Continuous preparation device and method for metal bare wires
By designing a metal bare wire preparation device using a rotary roller and a diameter detection system, using the toughness/brittleness difference of glass-covered wire and combined with ultrasonic cleaning, the problem of length and diameter limitation in the prior art is solved, and the problem of length and diameter limitations is achieved. Efficient and environmentally friendly ultrafine metal bare silk continuous preparation.
Patent Information
- Application Number
- CN202411099967.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-12
- Publication Date
- 2024-11-26
- Estimated Expiration
- 2044-08-12
AI Technical Summary
The prior art is difficult to achieve continuous preparation of ultrafine metal bare wires with a length greater than 1000 meters and a diameter of 20-60 microns, and the existing peeling methods have problems with low efficiency, damage to the wire, body and environmental friendliness.
A continuous preparation device for bare metal wire was designed to remove the glass layer by peeling the rotary roller and adjusting it through the diameter detection and control system using the toughness/brittleness difference between the inner core alloy wire of the glass-covered wire and the surface glass layer. The winding speed and rotary roller diameter are combined with ultrasonic cleaning to remove residual glass fragments, achieving efficient peeling and cleaning.
Continuous preparation of ultrafine metal bare wires with lengths greater than 1000 meters and diameters of 20-60 microns is achieved, which improves peeling efficiency and quality, and avoids wire damage and environmental pollution.
Smart Images

Figure CN119016444A_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the field of preparation of round-section bare metal wires, and in particular relates to a device and method for continuously preparing the bare metal wires. Background Art
[0002] Micron-level ultrafine metal wires are widely used in communication technology, electronic power, new energy vehicles, biomedicine, national defense and military industries due to their extremely small diameter and excellent mechanical and electromagnetic properties, and are of great strategic significance. For example, micron-level gold-silver-based bonding wires are widely used in the packaging and pin connection of microelectronic components and semiconductor chips due to their good electrical conductivity and heat dissipation; ferromagnetic CoFe-based alloy wires are widely used in many key fields such as target detection and tracking, non-destructive testing, and biomagnetic field measurement due to their excellent soft magnetic properties, high magnetic permeability and excellent magnetic sensitivity; in addition, ultrafine titanium-based wires can be used as structural materials due to their good shape memory function and mechanical properties, and are used in products such as tensile components, transmission shafts and textile reinforcement fibers.
[0003] At present, micron-level ultrafine metal wires are mainly prepared by two methods: multi-pass drawing of alloy bars and rapid quenching of molten alloys. Relatively speaking, drawing has problems such as cumbersome process, short continuous production length and mold loss. Rapid quenching of molten alloys is mainly divided into melt drawing method, inner circle water spinning method and glass coating method. Among them, the inner circle water spinning method and melt drawing method can directly produce metal bare wires, but the diameter of the obtained metal wires is large and still needs to be drawn. At the same time, its process also limits the length of the obtained metal wires, which is difficult to meet the process requirements of continuous batch processing at the back end. At present, only the glass coating method can realize the continuous preparation of 1000-10000m-level ultrafine metal wires. In most applications, metal wires are generally connected to the circuit as a conductive medium. For glass-coated wires, the glass layer on its surface will greatly affect its conductivity, limiting the application of glass-coated metal wires. Therefore, in order to meet the needs of industrial production and application, ultrafine metal bare wires can be obtained by removing the glass layer on the surface of the glass-coated wires.
[0004] At present, the glass layer on the surface of the glass-coated wire is mostly removed by corrosion with hydrofluoric acid or the like. For example, patent CN116179815A removes the glass layer by a mixed corrosive liquid composed of hydrofluoric acid, sodium thiocyanate and urotropine. However, this method of corrosive liquid corrosion usually has problems such as uncontrollable corrosion time, short length of the obtained bare wire, easy corrosion and damage to the metal wire body, and corrosive liquid harming the environment and personnel health. Patent CN107900297A crushes and removes the glass layer on the surface of the glass-coated wire by applying pressure on a flat plate. Although this mechanical method is more controllable than the corrosion method, is not easy to damage the metal wire body, and is friendly to the environment and the human body, it is still inefficient and difficult to achieve continuous removal of the glass layer. In addition, patent CN117655887A discloses a method and equipment for removing the glass layer by grinding with a grinding wheel, which can efficiently achieve continuous removal of the glass layer and winding and arranging of the bare metal wire, but grinding with a grinding wheel can cause scratches on the surface of the metal wire. Summary of the invention
[0005] The object of the present invention is to provide a device and method for continuously preparing bare metal wires, which can realize the task of continuously preparing ultra-fine bare metal wires with a length greater than 1000 meters and a diameter of 20-60 microns.
[0006] In order to achieve the first object of the present invention, the following technical scheme is provided: a continuous preparation device for metal bare wire, comprising a pay-off mechanism for providing glass-coated wire, a peeling mechanism for removing the outer layer of glass of the glass-coated wire, a cleaning mechanism, a winding mechanism for winding the inner core alloy wire of the glass-coated wire, and a control system used in conjunction with the winding mechanism;
[0007] The peeling mechanism comprises a frame and a rotary roller arranged on the frame, wherein the rotary roller is used for winding the glass-coated wire to form a rotary transmission direction;
[0008] The cleaning mechanism is used to remove glass fragments attached to the alloy wire in the inner core of the rolled glass-clad wire;
[0009] The control system includes a diameter detection component arranged at the winding inlet of the winding mechanism, and a control circuit. The control circuit adjusts the winding speed of the winding mechanism or replaces a rotating roller of different diameters by comparing the detection result of the diameter detection component with the diameter required by the preset process.
[0010] The device provided by the present invention utilizes the toughness / brittleness difference between the inner core alloy wire and the surface glass layer of the glass-coated wire, and realizes peeling by rotating and winding the raw materials on the rotating roller: during the rotating winding, the inner core alloy wire has good toughness and will not break; while the surface glass layer will be broken and removed due to brittle fracture. In addition, the peeling effect can be controlled by selecting rotating rollers of different diameters, and the winding speed can be controlled to ensure that the cleaning mechanism can fully remove the glass fragments remaining on the surface, thereby comprehensively controlling and improving the peeling efficiency and peeling quality.
[0011] Specifically, the unwinding mechanism includes an unwinding shaft for mounting the material coil, and an axial end cover used in conjunction with the unwinding shaft, wherein the axial end cover is used to limit the axial sliding of the material coil.
[0012] Specifically, the peeling mechanism further includes a support cover arranged outside the frame, and the support cover is used to support the rotating roller, prevent the glass fragments from splashing, and centrally recover the glass fragments.
[0013] Specifically, the diameter of the rotating roller is 2 to 6 times the diameter of the input glass coating wire and can be replaced according to demand. That is, if the diameter is too small, the rigidity and strength of the rotating roller will decrease and it will be easily damaged; if it is too thick, the peeling effect will be poor.
[0014] Specifically, the winding speed of the winding mechanism is in the range of 0.1 m / min to 10 m / min, that is, if the wire speed is too slow, the efficiency is low, and if the wire speed is too fast, the wire is easily broken.
[0015] Specifically, the cleaning mechanism includes an ultrasonic cleaning machine with a cleaning tank, and a wire guide wheel arranged in the cleaning tank for guiding the glass-coated wire into the cleaning tank to remove residual glass fragments.
[0016] Specifically, the rotary roller is made of a high-hardness, high-rigidity and wear-resistant metal rod to ensure that the force is stable during the process of stripping the surface glass of the glass-coated wire.
[0017] Specifically, the metal rod is a molybdenum rod or a tungsten rod.
[0018] In order to achieve the second object of the present invention, the following technical solution is provided: a continuous preparation method, which is implemented by the above-mentioned continuous preparation device for metal bare wire, comprises the following steps:
[0019] The coil wound with the unprocessed glass coating wire is placed on the unwinding shaft and axially fixed through the axial end cover;
[0020] The unprocessed glass-coated wire on the coil is drawn out and sequentially passes through a peeling mechanism and a cleaning mechanism until it reaches a winding mechanism;
[0021] Test start the equipment to ensure that the peeling mechanism, cleaning mechanism, and diameter detection assembly operate normally, and that the glass-coated wire is routed normally;
[0022] The winding speed is adjusted or the rotating rollers of different diameters are replaced according to the detection result of the diameter detection component until a glass-clad wire core alloy wire having a preset diameter is obtained.
[0023] Specifically, the winding speed is adjusted or the rotating rollers of different diameters are replaced according to the detection results of the diameter detection component. The diameter size in the detection result is actually compared with the preset diameter size to make rough and fine adjustments to the device:
[0024] When the local diameter continuously appears in the detection results to be larger than the preset diameter of the glass-clad wire inner core alloy wire, the diameter of the rotating roller is replaced with one fifth of the current rotating roller diameter;
[0025] When the detection result shows that the local diameter is larger than the preset diameter of the glass-clad wire inner core alloy wire, the diameter of the rotating roller is gradually replaced by two-thirds of the current rotating roller diameter until the glass-clad wire inner core alloy wire consistent with the preset diameter is obtained;
[0026] If the diameter of the replaced rotating roller is less than 2 times the diameter of the glass-coated wire, the winding speed is adjusted: when the detection results continuously show that the local diameter is larger than the preset diameter of the glass-coated wire inner core alloy wire, the winding speed is adjusted to half of the current winding speed. If the local diameter is still larger than the preset diameter of the glass-coated wire inner core alloy wire, the diameter of the rotating roller is gradually replaced with two-thirds of the current rotating roller diameter.
[0027] When the detection results show that the local diameter is larger than the preset diameter of the glass-clad wire core alloy wire, the winding speed is adjusted to four fifths of the current speed, and the adjustment is repeated until a glass-clad wire core alloy wire consistent with the preset diameter is obtained.
[0028] Compared with the prior art, the present invention has the following beneficial effects:
[0029] A corresponding peeling mechanism is designed based on the physical properties of the glass-coated wire to overcome the current problem of being unable to continuously prepare ultra-fine metal bare wires with a length greater than 1000 meters and a diameter of 20-60 microns. BRIEF DESCRIPTION OF THE DRAWINGS
[0030] Figure 1 A schematic diagram of a device for continuously preparing bare metal wire provided in this embodiment;
[0031] Figure 2 A diagram showing the peeling state of the glass-coated wire provided in this embodiment;
[0032] Figure 3A three-dimensional schematic diagram of the peeling mechanism provided in this embodiment;
[0033] Figure 4 A comparison chart of peeling effects of rotary rollers with different diameters provided in this embodiment;
[0034] In the figure, 1, material roll; 2, unwinding shaft; 3, peeling mechanism; 4, first wire guide wheel; 5, second wire guide wheel; 6, ultrasonic cleaning machine; 7, third wire guide wheel; 8, fourth wire guide wheel; 9, fifth wire guide wheel; 10, diameter detection component; 11, winding shaft; 12, winding wheel; 13, bearing; 14, rotating roller; 15, frame; 16, inner core alloy wire; 17, surface glass layer; 18, support cover. DETAILED DESCRIPTION
[0035] In order to make the purpose, technical scheme and advantages of the embodiments of the present invention clearer, the technical scheme in the embodiments of the present invention will be clearly and completely described below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. The components of the embodiments of the present invention generally described and shown in the drawings here can be arranged and designed in various different configurations. Therefore, the following detailed description of the embodiments of the present invention provided in the drawings is not intended to limit the scope of the claimed invention, but merely represents selected embodiments of the present invention. Based on the embodiments in the present invention, all other embodiments obtained by ordinary technicians in this field without making creative work are within the scope of protection of the present invention.
[0036] like Figure 1 As shown, the continuous preparation device of metal bare wire provided in this embodiment includes a wire-releasing mechanism for providing glass-coated wire, a peeling mechanism 3 for removing the outer layer of glass of the glass-coated wire, a cleaning mechanism for removing residual glass fragments, a winding mechanism for winding the inner core alloy wire of the glass-coated wire, and a control system used in conjunction with the winding mechanism.
[0037] The glass-coated wire is guided by a first wire guide wheel 4, a second wire guide wheel 5, a third wire guide wheel 7, a fourth wire guide wheel 8 and a fifth wire guide wheel 9 to complete the peeling and winding tasks.
[0038] The unwinding mechanism includes an unwinding shaft 2 for mounting the material roll 1 and an axial end cover used in conjunction with the unwinding shaft 2, wherein the axial end cover is used to limit the axial sliding of the material roll 1.
[0039] The winding mechanism includes a winding shaft 11 connected to the output motor, and a winding wheel 12 fixed on the winding shaft 11, wherein the circumferential surface of the winding wheel 12 is made of silicone material to prevent the wound product from slipping.
[0040] The cleaning mechanism includes an ultrasonic cleaning machine 6 with a cleaning tank and guide wire wheels, the guide wire wheels include a third guide wire wheel 7 and a fourth guide wire wheel 8, and the rotation center connection line of the third guide wire wheel 7 and the fourth guide wire wheel 8 is parallel to the bottom of the cleaning tank to ensure that the glass-coated wire is fully cleaned.
[0041] The control system includes a diameter detection component 10 arranged at the winding inlet of the winding mechanism, and a control circuit. The control circuit adjusts the winding speed of the winding mechanism by comparing the detection result of the diameter detection component 10 with the diameter required by the preset process. The diameter detection component selected in this embodiment mainly measures the diameter of the metal bare wire in real time, and the peeling effect can be directly judged by the diameter of the metal wire after peeling and cleaning.
[0042] like Figure 2 As shown, it is a demonstration diagram of glass-coated wire peeling provided in this embodiment. The device provided in this embodiment utilizes the toughness / brittleness difference between the inner core alloy wire 16 and the surface glass layer 17 of the glass-coated wire to achieve peeling by rotationally winding the raw materials on the rotating roller 14: during the rotational winding, the inner core alloy wire 16 has better toughness and will not break; while the surface glass layer 17 will be broken and removed due to brittle fracture.
[0043] like Figure 3 , which is a three-dimensional schematic diagram of the peeling mechanism provided in this embodiment, includes a frame 15 and a support cover 18 fixed on the frame, and the support cover 18 is connected to the rotating roller 14 through a bearing 13. The rotating roller 14 is used to wind the glass-coated wire and form a rotating transmission; the bearing 13 reduces the rotation damping of the rotating roller 14, so that the rotating roller 14 can rotate with the glass-coated wire wound thereon, preventing the rotating roller 14 from breaking the glass-coated wire during the peeling process; the support cover 18 supports the rotating roller 14 and can prevent the splashing of glass fragments during peeling.
[0044] More specifically, the rotating roller 14 provided in this embodiment uses a molybdenum rod, and the diameter is 2 to 6 times the diameter of the input glass cladding wire. If the diameter is too small, the rigidity and strength of the rotating roller will decrease and it will be easily damaged; if it is too thick, the peeling effect will be poor. In order to better illustrate the influence of the diameter provided in this embodiment on the peeling effect, the diameter of the glass cladding wire in the design test is about 65μm, of which the diameter of the inner core alloy wire is about 40μm, and two molybdenum rods with the same material but diameters of 325μm and 500μm are selected. The peeling effect is as follows: Figure 4 As shown, Figure 4 The red line in the middle is the diameter of the glass-coated wire core alloy wire after the molybdenum rod with a diameter of 325μm is peeled. Figure 4 The blue line in the middle is the diameter of the glass-coated wire core alloy wire after the molybdenum rod with a diameter of 500μm is peeled. Figure 4 The diameter of the unpeeled glass-coated wire in the middle black line;
[0045] It can be seen from the figure that when a rotating roller in a corresponding range is selected for the diameter of the unpeeled glass-coated wire, the corresponding peeling effect can be effectively improved.
[0046] At the same time, the winding speed of the winding mechanism mentioned in this embodiment is 0.2m / min.
[0047] This embodiment also provides a continuous preparation method, which is implemented by the continuous preparation device for metal bare wire provided in the above embodiment, and the steps include the following:
[0048] The coil wound with the unprocessed glass coating wire is placed on the unwinding shaft and axially fixed through the axial end cover;
[0049] The unprocessed glass-coated wire on the coil is drawn out and sequentially passes through a peeling mechanism and a cleaning mechanism until it reaches a winding mechanism;
[0050] Test start the equipment to ensure that the peeling mechanism, cleaning mechanism, and diameter detection assembly operate normally, and that the glass-coated wire is routed normally;
[0051] According to the test results of the diameter detection component, the winding speed is adjusted or the rotating rollers of different diameters are replaced until the glass-coated wire with the preset diameter is obtained. The process mainly compares the diameter size in the current test results with the preset diameter, and adjusts the design parameters of the device through coarse and fine adjustments:
[0052] When the local diameter continuously appears in the detection results to be larger than the preset diameter of the glass-clad wire inner core alloy wire, the diameter of the rotating roller is replaced with one fifth of the current rotating roller diameter;
[0053] When the detection result shows that the local diameter is larger than the preset diameter of the glass-clad wire inner core alloy wire, the diameter of the rotating roller is gradually replaced by two-thirds of the current rotating roller diameter until the glass-clad wire inner core alloy wire consistent with the preset diameter is obtained;
[0054] If the diameter of the replaced rotating roller is less than 2 times the diameter of the glass-coated wire, the winding speed is adjusted: when the detection results continuously show that the local diameter is larger than the preset diameter of the glass-coated wire inner core alloy wire, the winding speed is adjusted to half of the current winding speed. If the local diameter is still larger than the preset diameter of the glass-coated wire inner core alloy wire, the diameter of the rotating roller is gradually replaced with two-thirds of the current rotating roller diameter.
[0055] When the detection results show that the local diameter is larger than the preset diameter of the glass-coated wire core alloy wire, the winding speed is adjusted to four-fifths of the current speed, and the adjustment is repeated until the glass-coated wire core alloy wire with the preset diameter is obtained. The peeling effect is further optimized by means of coarse and fine adjustment.
Claims
1. A device for continuously preparing bare metal wire, characterized in that: It includes a pay-off mechanism for providing glass-clad wire, a peeling mechanism for removing the outer glass of the glass-clad wire, a cleaning mechanism, a winding mechanism for winding the inner core alloy wire of the glass-clad wire, and a control system used in conjunction with the winding mechanism; The peeling mechanism comprises a frame and a rotary roller arranged on the frame, wherein the rotary roller is used for winding the glass-coated wire to form a rotary transmission direction; The cleaning mechanism is used to remove glass fragments attached to the alloy wire in the inner core of the rolled glass-clad wire; The control system includes a diameter detection component arranged at the winding inlet of the winding mechanism, and a control circuit. The control circuit adjusts the winding speed of the winding mechanism or replaces a rotating roller of different diameters by comparing the detection result of the diameter detection component with the diameter required by the preset process.
2. The continuous preparation device for bare metal wire according to claim 1, characterized in that: The unwinding mechanism comprises an unwinding shaft for mounting the material coil, and an axial end cover used in conjunction with the unwinding shaft, wherein the axial end cover is used to limit the axial sliding of the material coil.
3. The continuous preparation device for bare metal wire according to claim 1, characterized in that: The peeling mechanism also includes a support cover arranged outside the frame, and the support cover is used to support the rotating roller, prevent glass fragments from splashing, and centrally recover glass fragments.
4. The continuous preparation device for bare metal wire according to claim 1, characterized in that: The diameter of the rotating roller is 2 to 6 times the diameter of the input glass cladding wire.
5. The continuous preparation device for bare metal wire according to claim 1, characterized in that: The winding speed range of the winding mechanism is 0.1 m / min to 10 m / min.
6. The continuous preparation device for bare metal wire according to claim 1, characterized in that: The cleaning mechanism comprises an ultrasonic cleaning machine with a cleaning tank, and a wire guide wheel arranged in the cleaning tank for guiding the glass-clad wire to enter the cleaning tank.
7. The continuous preparation device for bare metal wire according to claim 1, characterized in that: The rotary roller is made of a high-hardness, high-rigidity and wear-resistant metal bar.
8. A continuous preparation method, characterized in that: The method is realized by the continuous preparation device for bare metal wire according to any one of claims 1 to 7, and the steps include: The coil wound with the unprocessed glass coating wire is placed on the unwinding shaft and axially fixed through the axial end cover; The unprocessed glass-coated wire on the coil is drawn out and sequentially passes through a peeling mechanism and a cleaning mechanism until it reaches a winding mechanism; Test start the equipment to ensure that the peeling mechanism, cleaning mechanism, and diameter detection assembly operate normally, and that the glass-coated wire is routed normally; The winding speed is adjusted or the rotating rollers of different diameters are replaced according to the detection result of the diameter detection component until a glass-clad wire core alloy wire having a preset diameter is obtained.
9. The continuous preparation method according to claim 8, characterized in that: According to the detection result of the diameter detection component, the winding speed is adjusted or the rotating roller with different diameters is replaced, which specifically includes the following: When the local diameter continuously appears in the detection results to be larger than the preset diameter of the glass-clad wire inner core alloy wire, the diameter of the rotating roller is replaced with one fifth of the current rotating roller diameter; When the detection result shows that the local diameter is larger than the preset diameter of the glass-clad wire inner core alloy wire, the diameter of the rotating roller is gradually replaced by two-thirds of the current rotating roller diameter until the glass-clad wire inner core alloy wire consistent with the preset diameter is obtained; If the diameter of the replaced rotating roller is less than 2 times the diameter of the glass-coated wire, the winding speed is adjusted: when the detection results continuously show that the local diameter is larger than the preset diameter of the glass-coated wire inner core alloy wire, the winding speed is adjusted to half of the current winding speed. If the local diameter is still larger than the preset diameter of the glass-coated wire inner core alloy wire, the diameter of the rotating roller is gradually replaced with two-thirds of the current rotating roller diameter. When the detection results show that the local diameter is larger than the preset diameter of the glass-clad wire core alloy wire, the winding speed is adjusted to four fifths of the current speed, and the adjustment is repeated until a glass-clad wire core alloy wire consistent with the preset diameter is obtained.
Citation Information
Patent Citations
Device for removing glass coatings on alloy microwires
CN102976634A
Ultrafine metal wire continuous ultrasonic cleaning device
CN108380693A
Metal wire scrap edge collecting device for wired glass
CN109353891A
Device for removing glass coating of alloy fine wire
CN202220131U
Wear-resistant anti-pilling shoe belt
CN211581769U
Cited By
Metal wire polishing device
CN120170619A
A wire polishing device
CN120170619B