Semiconductor device
By using silicon nitride semi-insulating films of silicon and nitrogen in semiconductor devices, the problem of breakdown voltage fluctuation is solved, and a more stable electric field and a higher breakdown voltage are achieved.
Patent Information
- Application Number
- CN202410416772.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2023-05-16
- Filing Date
- 2024-04-08
- Publication Date
- 2024-11-22
AI Technical Summary
The breakdown voltage in existing semiconductor devices is prone to fluctuation when the voltage is applied, resulting in poor stability.
Using a semi-insulating film, a mixed crystal of silicon nitride and amorphous silicon containing silicon and nitrogen, the ratio of the sum of the number of silicon atoms and the number of nitrogen atoms is 0.64 or greater than 0.64, by adjusting the silane in the reaction gas The semi-insulating film is formed with the nitrogen flow ratio to ensure its extension between the electrodes, ease the electric field and improve the stability of the breakdown voltage.
Effectively suppress changes in breakdown voltage, improve the stability of semiconductor devices, reduce the fluctuations of electric fields, and enhance the isolation performance between electrodes.
Smart Images

Figure CN119008668A_ABST
Abstract
Description
[0001] CROSS-REFERENCE TO RELATED APPLICATIONS
[0002] The disclosure of Japanese Patent Application No. 2023-080585 filed on May 16, 2023 (including specification, drawings and abstract) is incorporated herein by reference in its entirety. Technical Field
[0003] The present disclosure relates to a semiconductor device. Background Art
[0004] For example, Japanese Unexamined Patent Application Publication No. 2022-074323 (Patent Document 1) describes a semiconductor device. The semiconductor device according to Patent Document 1 includes a semiconductor substrate, a first electrode, a second electrode, an insulating film, and a semi-insulating film. In a plan view, the semiconductor substrate has a first region and a second region surrounding the first region. The semiconductor substrate has a first surface and a second surface opposite to the first surface in the thickness direction of the semiconductor substrate. The semiconductor substrate includes an impurity region formed on a first surface of the first region. The insulating film covers the first surface in the second region. The first electrode is opposite to the impurity region, with the insulating film being inserted therebetween. In a plan view, the second electrode is arranged on the insulating film to surround the first electrode while being separated from the first electrode. The semi-insulating film is arranged to extend across the insulating film between the first electrode and the second electrode.
[0005] The disclosed technologies are listed below.
[0006] [Patent Document 1] Japanese Unexamined Patent Application Publication No. 2022-074323 Summary of the invention
[0007] In the semiconductor device described in Patent Document 1, the breakdown voltage may fluctuate every time a voltage is applied. Other objects and novel features will become apparent from the description of this specification and the accompanying drawings.
[0008] The semiconductor device disclosed in the present invention includes a semiconductor substrate, an insulating film, a first electrode, a second electrode and a semi-insulating film. The semiconductor substrate includes a first surface. In a plan view, the semiconductor substrate includes an element region and a terminal region surrounding the element region. The semiconductor substrate includes a first impurity region, which is formed on a first surface in the terminal region. The insulating film covers the first surface in the terminal region. The first electrode is electrically connected to the first impurity region and faces the first impurity region, wherein the insulating film is inserted between the first electrode and the first impurity region. In a plan view, the second electrode is arranged on the insulating film to surround the first electrode while being spaced apart from the first electrode. In a plan view, the semi-insulating film is arranged to extend across the insulating film between the first electrode and the second electrode. The semi-insulating film includes silicon and nitrogen. The ratio of the number of silicon atoms in the semi-insulating film to the sum of the number of silicon atoms and the number of nitrogen atoms is 0.64 or greater.
[0009] According to the semiconductor device of the present disclosure, variation in breakdown voltage can be suppressed. BRIEF DESCRIPTION OF THE DRAWINGS
[0010] Figure 1 is a plan view of the semiconductor device DEV1.
[0011] Figure 2 yes Figure 1 II-II is a cross-sectional view of the semiconductor device DEV1.
[0012] Figure 3 It is a manufacturing process diagram of the semiconductor device DEV1.
[0013] Figure 4 is a cross-sectional view illustrating the preparation process S1.
[0014] Figure 5 is a cross-sectional view for explaining the epitaxial growth process S2.
[0015] Figure 6 is a cross-sectional view illustrating the first insulating film forming step S3.
[0016] Figure 7 is a cross-sectional view describing the impurity region forming process S4.
[0017] Figure 8 : is a cross-sectional view for explaining the second insulating film forming step S5.
[0018] Fig. 9 is a cross-sectional view illustrating the first electrode forming step S6.
[0019] Fig.10 is a cross-sectional view illustrating a step of forming a semi-insulating film S7.
[0020] Fig.11is a cross-sectional view illustrating the second electrode forming step S8.
[0021] Fig.12 : is a graph showing the relationship between the ratio of the number of silicon atoms to the sum of the number of silicon atoms and the number of nitrogen atoms in the semi-insulating film SIF and the number of silicon-hydrogen bonds.
[0022] Fig.13 is a graph showing the relationship between the number of breakdown voltage measurements and the breakdown voltage.
[0023] Fig.14 : is a graph showing the relationship between the refractive index of the semi-insulating film SIF and the ratio of the number of silicon atoms to the sum of the number of silicon atoms and the number of nitrogen atoms in the semi-insulating film SIF.
[0024] Fig.15 : is a graph showing the relationship between the refractive index of the semi-insulating film SIF and the change in the thickness T1 of the semi-insulating film SIF.
[0025] Fig.16 is a cross-sectional view of the semiconductor device DEV2.
[0026] Fig.17 It is a manufacturing process diagram of the semiconductor device DEV2.
[0027] Fig.18 is a cross-sectional view of the semiconductor device DEV3.
[0028] Fig.19 It is a manufacturing process diagram of the semiconductor device DEV3.
[0029] Fig. 20 is a cross-sectional view illustrating the first impurity region forming step S10.
[0030] Fig.21 is a cross-sectional view for explaining the first insulating film forming step S3 in the method for manufacturing the semiconductor device DEV3.
[0031] Fig. 22 is a cross-sectional view describing the second impurity region forming step S11.
[0032] Fig.23 is a cross-sectional view of the semiconductor device DEV4.
[0033] Fig.24 It is a manufacturing process diagram of semiconductor device DEV4.
[0034] Fig.25 2 is a cross-sectional view for explaining the first insulating film forming step S3 in the method for manufacturing the semiconductor device DEV4.
[0035] Fig.26is a cross-sectional view for explaining the third impurity region forming step S12.
[0036] Fig. 27 is a cross-sectional view describing the fourth impurity region forming step S13. DETAILED DESCRIPTION
[0037] The details of the embodiments of the present disclosure will be described with reference to the accompanying drawings. In the following drawings, the same or corresponding parts are represented by the same reference numerals, and redundant descriptions will not be repeated.
[0038] (First embodiment)
[0039] A semiconductor device DEV1 according to a first embodiment will be described.
[0040] <Structure of semiconductor device DEV1>
[0041] The configuration of the semiconductor device DEV1 will be described below.
[0042] Figure 1 is a plan view of the semiconductor device DEV1. Figure 2 yes Figure 1 II-II is a cross-sectional view of the semiconductor device DEV1. Figure 1 and Figure 2 As shown in FIG. 1 , the semiconductor device DEV1 has a semiconductor substrate SUB. The semiconductor substrate SUB has a first surface FS and a second surface SS opposite to the first surface FS in the thickness direction of the semiconductor substrate SUB. The composition of the semiconductor substrate SUB is, for example, single crystal silicon (Si).
[0043] The semiconductor substrate SUB has an element region SUB1 and a termination region SUB2. In a plan view, the termination region SUB2 surrounds the element region SUB1.
[0044] The semiconductor substrate SUB includes an impurity region R1, an impurity region R2, an impurity region R3, an impurity region R4, and an impurity region R5. The conductivity type of the impurity region R1 and the conductivity type of the impurity region R2 are the first conductivity type. The first conductivity type is, for example, an n-type. The conductivity type of the impurity region R3 and the conductivity type of the impurity region R4 are the second conductivity type. The second conductivity type is, for example, a p-type. The conductivity type of the impurity region R5 is the first conductivity type or the second conductivity type.
[0045] Impurity region R1 is formed on second surface SS. Impurity region R2 is formed on first surface FS. Impurity region R2 is in contact with impurity region R1 on the other side of first surface FS. Impurity region R1 and impurity region R2 form, for example, a cathode of an FRD (fast recovery diode).
[0046] The impurity region R3 is formed on the first surface FS of the element region SUB1. The impurity region R4 is formed on the first surface of the termination region SUB2. The impurity region R3 is pn-bonded to the impurity region R2. The impurity region R3 is, for example, an anode of the FRD. As described above, in the semiconductor device DEV1, the FRD is formed in the element region SUB1.
[0047] Impurity region R4 is formed on the first surface FS in the terminal region SUB2. In a plan view, impurity region R4 extends over the boundary between element region SUB1 and terminal region SUB2. In a plan view, impurity region R4 surrounds impurity region R3. Impurity region R4 is in contact with impurity region R3. That is, impurity region R4 is electrically connected to impurity region R3. Impurity region R4 is pn-bonded to impurity region R2. The impurity concentration in impurity region R4 is lower than the impurity concentration in impurity region R3. That is, impurity region R4 forms a RESURF (reduced surface field) structure. Impurity region R5 is formed on the first surface FS in the terminal region SUB2. In a plan view, impurity region R5 surrounds impurity region R4. Impurity region R5 is separated from impurity region R4.
[0048] The semiconductor device DEV1 further includes an insulating film ISL. The insulating film ISL is disposed on the first surface FS. The insulating film ISL covers at least the first surface FS in the termination region SUB2. The insulating film ISL partially covers the first surface FS in the element region SUB1. An opening OP1 and an opening OP2 are formed in the insulating film ISL. The opening OP1 is formed on the impurity region R3. The opening OP2 is formed on the impurity region R5.
[0049] The insulating film ISL includes a first insulating film ISL1 and a second insulating film ISL2. The first insulating film ISL1 and the second insulating film ISL2 are made of, for example, silicon oxide (SiO 2 ). The first insulating film ISL1 covers the first surface FS between the impurity region R3 and the impurity region R5. The second insulating film ISL2 covers the first insulating film ISL1. Therefore, a step is formed in the upper surface of the insulating film ISL.
[0050] The semiconductor device DEV1 further includes a first electrode EL1 and a second electrode EL2. The first electrode EL1 and the second electrode EL2 are made of, for example, aluminum (Al) or an aluminum alloy.
[0051] The first electrode EL1 has a peripheral edge portion EL1a. The peripheral edge portion EL1a faces the impurity region R4, with the insulating film ISL interposed therebetween. The peripheral edge portion EL1a serves as a field plate. The first electrode EL1 is connected to the impurity region R3 via the opening portion OP1. As described above, since the impurity region R3 is in contact with the impurity region R4, the first electrode EL1 is electrically connected to the impurity region R4. The second electrode EL2 is disposed on the insulating film ISL. In a plan view, the second electrode EL2 surrounds the first electrode EL1. The second electrode EL2 is spaced apart from the first electrode EL1. The second electrode EL2 is connected to the impurity region R5 via the opening portion OP2. The second electrode EL2 is set to, for example, a ground potential.
[0052] The semiconductor device DEV1 further includes a semi-insulating film SIF. The semi-insulating film SIF includes silicon and nitrogen (N). The semi-insulating film SIF is made of, for example, silicon nitride (Si 3 N 4 ) and amorphous silicon. From another point of view, a part of silicon contained in the semi-insulating film SIF is bonded to hydrogen.
[0053] In the semi-insulating film SIF, the ratio of the number of silicon atoms to the sum of the number of silicon atoms and the number of nitrogen atoms (i.e., the number of silicon atoms divided by the sum of the number of silicon atoms and the number of nitrogen atoms) is 0.64 or greater. In the semi-insulating film SIF, the ratio of the number of silicon atoms to the sum of the number of silicon atoms and the number of nitrogen atoms may be 0.74 or less. The ratio of the number of silicon atoms to the sum of the number of silicon atoms and the number of nitrogen atoms in the semi-insulating film SIF is measured by XPS (X-ray photoelectron spectroscopy).
[0054] The refractive index of the semi-insulating film SIF is, for example, 2.55 or more. The refractive index of the semi-insulating film SIF is, for example, 2.90 or less. The refractive index of the semi-insulating film SIF is optically measured using a spectroscopic ellipsometer.
[0055] The semi-insulating film SIF is provided to extend across the insulating film ISL between the first electrode EL1 and the second electrode EL2. The semi-insulating film SIF has an inner peripheral edge portion SIFa. The inner peripheral edge portion SIFa is provided on the outer peripheral edge portion EL1a. The semi-insulating film SIF covers the second electrode EL2.
[0056] The thickness T1 of the semi-insulating film SIF is, for example, equal to or greater than 50 nm and equal to or less than 1000 nm. The variation of the thickness T1 is, for example, 0.02 or less. The variation of the thickness T1 is defined as the larger value of the following values:
[0057] (i) dividing the value obtained by (subtracting the average value of the thickness T1 from the maximum value of the thickness T1) by the average value of the thickness T1, and
[0058] (ii) Dividing the value obtained by (subtracting the minimum value of the thickness T1 from the average value of the thickness T1) by the average value of the thickness T1.
[0059] The thickness T2 of the insulating film ISL is, for example, greater than or equal to 0.5 μm (micrometer) and less than or equal to 3.0 μm (micrometer). The thickness T2 is measured at a portion between the first surface FS and the semi-insulating film SIF. From the perspective of ensuring a margin during wire bonding, the thickness T3 of the first electrode EL1 and the second electrode EL2 is, for example, greater than or equal to 2.0 μm (micrometer) and less than or equal to 6.0 μm (micrometer).
[0060] The semiconductor device DEV1 further includes a third electrode EL3. The third electrode EL3 may be made of aluminum or an aluminum alloy. The third electrode EL3 is disposed on the second surface SS.
[0061] The semiconductor device DEV1 further includes a passivation film PV. The passivation film PV is made of, for example, polyimide. The passivation film PV is provided on the semi-insulating film SIF.
[0062] <Method for Manufacturing Semiconductor Device DEV1>
[0063] Next, a method for manufacturing the semiconductor device DEV1 is described.
[0064] Figure 3 It is the manufacturing process diagram of semiconductor device DEV1. Figure 3 As shown in, the manufacturing method of the semiconductor device DEV1 includes a preparation step S1, an epitaxial growth step S2, a first insulating film forming step S3, an impurity region forming step S4, a second insulating film forming step S5, a first electrode forming step S6, a semi-insulating film forming step S7, a second electrode forming step S8 and a passivation film forming step S9.
[0065] Figure 4 is a cross-sectional view illustrating the preparation step S1. Figure 4 As shown in FIG. 1 , in the preparation process S1 , a semiconductor substrate SUB is prepared. At this stage, the semiconductor substrate SUB has only the impurity region R1 . Figure 5 FIG. 4 is a cross-sectional view of S2 illustrating the epitaxial growth process. Figure 5 As shown in FIG. 1 , in the epitaxial growth process S2 , the impurity region R2 is epitaxially grown on the impurity region R1 . The impurity region R2 is formed by, for example, CVD (Chemical Vapor Deposition).
[0066] Figure 6 2 is a cross-sectional view illustrating the first insulating film forming step S3. Figure 6As shown in the figure, in the first insulating film forming step S3, the first insulating film ISL1 is formed. In the first insulating film forming step S3, first, the constituent material of the first insulating film ISL1 is formed on the first surface FS by a thermal oxidation method or a CVD method. Next, the constituent material of the formed first insulating film ISL1 is etched using a resist pattern formed by photolithography.
[0067] Figure 7 2 is a cross-sectional view for explaining the impurity region forming step S4. Figure 7 As shown, in the impurity region forming step S4, impurity region R3, impurity region R4 and impurity region R5 are formed. In the impurity region forming step S4, first, a resist pattern is formed on the first surface FS and the first insulating film ISL1 by photolithography. Second, ion implantation is performed from the first surface FS side using the resist pattern as a mask. Third, the resist pattern is removed. Fourth, the implanted impurity ions are thermally diffused by annealing the semiconductor substrate SUB. Thus, impurity region R4 is formed. Impurity region R3 and impurity region R5 are also formed by the same process.
[0068] Figure 8 2 is a cross-sectional view illustrating the second insulating film forming step S5. Figure 8 As shown in, in the second insulating film forming step S5, the second insulating film ISL2 is formed. In the second insulating film forming step S5, first, the constituent material of the second insulating film ISL2 is formed by, for example, a CVD method to cover the first insulating film ISL1. Second, the constituent material of the formed second insulating film ISL2 is etched using a resist pattern formed by photolithography.
[0069] Fig. 9 2 is a cross-sectional view for explaining the first electrode forming step S6. Fig. 9 As shown in, in the first electrode forming step S6, the first electrode EL1 and the second electrode EL2 are formed. In the first electrode forming step S6, first, the constituent material of the first electrode EL1 (second electrode EL2) is deposited on the first surface FS and the insulating film ISL by, for example, a sputtering method. Second, the constituent material of the formed first electrode EL1 (second electrode EL2) is etched using a resist pattern formed by photolithography.
[0070] Fig.10 2 is a cross-sectional view illustrating the semi-insulating film forming step S7. Fig.10As shown in FIG. 1 , in the semi-insulating film forming step S7, the semi-insulating film SIF is formed. In the semi-insulating film forming step S7, first, the constituent material of the semi-insulating film SIF is formed by, for example, a CVD method so as to cover the first electrode EL1, the second electrode EL2, and the insulating film ISL. Second, the constituent material of the semi-insulating film SIF formed is patterned by etching using a resist pattern formed by photolithography. When the CVD method is performed, by adjusting the monosilane (SiH 4 ) and nitrogen (N 2 ) to obtain the ratio of the number of silicon atoms in the semi-insulating film SIF to the sum of the number of silicon atoms and the number of nitrogen atoms. As the flow rate of monosilane divided by the flow rate of nitrogen increases, the ratio of the number of silicon atoms in the semi-insulating film SIF to the sum of the number of silicon atoms and the number of nitrogen atoms increases.
[0071] Fig.11 2 is a cross-sectional view for explaining the second electrode forming step S8. Fig.11 As shown in FIG. 1 , in the second electrode forming step S8, the constituent material of the third electrode EL3 is formed on the second surface SS by, for example, sputtering to form the third electrode EL3. In the passivation film forming step S9, the passivation film PV is formed. In the passivation film forming step S9, first, the constituent material of the passivation film PV is formed to cover the semi-insulating film SIF and the first electrode EL1. Second, the constituent material of the passivation film PV is patterned by photolithography. Thus, a Figure 1 and Figure 2 Detailed description of the structure of the semiconductor device DEV1 shown in FIG.
[0072] In the above-mentioned manufacturing method embodiment, in the preparation step S1, a semiconductor substrate SUB having only the impurity region R1 is provided, but in the preparation step S1, a semiconductor substrate SUB having only the impurity region R2 may be provided. In this case, the epitaxial growth step S2 is not performed, and the impurity region R1 is formed by performing ion implantation from the second surface SS. Before the second electrode forming step S8, the impurity region R1 is formed by ion implantation.
[0073] <Modification example>
[0074] In the above description, the FRD is formed in the element region SUB1, but semiconductor elements other than the FRD may be formed in the element region SUB1. For example, an IGBT (Insulated Gate Bipolar Transistor) may be formed in the element region SUB1.
[0075] <Effect of semiconductor device DEV1>
[0076] Next, the effectiveness of the semiconductor device DEV1 will be described in comparison with the semiconductor device according to the comparative example. The configuration of the semiconductor device according to the comparative example is the same as that of the semiconductor device DEV1 except that the ratio of the number of silicon atoms to the sum of the number of silicon atoms and the number of nitrogen atoms in the semi-insulating film SIF is less than 0.64.
[0077] In the semiconductor device DEV1 and the semiconductor device according to the comparative example, since the semi-insulating film SIF is semi-insulating, a weak leakage current flows through the semi-insulating film SIF, so that the electric field is relaxed in the semiconductor substrate SUB facing the semi-insulating film SIF with the insulating film ISL interposed therebetween, and the breakdown voltage is improved. At this time, electrons are induced and captured in the semi-insulating film SIF.
[0078] Fig.12 Graphs showing the relationship between (i) the ratio of the number of silicon atoms to the sum of the number of silicon atoms and the number of nitrogen atoms in the semi-insulating film SIF and (ii) the number of silicon-hydrogen bonds. Fig.12 The graph of is obtained by performing FT-IR (Fourier transform infrared spectroscopy) analysis on Samples 1 to 6 of the semi-insulating films SIF.
[0079] The ratio of the number of silicon atoms to the sum of the number of silicon atoms and the number of nitrogen atoms in each sample is larger in the order of sample 1, sample 2, sample 3, sample 4, sample 5, and sample 6. The ratio of the number of silicon atoms to the sum of the number of silicon atoms and the number of nitrogen atoms in samples 1 to 3 is less than 0.64, and the ratio of the number of silicon atoms to the sum of the number of silicon atoms and the number of nitrogen atoms in samples 4 to 6 is 0.64 or greater.
[0080] like Fig.12 As shown in , no silicon-hydrogen bond was detected in samples 1 to 3. On the other hand, peaks derived from silicon-hydrogen bonds were detected in samples 4 to 6. In other words, the semiconductor device DEV1 includes amorphous silicon in the semi-insulating film SIF, while the semiconductor device according to the comparative example does not include amorphous silicon in the semi-insulating film SIF.
[0081] In the semiconductor device according to the comparative example, since the semi-insulating film SIF does not contain amorphous silicon through which current easily flows, the electrons induced and captured in the semi-insulating film SIF hardly escape from the semi-insulating film SIF. The electrons induced and captured in the semi-insulating film SIF cause the breakdown voltage to fluctuate. On the other hand, in the semiconductor device DEV1, since the semi-insulating film SIF contains amorphous silicon through which current easily flows, the induced and captured electrons flow to the second electrode EL2 and easily escape from the semi-insulating film SIF. Therefore, according to the semiconductor device DEV1, the variation of the breakdown voltage can be suppressed.
[0082] Fig.13 is a graph showing the relationship between the number of breakdown voltage measurements and the breakdown voltage. Fig.13 middle, Fig.12 Sample 2 in is used as the semi-insulating film SIF of the semiconductor device according to the comparative example, and Sample 4 or Sample 6 is used as the semi-insulating film SIF in the semiconductor device DEV1. Fig.13 The vertical axis of the graph shows the difference between the breakdown voltage in the nth measurement (n is an integer greater than or equal to 1 and less than or equal to 10) and the breakdown voltage in the first measurement. Since the vertical axis value in the first measurement is (withstand voltage in the first measurement)-(withstand voltage in the first measurement), it is 0. Fig.13 As shown in , in the semiconductor device according to the comparative example in which the ratio SIF of the number of silicon atoms in the semi-insulating film to the sum of the number of silicon atoms and the number of nitrogen atoms is less than 0.64, the breakdown voltage fluctuates greatly as the number of measurements increases. On the other hand, in the semiconductor device DEV1 in which the ratio of the number of silicon atoms in the semi-insulating film SIF to the sum of the number of silicon atoms and the number of nitrogen atoms is 0.64 or more, the change in the breakdown voltage is small even if the number of measurements increases.
[0083] Fig.14 Graph showing the relationship between the refractive index of the semi-insulating film SIF and the ratio of the number of silicon atoms to the sum of the number of silicon atoms and the number of nitrogen atoms in the semi-insulating film SIF. Fig.14 As shown in , as the refractive index of the semi-insulating film SIF increases, the ratio of the number of silicon atoms in the semi-insulating film SIF to the sum of the number of silicon atoms and the number of nitrogen atoms increases. More specifically, if the ratio of the number of silicon atoms in the semi-insulating film SIF to the sum of the number of silicon atoms and the number of nitrogen atoms is 0.64 or greater than 0.64, the refractive index of the semi-insulating film SIF is 2.55 or greater than 2.55. In addition, if the ratio of the number of silicon atoms in the semi-insulating film SIF to the sum of the number of silicon atoms and the number of nitrogen atoms is 0.74 or less than 0.74, the refractive index of the semi-insulating film SIF is 2.90 or less than 2.90. As described above, by setting the refractive index of the semi-insulating film SIF to 2.55 or greater than 2.55, the semiconductor device DEV1 can suppress the change in breakdown voltage.
[0084] Fig.15 : is a graph showing the relationship between the refractive index of the semi-insulating film SIF and the change in the thickness T1 of the semi-insulating film SIF. Fig.15As shown in , when the refractive index SIF of the semi-insulating film is greater than 2.90, that is, when the ratio of the number of silicon atoms in the semi-insulating film SIF to the sum of the number of silicon atoms and the number of nitrogen atoms is greater than 0.74, the variation of the thickness T1 increases. On the other hand, when the ratio of the number of silicon atoms in the semi-insulating film SIF to the sum of the number of silicon atoms and the number of nitrogen atoms is not less than 0.64 and not more than 0.74, the variation of the thickness T1 is not more than 0.02. Therefore, by setting the ratio of the number of silicon atoms in the semi-insulating film SIF to the sum of the number of silicon atoms and the number of nitrogen atoms to 0.64 or more and 0.74 or less, the variation of the thickness T1 can be suppressed while suppressing the variation of the breakdown voltage.
[0085] As the thickness T1 increases, current tends to flow through the semi-insulating film SIF, and the induced / captured electrons further tend to escape. On the other hand, if the thickness T1 is too large, the semi-insulating film SIF is hard, so that cracks are likely to occur in the semi-insulating film SIF. Therefore, by setting the thickness T1 to be equal to or greater than 50 nm and equal to or less than 1000 nm, the occurrence of cracks in the semi-insulating film SIF can be suppressed while suppressing the breakdown voltage variation.
[0086] As the thickness T2 increases, the capacitance composed of the semi-insulating film SIF, the insulating film ISL and the semiconductor substrate SUB decreases, and the change in breakdown voltage is suppressed. On the other hand, if the thickness T2 is too large, the embedding property of the first electrode EL1 and the second electrode EL2 deteriorates. If the thickness T2 is too large, the step formed in the upper surface of the insulating film ISL becomes larger, and cracks are likely to occur in the semi-insulating film SIF due to the step. Therefore, by setting the thickness T2 to be greater than or equal to 0.5μm (micrometer) and less than or equal to 3.0μm (micrometer), the occurrence of cracks in the semi-insulating film SIF and the degradation of the embedding property of the first electrode EL1 and the second electrode EL2 can be suppressed, while suppressing the change in breakdown voltage.
[0087] (Second embodiment)
[0088] A semiconductor device DEV2 according to a second embodiment will be described. Here, the difference from the semiconductor device DEV1 will be mainly described, and redundant description will not be repeated.
[0089] <Structure of semiconductor device DEV2>
[0090] The configuration of the semiconductor device DEV2 will be described below.
[0091] Fig.16 is a cross-sectional view of the semiconductor device DEV2. Fig.16 Shown with Figure 1 The cross section at the position corresponding to II-II in FIG. Fig.16As shown in , the semiconductor device DEV2 includes a semiconductor substrate SUB, an insulating film ISL, a first electrode EL1 and a second electrode EL2, a semi-insulating film SIF, and a passivation film PV. In the semiconductor device DEV2, the ratio of the number of silicon atoms in the semi-insulating film SIF to the sum of the number of silicon atoms and the number of nitrogen atoms is 0.64 or greater. In these respects, the configuration of the semiconductor device DEV2 is the same as that of the semiconductor device DEV1.
[0092] In the semiconductor device DEV2, the semi-insulating film SIF is disposed on the insulating film ISL. More specifically, in the semiconductor device DEV2, the semi-insulating film SIF is disposed on the inner side of the step formed on the upper surface of the insulating film ISL. In the semiconductor device DEV2, the semi-insulating film SIF has an inner peripheral edge portion SIFa and an outer peripheral edge portion SIFb. The inner peripheral edge portion SIFa and the outer peripheral edge portion SIFb are covered by the first electrode EL1 and the second electrode EL2, respectively. In these aspects, the configuration of the semiconductor device DEV2 is different from the configuration of the semiconductor device DEV1.
[0093] <Modification example>
[0094] In the above description, the ratio of the number of silicon atoms in the semi-insulating film SIF to the sum of the number of silicon atoms and the number of nitrogen atoms is 0.64 or greater, but in the semiconductor device DEV2, the ratio of the number of silicon atoms in the semi-insulating film SIF to the sum of the number of silicon atoms and the number of nitrogen atoms may be less than 0.64. In the semiconductor device DEV2, the semi-insulating film SIF may be formed of a material other than a material containing silicon and nitrogen (e.g., polycrystalline silicon).
[0095] <Method for manufacturing semiconductor device DEV2>
[0096] Next, a method for manufacturing the semiconductor device DEV2 is described.
[0097] Fig.17 It is a manufacturing process diagram of semiconductor device DEV2. Fig.17 As shown in , the manufacturing method of the semiconductor device DEV2 includes a preparation step S1, an epitaxial growth step S2, a first insulating film forming step S3, an impurity region forming step S4, a second insulating film forming step S5, a first electrode forming step S6, a semi-insulating film forming step S7, a second electrode forming step S8 and a passivation film forming step S9. In this respect, the manufacturing method of the semiconductor device DEV2 is the same as the manufacturing method of the semiconductor device DEV1.
[0098] In the manufacturing method of the semiconductor device DEV2, the semi-insulating film forming step S7 is performed after the second insulating film forming step S5. In the manufacturing method of the semiconductor device DEV2, the first electrode forming step S6 is performed after the semi-insulating film forming step S7. In this respect, the manufacturing method of the semiconductor device DEV2 is different from the manufacturing method of the semiconductor device DEV1.
[0099] <Effect of semiconductor device DEV2>
[0100] Advantages of the semiconductor device DEV2 will be described below.
[0101] A step is formed in the upper surface of the insulating film ISL. Therefore, in the semiconductor device DEV1, a step is also formed in the upper surface of the first electrode EL1 and the upper surface of the second electrode EL2, and the semi-insulating film SIF may be disposed on the step. Since stress concentration tends to occur near such a step, cracks tend to occur in the semi-insulating film SIF in the semiconductor device DEV1. Since the semi-insulating film SIF becomes brittle as the composition ratio of silicon becomes higher, and the characteristics become closer to silicon, such cracks may occur when the ratio of the number of silicon atoms in the semi-insulating film SIF to the sum of the number of silicon atoms and the number of nitrogen atoms is 0.64 or greater.
[0102] On the other hand, in the semiconductor device DEV2, the inner peripheral edge portion SIFa and the outer peripheral edge portion SIFb are covered by the first electrode EL1 and the second electrode EL2, respectively. That is, the semiconductor device DEV2 does not have a portion where the semi-insulating film SIF is provided on the first electrode EL1 and the second electrode EL2. Therefore, in the semiconductor device DEV2, cracks are less likely to occur in the semi-insulating film SIF without being affected by the steps formed on the upper surface of the first electrode EL1 and the upper surface of the second electrode EL2.
[0103] (Third Embodiment)
[0104] A semiconductor device DEV3 according to a third embodiment will be described. Here, the difference from the semiconductor device DEV1 will be mainly described, and redundant description will not be repeated.
[0105] <Structure of semiconductor device DEV3>
[0106] The configuration of the semiconductor device DEV3 will be described below.
[0107] Fig.18 is a cross-sectional view of the semiconductor device DEV3. Fig.18 Shows the corresponding Figure 1 The cross section at position II-II. Fig.18As shown in , the semiconductor device DEV3 includes a semiconductor substrate SUB, an insulating film ISL, a first electrode EL1 and a second electrode EL2, a semi-insulating film SIF, and a passivation film PV. In the semiconductor device DEV3, the ratio of the number of silicon atoms in the semi-insulating film SIF to the sum of the number of silicon atoms and the number of nitrogen atoms is 0.64 or greater. In these respects, the configuration of the semiconductor device DEV3 is the same as that of the semiconductor device DEV1.
[0108] In the semiconductor device DEV3, a groove RCS1 is formed on the first surface FS. The first surface FS is recessed in the groove RCS1 toward the second surface SS. In a plan view, the groove RCS1 is arranged to overlap with the impurity region R4. The groove RCS1 may extend to an adjacent side of the impurity region R5. In the semiconductor device DEV3, a first insulating film ISL1 is embedded in the groove RCS1, and a second insulating film ISL2 is arranged on the first surface FS in the terminal region SUB2 so as to cover the first insulating film ISL1. In the semiconductor device DEV3, for example, the first insulating film ISL1 is thicker than the second insulating film ISL2. In these aspects, the configuration of the semiconductor device DEV3 is different from the configuration of the semiconductor device DEV1.
[0109] <Modification example>
[0110] In the above description, the ratio of the number of silicon atoms in the semi-insulating film SIF to the sum of the number of silicon atoms and the number of nitrogen atoms is 0.64 or greater, but in the semiconductor device DEV3, the ratio of the number of silicon atoms in the semi-insulating film SIF to the sum of the number of silicon atoms and the number of nitrogen atoms may be less than 0.64. In the semiconductor device DEV3, the semi-insulating film SIF may be formed of a material other than a material containing silicon and nitrogen (e.g., polycrystalline silicon).
[0111] <Method for manufacturing semiconductor device DEV3>
[0112] Next, a method for manufacturing the semiconductor device DEV3 is described.
[0113] Fig.19 It is the manufacturing process diagram of semiconductor device DEV3. Fig.19 As shown in , the manufacturing method of the semiconductor device DEV3 includes a preparation step S1, an epitaxial growth step S2, a first insulating film forming step S3, a second insulating film forming step S5, a first electrode forming step S6, a semi-insulating film forming step S7, a second electrode forming step S8 and a passivation film forming step S9. In this respect, the manufacturing method of the semiconductor device DEV3 is the same as the manufacturing method of the semiconductor device DEV1.
[0114] The manufacturing method of the semiconductor device DEV3 includes a first impurity region forming step S10 and a second impurity region forming step S11 instead of the impurity region forming step S4.
[0115] The first impurity region forming step S10 is performed after the epitaxial growth step S2. Fig. 20 2 is a cross-sectional view for explaining the first impurity region forming step S10. Fig. 20 As shown in, in the first impurity region forming step S10, the impurity region R4 is formed. In the first impurity region forming step S10, first, a resist pattern is formed on the first surface FS by photolithography. Second, ion implantation is performed from the first surface FS side using the resist pattern as a mask. Third, the implanted impurity ions are thermally diffused by annealing the semiconductor substrate SUB.
[0116] In the manufacturing method of the semiconductor device DEV3, the first insulating film forming step S3 is performed after the first impurity region forming step S10. Fig.21 1 is a cross-sectional view illustrating a first insulating film forming step S3 in a method for manufacturing a semiconductor device DEV3. Fig.21 As shown in, in the manufacturing method of the semiconductor device DEV3, a groove RCS1 and a first insulating film ISL1 are formed in a first insulating film forming step S3. In the first insulating film forming step S3 in the manufacturing method of the semiconductor device DEV2, first, a resist pattern is formed on the first surface FS by photolithography. Second, the first surface FS is etched using the resist pattern as a mask to form the groove RCS1. Third, polysilicon is partially embedded in the recessed RCS1, for example, by CVD. Fourth, the embedded polysilicon is thermally oxidized to form the first insulating film ISL1. Note that when the first insulating film ISL1 protrudes from the groove RCS1, the protruding first insulating film ISL1 can be removed by a CMP (chemical mechanical polishing) method. In addition, in the above-mentioned embodiment, the first insulating film ISL1 is formed by partially embedding polysilicon in the groove RCS1 and performing thermal oxidation, but the first insulating film ISL1 can be formed only by thermal oxidation.
[0117] In the manufacturing method of the semiconductor device DEV3, the second impurity region forming step S11 is performed after the first insulating film forming step S3. Fig. 22 2 is a cross-sectional view for explaining the second impurity region forming step S11. Fig. 22 As shown in, in the second impurity region forming step S11, the impurity region R3 and the impurity region R5 are formed. In the second impurity region forming step S11, first, ion implantation is performed from the first surface FS side using the first insulating film ISL1 as a mask. Second, the semiconductor substrate SUB is annealed to thermally diffuse the implanted impurity ions.
[0118] In the manufacturing method of the semiconductor device DEV3, after the second impurity region forming step S11, the second insulating film forming step S5, the first electrode forming step S6, the semi-insulating film forming step S7, the second electrode forming step S8 and the passivation film forming step S9 are performed in sequence.
[0119] <Effect of semiconductor device DEV3>
[0120] Advantages of the semiconductor device DEV3 will be described below.
[0121] In the semiconductor device DEV3, since the first insulating film ISL1 is embedded in the groove RCS1 and the second insulating film ISL2 is provided to cover the first insulating film ISL1, there is less possibility of forming a step on the upper surface of the insulating film ISL and thus on the upper surfaces of the first electrode EL1 and the second electrode EL2. Therefore, according to the semiconductor device DEV3, even when the semi-insulating film SIF is provided on the first electrode EL1 and the second electrode EL2, cracks due to stress concentration are less likely to occur in the semi-insulating film SIF.
[0122] In the semiconductor device DEV3, the impurity region R4 is formed before the first insulating film ISL1 is formed, and therefore the ion implantation for forming the impurity region R4 is not performed via the first insulating film ISL1. Therefore, the semiconductor device DEV3 can reduce the acceleration voltage at the time of the ion implantation for forming the impurity region R4. In addition, in the semiconductor device DEV3, since the first insulating film ISL1 can be used as a mask for the ion implantation for forming the impurity region R3 and the impurity region R5, it is not necessary to separately form a resist pattern for the ion implantation for forming the impurity region R3 and the impurity region R5, and therefore the process can be simplified.
[0123] (Fourth embodiment)
[0124] A semiconductor device DEV4 according to a fourth embodiment will be described. Here, the difference from the semiconductor device DEV3 will be mainly described, and redundant description will not be repeated.
[0125] <Structure of semiconductor device DEV4>
[0126] The configuration of the semiconductor device DEV4 will be described below.
[0127] Fig.23 is a cross-sectional view of the semiconductor device DEV4. Fig.23 Shown with Figure 1 The cross section at the position corresponding to II-II in FIG. Fig.23As shown in , the semiconductor device DEV4 includes a semiconductor substrate SUB, an insulating film ISL, a first electrode EL1 and a second electrode EL2, a semi-insulating film SIF, and a passivation film PV. In the semiconductor device DEV4, the ratio of the number of silicon atoms in the semi-insulating film SIF to the sum of the number of silicon atoms and the number of nitrogen atoms is 0.64 or greater. In these respects, the configuration of the semiconductor device DEV4 is the same as that of the semiconductor device DEV3.
[0128] In the semiconductor device DEV4, a plurality of grooves RCS2 and grooves RCS3 are formed on the first surface FS. The first surface FS is recessed toward the second surface SS in the grooves RCS2 and the grooves RCS3. The plurality of grooves RCS2 are arranged to overlap with the impurity region R4 in a plan view. The plurality of grooves RCS2 are spaced apart from each other along a direction from the element region SUB1 toward the terminal region SUB2. The groove RCS3 is disposed between the outermost groove RCS2 and the impurity region R5 in a direction from the element region SUB1 toward the terminal region SUB2. The groove RCS3 may extend to an adjacent side of the impurity region R5.
[0129] In the semiconductor device DEV4, the first insulating film ISL1 is embedded in each of the plurality of grooves RCS2 and RCS3, and the second insulating film ISL2 is provided on the first surface FS in the termination region SUB2 so as to cover the first insulating film ISL1. In these respects, the configuration of the semiconductor device DEV4 is different from that of the semiconductor device DEV3.
[0130] <Modification example>
[0131] In the above description, the ratio of the number of silicon atoms in the semi-insulating film SIF to the sum of the number of silicon atoms and the number of nitrogen atoms is 0.64 or greater, but in the semiconductor device DEV4, the ratio of the number of silicon atoms in the semi-insulating film SIF to the sum of the number of silicon atoms and the number of nitrogen atoms may be less than 0.64. In the semiconductor device DEV4, the semi-insulating film SIF may be formed of a material other than a material containing silicon and nitrogen (e.g., polycrystalline silicon).
[0132] Fig.24 It is the manufacturing process diagram of semiconductor device DEV4. Fig.24 As shown in , the manufacturing method of the semiconductor device DEV4 includes a preparation step S1, an epitaxial growth step S2, a first insulating film forming step S3, a second insulating film forming step S5, a first electrode forming step S6, a semi-insulating film forming step S7, a second electrode forming step S8 and a passivation film forming step S9. In this respect, the manufacturing method of the semiconductor device DEV4 is the same as the manufacturing method of the semiconductor device DEV3.
[0133] In the manufacturing method of the semiconductor device DEV4, the first insulating film forming step S3 is performed after the epitaxial growth step S2. Fig.25 1 is a cross-sectional view illustrating a first insulating film forming step S3 in a method for manufacturing a semiconductor device DEV4. Fig.25 As shown in , in the manufacturing method of the semiconductor device DEV4, the groove RCS3, the plurality of grooves RCS2, and the first insulating film ISL1 are formed in the first insulating film forming step S3.
[0134] In the first insulating film forming step S3 in the manufacturing method of the semiconductor device DEV4, first, a resist pattern is formed on the first surface FS by photolithography. Second, a plurality of grooves RCS2 and grooves RCS3 are formed by etching the first surface FS using the resist pattern as a mask. Third, polysilicon is partially embedded in the plurality of grooves RCS2 and grooves RCS3, for example, by a CVD method. Fourth, the embedded polysilicon is thermally oxidized to form a first insulating film ISL1. Note that when the first insulating film ISL1 protrudes from the groove RCS1, the protruding first insulating film ISL1 can be removed by a CMP method.
[0135] The manufacturing method of the semiconductor device DEV4 has a third impurity region forming step S12 instead of the first impurity region forming step S10. The third impurity region forming step S12 is performed after the first insulating film forming step S3. Fig.26 2 is a cross-sectional view for explaining the third impurity region forming step S12. Fig.26 As shown in, in the third impurity region forming step S12, the impurity region R4 is formed. In the third impurity region forming step S12, first, ion implantation is performed from the first surface FS side using the first insulating film ISL1 as a mask. Therefore, the impurity ions are implanted between two adjacent grooves RCS2. Third, the implanted impurity ions are thermally diffused by annealing the semiconductor substrate SUB.
[0136] The manufacturing method of the semiconductor device DEV4 has a fourth impurity region forming step S13 instead of the second impurity region forming step S11. The fourth impurity region forming step S13 is performed after the third impurity region forming step S12. Fig. 27 2 is a cross-sectional view illustrating the fourth impurity region forming step S13. Fig. 27 As shown in, in the fourth impurity region forming step S13, impurity regions R3 and R5 are formed. First, in the fourth impurity region forming step S13, a resist pattern is formed on the first surface FS by photolithography. Second, ion implantation is performed from the first surface FS side using the resist pattern as a mask. Third, the implanted impurity ions are thermally diffused by annealing the semiconductor substrate SUB.
[0137] In the manufacturing method of the semiconductor device DEV4, after the fourth impurity region forming step S13, the second insulating film forming step S5, the first electrode forming step S6, the semi-insulating film forming step S7, the second electrode forming step S8 and the passivation film forming step S9 are sequentially performed.
[0138] In the semiconductor device DEV4, since the first insulating film ISL1 is embedded in the grooves RCS2 and RCS3, and the second insulating film ISL2 is provided to cover the first insulating film ISL1, there is less possibility of forming a step on the upper surface of the insulating film ISL and thus on the upper surfaces of the first electrode EL1 and the second electrode ISL2. Therefore, according to the semiconductor device DEV4, even when the semi-insulating film SIF is provided on the first electrode EL1 and the second electrode EL2, cracks due to stress concentration are less likely to occur in the semi-insulating film SIF.
[0139] In the semiconductor device DEV3, ion implantation for forming the impurity region R4 is performed between two adjacent grooves RCS2 without the first insulating film ISL1 interposed therebetween. Therefore, the semiconductor device DEV3 can reduce the acceleration voltage at the time of ion implantation for forming the impurity region R4. In the semiconductor device DEV4, since the impurity region R4 can be formed using the first insulating film ISL1 as a mask at the time of ion implantation, it is not necessary to separately form a resist pattern for ion implantation for forming the impurity region R4, and thus the process can be simplified.
[0140] Although the invention made by the present inventors has been described in detail based on the embodiments, it is needless to say that the present invention is not limited to the above-mentioned embodiments, and various modifications can be made without departing from the gist thereof.
Claims
1. A semiconductor device, comprising: Semiconductor substrate; Insulating film; a first electrode and a second electrode; as well as Semi-insulating film, wherein the semiconductor substrate comprises a first surface; Wherein in a plan view, the semiconductor substrate includes a component region and a terminal region surrounding the component region; wherein the semiconductor substrate includes a first impurity region, the first impurity region being formed on the first surface in the termination region; wherein the insulating film covers the first surface in the terminal region; wherein the first electrode is electrically connected to the first impurity region and faces the first impurity region, wherein the insulating film is interposed between the first electrode and the first impurity region; wherein the second electrode is disposed on the insulating film so as to surround the first electrode in a plan view while being spaced apart from the first electrode; wherein the semi-insulating film is arranged to extend across the insulating film between the first electrode and the second electrode in a plan view; wherein the semi-insulating film comprises silicon and nitrogen; wherein a ratio of the number of silicon atoms in the semi-insulating film to the sum of the number of silicon atoms and the number of nitrogen atoms is 0.64 or greater. 2 . The semiconductor device according to claim 1 , wherein the ratio of the number of silicon atoms to the sum of the number of silicon atoms and the number of nitrogen atoms in the semi-insulating film is 0.74 or less. 3 . The semiconductor device according to claim 1 , wherein some of the silicon in the semi-insulating film is bonded with hydrogen. 4 . The semiconductor device according to claim 1 , wherein the semi-insulating film is a mixed crystal of silicon nitride and amorphous silicon. 5 . The semiconductor device according to claim 1 , wherein a thickness of the semi-insulating film is not less than 50 nm and not more than 1000 nm. 6 . The semiconductor device according to claim 1 , wherein a thickness of the insulating film is greater than or equal to 0.5 micrometers and less than or equal to 3.0 micrometers. 7 . The semiconductor device according to claim 1 , wherein the first electrode and the second electrode are electrically connected through the semi-insulating film.
8. The semiconductor device according to claim 1, wherein the semiconductor substrate comprises a second impurity region, the second impurity region being formed on the first surface of the element region; wherein the first electrode is connected to the second impurity region; The impurity concentration in the second impurity region is higher than the impurity concentration in the first impurity region. 9 . The semiconductor device according to claim 1 , further comprising a passivation film formed to cover the semi-insulating film.
10. The semiconductor device according to claim 1, wherein the first electrode has a peripheral edge portion; wherein the semi-insulating film has an inner peripheral edge portion; wherein the semi-insulating film covers the second electrode; and Wherein the inner peripheral edge partially covers the outer peripheral edge portion.
11. The semiconductor device according to claim 1, wherein the semi-insulating film has an inner peripheral edge portion and an outer peripheral edge portion; and The first electrode and the second electrode cover the inner peripheral edge portion and the outer peripheral edge portion respectively.
12. The semiconductor device according to claim 1, wherein the semiconductor substrate comprises a second surface opposite to the first surface in a thickness direction of the semiconductor substrate; wherein a first groove recessed toward the second surface is formed in the first surface, the first groove being formed to overlap with the first impurity region in a plan view; and The insulating film includes a first insulating film and a second insulating film, the first insulating film is embedded in the first groove, and the second insulating film is disposed on the first surface to cover the first insulating film. 13 . The semiconductor device according to claim 12 , wherein the first insulating film is thicker than the second insulating film.
14. The semiconductor device according to claim 1, wherein the semiconductor substrate comprises a second surface opposite to the first surface in a thickness direction of the semiconductor substrate; wherein a plurality of second grooves recessed toward the first surface are formed in the first surface, and the plurality of second grooves are formed to overlap with the first impurity region in a plan view; wherein the plurality of second grooves are spaced apart along a direction from the element region toward the terminal region; and The insulating film includes a first insulating film and a second insulating film, the first insulating film is embedded in each of the plurality of second grooves, and the second insulating film is disposed on the first surface to cover the first insulating film.
15. The semiconductor device according to claim 1, wherein an FRD is formed in the element region.