Novel hydrogen energy source sealing ring mold with edge tearing groove
By introducing the rubber buffer zone and vertical fly break zone into the hydrogen energy sealing ring mold, combining the balance cylinder and mold release assembly, the problems of fly attachment and mold wear in the sealing ring production are solved, and the product pass rate is improved and The mold life improves production efficiency and material utilization.
Patent Information
- Application Number
- CN202411060976.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-05
- Publication Date
- 2024-11-22
AI Technical Summary
During the production process, existing seal ring molds have problems such as easy bonding, low material utilization, complex processing, and acute angle of edge tearing grooves, resulting in low production efficiency and short mold life.
A new type of hydrogen energy sealing ring mold for edge tearing grooves is designed, using a rubber buffer zone and a vertical fly break zone. The thickness of the rubber buffer zone is adjustable, combining a balanced cylinder and a mold release assembly to replace the traditional residual material groove. Enhance the strength of the flash fracture area to achieve air pressure equilibrium and stable mold release.
It improves the pass rate and material utilization rate of sealing ring products, shortens processing time, reduces mold costs, extends mold life, and solves the problems of low production efficiency of traditional molds and mold wear.
Smart Images

Figure CN118990879A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of sealing ring production, in particular to a hydrogen energy sealing ring mould with a novel tear edge groove. Background Art
[0002] Rubber sealing ring products are widely used in various fields due to their simple structure, easy use and maintenance. With the rapid development of the hydrogen energy field, the demand for rubber sealing rings is gradually increasing. However, traditional sealing ring molds are often accompanied by problems such as easy adhesion of products, flash, low material utilization, and complex processing during the production process.
[0003] For example, when demolding, tiny flash is very easy to adhere to the product and is very difficult to remove, resulting in unqualified cleanliness of the product; when discharging, the residual material trough is very easy to separate from the product, resulting in the residual material in the residual material trough needing to be demolded separately, which is inefficient; since the rubber material in the residual material trough does not belong to the product and cannot be reused, it leads to serious waste of rubber material and low utilization rate; in the prior art, the processing cost of the residual material trough accounts for about one tenth of the entire processing cycle, further affecting the efficiency of product production; and the tear edge groove of the product is a sharp angle, which makes the product easy to tear and incomplete, and the mold easy to wear and have a short life. Summary of the invention
[0004] The purpose of the invention is to provide a new hydrogen energy sealing ring mold with a tearing groove.
[0005] The technical problem solved by the present invention is to solve the problem in the prior art that the residual material in the residual material trough needs to be demolded separately, resulting in low production efficiency of rubber sealing ring products.
[0006] The present invention can be implemented through the following technical scheme: a new type of hydrogen energy sealing ring mold with a tearing groove, including an upper mold and a lower mold, the upper mold and the lower mold are cooperatively provided with an edge mechanism for realizing the tearing of the sealing ring, the edge mechanism includes a rubber molding area for realizing rubber molding, and a rubber buffer zone is provided on the side of the rubber molding area for slowing down the molding of the rubber during the flow process, and the thickness of the rubber buffer zone is adjustable.
[0007] A further technical improvement of the present invention is that an adjusting pressing plate is arranged on the rubber buffer zone, the adjusting pressing plate is longitudinally slidably arranged inside the upper mold, and the longitudinal height of the adjusting pressing plate is adjustable.
[0008] A further technical improvement of the present invention is that the adjustment plate is fixedly mounted on the support base, and the support base and the support column are cooperatively arranged, the support column is fixedly mounted on the driving turntable, and the driving turntable is driven by a power mechanism, and the driving turntable is located in the upper mold.
[0009] A further technical improvement of the present invention is that an adjustment groove for achieving gas discharge is provided on the adjustment pressure plate, and a balancing gas pipe is provided on the side of the adjustment groove.
[0010] A further technical improvement of the present invention is that a balancing cylinder is fixed inside the adjustment groove, a balancing pressure plate is arranged at the output end of the balancing cylinder, the balancing pressure plate is in a "T" shape, a limiting plate is fixed at the bottom of the adjustment groove, and the limiting plate and the balancing pressure plate are cooperatively connected.
[0011] A further technical improvement of the present invention is that a vertical flash fracture zone is arranged on the side of the rubber molding zone, and the tearing edge of the vertical flash fracture zone is a vertical edge with a certain width.
[0012] A further technical improvement of the present invention is that a pushing platform is arranged on the adjusting pressing plate, and a demoulding component for realizing the separation of the rubber ring and the adjusting pressing plate is arranged inside the upper mold.
[0013] A further technical improvement of the present invention is that the demoulding assembly includes a disengagement plate, the height of the disengagement plate is adjustable, and the disengagement plate cooperates with the adjustment pressing plate.
[0014] The further technical improvement of the present invention is that the disengagement plate is slidably installed on the output end of the connecting rod, and the disengagement plate and the upper mold are slidably connected, the connecting rod is rotatably installed on the end of the rotating rod, and the rotating rod is rotatably installed inside the upper mold, and the rotating rod and the pushing platform cooperate.
[0015] Compared with the prior art, the present invention has the following beneficial effects:
[0016] 1. The present application provides an edge mechanism for tearing the sealing ring on the upper mold and the lower mold, so that a rubber buffer zone is provided on the side of the rubber molding area for slowing down the molding of the rubber during the flow. In this process, the rubber buffer zone and the rubber molding area replace the original old-style residual material trough, which can solve the problem of low production efficiency caused by the need for separate demolding of the old-style residual material trough. At the same time, the thickness of the rubber buffer zone in the present application is adjustable, and the rubber buffer zone can make the rubber be spread flat, thereby improving the qualified rate of the product, improving the utilization rate of the rubber, shortening the processing time, and reducing the cost of the mold.
[0017] 2. The present application increases the strength of the vertical flash fracture zone by setting the fracture area of the flash at a right angle, so that the tear edge fracture point is forcibly locked between the product cavity and the vertical flash fracture zone, and the increase in the strength of the vertical flash fracture zone greatly improves the mold life.
[0018] 3. The present application utilizes a balancing cylinder to drive the balancing pressure plate to move longitudinally, so that the lowest end of the balancing pressure plate is higher than the highest end of the limiting plate, so that the gas can be discharged from the balancing air pipe, thereby achieving air pressure balance. After the injection is completed, the balancing cylinder is used to push the balancing pressure plate to move longitudinally, so that the lowest end of the balancing pressure plate and the lowest end of the limiting plate are balanced, thereby achieving the closure of the balancing air holes, thereby solving the formation of hole marks in the prior art. BRIEF DESCRIPTION OF THE DRAWINGS
[0019] In order to facilitate understanding by those skilled in the art, the present invention is further described below with reference to the accompanying drawings.
[0020] Figure 1 It is a schematic diagram of the location of the rubber buffer zone of the present invention;
[0021] Figure 2 This is a schematic diagram of the position of the old-style residual material trough area of the present invention;
[0022] Figure 3 It is a schematic diagram of the structure of the adjustment pressing plate of the present invention;
[0023] Figure 4 For the present invention Figure 3 A partial enlarged view of the middle A;
[0024] Figure 5 It is a schematic diagram of the demoulding assembly structure of the present invention.
[0025] In the figure: 1. Glue buffer zone; 2. Vertical flash fracture zone; 3. Glue molding zone; 4. Old-style excess material trough zone; 5. Thin flash easy to strip glue zone; 6. Old-style sharp flash fracture section; 7. Adjustment plate; 8. Support column; 9. Drive turntable; 10. Support base; 11. Adjustment slot; 12. Balance air pipe; 13. Balance cylinder; 14. Balance plate; 15. Limit plate; 16. Rotating rod; 17. Connecting rod; 18. Limit column; 19. Disengagement plate; 20. Limit slide groove; 21. Limit slider; 22. Pushing platform. DETAILED DESCRIPTION
[0026] In order to further explain the technical means and effects adopted by the present invention to achieve the predetermined invention purpose, the specific implementation mode, structure, characteristics and effects of the present invention are described in detail below in combination with the accompanying drawings and preferred embodiments.
[0027] See also Figure 1-5As shown, a new type of hydrogen energy sealing ring mold with a tearing groove includes an upper mold and a lower mold, and a tearing groove structure is provided at the corresponding positions of the upper mold and the lower mold. The upper mold and the lower mold are used to form a processing cavity for the sealing ring to realize the production of the sealing ring, and the tearing groove structure is used to realize the connection and unloading of the sealing ring. Therefore, in the present application, the tearing groove structure includes a vertical flash fracture zone 2, a rubber buffer zone 1 and a rubber molding zone 3. The tearing groove structure is used to form an edge tearing structure for the edge of the sealing ring to replace the traditional tearing groove structure.
[0028] The traditional tearing groove structure includes an old-style sharp-angle flash breaking part 6, and an old-style residual material groove area 4 is connected to the side of the old-style sharp-angle flash breaking part 6 through a thin flash easy-to-remove glue area 5. In this way, the processing cost of the old-style residual material groove area 4 accounts for one tenth of the entire processing cycle, and the tearing groove is in a sharp state, which is very easy to cause loss when the product is torn, causing wear of the mold and affecting the service life of the mold. At the same time, since the residual material groove is connected to the position of the old-style residual material groove area 4 through the thin flash easy-to-remove glue area 5, the old-style residual material groove area 4 needs to be demolded separately when discharging the material, which is inefficient.
[0029] In order to solve the above technical problems, the tear edge groove structure is used in the present application. Specifically, the present application firstly sets a rubber buffer zone 1 and a vertical flash fracture zone 2 on the side of the rubber molding zone 3, and sets the fracture area of the flash of the vertical flash fracture zone 2 to a right angle, thereby increasing the strength of the vertical flash fracture zone 2, so that the tear edge fracture point is forcibly locked between the product cavity and the vertical flash fracture zone 2, and the increase in the strength of the vertical flash fracture zone 2 greatly improves the mold life;
[0030] In the present application, the existence of the rubber buffer zone 1 is utilized to cancel the original old-style residual material groove area 4, thereby improving the demoulding efficiency. The rubber buffer zone 1 can make the rubber be spread flat, thereby improving the product qualification rate, improving the utilization rate of the rubber, shortening the processing time, and reducing the cost of the mold.
[0031] The present application innovatively designs the flash edge fracture area to be a straight surface, thereby increasing the strength of the flash edge fracture area, so that the tear edge fracture point is forcibly locked between the product cavity and the vertical flash edge fracture area 2. And due to the increase in the strength of the vertical flash edge fracture area 2, the mold life is greatly improved. At the same time, the product tearing is solved and the product qualification rate is increased.
[0032] As a further embodiment of the present application, the thickness of the rubber buffer zone 1 in the present application is adjustable, and an innovative tear edge groove rubber buffer zone 1 is provided. The tear edge groove rubber buffer zone 1 is used to slow down the rubber flow process and form rubber. Moreover, since the tear edge groove rubber buffer zone 1 has a certain thickness, the phenomenon of fine flash can be greatly reduced. Moreover, by controlling the thickness of the rubber buffer zone 1, the structure of the old-fashioned residual material groove zone 4 can be replaced, the residual material groove processing process can be reduced, and the utilization rate of the rubber material can be improved.
[0033] As a further embodiment of the present application, in order to control the thickness of the rubber buffer zone 1, the present application uses a control mechanism for control. The control mechanism is located inside the upper mold to control the size of the cavity of the rubber buffer zone 1, thereby being able to control the thickness of the rubber in the rubber buffer zone 1, thereby being able to replace the old-style residual material groove area 4, thereby being able to reduce the processing steps of the residual material groove and improve the utilization rate of the rubber material.
[0034] Therefore, the control mechanism includes an adjusting platen 7 that can move longitudinally, wherein the longitudinal movement of the adjusting platen 7 can adjust the cavity size of the rubber buffer zone 1, so the adjusting platen 7 and the upper mold are slidably connected, and the adjusting platen 7 is installed on a supporting base 10, and a driving device is provided on the supporting base 10 to control the height of the supporting base 10, thereby controlling the height of the adjusting platen 7, and realizing the adjustment of the cavity size of the rubber buffer zone 1.
[0035] Therefore, the driving device includes a driving turntable 9 and support columns 8. A driving motor is fixed inside the upper mold, and the driving motor drives the driving turntable 9, wherein a plurality of groups of support columns 8 are installed on the driving turntable 9, and the support columns 8 are located below the support base 10. The driving motor is used to drive the driving turntable 9 to rotate, so that the support base 10 is longitudinally supported by the support columns 8, thereby controlling the height of the pressure plate 7 to adjust the size of the cavity of the rubber buffer zone 1.
[0036] When the glue is filled, the gas will be discharged. Common pore discharge will form hole marks on the rubber buffer 1, resulting in the breakage of the rubber on the rubber buffer 1 in a thinner state. Therefore, in the present application, a gas pressure buffer component is provided on the adjustment plate 7, and the gas pressure buffer component includes an adjustment groove 11. An adjustment groove 11 is provided on the adjustment plate 7, wherein a limit plate 15 is fixed to the end of the adjustment groove 11, and a balancing air pipe 12 is provided on the side above the limit plate 15, and a balancing cylinder 13 is fixed inside the adjustment groove 11, and a balancing plate 14 is fixed to the output end of the balancing cylinder 13, wherein the balancing plate 14 is slidably connected to the adjustment groove 11, and the balancing plate 14 is T-shaped. The lowest end of the balancing plate 14 cooperates with the limit plate 15. When in use, the balancing cylinder 13 is used to drive the balancing plate 14 to move longitudinally, so that the lowest end of the balancing plate 14 is higher than the highest end of the limit plate 15, so that the gas can be discharged from the balancing air pipe 12, thereby achieving air pressure balance. After the glue injection is completed, the balancing cylinder 13 is used to push the balancing plate 14 to move longitudinally, so that the lowest end of the balancing plate 14 and the lowest end of the limit plate 15 are balanced, thereby achieving the closing of the balancing air hole, thereby solving the formation of hole marks in the prior art.
[0037] When the upper mold and the lower mold are separated, since the rubber buffer zone 1 is thin, the rubber buffer zone 1 adheres to the upper mold, resulting in the rubber buffer zone 1 being broken when the upper mold moves away from the lower mold, causing flying catkins to adhere to the finished product. Therefore, the present application includes a demoulding mechanism, which includes a rotating rod 16, wherein the rotating rod 16 is rotatably installed inside the upper mold, and a connecting rod 17 is rotatably installed at the end of the rotating rod 16, and a limiting slider 21 is fixed at the end of the connecting rod 17, wherein a limiting column 18 is also slidably arranged inside the upper mold, and a separation plate 19 is fixed at the end of the limiting column 18, and a limiting slide groove 20 is slidably arranged on the separation plate 19, and the limiting slide groove 20 and the limiting slide block 21 slide Dynamic connection, a pushing platform 22 for cooperating with the rotating rod 16 is provided on the adjusting pressure plate 7. In the present application, the rotating rod 16 is rotatably installed in the upper mold by a torsion spring. When in use, when the adjusting pressure plate 7 moves longitudinally to the highest end, the rotating rod 16 rotates to overcome the force of the torsion spring. At this time, the end of the connecting rod 17 is pressed downward. At this time, the connecting rod 17 slides under the action of the limiting slide groove 20, so that the disengagement plate 19 is pressed downward onto the rubber buffer zone 1. At this time, the rubber buffer zone 1 and the adjusting pressure plate 7 are separated, thereby avoiding the rubber on the rubber buffer zone 1 from adhering to the adjusting pressure plate 7 and causing tearing. Therefore, the demoulding function with the upper mold can be stably realized in the present application.
[0038] When the present invention is used, the present application firstly uses the side of the rubber molding area 3 to set the rubber buffer zone 1 and the vertical flash fracture zone 2, and uses the flash fracture area of the vertical flash fracture zone 2 to be set at a right angle, thereby increasing the strength of the vertical flash fracture zone 2, so that the tear edge fracture point is forcibly locked between the product cavity and the vertical flash fracture zone 2, and the increase in the strength of the vertical flash fracture zone 2 greatly improves the mold life;
[0039] In the present application, the existence of the rubber buffer zone 1 is utilized to cancel the original old-style residual material groove area 4, thereby improving the demoulding efficiency. The rubber buffer zone 1 can make the rubber be spread flat, thereby improving the product qualification rate, improving the utilization rate of the rubber, shortening the processing time, and reducing the cost of the mold.
[0040] When the thickness of the rubber buffer zone 1 needs to be adjusted, the present application uses a driving motor to drive the rotation of the driving turntable 9, so that the supporting column 8 is used to longitudinally support the supporting base 10, thereby controlling the height of the adjusting plate 7 to achieve the adjustment of the size of the cavity of the rubber buffer zone 1;
[0041] When the air pressure in the space is adjusted, the balancing cylinder 13 is used to drive the balancing plate 14 to move longitudinally, so that the lowest end of the balancing plate 14 is higher than the highest end of the limiting plate 15, so that the gas can be discharged from the balancing air pipe 12, thereby achieving air pressure balance. When the glue injection is completed, the balancing cylinder 13 is used to push the balancing plate 14 to move longitudinally, so that the lowest end of the balancing plate 14 and the lowest end of the limiting plate 15 are balanced, so that the balancing air hole can be closed, thereby solving the formation of hole marks in the prior art;
[0042] Subsequently, during demoulding, when the adjustment pressure plate 7 moves longitudinally to the highest end, the rotating rod 16 rotates to overcome the force of the torsion spring. At this time, the end of the connecting rod 17 is pressed downward. At this time, the connecting rod 17 slides under the action of the limiting slide groove 20, so that the disengagement plate 19 is pressed downward onto the rubber buffer zone 1. At this time, the rubber buffer zone 1 and the adjustment pressure plate 7 are separated, thereby avoiding the tearing caused by the rubber on the rubber buffer zone 1 adhering to the adjustment pressure plate 7. Therefore, the demoulding function with the upper mold can be stably realized in the present application.
[0043] The above description is only a preferred embodiment of the present invention and does not limit the present invention in any form. Although the present invention has been disclosed as a preferred embodiment as above, it is not used to limit the present invention. Any technical personnel in this field can make some changes or modify the technical contents disclosed above into equivalent embodiments without departing from the scope of the technical solution of the present invention. However, any simple modification, equivalent change and modification made to the above embodiments according to the technical essence of the present invention without departing from the content of the technical solution of the present invention still fall within the scope of the technical solution of the present invention.
Claims
1. A new type of hydrogen energy sealing ring mold with tearing edge groove, comprising an upper mold and a lower mold, wherein the upper mold and the lower mold are equipped with an edge mechanism for realizing the tearing edge of the sealing ring. Features: The edge mechanism comprises a rubber molding area (3) for realizing rubber molding, and a rubber buffer area (1) is arranged on the side of the rubber molding area (3) for decelerating the molding of the rubber during the flow process, and the thickness of the rubber buffer area (1) is adjustable.
2. According to claim 1, a new type of hydrogen energy sealing ring mold with tear edge groove, It is characterized in that An adjustment pressing plate (7) is arranged on the rubber buffer zone (1); the adjustment pressing plate (7) is longitudinally slidably arranged inside the upper mold, and the longitudinal height of the adjustment pressing plate (7) is adjustable.
3. According to claim 2, a new type of hydrogen energy sealing ring mold with tear edge groove, It is characterized in that The adjustment plate (7) is fixedly mounted on a support base (10), and the support base (10) and the support column (8) are arranged in coordination, the support column (8) is fixedly mounted on a driving turntable (9), and the driving turntable (9) is driven by a power mechanism, and the driving turntable (9) is located in the upper mold.
4. According to claim 2, a new type of hydrogen energy sealing ring mold with tear edge groove, It is characterized in that The adjustment pressure plate (7) is provided with an adjustment groove (11) for achieving gas discharge, and a balancing gas pipe (12) is provided on the side of the adjustment groove (11).
5. According to claim 4, a new type of hydrogen energy sealing ring mold with tear edge groove, It is characterized in that A balancing cylinder (13) is fixed inside the adjustment groove (11), a balancing pressure plate (14) is arranged at the output end of the balancing cylinder (13), and the balancing pressure plate (14) is in a "T" shape. A limiting plate (15) is fixed at the bottom of the adjustment groove (11), and the limiting plate (15) and the balancing pressure plate (14) are connected in a cooperative manner.
6. A novel hydrogen energy sealing ring mold with tear edge groove according to claim 1, It is characterized in that A vertical flash break zone (2) is arranged on the side of the rubber molding zone (3), and the tearing edge of the vertical flash break zone (2) is a vertical edge with a certain width.
7. According to claim 2, a new type of hydrogen energy sealing ring mold with tear edge groove, It is characterized in that A pushing platform (22) is provided on the adjusting pressing plate (7), and a demoulding component for realizing the separation of the rubber ring and the adjusting pressing plate (7) is provided inside the upper mold.
8. According to claim 7, a new type of hydrogen energy sealing ring mold with tear edge groove, It is characterized in that The demoulding assembly comprises a disengagement plate (19), the height of the disengagement plate (19) is adjustable, and the disengagement plate (19) cooperates with an adjustment pressing plate (7).
9. A novel hydrogen energy sealing ring mold with tear edge groove according to claim 8, It is characterized in that The disengagement plate (19) is slidably mounted on the output end of the connecting rod (17), and the disengagement plate (19) is slidably connected to the upper mold. The connecting rod (17) is rotatably mounted on the end of the rotating rod (16), and the rotating rod (16) is rotatably mounted inside the upper mold. The rotating rod (16) cooperates with the pushing platform (22).
