace production line gradually returns to the production temperature.
[0026] It can be seen from the above technical scheme that the length of the transition section A in the adjustment material provided in the present application matches the length of the annealing furnace production line, and the transition section A can completely replace the strip steel on the production line, thereby avoiding the situation in which the temperature of the annealing furnace production line changes when the grinding section enters the annealing furnace production line and the quality of the strip steel is affected, and there is no extra waste of transition section A. The time for transition section B to pass through the annealing furnace production line can restore the working temperature of the annealing furnace production line to the production temperature, so as to facilitate the subsequent production of strip steel. At the same time, the transition section A, the grinding section and the transition section B are connected in sequence. During the grinding process, only one roll of adjustment material is used to complete the entire grinding work, so as to reduce material loss and shorten the online time of the adjustment material, thereby reducing the production capacity loss of the annealing furnace production line, and the number of welding times at the feeding end of the annealing furnace production line is reduced, which has little impact on the production order, thereby reducing the cost of online grinding of the annealing furnace rollers. BRIEF DESCRIPTION OF THE DRAWINGS
[0027] Figure 1 This is a front view of an adjustment material in a rolled state in an embodiment of the present application.
[0028] Explanation of the reference numerals: 1 - transition section A; 2 - grinding section; 3 - transition section B. DETAILED DESCRIPTION
[0029] In order to enable technicians in the technical field to which the present application belongs to understand the present application more clearly, the technical solution of the present application is described in detail below through specific embodiments in conjunction with the accompanying drawings.
[0030] In the embodiment of the present application, the adjustment material includes a transition section A1, a grinding section 2 and a transition section B3; wherein,
[0031] The transition section A1, the grinding section 2 and the transition section B3 are connected in sequence;
[0032] The length of the transition section A1 matches the length of the annealing furnace production line. The transition section A1 can replace the strip steel on the production line to avoid the situation where the temperature and tension of the annealing furnace production line change when the grinding section 2 enters the annealing furnace production line, which affects the quality of the strip steel. At the same time, after the transition section A1 completely replaces the strip steel, it can bring the grinding section 2 into the annealing furnace production line for grinding work, and there is no material waste in the entire replacement process.
[0033] The time that the transition section B3 passes through the annealing furnace production line can restore the working temperature of the annealing furnace production line to the production temperature. When the end of the grinding section 2 away from the transition section A1 enters the feeding end of the annealing furnace, the grinding section 2 can bring the transition section B3 into the annealing furnace production line, so that the temperature of the annealing furnace production line affected by the grinding section 2 gradually recovers to the production temperature, and then the strip steel can continue to be fed in for strip steel production.
[0034] In some embodiments, when the length of the annealing furnace production line is greater than 400 m, the length of the transition section A1 is 0-200 m shorter than the length of the annealing furnace production line. For example, when the length of the annealing furnace production line is 400 m, the length of the transition section A1 can be selected to be 400 m, so that the strip steel on the annealing furnace production line can be completely replaced before the grinding section 2 enters the annealing furnace production line.
[0035] Of course, the length of transition section A1 can also be selected as 200m. When the grinding section 2 just enters the annealing furnace production line, the gap between the strip steel that has not been off the annealing furnace production line and the grinding section 2 is 200m (the length of transition section A1). The influence of the grinding section 2 on the temperature of the annealing furnace will not immediately and directly affect the quality of the strip steel that has not been off the line.
[0036] It should be noted that when the length of the above-mentioned annealing furnace is less than or equal to 400m, and the difference between the length of the transition section A1 and the length of the annealing furnace production line is selected to be 200m, the influence of the grinding section 2 on the temperature of the annealing furnace is likely to directly affect the quality of the strip that has not been off the line. Therefore, the length of the transition section A1 is 0-200m shorter than the length of the annealing furnace production line, which is suitable for the case where the length of the annealing furnace production line is greater than 400m.
[0037] In some embodiments, the thickness of the transition section A1 is 0.3-0.4 mm, so that its thickness is similar to or the same as the thickness of the strip steel produced by the annealing furnace production line, thereby reducing the impact of the transition section A1 on the temperature and tension of the annealing furnace production line.
[0038] In some embodiments, the length of the transition section B3 is 1-1.5 times the length of the annealing furnace production line, so that when the transition section B3 passes through the annealing furnace production line, the operating temperature of the annealing furnace production line will gradually return to the production temperature, facilitating the subsequent production of strip steel.
[0039] In some embodiments, the thickness of the transition section B3 is 0.3-0.4 mm, so that its thickness is similar to or the same as the thickness of the strip produced by the annealing furnace production line, so that the transition section B3 can facilitate the recovery of the temperature of the annealing furnace production line when passing through the annealing furnace production line.
[0040] In some embodiments, the length of the grinding section 2 is 3-4 times the length of the annealing furnace production line, so that the grinding section 2 can meet the grinding requirements of the furnace rollers.
[0041] In some embodiments, the grinding section 2 has a thickness of 0.5-0.65 mm and a weight greater than that of the steel strip, which can generate a greater pressure on the furnace roller (compared with the steel strip) to improve the grinding effect.
[0042] In order to better illustrate this embodiment, a large annealing furnace (the length of the annealing furnace production line is 1000m) is used as an example to illustrate the use of the adjustment material:
[0043] The length of the above-mentioned transition section A1 is 800-1000m; the length of the grinding section 2 is 3000-4000m; the length of the transition section B3 is 1000-1500m; preferably, the length of the transition section A1 is 1000m, the thickness of the transition section A1 is 0.35mm, the length of the grinding section 2 is 4000m, the thickness of the grinding section 2 is 0.6mm, the length of the transition section B3 is 1500m, and the thickness of the transition section B3 is 0.35mm; the adjustment material starts to roll up from the end of the transition section B3 away from the grinding section 2, and the adjustment material is rolled into a steel coil. At this time, the transition section A1 is located at the left outer layer of the steel coil, the grinding section 2 is located in the middle layer of the steel coil, and the transition section B3 is located in the innermost layer of the steel coil, such as Figure 1 As shown;
[0044] When there are nodules on the furnace rollers, the operator can prepare the adjustment material and send the prepared adjustment material to the loading end of the annealing furnace production line;
[0045] The head end of the transition section A1 in the adjustment material (the end away from the grinding section 2) is connected to the end of the strip on the annealing furnace production line. Driven by the strip and the furnace roller, the transition section A1 enters the annealing furnace production line until the head end of the transition section A1 moves to the offline end of the annealing furnace production line. The connection between the transition section A1 and the grinding section 2 just enters the online end of the annealing furnace production line. At this time, the strip on the annealing furnace production line is completely replaced by the transition section A1. The temperature and tension changes of the annealing furnace production line caused by the grinding section 2 entering the annealing furnace production line will not affect the quality of the strip. The transition section A1 with a thickness of 0.35 mm is relatively light, and its thickness is similar to or the same as that of the strip produced by the annealing furnace production line. In the process of replacing the strip, the temperature and tension of the annealing furnace production line will not change greatly. Therefore, the quality of the strip that has not been offline will not be affected in the process of replacing the strip by the transition section A1.
[0046] When the grinding section 2 enters the annealing furnace production line, the pressure of the 0.6mm thick grinding section 2 on the furnace roller increases, and there is a large speed difference between the running speed of the grinding section 2 and the linear speed of the furnace roller. The relative displacement between the grinding section 2 and the furnace roller surface can realize the grinding of the furnace roller.
[0047] After the grinding section 2 is released, the grinding section 2 can drive the transition section B3 to enter the annealing furnace production line. The 0.35mm thick transition section B3 is similar to or the same as the thickness of the strip produced by the annealing furnace production line, and has little effect on the temperature and tension of the annealing furnace production line. When the transition section B3 passes through the annealing furnace production line, the working temperature of the annealing furnace production line will gradually return to the production temperature to facilitate the production of the strip entering the annealing furnace production line.
[0048] It should be noted that the operating temperature of the annealing furnace production line mentioned above refers to the heating temperature of the heating section when the annealing furnace production line is working, and the production temperature of the annealing furnace production line mentioned above refers to the temperature value that the heating section of the annealing furnace production line needs to reach when the annealing furnace production line produces strip steel;
[0049] The length of the above-mentioned transition section A1 matches the length of the annealing furnace production line, which does not mean that the length of the transition section A1 is equal to the length of the annealing furnace production line. The length of the transition section A1 is close to the length of the annealing furnace production line, which satisfies the above-mentioned matching requirement, that is, the difference between the length of the transition section A1 and the length of the annealing furnace production line can be in the range of 0-200m.
[0050] Of course, the length and thickness of the transition section A1, grinding section 2 and transition section B3 are not limited to the above values, and can be specifically determined according to the length of the annealing furnace production line and the thickness of the strip produced by the annealing furnace production line.
[0051] In some embodiments, the above-mentioned transition section A1, grinding section 2 and transition section B3 are integrally formed components;
[0052] Alternatively, the transition section A1, the grinding section 2 and the transition section B3 are connected in sequence by welding;
[0053] During the online grinding of the annealing furnace rollers, the operators are not required to weld the transition section A1 and the grinding section 2, and the grinding section 2 and the transition section B3. It is only necessary to complete the welding of the head end of the transition section A1 and the end of the strip on the annealing furnace production line, and the end of the transition section B2 (the end of the transition section B2 away from the grinding section 2) and the head end of the new strip on the line, so as to simplify the working process, thereby improving the grinding efficiency of the furnace rollers and further reducing the grinding cost of the furnace rollers.
[0054] On the other hand, the present application also provides an online grinding method for an annealing furnace roller, the method adopting the above-mentioned adjustment material, the method comprising:
[0055] Obtain the surface condition information of the furnace rollers on the annealing furnace production line;
[0056] When nodules appear on the surface of the furnace roller, the material is adjusted at the feeding end of the annealing furnace production line, and the end of the transition section A1 in the adjusted material away from the grinding section 2 enters the annealing furnace production line along with the end of the strip at the feeding end of the annealing furnace production line;
[0057] The transition section A1 replaces the strip steel on the annealing furnace production line, and introduces the grinding section 2 into the annealing furnace production line, and realizes the grinding of the furnace roller by using the relative displacement between the surface of the grinding section 2 and the surface of the furnace roller;
[0058] The end of the grinding section 2 introduces the transition section B3 into the annealing furnace production line. When the transition section B3 passes through the annealing furnace production line, the working temperature of the annealing furnace production line gradually returns to the production temperature.
[0059] Through the above embodiments, the present application has the following beneficial effects or advantages:
[0060] 1) The length of the transition section A1 in the adjustment material matches the length of the annealing furnace production line. The transition section A1 can completely replace the strip steel on the production line, avoiding the situation where the temperature and tension of the annealing furnace production line change when the grinding section 2 enters the annealing furnace production line, thereby affecting the quality of the strip steel. There is no extra waste of the transition section A1, which reduces material loss and thus reduces the grinding cost of the furnace roller.
[0061] 2) The transition section A1, the grinding section 2 and the transition section B3 are connected in sequence. During the grinding process, only one roll of adjustment material is used to complete the entire grinding work, so as to reduce material loss and shorten the online time of the adjustment material, so as to further reduce the grinding cost of the furnace roller.
[0062] 3) The transition section A1, the grinding section 2 and the transition section B3 are connected in sequence. During the grinding process, the operator only needs to complete the welding of the head end of the transition section A1 with the end of the strip on the annealing furnace production line and the end of the transition section B2 with the head end of the newly put on line strip, which simplifies the process of adjusting the material on line, thereby improving the grinding efficiency.
[0063] Although the preferred embodiments of the present application have been described, those skilled in the art may make other changes and modifications to these embodiments once they have learned the basic creative concept. Therefore, the appended claims are intended to be interpreted as including the preferred embodiments and all changes and modifications that fall within the scope of the present application.
[0064] Obviously, those skilled in the art can make various changes and modifications to the present application without departing from the spirit and scope of the present application. Thus, if these modifications and variations of the present application fall within the scope of the claims of the present application and their equivalents, the present application is also intended to include these modifications and variations.
Claims
1. A regulating material, characterized in that: It comprises a transition section A (1), a grinding section (2) and a transition section B (3); The transition section A (1), the grinding section (2) and the transition section B (3) are connected in sequence; the length of the transition section A (1) matches the length of the annealing furnace production line, and the time for the transition section B (3) to pass through the annealing furnace production line is sufficient to restore the operating temperature of the annealing furnace production line to the production temperature; In the process of grinding the furnace rollers of the annealing furnace, the transition section A (1) is used to replace the strip steel on the annealing furnace production line, and the transition section B (3) is used for the transition of temperature recovery of the annealing furnace production line.
2. The adjusting material according to claim 1, characterized in that The thickness of the transition section A (1) and the thickness of the transition section B (3) both match the thickness of the steel strip processed by the annealing furnace production line.
3. The adjusting material according to claim 1, wherein: When the length of the annealing furnace production line is greater than 400 m, the length of the transition section A(1) is 0-200 m shorter than the length of the annealing furnace production line.
4. The adjustment material according to claim 3, characterized in that The thickness of the transition section A(1) is 0.3-0.4 mm.
5. The adjusting material according to claim 1, wherein: The length of the transition section B (3) is 1-1.5 times the length of the annealing furnace production line.
6. The adjusting material according to claim 5, characterized in that The thickness of the transition section B (3) is 0.3-0.4 mm.
7. The adjusting material according to claim 1, characterized in that The length of the grinding section (2) is 3-4 times the length of the annealing furnace production line.
8. The adjusting material according to claim 7, characterized in that The thickness of the grinding section (2) is 0.5-0.65 mm.
9. The adjusting material according to any one of claims 1 to 8, characterized in that The transition section A (1), the grinding section (2) and the transition section B (3) are integrally formed components, or, The transition section A (1), the grinding section (2) and the transition section B (3) are connected in sequence by welding.
10. An online grinding method for an annealing furnace roller, characterized in that: The method is performed using the adjusting material according to any one of claims 1 to 9, and the method comprises: Obtain the surface condition information of the furnace rollers on the annealing furnace production line; When nodules appear on the surface of the furnace roller, an adjustment material is put on the feeding end of the annealing furnace production line, and the end of the transition section A (1) in the adjustment material away from the grinding section (2) enters the annealing furnace production line along with the end of the strip at the feeding end of the annealing furnace production line; The transition section A (1) replaces the strip steel on the annealing furnace production line, and introduces the grinding section (2) into the annealing furnace production line, and the grinding of the furnace roller is achieved by using the relative displacement between the surface of the grinding section (2) and the surface of the furnace roller; The end of the grinding section (2) away from the transition section A (1) introduces the transition section B (3) into the annealing furnace production line. When the transition section B (3) passes through the annealing furnace production line, the working temperature of the annealing furnace production line gradually returns to the production temperature.
Citation Information
Patent Citations
On-line roll grinding method for carbon jacket hearth roll
CN102776347A
Method for processing furnace roller nodules on line without opening furnace
CN105385836A
Method for relieving accretion degree of furnace roller and conducting after-treatment of accretion of furnace roller
CN109266834A
Method for eliminating nodules on furnace roller
CN113801988A
Device for pre-heating hearth roll in annealing furnace
KR1020040054371A