Semiconductor device and method of manufacturing the same
In semiconductor device manufacturing, the deposition and immersion process of process gas in the alternating plasma power state is used to form a metal-semiconductor compound layer, which solves the defect problem during contact hole filling and improves the electrical characteristics of the device.
Patent Information
- Application Number
- CN202410532402.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2023-05-25
- Filing Date
- 2024-04-29
- Publication Date
- 2024-11-26
AI Technical Summary
In the process of reducing the size of semiconductor device components and improving performance, defects are prone to occur when filling contact holes with conductive materials, which affects electrical characteristics.
The metal-semiconductor compound layer and sidewall material layer are formed by repeatedly performing the deposition and immersion process in alternating states of plasma power on and off at the metal-semiconductor compound formation temperature to ensure the sidewalls of the contact holes and The upper surface is defect-free.
The resistance characteristics of the conductive structure are significantly improved, ensuring no gaps in the contact holes, and improving the overall electrical characteristics of the semiconductor device.
Smart Images

Figure CN119028905A_ABST
Abstract
Description
[0001] CROSS-REFERENCE TO RELATED APPLICATIONS
[0002] This application claims priority from Korean Patent Application No. 10-2023-0067626 filed on May 25, 2023, in the Korean Intellectual Property Office, the disclosure of which is incorporated herein in its entirety for all purposes by reference. Technical Field
[0003] The inventive concept relates to a semiconductor device and a method of manufacturing the semiconductor device. Background Art
[0004] Research is being conducted to reduce the size of elements constituting semiconductor devices and to improve performance. For example, as the size of a contact hole is reduced, defects may occur while filling the contact hole with a conductive material. Summary of the invention
[0005] Example embodiments provide a method of manufacturing a semiconductor device that may improve electrical characteristics.
[0006] Example embodiments provide a semiconductor device that may be manufactured by the disclosed method of manufacturing the semiconductor device.
[0007] According to example embodiments, a method for manufacturing a semiconductor device is provided. The method includes: forming a structure having a contact hole exposing a first region; and forming a metal-semiconductor compound layer on the first region exposed by the contact hole by performing a semiconductor process at a metal-semiconductor compound forming temperature using a process gas. The process gas includes a first process gas and a second process gas, the first process gas contains a metal element, and the second process gas generates plasma by applying a plasma power to the second process gas. Forming the metal-semiconductor compound layer includes: performing a first process of exposing the structure to the process gas in a state where the plasma power is turned off; after the first process, repeating the second process and the third process after the second process two or more times, wherein the second process includes repeatedly alternating between a plasma process performed within a first duration when the plasma power is turned on and a process of exposing the structure to the process gas within a second duration when the plasma power is turned off, and the third process includes exposing the structure to the process gas while the plasma power is turned off; and after repeating the second process and the third process two or more times, performing a fourth process of exposing the structure to the process gas while the plasma power is turned off.
[0008] According to an example embodiment, a method for manufacturing a semiconductor device is provided. The method includes: forming a substrate including a structure having a first region and a contact hole exposing the first region; loading the substrate into a process chamber; repeatedly performing a deposition process and an immersion process two or more times at a metal-semiconductor compound forming temperature or higher in the process chamber, the deposition process including repeatedly applying radio frequency (RF) plasma power to a process gas for a first duration and not applying radio frequency (RF) plasma power to the process gas for a second duration, the immersion process not using plasma, thereby forming a metal-semiconductor compound layer on the first region, a sidewall material layer on the sidewall of the contact hole, and an upper material layer on the structure; performing a removal process in the process chamber to remove at least a portion of the sidewall material layer; and unloading the substrate from the process chamber after performing the removal process.
[0009] According to an example embodiment, a method for manufacturing a semiconductor device is provided. The method includes: forming a substrate by performing a first semiconductor process, the substrate including a structure having a contact hole exposing a first region; loading the substrate into a process chamber; performing a second semiconductor process using a process gas at a metal-semiconductor compound forming temperature in the process chamber loaded with the substrate, forming a metal-semiconductor compound layer on the first region exposed by the contact hole, and at the same time, forming an upper material layer on the upper surface of the structure; after performing the second semiconductor process, unloading the substrate on which the metal-semiconductor compound layer and the upper material layer are formed from the process chamber; and performing a third semiconductor process on the substrate unloaded from the process chamber. The process gas includes a first process gas and a second process gas, the first process gas contains a metal element, and the second process gas generates plasma when a plasma power is applied. Performing a second semiconductor process using a process gas includes: performing a first process of exposing a substrate to the process gas in a state where a plasma power is turned off; after the first process, repeatedly performing a second process and a third process two or more times, the second process including repeatedly performing a plasma process on the substrate within a first duration in which the plasma power is turned on, and a process of exposing the substrate to the process gas for a second duration in which the plasma power is turned off, and the third process including exposing the substrate to the process gas while the plasma power is turned off; and after repeating the second process and the third process two or more times, performing a fourth process of exposing the substrate to the process gas while the plasma power is turned off.
[0010] According to an example embodiment, a semiconductor device is provided. The semiconductor device includes: a structure having a first region and a contact hole exposing the first region; and a conductive structure, the conductive structure including a lower region in the contact hole, and an upper region disposed on the lower region and the structure. At least a portion of the contact hole has an inclined sidewall. The conductive structure includes: a metal-semiconductor compound layer in contact with the first region; a conductive pattern in contact with the metal-semiconductor compound layer in the contact hole, disposed on the structure, and covering the upper surface of the structure; and an upper material layer between the upper surface of the structure and the conductive pattern. The metal-semiconductor compound layer includes a first metal element and a semiconductor element, the upper material layer includes the first metal element, and the thickness of the metal-semiconductor compound layer is greater than the thickness of the upper material layer. BRIEF DESCRIPTION OF THE DRAWINGS
[0011] The above and other aspects, features and advantages of the present inventive concept will be more clearly understood through the following detailed description taken in conjunction with the accompanying drawings, in which:
[0012] Figure 1 is a schematic cross-sectional view of an illustrative example of a semiconductor process apparatus for manufacturing a semiconductor device according to an example embodiment;
[0013] Figure 2A and Figure 2B is a process flow chart schematically illustrating a method of manufacturing a semiconductor device according to an example embodiment;
[0014] Figure 3 , Figure 4A , Figure 4B and Figure 5A is a cross-sectional view schematically illustrating a method of manufacturing a semiconductor device according to an example embodiment;
[0015] Figure 5B is a schematic cross-sectional view of a modified example of the semiconductor device according to the example embodiment;
[0016] Figure 6 is a graph showing the thickness of a side material layer formed by a method of manufacturing a semiconductor device according to example embodiments;
[0017] Figure 7 is a cross-sectional view schematically illustrating a modified example of the semiconductor device according to the example embodiment;
[0018] Figure 8 is a cross-sectional view schematically illustrating a modified example of the semiconductor device according to the example embodiment;
[0019] Fig. 9 is a cross-sectional view schematically illustrating a modified example of the semiconductor device according to the example embodiment;
[0020] Fig.10 is a schematic cross-sectional view of a modified example of the semiconductor device according to the example embodiment;
[0021] Fig.11 , Fig. 12A , Fig. 12B and Fig. 12C is a process flow chart schematically illustrating a method of manufacturing a semiconductor device according to an example embodiment;
[0022] Figures 13 to 17 is a diagram schematically illustrating a semiconductor device according to a method of manufacturing the semiconductor device according to example embodiments;
[0023] Fig.18 is a cross-sectional view schematically illustrating a modified example of a semiconductor device according to a method of manufacturing a semiconductor device according to example embodiments; and
[0024] Fig.19A and Fig.19B is a cross-sectional view schematically illustrating a modified example of a semiconductor device according to a method of manufacturing the semiconductor device according to example embodiments. DETAILED DESCRIPTION
[0025] The present disclosure will now be described more fully below with reference to the accompanying drawings showing various embodiments. However, the present invention may be embodied in a variety of different forms and should not be construed as being limited to the example embodiments set forth herein. These example embodiments are merely examples, and many implementations and variations that do not require the details provided herein are possible. It should also be emphasized that the present disclosure provides details of alternative examples, but the enumeration of such alternatives is not exhaustive. In addition, any consistency in details between the examples should not be construed as requiring such details, and it is impractical to list every possible variation of each feature described herein. Reference should be made to the language of the claims in determining the requirements of the present invention.
[0026] The terminology used herein is for the purpose of describing particular embodiments only and is not intended to be limiting of the invention.
[0027] For example, hereinafter, for ease of description, spatially relative terms such as "upper", "middle", "lower", "under", "below", "above", "top", "bottom", etc. may be used herein to describe positional relationships such as those shown in the figures. It will be understood that the spatially relative terms also cover different orientations of the device in addition to the orientation depicted in the figures. In addition, such spatially relative terms may be replaced with other terms, such as "first", "second", and "third", to describe the components of the specification.
[0028] Ordinal numbers such as "first", "second", "third", etc. may simply be used as labels for certain elements, steps, etc. to distinguish these elements, steps, etc. from each other. Terms that are not described using "first", "second", etc. in the specification may still be referred to as "first" or "second" in the claims. In addition, a term referenced with a specific ordinal number (e.g., "first" in a specific claim) may be described elsewhere with a different ordinal number (e.g., "second" in the specification or another claim).
[0029] Figure 1 is a cross-sectional view schematically illustrating an example of a semiconductor process apparatus for manufacturing a semiconductor device according to example embodiments.
[0030] refer to Figure 1 According to an example embodiment, a semiconductor process apparatus 1 for manufacturing a semiconductor device may include a process chamber 3, a wafer support 6 for supporting a substrate W in the process chamber 3, a heater 9 in the wafer support 6 for heating the substrate W, a showerhead structure 12 for providing a process gas on the substrate W supported by the wafer support 6, a process area 25 between the wafer support 6 and the showerhead structure 12, a high-frequency power supply 30 capable of supplying radio frequency (RF) power to the showerhead structure 12, a gas discharge hole 35 for supplying a process gas PG to the showerhead structure 12, a gas supply system 40 connected to the gas discharge hole 35 through a gas pipeline 55, and an outlet 60 for discharging the process gas PG from the process area 25 to the outside of the process chamber 3.
[0031] The substrate W may be a semiconductor wafer used to manufacture semiconductor devices.
[0032] The gas supply system 40 may include a gas supply device 45 capable of supplying a process gas PG required for manufacturing a semiconductor device, and a mass flow controller 50 capable of controlling flow rates of a plurality of process gases PG supplied from the gas supply device 45 .
[0033] The gas supply device 45 may include a first gas supply source 45a for providing a first process gas, a second gas supply source 45b for providing a second process gas, a third gas supply source 45c for providing a third process gas, and a fourth gas supply source 45d for providing a fourth process gas.
[0034] The type of process gas PG may vary depending on the semiconductor process to be performed. For example, in a semiconductor process for depositing Ti, the process gas PG may include TiCl 4 gas, Ar and H 2 In another example, in a semiconductor process for depositing TiN, the process gas PG may include TiCl 4 Gas, Ar, H2 Gas and NH 3 gas.
[0035] The showerhead structure 12 may include a pedestal 15, a shower plate 17 below the pedestal 15, and a gas diffusion space 19 between the pedestal 15 and the shower plate 17. A gas discharge hole 35 for supplying a process gas PG to the showerhead structure 12 may pass through the pedestal 15 and be connected to the gas diffusion space 19. The process gas PG supplied to the gas diffusion space 19 may be supplied to the process region 25 through the hole 17a of the shower plate 17.
[0036] In this manner, a semiconductor process may be performed on the substrate W using the process gas PG supplied to the process region 25 .
[0037] Hereinafter, a method of manufacturing a semiconductor device according to example embodiments, and a semiconductor device manufactured by the method will be described.
[0038] Figure 2A is a process flow chart schematically illustrating a method of manufacturing a semiconductor device according to an example embodiment, Figure 2B It is schematically shown Figure 2A a process flow diagram of some operations of the method, and Figure 3 , Figure 4A , Figure 4B and 5A is a cross-sectional view schematically illustrating a method of manufacturing a semiconductor device according to an example embodiment. Figure 2A and Figure 3 A first semiconductor process may be performed to form a substrate 103 a ( S10 ). The substrate 103 a may include a semiconductor substrate 106 , a first structure 109 on the semiconductor substrate 106 , and a second structure 118 on the first structure 109 .
[0039] The semiconductor substrate 106 may be formed of and / or include a semiconductor material (e.g., a Group IV semiconductor, a Group III-V compound semiconductor, or a Group II-VI compound semiconductor). For example, the Group IV semiconductor may include silicon, germanium, or silicon-germanium. The semiconductor substrate 106 may be provided as a bulk semiconductor wafer, a semiconductor substrate including an epitaxial layer, a silicon-on-insulator (SOI) substrate, or a semiconductor-on-insulator (SeOI) substrate.
[0040] The first structure 109 may include a first region 112, and a peripheral region 115 surrounding the first region 112. The first region 112 may be a conductive region formed by doping impurities into a semiconductor material, and may have a conductivity type determined by the impurities. For example, the first region 112 may be formed by doping Si, doping Ge, or doping SiGe, and / or include doped Si, doping Ge, or doping SiGe. The first region 112 may be a source / drain region of a transistor, but the embodiment is not limited thereto. For example, the first region 112 may be a conductive region constituting at least a portion of a contact plug. The peripheral region 115 may have a portion of at least a side surface surrounding the first region 112.
[0041] The second structure 118 may have a contact hole 118a that exposes at least a portion of the first region 112. The second structure 118 may be an insulating structure formed of an insulating material (e.g., silicon oxide or silicon nitride) and / or including an insulating material (e.g., silicon oxide or silicon nitride). The contact hole 118a may have an inclined side surface 118b. The side surface 118b of the contact hole 118a may have a positive slope. For example, the contact hole 118a may have a positively inclined side surface 118b so that the width of the upper region of the contact hole 118a is greater than the width of the lower region of the contact hole 118a.
[0042] The aspect ratio of the contact hole 118 a may be greater than or equal to 3.5:1 (eg, the depth of the contact hole 118 a divided by the width of the contact hole 118 a may be greater than or equal to 3.5).
[0043] The maximum width of the contact hole 118a may be 20 nm or less.
[0044] refer to Figure 1 , Figure 2A , Figure 2B , Figure 4A and Figure 4B , the substrate 103a may be loaded into the process chamber 3 (S20). The substrate 103a may be loaded onto the wafer support 6 in the process chamber 3.
[0045] The second semiconductor process (S30) may be performed on the substrate 103a. The second semiconductor process may include: performing the first process (S40); performing the second process (S45); performing the third process (S50); repeatedly performing the second process (S45) and the third process (S50) when a material layer of a desired thickness is not formed (e.g., repeating the second process (S45) and the third process (S50) until a material layer of a desired thickness is obtained); and performing the fourth process (S60) when a material layer having a desired thickness is formed.
[0046] In example embodiments, the second process ( S45 ) and the third process ( S50 ) may be repeated two or more times.
[0047] The operation of performing the second semiconductor process (S30) on the substrate 103a may be performed at a metal-semiconductor compound formation temperature (e.g., the temperature of the substrate 103a may be at the metal-semiconductor compound formation temperature). In some embodiments, the metal-semiconductor compound formation temperature may be in the range of about 400° C. to about 600° C. In other embodiments, the metal-semiconductor compound formation temperature may be in the range of about 500° C. to about 600° C.
[0048] The operation of performing the first process (S40) may include supplying a process gas PG into the process chamber 3 and performing the process at a first process temperature for a first time without using plasma. The operation of performing the first process (S40) may include exposing the substrate 103a to the process gas PG in a state where the plasma power is turned off. In example embodiments, the plasma power may be a radio frequency (RF) plasma power.
[0049] The operation of performing the second process (S45) may include: after the first process (S40), supplying the process gas PG into the process chamber 3, and performing the process at the second process temperature for a second time. For example, the operation of performing the second process (S45) may include: repeatedly performing a plasma process when the plasma power is turned on and a process of exposing the substrate 103a to the process gas PG when the plasma power is turned off. The second process may be a deposition process.
[0050] The operation of performing the third process (S50) may include performing a process at the second process temperature for a third time without using plasma while supplying the process gas PG into the process chamber 3. The operation of performing the third process (S50) may include a soaking process of exposing the substrate 103a to the process gas PG in a state where the plasma power is turned off.
[0051] The operation of performing the fourth process (S60) may include supplying the process gas PG into the process chamber 3 and performing the process at the third process temperature for a fourth time without using plasma. The operation of performing the fourth process (S60) may include exposing the substrate 103a to the process gas PG while the plasma power is turned off.
[0052] The process gas PG may include a first process gas, a second process gas, and a third process gas. The first process gas may be supplied to the process region 25 from a first gas supply source 45a, the second process gas may be supplied to the process region 25 from a second gas supply source 45b, and the third process gas may be supplied to the process region 25 from a third gas supply source 45c.
[0053] The first process gas may include a metal element. The second process gas may generate plasma when plasma power is applied. The third process gas may enhance the reliability of the metal-semiconductor compound layer 121.
[0054] In an example embodiment, the first process gas may be TiCl 4 gas, the second process gas may be Ar gas, and the third process gas may be H 2 Gas. Based on the first process gas being TiCl 4 gas, the second process gas is Ar gas, and the third process gas is H 2 However, the embodiment is not limited to supplying the three process gases PG to the process area 25 in the process chamber 3 .
[0055] The operation (S40) of performing the first process may include supplying a process gas (PG) to the process region 25 in the process chamber 3 at a temperature in a range of about 400° C. to about 600° C. for a time in a range of about 1 second to about 20 seconds in a state where the RF plasma power is turned off. In the first process, the TiCl supplied to the process region 25 4 The flow rate of the gas may be in the range of about 10 standard cubic centimeters per minute (sccm) to about 30 sccm, the flow rate of the Ar gas supplied to the process region 25 may be in the range of about 1500 sccm to about 2500 sccm, and the H gas supplied to the process region 25 may be in the range of about 1500 sccm to about 2500 sccm. 2 The flow rate of the gas may be in a range of about 2000 sccm to about 6000 sccm.
[0056] The operation of performing the second process (S45) may include supplying a process gas (PG) to the process region 25 in the process chamber 3 at a temperature in a range of about 400° C. to about 600° C. for a time in a range of about 1 second to about 15 seconds. In the second process, the duty ratio of the plasma power may be in a range of about 10% to about 50%, and the TiCl supplied to the process region 25 may be about 10%. 4 The flow rate of the gas may be in the range of about 10 sccm to about 30 sccm, the flow rate of the Ar gas supplied to the process region 25 may be in the range of about 1500 sccm to about 2500 sccm, and the H gas supplied to the process region 25 may be in the range of about 1500 sccm to about 2500 sccm. 2The flow rate of the gas may be in a range of about 2000 sccm to about 6000 sccm. In the second process, the RF plasma power may be about 100 watts (W) to about 1000 watts (W).
[0057] The operation of performing the third process (S50) may include supplying a process gas (PG) to the process region 25 in the process chamber 3 at a temperature in a range of about 400° C. to about 600° C. for a time in a range of about 0.6 seconds to about 30 seconds with the RF plasma power turned off. In the third process, the TiCl supplied to the process region 25 4 The flow rate of the gas may be in the range of about 10 sccm to about 30 sccm, the flow rate of the Ar gas supplied to the process region 25 may be in the range of about 1500 sccm to about 2500 sccm, and the H gas supplied to the process region 25 may be in the range of about 1500 sccm to about 2500 sccm. 2 The flow rate of the gas may be in a range of about 2000 sccm to about 6000 sccm.
[0058] In the operation of performing the second process (S45), the duty cycle may represent a ratio of the time that the RF plasma power is turned on during the process time of the second process. For example, performing the second process (S45) may include repeating a state in which the RF plasma power is turned on and a state in which the RF plasma power is turned off, and in some embodiments, the RF duty cycle may be in the range of about 10% to about 50%.
[0059] In some embodiments, the duration of the third process (e.g., the duration during which the RF plasma power is turned off during the third process) may be about 50 to about 1000 times the duration during which the RF plasma power is turned off in the second process. For example, when the RF plasma power is turned on and off in the second process, the duration of the third process may be 50 to 1000 times the duration of the off period during the second process.
[0060] In some embodiments, the duration of the third process (e.g., the duration that the RF plasma power is turned off during the third process) may be about 200 to about 600 times the duration when the RF plasma power is turned off in the second process. For example, when the RF plasma power is turned on and off in the second process, the duration of the third process may be about 200 to about 600 times the duration of the off period of the second process.
[0061] The operation of performing the fourth process (S60) may include supplying a process gas (PG) to the process region 25 in the process chamber 3 at a temperature in a range of about 400° C. to about 600° C. for a time in a range of about 1 second to about 30 seconds with the RF plasma power turned off. In the fourth process, the TiCl supplied to the process region 25 4 The flow rate of the gas may be in the range of about 10 sccm to about 30 sccm, the flow rate of the Ar gas supplied to the process region 25 may be in the range of about 1500 sccm to about 2500 sccm, and the H gas supplied to the process region 25 may be in the range of about 1500 sccm to about 2500 sccm. 2 The flow rate of the gas may be in a range of about 2000 sccm to about 6000 sccm.
[0062] In example embodiments, the process gas PG may further include a fourth process gas containing nitrogen. For example, the fourth process gas may include N 2 Gas or NH 3 gas.
[0063] After repeating the second and third processes, a metal-semiconductor compound layer 121 having a first thickness may be formed on the first region 112, an upper material layer 127U may be formed on the upper surface 118U of the second structure 118, and a side material layer 127S may be formed on the side surface 118b of the contact hole 118a.
[0064] The thickness of the side material layer 127S may be smaller than (e.g., less than) the thickness of the upper material layer 127U. The thickness of the upper region ST, the middle region SM, and the lower region SB of the side material layer 127S may be smaller than (e.g., less than) the thickness of the upper material layer 127U. The upper material layer 127U and the side material layer 127S may be formed as one continuous material layer.
[0065] The metal-semiconductor compound layer 121 may be formed of a compound containing a metal element and a semiconductor element, and / or include a compound containing a metal element and a semiconductor element. The upper material layer 127U and the side material layer 127S may be formed of a conductive material layer containing a metal element, and / or include a conductive material layer containing a metal element.
[0066] The metal-semiconductor compound layer 121 may be formed of a compound containing metal elements, semiconductor elements, and nitrogen elements. The upper material layer 127U and the side material layer 127S may be formed of and / or include a conductive material layer containing metal elements and nitrogen elements.
[0067] The upper material layer 127U and the side material layer 127S may be formed of and / or include a conductive material layer containing a metal element and a chlorine (Cl) element.
[0068] The upper material layer 127U and the side material layer 127S may be formed of a conductive material layer including a metal element, a nitrogen element, and a chlorine (Cl) element.
[0069] In example embodiments, the metal-semiconductor compound layer 121 may be a TiSi layer, and the upper material layer 127U and the side material layer 127S may be a Ti layer, but embodiments are not limited thereto and may be replaced with other materials. For example, the TiSi layer of the metal-semiconductor compound layer 121 may be replaced with a material layer such as a TiGe layer, a TiSiGe layer, a TiSiN layer, a TiGeN layer, a TiSiGeN layer, a CoSi layer, a CoGe layer, a CoSiGe layer, a CoSiN layer, a CoGeN layer, a CoSiGeN layer, a NiSi layer, a NiGe layer, a NiSiGe layer, a NiSiN layer, a NiGeN layer, a NiSiGeN layer, a TaSi layer, a TaGe layer, a TaSiGe layer, a TaSiN layer, a TaGeN layer, a TaSiGeN layer, a WSi layer, a WGe layer, a WSiGe layer, a WSiN layer, a WGeN layer, or a WSiGeN layer. The upper material layer 127U and the side material layer 127S may be replaced with material layers such as a Ti layer, a Ta layer, a Co layer, a Ni layer, a W layer, a TiN layer, a TaN layer, a CoN layer, a NiN layer, or a WN layer.
[0070] The upper material layer 127U and the side material layer 127S may further include Cl element as an impurity.
[0071] The metal-semiconductor compound layer 121 may include a lower region 121L and an upper region 121U on the lower region 121L. When the metal-semiconductor compound layer 121 is formed of an MSix material layer, M may be a metal element such as Ti, Co, Ni, Ta, or W, and the concentration of the Si element in the lower region 121L may be higher than that in the upper region 121U. In this case, the Si element may be replaced with Ge or SiGe.
[0072] The metal-semiconductor compound layer 121 may be formed by reacting a portion of the first region 112 with a metal element at a formation temperature of the metal-semiconductor compound. Therefore, in the metal-semiconductor compound layer 121, a lower region 121L is formed at a level lower than the upper surface of the peripheral region 115, and an upper region 121U may be formed to extend into the contact hole 118a.
[0073] In the metal-semiconductor compound layer 121, the concentration of the semiconductor element in the lower region 121L may be higher than the concentration of the semiconductor element in the upper region 121U. In this case, the semiconductor element may be at least one of Si or Ge.
[0074] When the metal-semiconductor compound layer 121 is formed of a material layer such as TiSiN, the concentration of the N element in the upper region 121U may be higher than that in the lower region 121L. In this case, Ti may be replaced with other metal elements, and Si may be replaced with Ge or SiGe.
[0075] When the metal-semiconductor compound layer 121 is formed of a material layer such as TiSiN, the concentration of Si element in the lower region 121L may be higher than that of N element, and the concentration of N element in the upper region 121U may be higher than that of Si element.
[0076] The thickness of the metal-semiconductor compound layer 121 may be in a range from about 1.5 nm to about 12 nm. In some embodiments, the thickness of the metal-semiconductor compound layer 121 may be in a range from about 2 nm to about 7 nm.
[0077] After the third process ( S50 ), the material layer having a desired thickness may be the metal-semiconductor compound layer 121 in a thickness range of about 1.5 nm to about 12 nm.
[0078] After the third process ( S50 ), the material layer having a desired thickness may be the metal-semiconductor compound layer 121 in a thickness range of about 2 nm to about 7 nm.
[0079] The fourth process (S60) may be a process of removing at least a portion of the side material layer 127S. Accordingly, the fourth process may be referred to as a removal process. The side material layer 127S before removing a portion of the side material layer 127S may be referred to as a preliminary sidewall material layer.
[0080] In an example, after performing the fourth process ( S60 ), the side material layer 127S may be completely removed.
[0081] In another example, after performing the fourth process ( S60 ), the thickness of the remaining side material layer 127S may be about 1 nm or less.
[0082] like Figure 4AAs shown, the fourth process (S60) is performed on the side material layer 127S and the upper material layer 127U, and the thickness of the upper material layer 127U can be reduced while removing the side material layer 127S. After the fourth process (S60), the upper material layer 127U remaining on the upper surface 118U of the second structure 118 may have the following Figure 4B The reduced thickness shown in FIG. 1 and the upper material layer 127a having the reduced thickness is formed. The upper material layer 127U before performing the fourth process may be referred to as a preliminary upper material layer.
[0083] Thus, the substrate 103b including the metal-semiconductor compound layer 121 and the upper material layer 127a may be formed.
[0084] The substrate 103 b on which the second semiconductor process has been performed may be unloaded from the process chamber 3 ( S70 ).
[0085] According to the above embodiment, forming the metal-semiconductor compound layer 121 may include: performing a first process (S40) of exposing the substrate 103a to the process gas PG in a state where the plasma power is turned off; after the first process (S40), repeatedly performing a second process (S45) and a third process (S50) two or more times, in which the plasma process performed within a first time when the plasma power is turned on and the process of exposing the substrate 103a to the process gas PG within a second time when the plasma power is turned off are repeatedly performed in the second process (S45), and in which the substrate 103a is exposed to the process gas PG while the plasma power is turned off in the third process (S50); and after repeating the second process and the third process (S45 and S50) two or more times, performing a fourth process (S60) of exposing the substrate 103a to the process gas PG in a state where the plasma power is turned off.
[0086] refer to Figure 1 , Figure 2A and Figure 5A , the unloaded substrate ( Figure 4B 103b) in the step of performing a third semiconductor process (S80).
[0087] The performing of the third semiconductor process (S80) may include: Figure 4BAt least one conductive material layer is formed on the metal-semiconductor compound layer 121 (103b), and the at least one conductive material layer is patterned to form a conductive structure (139). The at least one conductive material layer can be patterned to form a conductive pattern 130 (for example, a portion of the conductive material other than the conductive pattern 130 can be removed). The upper material layer 127a can be retained between the conductive pattern 130 and the upper surface 118U of the second structure 118. Therefore, a conductive structure 139 including the metal-semiconductor compound layer 121, the upper material layer 127a and the conductive pattern 130 can be formed.
[0088] The conductive pattern 130 may include a first material layer 133, and a second material layer 136 on the first material layer 133. The first material layer 133 may be formed of and / or include a metal nitride such as TiN, TaN, or WN, and the second material layer 136 may be formed of and / or include a metal such as W or Mo.
[0089] The first material layer 133 may be formed in a linear shape. The first material layer 133 may contact the metal-semiconductor compound layer 121, the side surface 118b of the contact hole 118a, and the upper material layer 127a. The second material layer 136 may contact the first material layer 133, and a portion of the second material layer 136 may be formed in the contact hole 118a.
[0090] According to example embodiments, a semiconductor device 100 manufactured by the above method may be provided. The semiconductor device 100 as described above may include the semiconductor substrate 106 as described above, a first structure 109 on the semiconductor substrate 106, a second structure 118 on the first structure 109, and a conductive structure 139. The first structure 109 may include a first region 112 and a peripheral region 115 surrounding the first region 112. The first region 112 may be a conductive region formed by doping impurities into a semiconductor material. The conductivity type of the conductive region may be determined by the type of impurities doped into the semiconductor material. The second structure 118 may have a contact hole 118a exposing at least a portion of the first region 112. The second structure 118 may be an insulating structure formed of an insulating material (e.g., silicon oxide or silicon nitride) and / or including an insulating material (e.g., silicon oxide or silicon nitride). The inclined side surface 118b of the contact hole 118a may have a positive slope. The conductive structure 139 may include a metal-semiconductor compound layer 121, an upper material layer 127a, and a conductive pattern 130, as described above with reference to Figure 5A The thickness of the first material layer 133 of the conductive pattern 130 may be substantially the same as the thickness of the metal-semiconductor compound layer 121. The thickness of the first material layer 133 may be greater than the thickness of the upper material layer 127a.
[0091] In the above-described embodiment, after the fourth process ( S60 ), the side material layer 127S may be completely removed, and the conductive pattern 130 may contact the sidewall of the contact hole 118 a .
[0092] In another example, after the fourth process (S60), the side material layer ( Figure 4A 127S in ). In this way, the reference Figure 5B Describes the side material layer that is retained ( Figure 4A 127S) in the example. Figure 5B After the fourth process (S60), the side material layer ( Figure 4A Schematic cross-sectional view of an illustrative example of 127S).
[0093] refer to Figure 5B , after the fourth process (S60), the side material layer ( Figure 4A 127S) can be formed as a side material layer with a reduced thickness ( Figure 5B 127b). The thickness of the remaining side material layer 127b may be about 1 nm or less. Therefore, the side material layer 127b may remain between the conductive pattern 130 and the side surface of the contact hole 118a. Accordingly, Figure 5B The conductive structure 139' may be similar to Figure 5A The conductive structure 139, except Figure 5B The conductive structure 139' also includes Figure 5B Outside the side material layer 127b shown.
[0094] According to an example embodiment, completely removing Figure 4A The side material layer 127S in the embodiment of the present invention is provided as follows: Figure 5A The conductive structure 139 in the embodiment of the present invention is preferably removed by partially removing the conductive structure 139 in the embodiment of the present invention. Figure 4A The side material layer 127S in the embodiment of the present invention is formed as follows: Figure 5B The remaining side material layer 127b has a thickness of about 1 nm or less to provide Figure 5B According to these embodiments, the conductive structure ( Figure 5A 139 and Figure 5B 139′ in FIG. 139′). Accordingly, the conductive structure can be improved ( Figure 5A 139 and Figure 5B 139′) resistance characteristics.
[0095] Next, refer to Figure 6 , the duration of performing the third process (S50) will be described. Figure 4A The side material layer described in ( Figure 4AThe thickness of 127S). Figure 6 is a graph showing the duration of performing the third process (S50), Figure 4A , and in this graph, the horizontal axis represents the duration of the third process (S50) (eg, the amount of time that has passed since the start of the process), and the vertical axis represents Figure 4A The remaining thickness of the side material layer 127S described in Figure 6 In the curve diagram, ST represents Figure 4A The remaining thickness of the upper region ST of the side material layer 127S, SM, is represented by Figure 4A The remaining thickness of the middle region SM of the side material layer 127S in FIG. 127A and SB represents Figure 4A The remaining thickness of the lower area SB of the side material layer 127S.
[0096] refer to Figure 4A and Figure 6 , when the duration of the third process (S50) is about 2 seconds, the thickness of the lower region SB is about 1.3 nm, the thickness of the middle region SM is about 1.4 nm, and the thickness of the upper region ST is about 1.7 nm. When the duration of the third process (S50) is about 4 seconds, the thickness of the lower region SB is about 0.1 nm, the thickness of the middle region SM is about 0.2 nm, and the thickness of the upper region ST is about 0.3 nm. It can be seen from the curve results that the thickness of the side material layer 127S begins to decrease rapidly after the third process (S50) lasts for about 2 seconds.
[0097] As the thickness of the side material layer 127S decreases, the volume of the conductive pattern 130 disposed within the contact hole 118a may increase. Accordingly, since the conductive pattern 130 may include a material having a lower resistance than the material of the side material layer 127S, such as tungsten, the electrical characteristics of the conductive structure 139 may be improved as the thickness of the side material layer 127b decreases.
[0098] As the thickness of the side material layer 127b decreases, the conductive pattern 130 can be formed in the contact hole 118a without defects such as voids or with reduced defects. Accordingly, since the conductive pattern 130 can be formed without defects such as voids or with reduced defects, the resistance characteristics of the conductive structure 139 can be improved as the thickness of the side material layer 127b decreases.
[0099] In some embodiments, in order to provide the conductive structure 139 with improved resistance characteristics, a third process time for performing the third process ( S50 ) may be in a range of about 2 seconds to about 6 seconds.
[0100] In some embodiments, in order to provide the conductive structure 139 with improved resistance characteristics, a third process time for performing the third process ( S50 ) may be in a range of about 3 seconds to about 5.5 seconds.
[0101] In the following, reference Figure 7 , Figure 8 , Fig. 9 and Fig.10 , various embodiments will be described, which may be previously described by unloading the substrate ( Figure 4B A variation of a semiconductor device formed by performing a third semiconductor process (S80) in 103b) of the present invention. Because some components may be substantially the same as the components described previously, these components may be briefly described, or the description of these components may be omitted. Various modified examples of the components of the above-described embodiments will be described below focusing on the modified or replaced components. In addition, the components that may be modified or replaced as described below are described with reference to the following drawings, but these components that may be modified or replaced may be combined with each other. Alternatively, in some embodiments, the semiconductor device may be configured in combination with the above-described components. Figure 7 , Figure 8 , Fig. 9 and Fig.10 It is schematically shown Figure 5A sectional views of various modified examples of the semiconductor device 100 described in FIG.
[0102] In reference Figure 7 In a modified example, the first material layer 133a may be Figure 5A and Figure 5B The first material layer 133a is similar to the first material layer 133a, but may have a thickness greater than that of the metal-semiconductor compound layer 121. The thickness of the first material layer 133a may be two or more times the thickness of the upper material layer 127a.
[0103] In reference Figure 8 In a modified example, the first material layer 133b may be Figure 5A and Figure 5B The first material layer 133 is similar to, but may have a thickness that is smaller (eg, smaller) than that of the metal-semiconductor compound layer 121 .
[0104] In an example, the thickness of the first material layer 133 b may be greater than the thickness of the upper material layer 127 a .
[0105] In another example, the thickness of the first material layer 133 b may be the same as the thickness of the upper material layer 127 a .
[0106] In another example, the thickness of the first material layer 133 b may be smaller than (eg, less than) the thickness of the upper material layer 127 a .
[0107] In reference Fig. 9 In a modified example of Figure 5A and Figure 5B The conductive pattern 130 is similar to that of FIG. 1 , but the lower material layer 133 c may contact the metal-semiconductor compound layer 121 , fill the contact hole 118 a , and cover the upper material layer 127 a .
[0108] The conductive pattern 130a may further include an intermediate material layer 134c on the lower material layer 133c, and an upper material layer 136c on the intermediate material layer 134c. The intermediate material layer 134c may be disposed between the lower material layer 133c and the upper material layer 136c.
[0109] The upper surface of the lower material layer 133c may be disposed at a higher level than the upper surface of the second structure 118. Accordingly, the intermediate material layer 134c and the upper material layer 136c may be disposed at a higher level than the upper surface of the second structure 118.
[0110] The lower material layer 133c may be formed of a metal nitride (e.g., TiN, TaN, or WN) and / or include a metal nitride (e.g., TiN, TaN, or WN). The intermediate material layer 134c may be formed of a conductive material (e.g., TiSiN, TaSiN, or WSiN) and / or include a conductive material (e.g., TiSiN, TaSiN, or WSiN). The upper material layer 136c may be formed of a metal material (e.g., W) and / or include a metal material (e.g., W).
[0111] In reference Fig.10 In the modified example of , the conductive structure 139a includes a lower region 139La disposed in the contact hole 118a and having an upper surface coplanar with an upper surface of the second structure 118, and an upper region 139Ua on the lower region 139La.
[0112] The lower region 139La may be formed as follows Figure 5A and Figure 5B The same metal-semiconductor compound layer 121 as described in the above and the plug portion 132 on the metal-semiconductor compound layer 121 are formed, and / or include Figure 5A and Figure 5B1 and a plug portion 132 on the metal-semiconductor compound layer 121. The plug portion 132 may include a first material layer 132a contacting the metal-semiconductor compound layer 121 and covering the side surface 118b of the contact hole 118a, and a second material layer 132b filling the contact hole 118a on the first material layer 132a. The first material layer 132a may be a barrier layer formed of and / or including a material such as TiN, and the second material layer 132b may be a metal layer formed of and / or including a material such as W.
[0113] The upper region 139Ua may contact an upper surface of the lower region 139La and an upper surface of the second structure 118. The upper region 139Ua may include at least one conductive material layer.
[0114] exist Figure 7 , Figure 8 , Fig. 9 and Fig.10 In the Figure 5A An embodiment of a modified example of some components of the conductive structure 139, and Figure 7 , Figure 8 , Fig. 9 and Fig.10 The conductive structures 139 and 139a may be modified to further include Figure 5B The side material layer in Figure 5B 127b).
[0115] In the following, reference Figures 11 to 17 , will describe the use of the above reference Figures 1 to 5A The method described in the following is an illustrative example of a method for manufacturing a semiconductor device, and an illustrative example of a semiconductor device manufactured using the method for manufacturing a semiconductor device. Figure 5B The side material layer in Figure 5B 127b), but in the following embodiments, as Figure 5B The side material layer shown in ( Figure 5B 127b) in the contact hole may remain on at least two sets of side surfaces of the contact hole.
[0116] exist Figures 11 to 17 middle, Fig.11 , Fig. 12A , Fig. 12B and Fig. 12C It is provided to use the above reference Figures 1 to 5A A process flow chart of an illustrative example of a method for manufacturing a semiconductor device is described, and Figures 13 to 17 It is shown by Figures 11 to 12CA method of manufacturing a semiconductor device is shown in FIG. 1 , and an example of a semiconductor device manufactured by the method is shown.
[0117] exist Figures 13 to 17 middle, Fig.13 is a top view conceptually illustrating a semiconductor device manufactured using a method of manufacturing a semiconductor device according to example embodiments, Fig.14 is conceptually shown along Fig.13 A cross-sectional view of the area cut by line II', Fig.15A yes Fig.14 A partial enlargement of the area marked as "A" in Fig. 15B yes Fig.14 A partial enlargement of the area marked as "B" in Fig.16 is conceptually shown along Fig.13 A cross-sectional view of a region cut along line II-II', and Fig.17 yes Fig.16 A partial enlarged view of the area indicated by “C” in FIG.
[0118] refer to Figures 11 to 12C as well as Figures 13 to 17 , performing a first semiconductor process, and forming a substrate SUB1 (including a first contact hole exposing a first source / drain region of a cell transistor) Fig.11 S110 in ).
[0119] The substrate SUB1 may include a lower structure STL, and a first structure ST1 on the lower structure STL.
[0120] The lower structure (STL) may include a semiconductor substrate 203 , an active region 206 on the semiconductor substrate 203 , and an isolation region 209 on the semiconductor substrate 203 covering a side surface of the active region 206 .
[0121] The semiconductor substrate 203 may be formed of, and / or include, a Group IV semiconductor, a Group III-V compound semiconductor, or a Group II-VI compound semiconductor. For example, a Group IV semiconductor may include silicon, germanium, or silicon-germanium. For example, the semiconductor substrate 203 may be formed of, and / or include, a silicon material (e.g., a single crystal silicon material). The semiconductor substrate 203 may be a silicon substrate, a silicon-on-insulator (SOI) substrate, a germanium substrate, a germanium-on-insulator (GOI) substrate, a silicon-germanium substrate, or a substrate including an epitaxial layer.
[0122] The isolation region 209 may define the active region 206 on the semiconductor substrate 203. The isolation region 209 may be a trench device isolation layer. The isolation region 209 may be formed of an insulating material (e.g., silicon oxide and / or silicon nitride) and / or include an insulating material (e.g., silicon oxide and / or silicon nitride).
[0123] Each active region 206 may have a fin shape protruding from the semiconductor substrate 203 in a vertical direction (Z). The active region 206 may be formed of the same material (e.g., silicon) as the semiconductor substrate 203. For example, the active region 206 may include single crystal silicon. The vertical direction Z may be a direction perpendicular to the upper surface of the substrate 203. The active regions 206 may be parallel to each other.
[0124] The lower structure (STL) may further include a gate trench 215 crossing the active region 206 and extending into the isolation region 209, a gate structure GS in the gate trench 215, and first and second source / drain regions SD1 and SD2 disposed in an upper region of the active region 206 and spaced apart from each other by the gate structure GS (e.g., on opposite sides (both sides) of the gate structure). The gate structures GS may be parallel to each other.
[0125] In the top view, each gate structure GS may have a linear shape extending in the first horizontal direction X. In the top view, each active region 206 may have a bar shape or a linear shape extending in an inclined direction D. The inclined direction D may be a direction crossing the first horizontal direction X while forming an obtuse angle or an acute angle with the first horizontal direction X.
[0126] Each gate structure GS may include a gate dielectric layer 218 covering an inner wall of the gate trench 215 , a gate electrode 220 partially filling the gate trench 215 on the gate dielectric layer 218 , and a gate capping pattern 222 filling the remaining portion of the gate trench 215 on the gate electrode 220 .
[0127] The gate dielectric layer 218 may be formed of at least one of silicon oxide and a high-k dielectric, and / or include at least one of silicon oxide and a high-k dielectric. The high-k dielectric may be a dielectric having a dielectric constant higher than that of silicon oxide. The gate electrode 220 may be formed of doped polysilicon, metal, conductive metal nitride, metal-semiconductor compound, conductive metal oxide, graphene, carbon nanotubes, or a combination thereof, and / or include doped polysilicon, metal, conductive metal nitride, metal-semiconductor compound, conductive metal oxide, graphene, carbon nanotubes, or a combination thereof. For example, the gate electrode 220 may be formed of doped polysilicon, Al, Cu, Ti, Ta, Ru, W, Mo, Pt, Ni, Co, TiN, TaN, WN, NbN, TiAl, TiAlN, TiSi, TiSiN, TaSi, TaSiN, RuTiN, NiSi, CoSi, IrOx, RuOx, graphene, carbon nanotubes, or a combination thereof, but is not limited thereto. The gate electrode 220 may include a single layer or multiple layers of the above materials. For example, the gate electrode 220 may include a first electrode layer 220a and a second electrode layer 220b on the first electrode layer 220a, the first electrode layer 220a may be formed of and / or include a metal material, and the second electrode layer 220b may be formed of and / or include doped polysilicon. The gate capping pattern 222 may be formed of and / or include an insulating material (e.g., silicon nitride).
[0128] The first source / drain region SD1 and the second source / drain region SD2 may be impurity regions having N-type conductivity. The first source / drain region SD1 and the second source / drain region SD2 may be formed of and / or include doped Si, doped SiGe, or doped Ge.
[0129] The first and second source / drain regions SD1 and SD2, the gate electrode 220, and the gate dielectric layer 218 may constitute a cell transistor TR. The cell transistor TR may be a cell transistor in a memory such as a DRAM.
[0130] The first source / drain region SD1 and the second source / drain region SD2 may be disposed in the active region 206. The first source / drain region SD1 and the second source / drain region SD2 may be disposed in an upper region of the active region 206.
[0131] In example embodiments, the first source / drain region SD1 and the second source / drain region SD2 may be described as an upper region referred to as an active region 206 .
[0132] One of the active regions 206 may intersect a pair of adjacent gate structures GS among the gate structures GS. In the top view, when viewed based on one of the active regions 206, one first source / drain region SD1 is disposed in the middle of the active region 206, and the second source / drain region SD2 may be disposed at both ends of the active region 206. The first source / drain region SD1 and the second source / drain region SD2 may be adjacent to the gate capping pattern 222.
[0133] The first structure ST1 may include a pad pattern 225 , an insulating isolation pattern 228 , and an insulating buffer pattern 231 on the pad pattern 225 and the insulating isolation pattern 228 .
[0134] The pad patterns 225 may be spaced apart from each other. The pad patterns 225 may be respectively connected to the second source / drain regions SD2 spaced apart from each other on the second source / drain regions SD2. For example, one pad pattern 225 may contact and be electrically connected to one second source / drain region SD2. One of the pad patterns 225 may contact the upper surface of the electrically connected second source / drain region SD2 and cover a portion of the upper surface of the isolation region 209 adjacent to the second source / drain region SD2.
[0135] Each pad pattern 225 may include at least one conductive layer. Each pad pattern 225 may be formed of doped silicon, metal, conductive metal nitride, metal-semiconductor compound, conductive metal oxide, graphene, carbon nanotube or a combination thereof, and / or include doped silicon, metal, conductive metal nitride, metal-semiconductor compound, conductive metal oxide, graphene, carbon nanotube or a combination thereof. For example, each pad pattern 225 may be formed of doped polysilicon, Al, Cu, Ti, Ta, Ru, W, Mo, Pt, Ni, Co, TiN, TaN, WN, NbN, TiAl, TiAlN, TiSi, TiSiN, TaSi, TaSiN, RuTiN, NiSi, CoSi, IrOx, RuOx, graphene, carbon nanotube or a combination thereof, but is not limited thereto. Each pad pattern 225 may include a single layer or multiple layers of the above materials.
[0136] The insulating isolation pattern 228 may be formed of an insulating material (e.g., silicon nitride or silicon oxide), and / or include an insulating material (e.g., silicon nitride or silicon oxide). The side surfaces of the insulating isolation pattern 228 and the pad pattern 225 may contact each other. For example, the side surface of the insulating isolation pattern 228 may contact the side surface of the pad pattern 225. The upper surface of the insulating isolation pattern 228 may be coplanar with the upper surface of the pad pattern 225. The upper surface of the insulating isolation pattern 228 may be disposed at a level substantially the same as the upper surface of the pad pattern 225. The lower surface of the insulating isolation pattern 228 may be disposed at a level lower than the lower surface of the pad pattern 225. The insulating isolation pattern 228 may pass between the pad patterns 225 and extend into the isolation region 209. The insulating isolation pattern 228 may cover a portion of the gate structure GS adjacent to the isolation region 209. For example, the insulating isolation pattern 228 may cover the upper surface of a portion of the gate capping pattern 222 and the upper portion of a portion of the gate dielectric layer 218.
[0137] The insulating buffer pattern 231 may include at least one insulating layer. For example, the insulating buffer pattern 231 may include a first buffer layer 231a, a second buffer layer 231b, and a third buffer layer 231c stacked sequentially. The first buffer layer 231a may be formed of and / or include silicon nitride, the second buffer layer 231b may be formed of and / or include silicon oxide, and the third buffer layer 231c may be formed of and / or include silicon nitride.
[0138] The first structure ST1 may further include a preliminary contact hole 235 passing through the pad pattern 225 and the insulating isolation pattern 228 and exposing the first source / drain region SD1, a spacer 240 covering a sidewall of the preliminary contact hole 235, and a first contact hole 237 defined by the spacer 240 and exposing the first source / drain region SD1.
[0139] The heights of upper surfaces of the first source / drain region SD1 , the isolation region 209 , and the gate capping pattern 222 exposed by the preliminary contact hole 235 through the process of forming the preliminary contact hole 235 may be lowered.
[0140] A plurality of preliminary contact holes 235 may be provided to expose each first source / drain region SD1. Hereinafter, for easier understanding, one preliminary contact hole 235 and one first source / drain region SD1 will be mainly described. However, the description may be applicable to other contact holes 235 and source / drain regions SD1.
[0141] Therefore, the operation (S110) of forming the substrate SUB1 including the first contact hole 237 exposing the first source / drain region SD1 of the cell transistor TR by performing the first semiconductor process may include: forming a lower structure STL including the cell transistor TR (S112), and forming a first structure ST1 (S114) including the first contact hole 237 exposing the first source / drain region SD1 of the cell transistor TR on the lower structure STL.
[0142] A bit line structure BLS may be formed using a second semiconductor process (S120). The second semiconductor process may be a reference Figures 1 to 5A For example, the operation (S120) of forming the bit line structure BLS by using the second semiconductor process may include: loading the substrate SUB1 including the first contact hole 237 exposing the first source / drain region SD1 of the cell transistor TR into the process chamber ( Figure 1 3) in (S122), a material layer 251 covering the upper surface of the first structure ST1 and a metal-semiconductor compound layer 250 contacting the first source / drain region SD1 are formed by performing a second semiconductor process on the substrate SUB1 (S124), and a semiconductor layer 250 is formed from the process chamber ( Figure 1 3) unloading the substrate on which the second semiconductor process has been performed (S126), performing a deposition process to sequentially form a bit line material layer and a bit line capping layer (S128), and forming a bit line structure BLS by patterning a structure including the sequentially stacked bit line material layer and the bit line capping layer (S130).
[0143] A second semiconductor process is performed on the substrate SUB1 to cover the upper surface of the first source / drain region SD1- and the first structure ST1. The material layer 251 and the metal-semiconductor compound layer 250 (S124) may be formed with Figure 2B The second semiconductor process (S30) performed on the substrate in the embodiment is substantially the same. Therefore, the metal-semiconductor compound layer 250 may be formed by Figure 5A The metal-semiconductor compound layer in Figure 5A 121) is formed of substantially the same material, and the material layer 251 can be made of Figure 5A The upper material layer 127a is formed of substantially the same material.
[0144] The metal-semiconductor compound layer 250 may include a lower region 250L and an upper region 250U on the lower region 250L. In the metal-semiconductor compound layer 250, the lower region 250L may be composed of the upper region 250U and the lower region 250L. Figure 5A 121L) is formed of the same material, and the upper region 250U can be made of the same material as the upper region ( Figure 5A 121U) in the same material.
[0145] The thickness of the metal-semiconductor compound layer 250 may be Figure 5A The metal-semiconductor compound layer in Figure 5A The thickness of the material layer 251 is substantially the same as that of the material layer 121. Figure 5A The upper material layer ( Figure 5A 127a) has substantially the same thickness.
[0146] Each of the bit line structures BLS may include a plug portion BP, a bit line BL, and a bit line capping pattern CP.
[0147] The plug portion BP is formed in the first contact hole 237 and may contact and be electrically connected to the first source / drain region SD1. The bit line BL is formed on the plug portion BP and extends in the second horizontal direction Y and may be formed on the upper surface of the first structure ST1. The second horizontal direction Y may be perpendicular to the first horizontal direction X.
[0148] The plug portion BP may partially fill the first contact hole 237 in the first horizontal direction X, and the plug portion BP may partially fill the first contact hole 237 in the second horizontal direction Y. Thus, the first contact hole 237 may be filled.
[0149] At least a portion of a cross-sectional structure of the conductive structure including the plug portion BP and the bit line BL taken along the second horizontal direction Y may be aligned with Figure 5A , Figure 5B , Figure 7 , Figure 8 , Fig. 9 and Fig.10 The cross-sectional structures of the conductive structures 139 and 139a in any of the embodiments are similar. Fig.16 and Fig.17 As shown, at least a portion of the cross-sectional structure of the plug portion BP and the bit line BL taken along the second horizontal direction Y may be aligned with Figure 5A The conductive structure described in ( Figure 5A For example, a cross-sectional structure of the conductive structure including the plug portion BP and the bit line BL taken along the second horizontal direction Y may include a metal-semiconductor compound layer 250 in contact with the first source / drain region SD1, a linear-shaped first material layer 252 covering the metal-semiconductor compound layer 250, a second material layer 254 on the first material layer 252, and the first material layer 252 and the material layer 251 covering the upper surface of the first structure ST1. A portion of the second material layer 254 may be formed in the first contact hole 237.
[0150] The first material layer 252 may be made of Figure 5A The first material layer described ( Figure 5A133) is formed of the same material, and the second material layer 254 can be made of the same material as the reference Figure 5A The second material layer described ( Figure 5A 136) are formed of the same material.
[0151] The first material layer 252 may include a first lower portion 252L located within the first contact hole 237, and a first upper portion 252U located at a higher level than the first contact hole 237. The second material layer 254 may include a second lower portion 254L located within the first contact hole 237, and a second upper portion 254U located at a higher level than the first contact hole 237. Accordingly, the plug portion BP may include the metal-semiconductor compound layer 250, the first lower portion 252L, and the second lower portion 254L, and the bit line BL may include the material layer 251, the first upper portion 252U, and the second upper portion 254U.
[0152] In such Fig.16 and Fig.17 In the cross-sectional structure of the conductive structure including the plug portion BP and the bit line BL taken along the second horizontal direction Y, the first material layer 252 is formed in a linear shape under the second material layer 254 and may cover the metal-semiconductor compound layer 250. In addition, the first material layer 252 may contact the gate capping pattern (222).
[0153] In the second horizontal direction Y, the width of the plug portion BP may be greater than the width of the first source / drain region SD1 .
[0154] In such Fig.14 and Fig.15A In the cross-sectional structure of the plug portion BP taken along the first horizontal direction X, the first lower portion 252L may be disposed below a lower surface of the second lower portion 254L, may not cover a side surface of the second lower portion 254L, and may contact the isolation region 209 adjacent to the first source / drain region SD1.
[0155] The bit line BL may include a material layer 251 , a first upper portion 252U, and a second upper portion 254U sequentially stacked on an upper surface of the first structure ST1 .
[0156] The bit line capping pattern CP may be formed on the bit line BL. The bit line capping pattern CP may be formed of an insulating material such as silicon nitride. The bit line capping pattern CP may include at least one material layer. For example, the bit line capping pattern CP may include a first capping layer 258a, a second capping layer 258b, and a third capping layer 258c stacked sequentially.
[0157] The spacer structure SP may be formed on a side surface of the bit line structure BLS. The spacer structure SP may include a first spacer 265 a, a second spacer 265 b, a third spacer 265 c, and a lower spacer 263 .
[0158] The first spacer 265a may cover the side surface of the bit line structure BLS and may extend to cover the inner wall of the first contact hole 237 that is not filled with the plug portion BP. The second spacer 265b may cover the first spacer 265a on the side surface of the bit line BL. The third spacer 265c may cover the second spacer 265b on the side surface of the bit line BL. The second spacer 265b may be disposed between the first spacer 265a and the third spacer 265c. The upper end of the first spacer 265a may be disposed at a level higher than the upper ends of the second spacer 265b and the third spacer 265c. The upper ends of the second spacer 265b and the third spacer 265c may be disposed at a level higher than the upper end of the bit line BL.
[0159] A portion of the third spacer 265c may extend into the first contact hole 237. The lower spacer 263 may fill a portion of the first contact hole 237 that is not filled with the plug portion BP on the first spacer 265a.
[0160] The first spacer 265a may be formed of at least one of SiN, SiCN, SiON, and SiOCN, and / or include at least one of SiN, SiCN, SiON, and SiOCN. The second spacer 265b may be an air gap. It should be understood that an "air gap" may include a gap with air or other gases (e.g., such as those present during manufacturing), or may include a gap in which a vacuum is formed. The third spacer 265c may be formed of at least one of SiN, SiCN, SiON, and SiOCN, and / or include at least one of SiN, SiCN, SiON, and SiOCN. The lower spacer 263 may be formed of at least one of SiN and SiCN, and / or include at least one of SiN and SiCN.
[0161] The contact hole 270 may be formed between the bit line structures BLS. The contact hole 270 may expose at least a portion of the pad pattern 225.
[0162] The lower contact plug 272 may be formed to partially fill the contact hole 270 and have an upper surface located at a level lower than the upper ends of the second spacer 265b and the third spacer 265c. The lower contact plug 272 may be formed of doped polysilicon and / or include doped polysilicon. For example, the lower contact plug 272 may be formed of polysilicon having N-type conductivity and / or include polysilicon having N-type conductivity.
[0163] An upper spacer 273 covering the side surface of the contact hole 270 may be formed on the lower contact plug 272. The upper spacer 273 may be formed of an insulating material (eg, silicon nitride or silicon oxide). The second contact hole 275 may be defined by the upper spacer 273 in the upper region of the contact hole 270.
[0164] Accordingly, a structure ST2 including a bit line structure BLS, a spacer structure SP, a lower contact plug 272, an upper spacer 273, and a second contact hole 275 may be formed. In this case, the structure ST2 may also be referred to as a second structure. The lower contact plug 272 exposed by the second contact hole 275 may be referred to as a conductive region, or a conductive region doped with impurities.
[0165] The first substrate SUB1 and the second structure ST2 may form a substrate SUB2. Accordingly, the substrate SUB2 may include a second contact hole 275. The substrate SUB2 may also be referred to as a second substrate. Accordingly, a substrate SUB2 including a structure ST2 having a second contact hole 275 may be formed (S150).
[0166] A second semiconductor process may be used to form the conductive structure 278 (S150). The second semiconductor process may be a reference Figures 1 to 5A For example, forming the conductive structure 278 (S150) using the second semiconductor process may include: loading the substrate SUB2 having the second contact hole 275 into the process chamber ( Figure 1 3) in the process (S152), a second semiconductor process is performed on the substrate SUB2 to form a metal-semiconductor compound layer 280 contacting the lower contact plug 272 exposed by the second contact hole 275 and a material layer 279 covering the upper surface of the structure ST2 (S154), the substrate SUB2 on which the second semiconductor process has been performed is unloaded from the process chamber 3 (S156), a conductive material layer is formed by performing a deposition process (S158), and a conductive structure 278 is formed by patterning the conductive material layer (S160).
[0167] The operation (S154) of forming the metal-semiconductor compound layer 280 contacting the lower contact plug 272 exposed by the second contact hole 275 and the material layer 279 covering the upper surface of the structure ST2 by performing the second semiconductor process on the substrate SUB2 can be similar to the operation (S154) of Figure 2B The second semiconductor process (S30) is substantially the same as that performed on the substrate in the embodiment of the present invention. Accordingly, the metal-semiconductor compound layer 280 may be formed by Figure 5A The metal-semiconductor compound layer in Figure 5A 121) is formed of substantially the same material, and the material layer 279 can be made of Figure 5A The upper material layer 127a is formed of substantially the same material.
[0168] The metal-semiconductor compound layer 280 may include a lower region 280L and an upper region 280U on the lower region 280L. In the metal-semiconductor compound layer 280, the lower region 280L may be composed of the lower region ( Figure 5A 121L) is formed of the same material, and the upper region 280U can be made of the same material as the upper region ( Figure 5A 121U) in the same material.
[0169] The thickness of the metal-semiconductor compound layer 280 may be Figure 5A The metal-semiconductor compound layer in Figure 5A The thickness of 121) is substantially the same, and the thickness of the material layer 279 can be Figure 5A The upper material layer ( Figure 5A 127a) has substantially the same thickness.
[0170] The conductive structure 278 may further include a first material layer 283 and a second material layer 285. The first material layer 283 may contact the upper surface of the metal-semiconductor compound layer 280 and cover the side surface of the second contact hole 275, and may cover the upper surface of the material layer 279. The second material layer 285 may be formed on the first material layer 283. The first material layer 283 may be formed of the same material as the reference material. Figure 5A The first material layer described ( Figure 5A 133) is formed of the same material, and the second material layer 285 can be made of the same material as the reference Figure 5A The second material layer described ( Figure 5A The material layer 279 may overlap a portion of the bit line BL in the vertical direction Z. Accordingly, the conductive structure 278 may vertically overlap a portion of the bit line BL in the vertical direction Z.
[0171] The conductive structure 278 and the lower contact plug 272 may form a contact structure 281. In the contact structure 281, a region located at a higher level than the second structure ST2 may be defined as a pad region.
[0172] At least a portion of the cross-sectional structure of conductive structure 278 may be conceptually similar to reference Figure 8 The conductive structure described ( Figure 8 For example, at least a portion of the second contact hole 275 may have a shape similar to Figure 8 The metal-semiconductor compound layer 280 may be connected to the inclined side surface of the contact hole 118a in the Figure 8 The metal-semiconductor compound layer 121 in the embodiment is substantially the same, and the material layer 279 may correspond to Figure 8 The upper material layer 127a in the embodiment of the present invention, the first material layer 283 may correspond to Figure 8 The first material layer 133b in the embodiment, and the second material layer 285 may correspond to Figure 8 Thus, at least a portion of the cross-sectional structure of the conductive structure 278 may be conceptually similar to that of the conductive structure 278. Figure 8 The conductive structure described in ( Figure 8 139), but example embodiments are not limited thereto. For example, at least a portion of the cross-sectional structure of the conductive structure 278 may be similar to Figure 5A , Figure 5B , Figure 7 , Fig. 9 and Fig.10 The cross-sectional structures of the conductive structures 139 and 139a in any of the embodiments are similar.
[0173] An insulating isolation pattern 286 that extends downward and defines a side surface of a pad region of the contact structure 281 may be formed. The insulating isolation pattern 286 may be formed of an insulating material (e.g., silicon nitride) and / or include an insulating material (e.g., silicon nitride). A lower surface of the insulating isolation pattern 286 may be disposed at a higher level than the metal-semiconductor compound layer 280. The insulating isolation pattern 286 may contact the bit line capping pattern CP and the conductive structure 278. The insulating isolation pattern 286 may vertically overlap a portion of the bit line BL and a portion of the lower contact plug 272.
[0174] An etch stop layer 289 may be formed on the insulating isolation pattern 286 and the conductive structure 278. The etch stop layer 289 may be formed of and / or include an insulating material. A data storage structure DS electrically connected to the conductive structure 278 may be formed.
[0175] In an example, the data storage structure DS may be a capacitor for storing information in a DRAM. For example, the data storage structure DS may be a capacitor of a DRAM, the capacitor including a first electrode 291 passing through the etch stop layer 289 and electrically connected to the conductive structure 278, a dielectric layer 293 covering the first electrode 291 and the etch stop layer 289, and a second electrode 295 on the dielectric layer 293. The dielectric layer 293 may be formed of and / or include a high-k dielectric, silicon oxide, silicon nitride, silicon oxynitride, or a combination thereof.
[0176] In another example, the data storage structure DS may be a structure for storing DRAM and other memory information. For example, the data storage structure DS may be a capacitor of a ferroelectric memory (FeRAM), which includes a dielectric layer 293 disposed between a first electrode 291 and a second electrode 295 and including a ferroelectric layer. For example, the dielectric layer 293 may include a ferroelectric layer capable of recording data using a polarization state.
[0177] As referenced above Fig.16 and Fig.17 As described above, at least a portion of the cross-sectional structure of the plug portion BP and the bit line BL taken along the second horizontal direction Y may be different from Figure 5A The conductive structure described in ( Figure 5A 139) is similar to that of the embodiment, but the embodiment is not limited thereto. For example, at least a portion of the cross-sectional structure of the plug portion BP and the bit line BL may be similar to that of the embodiment of the present invention. Figure 5B , Figure 7 , Figure 8 , Fig. 9 and Fig.10 The cross-sectional structures of the conductive structures 139', 139 and 139a of any one of the embodiments are similar. For example, at least a portion of the cross-sectional structures of the plug portion BP and the bit line BL described above may be similar to Fig. 9 The conductive structure described in ( Fig. 9 139) is similar in cross-sectional structure. In this way, the reference Fig.18 To describe at least a portion of the cross-sectional structure of the plug portion BP and the bit line BL described above and Fig. 9 The conductive structure described in ( Fig. 9 An example with a similar cross-sectional structure to 139). Fig.18 is conceptually shown along Fig.13 A cross-sectional view of the area taken along line II'.
[0178] refer to Fig.18 The plug portion (BPa) may include the metal-semiconductor compound layer 250 , and a lower portion 352L extending upward on the metal-semiconductor compound layer 250 and contacting the metal-semiconductor compound layer 250 .
[0179] The bit line (BLa) may include an upper portion 352U extending from the lower portion 352L, a material layer 351 disposed between the upper portion 352U and an upper surface of the insulating buffer pattern 231 , and an upper material layer 354 on the upper portion 352U.
[0180] The bit line BLa may further include an intermediate material layer 353 between the upper portion 352U and the upper material layer 354. The lower portion 352L and the upper portion 352U may be formed integrally. Thus, the lower portion 352L and the upper portion 352U may be formed as one continuous material layer, which may form the lower material layer. The upper material layer 354 may be formed of Fig. 9 The middle material layer 353 may be formed of the same material as the upper material layer 136c in Fig. 9 The lower material layer including the lower portion 352L and the upper portion 352U may be formed of the same material as the middle material layer 134c in the Fig. 9The material layer 351 may be formed of the same material as the lower material layer 133c in the embodiment of the present invention. Fig. 9 The upper material layer 127a is formed of the same material.
[0181] As described above, at least a portion of the cross-sectional structure of conductive structure 278 may be conceptually similar to Figure 5A , Figure 5B , Figure 7 , Figure 8 , Fig. 9 and Fig.10 The cross-sectional structure of the conductive structures 139 and 139a in any one of the embodiments is similar. Fig.19A and Fig.19B , will describe the conceptually similar Fig.10 The conductive structure ( Fig.10 139a) is a modified example of a conductive structure 278 similar to that of FIG. Fig.19A is conceptually shown along Fig.13 A cross-sectional view of the region taken along line II', and Fig.19B yes Fig.19A A partial enlarged view of the area indicated by “Ba” in FIG.
[0182] refer to Fig.19A and Fig.19B , the conductive pattern 378 can be connected with Fig.10 The conductive structure in Fig.10 Accordingly, a contact structure 381 including a conductive pattern 378 and a contact plug 272 may be provided.
[0183] The conductive pattern 378 may include a lower region 378L in the second contact hole 275, and an upper region 378U on the lower region 378L. The lower region 378L may include the metal-semiconductor compound layer 280 as described above. The lower region 378L may also include a first material layer 383 and a second material layer 385. The first material layer 383 may contact the upper surface of the metal-semiconductor compound layer 280 and cover the side surface of the second contact hole 275. The second material layer 385 may be formed on the first material layer 383. The first material layer 383 may be formed of a metal-semiconductor compound layer 280 having a metal-semiconductor compound layer 280 and a metal-semiconductor compound layer 280 having a metal-semiconductor compound layer 280 ... Fig.10 The first material layer described ( Fig.10 132a), and the second material layer 385 may be made of the same material as the reference Fig.10 The second material layer described ( Fig.10 The upper region 378U may cover the upper surfaces of the first material layer 383 and the second material layer 385, and may cover a portion of the second structure ST2. The upper region 378U may be made of the same material as that of the first material layer 383 and the second material layer 385. Fig.10The upper region 139Ua described above is formed of the same material.
[0184] As described above, according to example embodiments, by not forming a metal layer on the inclined sidewall of the contact hole, or by forming a metal layer of about 1 nm or less on the inclined sidewall of the contact hole, a method for forming a metal-semiconductor compound layer in a region exposed by a contact hole can be provided. In this way, since the volume of the contact hole can be significantly ensured while forming the metal-semiconductor compound layer, a conductive pattern can be formed without defects such as voids in the contact hole, or a conductive pattern including a low-resistance material can be formed in the contact hole. Therefore, according to example embodiments, since the resistance characteristics of the conductive structure including the metal-semiconductor compound layer and the conductive pattern can be improved, the electrical characteristics of the semiconductor device including the conductive structure can be improved.
[0185] While example embodiments have been shown and described above, it will be apparent to those skilled in the art that modifications and variations may be made without departing from the scope of the inventive concept as defined by the appended claims.
Claims
1. A method for manufacturing a semiconductor device, include: forming a structure having a contact hole exposing the first region; as well as forming a metal-semiconductor compound layer on the first region exposed by the contact hole by performing a semiconductor process at a metal-semiconductor compound forming temperature using a process gas, wherein the process gas comprises a first process gas and a second process gas, the first process gas contains a metal element, the second process gas generates plasma by applying a plasma power to the second process gas, and Wherein, forming the metal-semiconductor compound layer comprises: performing a first process of exposing the structure to the process gas in a state where the plasma power is turned off; after the first process, repeating a second process and a third process after the second process two or more times, wherein the second process includes repeatedly alternating between a plasma process for a first duration in which the plasma power is turned on and a process in which the structure is exposed to the process gas for a second duration in which the plasma power is turned off, and the third process includes exposing the structure to the process gas while the plasma power is turned off; and After repeating the second process and the third process two or more times, a fourth process of exposing the structure to the process gas while the plasma power is turned off is performed.
2. The method according to claim 1, further comprising: include: forming a preliminary sidewall material layer and a preliminary upper material layer, Wherein, at least a portion of the contact hole has an inclined sidewall, wherein the preliminary sidewall material layer covers the inclined sidewall of the contact hole, and the preliminary upper material layer covers the upper surface of the structure, wherein, while forming the metal-semiconductor compound layer, the preliminary sidewall material layer and the preliminary upper material layer are formed by repeating the second process and the third process two or more times, Wherein, the thickness of the preliminary upper material layer is greater than the thickness of the preliminary sidewall material layer, wherein the thickness of the preliminary upper material layer is reduced by the fourth process, and an upper material layer remaining on the upper surface of the structure is formed, and Wherein, at least a portion of the preliminary sidewall material layer is removed by the fourth process.
3. The method according to claim 2, further comprising: include: After forming the metal-semiconductor compound layer, forming a conductive material layer in the contact hole, Wherein, the conductive material layer contacts at least a portion of the inclined sidewall of the contact hole.
4. The method according to claim 2, further comprising: include: After forming the metal-semiconductor compound layer, forming a conductive material layer in the contact hole, wherein the preliminary sidewall material layer is formed by a sidewall material layer whose thickness is reduced to 1 nm or less by the fourth process, and Wherein, the sidewall material layer is retained between the sidewall of the contact hole and the conductive material layer.
5. The method according to claim 1, in, The process gas further includes a third process gas, Wherein, the first process gas includes TiCl 4 gas, Wherein, the second process gas comprises Ar gas, and Wherein, the third process gas includes H 2 gas.
6. The method according to claim 5, in, The metal-semiconductor compound layer includes TiSi.
7. The method according to claim 5, in, The process gas further includes a fourth process gas containing nitrogen, and Wherein, the metal-semiconductor compound layer includes a TiSiN layer.
8. The method according to claim 1, in, The metal-semiconductor compound formation temperature is in the range of 400°C to 600°C.
9. The method according to claim 1, in, The second process has a duty cycle in the range of 10% to 50%, and The duty cycle is a ratio of a duration of the plasma power being turned on to a duration of the second process.
10. The method according to claim 1, in, The duration of the third process is 50 to 1000 times longer than the duration of the state in which the plasma power is turned off in the second process.
11. The method according to claim 1, in, The duration of the third process is in the range of 3 seconds to 6 seconds.
12. The method according to claim 1, further comprising: include: forming at least one layer of conductive material on the structure; as well as forming a bit line by patterning the at least one conductive material layer, Wherein, the structure comprises a lower structure and a first structure on the lower structure, Wherein, the lower structure comprises: Semiconductor substrate; an active region on the semiconductor substrate; an isolation region, disposed on the semiconductor substrate and disposed on a side surface of the active region; a gate trench intersecting the active region and extending into the isolation region; a gate structure in the gate trench; and A first source / drain region and a second source / drain region are arranged at both sides of the gate structure in the active region and are spaced apart from each other, wherein the first structure has the contact hole exposing at least a portion of the first source / drain region, Wherein, the first region is the first source / drain region, wherein the metal-semiconductor compound layer is in contact with the first source / drain region, and Wherein, the bit line is electrically connected to the metal-semiconductor compound layer.
13. The method according to claim 1, further comprising: include: forming at least one conductive material layer on the structure, the at least one conductive material layer being in contact with the metal-semiconductor compound layer; patterning the at least one layer of conductive material; as well as forming a data storage structure on the patterned at least one conductive material layer, Wherein, the structure comprises: A unit transistor, the unit transistor comprising a first source / drain region, a second source / drain region and a gate electrode; a bit line electrically connected to the first source / drain region; a contact plug electrically connected to the second source / drain region; and The contact hole exposes at least a portion of the contact plug, wherein the first region is the contact plug, and Wherein, the metal-semiconductor compound layer is in contact with the contact plug.
14. A method of manufacturing a semiconductor device, include: forming a substrate including a structure having a first region and a contact hole exposing the first region; loading the substrate into a process chamber; Repeating a deposition process and an immersion process two or more times at a metal-semiconductor compound forming temperature or higher in the process chamber, the deposition process comprising repeatedly applying a radio frequency (RF) plasma power to a process gas for a first duration and not applying the radio frequency (RF) plasma power to the process gas for a second duration, the immersion process not using plasma, thereby forming a metal-semiconductor compound layer on the first region, a sidewall material layer on the sidewall of the contact hole, and an upper material layer on the structure; performing a removal process in the process chamber to remove at least a portion of the sidewall material layer; as well as The substrate is unloaded from the process chamber after performing the removal process.
15. The method according to claim 14, in, The deposition process has a duty cycle in the range of 10% to 50%, and The duty cycle is a ratio of a duration when the RF plasma power is turned on to a duration of the deposition process.
16. The method according to claim 14, in, The duration of the soaking process is in the range of 3 seconds to 6 seconds.
17. A method of manufacturing a semiconductor device, include: forming a substrate by performing a first semiconductor process, the substrate including a structure having a contact hole exposing a first region; loading the substrate into a process chamber; performing a second semiconductor process using a process gas at a metal-semiconductor compound forming temperature in the process chamber loaded with the substrate to form a metal-semiconductor compound layer on the first region exposed by the contact hole and, at the same time, forming an upper material layer on an upper surface of the structure; After performing the second semiconductor process, unloading the substrate on which the metal-semiconductor compound layer and the upper material layer are formed from the process chamber; as well as performing a third semiconductor process on the substrate unloaded from the process chamber, The process gas includes a first process gas and a second process gas, the first process gas contains a metal element, and the second process gas generates plasma when a plasma power is applied. Wherein, performing the second semiconductor process using the process gas comprises: performing a first process of exposing the substrate to the process gas in a state where the plasma power is turned off; After the first process, repeatedly performing a second process and a third process after the second process two or more times, the second process comprising repeatedly performing a plasma process on the substrate for a first duration when the plasma power is turned on and a process of exposing the substrate to the process gas for a second duration when the plasma power is turned off, and the third process comprising exposing the substrate to the process gas while the plasma power is turned off; and After repeating the second process and the third process two or more times, a fourth process of exposing the substrate to the process gas while the plasma power is turned off is performed.
18. The method according to claim 17, further comprising: include: forming a preliminary sidewall material layer, Wherein, at least a portion of the contact hole has an inclined sidewall, wherein the metal-semiconductor compound layer contacts the first region, a preliminary sidewall material layer is formed on the inclined sidewall of the contact hole, and a preliminary upper material layer covers the upper surface of the structure, wherein the metal-semiconductor compound layer, the preliminary sidewall material layer and the preliminary upper material layer are formed by repeating the second process and the third process two or more times, Wherein, the thickness of the preliminary upper material layer is greater than the thickness of the preliminary sidewall material layer, wherein the thickness of the preliminary upper material layer is reduced by the fourth process to form an upper material layer remaining on the upper surface of the structure, and Wherein, at least a portion of the preliminary sidewall material layer is removed by the fourth process.
19. The method according to claim 17, in, The metal-semiconductor compound formation temperature is in the range of 400°C to 600°C.
20. The method according to claim 17, in, The second process has a duty cycle in the range of 10% to 50%, The duty cycle is a ratio of the first duration of the plasma power being turned on to the duration of the second process, wherein the duration of the third process is 50 to 1000 times the second duration of the plasma power being turned off in the second process, and The duration of the third process is in the range of 3 seconds to 6 seconds.
Citation Information
Patent Citations
Energy Harvesting and Storage Feedback Cell
KR1020230067626A
Cited By
Semiconductor device and method of manufacturing the same
US20240395615A1