Blending process of cloud silk
By pretreating and adding reagents in the blending process of cloud silk, negative ion gas is introduced, single and double phase textile and surface wool treatment are used to solve the problem of cloud silk stickiness and improve the breathability and comfort of the product.
Patent Information
- Application Number
- CN202411023944.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-29
- Publication Date
- 2024-11-22
AI Technical Summary
The problem of existing cloud silk being easy to stick and stick during the production process and in the finished product affects its performance.
By pretreating mulberry silk and hot fuse in the blending process, adding appropriate reagents, and introducing negative ion gas during the textile process, using single and double-phase blending method and surface wool treatment to avoid sticking, and using softness The agent and polymeric emulsion are soaked and dried.
It realizes the silky smoothness, breathability and comfort of cloud silk fabrics, avoids sticky problems, and improves the performance of the product.
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of blended spinning of cloud silk, and in particular to a blended spinning process of cloud silk. Background Art
[0002] Yun silk is a high-quality silk variety. It is a filament formed by the liquid secreted by the glands of silkworm pupae after applying tension and subsequent processing. This silk is collected from humid and cold areas such as the Qinling Mountains, Bashan and Shushui. Since the silkworms spin silk for a long time and the silk is flexible, the silk produced is of higher quality. Yun silk is mainly made of silk. Its fibers are fine and uniform, and it feels very comfortable, soft and shiny, with natural light shining through the silk.
[0003] At present, the cloud silk on the market is made of a mixed material of 50% mulberry silk and 50% hot-melt silk. It is the most environmentally friendly mattress material on the market. It has good support and comfort, can effectively relieve human fatigue and improve sleep quality. In addition, the cloud silk mattress also has antibacterial and anti-mite properties, which can effectively inhibit the growth of bacteria and mites, and provide users with a healthy sleeping environment.
[0004] However, at present, many cloud silks have adhesiveness during the production process and in the finished products after production, and are easy to stick and adsorb together. Therefore, an improved technology is urgently needed to solve this problem existing in the prior art. Summary of the invention
[0005] The purpose of the present invention is to provide a cloud silk blending process that will not cause sticking during the blending process and the resulting fabric has both comfort, softness and breathability, so as to solve the problems raised in the above background technology.
[0006] To achieve the above object, the present invention provides the following technical solution: a blending process of cloud silk, the blending process of cloud silk comprising:
[0007] Prepare mulberry silk and hot-melt yarn, pre-treat the mulberry silk, then wash the treated mulberry silk and hot-melt yarn with clean water, add appropriate reagents to the clean water and then dry them;
[0008] After the processing, the cloud silk is arranged in proportion, and the warp and weft of the fabric are mixed and spun with different thread ratios;
[0009] Negative ion gas is introduced during the blending process, and the surface of the fabric after blending is treated with wool sticking;
[0010] The treated fabric is soaked and cleaned with a softener and finally dried before spinning.
[0011] Preferably, the mulberry silk is soaked in clean water at room temperature for 5 minutes, the temperature of the clean water is first heated to 45-50°C, and the mulberry silk is soaked in warm water at 45-50°C for 10 minutes, then the water temperature is heated to 70-75°C, and the mulberry silk is also allowed to stand in water at 70-75°C for 10 minutes, and finally the water temperature is heated to 90°C, and the mulberry silk is allowed to stand in water at 90°C for 1 minute, and then the silk is taken out and washed with distilled water at room temperature.
[0012] Preferably, the reagents added in the blending process of the cloud silk are citric acid: 20-40 g / L, polyethylene glycol 100: 5-10 g / L, softener: 2-5 g / L, antibacterial agent: 1-3 g / L, and penetrant JFC: 1-2 g / L.
[0013] Preferably, in the blending process of the cloud silk, the cloud silk and the hot-melt yarn are configured in a ratio of 3:2, and the cloud silk and the hot-melt yarn are mixed and twisted.
[0014] Preferably, in the blending process of the cloud silk, the warp is double-ply and the weft is single-ply, and the weft is spun in an alternating single-ply and double-ply blending manner.
[0015] Preferably, during the blending process, a rectangular channel is provided on the outside of the cloud silk, and the blended warp and weft threads pass through the channel, and negative ion gas is introduced into the inside of the rectangular channel of the cloud silk blend.
[0016] Preferably, the cloud silk blended yarn is soaked in a softener for 10-15 minutes after being spun, and the softener is a polymer emulsion such as silicone resin.
[0017] Compared with the prior art, the present invention has the following beneficial effects:
[0018] (1) In the blending process of cloud silk, cloud silk and hot-melt yarn are configured in a ratio of 3:2, cloud silk and hot-melt yarn are mixed and twisted, and in the blending process of cloud silk, the warp is double-stranded and the weft is single-stranded, and the single-double blending method is adopted for weaving. In this way, the cloud silk spun is not only smooth, but also has good air permeability;
[0019] (2) During the blending process, a rectangular channel is provided on the outside of the cloud silk, and the warp and weft of the blended yarn pass through the channel. Negative ion gas is introduced into the inside of the rectangular channel of the cloud silk blended yarn. After the blending is completed, the surface of the fabric is treated with a hair-sticking treatment. The negative ion gas can remove the static ions generated by the friction of the fabric, so that the cloud silk material does not stick during the blending process;
[0020] (3) The blending process of the cloud silk is simple, and no sticking occurs during the blending process. The resulting fabric is comfortable, soft, and breathable. DETAILED DESCRIPTION
[0021] The following will be combined with the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0022] The present invention provides a technical solution: a blending process of cloud silk, the blending process of cloud silk comprising:
[0023] Prepare mulberry silk and hot-melt silk, and pre-treat the mulberry silk. Soak the mulberry silk in clean water at room temperature for 5 minutes. First, heat the temperature of the clean water to 45-50℃, and let the mulberry silk stay in the warm water at 45-50℃ for 10 minutes. Then, heat the water temperature to 70-75℃, and let the mulberry silk stand in the water at 70-75℃ for 10 minutes. Finally, heat the water temperature to 90℃, let the mulberry silk stand in the water at 90℃ for 1 minute, and take out and wash it with distilled water at room temperature.
[0024] The processed mulberry silk and hot-melt silk are then washed with clean water. During the washing process, appropriate reagents are added to the clean water and then dried. The reagents added in the blending process of Yun silk are citric acid: 20-40g / L, polyethylene glycol 100: 5-10g / L, softener: 2-5g / L, antibacterial agent: 1-3g / L, and penetrant JFC: 1-2g / L.
[0025] After the processing, the cloud silk is configured according to the proportion. In the blending process of cloud silk, cloud silk and hot melt silk are configured in a ratio of 3:2, and the warp and weft of the fabric are mixed and spun with different thread strand ratios. In the blending process of cloud silk, cloud silk and hot melt silk are configured in a ratio of 3:2. Cloud silk and hot melt silk are mixed and twisted. In the blending process of cloud silk, the warp is double-stranded and the weft is single-stranded, and the weft is spun in a single-double alternating blending method. The cloud silk spun in this way is not only silky, but also has good breathability.
[0026] Negative ion gas is introduced into the cloud silk during the blending process. A rectangular channel is set outside the cloud silk during the blending process. The warp and weft of the blended silk pass through the channel, and negative ion gas is introduced into the inside of the rectangular channel of the cloud silk blended silk. After the blending is completed, the surface of the fabric is treated with wool sticking. The negative ion gas can remove the static electricity ions generated by the friction of the fabric, so that the cloud silk material will not be sticky during the blending process.
[0027] The treated fabric is soaked and cleaned with softener. After the cloud silk blend is completed, it is soaked in softener for 10-15 minutes. The softener is a high molecular polymer emulsion such as silicone resin. The softened fabric is washed with clean water 2-3 times. After washing, the fabric is first hung to drain, and then dehydrated with a high-speed rotation dehydrator. Finally, it is dried to complete the weaving of cloud silk.
[0028] Embodiment 1,
[0029] Prepare mulberry silk and hot melt silk, and pre-treat the mulberry silk. Soak the mulberry silk in clean water at room temperature for 5 minutes. First, heat the clean water to 46°C, and let the mulberry silk stay in the warm water at 46°C for 10 minutes. Then heat the water to 72°C, and let the mulberry silk stand in the water at 72°C for 10 minutes. Finally, heat the water to 90°C, let the mulberry silk stand in the water at 90°C for 1 minute, and take it out and wash it with distilled water at room temperature. Then wash the treated mulberry silk and hot melt silk with clean water, and add appropriate reagents to the clean water during washing and dry it.
[0030] After the processing, the cloud silk is configured according to the proportion. In the blending process of cloud silk, cloud silk and hot-melt silk are configured in a ratio of 3:2, and the warp and weft of the fabric are mixed and spun with different thread strand ratios. In the blending process of cloud silk, cloud silk and hot-melt silk are configured in a ratio of 3:2. Cloud silk and hot-melt silk are mixed and twisted. In the blending process of cloud silk, the warp is double-stranded and the weft is single-stranded, and the weft is spun in a single-double alternating blending method.
[0031] Embodiment 2,
[0032] Prepare mulberry silk and hot-melt silk, and pre-treat the mulberry silk. Soak the mulberry silk in clean water at room temperature for 5 minutes. First, heat the temperature of the clean water to 47°C, and let the mulberry silk stay in the warm water at 47°C for 10 minutes. Then, heat the water temperature to 73°C, and let the mulberry silk stand in the water at 73°C for 10 minutes. Finally, heat the water temperature to 90°C, let the mulberry silk stand in the water at 90°C for 1 minute, and take out and wash it with distilled water at room temperature.
[0033] The processed mulberry silk and hot-melt yarn are then washed with clean water, and appropriate reagents are added to the clean water for drying.
[0034] After the processing, the cloud silk is configured according to the proportion. In the blending process of cloud silk, cloud silk and hot-melt silk are configured in a ratio of 3:2, and the warp and weft of the fabric are mixed and spun with different thread strand ratios. In the blending process of cloud silk, cloud silk and hot-melt silk are configured in a ratio of 3:2. Cloud silk and hot-melt silk are mixed and twisted. In the blending process of cloud silk, the warp is double-stranded and the weft is single-stranded, and the weft is spun in a single-double alternating blending method.
[0035] Embodiment 3,
[0036] Prepare mulberry silk and hot-melt silk, and pre-treat the mulberry silk. Soak the mulberry silk in clean water at room temperature for 5 minutes. First, heat the temperature of the clean water to 48°C, and let the mulberry silk stay in the warm water at 48°C for 10 minutes. Then, heat the water temperature to 74°C, and let the mulberry silk stand in the water at 74°C for 10 minutes. Finally, heat the water temperature to 90°C, let the mulberry silk stand in the water at 90°C for 1 minute, and take out and wash it with distilled water at room temperature.
[0037] The processed mulberry silk and hot-melt yarn are then washed with clean water, and appropriate reagents are added to the clean water for drying.
[0038] After the processing, the cloud silk is configured according to the proportion. In the blending process of cloud silk, cloud silk and hot-melt silk are configured in a ratio of 3:2, and the warp and weft of the fabric are mixed and spun with different thread strand ratios. In the blending process of cloud silk, cloud silk and hot-melt silk are configured in a ratio of 3:2. Cloud silk and hot-melt silk are mixed and twisted. In the blending process of cloud silk, the warp is double-stranded and the weft is single-stranded, and the weft is spun in a single-double alternating blending method.
[0039] Embodiment 4,
[0040] Prepare mulberry silk and hot-melt silk, and pre-treat the mulberry silk. Soak the mulberry silk in clean water at room temperature for 5 minutes. First, heat the temperature of the clean water to 50°C, and let the mulberry silk stay in the warm water at 50°C for 10 minutes. Then, heat the water temperature to 75°C, and let the mulberry silk stand in the water at 75°C for 10 minutes. Finally, heat the water temperature to 90°C, let the mulberry silk stand in the water at 90°C for 1 minute, and take out and wash it with distilled water at room temperature.
[0041] The processed mulberry silk and hot-melt yarn are then washed with clean water, and appropriate reagents are added to the clean water for drying.
[0042] After the processing, the cloud silk is configured according to the proportion. In the blending process of cloud silk, cloud silk and hot-melt silk are configured in a ratio of 3:2, and the warp and weft of the fabric are mixed and spun with different thread strand ratios. In the blending process of cloud silk, cloud silk and hot-melt silk are configured in a ratio of 3:2. Cloud silk and hot-melt silk are mixed and twisted. In the blending process of cloud silk, the warp is double-stranded and the weft is single-stranded, and the weft is spun in a single-double alternating blending method.
[0043] By controlling the cloud silk thread at different temperatures, the strength of the cloud silk processed at different temperatures is different. When the mulberry silk in the cloud silk is soaked in clean water at room temperature for 5 minutes, the temperature of the clean water is first heated to 48°C, and the mulberry silk is soaked in warm water at 48°C for 10 minutes, then the water temperature is heated to 74°C, and the mulberry silk is also allowed to stand in water at 74°C for 10 minutes, and finally the water temperature is heated to 90°C, and the mulberry silk is allowed to stand in water at 90°C for 1 minute, and then taken out and washed with distilled water at room temperature. The overall tensile properties and comprehensive index of softness of the cloud silk processed under this temperature environment are the best.
[0044] The blending process of cloud silk is simple, and there will be no sticking during the blending process. The resulting fabric is comfortable, soft and breathable.
[0045] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.
Claims
1. A blending process of cloud silk, characterized by: The blending process of the cloud silk includes: Prepare mulberry silk and hot-melt yarn, pre-treat the mulberry silk, then wash the treated mulberry silk and hot-melt yarn with clean water, add appropriate reagents to the clean water and then dry them; After the processing, the cloud silk is arranged in proportion, and the warp and weft of the fabric are mixed and spun with different thread ratios; Negative ion gas is introduced during the blending process, and the surface of the fabric after blending is treated with wool sticking; The treated fabric is soaked and cleaned with a softener and finally dried before spinning.
2. The blending process of cloud silk according to claim 1, characterized in that: The mulberry silk is soaked in clean water at room temperature for 5 minutes, the temperature of the clean water is first heated to 45-50°C, and the mulberry silk is soaked in warm water at 45-50°C for 10 minutes, then the water temperature is heated to 70-75°C, and the mulberry silk is also allowed to stand in water at 70-75°C for 10 minutes, and finally the water temperature is heated to 90°C, and the mulberry silk is allowed to stand in water at 90°C for 1 minute, and then the silk is taken out and cleaned with distilled water at room temperature.
3. The blending process of cloud silk according to claim 1, characterized in that: The reagents added in the blending process of the cloud silk are citric acid: 20-40 g / L, polyethylene glycol 100: 5-10 g / L, softener: 2-5 g / L, antibacterial agent: 1-3 g / L, and penetrant JFC: 1-2 g / L.
4. The blending process of cloud silk according to claim 1, characterized in that: In the blending process of the cloud silk, the cloud silk and the hot-melt yarn are configured in a ratio of 3:2, and the cloud silk and the hot-melt yarn are mixed and twisted.
5. The blending process of cloud silk according to claim 1, characterized in that: In the blended spinning process of the cloud silk, the warp is double-ply and the weft is single-ply, and the weft is spun in a blended spinning method of alternating single and double strands.
6. The blending process of cloud silk according to claim 1, characterized in that: During the blending process of the cloud silk, a rectangular channel is provided on the outside, and the blended warp and weft threads pass through the channel, and negative ion gas is introduced into the inside of the rectangular channel of the cloud silk blend.
7. The blending process of cloud silk according to claim 1, characterized in that: After the cloud silk blending is completed, it is soaked in a softener for 10-15 minutes. The softener is a high molecular polymer emulsion such as silicone resin.
Citation Information
Patent Citations
White steam filature yarn pre-treatment technology before production
CN104451897A
Low-melting-point polyester composite fabric
CN107227543A
Silk scarf with surface brightening treatment
CN110623348A
Mulberry silk soft water treatment process
CN117211061A
Industrial textile machine capable of tightening yarns
CN218291225U