Cover body and electronic equipment
By using a laminated structure of a fiber substrate and a reflection-enhancing film in the cover of the electronic device, the high-brightness reflection effect is achieved by using light interference, which solves the problems of complex production and low production yield of the ceramic cover, and achieves thinning and cost reduction.
Patent Information
- Application Number
- CN202310565761.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2023-05-18
- Publication Date
- 2024-11-22
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
The prior art is difficult to provide an electronic equipment cover body that is easy to form and has a high brightness reflective effect. The ceramic cover body is made in complex processes and has low production yields.
A fiber substrate is used as the substrate, and a color paint layer and a reflection-enhancing film are provided. The reflection-enhancing film is arranged through the interlacing of the low refractive index layer and the high refractive index layer, and the reflectivity is improved by using light interference to achieve a high-bright reflection effect.
It has achieved a lightweight design and high-gloss reflective effect, with high production yield and low production cost. It has a weight reduction of 30% to 50% compared to ceramic covers and a 30% to 70% reduction in production costs.
Smart Images

Figure CN119012597A_ABST
Abstract
Description
Technical Field
[0001] The embodiments of the present application relate to the technical field of electronic device covers, and more particularly to a cover and an electronic device. Background Art
[0002] In order to improve the user experience of electronic devices such as mobile phones, the covers of electronic devices are designed to be thin and light. The covers can also be made of different materials such as plastics and ceramics to obtain a variety of appearance effects. The plastic cover in the related art has a paint layer on the fiber layer, and the plastic cover cannot achieve a high-brightness reflective effect. The ceramic cover in the related art has a good high-brightness reflective effect. However, the manufacturing process of the ceramic cover is relatively complicated. It has to go through ceramic powder dry pressing mold molding, medium-temperature degreasing, high-temperature sintering, CNC grinding, rough polishing and fine polishing, and the production yield is low. How to provide a cover that is easy to form and has a high-brightness reflective effect has become an urgent problem that the industry needs to solve. Summary of the invention
[0003] The embodiments of the present application provide a cover body and an electronic device, which solve the problem of how to provide a cover body that is easy to shape and has a high-brightness reflective effect.
[0004] The embodiment of the present application adopts the following technical solution:
[0005] In a first aspect, an embodiment of the present application provides a cover body, including a fiber substrate, a color paint layer and an anti-reflection film, wherein the color paint layer is disposed on the outer surface of the fiber substrate, and the anti-reflection film is disposed on the outer surface of the color paint layer, and the anti-reflection film is used for allowing external light to be incident and causing the reflected light to constructively interfere.
[0006] The cover provided in the embodiment of the present application uses a fiber substrate as a base, a color paint layer is arranged on the fiber substrate to provide a base color, and an anti-reflection film is arranged on the color paint layer. When external light is irradiated onto the anti-reflection film, reflected light will be formed on the anti-reflection film, and these reflected lights will undergo constructive interference, and the reflected light will be enhanced, so that the reflectivity of the cover is improved, thereby achieving a high-brightness reflective effect. Compared with the ceramic cover of the related art, the cover of the present application adopts a stacked structure, which is easy to shape and manufacture, has a high production yield, can achieve a lightweight design and a high-brightness reflective effect, and has a low production cost.
[0007] In an optional implementation, the cover body can achieve a reflectivity of 10% to 40% by setting a reflective film of a predetermined number of layers, thickness and material. The reflectivity of a plastic cover body in the related art is less than 5%. The reflectivity of the cover body of this embodiment is enhanced by setting a reflective film, thereby achieving a high-brightness reflective effect.
[0008] In an optional implementation, the cover body can have a reflectivity of 20% to 40% by providing an anti-reflection film of a predetermined number of layers, thickness and material. Compared with a ceramic cover body having a reflectivity of approximately 10% to 20%, the reflectivity of the cover body in this embodiment is enhanced, which can improve the high-brightness reflective effect.
[0009] In an optional implementation, the fiber substrate is a laminated structure, and the fiber substrate includes a resin layer and one or more fiber layers, and the one or more fiber layers are laminated on the resin layer.
[0010] The fiber substrate adopts a laminated structure of a resin layer and a fiber layer, is easy to shape, has a small thickness, has a certain strength, and has certain compression, bending and shear resistance.
[0011] In an optional implementation, when the fiber substrate is a stacked structure, the fiber substrate further includes a weight-reducing material, and the weight-reducing material is disposed on any fiber layer. By arranging the weight-reducing material, the weight of the fiber substrate can be reduced.
[0012] In an optional implementation, the weight-reducing material can be provided as a weight-reducing layer. The weight-reducing layer is easy to shape, can reduce the weight of the fiber substrate, and can make the fiber substrate have a certain strength and a reliable structure.
[0013] In an optional implementation, the fiber substrate is a hybrid structure, and the fiber substrate is mainly composed of a mixture of resin and fiber.
[0014] The fiber substrate adopts a mixed structure of resin and fiber, which is easy to shape, has a small thickness, has a certain strength, and has a certain ability to resist compression, bending and shearing. The fiber substrate can be injection molded with high molding efficiency.
[0015] In an optional implementation, when the fiber substrate is a mixed structure, the fiber substrate is mainly composed of a mixture of resin, fiber and weight-reducing material. By providing the weight-reducing material, the weight of the fiber substrate can be reduced.
[0016] In an optional implementation, the fiber in the fiber substrate is at least one of glass fiber, carbon fiber, inorganic whisker and polymer fiber. The above fibers can be used as reinforcing materials for the fiber substrate, so that the fiber substrate has a certain strength and a reliable structure.
[0017] In an optional implementation, the resin in the fiber substrate is one of epoxy resin, acrylic resin, polyurethane resin, and silicone resin, and the above resin is easy to combine with the fiber layer (weight reduction material) to form a limiting substrate with a small thickness and a certain strength.
[0018] In an optional implementation, the ratio of the weight of the resin in the fiber substrate to the weight of the fiber substrate is in a range of 20% to 70%, which is beneficial to the combination of the resin and the fiber layer and the molding of the fiber substrate.
[0019] In an optional implementation, the fiber substrate has a thickness ranging from 0.2 mm to 1.0 mm. The fiber substrate with this configuration is easy to shape, has a small thickness, and has a certain strength, meeting the requirements of compression resistance, bending resistance, and shear resistance when the cover is applied to electronic equipment.
[0020] In an optional implementation, the weight-reducing material is at least one of glass microspheres, phenolic microspheres, hollow ceramic microspheres, wood powder and fiber powder. These weight-reducing materials have a relatively low density and are easily combined with the resin layer or the fiber layer to reduce the weight of the fiber substrate and make the fiber substrate have a certain strength and a reliable structure.
[0021] In an optional implementation, the particle size range of the weight-reducing material is 10 micrometers (um) to 200um. Setting the particle size of the weight-reducing material within the above range is conducive to distribution in the resin layer or fiber layer, thereby achieving the combination of the weight-reducing material and the resin layer or fiber layer.
[0022] In an optional implementation, the ratio of the weight of the weight-reducing material in the fiber substrate to the weight of the fiber substrate is in the range of 2% to 40%, which can effectively reduce the weight of the fiber substrate and make the fiber substrate have a certain strength, certain compression resistance, bending resistance, and shear resistance, and a reliable structure.
[0023] In an optional implementation, the anti-reflection film includes one or more low-refractive index layers and one or more high-refractive index layers that are alternately stacked in sequence.
[0024] By setting low refractive index layers and high refractive index layers of appropriate thickness, an anti-reflection film that can improve reflectivity is formed. When external light is irradiated onto the anti-reflection film, reflected light will be formed on the two opposite sides of each low refractive index layer (the two opposite sides of each high refractive index layer). The reflected light on the two opposite sides of the same low refractive index layer (high refractive index layer) will undergo constructive interference, which will increase the intensity of the reflected light, thereby improving the reflectivity of the cover and achieving a high-brightness reflective effect.
[0025] In an optional implementation, the refractive index of the low refractive index layer is less than or equal to 1.46. The low refractive index layer is a silicon dioxide layer, a magnesium fluoride layer, an aluminum fluoride layer or others.
[0026] In an optional implementation, the refractive index of the high refractive index layer is greater than or equal to 1.5. The high refractive index layer is a titanium pentoxide layer, a niobium pentoxide layer, an aluminum oxide layer, a zinc sulfide layer or others.
[0027] In an optional implementation, the anti-reflection film includes at least two low refractive index layers and at least one high refractive index layer, wherein one high refractive index layer is sandwiched between two low refractive index layers. The reflected light on both sides of each low refractive index layer (high refractive index layer) produces constructive interference, so that the intensity of the reflected light is enhanced, which can better improve the reflectivity of the cover and achieve a high-brightness reflective effect.
[0028] In an optional implementation, the anti-reflection film is configured with a first low refractive index layer, a high refractive index layer, and a second low refractive index layer stacked in sequence, and the first low refractive index layer is arranged closer to the fiber substrate than the second low refractive index layer. The thickness of the first low refractive index layer ranges from 10 nanometers (nm) to 20nm, the thickness of the high refractive index layer ranges from 20nm to 100nm, and the thickness of the second low refractive index layer ranges from 10nm to 100nm. The anti-reflection film can better improve the reflectivity and achieve a high-brightness reflective effect.
[0029] In an optional implementation, the anti-reflection film includes at least one low refractive index layer and at least two high refractive index layers, wherein one low refractive index layer is sandwiched between two high refractive index layers. The reflected light on both sides of each low refractive index layer (high refractive index layer) produces constructive interference, so that the intensity of the reflected light is enhanced, which can better improve the reflectivity of the cover and achieve a high-brightness reflective effect.
[0030] In an optional implementation, the anti-reflection film is configured with a first high refractive index layer, a low refractive index layer, and a second high refractive index layer stacked in sequence, and the first high refractive index layer is arranged closer to the fiber substrate than the second high refractive index layer. The thickness of the first high refractive index layer ranges from 10nm to 100nm, the thickness of the low refractive index layer ranges from 10nm to 20nm, and the thickness of the second high refractive index layer ranges from 10nm to 100nm. The anti-reflection film can improve the reflectivity well and achieve a high-brightness reflective effect.
[0031] In an optional implementation, the anti-reflection film can be configured as multiple low-refractive index layers and multiple high-refractive index layers that are stacked and staggered. By setting a larger number of low-refractive index layers and high-refractive index layers of appropriate thickness, the intensity of the reflected light can be further improved, thereby improving the reflectivity of the cover.
[0032] In an optional implementation, the thickness of the anti-reflection film ranges from 10 nm to 300 nm. The anti-reflection film is easy to shape and the layer can be made smaller, which can improve the reflectivity and achieve a high-brightness reflective effect.
[0033] In an optional implementation, the thickness of each low refractive index layer or high refractive index layer ranges from 10 nm to 100 nm. The low refractive index layer or high refractive index layer is easy to shape and make the layer small, which can better improve the reflectivity and achieve a high-brightness reflective effect.
[0034] In an optional implementation, the low refractive index layer and the high refractive index layer in the anti-reflection film can be formed by vacuum evaporation coating or magnetron sputtering coating. The anti-reflection film produced by these methods is easy to shape and has a stable structure.
[0035] In an optional implementation, a light-transmitting texture layer is provided on the outer surface of the color paint layer, and the texture layer has a texture pattern. Alternatively, a light-transmitting texture layer is provided on the outer surface of the anti-reflection film, and the texture layer has a texture pattern. The texture layer is light-transmitting, and by providing the texture layer, the cover can display a predetermined texture pattern, thereby improving the user experience.
[0036] In an optional implementation, the texture layer can be an ultraviolet (UV) transfer texture layer. The texture pattern is transferred to a film or other target surface through a UV transfer process. This method is easy to produce a predetermined texture pattern and has a stable structure.
[0037] In an optional implementation, the thickness of the texture layer ranges from 10 nm to 500 nm. The texture layer is easy to shape and can be made smaller, and can better show a predetermined texture pattern.
[0038] In an optional implementation, when a texture layer is provided on the outer surface of the color paint layer, a first varnish layer is provided between the color paint layer and the texture layer. The first varnish layer serves as a transition layer, which facilitates the provision of the texture layer on the color paint layer, so that the combination effect between different layers is better. The thickness of the first varnish layer can range from 10um to 100um, which is easy to shape in terms of process, and the layer can be made smaller.
[0039] In an optional implementation, a first varnish layer is first formed on the outer surface of the color paint layer, and then a texture layer is made on the outer surface of the first varnish layer, thereby forming a texture layer on the color paint layer.
[0040] In an optional implementation, the film is first used as the first varnish layer, then a texture layer is formed on the first varnish layer, and finally the first varnish layer with the texture layer is connected to the outer surface of the color paint layer, thereby forming a texture layer on the color paint layer.
[0041] In an optional implementation, when a texture layer is provided on the outer surface of the anti-reflection film, a first varnish layer is provided between the anti-reflection film and the texture layer. The first varnish layer serves as a transition layer, which facilitates the provision of the texture layer on the anti-reflection film, so that the combination effect between different layers is better. The thickness of the first varnish layer can range from 10um to 100um, which is easy to shape in the process and can make the layer smaller.
[0042] In an optional implementation, a first varnish layer is first formed on the outer surface of the anti-reflection film, and then a texture layer is made on the first varnish layer, thereby forming a texture layer on the anti-reflection film.
[0043] In an optional implementation, the film is first used as the first varnish layer, then a texture layer is formed on the first varnish layer, and finally the first varnish layer with the texture layer is connected to the outer surface of the anti-reflection film to form a texture layer on the anti-reflection film.
[0044] In an optional implementation, the cover body is not provided with a texture layer, and a higher reflectivity is provided by the anti-reflection film of the cover body to enhance the high-brightness reflective effect.
[0045] When setting the color paint layer, the thickness of the color paint layer ranges from 10um to 80um. The color paint layer is easy to form and the layer is made small, which can better present the base color.
[0046] In an optional implementation, a second varnish layer is provided on the outer surface of the anti-reflection film. Alternatively, a second varnish layer is provided on the outer surface of the texture layer. The second varnish layer is located on the outermost side of the cover body, and serves as a protective layer for other layer structures, and also plays an anti-fingerprint role. The second varnish layer needs to allow light to pass through. The thickness of the second varnish layer ranges from 10um to 100um, which is easy to form in the process and makes the layer smaller.
[0047] In a second aspect, an embodiment of the present application provides an electronic device, comprising the above-mentioned cover body.
[0048] In an optional implementation, the electronic device is a mobile phone, and the electronic device includes a display screen, a back cover, and a middle frame, wherein the display screen and the back cover are respectively arranged on opposite sides of the middle frame.
[0049] In an optional implementation, the middle frame may have a frame body portion, and the cover body may be applied to the frame body portion of the middle frame.
[0050] In an optional implementation, the back cover may include a flat plate portion, and the edge of the flat plate portion may be provided with a rounded corner or a chamfered corner. Alternatively, the back cover includes a flat plate portion and a frame portion connected to each other, and the frame portion is extended and provided at the edge of the flat plate portion. In the above two methods, a boss portion may also be provided on the flat plate portion, and the inner space of the boss portion is used for accommodating and installing a camera. The cover body may be applied to back covers of different forms. BRIEF DESCRIPTION OF THE DRAWINGS
[0051] Figure 1 A schematic diagram of the structure of an electronic device provided in an embodiment of the present application;
[0052] Figure 2 for Figure 1 An exploded view of an electronic device;
[0053] Figure 3 A three-dimensional exploded view of an electronic device provided in another embodiment of the present application;
[0054] Figure 4A schematic diagram of the structure of an electronic device provided in another embodiment of the present application;
[0055] Figure 5 A cross-sectional view of a cover provided in an embodiment of the present application;
[0056] Figure 6 A cross-sectional view of a cover body provided in another embodiment of the present application;
[0057] Figure 7 (a) to (c) are cross-sectional views of the fiber substrate in the cover provided by different embodiments of the present application;
[0058] Figure 8 A cross-sectional view of a cover body provided in another embodiment of the present application;
[0059] Fig. 9 A cross-sectional view of a cover body provided in another embodiment of the present application;
[0060] Fig.10 A cross-sectional view of a cover body provided in another embodiment of the present application. DETAILED DESCRIPTION
[0061] In order to make the technical problems, technical solutions and beneficial effects to be solved by the present application clearer, the present application is further described in detail below in conjunction with the accompanying drawings and embodiments. It should be understood that the specific embodiments described herein are only used to explain the present application and are not used to limit the present application. Although the description of the present application will be introduced in conjunction with some embodiments, this does not mean that the features of this application are limited to the implementation mode. On the contrary, the purpose of combining the implementation mode as an application introduction is to cover other options or modifications that may be extended based on the claims of the present application. In order to provide a deep understanding of the present application, many specific details will be included in the following description. The present application can also be implemented without using these details. In addition, in order to avoid confusion or blurring the focus of the present application, some specific details will be omitted in the description. It should be noted that the embodiments in the present application and the features in the embodiments can be combined with each other without conflict.
[0062] It should be noted that when an element is referred to as being "fixed to" or "disposed on" another element, it can be directly on the other element or indirectly on the other element. When an element is referred to as being "connected to" another element, it can be directly connected to the other element or indirectly connected to the other element.
[0063] It should be understood that in the description of the embodiments of the present application, it should be noted that, unless otherwise clearly specified and limited, the terms "installation" and "connection" should be understood in a broad sense. For example, "connection" can be a detachable connection or a non-detachable connection; it can be a direct connection or an indirect connection through an intermediate medium. The terms "length", "width", "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside", "outside", etc. indicate positions or positional relationships based on the positions or positional relationships shown in the accompanying drawings. They are only for the convenience of describing the present application and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as a limitation on the present application.
[0064] In addition, the terms "first" and "second" are used for descriptive purposes only and should not be understood as indicating or implying relative importance or implicitly indicating the number of the indicated technical features. Thus, a feature defined as "first" or "second" may explicitly or implicitly include one or more of the features. In the description of this application, the meaning of "plurality" is two or more, unless otherwise clearly and specifically defined.
[0065] In the embodiments of the present application, "and / or" is only a description of the association relationship of the associated objects, indicating that there can be three relationships. For example, A and / or B can represent: A exists alone, A and B exist at the same time, and B exists alone. In addition, the character " / " in this article generally indicates that the associated objects before and after are in an "or" relationship.
[0066] References to "one embodiment" or "some embodiments" etc. described in this specification mean that a particular feature, structure or characteristic described in conjunction with the embodiment is included in one or more embodiments of the present application. Thus, the phrases "in one embodiment", "in some embodiments", "in some other embodiments", "in some other embodiments", etc. that appear at different places in this specification do not necessarily refer to the same embodiment, but mean "one or more but not all embodiments", unless otherwise specifically emphasized in other ways. The terms "including", "comprising", "having" and their variations all mean "including but not limited to", unless otherwise specifically emphasized in other ways.
[0067] The embodiment of the present application provides a cover body, which can be applied to an electronic device as a shell. The electronic device can be a mobile phone, a watch, a tablet computer, a laptop computer, a super mobile personal computer, an e-book reader, a netbook, a personal digital assistant, an augmented reality (AR) device, a virtual reality (VR) device, a vehicle-mounted device, etc.
[0068] For example, see Figures 1 to 4 The electronic device 100 is a mobile phone. The electronic device 100 includes a display screen 110, a back cover 120 and a middle frame 130. The display screen 110 and the back cover 120 are respectively arranged on opposite sides of the middle frame 130. The middle frame 130 may be provided with components such as a battery, a mainboard, an earpiece, and a speaker. The display screen 110 and the middle frame 130 may be connected by bonding or the like. The middle frame 130 and the back cover 120 may be connected by bonding, snapping or the like.
[0069] When the middle frame 130 is provided, the middle frame 130 may have a frame body portion 131 , and the frame body portion 131 may be provided with a volume key hole, a power key hole, a speaker sound outlet hole, a data line hole, etc.
[0070] When the back cover 120 is provided, the back cover 120 can be implemented in different ways. Figure 2 The back cover 120 may include a flat plate portion 121, and the edge of the flat plate portion 121 may be rounded or chamfered. Figure 3 The back cover 120 includes a flat plate portion 121 and a frame portion 122 connected to each other, and the frame portion 122 is extended at the edge of the flat plate portion 121. Figure 4 A boss portion 123 may also be provided on the flat plate portion 121, and the inner space of the boss portion 123 is used for accommodating and installing a camera.
[0071] The cover body of the embodiment of the present application can be applied to Figures 2 to 4 The different forms of the back cover 120 shown can also be applied to Figure 2 The frame body 131 of the middle frame 130 is shown.
[0072] See also Figure 5 , Figure 6 The embodiment of the present application provides a cover body 1, including a fiber substrate 10, a color paint layer 20 and an anti-reflection film 30, the color paint layer 20 is arranged on the outer surface 10a of the fiber substrate 10, and the anti-reflection film 30 is arranged on the outer surface 20a of the color paint layer 20, and the anti-reflection film 30 is used for external light to be incident and to make the reflected light constructively interfere.
[0073] The fiber substrate 10 is a plate made of fiber material, which can be set to a smaller thickness, has a certain strength, is easy to shape, and can be used as a base for layer structures such as the color paint layer 20 and the anti-reflection film 30. The outer surface 10a of the fiber substrate 10 refers to the surface of the fiber substrate 10 closest to the outer side of the cover body 1 when the cover body 1 is applied to an electronic device.
[0074] The color paint layer 20 is the base color of the cover 1 and can be set to black, white, red or other colors. The outer surface 20a of the color paint layer 20 refers to the surface of the color paint layer 20 closest to the outer side of the cover 1 when the cover 1 is applied to an electronic device.
[0075] See also Figure 6 The anti-reflection film 30 can be directly disposed on the outer surface 20a of the color paint layer 20. Figure 5 The anti-reflection film 30 can be indirectly disposed on the outer surface 20a of the color paint layer 20, that is, the outer surface 20a of the color paint layer 20 is provided with a predetermined layer structure, and the anti-reflection film 30 is disposed on the predetermined layer structure.
[0076] The anti-reflection film 30 is used to improve the reflectivity of the cover 1. The anti-reflection film 30 may include staggered low refractive index layers and high refractive index layers. By setting the low refractive index layers and high refractive index layers of appropriate thickness, each low refractive index layer (high refractive index layer) produces constructive interference with the reflected light on the two sides, thereby enhancing the reflected light. The refractive index of the low refractive index layer and the refractive index of the high refractive index layer are relative, and the refractive index of the low refractive index layer is less than the refractive index of the high refractive index layer.
[0077] Exemplarily, the cover 1 can achieve a reflectivity of 10% to 40% by setting a predetermined number of layers, thickness and material of the anti-reflection film 30. In the plastic cover of the related art, a paint layer is set on the fiber layer, and the external light is diffusely reflected by the color paint layer, and the reflectivity of the plastic cover is less than 5%. In this embodiment, the cover 1 is provided with an anti-reflection film 30, and the reflectivity is enhanced to achieve a high-brightness reflective effect.
[0078] Exemplarily, by setting a reflection-enhancing film 30 of a predetermined number of layers, thickness and material, the cover body 1 can achieve a reflectivity of 20% to 40%. Compared with the reflectivity of a ceramic cover of about 10% to 20%, the reflectivity of the cover body 1 in this embodiment is enhanced, which can improve the high-brightness reflective effect.
[0079] The cover 1 provided in the embodiment of the present application uses a fiber substrate 10 as a base, a color paint layer 20 is arranged on the fiber substrate 10 to provide a base color, and an anti-reflection film 30 is arranged on the color paint layer 20. When external light is irradiated onto the anti-reflection film 30, reflected light will be formed on the anti-reflection film 30, and these reflected lights will undergo constructive interference, and the reflected light will be enhanced, so that the reflectivity of the cover 1 is improved, thereby achieving a high-brightness reflective effect. Compared with the ceramic cover of the related art, the cover 1 of the present application adopts a stacked structure, which is easy to shape and manufacture, has a high production yield, can achieve a lightweight design and a high-brightness reflective effect, and has a low production cost.
[0080] There are different ways to implement the fiber substrate 10. Figure 7In (a) to (c), the first fiber substrate 10 is realized as follows: the fiber substrate 10 is a laminated structure, the fiber substrate 10 includes a resin layer 11 and one or more fiber layers 12, and the one or more fiber layers 12 are stacked on the resin layer 11.
[0081] The fiber substrate 10 adopts a laminated structure of a resin layer 11 and a fiber layer 12, is easy to shape, has a small thickness, has a certain strength, and has a certain compression resistance, bending resistance, and shear resistance. The fiber layer 12 is formed by weaving a fiber material, and a resin material is coated on the fiber layer 12, and the fiber layer 12 coated with the resin material is cured to achieve the combination of the fiber layer 12 and the resin layer 11.
[0082] See also Figure 7 In (b) and (c), when the fiber substrate 10 is a laminated structure, the fiber substrate 10 further includes a weight-reducing material 13, and the weight-reducing material 13 is provided on any fiber layer 12. By providing the weight-reducing material 13, the weight of the fiber substrate 10 can be reduced.
[0083] Exemplarily, the weight-reducing material 13 can be provided as a weight-reducing layer 13a. When there is one fiber layer 12, the weight-reducing layer 13a is provided on one side of the fiber layer 12. When there are multiple fiber layers 12, multiple weight-reducing layers 13a are provided, and multiple weight-reducing layers 13a and multiple fiber layers 12 are stacked and distributed at intervals. The weight-reducing layer 13a is easy to shape, can reduce the weight of the fiber substrate 10, and make the fiber substrate 10 have a certain strength and a reliable structure.
[0084] The second implementation of the fiber substrate 10 is that the fiber substrate 10 is a mixed structure, and the fiber substrate 10 is mainly composed of a mixture of resin and fiber.
[0085] The fiber substrate 10 adopts a mixed structure of resin and fiber, is easy to shape, has a small thickness, has a certain strength, and has a certain ability to resist compression, bending, and shearing. Fibers are added to the molten resin so that the fibers are distributed in the resin, and the resin and fibers are combined after the resin is solidified. The fiber substrate 10 can be injection molded, and the molding efficiency is high.
[0086] When the fiber substrate 10 is a mixed structure, the fiber substrate 10 is mainly composed of a mixture of resin, fiber and weight-reducing material 13. The weight of the fiber substrate 10 can be reduced by providing the weight-reducing material 13. The fiber and weight-reducing material 13 are added to the molten resin so that the fiber and weight-reducing material 13 are distributed in the resin, and the resin, fiber and weight-reducing material 13 are combined after the resin is solidified.
[0087] When the fiber substrate 10 is a laminated structure or a mixed structure, the fiber in the fiber substrate 10 is at least one of glass fiber, carbon fiber, inorganic whisker and polymer fiber, that is, one, two or more fiber materials can be selected. The above fibers can be used as reinforcing materials for the fiber substrate 10, so that the fiber substrate 10 has a certain strength and a reliable structure.
[0088] Glass fiber is an inorganic non-metallic material with good insulation, strong heat resistance, good corrosion resistance, high mechanical strength, etc. The main components of glass fiber are silicon dioxide, aluminum oxide, calcium oxide, boron oxide, magnesium oxide, sodium oxide, etc.
[0089] Carbon fiber is a fiber with a carbon content of more than 90%. It has the characteristics of high temperature resistance, friction resistance, heat conductivity, corrosion resistance, and high axial strength. Carbon fiber is made of acrylic and viscose fibers and is made by high-temperature oxidation and carbonization.
[0090] Inorganic whiskers are short fibers grown from single crystals, which have the characteristics of good insulation, strong heat resistance, good corrosion resistance, high mechanical strength, etc. Inorganic whiskers can be zinc oxide whiskers, magnesium borate whiskers, aluminum borate whiskers, calcium carbonate whiskers, calcium sulfate whiskers, etc.
[0091] The polymer fiber may be polyimide fiber, aromatic polyamide fiber, etc. These polymer fibers have high mechanical strength.
[0092] The fiber substrate 10 has a stacked structure or a mixed structure. When configuring the resin material, the resin in the fiber substrate 10 is one of epoxy resin, acrylic resin, polyurethane resin, and silicone resin, that is, one, two or more resins can be selected. The above resins are easy to combine with the fiber layer 12 (weight reduction material 13) to form a limiting substrate with a smaller thickness and a certain strength.
[0093] For example, see Figure 7 In (a), the fiber substrate 10 is a laminated structure, the resin layer 11 is epoxy resin, the fiber layer 12 is glass fiber, and 2 to 6 layers of glass fiber are stacked on the resin layer 11. The formed fiber substrate 10 has a small thickness and a certain strength.
[0094] Exemplarily, the fiber substrate 10 is a mixed structure, using epoxy resin and glass fiber, and glass fiber is added to the molten epoxy resin to form the fiber substrate 10 through injection molding. The formed fiber substrate 10 has a small thickness and a certain strength.
[0095] In some embodiments, the weight ratio of the resin in the fiber substrate 10 to the weight of the fiber substrate 10 is in the range of 20% to 70%. The fiber substrate 10 has a total weight of 100 parts, and the resin material accounts for 20 to 70 parts, which is conducive to the combination of the resin and the fiber layer 12 and the molding of the fiber substrate 10.
[0096] Illustratively, the ratio of the weight of the resin in the fiber substrate 10 to the weight of the fiber substrate 10 may be 20%, 30%, 40%, 50%, 60%, 70%, etc., as required.
[0097] In some embodiments, the thickness of the fiber substrate 10 ranges from 0.2 millimeters (mm) to 1.0 mm. The fiber substrate 10 with this configuration is easy to shape, has a small thickness, and has a certain strength, meeting the requirements of compression resistance, bending resistance, and shear resistance when the cover 1 is applied to the electronic device 100. The thickness of the fiber substrate 10 can be 0.2 mm, 0.3 mm, 0.5 mm, 0.8 mm, 1.0 mm, etc., which can be set as needed.
[0098] For the fiber substrate 10 having a laminated structure or a mixed structure, see Figure 7 In (b) and (c), when configuring the weight-reducing material 13, the weight-reducing material 13 is at least one of glass microspheres, phenolic microspheres, hollow ceramic microspheres, wood powder and fiber powder, that is, one, two or more weight-reducing materials 13 can be selected. Glass microspheres, phenolic microspheres and hollow ceramic microspheres are all spherical microspheres. Wood powder and fiber powder are powders. These weight-reducing materials 13 have a relatively low density and are easily combined with the resin layer 11 or the fiber layer 12 to reduce the weight of the fiber substrate 10 and make the fiber substrate 10 have a certain strength and a reliable structure.
[0099] When the fiber substrate 10 is a laminated structure or a mixed structure, the particle size range of the weight-reducing material 13 is 10 micrometers (um) to 200um. Particle size refers to the size of particles. The particle size of the weight-reducing material 13 is set within the above range, which is conducive to distribution in the resin layer 11 or the fiber layer 12, so as to achieve the combination of the weight-reducing material 13 and the resin layer 11 or the fiber layer 12.
[0100] Exemplarily, the particle size of the weight-reducing material 13 can be 10um, 20um, 30um, 50um, 80um, 100um, 150um, 200um, etc., as required.
[0101] When the fiber substrate 10 is a laminated structure or a mixed structure, the weight of the weight-reducing material 13 in the fiber substrate 10 and the weight of the fiber substrate 10 are in the range of 2% to 40%. The overall weight of the fiber substrate 10 is 100 parts, and the weight-reducing material 13 accounts for 2 to 40 parts, which can well reduce the weight of the fiber substrate 10, and make the fiber substrate 10 have a certain strength, a certain compression resistance, bending resistance, and shear resistance, and a reliable structure.
[0102] Exemplarily, the ratio of the weight of the weight-reducing material 13 in the fiber substrate 10 to the weight of the fiber substrate 10 can be 2%, 5%, 10%, 15%, 20%, 30%, 40%, etc., which can be set as needed.
[0103] See also Figure 8 , Fig. 9 When the anti-reflection film 30 is provided, the anti-reflection film 30 includes one or more low refractive index layers 31 and one or more high refractive index layers 32 which are alternately stacked in sequence. The refractive index of the low refractive index layer 31 and the refractive index of the high refractive index layer 32 are relative, and the refractive index of the low refractive index layer 31 is less than the refractive index of the high refractive index layer 32.
[0104] By setting the low refractive index layer 31 and the high refractive index layer 32 of appropriate thickness, an anti-reflection film 30 that can improve the reflectivity is formed. When the external light 2 is irradiated onto the anti-reflection film 30, reflected light 3 will be formed on the two opposite sides of each low refractive index layer 31 (the two opposite sides of each high refractive index layer 32), and the reflected light 3 on the two opposite sides of the same low refractive index layer 31 (high refractive index layer 32) will cause constructive interference, that is, the peaks (or troughs) of the two reflected lights 3 arrive at the same place at the same time, the two reflected lights 3 are in phase at this point, and the interference light produces the largest amplitude, which strengthens the intensity of the reflected light 3, thereby improving the reflectivity of the cover 1 and achieving a high-brightness reflective effect.
[0105] The refractive index of the low refractive index layer 31 is less than or equal to 1.46. The low refractive index layer 31 is a silicon dioxide layer, a magnesium fluoride layer, an aluminum fluoride layer or other. When multiple low refractive index layers 31 are provided, the same or different low refractive index layers 31 can be selected respectively.
[0106] The refractive index of the high refractive index layer 32 is greater than or equal to 1.5. The high refractive index layer 32 is a titanium pentoxide layer, a niobium pentoxide layer, an aluminum oxide layer, a zinc sulfide layer or other. When multiple high refractive index layers 32 are provided, the same or different high refractive index layers 32 can be selected respectively.
[0107] In some embodiments, see Figure 8The anti-reflection film 30 includes at least two low refractive index layers 31 and at least one high refractive index layer 32, wherein one high refractive index layer 32 is sandwiched between two low refractive index layers 31. In the anti-reflection film 30, each low refractive index layer 31 (high refractive index layer 32) generates constructive interference with the reflected light 3 on both sides, so that the intensity of the reflected light 3 is enhanced, which can better improve the reflectivity of the cover body 1 and achieve a high-brightness reflective effect.
[0108] For example, see Figure 8 The anti-reflection film 30 is provided with a first low refractive index layer 31a, a high refractive index layer 32 and a second low refractive index layer 31b which are stacked in sequence. The first low refractive index layer 31a is arranged closer to the fiber substrate 10 than the second low refractive index layer 31b. The first low refractive index layer 31a and the second low refractive index layer 31b are both silicon dioxide layers, and the high refractive index layer 32 is a titanium pentoxide layer. The thickness of the first low refractive index layer 31a ranges from 10 nanometers (nm) to 20nm, the thickness of the high refractive index layer 32 ranges from 20nm to 100nm, and the thickness of the second low refractive index layer 31b ranges from 10nm to 100nm. The anti-reflection film 30 can improve the reflectivity well and achieve a high-brightness reflective effect.
[0109] In some embodiments, see Fig. 9 The anti-reflection film 30 includes at least one low refractive index layer 31 and at least two high refractive index layers 32, wherein one low refractive index layer 31 is sandwiched between two high refractive index layers 32. In the anti-reflection film 30, each low refractive index layer 31 (high refractive index layer 32) generates constructive interference with the reflected light 3 on both sides, so that the intensity of the reflected light 3 is enhanced, which can better improve the reflectivity of the cover body 1 and achieve a high-brightness reflective effect.
[0110] For example, see Fig. 9 The anti-reflection film 30 is provided with a first high refractive index layer 32a, a low refractive index layer 31 and a second high refractive index layer 32b stacked in sequence, and the first high refractive index layer 32a is arranged closer to the fiber substrate 10 than the second high refractive index layer 32b. The first high refractive index layer 32a and the second high refractive index layer 32b are both zinc sulfide layers, and the low refractive index layer 31 is a magnesium fluoride layer. The thickness of the first high refractive index layer 32a ranges from 10nm to 100nm, the thickness of the low refractive index layer 31 ranges from 10nm to 20nm, and the thickness of the second high refractive index layer 32b ranges from 10nm to 100nm. The anti-reflection film 30 can improve the reflectivity well and achieve a high-brightness reflective effect.
[0111] It can be understood that the anti-reflection film 30 can be configured as a plurality of low refractive index layers 31 and a plurality of high refractive index layers 32 that are stacked and staggered. By setting a larger number of low refractive index layers 31 and high refractive index layers 32 with appropriate thicknesses, the intensity of the reflected light can be further improved, thereby improving the reflectivity of the cover body 1.
[0112] In some embodiments, see Figure 8 , Fig. 9 , the thickness of the anti-reflection film 30 ranges from 10nm to 300nm. The anti-reflection film 30 of this configuration is easy to shape and make the layer smaller, which can better improve the reflectivity and achieve a high-brightness reflective effect. The thickness of the anti-reflection film 30 can be 10nm, 50nm, 80nm, 100nm, 120nm, 150nm, 200nm, 300nm, etc., which can be set as needed.
[0113] In some embodiments, the thickness of each low refractive index layer 31 or high refractive index layer 32 ranges from 10 nm to 100 nm. The low refractive index layer 31 or high refractive index layer 32 of this configuration is easy to shape and make the layer small, which can better improve the reflectivity and achieve a high-brightness reflective effect. The thickness of each low refractive index layer 31 or high refractive index layer 32 can be 10 nm, 20 nm, 30 nm, 50 nm, 60 nm, 80 nm, 100 nm, etc., which can be set as needed.
[0114] When making the anti-reflection film 30, refer to Figure 8 , Fig. 9 The low refractive index layer 31 and the high refractive index layer 32 in the anti-reflection film 30 can be formed by vacuum evaporation coating or magnetron sputtering coating. The anti-reflection film 30 made by these methods is easy to shape and has a stable structure.
[0115] Vacuum evaporation coating is to heat the film material and evaporate it into gas, so that the particles fly to the target surface and deposit.
[0116] Magnetron sputtering coating uses the film material as the target cathode, applies an electric field between the target and the vacuum chamber wall, ionizes the argon gas and causes the argon ions to bombard the target surface. After the target is hit, the target atoms overflow and fly to the target surface and deposit.
[0117] In some embodiments, see Figure 5 , a light-transmissive texture layer 40 is provided on the outer surface 20a of the color paint layer 20, and the texture layer 40 has a texture pattern. Or, refer to Fig.10 A light-transmissive texture layer 40 is disposed on the outer surface 30a of the anti-reflection film 30, and the texture layer 40 has a texture pattern.
[0118] The texture pattern can be wavy, grid-like, etc., which can be set as needed. The texture layer 40 is light-transmissive. By setting the texture layer 40, the cover 1 can show a predetermined texture pattern, thereby improving the user experience.
[0119] When setting texture layer 40, refer to Figure 5 , Fig.10The texture layer 40 can be an ultraviolet (UV) transfer texture layer. The texture pattern is transferred to a film or other target surface through a UV transfer process. This method is easy to produce a predetermined texture pattern and has a stable structure.
[0120] The UV transfer process requires a mold, and the mold's glue injection part is processed into a predetermined texture pattern through laser engraving and other technologies. The process of making the texture layer 40 includes the following steps: applying UV glue to the mold's glue injection part; placing a film on the glue to make the glue and the film fit together; after UV light curing, the film is separated from the mold, the UV glue is cured on the film, and the predetermined pattern texture on the mold is transferred to the film through the UV glue.
[0121] In some embodiments, see Figure 5 , Fig.10 The thickness of the texture layer 40 ranges from 10 nm to 500 nm. The texture layer 40 of this configuration is easy to shape and make the layer small, and can better show the predetermined texture pattern. The texture layer 40 can be 10 nm, 50 nm, 100 nm, 200 nm, 300 nm, 400 nm, 500 nm, etc., and can be set as needed.
[0122] In some embodiments, see Figure 5 When the texture layer 40 is provided on the outer surface 20a of the color paint layer 20, a first varnish layer 50 is provided between the color paint layer 20 and the texture layer 40. The first varnish layer 50 serves as a transition layer, which facilitates the provision of the texture layer 40 on the color paint layer 20, so that the combination effect between different layers is better.
[0123] The first varnish layer 50 needs to be transparent to light and can be a transparent resin, such as polyethylene terephthalate (PET), polycarbonate (PC), polymethyl methacrylate (PMMA), etc. The thickness of the first varnish layer 50 can range from 10um to 100um, which is easy to shape in the process and can make the layer small.
[0124] For example, see Figure 5 First, the first varnish layer 50 is formed on the outer surface 10 a of the color paint layer 20 , and then the texture layer 40 is made on the outer surface 10 a of the first varnish layer 50 , thereby forming the texture layer 40 on the color paint layer 20 .
[0125] For example, see Figure 5First, the film is used as the first varnish layer 50, and then the texture layer 40 is formed on the first varnish layer 50. Finally, the first varnish layer 50 with the texture layer 40 is connected to the outer surface 10a of the color paint layer 20, so as to form the texture layer 40 on the color paint layer 20.
[0126] In some embodiments, see Fig.10 When the texture layer 40 is provided on the outer surface 30a of the anti-reflection film 30, a first varnish layer 50 is provided between the anti-reflection film 30 and the texture layer 40. The first varnish layer 50 serves as a transition layer, which facilitates the provision of the texture layer 40 on the anti-reflection film 30, so that the combination effect between different layers is better.
[0127] The first varnish layer 50 needs to be transparent to light and can be a transparent resin. The thickness of the first varnish layer 50 can range from 10um to 100um, which is easy to shape in the process and can make the layer small.
[0128] For example, see Fig.10 First, a first varnish layer 50 is formed on the outer surface 30 a of the anti-reflection film 30 , and then a texture layer 40 is made on the first varnish layer 50 , thereby forming the texture layer 40 on the anti-reflection film 30 .
[0129] For example, see Fig.10 First, the film is used as the first varnish layer 50, and then the texture layer 40 is formed on the first varnish layer 50. Finally, the first varnish layer 50 with the texture layer 40 is connected to the outer surface 30a of the anti-reflection film 30, so as to form the texture layer 40 on the anti-reflection film 30.
[0130] In other embodiments, see Figure 6 The cover body 1 may not be provided with the texture layer 40, and the anti-reflection film 30 of the cover body 1 provides a higher reflectivity to enhance the high-brightness reflective effect.
[0131] When setting color paint layer 20, refer to Figure 5 The thickness of the color paint layer 20 ranges from 10um to 80um. The color paint layer 20 of this configuration is easy to shape and make the layer small, which can better present the base color. The thickness of the color paint layer 20 can be 10um, 20um, 30um, 50um, 80um, etc., which can be set as needed.
[0132] In some embodiments, see Figure 5 The outer surface 30a of the anti-reflection film 30 is provided with a second varnish layer 60. Alternatively, see Fig.10, the outer surface 40a of the texture layer 40 is provided with a second varnish layer 60. The second varnish layer 60 is located at the outermost side of the cover body 1, and serves as a protective layer for other layer structures, and also plays an anti-fingerprint role. The second varnish layer 60 needs to allow light to pass through. The second varnish layer 60 can be a transparent resin. The thickness of the second varnish layer 60 ranges from 10um to 100um, which is easy to shape in the process and makes the layer small.
[0133] Several specific embodiments and comparative examples are given below to demonstrate the advantages of the cover body 1 of the embodiment of the present application in terms of reflectivity, weight and production cost.
[0134] The comparative example is a ceramic cover of the related art, with a reflectivity of about 10% to 20% and a weight of about 30 grams (g) to 40g. The manufacturing process of the ceramic cover is relatively complicated, and it needs to go through the steps of ceramic powder dry pressing mold forming, medium temperature degreasing, high temperature sintering, CNC grinding, rough polishing and fine polishing, and the production yield is low.
[0135] Embodiment 1:
[0136] See also Figure 5 The cover 1 of this embodiment includes a fiber substrate 10, a black color paint layer 20, a first varnish layer 50, a texture layer 40, an anti-reflection film 30, and a second varnish layer 60, which are stacked in sequence. The fiber substrate 10 has a thickness of 0.5 mm, a color paint layer 20 has a thickness of 40 μm, a first varnish layer 50 has a thickness of 30 μm, a texture layer 40 has a thickness of 50 nm, an anti-reflection film 30 has a thickness of 150 nm, and a second varnish layer 60 has a thickness of 40 μm.
[0137] The cover body 1 of this embodiment can achieve a reflective effect similar to that of black ceramics, and the reflectivity can reach 10% to 40%. Compared with the ceramic cover body, it can have a better reflectivity to provide a high-brightness reflective effect; the weight of the cover body 1 of this embodiment is about 10g to 20g, which is about 30% to 50% lighter than the ceramic cover body; the production cost is reduced by about 30% to 70%.
[0138] Embodiment 2:
[0139] See also Figure 6 The cover 1 of this embodiment includes a fiber substrate 10, a red color paint layer 20, an anti-reflection film 30, and a second varnish layer 60 which are stacked in sequence. The fiber substrate 10 has a thickness of 0.5 mm, the color paint layer 20 has a thickness of 40 μm, the anti-reflection film 30 has a thickness of 150 nm, and the second varnish layer 60 has a thickness of 40 μm.
[0140] The cover body 1 of this embodiment can achieve a reflective effect similar to that of red ceramics, and the reflectivity can reach 10% to 40%. Compared with the ceramic cover body, it can have a better reflectivity to provide a high-brightness reflective effect; the weight of the cover body 1 of this embodiment is about 10g to 20g, which is about 30% to 50% lighter than the ceramic cover body; the production cost is reduced by about 30% to 70%.
[0141] Embodiment 3:
[0142] The cover 1 of this embodiment comprises a fiber substrate 10, a white color paint layer 20, a first varnish layer 50, a texture layer 40, an anti-reflection film 30, and a second varnish layer 60, which are stacked in sequence. The fiber substrate 10 has a thickness of 0.5 mm, a color paint layer 20 has a thickness of 40 μm, a first varnish layer 50 has a thickness of 30 μm, a texture layer 40 has a thickness of 50 nm, an anti-reflection film 30 has a thickness of 150 nm, and a second varnish layer 60 has a thickness of 40 μm.
[0143] The cover body 1 of this embodiment can achieve a reflective effect similar to that of white ceramics, and the reflectivity can reach 10% to 40%. Compared with the ceramic cover body, it can have a better reflectivity to provide a high-brightness reflective effect; the weight of the cover body 1 of this embodiment is about 10g to 20g, which is about 30% to 50% lighter than the ceramic cover body; the production cost is reduced by about 30% to 70%.
[0144] It can be seen that compared with the ceramic cover of the related art, the cover 1 provided in the embodiment of the present application has better reflectivity to provide a high-brightness reflection effect, is lighter in weight, and has lower production costs.
[0145] Finally, it should be noted that the above is only a specific implementation of the present application, but the protection scope of the present application is not limited thereto. Any changes or substitutions within the technical scope disclosed in the present application should be included in the protection scope of the present application. Therefore, the protection scope of the present application should be based on the protection scope of the claims.
Claims
1. A cover body, characterized in that: include: A fiber substrate, a color paint layer and an anti-reflection film, wherein the color paint layer is arranged on the outer surface of the fiber substrate, the anti-reflection film is arranged on the outer surface of the color paint layer, and the anti-reflection film is used for incident external light and making the reflected light constructively interfere.
2. The cover according to claim 1, characterized in that: The fiber substrate is a laminated structure, comprising a resin layer and one or more fiber layers, wherein the one or more fiber layers are laminated on the resin layer; Alternatively, the fiber substrate is a mixed structure, and the fiber substrate is mainly composed of a mixture of resin and fiber.
3. The cover according to claim 2, characterized in that: The fiber in the fiber substrate is at least one of glass fiber, carbon fiber, inorganic whisker and polymer fiber; And / or, the resin in the fiber substrate is one of epoxy resin, acrylic resin, polyurethane resin and silicone resin; and / or, the ratio of the weight of the resin in the fiber substrate to the weight of the fiber substrate ranges from 20% to 70%; And / or, the fiber substrate has a thickness ranging from 0.2 mm to 1.0 mm.
4. The cover according to claim 2 or 3, characterized in that: When the fiber substrate is a stacked structure, the fiber substrate further comprises a weight-reducing material, and the weight-reducing material is disposed on any one of the fiber layers; When the fiber substrate is a mixed structure, the fiber substrate is mainly formed by mixing resin, fiber and weight-reducing material.
5. The cover according to claim 4, characterized in that: When the fiber substrate is a laminated structure, the weight-reducing material is provided as a weight-reducing layer; Or, the weight-reducing material is at least one of glass microspheres, phenolic microspheres, hollow ceramic microspheres, wood powder and fiber powder; Or, the particle size range of the weight-reducing material is 10um to 200um; Alternatively, the ratio of the weight of the weight-reducing material in the fiber substrate to the weight of the fiber substrate is in a range of 2% to 40%.
6. The cover according to any one of claims 1 to 5, characterized in that: The anti-reflection film comprises one or more low-refractive index layers and one or more high-refractive index layers which are alternately stacked in sequence.
7. The cover according to claim 6, characterized in that: The low refractive index layer is at least one of a silicon dioxide layer, a magnesium fluoride layer, and an aluminum fluoride layer; And / or, the high refractive index layer is at least one of a titanium pentoxide layer, a niobium pentoxide layer, an aluminum oxide layer, and a zinc sulfide layer; And / or, the refractive index of the low refractive index layer is less than or equal to 1.46, and the refractive index of the high refractive index layer is greater than or equal to 1.5; And / or, the thickness of the low refractive index layer or the high refractive index layer ranges from 10 nm to 100 nm; And / or, the anti-reflection film is formed by vacuum evaporation coating or magnetron sputtering coating.
8. The cover according to any one of claims 1 to 7, characterized in that: A light-transmissive texture layer is provided on the outer surface of the color paint layer or the outer surface of the anti-reflection film, and the texture layer has a texture pattern.
9. The cover according to claim 8, characterized in that: The texture layer is an ultraviolet transfer texture layer; Or, the thickness of the texture layer ranges from 10 nm to 500 nm; Or, when a texture layer is provided on the outer surface of the color paint layer, a first varnish layer is provided between the color paint layer and the texture layer; Alternatively, when a texture layer is provided on the outer surface of the anti-reflection film, a first varnish layer is provided between the anti-reflection film and the texture layer.
10. The cover according to any one of claims 1 to 9, characterized in that: The outer surface of the anti-reflection film is provided with a second varnish layer; And / or, the thickness of the color paint layer ranges from 10um to 80um; And / or, the thickness of the anti-reflection film ranges from 10 nm to 300 nm.
11. An electronic device, characterized in that: It comprises the cover body according to any one of claims 1 to 10.