Safety nondestructive monitoring method suitable for assembly type engineering connection node

By wrapping copper wires around the sleeve and reinforcing bars and measuring the resistance value, the problem of non-destructive testing of grouting sleeves has been solved, realizing efficient and low-cost testing of grouting sleeves and accurately determining their fullness and service condition.

CN119000798APending Publication Date: 2024-11-22HUBEI UNIV OF TECH
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411191485.7
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-28
Publication Date
2024-11-22

AI Technical Summary

Technical Problem

Existing technologies cannot effectively perform non-destructive testing of grouting sleeves, especially in accurately determining the grouting fullness and service condition. Furthermore, traditional testing methods suffer from problems such as high destructiveness, high cost, and complex operation.

Method used

Copper wires are wound around the outer surface of the sleeve and the top of the reinforcing bar, and fixed with conductive adhesive. The fullness and service condition of the grouting sleeve are judged by measuring the resistance value of the grouting material. Non-destructive testing is carried out using self-sensing grouting material.

Benefits of technology

It enables non-destructive testing of grouting sleeves, reduces testing costs, improves testing efficiency, accurately determines grouting fullness and service status, and is easy to operate.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119000798A_ABST
    Figure CN119000798A_ABST
Patent Text Reader

Abstract

The invention relates to the technical field of assembly type construction engineering, and discloses a safety nondestructive monitoring method suitable for an assembly type engineering connection node, which comprises the following steps: winding a copper wire on the outer surface of a sleeve, winding the copper wire on the top end of a steel bar, reinforcing the copper wire by using a conductive adhesive, and performing thermal insulation on the copper wire; a grouting material is injected into the sleeve through the grouting opening, and a universal meter is used for measuring a resistance measured value Rmeasured 1 of the grouting material after the grouting material is mixed for 30 min and a resistance measured value Rmeasured 2 of the grouting material at the age of 28 d; and calculating a resistance calculation value R < 1 > after mixing for 30 minutes and a resistance calculation value R < 2 > at the age of 28 days according to the radius H1 of the reinforcing steel bar, the radius H2 of the inner wall of the sleeve and the resistivity rho < 1 > and the resistivity rho < 2 > of the grouting material. According to the safety nondestructive monitoring method suitable for the assembly type engineering connection node, the electric conduction copper wire is pre-buried for resistance detection of the grouting sleeve, nondestructive detection of the plumpness and the service state of the sleeve can be achieved, the manual detection cost is reduced, and trouble and labor are saved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of prefabricated construction engineering, and in particular to a safety non-destructive monitoring method suitable for connection nodes of prefabricated engineering. Background Art

[0002] As a product of the development of the construction industry, prefabricated buildings have great development prospects in the current green and low-carbon transformation and sustainable development. The steel connection between prefabricated components is an important factor in the quality stability of prefabricated building projects and a technical difficulty of prefabricated buildings. In recent years, many studies have been conducted on steel bar connections, mainly including steel bar lap splicing bolt connection, steel bar slurry anchor connection, grouting sleeve connection, etc. Grouting sleeve connection is a more reliable component connection method with better seismic resistance. The performance of sleeve grouting connection is a hot issue in the field of prefabricated structures. In order to ensure the safety of building structures, it is necessary to detect and monitor the service status of grouting sleeve connection nodes. However, the inspection of grouting sleeves is concealed, and the fullness of grouting sleeves cannot be effectively checked. In addition, there are few means to detect the service status of grouting sleeves and they have defects. At present, the fullness test methods of sleeve grouting are mainly divided into two categories: destructive testing and non-destructive testing.

[0003] The traditional destructive testing method is to destroy the outer concrete and sleeve to observe the fullness of the internal grouting material. Although this method is intuitive, it damages the structure and weakens the safety of the building. Non-destructive testing methods mainly include ultrasonic method, X-ray method, endoscopic detection method, etc. These methods are highly applicable in the detection process of prefabricated buildings, but they also have certain defects. Among them, the ultrasonic method uses the propagation path of ultrasonic waves in the grouting sleeve to propagate along the radial direction of the sleeve. The density of the sleeve is detected according to the sound velocity and amplitude parameters measured by the ultrasonic first wave acoustic time method. However, this detection method cannot determine the specific location of the void defect. As the fullness of the grouting material in the sleeve decreases, the mean sound velocity decreases and the deviation coefficient increases; X-ray technology uses rays to penetrate the inspected sleeve, and reflects the defects inside the sleeve through the attenuation and distribution law of the ray photons. The film imaging quality is not high and the definition is low. It is not suitable for thickness > 200 The detection of the fullness of the sleeve grouting of mm is not suitable for the detection of the sleeve grouting defects of the double-row arrangement. At the same time, there are problems such as high cost, complicated operation, and certain harm to the human body. The pre-hole endoscope detection method is a repeatable, high-precision, qualitative and quantitative non-destructive detection method, but this method has problems such as difficult hole positioning, high detection time requirements, and cannot be used on a large scale. The Chinese patent document with publication number CN109959683A proposes a method to detect the grouting fullness of the steel bar connection sleeve by measuring the resistance value with a pre-embedded probe around the sleeve. Its essence is to use the steel bars at both ends of the sleeve, the pre-embedded probes distributed around the sleeve, and the grouting port and overflow port to carry out resistance measurements between the connected steel bars, between each steel bar and the pre-embedded probes on the surrounding sleeve, the grouting port or overflow port, between the pre-embedded probes on the upper part of the sleeve, and between the pre-embedded probes on the upper part of the sleeve and the grouting port or overflow port, and compare them with the resistance value when the conductive slurry is continuous and has no obvious defects. This detection method requires the pre-embedded probe to be placed in the grouting material for detection, which causes certain damage to the grouting material. In addition, this detection method cannot determine the service status of the subsequent grouting material, so a safety non-destructive monitoring method suitable for prefabricated engineering connection nodes is proposed to solve the above problems. Summary of the invention

[0004] In view of the shortcomings of the prior art, the present invention provides a safety non-destructive monitoring method suitable for connection nodes of prefabricated projects, which has the characteristics of low detection cost, simple operation, fast detection speed and high efficiency. At the same time, it can make accurate judgments on the grouting fullness and service status, and solves the problems mentioned in the above background technology.

[0005] To achieve the above object, the present invention provides the following technical solution: a safety non-destructive monitoring method applicable to assembly engineering connection nodes, comprising the following steps: S1: Wrap the copper wire around the outer surface of the sleeve and the top of the steel bar, and use conductive glue to reinforce the copper wire; S2: inject grouting material into the sleeve through the grouting port; S3: Use a multimeter to measure the actual resistance value R of the grouting material after mixing for 30 minutes 测1 And the measured resistance value R at 28 days 测2 ; S4: Calculate the resistance value R after mixing for 30 minutes by using the radius H1 of the steel bar, the radius H2 of the inner wall of the sleeve, and the resistivity ρ1 and resistivity ρ2 of the grouting material. 计1 And the calculated resistance value R at 28 days 计2 ; S5: The measured resistance value R after 30 minutes of mixing 测1 and the calculated resistance value R 计1 The ratio A1 of the grouting material is used to analyze the fullness of the grouting material. The measured resistance value R at the age of 28 days is 测2 and the calculated resistance value R 计2 The ratio A2 is used to analyze the service status of the grouting material.

[0006] Preferably, the sleeve is a fully grouted sleeve formed by machine tool processing or extrusion, the sleeve is made of steel, the top and bottom ends of the sleeve are provided with insulating sealing rings, the insulating sealing rings are connected to the sleeve by grouting, and one end of the sleeve is provided with a grout outlet.

[0007] Preferably, the grouting material is a self-sensing grouting material, which is a cement-based grouting material modified with a conductive filler. The compressive strength of the grouting material at 28 days of age is greater than 85 MPa, and the resistivity change rate is greater than or equal to 35%.

[0008] Preferably, the method for measuring the resistivity ρ1 and the resistivity ρ2 of the grouting material in step S4 is: S4.1: Inject the grouting material into the insulation mold and place two stainless steel meshes in the grouting material; S4.2: Use a multimeter to measure the resistance value Z1 of the grouting material after mixing for 30 minutes; S4.3: After curing the grouting material for 1 day, remove the mold, seal and cure for 28 days, and use the multimeter to measure the resistance value Z2 of the grouting material again; S4.4: Calculate the resistivity ρ1 of the grouting material after mixing for 30 minutes using the expression: ρ1=Z1S / L Where S is the cross-sectional area of ​​the specimen, and L is the distance between the two stainless steel meshes; S4.5: Calculate the resistivity ρ2 of the grouting material after 28 days of curing, using the expression: ρ2=Z2S / L Where S is the cross-sectional area of ​​the specimen, and L is the distance between the two stainless steel meshes.

[0009] Preferably, the size of the insulating mold is 40mm*40mm*160mm, the mesh size of the stainless steel mesh is no larger than 0.5mm, and the distance between two stainless steel meshes is 100mm.

[0010] Preferably, the calculated resistance value R 计1 The expression is: Among them, Q is the total length of the sleeve; The calculated resistance value R 计2 The expression is: Among them, Q is the total length of the sleeve.

[0011] Preferably, the fullness expression is: The service status expression is: Compared with the prior art, the present invention provides a safety non-destructive monitoring method applicable to assembly engineering connection nodes, which has the following beneficial effects: 1. This nondestructive safety monitoring method for connection nodes of prefabricated projects can realize nondestructive testing of the fullness and service status of the sleeve by pre-buried conductive copper wire for resistance detection of the grouting sleeve, reducing the cost of manual testing and saving time and effort.

[0012] 2. This nondestructive safety monitoring method for prefabricated engineering connection nodes can qualitatively and quantitatively analyze the fullness and service status of the grouting sleeve by comparing the measured resistance value with the calculated value. It is easy to operate, has high detection efficiency and low detection cost, and can be widely promoted and used. BRIEF DESCRIPTION OF THE DRAWINGS

[0013] Figure 1 A schematic diagram of the resistance detection of the steel grouting sleeve of a safety non-destructive monitoring method for prefabricated engineering connection nodes proposed by the present invention; Figure 2 This is a schematic diagram of resistivity testing of a nondestructive safety monitoring method for connection nodes of prefabricated projects proposed in the present invention.

[0014] In the figure: 1 sleeve, 2 steel bars, 3 grouting material, 4 grouting port, 5 grouting outlet, 6 multimeter, 7 conductive glue, 8 copper wire, 9 insulating sealing ring, 10 insulating mold, 11 stainless steel mesh. DETAILED DESCRIPTION

[0015] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0016] Example 1: Please refer to Figure 1-2 A nondestructive safety monitoring method for assembly engineering connection nodes includes the following steps: S1: Wrap the copper wire 8 around the outer surface of the sleeve 1 and the top of the steel bar 2, and use the conductive glue 7 to reinforce the copper wire 8. The inner diameter of the sleeve 1 is 0.39m, the total length of the inner wall is 0.46m, and the radius of the steel bar 2 is 0.006m; S2: injecting a grouting material 3 into the sleeve 1 through the grouting port 4, wherein the grouting material 3 is a self-sensing grouting material of carbon nanotubes; S3: Use multimeter 6 to measure the actual resistance value R of grouting material 3 after grouting material 3 is mixed for 30 minutes 测1The measured resistance value R is 4.334 kΩ and the age is 28 days 测2 14.744kΩ; S4: Calculate the resistance value R after mixing for 30 minutes by using the radius H1 of the steel bar 2, the inner wall radius H2 of the sleeve 1, and the resistivity ρ1 and resistivity ρ2 of the grouting material 3. 计1 And the calculated resistance value R at 28 days 计2,电阻计算值R计1 The calculated resistance value R is 3.704 kΩ. 计2为4.64kΩ; S5: The measured resistance value R after 30 minutes of mixing 测1 and the calculated resistance value R 计1 The ratio A1 is 1.17. The fullness of grouting material 3 is analyzed by measuring the resistance value R at the age of 28 days. 测2 and the calculated resistance value R 计2的比值A2 It is 2.48, analyzing the service status of grouting material 3.

[0017] The sleeve 1 is a fully grouted sleeve formed by machine tool processing or extrusion. The sleeve 1 is made of steel. The top and bottom of the sleeve 1 are both provided with insulating sealing rings 9, which are connected to the sleeve 1 through grouting. One end of the sleeve 1 is provided with a grouting outlet 5. The grouting material 3 is a self-sensing grouting material, which is a cement-based grouting material modified with conductive fillers. The compressive strength of the grouting material 3 at 28 days is greater than 85 MPa, and the resistivity change rate is 35.05%.

[0018] Secondly, the method for measuring the resistivity ρ1 and the resistivity ρ2 of the grouting material 3 in step S4 is: S4.1: inject the grouting material 3 into the insulating mold 10, and place two stainless steel meshes 11 in the grouting material 3; S4.2: Use a multimeter 6 to measure the resistance value Z1 of the grouting material 3 after mixing for 30 minutes, which is 9.6481 kΩ; S4.3: After curing the grouting material 3 for 1 day, the mold is removed, and after sealing and curing for 28 days, the resistance value Z2 of the grouting material 3 is 12.1044 kΩ using the multimeter 6 again; S4.4: Calculate the resistivity ρ1 of grouting material 3 after mixing for 30 minutes, which is 1.5437 kΩ.m. The expression is: ρ1=Z1S / L Wherein, S is the cross-sectional area of ​​the specimen, and L is the distance between the two stainless steel meshes 11; S4.5: The resistivity ρ2 of grouting material 3 after curing for 28 days is calculated to be 1.9367 kΩ.m, expressed as: ρ2=Z2S / L Wherein, S is the cross-sectional area of ​​the specimen, and L is the distance between the two stainless steel meshes 11 .

[0019] The size of the insulating mold 10 is 40mm*40mm*160mm, the mesh size of the stainless steel mesh 11 is no larger than 0.5mm, and the distance between the two stainless steel meshes 11 is 100mm.

[0020] Calculated resistance value R 计1 The expression is: Wherein, Q is the total length of sleeve 1; Calculated resistance value R 计2 The expression is: Wherein, Q is the total length of the sleeve 1.

[0021] The expression of fullness is: The service status expression is: Example 2: Please refer to Figure 1-2 A nondestructive safety monitoring method for assembly engineering connection nodes includes the following steps: S1: Wrap the copper wire 8 around the outer surface of the sleeve 1 and the top of the steel bar 2, and use the conductive glue 7 to reinforce the copper wire 8. The inner diameter of the sleeve 1 is 0.39m, the total length of the inner wall is 0.46m, and the radius of the steel bar 2 is 0.006m; S2: injecting grouting material 3 into the sleeve 1 through the grouting port 4, the grouting material 3 is carbon nanotubes and steel fibers; S3: Use multimeter 6 to measure the actual resistance value R of grouting material 3 after grouting material 3 is mixed for 30 minutes 测1 The measured resistance value R is 4.380 kΩ and the age is 28 days 测2 14.744kΩ; S4: Calculate the resistance value R after mixing for 30 minutes by using the radius H1 of the steel bar 2, the inner wall radius H2 of the sleeve 1, and the resistivity ρ1 and resistivity ρ2 of the grouting material 3. 计1 And the calculated resistance value R at 28 days 计2, Calculated resistance value R 计1 The calculated resistance value R is 3.261 kΩ. 计2 4.37kΩ; S5: The measured resistance value R after 30 minutes of mixing 测1 and the calculated resistance value R 计1 The ratio A1 is 1.23. The fullness of grouting material 3 is analyzed by measuring the resistance value R at the age of 28 days. 测2 and the calculated resistance value R 计2的比值A2It is 3.37, analyzing the service status of grouting material 3.

[0022] The sleeve 1 is a fully grouted sleeve formed by machine tool processing or extrusion. The sleeve 1 is made of steel. The top and bottom of the sleeve 1 are both provided with insulating sealing rings 9, which are connected to the sleeve 1 through grouting. One end of the sleeve 1 is provided with a grouting outlet 5. The grouting material 3 is a self-sensing grouting material, which is a cement-based grouting material modified with conductive fillers. The compressive strength of the grouting material 3 at 28 days is greater than 85 MPa, and the resistivity change rate is 39.04%.

[0023] Secondly, the method for measuring the resistivity ρ1 and the resistivity ρ2 of the grouting material 3 in step S4 is: S4.1: inject the grouting material 3 into the insulating mold 10, and place two stainless steel meshes 11 in the grouting material 3; S4.2: Use a multimeter 6 to measure the resistance value Z1 of the grouting material 3 after mixing for 30 minutes, which is 9.275 kΩ; S4.3: After curing the grouting material 3 for 1 day, the mold is removed, and after sealing and curing for 28 days, the resistance value Z2 of the grouting material 3 is 11.375 kΩ using the multimeter 6 again; S4.4: Calculate the resistivity ρ1 of grouting material 3 after mixing for 30 minutes, which is 1.484 kΩ.m. The expression is: ρ1=Z1S / L Wherein, S is the cross-sectional area of ​​the specimen, and L is the distance between the two stainless steel meshes 11; S4.5: The resistivity ρ2 of grouting material 3 after curing for 28 days is calculated to be 1.820 kΩ.m, expressed as: ρ2=Z2S / L Wherein, S is the cross-sectional area of ​​the specimen, and L is the distance between the two stainless steel meshes 11 .

[0024] The size of the insulating mold 10 is 40mm*40mm*160mm, the mesh size of the stainless steel mesh 11 is no larger than 0.5mm, and the distance between the two stainless steel meshes 11 is 100mm.

[0025] Calculated resistance value R 计1 The expression is: Wherein, Q is the total length of sleeve 1; Calculated resistance value R 计2 The expression is: Wherein, Q is the total length of the sleeve 1.

[0026] The expression of fullness is: The service status expression is: Example 3: Please refer to Figure 1-2 A nondestructive safety monitoring method for assembly engineering connection nodes includes the following steps: S1: Wrap the copper wire 8 around the outer surface of the sleeve 1 and the top of the steel bar 2, and use the conductive glue 7 to reinforce the copper wire 8. The inner diameter of the sleeve 1 is 0.39m, the total length of the inner wall is 0.46m, and the radius of the steel bar 2 is 0.006m; S2: injecting grouting material 3 into the sleeve 1 through the grouting port 4, the grouting material 3 is carbon black and steel fiber; S3: Use multimeter 6 to measure the actual resistance value R of grouting material 3 after grouting material 3 is mixed for 30 minutes 测1 The measured resistance value R is 5.784 kΩ and the age is 28 days 测2 20.16kΩ; S4: Calculate the resistance value R after mixing for 30 minutes by using the radius H1 of the steel bar 2, the inner wall radius H2 of the sleeve 1, and the resistivity ρ1 and resistivity ρ2 of the grouting material 3. 计1 And the calculated resistance value R at 28 days 计2,电阻计算值R计1 The calculated resistance value R is 3.989 kΩ. 计2为4.80kΩ; S5: The measured resistance value R after 30 minutes of mixing 测1 and the calculated resistance value R 计1 The ratio A1 is 1.45. The fullness of grouting material 3 is analyzed by measuring the resistance value R at the age of 28 days. 测2 and the calculated resistance value R 计2的比值A2 4.2, analyze the service status of grouting material 3.

[0027] The sleeve 1 is a fully grouted sleeve formed by machine tool processing or extrusion. The sleeve 1 is made of steel. The top and bottom of the sleeve 1 are both provided with insulating sealing rings 9, which are connected to the sleeve 1 through grouting. One end of the sleeve 1 is provided with a grouting outlet 5. The grouting material 3 is a self-sensing grouting material, which is a cement-based grouting material modified with conductive fillers. The compressive strength of the grouting material 3 at 28 days is greater than 85 MPa, and the resistivity change rate is 39.02%.

[0028] Secondly, the method for measuring the resistivity ρ1 and the resistivity ρ2 of the grouting material 3 in step S4 is: S4.1: inject the grouting material 3 into the insulating mold 10, and place two stainless steel meshes 11 in the grouting material 3; S4.2: Use a multimeter 6 to measure the resistance value Z1 of the grouting material 3 after mixing for 30 minutes, which is 10.3875 kΩ; S4.3: After curing the grouting material 3 for 1 day, the mold is removed, and after sealing and curing for 28 days, the resistance value Z2 of the grouting material 3 is 12.4875 kΩ using the multimeter 6 again; S4.4: Calculate the resistivity ρ1 of grouting material 3 after mixing for 30 minutes, which is 1.662 kΩ.m. The expression is: ρ1=Z1S / L Wherein, S is the cross-sectional area of ​​the specimen, and L is the distance between the two stainless steel meshes 11; S4.5: The resistivity ρ2 of grouting material 3 after curing for 28 days is calculated to be 1.998 kΩ.m, expressed as: ρ2=Z2S / L Wherein, S is the cross-sectional area of ​​the specimen, and L is the distance between the two stainless steel meshes 11 .

[0029] The size of the insulating mold 10 is 40mm*40mm*160mm, the mesh size of the stainless steel mesh 11 is no larger than 0.5mm, and the distance between the two stainless steel meshes 11 is 100mm.

[0030] Calculated resistance value R 计1 The expression is: Wherein, Q is the total length of sleeve 1; Calculated resistance value R 计2 The expression is: Wherein, Q is the total length of the sleeve 1.

[0031] The expression of fullness is: The service status expression is: The data of Examples 1 to 3 were compared and analyzed. The measured resistance value R at the end of grouting was 测1 and the calculated resistance value R 计1 The ratio A1 is used to analyze whether the grouting material is full, and the measured resistance value R at any age after 28 days of grouting is calculated. 测2与电阻计算值R计2 The ratio A 2进行分析判断其服役状态,结果见表2。 Table 2 In summary, this safety nondestructive monitoring method applicable to prefabricated engineering connection nodes can realize nondestructive testing of sleeve fullness and service status by pre-buried conductive copper wire for resistance detection of grouting sleeve, thus reducing manual testing costs and saving time and effort. Moreover, by comparing the measured resistance value with the calculated value, the fullness and service status of the grouting sleeve can be qualitatively and quantitatively analyzed. The operation is convenient, the detection efficiency is high, the detection cost is low, and it can be widely promoted and used.

[0032] It should be noted that the terms "include", "comprises" or any other variations thereof are intended to cover non-exclusive inclusion, so that a process, method, article or device including a series of elements includes not only those elements, but also other elements not explicitly listed, or also includes elements inherent to such process, method, article or device. In the absence of further restrictions, an element defined by the sentence "comprises a ..." does not exclude the existence of other identical elements in the process, method, article or device including the element.

[0033] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.

Claims

1. A non-destructive safety monitoring method for assembly engineering connection nodes, characterized in that: The following steps are involved: S1: Wrap the copper wire (8) around the outer surface of the sleeve (1) and the top of the steel bar (2), and use conductive glue (7) to reinforce the copper wire (8); S2: injecting grouting material (3) into the sleeve (1) through the grouting port (4); S3: Use a multimeter (6) to measure the actual resistance value R of the grouting material (3) after the grouting material (3) has been mixed for 30 minutes. 测1 And the measured resistance value R at 28 days 测2 ; S4: Calculate the resistance value R after mixing for 30 minutes by using the radius H1 of the steel bar (2), the inner wall radius H2 of the sleeve (1) and the resistivity ρ1 and resistivity ρ2 of the grouting material (3). 计1 And the calculated resistance value R at 28 days 计2; S5: The measured resistance value R after 30 minutes of mixing 测1 and the calculated resistance value R 计1 The ratio A1 of the grouting material (3) is used to analyze the fullness of the grouting material. The measured resistance value R at the age of 28 days is 测2 and the calculated resistance value R 计2的比值A2 Analyze the service status of the grouting material (3).

2. A nondestructive safety monitoring method for assembly engineering connection nodes according to claim 1, characterized in that: The sleeve (1) is a fully grouted sleeve formed by machine tool processing or extrusion. The sleeve (1) is made of steel. The top and bottom ends of the sleeve (1) are both provided with insulating sealing rings (9). The insulating sealing rings (9) are connected to the sleeve (1) by grouting. One end of the sleeve (1) is provided with a grout outlet (5).

3. A nondestructive safety monitoring method for assembly engineering connection nodes according to claim 1, characterized in that: The grouting material (3) is a self-sensing grouting material, which is a cement-based grouting material modified with a conductive filler. The compressive strength of the grouting material (3) at 28 days is greater than 85 MPa, and the resistivity change rate is greater than or equal to 35%.

4. A nondestructive safety monitoring method for assembly engineering connection nodes according to claim 1, characterized in that: The method for measuring the resistivity ρ1 and the resistivity ρ2 of the grouting material (3) in step S4 is: S4.1: injecting a grouting material (3) into the insulating mold (10), and placing two stainless steel meshes (11) in the grouting material (3); S4.2: Use a multimeter (6) to measure the resistance value Z1 of the grouting material (3) after mixing for 30 minutes; S4.3: After curing the grouting material (3) for 1 day, remove the mold, seal and cure for 28 days, and use the multimeter (6) again to measure the resistance value Z2 of the grouting material (3); S4.4: Calculate the resistivity ρ1 of the grouting material (3) after mixing for 30 min using the expression: ρ1=Z1S / L Wherein, S is the cross-sectional area of ​​the specimen, and L is the distance between the two stainless steel meshes (11); S4.5: Calculate the resistivity ρ2 of the grouting material (3) after 28 days of curing, using the expression: ρ2=Z2S / L Wherein, S is the cross-sectional area of ​​the specimen, and L is the distance between the two stainless steel meshes (11).

5. A nondestructive safety monitoring method for assembly engineering connection nodes according to claim 4, characterized in that: The insulating mold (10) has a size of 40 mm*40 mm*160 mm, the mesh size of the stainless steel mesh (11) is no larger than 0.5 mm, and the distance between two stainless steel meshes (11) is 100 mm.

6. A nondestructive safety monitoring method for assembly engineering connection nodes according to claim 1, characterized in that: The calculated resistance value R 计1 The expression is: Wherein, Q is the total length of the sleeve (1); The calculated resistance value R 计2 The expression is: Wherein, Q is the total length of the sleeve (1).

7. The method for nondestructive safety monitoring of assembly-type engineering connection nodes according to claim 1 is characterized in that: The fullness expression is: The service status expression is: