Method and device for establishing ion doping model, electronic equipment and readable medium
By obtaining the crystal structure primitive file of rutile titanium dioxide, writing substituted ion information and performing cellular expansion processing, the target model is determined based on free energy, and the problem of insufficient model modeling accuracy in the prior art is solved, and the model is improved Accuracy and reliability.
Patent Information
- Application Number
- CN202411036633.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-30
- Publication Date
- 2024-11-26
AI Technical Summary
In the prior art, the modeling accuracy of the ion-doped crystal structure model is low and it is difficult to get close to the real situation of the experiment, resulting in errors in material analysis.
By obtaining the crystal structure cellular files of rutile titanium dioxide, writing the correlation information of the substituted ions, performing cell expansion processing, determining the target model based on free energy, considering information such as atomic placeholding and ion valence state, improving the accuracy and reliability of the model .
The established model better reflects the physical mechanism, improves the reliability and accuracy of the model, is close to the real situation, and reduces errors in material analysis.
Smart Images

Figure CN119026329A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the field of computer technology, and in particular to a method for establishing an ion doping model, a device for establishing an ion doping model, an electronic device and a computer-readable medium. Background Art
[0002] In the prior art, the ion-doped crystal structure model is usually established by replacing the matrix ions in the initial crystal structure with doping atoms on the basis of the initial crystal structure to obtain the ion-doped crystal structure model. However, the modeling accuracy of the ion-doped crystal structure model established in this way is usually low, and it is difficult to approach the actual experimental situation, which leads to errors in subsequent material analysis. Summary of the invention
[0003] The embodiment of the present invention provides a method, device, electronic device and computer-readable storage medium for establishing an ion doping model to solve the problem of insufficient modeling accuracy of the ion doping model.
[0004] The embodiment of the present invention discloses a method for establishing an ion doping model, comprising:
[0005] Obtain the unit cell crystal structure file of the crystal structure of rutile titanium dioxide;
[0006] Writing the associated information of the replacement ions into the unit cell crystal structure file to obtain a modified crystal structure file; wherein the replacement ions include doping ions and / or oxygen vacancies;
[0007] According to the associated information of the substituent ions in the modified crystal structure file, the crystal structure of rutile titanium dioxide is expanded to obtain at least one expanded rutile titanium dioxide phase ion doping model;
[0008] Based on the free energy of the rutile titania phase ion doping model, a target rutile titania phase ion doping model is determined in at least one rutile titania phase ion doping model.
[0009] Optionally, the step of writing the associated information of the substituted ions in the unit cell crystal structure file to obtain a modified crystal structure file includes:
[0010] Add a substitution ion label and at least one of the element name associated with the substitution ion label, the fractional coordinates of the substitution ion, the substitution ion concentration, the substitution ion valence, and the atomic displacement information to the unit cell crystal structure file to obtain a modified crystal structure file.
[0011] Optionally, the atomic displacement information includes atomic lattice vibration amplitude information and / or atomic displacement type information;
[0012] The step of adding a substitution ion label and at least one of an element name associated with the substitution ion label, a fractional coordinate of the substitution ion, a substitution ion concentration, a substitution ion valence state, and atomic displacement information to the unit cell crystal structure file to obtain a modified crystal structure file comprises:
[0013] Adding a substitution ion label to the column where the atom label parameter in the unit cell crystal structure file is located;
[0014] Adding the element name of the substituent ion in the column where the atomic chemical symbol parameter in the unit cell crystal structure file is located; and / or,
[0015] Adding the fractional coordinate information of the substitution ion to the columns where the fractional x-coordinate parameter, fractional y-coordinate parameter, and fractional z-coordinate parameter in the unit cell crystal structure file are located; and / or,
[0016] Adding the content of the substitution ion relative to the matrix ion in the column where the atomic occupancy parameter is located in the unit cell crystal structure file to obtain substitution ion concentration information; and / or,
[0017] adding the valence information of the substituent ion in the column where the atomic valence parameters are located in the unit cell crystal structure file; and / or,
[0018] Add the atomic lattice vibration amplitude information of the substitution ion in the column where the atomic lattice vibration amplitude parameter is located in the unit cell crystal structure file; and / or,
[0019] The atomic displacement type information of the substituent ion is added to the column where the atomic displacement type parameter is located in the unit cell crystal structure file.
[0020] Optionally, the method comprises:
[0021] Based on the symmetry of the crystal structure and the size of the unit cell, determining the expansion multiples of the rutile titanium dioxide in each direction in the three-dimensional lattice direction;
[0022] Based on the expansion multiple, the size of the unit cell in each direction of the three-dimensional lattice in the unit cell crystal structure file is enlarged to obtain a modified crystal structure file.
[0023] Optionally, the step of performing cell expansion processing on the crystal structure of rutile titanium dioxide according to the associated information of the substitution ions in the modified crystal structure file to obtain at least one cell expanded rutile titanium dioxide phase ion doping model comprises:
[0024] According to the modified crystal structure file, the crystal structure of the rutile titanium dioxide is expanded to obtain a crystal structure model after expansion;
[0025] According to the associated information of the substituent ions in the modified crystal structure file, a random atomic substitution operation is performed on the expanded crystal structure model to obtain at least one expanded rutile titanium dioxide phase ion doping model.
[0026] Optionally, the doping ions include donor ions and acceptor ions;
[0027] The step of performing a random atomic substitution operation on the expanded crystal structure model according to the associated information of the replacement ions in the modified crystal structure file to obtain at least one expanded rutile titanium dioxide phase ion doping model comprises:
[0028] According to at least one of the donor ion valence, donor ion concentration, and donor ion fractional coordinates in the modified crystal structure file, performing a random atomic substitution operation on the expanded crystal structure model to obtain at least one intermediate doping model;
[0029] According to the charge balance principle, acceptor ion substitution and / or oxygen vacancies are performed in the intermediate doping model to obtain at least one expanded rutile titanium dioxide phase ion doping model.
[0030] Optionally, the step of determining a target rutile titania phase ion doping model in at least one rutile titania phase ion doping model based on the free energy of the rutile titania phase ion doping model comprises:
[0031] Performing structural relaxation on the rutile titanium dioxide phase ion doping model to determine the free energy of the rutile titanium dioxide phase ion doping model;
[0032] A rutile titania phase ion doping model with a free energy smaller than that of other rutile titania phase ion doping models is selected as the target rutile titania phase ion doping model.
[0033] The embodiment of the present invention further provides a device for establishing an ion doping model, comprising:
[0034] A structure file acquisition module, used to obtain the unit cell crystal structure file of the crystal structure of rutile titanium dioxide;
[0035] A structure file modification module, used for writing the associated information of the substitution ions in the unit cell crystal structure file to obtain a modified crystal structure file; wherein the substitution ions include doping ions and / or oxygen vacancies;
[0036] A cell expansion module, used to expand the crystal structure of rutile titanium dioxide according to the associated information of the replacement ions in the modified crystal structure file, to obtain at least one expanded rutile titanium dioxide phase ion doping model;
[0037] The target model determination module is used to determine a target rutile titania phase ion doping model in at least one rutile titania phase ion doping model based on the free energy of the rutile titania phase ion doping model.
[0038] Optionally, the structure file modification module includes:
[0039] The structure file modification submodule is used to add a substitution ion label and at least one of the element name associated with the substitution ion label, the fractional coordinates of the substitution ion, the substitution ion concentration, the substitution ion valence state, and the atomic displacement information to the unit cell crystal structure file to obtain a modified crystal structure file.
[0040] Optionally, the atomic displacement information includes atomic lattice vibration amplitude information and / or atomic displacement type information;
[0041] The structure file modification submodule includes:
[0042] A label adding unit, used for adding a substitution ion label to the column where the atomic label parameter in the unit cell crystal structure file is located;
[0043] an element name adding unit, used to add the element name of the substituent ion to the column where the atomic chemical symbol parameter in the unit cell crystal structure file is located; and / or,
[0044] A fractional coordinate adding unit, used to add the fractional coordinate information of the substitution ion to the columns where the fractional x coordinate parameter, the fractional y coordinate parameter and the fractional z coordinate parameter in the unit cell crystal structure file are located; and / or,
[0045] A concentration adding unit, used for adding the content of the substitution ion relative to the matrix ion in the column where the atomic occupancy parameter of the unit cell crystal structure file is located, to obtain the substitution ion concentration information; and / or,
[0046] a valence adding unit, used for adding the valence information of the substituent ion in the column where the atomic valence parameters are located in the unit cell crystal structure file; and / or,
[0047] An amplitude adding unit is used to add the atomic lattice vibration amplitude information of the substituent ion in the column where the atomic lattice vibration amplitude parameter is located in the unit cell crystal structure file; and / or,
[0048] The displacement adding unit is used to add the atomic displacement type information of the substituent ion in the column where the atomic displacement type parameter is located in the primitive cell crystal structure file.
[0049] Optionally, the device comprises:
[0050] An expansion multiple determination module, used to determine the expansion multiple corresponding to each direction of the rutile titanium dioxide in the three-dimensional lattice direction based on the symmetry of the crystal structure and the size of the unit cell;
[0051] The size modification module is used to expand the size of the primitive cell in each direction of the three-dimensional lattice direction in the primitive cell crystal structure file based on the expansion multiple to obtain a modified crystal structure file.
[0052] Optionally, the cell expansion module includes:
[0053] A cell expansion processing submodule, used for performing cell expansion processing on the crystal structure of the rutile titanium dioxide according to the modified crystal structure file to obtain a crystal structure model after cell expansion;
[0054] The atomic substitution submodule is used to perform random atomic substitution operations on the expanded crystal structure model according to the associated information of the replacement ions in the modified crystal structure file to obtain at least one expanded rutile titanium dioxide phase ion doping model.
[0055] Optionally, the doping ions include donor ions and acceptor ions;
[0056] The atomic substitution submodule includes:
[0057] A donor substitution unit, configured to perform a random atomic substitution operation on the expanded crystal structure model according to at least one of the donor ion valence, donor ion concentration, and donor ion fractional coordinates in the modified crystal structure file, to obtain at least one intermediate doping model;
[0058] The acceptor substitution unit is used to perform acceptor ion substitution and / or establish oxygen vacancies in the intermediate doping model according to the charge balance principle to obtain at least one expanded rutile titanium dioxide phase ion doping model.
[0059] Optionally, the target model determination module includes:
[0060] A free energy determination submodule, used for performing structural relaxation on the rutile titanium dioxide phase ion doping model to determine the free energy of the rutile titanium dioxide phase ion doping model;
[0061] The target model determination submodule is used to select a rutile titanium dioxide phase ion doping model with a free energy smaller than other rutile titanium dioxide phase ion doping models as a target rutile titanium dioxide phase ion doping model.
[0062] The embodiment of the present invention further discloses an electronic device, comprising a processor, a communication interface, a memory and a communication bus, wherein the processor, the communication interface and the memory communicate with each other via the communication bus;
[0063] The memory is used to store computer programs;
[0064] The processor is used to implement the method described in the embodiment of the present invention when executing the program stored in the memory.
[0065] The embodiment of the present invention further discloses one or more computer-readable media on which instructions are stored. When executed by one or more processors, the processors are enabled to execute the method described in the embodiment of the present invention.
[0066] The embodiments of the present invention include the following advantages:
[0067] The method for establishing an ion doping model provided by an embodiment of the present invention is to obtain a unit cell crystal structure file of the crystal structure of rutile titanium dioxide; write the associated information of the substitution ions in the unit cell crystal structure file to obtain a modified crystal structure file; wherein the substitution ions include doping ions and / or oxygen vacancies; according to the associated information of the substitution ions in the modified crystal structure file, the crystal structure of rutile titanium dioxide is expanded to obtain at least one rutile titanium dioxide phase ion doping model after expansion; based on the free energy of the rutile titanium dioxide phase ion doping model, the target rutile titanium dioxide phase ion doping model is determined in at least one rutile titanium dioxide phase ion doping model. Before cell expansion, the associated information of the substitution ions can be written in the unit cell crystal structure file, and the influence of the associated information of the substitution ions such as atomic occupancy and ion valence can be considered in the cell expansion process, and the rutile titanium dioxide phase ion doping model that is more likely to exist in reality is selected based on the free energy. The established model can better reflect the physical mechanism and improve the reliability and accuracy of the model.
[0068] The above description is only an overview of the technical solution of the present invention. In order to more clearly understand the technical means of the present invention, it can be implemented according to the contents of the specification. In order to make the above and other purposes, features and advantages of the present invention more obvious and easy to understand, the specific implementation methods of the present invention are listed below. BRIEF DESCRIPTION OF THE DRAWINGS
[0069] Various other advantages and benefits will become apparent to those of ordinary skill in the art by reading the detailed description of the preferred embodiments below. The accompanying drawings are only for the purpose of illustrating the preferred embodiments and are not to be considered as limiting the present invention. Moreover, the same reference symbols are used throughout the accompanying drawings to represent the same components. In the accompanying drawings:
[0070] Figure 1 is a flowchart of a method for establishing an ion doping model provided in an embodiment of the present invention;
[0071] Figure 2 It is a schematic diagram of a crystal structure cell expansion process provided by an embodiment of the present invention;
[0072] Figure 3 is a schematic diagram of a rutile titanium dioxide phase ion doping model provided in an embodiment of the present invention;
[0073] Figure 4 is a structural block diagram of a device for establishing an ion doping model provided in an embodiment of the present invention;
[0074] Figure 5 is a block diagram of an electronic device provided in an embodiment of the present invention;
[0075] Figure 6 is a schematic diagram of a computer-readable medium provided in an embodiment of the present invention. DETAILED DESCRIPTION
[0076] To make the purpose, technical scheme and advantages of the embodiments of the present invention clearer, the embodiments of the present invention will be described in detail below in conjunction with the accompanying drawings. However, it will be appreciated by those skilled in the art that in the embodiments of the present invention, many technical details are proposed in order to enable the reader to better understand the present application. However, even without these technical details and various changes and modifications based on the following embodiments, the technical scheme claimed in the present application can also be implemented. The division of the following embodiments is for the convenience of description, and should not constitute any limitation on the specific implementation of the present invention. The various embodiments can be combined and referenced with each other without contradiction.
[0077] In order to make the above-mentioned objects, features and advantages of the present invention more obvious and easy to understand, the present invention is further described in detail below with reference to the accompanying drawings and specific embodiments.
[0078] Reference Figure 1 , shows a flowchart of a method for establishing an ion doping model provided in an embodiment of the present invention, which may specifically include the following steps:
[0079] Step 101, obtaining a unit cell crystal structure file of the crystal structure of rutile titanium dioxide;
[0080] In an embodiment of the present invention, in order to realize the construction of the rutile titanium dioxide phase ion doping model, the unit cell crystal structure file of the crystal structure of rutile titanium dioxide can be first obtained. Among them, the unit cell crystal structure file can be a crystallographic information file (Crystallographic Information File, CIF) defined in the International Tables for Crystallography. It can record several crystallographic data such as lattice parameters, atomic positions, symmetry information, atomic displacement parameters, etc.
[0081] In a specific implementation, the unit cell crystal structure file of the rutile titanium dioxide crystal structure model can be obtained from an open source crystal structure database, such as Crystallography Open Database (COD). The unit cell crystal structure file of the rutile titanium dioxide crystal structure model can also be established and output by the open source crystal structure modeling software, such as Visual Electron-beam Software for Technology of Atoms (VESTA), and the present invention does not limit this.
[0082] Step 102, writing the associated information of the replacement ions into the unit cell crystal structure file to obtain a modified crystal structure file; wherein the replacement ions include doping ions and / or oxygen vacancies;
[0083] In order to improve the accuracy of establishing the rutile titanium dioxide phase ion doping model, before performing the cell expansion process, the unit cell crystal structure file can be modified first, and the associated information of the substitution ions can be written into the unit cell crystal structure file, so that in the subsequent expansion process, the characteristic information of the substitution ions can be taken into account to construct a rutile titanium dioxide phase ion doping model with higher accuracy.
[0084] Specifically, the rutile titanium dioxide phase ion doping model established by the target may contain ion doping or oxygen vacancies. Therefore, the associated information of the substituent ions may include associated information of the doping ions and / or oxygen vacancies.
[0085] Step 103, performing cell expansion processing on the crystal structure of rutile titanium dioxide according to the associated information of the replacement ions in the modified crystal structure file, to obtain at least one cell-expanded rutile titanium dioxide phase ion doping model;
[0086] In an embodiment of the present invention, the crystal structure of rutile titanium dioxide is subjected to cell expansion processing, and the overall structure or properties of the crystal are changed by increasing the size of the unit cell in the crystal structure. At the same time, in the process of cell expansion processing, it is possible to consider modifying the associated information of the replacement ions in the crystal structure file, so that in the process of cell expansion, the characteristics of the replacement ions can be considered to form a rutile titanium dioxide phase ion doping model that conforms to the atomic occupancy and ion valence of the replacement ions, so that the established model can better reflect the physical mechanism and improve the reliability and accuracy of the model.
[0087] Step 104 : determining a target rutile titania phase ion doping model in at least one rutile titania phase ion doping model based on the free energy of the rutile titania phase ion doping model.
[0088] Furthermore, in establishing a rutile titanium dioxide phase ion doping model, since the substituent ions can randomly select matrix ions for substitution in the process of replacing matrix ions in the rutile titanium dioxide crystal structure, at least one rutile titanium dioxide phase ion doping model can be generated after the cell expansion process. Among them, some rutile titanium dioxide phase ion doping models may be models with reasonable structures, while some rutile titanium dioxide phase ion doping models may be models that are difficult to exist in reality. In order to determine a reasonable rutile titanium dioxide phase ion doping model, the free energy of different rutile titanium dioxide phase ion doping models can be further analyzed.
[0089] Generally speaking, crystal structures that can actually exist in reality tend to exist in a state with lower free energy. Therefore, based on the free energy of the rutile titania phase ion doping model, the target rutile titania phase ion doping model can be determined in at least one rutile titania phase ion doping model, thereby obtaining a rutile titania phase ion doping model with higher accuracy and reliability.
[0090] The method for establishing an ion doping model provided by an embodiment of the present invention is to obtain a unit cell crystal structure file of the crystal structure of rutile titanium dioxide; write the associated information of the substitution ions in the unit cell crystal structure file to obtain a modified crystal structure file; wherein the substitution ions include doping ions and / or oxygen vacancies; according to the associated information of the substitution ions in the modified crystal structure file, the crystal structure of rutile titanium dioxide is expanded to obtain at least one rutile titanium dioxide phase ion doping model after expansion; based on the free energy of the rutile titanium dioxide phase ion doping model, the target rutile titanium dioxide phase ion doping model is determined in at least one rutile titanium dioxide phase ion doping model. Before cell expansion, the associated information of the substitution ions can be written in the unit cell crystal structure file. In the process of cell expansion, the influence of the associated information of the substitution ions such as atomic occupancy and ion valence can be considered. At the same time, the rutile titanium dioxide phase ion doping model that is more likely to exist in reality is selected based on the free energy. The established model can better reflect the physical mechanism and improve the reliability and accuracy of the model.
[0091] In one embodiment of the present invention, the step of writing the associated information of the substituted ions in the unit cell crystal structure file to obtain a modified crystal structure file includes:
[0092] S11, adding a substitution ion label and at least one of the element name associated with the substitution ion label, the fractional coordinates of the substitution ion, the substitution ion concentration, the substitution ion valence state, and the atomic displacement information to the unit cell crystal structure file to obtain a modified crystal structure file.
[0093] In an embodiment of the present invention, in order to consider the associated information such as the fractional coordinates of the substitution ions, the substitution ion concentration, the substitution ion valence state, the atomic displacement information, etc. during the cell expansion process, the associated information of the substitution ions can be first written into the original cell crystal structure file, so that the associated information of the substitution ions can be considered during the cell expansion process, and a rutile titanium dioxide phase ion doping model that satisfies the associated information of the substitution ions is generated, thereby improving the reliability and accuracy of the model.
[0094] Specifically, a substitution ion label and at least one of the element name associated with the substitution ion label, the fractional coordinates of the substitution ion, the substitution ion concentration, the substitution ion valence state, and the atomic displacement information can be added to the unit cell crystal structure file to obtain a modified crystal structure file.
[0095] In a specific implementation, the distribution of doping ions and oxygen vacancies can be evaluated by testing and analyzing methods such as SEM (Scanning Electron Microscopy), MAPPING (Elemental Mapping), XRD (X-ray Diffraction), and XPS, and the specific position of doping ions in the rutile titanium dioxide crystal structure can be determined. Based on the information obtained from the test, the information added to the unit cell crystal structure file, such as the fractional coordinates of the substitution ions, the substitution ion concentration, the substitution ion valence, atomic displacement information, etc., can be determined. This can further improve the reliability and accuracy of the model.
[0096] In one embodiment of the present invention, the atomic displacement information includes atomic lattice vibration amplitude information and / or atomic displacement type information;
[0097] The step of adding a substitution ion label and at least one of an element name associated with the substitution ion label, a fractional coordinate of the substitution ion, a substitution ion concentration, a substitution ion valence state, and atomic displacement information to the unit cell crystal structure file to obtain a modified crystal structure file comprises:
[0098] S21, adding a substitution ion label in the column where the atomic label parameter in the unit cell crystal structure file is located;
[0099] In a specific implementation, the primitive cell crystal structure file may include multiple parameters, for example, the parameter information shown in Table 1.
[0100] Table 1 Related parameters of the unit cell crystal structure file
[0101]
[0102]
[0103] Therefore, in order to record the information of the substitution ion in the unit cell crystal structure file, the column where the atom label (_atom_site_label) parameter is located can be first searched in the unit cell crystal structure file, and the information of the substitution ion is written into the atom label.
[0104] S23, adding the element name of the substitution ion in the column where the atomic chemical symbol parameter in the unit cell crystal structure file is located; and / or,
[0105] Afterwards, you can search the column where the atomic chemical symbol (_atom_site_type_symbol) parameter is located in the unit cell crystal structure file and add the element name of the substituent ion to it.
[0106] S24, adding the fractional coordinate information of the substitution ion to the columns where the fractional x-coordinate parameter, the fractional y-coordinate parameter, and the fractional z-coordinate parameter in the unit cell crystal structure file are located; and / or,
[0107] You can search for the columns where the fractional x coordinate parameter (_atom_site_fract_x), fractional y coordinate parameter (_atom_site_fract_y), and fractional z coordinate parameter (_atom_site_fract_z) are located in the unit cell crystal structure file, and add the fractional coordinate information of the substituent ions respectively.
[0108] Specifically, the fractional coordinates of the substitution ion may have a component in the x-axis direction, a component in the y-axis direction, and a component in the z-axis direction. The component in the x-axis direction may be filled into the fractional x-coordinate, the component in the y-axis direction may be filled into the fractional y-coordinate, and the component in the z-axis direction may be filled into the fractional z-coordinate, thereby completing the addition of the fractional coordinate information of the substitution ion.
[0109] S25, adding the content of the substitution ion relative to the matrix ion in the column where the atomic occupancy parameter of the unit cell crystal structure file is located to obtain substitution ion concentration information; and / or,
[0110] You can search for the column where the atomic occupancy (_atom_site_occupancy) parameter is located in the unit cell crystal structure file, and obtain the substitution ion concentration information by comparing the content of the substitution ion relative to the matrix ion.
[0111] The matrix ions may be ions that constitute the material matrix in the original rutile titanium dioxide structure, and may be titanium ions or oxygen ions.
[0112] S26, adding the valence information of the substitution ion in the column where the atomic valence parameters are located in the unit cell crystal structure file; and / or,
[0113] You can find the column where the atomic valence parameter (_atom_type_valence) is located in the unit cell crystal structure file and enter the valence of the substituent ion there.
[0114] Specifically, when the substitution ion is a doping ion, corresponding information may be filled in according to the valence state of the doping ion. When the substitution ion is an oxygen vacancy, the valence state of the input substitution ion may be zero.
[0115] S27, adding the atomic lattice vibration amplitude information of the substitution ion in the column where the atomic lattice vibration amplitude parameter is located in the unit cell crystal structure file; and / or,
[0116] You can find the column where the atomic lattice vibration amplitude parameter (_atom_site_U_iso_or_equiv) is located in the unit cell crystal structure file, and add the atomic lattice vibration amplitude information of the substituent ion to it.
[0117] In a specific implementation, the atomic lattice vibration may not be considered, and the atomic lattice vibration amplitude information may be 0.
[0118] S28, adding the atomic displacement type information of the substituent ion in the column where the atomic displacement type parameter is located in the primitive cell crystal structure file.
[0119] You can find the column where the atomic displacement type (_atom_site_adp_type) parameter is located in the unit cell crystal structure file, and add the atomic displacement type information of the substituent ion to it.
[0120] In a specific implementation, the atomic vibration may be set to be uniform in all directions, and the atomic displacement type information of the substituted ion may be added as "Uiso".
[0121] In one embodiment of the present invention, the method comprises:
[0122] S31, based on the symmetry of the crystal structure and the size of the unit cell, determining the expansion multiple of the rutile titanium dioxide in each direction in the three-dimensional lattice direction;
[0123] S32, based on the expansion multiple, enlarging the size of the primitive cell in each direction of the three-dimensional lattice in the primitive cell crystal structure file to obtain a modified crystal structure file.
[0124] In a specific implementation, the crystal structure model of rutile titanium dioxide usually cannot meet the requirements of plasma substitution such as substitution ion concentration. Therefore, it is usually necessary to expand the crystal structure model of rutile titanium dioxide. In order to make the model obtained by cell expansion have good accuracy and reliability. Experimental tests related to cell expansion can be carried out on rutile titanium dioxide, and the symmetry of the crystal structure and the size of the unit cell can be analyzed during the test. The crystal structure model of rutile titanium dioxide is determined based on the experimental test results, that is, the change of the unit cell in the three lattice directions of a, b, and c, so as to determine the expansion multiples of rutile titanium dioxide corresponding to each direction in the three-dimensional lattice direction. Therefore, the symmetry of the crystal structure and the size of the unit cell in the real data can be further considered in the process of establishing the ion doping model of the rutile titanium dioxide phase, which further improves the accuracy and reliability of the model establishment.
[0125] In one embodiment of the present invention, the step of performing cell expansion processing on the crystal structure of rutile titanium dioxide according to the associated information of the substitution ions in the modified crystal structure file to obtain at least one cell expanded rutile titanium dioxide phase ion doping model comprises:
[0126] S41, performing cell expansion processing on the crystal structure of the rutile titanium dioxide according to the modified crystal structure file to obtain a crystal structure model after cell expansion;
[0127] After the modified crystal structure file is determined, the crystal structure of rutile titanium dioxide can be expanded based on the modified crystal structure file to obtain a crystal structure model after expansion.
[0128] In a specific implementation, the expanded size of each direction in the three-dimensional lattice direction of the crystal structure model is determined according to the expansion multiples corresponding to each direction in the three-dimensional lattice direction of rutile titanium dioxide. Based on the expanded size, the crystal structure model is expanded to obtain the expanded crystal structure model.
[0129] As a specific example of the present invention, Figure 2 A schematic diagram of a crystal structure cell expansion process provided in an embodiment of the present invention.
[0130] Among them, the initial crystal structure model of rutile titanium dioxide can be obtained first, such as Figure 2 (a) is shown. Afterwards, the expanded length information can be calculated based on the expansion multiples corresponding to each direction in the three-dimensional lattice direction of rutile titanium dioxide and the original length in each direction.
[0131] For example, the length of the modified primitive cell in the a-axis direction (_cell_length_a) = the length of the initial primitive cell in the a-axis direction (_cell_length_a) × the expansion multiple in the a-axis direction (a x );
[0132] The length of the modified primitive cell in the b-axis direction (_cell_length_b) = the length of the initial primitive cell in the b-axis direction (_cell_length_b) × the expansion multiple in the b-axis direction (b x )
[0133] The length of the modified primitive cell in the c-axis direction (_cell_length_c) = the length of the initial primitive cell in the c-axis direction (_cell_length_c) × the expansion multiple in the c-axis direction (c x )
[0134] Subsequently, in the unit cell crystal structure file corresponding to the initial rutile titanium dioxide crystal structure model, the size information of the unit cell in each direction of the three-dimensional lattice in the crystal structure model is updated, and the associated information of the substituted ions is added to obtain a modified crystal structure file, and at the same time, a crystal structure model with modified parameters is obtained, such as Figure 2 (b) as shown.
[0135] Subsequently, based on the size information of each direction in the three-dimensional lattice direction updated in the modified crystal structure file, the crystal structure of rutile titanium dioxide is expanded to obtain a crystal structure model after expansion, such as Figure 2 (c) as shown.
[0136] S42, performing a random atomic substitution operation on the expanded crystal structure model according to the associated information of the replacement ions in the modified crystal structure file, to obtain at least one expanded rutile titanium dioxide phase ion doping model.
[0137] Afterwards, according to modifying the associated information of the substituted ions in the crystal structure file, a random atomic substitution operation can be performed on the expanded crystal structure model, so that the crystal structure model after the atomic substitution operation can meet the requirements for the substituted ions in the associated information of the substituted ions, and the model can be closer to the real state.
[0138] Since there is at least one crystal structure model obtained by the random atomic substitution operation, and there can be at least one that can meet the requirements for the substitution ions in the associated information of the substitution ions, at least one ion doping model of the rutile titanium dioxide phase after cell expansion can be obtained.
[0139] In one embodiment of the present invention, the doping ions include donor ions and acceptor ions;
[0140] The step of performing a random atomic substitution operation on the expanded crystal structure model according to the associated information of the replacement ions in the modified crystal structure file to obtain at least one expanded rutile titanium dioxide phase ion doping model comprises:
[0141] S51, performing a random atomic substitution operation on the expanded crystal structure model according to at least one of the donor ion valence, donor ion concentration, and donor ion fractional coordinates in the modified crystal structure file to obtain at least one intermediate doping model;
[0142] Doping ions may include donor ions and acceptor ions. Donor ions may be impurity atoms that introduce extra electrons, which usually have more valence electrons than matrix ions. Acceptor ions may be impurity atoms that introduce extra holes, which usually have fewer valence electrons than matrix ions.
[0143] In a specific implementation, at least one of the donor ion valence (_atom_type_valence), donor ion concentration (_atom_site_occupancy), and donor ion fraction coordinates (_atom_site_fract_x, _atom_site_fract_y, _atom_site_fract_z) described in the modified crystal structure file can be first subjected to random atomic substitution operations on the expanded crystal structure model, and donor ions can be introduced into the model to obtain at least one intermediate doping model. Among them, the donor ions can perform random atomic substitution operations on titanium ions in the expanded crystal structure model.
[0144] Alternatively, the number of intermediate doping models P0 can be expressed as:
[0145]
[0146] Among them, Total(Ti) is the number of titanium ions, _atom_site_occupancy donor is the donor ion concentration.
[0147] S52, according to the charge balance principle, performing acceptor ion substitution and / or establishing oxygen vacancies in the intermediate doping model to obtain at least one expanded rutile titanium dioxide phase ion doping model.
[0148] After completing the atomic substitution operation of the donor ion, based on the charge balance principle, that is, the valence valence (O) + valence valence (Ti) + valence valence (donor ion) + valence valence (acceptor ion) = 0, acceptor ion substitution and / or establishment of oxygen vacancies can be performed in the intermediate doping model to obtain the rutile titanium dioxide phase ion doping model after cell expansion. At this time, the rutile titanium dioxide phase ion doping model after cell expansion can meet the charge balance principle and also meet the requirements for modifying the acceptor ions and / or oxygen vacancies in the crystal structure file, so that it can be closer to the actual situation, and the model has good accuracy and reliability.
[0149] Alternatively, the number P1 of the rutile titania phase ion doping model can be expressed as:
[0150]
[0151] Among them, P0 is the number of intermediate doping models, Total(Ti) is the number of titanium ions, Total(O) is the number of oxygen ions, _atom_site_occupancy donoris the donor ion concentration, _atom_site_occupancy acceptor is the acceptor ion concentration.
[0152] As a specific example of the present invention, Figure 3 Schematic diagram of a rutile titanium dioxide phase ion doping model provided by an embodiment of the present invention. Figure 3 (l) Figure 3 (n) Figure 3 (k) and other forms, the crystal structure file of the rutile titanium dioxide phase ion doping model can be output, and the number of crystal structure files of the rutile titanium dioxide phase ion doping model is P1. Based on the crystal structure file of the rutile titanium dioxide phase ion doping model, the free energy of the rutile titanium dioxide phase ion doping model can be further calculated later.
[0153] In one embodiment of the present invention, the step of determining a target rutile titania phase ion doping model in at least one rutile titania phase ion doping model based on the free energy of the rutile titania phase ion doping model comprises:
[0154] S61, performing structural relaxation on the rutile titanium dioxide phase ion doping model to determine the free energy of the rutile titanium dioxide phase ion doping model;
[0155] In an embodiment of the present invention, at least one rutile titanium dioxide phase ion doping model obtained can be subjected to structural relaxation. Structural relaxation can use a computational simulation method (such as molecular dynamics, first principle calculation, finite element analysis, etc.) to perform relaxation calculations on the rutile titanium dioxide phase ion doping model, and the relaxation process can adjust the position of atoms or ions until the rutile titanium dioxide phase ion doping model reaches the lowest energy state. Thereafter, free energy can be calculated based on the relaxed rutile titanium dioxide phase ion doping model.
[0156] In specific implementation, the cell expansion process can usually be implemented in open source crystal structure modeling software, such as VESTA, etc. The calculation of free energy usually needs to be implemented through first principle calculation software, such as VASP, Quantum ESPRESSO, ABINIT, etc. Therefore, the crystal structure file output by the open source crystal structure modeling software can be converted into a format to obtain a crystal structure file adapted to the first principle calculation software, and based on the crystal structure file of the rutile titanium dioxide phase ion doping model, a simulation is performed in the first principle calculation software to obtain the free energy of the rutile titanium dioxide phase ion doping model.
[0157] S62, selecting a rutile titania phase ion doping model having a free energy smaller than that of other rutile titania phase ion doping models as a target rutile titania phase ion doping model.
[0158] Subsequently, the rutile titania phase ion doping model with a free energy smaller than that of other rutile titania phase ion doping models can be considered as the most likely rutile titania phase ion doping structure in reality. Therefore, the rutile titania phase ion doping model with a free energy smaller than that of other rutile titania phase ion doping models can be used as the target rutile titania phase ion doping model, thereby obtaining a model with higher accuracy and reliability.
[0159] In a specific implementation, the rutile titanium dioxide phase ion doping model with the lowest free energy may be used as the target rutile titanium dioxide phase ion doping model.
[0160] As a specific example of the present invention, if the rutile titanium dioxide phase ion doping model is a rutile structure (La 0.5 Nb 0.5 ) 0.2 Ti 0.8 O2 model, the method comprises:
[0161] 1) Search for the ideal crystal structure of rutile TiO2 in the open source crystal structure database (COD) and obtain the corresponding unit cell crystal structure file;
[0162] 2) Based on the characterization test results and theoretical analysis, the donor ion (+5), acceptor ion (+3), Ti 4+ and Ti 3+ The ratio of ions is 1:1:6:2.
[0163] 3) According to the physical principle of charge balance, that is The ratio between oxygen atoms and oxygen vacancies was determined to be 19:1;
[0164] 4) According to the interatomic ratio coefficient in step 3), determine the expansion coefficients of the rutile TiO2 unit cell in the x, y and z directions respectively, as shown in the following table. x 、b x 、c xMultiply them with the parameters _cell_length_a (the length of the primitive cell in the a-axis direction), _cell_length_b (the length of the primitive cell in the b-axis direction), and _cell_length_c (the length of the primitive cell in the c-axis direction) in the crystal structure file respectively to obtain new _cell_length_a, _cell_length_b, and _cell_length_c to obtain the modified crystal structure file.
[0165] Table 2 Expansion coefficients of rutile TiO2 primitive cells in the x, y and z directions
[0166] serial number <![CDATA[a x ]]> <![CDATA[b x ]]> <![CDATA[c x ]]> 1 1 2 5 2 1 5 2 3 2 1 5 4 2 5 1 5 5 1 2 6 5 2 1
[0167] 5) Modify the associated information of the substituted ions in the modified crystal structure file, as shown in the following table:
[0168] Table 3 Modify the values of the associated information of the substituted ions in the crystal structure file
[0169]
[0170]
[0171] 6) Based on the modified crystal structure file, the crystal structure of rutile titanium dioxide is expanded to obtain at least one expanded rutile titanium dioxide phase ion doping model, and output the crystal structure file corresponding to the rutile titanium dioxide phase ion doping model;
[0172] 7) Using open source crystal structure modeling software, such as VESTA, the crystal structure file corresponding to the rutile titanium dioxide phase ion doping model is converted into a crystal structure file calculated by first principles;
[0173] 8) Using first-principles calculation software, the crystal structure of the rutile titania phase ion-doped model is structurally relaxed, and the rutile titania phase ion-doped model with the smallest free energy is screened out as the target rutile titania phase ion-doped model.
[0174] As a specific example of the present invention, if the rutile titanium dioxide phase ion doping model is a rutile structure (La 0.5 Nb 0.5 ) 0.3 Ti 0.7 O2 model, the method comprises:
[0175] 1) Search for the ideal crystal structure of rutile TiO2 in the open source crystal structure database (COD) and obtain the corresponding unit cell crystal structure file;
[0176] 2) Based on the characterization test results and theoretical analysis, the donor ion (+5), acceptor ion (+3), Ti 4+ and Ti 3+ The ratio of ions is 1.5:1.5:5:2.
[0177] 3) According to the physical principle of charge balance, that is The ratio between oxygen atoms and oxygen vacancies was determined to be 19:1;
[0178] 4) According to the interatomic ratio coefficient in step 3), determine the expansion coefficients of the rutile TiO2 unit cell in the x, y and z directions respectively, as shown in the following table. x 、b x 、c x Multiply them with the parameters _cell_length_a (the length of the primitive cell in the a-axis direction), _cell_length_b (the length of the primitive cell in the b-axis direction), and _cell_length_c (the length of the primitive cell in the c-axis direction) in the crystal structure file respectively to obtain new _cell_length_a, _cell_length_b, and _cell_length_c to obtain the modified crystal structure file.
[0179] Table 4 Expansion coefficients of rutile TiO2 primitive cells in the x, y and z directions
[0180] serial number <![CDATA[a x ]]> <![CDATA[b x ]]> <![CDATA[c x ]]> 1 1 2 5 2 1 5 2 3 2 1 5 4 2 5 1 5 5 1 2 6 5 2 1
[0181] 5) Modify the associated information of the substituted ions in the modified crystal structure file, as shown in the following table:
[0182] Table 5 Modify the values of the associated information of the substituted ions in the crystal structure file
[0183]
[0184]
[0185] 6) Based on the modified crystal structure file, the crystal structure of rutile titanium dioxide is expanded to obtain at least one expanded rutile titanium dioxide phase ion doping model, and output the crystal structure file corresponding to the rutile titanium dioxide phase ion doping model;
[0186] 7) Using open source crystal structure modeling software, such as VESTA, the crystal structure file corresponding to the rutile titanium dioxide phase ion doping model is converted into a crystal structure file calculated by first principles;
[0187] 8) Using first-principles calculation software, the crystal structure of the rutile titania phase ion-doped model is structurally relaxed, and the rutile titania phase ion-doped model with the smallest free energy is screened out as the target rutile titania phase ion-doped model.
[0188] As a specific example of the present invention, if the rutile titanium dioxide phase ion doping model is a rutile structure (La 0.5 Nb 0.5 ) 0.4 Ti 0.6 O2 model, the method comprises:
[0189] 1) Search for the ideal crystal structure of rutile TiO2 in the open source crystal structure database (COD) and obtain the corresponding unit cell crystal structure file;
[0190] 2) Based on the characterization test results and theoretical analysis, the donor ion (+5), acceptor ion (+3), Ti 4+ and Ti 3+ The ratio of ions is 1:1:2:1.
[0191] 3) According to the physical principle of charge balance, that is The ratio between oxygen atoms and oxygen vacancies was determined to be 19:1;
[0192] 4) According to the interatomic ratio coefficient in step 3), determine the expansion coefficients of the rutile TiO2 unit cell in the x, y and z directions respectively, as shown in the following table. x 、b x 、c x Multiply them with the parameters _cell_length_a (the length of the primitive cell in the a-axis direction), _cell_length_b (the length of the primitive cell in the b-axis direction), and _cell_length_c (the length of the primitive cell in the c-axis direction) in the crystal structure file respectively to obtain new _cell_length_a, _cell_length_b, and _cell_length_c to obtain the modified crystal structure file.
[0193] Table 6 Expansion coefficients of rutile TiO2 primitive cells in the x, y and z directions
[0194] serial number <![CDATA[a x ]]> <![CDATA[b x ]]> <![CDATA[c x ]]> 1 1 1 5 2 1 5 1 3 5 1 1
[0195] 5) Modify the associated information of the substituted ions in the modified crystal structure file, as shown in the following table:
[0196] Table 7 Modify the values of the associated information of the substituted ions in the crystal structure file
[0197]
[0198]
[0199] 6) Based on the modified crystal structure file, the crystal structure of rutile titanium dioxide is expanded to obtain at least one expanded rutile titanium dioxide phase ion doping model, and output the crystal structure file corresponding to the rutile titanium dioxide phase ion doping model;
[0200] 7) Using open source crystal structure modeling software, such as VESTA, the crystal structure file corresponding to the rutile titanium dioxide phase ion doping model is converted into a crystal structure file calculated by first principles;
[0201] 8) Using first-principles calculation software, the crystal structure of the rutile titania phase ion-doped model is structurally relaxed, and the rutile titania phase ion-doped model with the smallest free energy is screened out as the target rutile titania phase ion-doped model.
[0202] It should be noted that, for the sake of simplicity, the method embodiments are described as a series of action combinations, but those skilled in the art should be aware that the embodiments of the present invention are not limited by the order of the actions described, because according to the embodiments of the present invention, certain steps can be performed in other orders or simultaneously. Secondly, those skilled in the art should also be aware that the embodiments described in the specification are all preferred embodiments, and the actions involved are not necessarily required by the embodiments of the present invention.
[0203] Reference Figure 4 , shows a structural block diagram of a device for establishing an ion doping model provided in an embodiment of the present invention, which may specifically include the following modules:
[0204] The structure file acquisition module 401 is used to acquire the unit cell crystal structure file of the crystal structure of rutile titanium dioxide;
[0205] The structure file modification module 402 is used to write the associated information of the substitution ions in the unit cell crystal structure file to obtain a modified crystal structure file; wherein the substitution ions include doping ions and / or oxygen vacancies;
[0206] The cell expansion module 403 is used to expand the crystal structure of rutile titanium dioxide according to the associated information of the replacement ions in the modified crystal structure file to obtain at least one expanded rutile titanium dioxide phase ion doping model;
[0207] The target model determination module 404 is used to determine a target rutile titania phase ion doping model in at least one rutile titania phase ion doping model based on the free energy of the rutile titania phase ion doping model.
[0208] Optionally, the structure file modification module includes:
[0209] The structure file modification submodule is used to add a substitution ion label and at least one of the element name associated with the substitution ion label, the fractional coordinates of the substitution ion, the substitution ion concentration, the substitution ion valence state, and the atomic displacement information to the unit cell crystal structure file to obtain a modified crystal structure file.
[0210] Optionally, the atomic displacement information includes atomic lattice vibration amplitude information and / or atomic displacement type information;
[0211] The structure file modification submodule includes:
[0212] A label adding unit, used for adding a substitution ion label to the column where the atomic label parameter in the unit cell crystal structure file is located;
[0213] an element name adding unit, used to add the element name of the substituent ion to the column where the atomic chemical symbol parameter in the unit cell crystal structure file is located; and / or,
[0214] A fractional coordinate adding unit, used to add the fractional coordinate information of the substitution ion to the columns where the fractional x coordinate parameter, the fractional y coordinate parameter and the fractional z coordinate parameter in the unit cell crystal structure file are located; and / or,
[0215] A concentration adding unit, used for adding the content of the substitution ion relative to the matrix ion in the column where the atomic occupancy parameter of the unit cell crystal structure file is located, to obtain the substitution ion concentration information; and / or,
[0216] a valence adding unit, used for adding the valence information of the substituent ion in the column where the atomic valence parameters are located in the unit cell crystal structure file; and / or,
[0217] An amplitude adding unit is used to add the atomic lattice vibration amplitude information of the substituent ion in the column where the atomic lattice vibration amplitude parameter is located in the unit cell crystal structure file; and / or,
[0218] The displacement adding unit is used to add the atomic displacement type information of the substituent ion in the column where the atomic displacement type parameter is located in the primitive cell crystal structure file.
[0219] Optionally, the device comprises:
[0220] An expansion multiple determination module, used to determine the expansion multiple corresponding to each direction of the rutile titanium dioxide in the three-dimensional lattice direction based on the symmetry of the crystal structure and the size of the unit cell;
[0221] The size modification module is used to expand the size of the primitive cell in each direction of the three-dimensional lattice direction in the primitive cell crystal structure file based on the expansion multiple to obtain a modified crystal structure file.
[0222] Optionally, the cell expansion module includes:
[0223] A cell expansion processing submodule, used for performing cell expansion processing on the crystal structure of the rutile titanium dioxide according to the modified crystal structure file to obtain a crystal structure model after cell expansion;
[0224] The atomic substitution submodule is used to perform random atomic substitution operations on the expanded crystal structure model according to the associated information of the replacement ions in the modified crystal structure file to obtain at least one expanded rutile titanium dioxide phase ion doping model.
[0225] Optionally, the doping ions include donor ions and acceptor ions;
[0226] The atomic substitution submodule includes:
[0227] A donor substitution unit, configured to perform a random atomic substitution operation on the expanded crystal structure model according to at least one of the donor ion valence, donor ion concentration, and donor ion fractional coordinates in the modified crystal structure file, to obtain at least one intermediate doping model;
[0228] The acceptor substitution unit is used to perform acceptor ion substitution and / or establish oxygen vacancies in the intermediate doping model according to the charge balance principle to obtain at least one expanded rutile titanium dioxide phase ion doping model.
[0229] Optionally, the target model determination module includes:
[0230] A free energy determination submodule, used for performing structural relaxation on the rutile titanium dioxide phase ion doping model to determine the free energy of the rutile titanium dioxide phase ion doping model;
[0231] The target model determination submodule is used to select a rutile titanium dioxide phase ion doping model with a free energy smaller than other rutile titanium dioxide phase ion doping models as a target rutile titanium dioxide phase ion doping model.
[0232] As for the device embodiment, since it is basically similar to the method embodiment, the description is relatively simple, and the relevant parts can be referred to the partial description of the method embodiment.
[0233] In addition, an embodiment of the present invention further provides an electronic device, such as Figure 5 As shown, it includes a processor 501, a communication interface 502, a memory 503 and a communication bus 504, wherein the processor 501, the communication interface 502, and the memory 503 communicate with each other through the communication bus 504.
[0234] Memory 503, used for storing computer programs;
[0235] The processor 501 is used to execute the program stored in the memory 503, and implements the following steps:
[0236] Obtain the unit cell crystal structure file of the crystal structure of rutile titanium dioxide;
[0237] Writing the associated information of the replacement ions into the unit cell crystal structure file to obtain a modified crystal structure file; wherein the replacement ions include doping ions and / or oxygen vacancies;
[0238] According to the associated information of the substituent ions in the modified crystal structure file, the crystal structure of rutile titanium dioxide is expanded to obtain at least one expanded rutile titanium dioxide phase ion doping model;
[0239] Based on the free energy of the rutile titania phase ion doping model, a target rutile titania phase ion doping model is determined in at least one rutile titania phase ion doping model.
[0240] Optionally, the step of writing the associated information of the substituted ions in the unit cell crystal structure file to obtain a modified crystal structure file includes:
[0241] Add a substitution ion label and at least one of the element name associated with the substitution ion label, the fractional coordinates of the substitution ion, the substitution ion concentration, the substitution ion valence, and the atomic displacement information to the unit cell crystal structure file to obtain a modified crystal structure file.
[0242] Optionally, the atomic displacement information includes atomic lattice vibration amplitude information and / or atomic displacement type information;
[0243] The step of adding a substitution ion label and at least one of an element name associated with the substitution ion label, a fractional coordinate of the substitution ion, a substitution ion concentration, a substitution ion valence state, and atomic displacement information to the unit cell crystal structure file to obtain a modified crystal structure file comprises:
[0244] Adding a substitution ion label to the column where the atom label parameter in the unit cell crystal structure file is located;
[0245] Adding the element name of the substituent ion in the column where the atomic chemical symbol parameter in the unit cell crystal structure file is located; and / or,
[0246] Adding the fractional coordinate information of the substitution ion to the columns where the fractional x-coordinate parameter, fractional y-coordinate parameter, and fractional z-coordinate parameter in the unit cell crystal structure file are located; and / or,
[0247] Adding the content of the substitution ion relative to the matrix ion in the column where the atomic occupancy parameter is located in the unit cell crystal structure file to obtain substitution ion concentration information; and / or,
[0248] adding the valence information of the substituent ion in the column where the atomic valence parameters are located in the unit cell crystal structure file; and / or,
[0249] Add the atomic lattice vibration amplitude information of the substitution ion in the column where the atomic lattice vibration amplitude parameter is located in the unit cell crystal structure file; and / or,
[0250] The atomic displacement type information of the substituent ion is added to the column where the atomic displacement type parameter is located in the unit cell crystal structure file.
[0251] Optionally, the method comprises:
[0252] Based on the symmetry of the crystal structure and the size of the unit cell, determining the expansion multiples of the rutile titanium dioxide in each direction in the three-dimensional lattice direction;
[0253] Based on the expansion multiple, the size of the unit cell in each direction of the three-dimensional lattice in the unit cell crystal structure file is enlarged to obtain a modified crystal structure file.
[0254] Optionally, the step of performing cell expansion processing on the crystal structure of rutile titanium dioxide according to the associated information of the substitution ions in the modified crystal structure file to obtain at least one cell expanded rutile titanium dioxide phase ion doping model comprises:
[0255] According to the modified crystal structure file, the crystal structure of the rutile titanium dioxide is expanded to obtain a crystal structure model after expansion;
[0256] According to the associated information of the substituent ions in the modified crystal structure file, a random atomic substitution operation is performed on the expanded crystal structure model to obtain at least one expanded rutile titanium dioxide phase ion doping model.
[0257] Optionally, the doping ions include donor ions and acceptor ions;
[0258] The step of performing a random atomic substitution operation on the expanded crystal structure model according to the associated information of the replacement ions in the modified crystal structure file to obtain at least one expanded rutile titanium dioxide phase ion doping model comprises:
[0259] According to at least one of the donor ion valence, donor ion concentration, and donor ion fractional coordinates in the modified crystal structure file, performing a random atomic substitution operation on the expanded crystal structure model to obtain at least one intermediate doping model;
[0260] According to the charge balance principle, acceptor ion substitution and / or oxygen vacancies are performed in the intermediate doping model to obtain at least one expanded rutile titanium dioxide phase ion doping model.
[0261] Optionally, the step of determining a target rutile titania phase ion doping model in at least one rutile titania phase ion doping model based on the free energy of the rutile titania phase ion doping model comprises:
[0262] Performing structural relaxation on the rutile titanium dioxide phase ion doping model to determine the free energy of the rutile titanium dioxide phase ion doping model;
[0263] A rutile titania phase ion doping model with a free energy smaller than that of other rutile titania phase ion doping models is selected as the target rutile titania phase ion doping model.
[0264] The communication bus mentioned in the above terminal can be a Peripheral Component Interconnect (PCI) bus or an Extended Industry Standard Architecture (EISA) bus, etc. The communication bus can be divided into an address bus, a data bus, a control bus, etc. For ease of representation, only one thick line is used in the figure, but it does not mean that there is only one bus or one type of bus.
[0265] The communication interface is used for communication between the above terminal and other devices.
[0266] The memory may include a random access memory (RAM) or a non-volatile memory, such as at least one disk memory. Optionally, the memory may also be at least one storage device located away from the aforementioned processor.
[0267] The above-mentioned processor can be a general-purpose processor, including a central processing unit (CPU), a network processor (NP), etc.; it can also be a digital signal processor (DSP), an application specific integrated circuit (ASIC), a field programmable gate array (FPGA) or other programmable logic devices, discrete gate or transistor logic devices, discrete hardware components.
[0268] like Figure 6 As shown, in another embodiment provided by the present invention, a computer-readable storage medium 601 is also provided, in which instructions are stored. When the computer-readable storage medium is run on a computer, the computer executes the method for establishing the ion doping model described in the above embodiment.
[0269] In another embodiment of the present invention, a computer program product including instructions is provided, which, when executed on a computer, enables the computer to execute the method for establishing the ion doping model described in the above embodiment.
[0270] In the above embodiments, it can be implemented in whole or in part by software, hardware, firmware or any combination thereof. When implemented by software, it can be implemented in whole or in part in the form of a computer program product. The computer program product includes one or more computer instructions. When the computer program instructions are loaded and executed on a computer, the process or function described in the embodiment of the present invention is generated in whole or in part. The computer can be a general-purpose computer, a special-purpose computer, a computer network, or other programmable device. The computer instructions can be stored in a computer-readable storage medium, or transmitted from one computer-readable storage medium to another computer-readable storage medium. For example, the computer instructions can be transmitted from a website site, computer, server or data center to another website site, computer, server or data center by wired (e.g., coaxial cable, optical fiber, digital subscriber line (DSL)) or wireless (e.g., infrared, wireless, microwave, etc.). The computer-readable storage medium can be any available medium that a computer can access or a data storage device such as a server or data center that includes one or more available media integrated. The available medium can be a magnetic medium (e.g., a floppy disk, a hard disk, a tape), an optical medium (e.g., a DVD), or a semiconductor medium (e.g., a solid-state hard disk Solid State Disk (SSD)), etc.
[0271] It should be noted that, in this article, relational terms such as first and second, etc. are only used to distinguish one entity or operation from another entity or operation, and do not necessarily require or imply any such actual relationship or order between these entities or operations. Moreover, the terms "include", "comprise" or any other variants thereof are intended to cover non-exclusive inclusion, so that a process, method, article or device including a series of elements includes not only those elements, but also other elements not explicitly listed, or also includes elements inherent to such process, method, article or device. In the absence of further restrictions, the elements defined by the sentence "comprise a ..." do not exclude the existence of other identical elements in the process, method, article or device including the elements.
[0272] Each embodiment in this specification is described in a related manner, and the same or similar parts between the embodiments can be referred to each other, and each embodiment focuses on the differences from other embodiments. In particular, for the system embodiment, since it is basically similar to the method embodiment, the description is relatively simple, and the relevant parts can be referred to the partial description of the method embodiment.
[0273] The above description is only a preferred embodiment of the present invention and is not intended to limit the protection scope of the present invention. Any modification, equivalent replacement, improvement, etc. made within the spirit and principle of the present invention are included in the protection scope of the present invention.
Claims
1. A method for establishing an ion doping model, characterized in that: include: Obtain the unit cell crystal structure file of the crystal structure of rutile titanium dioxide; Writing the associated information of the replacement ions into the unit cell crystal structure file to obtain a modified crystal structure file; wherein the replacement ions include doping ions and / or oxygen vacancies; According to the associated information of the substituent ions in the modified crystal structure file, the crystal structure of rutile titanium dioxide is expanded to obtain at least one expanded rutile titanium dioxide phase ion doping model; Based on the free energy of the rutile titania phase ion doping model, a target rutile titania phase ion doping model is determined in at least one rutile titania phase ion doping model.
2. The method according to claim 1, characterized in that The step of writing the associated information of the substituted ions into the unit cell crystal structure file to obtain a modified crystal structure file comprises: A substitution ion label and at least one of the element name associated with the substitution ion label, the fractional coordinates of the substitution ion, the substitution ion concentration, the substitution ion valence state, and the atomic displacement information are added to the unit cell crystal structure file to obtain a modified crystal structure file.
3. The method according to claim 1, characterized in that The atomic displacement information includes atomic lattice vibration amplitude information and / or atomic displacement parameter type information; The step of adding a substitution ion label and at least one of an element name associated with the substitution ion label, a fractional coordinate of the substitution ion, a substitution ion concentration, a substitution ion valence state, and atomic displacement information to the unit cell crystal structure file to obtain a modified crystal structure file comprises: Adding a substitution ion label to the column where the atom label parameter in the unit cell crystal structure file is located; Adding the element name of the substituent ion in the column where the atomic chemical symbol parameter in the unit cell crystal structure file is located; and / or, Adding the fractional coordinate information of the substitution ion to the columns where the fractional x-coordinate parameter, fractional y-coordinate parameter, and fractional z-coordinate parameter in the unit cell crystal structure file are located; and / or, Adding the content of the substitution ion relative to the matrix ion in the column where the atomic occupancy parameter is located in the unit cell crystal structure file to obtain substitution ion concentration information; and / or, adding the valence information of the substituent ion in the column where the atomic valence parameters are located in the unit cell crystal structure file; and / or, Add the atomic lattice vibration amplitude information of the substitution ion in the column where the atomic lattice vibration amplitude parameter is located in the unit cell crystal structure file; and / or, The atomic displacement parameter type information of the substituent ion is added in the column where the atomic displacement parameter type parameter is located in the primitive cell crystal structure file.
4. The method according to claim 1, characterized in that The method comprises: Based on the symmetry of the crystal structure and the size of the unit cell, determining the expansion multiples of the rutile titanium dioxide in each direction in the three-dimensional lattice direction; Based on the expansion multiple, the size of the unit cell in each direction of the three-dimensional lattice in the unit cell crystal structure file is enlarged to obtain a modified crystal structure file.
5. The method according to claim 4, characterized in that The step of performing cell expansion processing on the crystal structure of rutile titanium dioxide according to the associated information of the substitution ions in the modified crystal structure file to obtain at least one cell expanded rutile titanium dioxide phase ion doping model comprises: According to the modified crystal structure file, the crystal structure of the rutile titanium dioxide is expanded to obtain a crystal structure model after expansion; According to the associated information of the substituent ions in the modified crystal structure file, a random atomic substitution operation is performed on the expanded crystal structure model to obtain at least one expanded rutile titanium dioxide phase ion doping model.
6. The method according to claim 5, characterized in that The doping ions include donor ions and acceptor ions; The step of performing a random atomic substitution operation on the expanded crystal structure model according to the associated information of the replacement ions in the modified crystal structure file to obtain at least one expanded rutile titanium dioxide phase ion doping model comprises: According to at least one of the donor ion valence, donor ion concentration, and donor ion fractional coordinates in the modified crystal structure file, performing a random atomic substitution operation on the expanded crystal structure model to obtain at least one intermediate doping model; According to the charge balance principle, acceptor ion substitution and / or oxygen vacancies are performed in the intermediate doping model to obtain at least one expanded rutile titanium dioxide phase ion doping model.
7. The method according to claim 1, characterized in that The step of determining a target rutile titania phase ion doping model in at least one rutile titania phase ion doping model based on the free energy of the rutile titania phase ion doping model comprises: Performing structural relaxation on the rutile titanium dioxide phase ion doping model to determine the free energy of the rutile titanium dioxide phase ion doping model; A rutile titania phase ion doping model with a free energy smaller than that of other rutile titania phase ion doping models is selected as the target rutile titania phase ion doping model.
8. A device for establishing an ion doping model, characterized in that: include: A structure file acquisition module, used to obtain the unit cell crystal structure file of the crystal structure of rutile titanium dioxide; A structure file modification module, used for writing the associated information of the substitution ions in the unit cell crystal structure file to obtain a modified crystal structure file; wherein the substitution ions include doping ions and / or oxygen vacancies; A cell expansion module, used to expand the crystal structure of rutile titanium dioxide according to the associated information of the replacement ions in the modified crystal structure file, to obtain at least one expanded rutile titanium dioxide phase ion doping model; The target model determination module is used to determine a target rutile titania phase ion doping model in at least one rutile titania phase ion doping model based on the free energy of the rutile titania phase ion doping model.
9. An electronic device, characterized in that: It includes a processor, a communication interface, a memory and a communication bus, wherein the processor, the communication interface and the memory communicate with each other through the communication bus; The memory is used to store computer programs; The processor is used to implement the method according to any one of claims 1 to 7 when executing the program stored in the memory.
10. A computer-readable medium having instructions stored thereon, which, when executed by one or more processors, cause the processors to perform the method according to any one of claims 1 to 7.