Biosensor of III-V group vertical tunneling field effect transistor with P-type buffer layer and buried channel region and preparation method of biosensor
By introducing a P-type buffer layer and a group III-V vertical tunneling field effect transistor structure in the biosensor, the problems of high power consumption and low sensitivity in the prior art are solved, and high at low voltages are achieved Sensitivity biomolecular detection, suitable for low power consumption fields.
Patent Information
- Application Number
- CN202411115910.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-14
- Publication Date
- 2024-11-26
AI Technical Summary
Existing biosensors have problems with high power consumption, low sensitivity and insufficient conduction current when detecting biomolecules, especially in the low-power consumption field and neutral biomolecule detection.
The III-V vertical tunneling field effect transistor structure with P-type buffer layer and buried channel region is adopted to increase the probability of carrier tunneling in the source region by introducing buried channel region, and the P-type buffer layer is used to increase the organism The electrical characteristics differences before and after molecular coupling improve the conduction current and sensitivity.
It realizes a high-sensitivity biosensor operating at low voltages, reduces power consumption, and improves sensing capability and tunneling generation rate, suitable for biomolecular detection in the field of low power consumption.
Smart Images

Figure CN119029039A_ABST
Abstract
Description
Technical Field
[0001] The present invention belongs to the technical field of semiconductor devices, and in particular relates to a biosensor of a III-V vertical tunneling field effect transistor with a P-type buffer layer and a buried channel region and a preparation method thereof, which is used for detecting unknown biological molecules. Background Art
[0002] With the rapid development of the healthcare field, biosensors have been rapidly applied and developed in the fields of biomolecule detection, remote monitoring and diagnosis of diseases. Label-free detection biosensors based on field effect transistors (FETs) affect the electrical properties of transistors through the inherent properties of biomolecules in the cavity, solving the problems of complex operation and high manufacturing cost of labeled detection such as fluorescent labels and radioactive isotopes, and also making up for the defect that ion-sensitive field effect transistor (ISFET) biosensors cannot detect neutral biomolecules. These advantages have made it a hot topic in the field of biosensors.
[0003] However, as the process size continues to decrease, the short channel effect of common metal oxide semiconductor field effect transistor (MOSFET) biosensors is becoming more and more serious, which leads to a continuous increase in the power consumption of the device. At the same time, due to the working mechanism of its own carrier hot injection, its subthreshold swing (SS) cannot escape the limit of 60mV / dec at room temperature. For MOSFET-based biosensors, the detector length is usually more than half of the gate length, which greatly limits its integration on SOC. Although biosensors based on TFET (tunneling field effect transistor) can overcome these shortcomings well, their low on-current and sensitivity are some important issues that need to be solved.
[0004] The Chinese patent application with publication number CN112736142A discloses a biosensor based on a nanosheet stacked field effect transistor and a preparation method. Three vertically stacked nanosheets form a channel, and a nanocavity is etched on the side close to the source end. This structure leads to a higher leakage current, resulting in higher power consumption and lower sensitivity of the device.
[0005] Shruti Shreya et al. disclosed Core-Shell Junctionless Nanotube Tunnel Field Effect Transistor: Design and Sensitivity Analysis for Biosensing Application (Shruti Shreya. Core-Shell Junctionless Nanotube Tunnel Field Effect Transistor: Design and Sensitivity Analysis for Biosensing Application [J]. IEEE Sensors Journal, 2020, 20 (2): pp. 672–679.), proposed a core-shell junctionless nanotube tunneling field effect transistor structure, and used charge plasma technology to induce source and drain regions, making it less sensitive when detecting biological molecules.
[0006] Sangeeta Jana Mukhopadhyay et al. published Performance Analysis of the Diagonal Tunneling Based Dielectrically Modulated Tunnel FET for Bio-Sensing Applications (Performance Analysis of the Diagonal Tunneling Based Dielectrically Modulated Tunnel FET for Bio-Sensing Applications [J]. IEEE Sensors Journal, 2021, 21 (19): pp. 21643–21652.), and proposed a diagonal tunneling dielectric modulated tunnel field effect transistor architecture for label-free biosensing applications. Diagonal tunneling results in little difference in the electrical properties before and after coupling of biomolecules, and the device operating voltage is relatively large, which is not suitable for application in the low-power field. Summary of the invention
[0007] In order to overcome the shortcomings of the above-mentioned prior art, the purpose of the present invention is to provide a biosensor of a III-V vertical tunneling field effect transistor with a P-type buffer layer and a buried channel region and a preparation method thereof. By introducing the concept of a buried channel region, the probability of band-to-band tunneling of carriers in the source region is increased, and the on-current of the device is increased. At the same time, the presence of the P-type buffer layer increases the difference in electrical properties before and after coupling of biomolecules. The biosensor has a strong ability to detect biomolecules and high sensitivity. At the same time, due to the low leakage current and the ability to work at low voltage, the sensor can also be used in the field of low power consumption.
[0008] In order to achieve the above object, the technical solution adopted by the present invention is:
[0009] A biosensor of a III-V vertical tunneling field effect transistor with a P-type buffer layer and a buried channel region comprises a substrate 5, a drain region 4, a buffer layer 3, a channel 2, a source region 1 and a source electrode 11 which are stacked from bottom to top. The drain region 1 is embedded in the channel 2 to form a buried structure and produces a vertical tunneling field effect. Gate oxide layers 7 are arranged on both sides of the bottom of the channel 2. An auxiliary metal gate 10 is arranged on the side of each gate oxide layer 7 away from the channel 2. A tunneling metal gate 9 is stacked on the upper surface of each auxiliary metal gate 10. The tunneling metal gate 9, the auxiliary metal gate 10, the gate oxide layer 7 and the channel 2 form a biomolecule cavity 8. Drain electrodes 6 are also arranged on both ends of the upper surface of the substrate 5.
[0010] The source region 1 is made of GaSb material, a narrow bandgap compound of group III-V; the channel 2, the buffer layer 3, the drain region 4 and the substrate 5 are all made of Si material; the drain 6 and the source 11 are both made of polysilicon material; the gate oxide layer 7 is made of SiO2 material, Al2O3 material or HfO2 material; the tunneling metal gate 9 is made of metal aluminum material or metal silver material; the auxiliary metal gate 10 is made of metal chromium material or metal hafnium material.
[0011] The source region 1 is a P-type heavily doped region with a doping concentration of 1×10 19 cm -3 ~1×10 20 cm -3 ; Channel 2 is an N-type lightly doped region with a doping concentration of 1×10 15 cm -3 ~1×10 17 cm -3 ; The buffer layer 3 is a P-type lightly doped region with a doping concentration of 5×10 15 cm -3 ~1×10 17 cm -3 The drain region 4 and the substrate 5 are both N-type heavily doped regions with the same doping concentration of 5×10 18 cm -3~1×10 20 cm -3 .
[0012] The substrate 5 has a length of 40nm to 80nm and a width of 20nm to 40nm; the drain region 4, the buffer layer 3 and the channel 2 have the same length, the drain region 4 is located above the center of the substrate 5, has a length of 20nm to 25nm and a width of 10nm to 15nm; the buffer layer 3 is located above the drain region 4, has a width of 20nm to 25nm; the channel 2 is located above the buffer layer 3, has a width of 40nm to 50nm; the top of the source region 1 is flush with the top of the channel 2, has a width of 15nm to 20nm, and the channels 2 on both sides of the source region 1 have the same length, both of which are 2nm to 3nm; the bottom of the gate oxide layer 7 is flush with the bottom of the channel 2, has a length of 5nm to 7nm and a width of 15nm to 20nm; The biomolecule cavity 8 is located above the gate oxide layer 7, has the same length as the gate oxide layer 7, and has a width of 17nm to 25nm; the lengths of the tunneling metal gate 9 and the auxiliary metal gate 10 are both 3nm to 5nm, the sum of the widths of the tunneling metal gate 9 and the auxiliary metal gate 10 is the same as the sum of the widths of the gate oxide layer 7 and the biomolecule cavity 8, and the width ratio of the tunneling metal gate 9 to the auxiliary metal gate 10 is (1 to 1.3): 1; the drain 6 is located at the edges of both sides of the substrate 5, has a length of 4nm to 5nm, and has a width of 2nm to 3nm; the source 11 is located above the source region 1, has a length consistent with that of the source region 1, and has a width of 2nm to 3nm.
[0013] The method for preparing a biosensor of a III-V vertical tunneling field effect transistor with a P-type buffer layer and a buried channel region comprises the following steps:
[0014] Step 1: Prepare a heavily doped N-type semiconductor as a substrate 5;
[0015] Step 2: growing a layer of heavily doped N-type semiconductor as a drain region 4 on the substrate 5 prepared in step 1;
[0016] Step 3: growing a layer of lightly doped P-type semiconductor as a buffer layer 3 on the N-type semiconductor prepared in step 2;
[0017] Step 4: growing a lightly doped N-type semiconductor region on the buffer layer 3 prepared in step 3;
[0018] Step 5: etching the center of the lightly doped N-type semiconductor region generated in step 4 to form a source pre-growth region, and the lightly doped N-type semiconductor after etching serves as a channel 2;
[0019] Step 6: growing a layer of heavily doped P-type semiconductor in the source pre-growth region etched in step 5 as source region 1;
[0020] Step 7: depositing a layer of dielectric material on both sides of the channel 2 obtained in step 4 as a gate oxide layer region;
[0021] Step 8: The dielectric material deposited in step 7 is etched to form a gate oxide layer 7 and a biomolecule cavity 8, and then two metals with different work functions are deposited on both sides of the gate oxide layer 7 and the biomolecule cavity 8 as a tunneling metal gate 9 and an auxiliary metal gate 10, a layer of polycrystalline material is deposited above the source region 1 as a source 11, and a layer of polycrystalline material is deposited on both sides of the substrate 5 as a drain 6.
[0022] The material of the N-type semiconductor substrate 5 in step 1 is silicon.
[0023] The material of the N-type semiconductor drain region 4 in step 2 is silicon.
[0024] The material of the P-type semiconductor buffer layer 3 in step 3 is silicon.
[0025] The material of the N-type semiconductor region in step 4 is silicon.
[0026] The material of the P-type semiconductor source region 1 in step 6 is GaSb.
[0027] The gate oxide layer material in step 7 is SiO2, Al2O3 or HfO2.
[0028] The material of the tunneling metal gate 9 in step 8 is metal aluminum or metal silver, the material of the auxiliary metal gate 10 is metal chromium or metal hafnium, and the materials of the drain 6 and the source 11 are both polysilicon.
[0029] The heavily doped N-type semiconductor substrate 5 in step 1 has a length of 40 nm to 80 nm and a width of 20 nm to 40 nm.
[0030] The heavily doped N-type semiconductor drain region 4 in step 2 is located above the center of the substrate 5 and has a length of 20 nm to 25 nm and a width of 10 nm to 15 nm.
[0031] The lightly doped P-type semiconductor buffer layer 3 in step 3 is located above the drain region 4 , has the same length as the drain region 4 , and has a width of 20 nm to 25 nm.
[0032] The N-type semiconductor region in step 4 is located above the lightly doped P-type semiconductor buffer layer 3 , has the same length as the lightly doped P-type semiconductor buffer layer 3 , and has a width of 40 nm to 50 nm.
[0033] The top of the source pre-growth region in step 5 is flush with the top of the channel 2 and has a width of 15 nm to 20 nm. The lengths of both sides of the source pre-growth region and the channel 2 are the same, both of which are 2 nm to 3 nm.
[0034] The size of the heavily doped P-type semiconductor source region 1 in step 6 is the same as the size of the source pre-growth region in step 5 .
[0035] The gate oxide layer region in step 7 has a length of 5 nm to 7 nm and a width of 20 nm to 30 nm.
[0036] The bottom of the gate oxide layer 7 in the step 8 is flush with the bottom of the channel 2, with a length of 5nm to 7nm and a width of 3nm to 5nm. The biomolecule cavity 8 is located above the gate oxide layer 7, with a length the same as that of the gate oxide layer 7 and a width of 17nm to 25nm. The tunneling metal gate 9 and the auxiliary metal gate 10 are located on the side of the gate oxide layer 7 and the biomolecule cavity 8 away from the channel 2, with a length of 3nm to 5nm. The sum of the widths of the tunneling metal gate 9 and the auxiliary metal gate 10 is the same as the sum of the widths of the gate oxide layer 7 and the biomolecule cavity 8, and the width ratio of the tunneling metal gate 9 to the auxiliary metal gate 10 is (1 to 1.3): 1. The drain 6 is located at the edges of both sides of the substrate 5, with a length of 4nm to 5nm and a width of 2nm to 3nm. The source 11 is located above the source region 1, with a length consistent with that of the source region 1 and a width of 2nm to 3nm.
[0037] The heavily doped N-type semiconductor in step 1 is prepared by ion implantation, using phosphorus (P) as a dopant with a doping concentration of 5×10 18 cm -3 ~1×10 20 cm -3 The injection energy is controlled to be 100keV to 200keV, and the entire ion injection process is carried out at 20℃ to 25℃. After the ion injection is completed, thermal annealing is performed to activate the phosphorus ions. The thermal annealing temperature is between 600℃ and 1000℃, and the thermal annealing time is controlled to be 30 minutes to 60 minutes.
[0038] The heavily doped N-type semiconductor generated in step 2 adopts an epitaxial growth process. First, the silicon substrate for epitaxial growth is cleaned, and then the cleaned silicon substrate is placed in an epitaxial growth chamber for subsequent operations. The epitaxial growth chamber is a vacuum or inert gas environment, and the growth temperature is set at 1100° C. to 1300° C., and the pressure is a low-pressure environment of 90 Pa to 100 Pa. The flow rate of the silicon source gas is set at 15 sccm to 20 sccm, and the flow rate of hydrogen as a carrier gas is set at 180 sccm to 200 sccm. During the growth process, phosphine (PH3) is introduced as a dopant gas, and the doping concentration is 5×10 18 cm -3 ~1×10 20 cm -3The growth time is set at 50 minutes to 120 minutes. After the growth is completed, it is subjected to thermal annealing treatment. The thermal annealing temperature is 400° C. to 800° C., and the thermal annealing time is controlled at 10 minutes to 30 minutes.
[0039] The lightly doped P-type semiconductor generated in step 3 adopts an epitaxial growth process. First, the silicon substrate for epitaxial growth is cleaned, and then the cleaned silicon substrate is placed in an epitaxial growth chamber for subsequent operations. The epitaxial growth chamber is a vacuum or inert gas environment, and the growth temperature is set at 800°C to 1100°C and the pressure is a low-pressure environment of 90Pa to 100Pa. Boron (B) is introduced as a dopant with a doping concentration of 5×10 15 cm -3 ~1×10 17 cm -3 The growth time is set at 50 minutes to 80 minutes. After the growth is completed, it is subjected to thermal annealing treatment. The thermal annealing temperature is 400° C. to 600° C., and the thermal annealing time is controlled at 10 minutes to 30 minutes.
[0040] The lightly doped N-type semiconductor generated in step 4 adopts an epitaxial growth process. First, the silicon substrate for epitaxial growth is cleaned, and then the cleaned silicon substrate is placed in an epitaxial growth chamber for subsequent operations. The epitaxial growth chamber is a vacuum or inert gas environment, and the growth temperature is set at 1000° C. to 1200° C., and the pressure is a low-pressure environment of 90 Pa to 100 Pa. The flow rate of the silicon source gas is set at 15 sccm to 20 sccm, and the flow rate of hydrogen as a carrier gas is set at 180 sccm to 200 sccm. During the growth process, phosphine (PH3) is introduced as a dopant gas, and the doping concentration is 5×10 15 cm -3 ~1×10 17 cm -3 The growth time is set at 50 minutes to 80 minutes. After the growth is completed, it is subjected to thermal annealing treatment. The thermal annealing temperature is 400° C. to 600° C., and the thermal annealing time is controlled at 10 minutes to 30 minutes.
[0041] The source pre-growth region in step 5 is formed by dry etching technology, using a high-frequency inductively coupled plasma reactor (ICP-RIE), selecting chlorine (Cl2) as the etching gas, setting the RF power at 100W to 200W, the frequency at 13.56MHz, the pressure in the etching chamber at 10mTorr to 50mTorr, etching at 25°C to 30°C, and the etching rate at 30nm / min to 50nm / min.
[0042] The heavily doped P-type semiconductor in step 6 is generated by molecular beam epitaxy (MBE) technology. First, the silicon substrate for epitaxial growth is cleaned, and then the cleaned silicon substrate is placed in a MOCVD reaction chamber for subsequent operations. The reaction temperature is set to 500°C to 700°C, and trimethyl gallium (TMGa) and arsenic (AsH3) are used as reaction gases in a ratio of 1: (8 to 12). During the growth process, dimethyl germanium (GeH2) or dimethyl zinc (Zn(CH3)2) is added as a dopant with a doping concentration of 1×10 19 cm -3 ~1×10 20 cm -3 After the growth is completed, a thermal annealing treatment is performed, the thermal annealing temperature is 300° C. to 500° C., and the time is 30 minutes to 50 minutes.
[0043] The dielectric constant of the dielectric material deposited in step 7 is 4 to 25. An atomic layer deposition (ALD) process is used. First, the semiconductor material is chemically cleaned or hydrogen-treated to remove oxides and organic residues to ensure optimal surface receptivity. Trimethoxyhafnium, trimethoxyaluminum or dimethyl silicon oxide is used as a precursor for depositing a dielectric layer. The precursor is introduced into a reaction chamber to adsorb the precursor on the silicon surface. Oxygen or nitrogen is introduced to remove unreacted precursors and by-products. Water vapor is introduced as an oxidant to react with the adsorbed precursor to generate a dielectric layer film. The purification step is repeated to remove by-products and unreacted gases generated during the reaction. During this process, the temperature is controlled at 200° C. to 400° C. and adjusted according to the characteristics of the ALD precursor and the reaction conditions. The ambient pressure is maintained at 2 to 10 Torr. The thickness of the dielectric layer film is increased by repeating the ALD cycle, and the thickness increases by 5 angstroms to 20 angstroms per cycle.
[0044] In step 8, the dielectric material is etched using dry etching technology, and an inductively coupled plasma (ICP) etcher and hydrogen fluoride (HF) are selected as etching gases for operation. The overall ambient temperature is maintained at 20° C. to 25° C. The inductively coupled plasma (ICP) etcher is started to generate plasma, and then hydrogen fluoride etching gas is input to ensure that the flow rate is 40 sccm to 50 sccm. The pressure of the reaction chamber is adjusted to 40 mTorr to 50 mTorr to maintain a stable etching atmosphere. At a discharge power of 200 W to 300 W and a discharge pressure of 13.56 At a frequency of 1 MHz, hydrogen fluoride reacts with the surface of the dielectric material to generate compounds to achieve etching. After the etching is completed, cleaning is performed to remove the etching residues. The work function of the deposited tunneling metal gate 9 is 3.7eV~4.1eV, and the work function of the auxiliary metal gate 10 is 4.2eV~4.5eV. The reactive sputtering process is used to deposit the target material using a magnetron sputtering system. First, the target material is heated to 300℃~600℃ to increase the evaporation rate of the metal. At the same time, the temperature of the substrate is controlled at 100℃~300℃ to avoid thermal damage to the film on the substrate. The pressure of the sputtering chamber is set at 10 -6 Torr~10 -8 Torr, start the sputtering system, heat the target materials of the tunneling metal gate 9 and the auxiliary metal gate 10 and apply an electric field to sputter the target materials from the surface of the target gun to the silicon substrate, set the sputtering power of the material of the tunneling metal gate 9 to 80W-200W, and the sputtering power of the material of the auxiliary metal gate 10 to 50W-150W, so as to form the required metal film on the semiconductor surface. After the sputtering process is completed, release the vacuum chamber gas and take out the semiconductor substrate, and use characterization technology to evaluate the morphology, composition and bonding state of the metal film. The characterization technology includes SEM and XPS to ensure the quality and stability of the gate electrode; the conductivity of the drain 6 and the source 11 is 10 -3 S / m~10 -1 S / m, formed by chemical vapor deposition (CVD), first preheating the CVD reaction chamber to 500-700°C and controlling the pressure in the chamber at 10 -2 Torr~10 1 Torr, to promote subsequent deposition, dimethylsilane (SiH2(CH3)2) is introduced as a silicon source gas, and the flow rate is set to 50sccm~100sccm, hydrogen (H2) is used as a diluent gas, and the flow rate is set to 200sccm~500sccm, the silicon source gas is decomposed in the reaction chamber and an electrode film is deposited on the surface of the substrate, and then the deposited electrode film is annealed to improve its crystallinity and electrical properties, the thermal annealing temperature is 500℃~1000℃, and the thermal annealing time is controlled at 20 minutes to 40 minutes.
[0045] Compared with the prior art, the beneficial effects of the present invention are:
[0046] 1. The present invention introduces a lightly doped P-type buffer layer 3 above the drain region 4. When no biomolecule enters the biomolecule cavity 8, the effective coupling between the tunneling metal gate 9 and the auxiliary metal gate 10 and the channel 2 is very weak, and the concentration of electrons that can tunnel from the source region 1 is very low. Most of them will recombine when passing through the lightly doped P-type buffer layer 3, and the on-current of the device will decrease, greatly reducing the reference standard of sensitivity; when biomolecules enter the biomolecule cavity 8, the effective coupling between the tunneling metal gate 9 and the auxiliary metal gate 10 and the channel 2 is enhanced, and the concentration of electrons that recombine in the lightly doped P-type buffer layer 3 is much smaller than the concentration of electrons tunneled from the source region 1, and the on-current of the device remains basically unchanged, thereby greatly increasing its sensing capability.
[0047] 2. The III-V vertical structure TFET biosensor of the present invention has a larger on-current, and the source region 1 of the structure is buried in the channel region, which increases the band-to-band tunneling generation rate at the source-channel junction and can effectively compensate for the low on-current defect of the traditional horizontal pin structure.
[0048] 3. The present invention uses metal gates with different work functions. A tunneling metal gate 9 with a smaller work function is used on the side close to the tunneling junction, and an auxiliary metal gate 10 with a larger work function is used on the side far from the tunneling junction. Compared with the traditional single-gate structure, the present invention can effectively improve the electrical characteristics of the TFET device while having high sensitivity.
[0049] 4. The present invention adopts a buried source region structure, which can achieve high sensitivity at a relatively low voltage, thereby effectively reducing the power consumption of the device.
[0050] In summary, the present invention has the characteristics of strong sensing capability, high tunneling generation rate, high sensitivity and low power consumption. BRIEF DESCRIPTION OF THE DRAWINGS
[0051] Figure 1 The biosensor according to Example 1 of the present invention is simulated by computer-aided design.
[0052] Figure 2 The present invention is a flow chart of the preparation method of the embodiment of the present invention.
[0053] Figure 3 This is a transfer characteristic curve diagram of computer-aided design software simulation according to Example 1 of the present invention.
[0054] Figure 4 The on-current sensitivity of biomolecules with different dielectric constants is compared between Example 1 of the present invention and a biosensor based on a traditional VTFET.
[0055] Figure 5This is a transfer characteristic curve diagram of computer-aided design software simulation according to implementation 2 of the present invention.
[0056] Figure 6 The on-current sensitivity of biomolecules with different dielectric constants is compared between Example 2 of the present invention and a biosensor based on a traditional VTFET.
[0057] Figure 7 This is a transfer characteristic curve diagram of computer-aided design software simulation according to implementation 3 of the present invention.
[0058] Figure 8 The on-current sensitivity of biomolecules with different dielectric constants of Example 3 of the present invention is compared with that of the conventional VTFET-based biosensor.
[0059] In the figure, 1 is the source region, 2 is the channel, 3 is the buffer layer, 4 is the drain region, 5 is the substrate, 6 is the drain, 7 is the gate oxide layer, 8 is the biomolecule cavity, 9 is the tunneling metal gate, 10 is the auxiliary metal gate, and 11 is the source. DETAILED DESCRIPTION
[0060] The present invention will be described in detail below in conjunction with the accompanying drawings.
[0061] like Figure 1 As shown, a biosensor of a III-V vertical tunneling field effect transistor with a P-type buffer layer and a buried channel region includes a substrate 5, a drain region 4, a buffer layer 3, a channel 2, a source region 1 and a source electrode 11 stacked from bottom to top. The drain region 1 is embedded in the channel 2 to form a buried structure and produces a vertical tunneling field effect. Gate oxide layers 7 are arranged on both sides of the bottom of the channel 2. An auxiliary metal gate 10 is arranged on the side of each gate oxide layer 7 away from the channel 2. A tunneling metal gate 9 is stacked on the upper surface of each auxiliary metal gate 10. The tunneling metal gate 9, the auxiliary metal gate 10, the gate oxide layer 7 and the channel 2 surround a biomolecule cavity 8. Drain electrodes 6 are also arranged at both ends of the upper surface of the substrate 5.
[0062] like Figure 2 As shown, the method for preparing a biosensor of a III-V vertical tunneling field effect transistor with a P-type buffer layer and a buried channel region comprises the following steps:
[0063] Step 1: Prepare a heavily doped N-type semiconductor as a substrate 5;
[0064] Step 2: growing a layer of heavily doped N-type semiconductor as a drain region 4 on the substrate 5 prepared in step 1;
[0065] Step 3: growing a layer of lightly doped P-type semiconductor as a buffer layer 3 on the N-type semiconductor prepared in step 2;
[0066] Step 4: growing a lightly doped N-type semiconductor region on the buffer layer 3 prepared in step 3;
[0067] Step 5: etching the center of the lightly doped N-type semiconductor region generated in step 4 to form a source pre-growth region, and the lightly doped N-type semiconductor after etching serves as a channel 2;
[0068] Step 6: growing a layer of heavily doped P-type semiconductor in the source pre-growth region etched in step 5 as source region 1;
[0069] Step 7: depositing a layer of dielectric material on both sides of the channel 2 obtained in step 4 as a gate oxide layer region;
[0070] Step 8: The dielectric material deposited in step 7 is etched to form a gate oxide layer 7 and a biomolecule cavity 8, and then two metals with different work functions are deposited on both sides of the gate oxide layer 7 and the biomolecule cavity 8 as a tunneling metal gate 9 and an auxiliary metal gate 10, a layer of polycrystalline material is deposited above the source region 1 as a source 11, and a layer of polycrystalline material is deposited on both sides of the substrate 5 as a drain 6.
[0071] Based on the above-mentioned III-V vertical tunneling field effect transistor with a P-type buffer layer and a buried channel region and the preparation method thereof, further description is given in combination with embodiments of different materials, sizes and processes.
[0072] Example 1
[0073] The heavily doped N-type semiconductor material in step 1 is silicon, with a length of 40 nm and a width of 20 nm. Phosphorus (P) is selected as the dopant by ion implantation, and the doping concentration is 5×10 18 cm -3 The injection energy is controlled to be 100 keV, and the entire ion injection process is carried out at 20°C. After the ion injection is completed, thermal annealing is performed to activate the phosphorus ions. The thermal annealing temperature is between 600°C and the thermal annealing time is controlled to be 30 minutes.
[0074] The heavily doped N-type semiconductor material generated in step 2 is silicon, with a length of 20 nm and a width of 10 nm. An epitaxial growth process is adopted. First, the silicon substrate for epitaxial growth is cleaned, and then the cleaned silicon substrate is placed in an epitaxial growth chamber for subsequent operations. The epitaxial growth chamber is a vacuum environment, and the growth temperature is set at 1100° C. The pressure is a low-pressure environment of 90 Pa. The flow rate of the silicon source gas is set at 15 sccm, and the flow rate of hydrogen as a carrier gas is set at 180 sccm. During the growth process, phosphine (PH3) is introduced as a dopant gas, and the doping concentration is 5×10 18 cm -3The growth time is set at 50 minutes. After the growth is completed, it is subjected to thermal annealing treatment. The thermal annealing temperature is 400°C and the thermal annealing time is controlled at 10 minutes.
[0075] The lightly doped P-type semiconductor material generated in step 3 is silicon, with a length the same as that of the drain region 4 and a width of 20 nm. The epitaxial growth process is adopted. First, the silicon substrate for epitaxial growth is cleaned, and then the cleaned silicon substrate is placed in an epitaxial growth chamber for subsequent operations. The epitaxial growth chamber is a vacuum environment, and the growth temperature is set at 800° C. The pressure is a low-pressure environment of 90 Pa. Boron (B) is introduced as a dopant with a doping concentration of 5×10 15 cm -3 The growth time is set at 50 minutes. After the growth is completed, it is subjected to thermal annealing treatment. The thermal annealing temperature is 400°C and the thermal annealing time is controlled at 10 minutes.
[0076] The lightly doped N-type semiconductor material generated in step 4 is silicon, with a length the same as that of the semiconductor buffer layer 3 and a width of 40 nm. An epitaxial growth process is adopted. First, the silicon substrate for epitaxial growth is cleaned, and then the cleaned silicon substrate is placed in an epitaxial growth chamber for subsequent operations. The epitaxial growth chamber is a vacuum environment, and the growth temperature is set at 1000° C. and the pressure is a low-pressure environment of 90 Pa. The flow rate of the silicon source gas is set at 15 sccmsccm, and the flow rate of hydrogen as a carrier gas is set at 180 sccm. During the growth process, phosphine (PH3) is introduced as a dopant gas, and the doping concentration is 5×10 15 cm -3 The growth time is set at 50 minutes. After the growth is completed, it is subjected to thermal annealing treatment. The thermal annealing temperature is 400°C and the thermal annealing time is controlled at 10 minutes.
[0077] The source pre-growth region in the step 5 is formed by dry etching technology. The top is flush with the top of the channel 2 and has a width of 15 nm. The two sides of the source pre-growth region have the same length as the channel 2, both of which are 2 nm. A high-frequency inductively coupled plasma reactor (ICP-RIE) is used, and chlorine (Cl2) is selected as the etching gas. The RF power is set at 100 W, the frequency is 13.56 MHz, the pressure of the etching chamber is 10 mTorr, and etching is performed at 25°C with an etching rate of 30 nm / min.
[0078] The heavily doped P-type semiconductor material in step 6 is a III-V narrow bandgap compound GaSb, which has the same size as the source pre-growth region and is grown using molecular beam epitaxy (MBE) technology. First, the silicon substrate for epitaxial growth is cleaned, and then the cleaned silicon substrate is placed in an MOCVD reaction chamber for subsequent operations. The reaction temperature is set to 500°C, and trimethyl gallium (TMGa) and arsenic (AsH3) are used as reaction gases in a ratio of 1:8. During the growth process, dimethyl germanium (GeH2) is added as a dopant with a doping concentration of 1×10 19 cm -3 After the growth is completed, thermal annealing is performed at a temperature of 300°C for 30 minutes.
[0079] The dielectric material deposited in step 7 is SiO2, and the dielectric constant of the deposited dielectric material is 4, the length is 5nm, and the width is 20nm. The atomic layer deposition process (ALD) is used. First, the semiconductor material is chemically cleaned to remove oxides and organic residues to ensure optimal surface acceptance. Dimethyl silicon oxide is used as a precursor for depositing the dielectric layer. The precursor is introduced into the reaction chamber and adsorbed on the silicon surface. Oxygen is introduced to remove unreacted precursors and by-products. Water vapor is introduced as an oxidant to react with the adsorbed precursor to generate a dielectric layer film. The purification step is repeated to remove by-products and unreacted gases generated during the reaction. During this process, the temperature is controlled at 200°C and adjusted according to the characteristics of the ALD precursor and the reaction conditions. The ambient pressure is maintained at 2Torr. The thickness of the dielectric layer film is increased by repeating the ALD cycle, and the thickness increases by 5 angstroms each cycle.
[0080] In the step 8, the dielectric material is etched using dry etching technology, an inductively coupled plasma (ICP) etcher and hydrogen fluoride (HF) are selected as etching gases for operation, the overall ambient temperature is maintained at 20° C., the inductively coupled plasma (ICP) etcher is started to generate plasma, and then hydrogen fluoride etching gas is input to ensure that the flow rate is 40 sccm, and the pressure of the reaction chamber is adjusted to 40 mTorr to maintain a stable etching atmosphere. At a discharge power of 200 W and a frequency of 13.56 MHz, hydrogen fluoride reacts with the surface of the dielectric material to generate compounds to achieve etching, and after the etching is completed, cleaning is performed to remove etching residues. After the etching is completed, the bottom of the gate oxide layer 7 formed is flush with the bottom of the channel 2, with a length of 5 nm and a width of 3 nm. The biomolecule cavity 8 is located above the gate oxide layer 7, with a length the same as that of the gate oxide layer 7 and a width of 17 nm;
[0081] The deposited tunneling metal gate 9 is made of metal aluminum with a work function of 3.7 eV; the auxiliary metal gate 10 is made of metal chromium with a work function of 4.2 eV. The tunneling metal gate 9 and the auxiliary metal gate 10 are located on the side of the gate oxide layer 7 and the biomolecule cavity 8 away from the channel 2, and both have a length of 3 nm. The sum of the widths of the tunneling metal gate 9 and the auxiliary metal gate 10 is the same as the sum of the widths of the gate oxide layer 7 and the biomolecule cavity 8, and the width ratio of the tunneling metal gate 9 to the auxiliary metal gate 10 is 1:1. The deposition is carried out using a reactive sputtering process using a magnetron sputtering system. First, the target material is heated to 300°C to increase the evaporation rate of the metal, and the temperature of the substrate is controlled at 100°C to avoid thermal damage to the film on the substrate. The pressure of the sputtering chamber is set at 10 -6 Torr, start the sputtering system, heat the target materials of the tunneling metal gate 9 and the auxiliary metal gate 10 and apply an electric field to sputter the target materials from the surface of the target gun to the silicon substrate, set the sputtering power of the material of the tunneling metal gate 9 to 80W, and the sputtering power of the material of the auxiliary metal gate 10 to 50W, so as to form the required metal film on the semiconductor surface. After the sputtering process is completed, release the vacuum chamber gas and take out the semiconductor substrate, and use the characterization technology to evaluate the morphology, composition and bonding state of the metal film. The characterization technology is SEM to ensure the quality and stability of the gate electrode;
[0082] The drain 6 and the source 11 are both made of polysilicon. The drain 6 is located at the edges of both sides of the substrate 5, with a length of 4 nm and a width of 2 nm. The source 11 is located above the source region 1, with a length consistent with that of the source region 1 and a width of 2 nm. The conductivity is 10 -3 S / m, formed by chemical vapor deposition (CVD), first preheat the CVD reaction chamber to 500, and control the pressure in the chamber to 10 - 2 Torr, to promote subsequent deposition, dimethylsilane (SiH2(CH3)2) is introduced as the silicon source gas with a flow rate of 50sccm, and hydrogen (H2) is used as the diluent gas with a flow rate of 200sccm. The silicon source gas is decomposed in the reaction chamber and an electrode film is deposited on the surface of the substrate. The deposited electrode film is then annealed to improve its crystallinity and electrical properties. The thermal annealing temperature is 500°C and the thermal annealing time is controlled to 20 minutes.
[0083] Example 2
[0084] The heavily doped N-type semiconductor material in step 1 is silicon, with a length of 80 nm and a width of 40 nm. Phosphorus (P) is selected as the dopant by ion implantation, and the doping concentration is 1×10 20 cm -3The injection energy is controlled to be 200keV, and the entire ion injection process is carried out at 25°C. After the ion injection is completed, thermal annealing is performed to activate the phosphorus ions. The thermal annealing temperature is between 1000°C and the thermal annealing time is controlled to be 60 minutes.
[0085] The heavily doped N-type semiconductor material generated in step 2 is silicon, with a length of 25 nm and a width of 15 nm. An epitaxial growth process is adopted. First, the silicon substrate for epitaxial growth is cleaned, and then the cleaned silicon substrate is placed in an epitaxial growth chamber for subsequent operations. The epitaxial growth chamber is an inert gas environment, and the growth temperature is set at 1300° C. The pressure is a low-pressure environment of 100 Pa. The flow rate of the silicon source gas is set at 20 sccm, and the flow rate of hydrogen as a carrier gas is set at 200 sccm. During the growth process, phosphine (PH3) is introduced as a dopant gas, and the doping concentration is 1×10 20 cm -3 The growth time is set at 120 minutes. After the growth is completed, it is subjected to thermal annealing treatment. The thermal annealing temperature is 800°C and the thermal annealing time is controlled at 30 minutes.
[0086] The lightly doped P-type semiconductor material generated in step 3 is silicon, with a length the same as that of the drain region 4 and a width of 25 nm. The epitaxial growth process is adopted. First, the silicon substrate for epitaxial growth is cleaned, and then the cleaned silicon substrate is placed in an epitaxial growth chamber for subsequent operations. The epitaxial growth chamber is an inert gas environment, and the growth temperature is set at 1100° C. The pressure is a low-pressure environment of 100 Pa. Boron (B) is introduced as a dopant with a doping concentration of 1×10 17 cm -3 The growth time is set at 80 minutes. After the growth is completed, it is subjected to thermal annealing treatment. The thermal annealing temperature is 600°C and the thermal annealing time is controlled at 30 minutes.
[0087] The lightly doped N-type semiconductor material generated in step 4 is silicon, with a length the same as that of the semiconductor buffer layer 3 and a width of 50 nm. An epitaxial growth process is adopted. First, the silicon substrate for epitaxial growth is cleaned, and then the cleaned silicon substrate is placed in an epitaxial growth chamber for subsequent operations. The epitaxial growth chamber is an inert gas environment, and the growth temperature is set at 1200° C. The pressure is a low-pressure environment of 100 Pa. The flow rate of the silicon source gas is set at 20 sccm, and the flow rate of hydrogen as a carrier gas is set at 200 sccm. During the growth process, phosphine (PH3) is introduced as a dopant gas, and the doping concentration is 1×10 17 cm -3 The growth time is set at 80 minutes. After the growth is completed, it is subjected to thermal annealing treatment. The thermal annealing temperature is 600°C and the thermal annealing time is controlled at 30 minutes.
[0088] The source pre-growth region in the step 5 is formed by dry etching technology. The top is flush with the top of the channel 2 and has a width of 20 nm. The two sides of the source pre-growth region have the same length as the channel 2, both of which are 3 nm. A high-frequency inductively coupled plasma reactor (ICP-RIE) is used, and chlorine (Cl2) is selected as the etching gas. The RF power is set at 200 W, the frequency is 13.56 MHz, the pressure of the etching chamber is 50 mTorr, and etching is performed at 30°C with an etching rate of 50 nm / min.
[0089] The heavily doped P-type semiconductor material in step 6 is a III-V narrow bandgap compound GaSb, which has the same size as the source pre-growth region and is grown using molecular beam epitaxy (MBE) technology. First, the silicon substrate for epitaxial growth is cleaned, and then the cleaned silicon substrate is placed in an MOCVD reaction chamber for subsequent operations. The reaction temperature is set to 700°C, and trimethyl gallium (TMGa) and arsenic (AsH3) are used as reaction gases in a ratio of 1:12. During the growth process, dimethyl zinc (Zn(CH3)2) is added as a dopant with a doping concentration of 1×10 20 cm -3 After the growth is completed, thermal annealing is performed at a temperature of 500°C for 50 minutes.
[0090] The dielectric material deposited in step 7 is HfO2, and the dielectric constant of the deposited dielectric material is 25, the length is 7nm, and the width is 30nm. The atomic layer deposition process (ALD) is used. First, the semiconductor material is treated with hydrogen to remove oxides and organic residues to ensure optimal surface acceptance. Trimethoxyhafnium is used as a precursor for depositing the dielectric layer. The precursor is introduced into the reaction chamber and adsorbed on the silicon surface. Nitrogen is introduced to remove unreacted precursors and by-products. Water vapor is introduced as an oxidant to react with the adsorbed precursor to generate a dielectric layer film. The purification step is repeated to remove by-products and unreacted gases generated during the reaction. During this process, the temperature is controlled at 400°C and adjusted according to the characteristics of the ALD precursor and the reaction conditions. The ambient pressure is maintained at 10 Torr. The thickness of the dielectric layer film is increased by repeating the ALD cycle, and the thickness increases by 20 angstroms per cycle.
[0091] In the step 8, the dielectric material is etched using dry etching technology, an inductively coupled plasma (ICP) etcher and hydrogen fluoride (HF) are selected as etching gases for operation, the overall ambient temperature is maintained at 25° C., the inductively coupled plasma (ICP) etcher is started to generate plasma, and then hydrogen fluoride etching gas is input to ensure that the flow rate is 50 sccm, and the pressure of the reaction chamber is adjusted to 50 mTorr to maintain a stable etching atmosphere. At a discharge power of 300 W and a frequency of 13.56 MHz, hydrogen fluoride reacts with the surface of the dielectric material to generate compounds to achieve etching, and after the etching is completed, cleaning is performed to remove etching residues. After the etching is completed, the bottom of the gate oxide layer 7 formed is flush with the bottom of the channel 2, with a length of 7 nm and a width of 5 nm. The biomolecule cavity 8 is located above the gate oxide layer 7, with a length the same as that of the gate oxide layer 7 and a width of 25 nm.
[0092] The deposited tunneling metal gate 9 is made of metallic silver with a work function of 4.1 eV; the auxiliary metal gate 10 is made of metallic hafnium with a work function of 4.5 eV. The tunneling metal gate 9 and the auxiliary metal gate 10 are located on the side of the gate oxide layer 7 and the biomolecule cavity 8 away from the channel 2, and both have a length of 5 nm. The sum of the widths of the tunneling metal gate 9 and the auxiliary metal gate 10 is the same as the sum of the widths of the gate oxide layer 7 and the biomolecule cavity 8, and the width ratio of the tunneling metal gate 9 to the auxiliary metal gate 10 is 1.3:1. The deposition is carried out using a magnetron sputtering system using a reactive sputtering process. First, the target material is heated to 600°C to increase the evaporation rate of the metal. At the same time, the temperature of the substrate is controlled at 300°C to avoid thermal damage to the film on the substrate. The pressure of the sputtering chamber is set at 10 - 8 Torr, start the sputtering system, heat the target materials of the tunneling metal gate 9 and the auxiliary metal gate 10 and apply an electric field to sputter the target materials from the surface of the target gun to the silicon substrate, set the sputtering power of the material of the tunneling metal gate 9 to 200W, and the sputtering power of the material of the auxiliary metal gate 10 to 150W, so as to form the required metal film on the semiconductor surface. After the sputtering process is completed, release the vacuum chamber gas and take out the semiconductor substrate, and use the characterization technology to evaluate the morphology, composition and bonding state of the metal film, and the characterization technology is XPS to ensure the quality and stability of the gate electrode;
[0093] The drain 6 and the source 11 are both made of polysilicon. The drain 6 is located at the edges of both sides of the substrate 5, with a length of 5 nm and a width of 3 nm. The source 11 is located above the source region 1, with a length consistent with that of the source region 1 and a width of 3 nm. The conductivity is 10 -1 S / m, formed by chemical vapor deposition (CVD), first preheating the CVD reaction chamber to 700 ° C, and controlling the pressure in the chamber at 10 1Torr, to promote subsequent deposition, dimethylsilane (SiH2(CH3)2) is introduced as the silicon source gas with a flow rate of 100sccm, and hydrogen (H2) is used as the diluent gas with a flow rate of 500sccm. The silicon source gas is decomposed in the reaction chamber and an electrode film is deposited on the surface of the substrate. The deposited electrode film is then annealed to improve its crystallinity and electrical properties. The thermal annealing temperature is 1000°C and the thermal annealing time is controlled at 40 minutes.
[0094] Example 3
[0095] The heavily doped N-type semiconductor material in step 1 is silicon, with a length of 60 nm and a width of 30 nm. Phosphorus (P) is selected as the dopant by ion implantation, and the doping concentration is 1×10 19 cm -3 The injection energy is controlled to be 180keV, and the entire ion injection process is carried out at 22°C. After the ion injection is completed, thermal annealing is performed to activate the phosphorus ions. The thermal annealing temperature is between 800°C and the thermal annealing time is controlled to be 40 minutes.
[0096] The heavily doped N-type semiconductor material generated in step 2 is silicon, with a length of 22 nm and a width of 12 nm. An epitaxial growth process is adopted. First, the silicon substrate for epitaxial growth is cleaned, and then the cleaned silicon substrate is placed in an epitaxial growth chamber for subsequent operations. The epitaxial growth chamber is a vacuum or environment, and the growth temperature is set at 1200° C. and the pressure is a low-pressure environment of 95 Pa. The flow rate of the silicon source gas is set at 18 sccm, and the flow rate of hydrogen as a carrier gas is set at 190 sccm. During the growth process, phosphine (PH3) is introduced as a dopant gas, and the doping concentration is 1×10 19 cm -3 The growth time is set at 70 minutes. After the growth is completed, it is subjected to thermal annealing treatment. The thermal annealing temperature is 600°C and the thermal annealing time is controlled at 20 minutes.
[0097] The lightly doped P-type semiconductor material generated in step 3 is silicon, with a length the same as that of the drain region 4 and a width of 22 nm. The epitaxial growth process is adopted. First, the silicon substrate for epitaxial growth is cleaned, and then the cleaned silicon substrate is placed in an epitaxial growth chamber for subsequent operations. The epitaxial growth chamber is a vacuum environment, and the growth temperature is set at 1000° C. and the pressure is a low-pressure environment of 95 Pa. Boron (B) is introduced as a dopant with a doping concentration of 1×10 16 cm -3 The growth time is set at 70 minutes. After the growth is completed, it is subjected to thermal annealing treatment. The thermal annealing temperature is 500°C and the thermal annealing time is controlled at 20 minutes.
[0098] The lightly doped N-type semiconductor material generated in step 4 is silicon, with a length the same as that of the semiconductor buffer layer 3 and a width of 45 nm. An epitaxial growth process is adopted. First, the silicon substrate for epitaxial growth is cleaned, and then the cleaned silicon substrate is placed in an epitaxial growth chamber for subsequent operations. The epitaxial growth chamber is a vacuum environment, and the growth temperature is set at 1100° C. and the pressure is a low-pressure environment of 95 Paa. The flow rate of the silicon source gas is set at 18 sccm, and the flow rate of hydrogen as a carrier gas is set at 190 sccm. During the growth process, phosphine (PH3) is introduced as a dopant gas, and the doping concentration is 1×10 16 cm -3 The growth time is set at 60 minutes. After the growth is completed, it is subjected to thermal annealing treatment. The thermal annealing temperature is 500°C and the thermal annealing time is controlled at 20 minutes.
[0099] The source pre-growth region in the step 5 is formed by dry etching technology. The top is flush with the top of the channel 2 and has a width of 18 nm. The two sides of the source pre-growth region have the same length as the channel 2, both of which are 2 nm. A high-frequency inductively coupled plasma reactor (ICP-RIE) is used, and chlorine (Cl2) is selected as the etching gas. The RF power is set at 150 W, the frequency is 13.56 MHz, the pressure of the etching chamber is 30 mTorr, and etching is performed at 28°C at an etching rate of 40 nm / min.
[0100] The heavily doped P-type semiconductor material in step 6 is a III-V narrow bandgap compound GaSb, which has the same size as the source pre-growth region and is grown using molecular beam epitaxy (MBE) technology. First, the silicon substrate for epitaxial growth is cleaned, and then the cleaned silicon substrate is placed in an MOCVD reaction chamber for subsequent operations. The reaction temperature is set to 600°C, and trimethyl gallium (TMGa) and arsenic (AsH3) are used as reaction gases in a ratio of 1:10. During the growth process, dimethyl germanium (GeH2) is added as a dopant with a doping concentration of 5×10 19 cm -3 After the growth is completed, thermal annealing is performed at a temperature of 400°C for 40 minutes.
[0101] The dielectric material deposited in step 7 is Al2O3, and the dielectric constant of the deposited dielectric material is 10, the length is 6nm, and the width is 25nm. The atomic layer deposition process (ALD) is used. First, the semiconductor material is chemically cleaned to remove oxides and organic residues to ensure optimal surface acceptance. Trimethoxyaluminum is used as a precursor for depositing the dielectric layer. The precursor is introduced into the reaction chamber and adsorbed on the silicon surface. Oxygen is introduced to remove unreacted precursors and by-products. Water vapor is introduced as an oxidant to react with the adsorbed precursor to generate a dielectric layer film. The purification step is repeated to remove by-products and unreacted gases generated during the reaction. During this process, the temperature is controlled at 300°C and adjusted according to the characteristics of the ALD precursor and the reaction conditions. The ambient pressure is maintained at 8Torr. The thickness of the dielectric layer film is increased by repeating the ALD cycle, and the thickness increases by 10 angstroms each cycle.
[0102] In the step 8, the dielectric material is etched using dry etching technology, and an inductively coupled plasma (ICP) etcher and hydrogen fluoride (HF) are selected as etching gases for operation. The overall ambient temperature is maintained at 22° C. The inductively coupled plasma (ICP) etcher is started to generate plasma, and then hydrogen fluoride etching gas is input to ensure that the flow rate is 45 sccm. The pressure of the reaction chamber is adjusted to 45 mTorr to maintain a stable etching atmosphere. At a discharge power of 250 W and a frequency of 13.56 MHz, hydrogen fluoride reacts with the surface of the dielectric material to generate compounds to achieve etching. After the etching is completed, cleaning is performed to remove the etching residues. After the etching is completed, the bottom of the gate oxide layer 7 formed is flush with the bottom of the channel 2, with a length of 6 nm and a width of 4 nm. The biomolecule cavity 8 is located above the gate oxide layer 7, with a length the same as that of the gate oxide layer 7 and a width of 20 nm.
[0103] The deposited tunneling metal gate 9 is made of metal aluminum with a work function of 3.7 eV; the auxiliary metal gate 10 is made of metal hafnium with a work function of 4.5 eV. The tunneling metal gate 9 and the auxiliary metal gate 10 are located on the side of the gate oxide layer 7 and the biomolecule cavity 8 away from the channel 2, and both have a length of 4 nm. The sum of the widths of the tunneling metal gate 9 and the auxiliary metal gate 10 is the same as the sum of the widths of the gate oxide layer 7 and the biomolecule cavity 8, and the width ratio of the tunneling metal gate 9 to the auxiliary metal gate 10 is 1.2:1. The deposition is carried out using a reactive sputtering process using a magnetron sputtering system. First, the target material is heated to 500°C to increase the evaporation rate of the metal, and the temperature of the substrate is controlled at 200°C to avoid thermal damage to the film on the substrate. The pressure of the sputtering chamber is set at 10 - 7Torr, start the sputtering system, heat the target materials of the tunneling metal gate 9 and the auxiliary metal gate 10 and apply an electric field to sputter the target materials from the surface of the target gun to the silicon substrate, set the sputtering power of the material of the tunneling metal gate 9 to 100W, and the sputtering power of the material of the auxiliary metal gate 10 to 120W, so as to form the required metal film on the surface of the semiconductor. After the sputtering process is completed, release the vacuum chamber gas and take out the semiconductor substrate, and use the characterization technology to evaluate the morphology, composition and bonding state of the metal film, and the characterization technology is XPS to ensure the quality and stability of the gate electrode;
[0104] The drain 6 and the source 11 are both made of polysilicon. The drain 6 is located at the edges of both sides of the substrate 5, with a length of 5 nm and a width of 3 nm. The source 11 is located above the source region 1, with a length consistent with that of the source region 1 and a width of 3 nm. The conductivity is 10 -2 S / m, formed by chemical vapor deposition (CVD), first preheat the CVD reaction chamber to 600, and control the pressure in the chamber at 10 - 1 Torr, to promote subsequent deposition, dimethylsilane (SiH2(CH3)2) is introduced as the silicon source gas with a flow rate of 80sccm, and hydrogen (H2) is used as the diluent gas with a flow rate of 300sccm. The silicon source gas is decomposed in the reaction chamber and an electrode film is deposited on the surface of the substrate. The deposited electrode film is then annealed to improve its crystallinity and electrical properties. The thermal annealing temperature is 800°C and the thermal annealing time is controlled to 30 minutes.
[0105] Simulation experiment
[0106] Figure 3 The transfer characteristic curves obtained by the biosensor of Example 1 for detecting biomolecules with different dielectric constants. In the figure, K=3, 7, and 12 represent biomolecules with different dielectric constants, while K=1 represents the dielectric constant of air, i.e., the situation when no biomolecules enter. V DS represents the drain-source voltage; due to the presence of the P-type buffer layer, the difference in electrical properties of biomolecules after entering the cavity is increased, and the sensor has greater sensitivity. Figure 3 It can be seen that when detecting biological molecules with K = 12, it reaches about 5.62×10 -6 A / μm, reaching about 1.36×10 -6 A / μm, reaching about 3.11×10 -8 A / μm. Figure 4: is a sensitivity comparison diagram of the biosensor of Example 1 and the traditional TFET biosensor when detecting biomolecules with different dielectric constants. The sensitivity is obtained by calculating the ratio of the saturated conduction current when biomolecules with different dielectric constants enter the cavity to the saturated conduction current when air enters the cavity, where V GS Represents the drain-source voltage, V DS Represents the drain-source voltage. Figure 4 It can be seen that the sensitivity is about 187.5 when detecting biomolecules with K=3, and the sensitivity is about 8.24×10 3 , when detecting biological molecules with K=12, it is about 3.4×10 4 , indicating that the biosensor structure prepared by the present invention has a higher sensitivity for detecting biomolecules with a larger dielectric constant. Compared with the traditional TFET biosensor, the sensitivity of the biosensor prepared by the present invention is about 4.12 times higher when detecting biomolecules with K=3, about 23.3 times higher when detecting biomolecules with K=7, and about 16.02 times higher when detecting biomolecules with K=12, indicating that the sensitivity of the biosensor prepared by the present invention is higher.
[0107] Figure 5 The transfer characteristic curves obtained by the biosensor of Example 2 for detecting biomolecules with different dielectric constants. In the figure, K=3, 7, and 12 represent biomolecules with different dielectric constants, while K=1 represents the dielectric constant of air, i.e., the situation when no biomolecules enter. V DS represents the drain-source voltage; due to the presence of the P-type buffer layer, the difference in electrical properties of biomolecules after entering the cavity is increased, and the sensor has greater sensitivity. Figure 5 It can be seen that when detecting biological molecules with K = 12, it reaches about 5.68×10 -6 A / μm, reaching about 1.42×10 -6 A / μm, reaching about 3.23×10 -8 A / μm. Figure 6 : is a sensitivity comparison diagram of the biosensor of Example 2 and the traditional TFET biosensor when detecting biomolecules with different dielectric constants. The sensitivity is obtained by calculating the ratio of the saturated conduction current when biomolecules with different dielectric constants enter the cavity to the saturated conduction current when air enters the cavity, where V GS Represents the drain-source voltage, V DS Represents the drain-source voltage. Figure 6 It can be seen that the sensitivity is about 1.86×10 3, the sensitivity is about 8.11×10 4 , when detecting biological molecules with K=12, it is about 3.34×10 5 , indicating that the biosensor structure prepared by the present invention has a higher sensitivity for detecting biomolecules with a larger dielectric constant. Compared with the traditional TFET biosensor, the sensitivity of the biosensor prepared by the present invention is about 40.9 times higher when detecting biomolecules with K=3, about 228.9 times higher when detecting biomolecules with K=7, and about 157.5 times higher when detecting biomolecules with K=12, indicating that the sensitivity of the biosensor prepared by the present invention is higher.
[0108] Figure 7 The transfer characteristic curves obtained by the biosensor of Example 3 for detecting biomolecules with different dielectric constants. In the figure, K=3, 7, and 12 represent biomolecules with different dielectric constants, while K=1 represents the dielectric constant of air, i.e., the situation when no biomolecules enter. V DS represents the drain-source voltage; due to the presence of the P-type buffer layer, the difference in electrical properties of biomolecules after entering the cavity is increased, and the sensor has greater sensitivity. Figure 7 It can be seen that when detecting biological molecules with K = 12, the value reached about 4.87×10 -6 A / μm, reaching about 1.57×10 -7 A / μm, reaching about 6.88×10 -9 A / μm. Figure 8 : is a comparison chart of the sensitivity of the biosensor of Example 3 and the traditional TFET biosensor when detecting biomolecules with different dielectric constants. The sensitivity is obtained by calculating the ratio of the saturated conduction current when biomolecules with different dielectric constants enter the cavity to the saturated conduction current when air enters the cavity, where V GS Represents the drain-source voltage, V DS Represents the drain-source voltage. Figure 8 It can be seen that the sensitivity is about 60.1 when detecting biomolecules with K=3, and the sensitivity is about 1.39×10 4 , when detecting biological molecules with K=12, it is about 4.3×10 5, indicating that the biosensor structure prepared by the present invention has a higher sensitivity for detecting biomolecules with a larger dielectric constant. Compared with the traditional TFET biosensor, the sensitivity of the biosensor prepared by the present invention is about 1.45 times higher when detecting biomolecules with K=3, about 39.2 times higher when detecting biomolecules with K=7, and about 202.7 times higher when detecting biomolecules with K=12, indicating that the sensitivity of the biosensor prepared by the present invention is higher.
Claims
1. A biosensor of a III-V vertical tunneling field effect transistor with a P-type buffer layer and a buried channel region, characterized in that: The invention comprises a substrate (5), a drain region (4), a buffer layer (3), a channel (2), a source region (1) and a source electrode (11) which are stacked from bottom to top. The drain region (1) is embedded in the channel (2) to form a buried structure and generate a vertical tunneling field effect. Gate oxide layers (7) are arranged on both sides of the bottom of the channel (2). An auxiliary metal gate (10) is arranged on the side of each gate oxide layer (7) away from the channel (2). A tunneling metal gate (9) is stacked on the upper surface of each auxiliary metal gate (10). The tunneling metal gate (9), the auxiliary metal gate (10), the gate oxide layer (7) and the channel (2) form a biomolecule cavity (8). Drain electrodes (6) are also arranged at both ends of the upper surface of the substrate (5).
2. A biosensor of a III-V vertical tunneling field effect transistor with a P-type buffer layer and a buried channel region according to claim 1, characterized in that: The source region (1) is made of III-V narrow bandgap compound GaSb material; The channel (2), buffer layer (3), drain region (4) and substrate (5) are all made of Si material; The drain (6) and the source (11) are both made of polysilicon material; The gate oxide layer (7) is made of SiO2 material, Al2O3 material or HfO2 material; The tunneling metal gate (9) is made of metal aluminum material or metal silver material; The auxiliary metal grid (10) is made of metal chromium material or metal hafnium material.
3. A biosensor of a III-V vertical tunneling field effect transistor with a P-type buffer layer and a buried channel region according to claim 1, characterized in that: The source region (1) is a P-type heavily doped region with a doping concentration of 1×10 19 cm -3 ~1×10 20 cm -3 ; The channel (2) is an N-type lightly doped region with a doping concentration of 1×10 15 cm -3 ~1×10 17 cm -3 ; The buffer layer (3) is a P-type lightly doped region with a doping concentration of 5×10 15 cm -3 ~1×10 17 cm -3 ; The drain region (4) and the substrate (5) are both N-type heavily doped regions with the same doping concentration of 5×10 18 cm -3 ~1×10 20 cm -3 .
4. A biosensor of a III-V vertical tunneling field effect transistor with a P-type buffer layer and a buried channel region according to claim 1, characterized in that: The substrate (5) has a length of 40nm to 80nm and a width of 20nm to 40nm; the drain region (4), the buffer layer (3) and the channel (2) have the same length, the drain region (4) is located above the center of the substrate (5), has a length of 20nm to 25nm and a width of 10nm to 15nm; the buffer layer (3) is located above the drain region (4), has a width of 20nm to 25nm; the channel (2) is located above the buffer layer (3), has a width of 40nm to 50nm; the top of the source region (1) is flush with the top of the channel (2), has a width of 15nm to 20nm, and the channels (2) on both sides of the source region (1) have the same length, both of which are 2nm to 3nm; the bottom of the gate oxide layer (7) is flush with the bottom of the channel (2), has a length of 5nm to 7nm and a width of The biomolecule cavity (8) is located above the gate oxide layer (7), has the same length as the gate oxide layer (7), and has a width of 17nm to 25nm; the tunneling metal gate (9) and the auxiliary metal gate (10) are both 3nm to 5nm long, the sum of the widths of the tunneling metal gate (9) and the auxiliary metal gate (10) is the same as the sum of the widths of the gate oxide layer (7) and the biomolecule cavity (8), and the width ratio of the tunneling metal gate (9) to the auxiliary metal gate (10) is (1 to 1.3):1; the drain (6) is located at the edges of both sides of the substrate (5), has a length of 4nm to 5nm, and has a width of 2nm to 3nm; the source (11) is located above the source region (1), has a length consistent with the length of the source region (1), and has a width of 2nm to 3nm.
5. A method for preparing a biosensor of a III-V vertical tunneling field effect transistor with a P-type buffer layer and a buried channel region according to any one of claims 1 to 4, characterized in that: The following steps are involved: Step 1: Prepare a heavily doped N-type semiconductor as a substrate (5); Step 2: growing a layer of heavily doped N-type semiconductor as a drain region (4) on the substrate (5) prepared in step 1; Step 3: growing a layer of lightly doped P-type semiconductor as a buffer layer (3) on the N-type semiconductor prepared in step 2; Step 4: growing a lightly doped N-type semiconductor region on the buffer layer (3) prepared in step 3; Step 5: etching the center of the lightly doped N-type semiconductor region generated in step 4 to form a source pre-growth region, and the lightly doped N-type semiconductor after etching serves as a channel (2); Step 6: growing a layer of heavily doped P-type semiconductor in the source pre-growth region etched in step 5 as a source region (1); Step 7: depositing a layer of dielectric material on both sides of the channel (2) obtained in step 4 as a gate oxide layer region; Step 8: Etching the dielectric material deposited in step 7 to form a gate oxide layer (7) and a biomolecule cavity (8), then depositing two metals with different work functions on both sides of the gate oxide layer (7) and the biomolecule cavity (8) as a tunneling metal gate (9) and an auxiliary metal gate (10), depositing a layer of polycrystalline material on the source region (1) as a source electrode (11), and depositing a layer of polycrystalline material on both sides of the substrate (5) as a drain electrode (6).
6. The method for preparing a biosensor of a III-V vertical tunneling field effect transistor with a P-type buffer layer and a buried channel region according to claim 5, characterized in that: The material of the N-type semiconductor substrate (5) in step 1 is silicon; The material of the N-type semiconductor drain region (4) in step 2 is silicon; The material of the P-type semiconductor buffer layer (3) in step 3 is silicon; The material of the N-type semiconductor region in step 4 is silicon; The material of the P-type semiconductor source region (1) in step 6 is GaSb; The gate oxide layer material in step 7 is SiO2, Al2O3 or HfO2; The material of the tunneling metal gate (9) in step 8 is metal aluminum or metal silver, the material of the auxiliary metal gate (10) is metal chromium or metal hafnium, and the materials of the drain (6) and the source (11) are both polysilicon.
7. The method for preparing a biosensor of a III-V vertical tunneling field effect transistor with a P-type buffer layer and a buried channel region according to claim 5, characterized in that: The heavily doped N-type semiconductor substrate (5) in step 1 has a length of 40 nm to 80 nm and a width of 20 nm to 40 nm; The heavily doped N-type semiconductor drain region (4) in step 2 is located above the center of the substrate (5), has a length of 20 nm to 25 nm, and a width of 10 nm to 15 nm; The lightly doped P-type semiconductor buffer layer (3) in step 3 is located above the drain region (4), has the same length as the drain region (4), and has a width of 20 nm to 25 nm; The N-type semiconductor region in step 4 is located above the lightly doped P-type semiconductor buffer layer (3), has the same length as the lightly doped P-type semiconductor buffer layer (3), and has a width of 40 nm to 50 nm; The top of the source pre-growth region in step 5 is flush with the top of the channel (2), with a width of 15 nm to 20 nm, and the lengths of both sides of the source pre-growth region are the same as those of the channel (2), both of which are 2 nm to 3 nm; The size of the heavily doped P-type semiconductor source region (1) in step 6 is the same as the size of the source pre-growth region in step 5; The gate oxide layer region in step 7 has a length of 5 nm to 7 nm and a width of 20 nm to 30 nm; The bottom of the gate oxide layer (7) in step 8 is flush with the bottom of the channel (2), has a length of 5nm to 7nm, and a width of 3nm to 5nm. The biomolecule cavity (8) is located above the gate oxide layer (7), has the same length as the gate oxide layer (7), and has a width of 17nm to 25nm. The tunneling metal gate (9) and the auxiliary metal gate (10) are located on the side of the gate oxide layer (7) and the biomolecule cavity (8) away from the channel (2), have a length of 3nm to 5nm, and the tunneling metal gate (9) and the auxiliary metal gate (10) are located on the side of the gate oxide layer (7) and the biomolecule cavity (8) away from the channel (2). The sum of the widths of the tunneling metal gate (9) and the auxiliary metal gate (10) is the same as the sum of the widths of the gate oxide layer (7) and the biomolecule cavity (8), and the width ratio of the tunneling metal gate (9) and the auxiliary metal gate (10) is (1-1.3):1; the drain (6) is located at the edges of both sides of the substrate (5), with a length of 4nm-5nm and a width of 2nm-3nm; the source (11) is located above the source region (1), with a length consistent with that of the source region (1) and a width of 2nm-3nm.
8. The method for preparing a biosensor of a III-V vertical tunneling field effect transistor with a P-type buffer layer and a buried channel region according to claim 5, characterized in that: The heavily doped N-type semiconductor in step 1 is prepared by ion implantation, using phosphorus (P) as a dopant with a doping concentration of 5×10 18 cm -3 ~1×10 20 cm -3 , control the injection energy to 100keV to 200keV, maintain the entire ion injection process at 20°C to 25°C, and after the ion injection is completed, perform thermal annealing to activate the phosphorus ions, the thermal annealing temperature is between 600°C and 1000°C, and the thermal annealing time is controlled to be between 30 minutes and 60 minutes; The heavily doped N-type semiconductor generated in step 2 adopts an epitaxial growth process. First, the silicon substrate for epitaxial growth is cleaned, and then the cleaned silicon substrate is placed in an epitaxial growth chamber for subsequent operations. The epitaxial growth chamber is a vacuum or inert gas environment, and the growth temperature is set at 1100° C. to 1300° C., and the pressure is a low-pressure environment of 90 Pa to 100 Pa. The flow rate of the silicon source gas is set at 15 sccm to 20 sccm, and the flow rate of hydrogen as a carrier gas is set at 180 sccm to 200 sccm. During the growth process, phosphine (PH3) is introduced as a dopant gas, and the doping concentration is 5×10 18 cm -3 ~1×10 20 cm -3 The growth time is set at 50 minutes to 120 minutes. After the growth is completed, a thermal annealing treatment is performed on it. The thermal annealing temperature is 400° C. to 800° C., and the thermal annealing time is controlled at 10 minutes to 30 minutes. The lightly doped P-type semiconductor generated in step 3 adopts an epitaxial growth process. First, the silicon substrate for epitaxial growth is cleaned, and then the cleaned silicon substrate is placed in an epitaxial growth chamber for subsequent operations. The epitaxial growth chamber is a vacuum or inert gas environment, and the growth temperature is set at 800°C to 1100°C and the pressure is a low-pressure environment of 90Pa to 100Pa. Boron (B) is introduced as a dopant with a doping concentration of 5×10 15 cm -3 ~1×10 17 cm -3 The growth time is set at 50 minutes to 80 minutes. After the growth is completed, a thermal annealing treatment is performed on it. The thermal annealing temperature is 400°C to 600°C, and the thermal annealing time is controlled at 10 minutes to 30 minutes. The lightly doped N-type semiconductor generated in step 4 adopts an epitaxial growth process. First, the silicon substrate for epitaxial growth is cleaned, and then the cleaned silicon substrate is placed in an epitaxial growth chamber for subsequent operations. The epitaxial growth chamber is a vacuum or inert gas environment, and the growth temperature is set at 1000° C. to 1200° C., and the pressure is a low-pressure environment of 90 Pa to 100 Pa. The flow rate of the silicon source gas is set at 15 sccm to 20 sccm, and the flow rate of hydrogen as a carrier gas is set at 180 sccm to 200 sccm. During the growth process, phosphine (PH3) is introduced as a dopant gas, and the doping concentration is 5×10 15 cm -3 ~1×10 17 cm -3 The growth time is set at 50 minutes to 80 minutes. After the growth is completed, a thermal annealing treatment is performed on it. The thermal annealing temperature is 400°C to 600°C, and the thermal annealing time is controlled at 10 minutes to 30 minutes. The source pre-growth region in step 5 is formed by dry etching technology, using a high-frequency inductively coupled plasma reactor (ICP-RIE), selecting chlorine (Cl2) as the etching gas, setting the RF power at 100W to 200W, the frequency at 13.56MHz, the pressure of the etching chamber at 10mTorr to 50mTorr, etching at 25°C to 30°C, and the etching rate at 30nm / min to 50nm / min; The heavily doped P-type semiconductor in step 6 is generated by molecular beam epitaxy (MBE) technology. First, the silicon substrate for epitaxial growth is cleaned, and then the cleaned silicon substrate is placed in a MOCVD reaction chamber for subsequent operations. The reaction temperature is set to 500°C to 700°C, and trimethyl gallium (TMGa) and arsenic (AsH3) are used as reaction gases in a ratio of 1: (8 to 12). During the growth process, dimethyl germanium (GeH2) or dimethyl zinc (Zn(CH3)2) is added as a dopant with a doping concentration of 1×10 19 cm -3 ~1×10 20 cm -3 After the growth is completed, a thermal annealing treatment is performed, the thermal annealing temperature is 300° C. to 500° C., and the time is 30 minutes to 50 minutes; The dielectric constant of the dielectric material deposited in step 7 is 4 to 25. The atomic layer deposition process (ALD) is used. The semiconductor material is first chemically cleaned or hydrogen-treated to remove oxides and organic residues to ensure optimal surface acceptance. Trimethoxyhafnium, trimethoxyaluminum or dimethyl silicon oxide is used as a precursor for depositing the dielectric layer. The precursor is introduced into the reaction chamber to adsorb the precursor on the silicon surface. Oxygen or nitrogen is introduced to remove unreacted precursors and by-products. Water vapor is introduced as an oxidant to react with the adsorbed precursor to generate a dielectric layer film. The purification step is repeated to remove by-products and unreacted gases generated during the reaction. During this process, the temperature is controlled at 200° C. to 400° C. and adjusted according to the characteristics of the ALD precursor and the reaction conditions. The ambient pressure is maintained at 2 to 10 Torr. The thickness of the dielectric layer film is increased by repeating the ALD cycle, and the thickness increases by 5 angstroms to 20 angstroms per cycle. In step 8, the dielectric material is etched using dry etching technology, and an inductively coupled plasma (ICP) etcher and hydrogen fluoride (HF) are selected as etching gases for operation. The overall ambient temperature is maintained at 20° C. to 25° C. The inductively coupled plasma (ICP) etcher is started to generate plasma, and then hydrogen fluoride etching gas is input to ensure that the flow rate is 40 sccm to 50 sccm. The pressure of the reaction chamber is adjusted to 40 mTorr to 50 mTorr to maintain a stable etching atmosphere. At a discharge power of 200 W to 300 W and a discharge pressure of 13.56 MH At a frequency of 0.04 z, hydrogen fluoride reacts with the surface of the dielectric material to generate a compound to achieve etching, and after the etching is completed, cleaning is performed to remove the etching residue; the work function of the deposited tunneling metal gate (9) is 3.7 eV to 4.1 eV, and the work function of the auxiliary metal gate (10) is 4.2 eV to 4.5 eV. The reactive sputtering process is used to deposit the target material using a magnetron sputtering system. First, the target material is heated to 300° C. to 600° C. to increase the evaporation rate of the metal, and the temperature of the substrate is controlled at 100° C. to 300° C. to avoid thermal damage to the thin film on the substrate. The pressure of the sputtering chamber is set at 10 -6 Torr~10 -8 Torr, start the sputtering system, heat the target materials of the tunneling metal gate (9) and the auxiliary metal gate (10) and apply an electric field to sputter the target materials from the surface of the target gun onto the silicon substrate, set the sputtering power of the material of the tunneling metal gate (9) to 80W-200W, and the sputtering power of the material of the auxiliary metal gate (10) to 50W-150W, so as to form a desired metal film on the semiconductor surface, after the sputtering process is completed, release the vacuum chamber gas and remove the semiconductor substrate, and use characterization technology to evaluate the morphology, composition and bonding state of the metal film, the characterization technology includes SEM and XPS, to ensure the quality and stability of the gate electrode; The conductivity of the drain (6) and source (11) is 10 -3 S / m~10 -1 S / m, formed by chemical vapor deposition (CVD), first preheating the CVD reaction chamber to 500-700°C and controlling the pressure in the chamber at 10 -2 Torr~10 1 Torr, to promote subsequent deposition, dimethylsilane (SiH2(CH3)2) is introduced as a silicon source gas, and the flow rate is set to 50sccm~100sccm, hydrogen (H2) is used as a diluent gas, and the flow rate is set to 200sccm~500sccm, the silicon source gas is decomposed in the reaction chamber and an electrode film is deposited on the surface of the substrate, and then the deposited electrode film is annealed to improve its crystallinity and electrical properties, the thermal annealing temperature is 500℃~1000℃, and the thermal annealing time is controlled at 20 minutes to 40 minutes.
Citation Information
Cited By
Biosensor based on graphene bi-material grid tunneling field effect transistor
CN119894042A