Titanium alloy plate manufacturing method
By rapidly cooling during heating and stamping in the manufacturing of titanium alloy sheets, the needle-like structure is formed, which solves the problem of crystallization structure failure during stamping, and realizes the ultra-low Young's coefficient and high mechanical characteristics of titanium alloy sheets, which are suitable for golf Club head.
Patent Information
- Application Number
- CN202310601032.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2023-05-25
- Publication Date
- 2024-11-26
AI Technical Summary
During the manufacturing process of titanium alloy rod heads, the stamping process easily destroys the crystalline structure of the titanium alloy sheet, resulting in changes in its mechanical characteristics and failing to achieve the expected performance.
The titanium alloy substrate is heated to 860°C to 910°C and then stamped, and is rapidly cooled to below 400°C at the same time to form a semi-finished product with a needle-like structure, and then it is kept warm between 300°C and 500°C and cooled with an inert gas. Titanium alloy sheets with ultra-low Young's coefficient were produced.
It keeps the mechanical characteristics of titanium alloy sheets unchanged, improves its tensile strength and submersible strength, is suitable for golf club heads, extends the contact time between balls and titanium alloy sheets, and is suitable for non-competitive golf club heads.
Smart Images

Figure CN119020564A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to a titanium alloy manufacturing method, in particular to a titanium alloy plate manufacturing method with an ultra-low Young's modulus. Background Art
[0002] In the early days, golf clubs were mostly made of wood, which were gradually replaced by stainless steel. In modern times, titanium metal has been gradually introduced into the club heads of golf clubs. Titanium alloy club heads have excellent stability and elasticity. Titanium alloys have low density, high strength and good corrosion resistance. Under the same weight, club heads made of titanium alloys have excellent stability and elasticity, allowing players to hit the ball farther and straighter, thus promoting the development of titanium golf clubs.
[0003] Generally speaking, in the manufacture of titanium alloy club heads, most of the semi-finished titanium alloy sheets on the market are stamped into the required shape to obtain the finished titanium alloy sheets. The semi-finished titanium alloy sheets on the market are processed by special processes to give them specific mechanical properties, such as specific elasticity, rigidity, ductility, etc. However, during the stamping process, the crystal structure in the semi-finished titanium alloy sheets is easily destroyed, which changes its mechanical properties and makes the club unable to achieve the expected performance.
[0004] In view of this, the inventor has devoted himself to studying the above-mentioned prior art and has applied theoretical knowledge to try his best to solve the above-mentioned problems, which has become the goal of the inventor's improvement. Summary of the invention
[0005] The invention provides a method for manufacturing a titanium alloy plate with an ultra-low Young's modulus.
[0006] The present invention provides a method for manufacturing a titanium alloy plate, which comprises the following steps: providing a titanium alloy substrate, the titanium alloy substrate comprising titanium, aluminum, molybdenum, vanadium, silicon, iron, carbon, zirconium and oxygen, wherein the proportion of aluminum in the titanium alloy substrate is 3.9-6.5 at%, the proportion of molybdenum is 2.3-2.7 at%, the proportion of vanadium is 3.8-4.5 at%, the proportion of silicon is not more than 0.3 at%, the proportion of iron is not more than 0.2 at%, and the total proportion of carbon, zirconium and oxygen is not more than 0.1 at%; heating the titanium alloy substrate to 860-910° C., then stamping and rapidly cooling to below 400° C. to obtain a semi-finished product, wherein the metallographic structure of the semi-finished product has a needle-like structure, the rapid cooling rate is not less than 300° C. per second, and the width of the needle-like structure is between 0.001 and 0.002 mm; and the semi-finished product is kept at a temperature between 300-500° C. for a total of 30-90 minutes and then cooled to 20-30° C. with an inert gas to obtain a titanium alloy plate.
[0007] In one embodiment of the present invention, the titanium alloy plate manufacturing method further comprises the step of heating the semi-finished product to 860° C. to 910° C. and then stamping it and rapidly cooling it to below 400° C. The aforementioned steps can be repeated for a predetermined number of times.
[0008] In one embodiment of the present invention, the density of the titanium alloy plate is 4.60-4.62 g / cm 3 .
[0009] In one embodiment of the present invention, the β-phase content of the titanium alloy substrate is 3% to 30%.
[0010] In one embodiment of the present invention, the semi-finished product is placed in a continuous furnace and heated to 860° C. to 910° C. and then input into a stamping machine. The titanium alloy substrate is stamped in the stamping machine and rapidly cooled to below 400° C. at the same time.
[0011] In one embodiment of the present invention, the titanium alloy substrate is placed in a continuous furnace and heated to 860° C. to 910° C. and then fed into a punching machine. The titanium alloy substrate is punched in the punching machine and rapidly cooled to below 400° C. at the same time.
[0012] In one embodiment of the present invention, the stamping machine is provided with a heat sink, and the heat sink contacts the titanium alloy substrate or the semi-finished product during stamping. A flow channel may be provided in the heat sink.
[0013] The titanium alloy plate manufacturing method of the present invention rapidly cools the titanium alloy substrate during stamping so that the titanium in the titanium alloy plate forms crystals of a needle structure, thereby making the titanium alloy plate have an ultra-low Young's series. BRIEF DESCRIPTION OF THE DRAWINGS
[0014] Figure 1 The present invention is a flowchart of a method for manufacturing a titanium alloy plate according to an embodiment of the present invention.
[0015] Figure 2 The present invention is a flowchart of the forming steps in a method for manufacturing a titanium alloy sheet according to an embodiment of the present invention.
[0016] Figure 3 The present invention is a flowchart of the processing steps in a method for manufacturing a titanium alloy plate according to an embodiment of the present invention.
[0017] Figure 4 The figure is a schematic diagram of a solution treatment step in a method for manufacturing a titanium alloy plate according to an embodiment of the present invention.
[0018] Figure 5 to Figure 6 The figure is a schematic diagram of a stamping step in a method for manufacturing a titanium alloy sheet according to an embodiment of the present invention.
[0019] Figure 7It is a schematic diagram of the secondary stamping step in the method for manufacturing a titanium alloy plate according to an embodiment of the present invention.
[0020] Figure 8 The semi-finished product manufactured by the titanium alloy plate manufacturing method according to one embodiment of the present invention has needle-like structure crystals.
[0021] Fig. 9 A comparison table of specific time parameters and temperature parameters for aging treatment of titanium alloy plates and the corresponding mechanical properties.
[0022] Description of reference numerals:
[0023] 110: titanium alloy substrate;
[0024] 120: semi-finished product;
[0025] 120D: width;
[0026] 200 continuous furnace;
[0027] 300: punching machine;
[0028] 310: punch;
[0029] 320: Mould. DETAILED DESCRIPTION
[0030] The present invention provides a method for manufacturing a titanium alloy plate, which is used to manufacture a titanium alloy plate with an ultra-low Young's modulus, wherein the ultra-low Young's modulus refers to a Young's modulus less than 95 GPa.
[0031] See also Figure 1 The present invention provides a method for manufacturing a titanium alloy sheet, which includes the steps described below.
[0032] See also Figure 1 First, in step a, a titanium alloy substrate 110 is provided, and the shape of the titanium alloy substrate 110 is not limited. The titanium alloy substrate 110 contains titanium, aluminum, molybdenum, vanadium, silicon, iron, carbon, zirconium, and oxygen. In the titanium alloy substrate 110 of the present embodiment, aluminum accounts for 3.9 to 6.5 at%, molybdenum accounts for 2.3 to 2.7 at%, vanadium accounts for 3.8 to 4.5 at%, silicon accounts for no more than 0.3 at%, iron accounts for no more than 0.2 at%, and carbon, zirconium, and oxygen account for no more than 0.1 at%. The remaining part of the titanium alloy substrate 110 is titanium, and titanium may contain unavoidable impurities. The β-phase content of the titanium alloy substrate is 3% to 30%. Among them, the atomic percentage (at%) of a certain element in the titanium alloy substrate 110 is: (the number of atoms of the element) / (the sum of the number of atoms of all elements in the alloy).
[0033] See also Figure 1Then, step b is a forming step, in which solid solution is carried out and then stamping and rapid cooling are carried out simultaneously. The forming step at least includes the following steps: Figure 2 and Figures 4 to 6 In step b1, the titanium alloy substrate 110 is placed in a continuous furnace 200 and heated to a temperature of 860°C to 910°C, which is approximately equal to the melting point of the titanium alloy substrate 110. The temperature is maintained for about 20 minutes, and then the titanium alloy substrate 110 is input into a punching machine 300. The titanium alloy substrate 110 of this embodiment is punched in the punching machine 300 and rapidly cooled to below 400°C to obtain a semi-finished product 120. Specifically, the rapid cooling rate is not less than 300°C per second. Figure 6 and Figure 8 After rapid cooling, the semi-finished product 120 has a needle-like structure crystal, and the width 120D of the needle-like structure is between 0.001 and 0.002 mm. The needle-like structure makes the semi-finished product 120 have an ultra-low Young's modulus, wherein the ultra-low Young's modulus refers to a Young's modulus less than 95 GPa.
[0034] See also Figure 1 , Figure 2 and Figure 7 According to the specification requirements of titanium alloy plates (such as shape, size, density, etc.), when one stamping cannot meet the required specifications, a secondary stamping step can be performed:
[0035] In step b2, the semi-finished product 120 is placed in the continuous furnace 200, heated to 860°C to 910°C, and then input into the punching machine 300. The semi-finished product 120 is punched in the punching machine 300 and rapidly cooled to below 400°C. Step b2 can be repeated a predetermined number of times according to the specification requirements of the titanium alloy plate before executing step c. For example, step b2 is repeated a predetermined number of times until the thickness of the semi-finished product 120 reaches the required size. After the forming step is completed, the mechanical properties of the semi-finished product 120 can be determined. In this embodiment, the semi-finished product has an ultra-low Young's modulus of less than 95GPa, and the density of the semi-finished product is between 4.60 and 4.62g / cm 3 The tensile strength of the semi-finished product is between 150 and 170 ksi (thousand pounds force per square inch), and the yield strength of the semi-finished product is between 130 and 150 ksi.
[0036] See also Figures 4 to 7The punching machine 300 has a punch 310, which can be a movable steel block. During punching, the punch 310 squeezes the titanium alloy substrate 110 or the semi-finished product 120 to deform it. The punch 310 can also cooperate with the mold 320 to extrude the titanium alloy substrate 110 or the semi-finished product 120 into a specific shape as required. The mold 320 can be a steel block. The punching machine 300 is provided with a heat sink, and the heat sink contacts the titanium alloy substrate 110 or the semi-finished product 120 during punching, thereby removing heat energy from the titanium alloy substrate 110 to achieve a rapid cooling effect. The present invention does not limit the form of the heat sink, and the heat sink can be set at any position on the punching machine 300 or formed by any part on the punching machine 300, so it is not specified in the figure. For example, the heat sink can be a steel block, and a flow channel can also be provided in the heat sink for heat dissipation.
[0037] See also Figure 1 and Figure 3 , following the forming step of step b, step c is an aging step, which at least includes a temperature holding step c1 and a cooling step c2. Fig. 9 Different holding temperature parameters and time parameters can make titanium alloy plates achieve different mechanical properties.
[0038] See also Figure 1 and Figure 3 and Fig. 9 In this embodiment, in step c1, the semi-finished product obtained in step b is kept at a temperature between 300°C and 500°C for a total of 30 to 90 minutes. Specifically, in this embodiment, the semi-finished product is placed in a vacuum heat treatment furnace (not shown) and heated to 400°C for 60 minutes. The structural strength of the titanium alloy plate can be improved by the aging treatment step.
[0039] Following step c1, in step c2, the semi-finished product that has been initially cooled is taken out from the vacuum heat treatment furnace, and then rapidly cooled to the ambient temperature of 20°C to 30°C with an inert gas to obtain a titanium alloy plate. The inert gas can be argon. The titanium alloy plate has an ultra-low Young's modulus of less than 95GPa. The density of the titanium alloy plate of this embodiment is between 4.60 and 4.62g / cm3, the tensile strength of the titanium alloy plate of this embodiment is between 150 and 170ksi (thousand pounds force per square inch), and the yield strength of the titanium alloy plate of this embodiment is between 130 and 150ksi.
[0040] The titanium alloy sheet manufacturing method of the present invention performs heat treatment and forming on the titanium alloy substrate at the same time, so the crystal structure of the titanium alloy sheet will not be destroyed and the mechanical properties will not be changed due to the subsequent stamping process. Therefore, the titanium alloy sheet obtained by the titanium alloy sheet manufacturing method of the present invention has better mechanical properties than the semi-finished product secondary stamping process. The needle-like structure of the titanium alloy sheet obtained by the titanium alloy sheet manufacturing method of the present invention makes the surface of the titanium alloy sheet highly elastic, so when it is used in a golf club head, the contact time (CT, characteristic time) between the ball and the titanium alloy sheet when hitting the ball is larger and higher than the upper limit of 257 microseconds commonly used in current golf competitions. Therefore, the titanium alloy sheet of the present invention is suitable for use in non-competitive golf club heads.
Claims
1. A method for manufacturing a titanium alloy sheet, comprising the following steps: a) providing a titanium alloy substrate, wherein the titanium alloy substrate comprises titanium, aluminum, molybdenum, vanadium, silicon, iron, carbon, zirconium and oxygen, wherein the proportion of aluminum in the titanium alloy substrate is 3.9-6.5 at%, the proportion of molybdenum is 2.3-2.7 at%, the proportion of vanadium is 3.8-4.5 at%, the proportion of silicon is no more than 0.3 at%, the proportion of iron is no more than 0.2 at%, and the total proportion of carbon, zirconium and oxygen is no more than 0.1 at%; b) heating the titanium alloy substrate to 860° C. to 910° C., then stamping and rapidly cooling to below 400° C. to obtain a semi-finished product, wherein the metallographic structure of the semi-finished product has a needle-like structure, the rapid cooling rate is not less than 300° C. per second, and the width of the needle-like structure is between 0.001 and 0.002 mm; and c) the semi-finished product is kept at a temperature between 300° C. and 500° C. for a total of 30 to 90 minutes and then cooled to 20° C. to 30° C. with an inert gas to obtain a titanium alloy plate.
2. The method for manufacturing a titanium alloy sheet material according to claim 1, further comprising the steps of: b2) heating the semi-finished product to 860° C. to 910° C. and then punching it and rapidly cooling it to below 400° C. at the same time.
3. The method for manufacturing a titanium alloy sheet material as claimed in claim 2, wherein step b comprises repeating step b2 for a predetermined number of times before executing step c.
4. The method for manufacturing a titanium alloy sheet according to claim 1, wherein the density of the titanium alloy sheet is 4.60-4.62 g / cm 3 .
5. The method for manufacturing a titanium alloy sheet material according to claim 1, wherein the β-phase content of the titanium alloy substrate is 3% to 30%.
6. The method for manufacturing a titanium alloy sheet material as claimed in claim 1, wherein in step b, the semi-finished product is placed in a continuous furnace and heated to 860°C to 910°C and then input into a stamping machine, and the titanium alloy substrate is stamped in the stamping machine and rapidly cooled to below 400°C at the same time.
7. The method for manufacturing a titanium alloy sheet material as described in claim 2, wherein in step b2, the titanium alloy substrate is placed in a continuous furnace and heated to 860°C to 910°C and then input into a stamping machine, and the titanium alloy substrate is stamped in the stamping machine and rapidly cooled to below 400°C at the same time. 8 . The method for manufacturing a titanium alloy plate according to claim 1 , wherein the punching machine is provided with a heat sink, and the heat sink contacts the titanium alloy substrate during punching.
9. The method for manufacturing a titanium alloy sheet material according to claim 2, wherein the stamping machine is provided with a heat sink, and the heat sink contacts the semi-finished product during stamping.
10. The method for manufacturing a titanium alloy plate according to claim 8 or 9, wherein a flow channel is provided in the heat dissipation block.