Method for testing package substrate and equipment for testing package substrate
Through electron beam testing, the packaging substrate is tested for non-contact testing, which solves the rapid reliability problem of packaging substrate testing in complex microelectronic devices, and effectively detects the path of miniaturized and high-density electrical interconnects, avoids contact damage , suitable for mass production.
Patent Information
- Application Number
- CN202280095571.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2022-05-10
- Publication Date
- 2024-11-26
AI Technical Summary
The prior art is difficult to quickly and reliably test package substrates in complex microelectronic devices, especially panel-level package substrates and advanced package substrates, especially in miniaturization and high density conditions, where traditional contact testing methods have contact damage and mechanical spacing. Problem of limitations.
Using electron beam testing method, the surface contact points of the package substrate are tested by using electron beam columns in a vacuum chamber, and signal detection is performed using electron beams of different beam diameters and impact angles to identify and characterize electrical interconnects. Defects in the path, such as short circuit, open circuit, and leakage.
It realizes fast and reliable non-contact testing of the package substrate of complex microelectronic devices, avoids contact damage, is suitable for miniaturized and high-density electrical interconnect paths, improves test speed and accuracy, and is suitable for mass production.
Smart Images

Figure CN119032281A_ABST
Abstract
Description
Technical Field
[0001] The present disclosure relates to a method and apparatus for testing a packaging substrate. More specifically, embodiments described herein relate to non-contact testing of electrical interconnects in a packaging substrate (i.e., a panel-level packaging (PLP) substrate or an advanced packaging (AP) substrate) by using an electron beam, particularly for identifying and characterizing defects such as shorts, opens, and / or leakages. In particular, embodiments of the present disclosure relate to a method for testing a packaging substrate, which is a panel-level packaging substrate or an advanced packaging substrate, to an apparatus for testing a packaging substrate according to the method described herein, and to an apparatus for non-contact testing of a packaging substrate. Background Art
[0002] In many applications, substrates need to be inspected to monitor the quality of the substrate. Since defects may for example appear during processing of the substrate, such as during structuring or coating of the substrate, inspecting the substrate to detect defects and monitor quality may be beneficial.
[0003] Semiconductor packaging substrates and printed circuit boards used to manufacture complex microelectronic and / or micromechanical components are often tested during and / or after manufacturing to determine defects, such as shorts or opens, in the metal paths and interconnections provided at the substrate. For example, a substrate used to manufacture a complex microelectronic device may include multiple interconnect paths for connecting semiconductor chips or other electronic devices to be mounted on the packaging substrate.
[0004] Various methods for testing such components are known. For example, the contact pads of the component to be tested can be contacted with a contact probe to determine whether the component is defective. As the miniaturization of components progresses, the components and contact pads become smaller and smaller, making it difficult for the contact probe to contact the contact pads, and it may even damage the device under test during the test.
[0005] The complexity of package substrates is increasing, while design rules (feature size) are decreasing significantly. Within such substrates, surface contacts (for later flip-chip or other chip mounting) connect to other surface contacts on the package substrate to interconnect semiconductor (or other) devices. Standard methods such as electromechanical probing for electrical testing cannot meet the requirements of mass production test due to decreased throughput (higher number of test points) and decreased contact reliability (smaller contact size). In addition to the issues of reduced size and possible damage to contact pads, the topography of package substrates causes difficulties for other test methods, such as those using capacitive detectors or electric field detectors, because these methods advantageously have small mechanical spacing.
[0006] Therefore, it would be beneficial to provide a testing method and a testing apparatus suitable for reliably and quickly testing complex microelectronic devices, in particular packaging substrates such as AP substrates and PLP substrates. Summary of the invention
[0007] In view of this, according to the independent claims, a packaging substrate testing method and apparatus are provided. Further aspects, advantages, and features are apparent from the dependent claims, the description, and the accompanying drawings.
[0008] According to one embodiment, a method for testing a package substrate using at least one electron beam column is provided. The package substrate is a panel-level package substrate or an advanced package substrate. The method comprises: placing the package substrate on a platform in a vacuum chamber; placing at least one electron beam column having a landing energy U pe , a first beam diameter BD1 and a first impact angle θ1 to one or more first surface contacts on a package substrate; an electron beam having at least one of a second beam diameter BD2 and a second impact angle θ2 is directed to one or more second surface contacts different from the one or more first surface contacts, wherein at least one of the following applies: i) the first impact angle θ1 is different from the second impact angle θ2, and ii) the second beam diameter BD2 is different from the first beam diameter BD1. Furthermore, the method includes detecting signal electrons emitted upon impact of the electron beam to test at least a first device-to-device electrical interconnect path of the package substrate.
[0009] According to one embodiment, a device for testing a package substrate is provided, wherein the device is configured to perform a test according to a test method according to any specific embodiment of the present disclosure.
[0010] According to one embodiment, a device for contactlessly testing a packaging substrate is provided. The device includes a vacuum chamber; a platform located in the vacuum chamber, the platform being configured to support a packaging substrate, the packaging substrate being a panel-level packaging substrate or an advanced packaging substrate; and a charged particle beam column, the charged particle beam column being configured to generate an electron beam. The device (specifically, an electron beam column) includes an objective lens configured to focus the electron beam on the packaging substrate and a scanning deflector configured to scan the electron beam to different positions on the packaging substrate. In addition, the device includes an electron detector for detecting signal electrons emitted when the electron beam hits the packaging substrate; one or more power supplies provide a landing energy U of the electron beam. peThe apparatus further includes a controller configured to control the scanning deflector and the objective lens to: a) direct the electron beam onto one or more first surface contact points on the package substrate at a first beam diameter and a first impact angle θ1, and b) direct the electron beam onto one or more second surface contact points different from the one or more first surface contact points at at least one of a second beam diameter and a second impact angle θ2. At least one of the following applies: i) the first impact angle θ1 is different from the second impact angle θ2, and ii) the second beam diameter BD2 is different from the first beam diameter BD1.
[0011] Specific embodiments also relate to apparatus for practicing the disclosed methods, and include apparatus components for performing each described method aspect. Method aspects may be performed by hardware components, by a computer programmed by appropriate software, by any combination of the two, or in any other manner. In addition, embodiments according to the present disclosure also relate to methods for operating the described apparatus and methods for manufacturing the apparatus and devices described herein. Methods for operating the described apparatus include method aspects for performing each function of the apparatus. BRIEF DESCRIPTION OF THE DRAWINGS
[0012] In order to be able to understand in detail the manner in which the above features of the present disclosure are achieved, reference may be made to the embodiments for a more detailed description of the present disclosure briefly summarized above. The accompanying drawings are related to the embodiments and are described as follows:
[0013] FIG. 1 illustrates a schematic cross-sectional view of an apparatus for testing a package substrate according to any of the testing methods described herein;
[0014] 2A and 2B show enlarged cross-sectional views of a package substrate during any of the testing methods described herein;
[0015] FIG3 illustrates an enlarged top view of a package substrate during any of the testing methods described herein;
[0016] 4A-4D illustrate enlarged cross-sectional views of a package substrate that may be tested according to the methods described herein;
[0017] FIG5 illustrates a graph of total electron yield and sample charging as a function of primary beam energy (eg, landing energy of the electron beam on the packaging substrate) for different impact angles θ;
[0018] FIG6A illustrates an electron beam directed to a surface contact point at an impact angle θ of θ=0°, resulting in negative charging;
[0019] FIG6B illustrates an electron beam directed to a surface contact point at an impact angle θ of θ>0°, specifically 80°≤θ≤90°, resulting in positive charging;
[0020] FIG6C illustrates an example of an electron beam directed to a surface contact point, the electron beam diameter substantially corresponding to the diameter of the surface contact point, resulting in positive charging;
[0021] 7A and 7B illustrate images and illustrate portions of a package substrate according to the testing methods described herein;
[0022] 8A and 8B illustrate images and portions of a package substrate according to the testing methods described herein;
[0023] 9 illustrates a schematic side view of surface contacts on a packaging substrate according to embodiments described herein;
[0024] FIG. 10 illustrates a schematic top view of surface contacts on a packaging substrate according to embodiments described herein; and
[0025] 11 and 12 show flow charts of methods of testing a package substrate according to embodiments described herein. DETAILED DESCRIPTION
[0026] Reference will now be made in detail to various exemplary embodiments, one or more examples of which are illustrated in the various figures. Each example is provided for the purpose of explanation and is not intended to be limiting. For example, features illustrated or described as part of one embodiment may be used on other embodiments or used in conjunction with other embodiments to produce yet another embodiment. The present disclosure is intended to include such modifications and variations.
[0027] In the following description of the drawings, the same reference numerals represent the same components. Only the differences with respect to individual embodiments are described. The structures shown in the figures are not necessarily drawn to scale, but are provided for a better understanding of the embodiments.
[0028] Over the years, the complexity of packaging substrates has been increasing in order to reduce the space requirements of semiconductor packaging. In order to reduce manufacturing costs, packaging technologies such as 2.5D IC, 3D-IC and wafer-level packaging (WLP), such as fan-out WLP, have been proposed. In WLP technology, integrated circuits are packaged before being cut. As used herein, "packaging substrate" and packaging substrates configured for advanced packaging technology, in particular WLP technology or panel-level packaging (PLP) technology.
[0029] "2.5D integrated circuits" (2.5D ICs) and "3D integrated circuits" (3D ICs) combine multiple dies in a single integrated package. Here, two or more dies are placed on a packaging substrate, such as a silicon interposer or a panel-level packaging substrate. In a 2.5D IC, the dies are placed side by side on the packaging substrate, while in a 3D IC, at least some of the dies are stacked on top of each other. Components can be packaged as a single part, which reduces cost and size compared to traditional 2D circuit board assemblies.
[0030] The package substrate typically includes a plurality of inter-device electrical interconnect paths for providing electrical connections between chips or dies to be placed on the package substrate. The inter-device electrical interconnect paths may extend vertically (perpendicular to the surface of the package substrate) and / or horizontally (parallel to the surface of the package substrate) through the body of the package substrate in a complex network of connections, with their endpoints (referred to herein as surface contacts) exposed at the surface of the package substrate.
[0031] Advanced packaging (AP) substrates provide inter-device electrical interconnect paths on or within a wafer (e.g., a silicon wafer). For example, an AP substrate may include through silicon vias (TSVs) (e.g., provided in a silicon interposer), other conductive lines extending through the AP substrate. Panel-level packaging substrates are provided by composite materials, such as printed circuit board (PCB) material or another composite material, including, for example, ceramic and glass materials.
[0032] Panel-level packaging substrates are manufactured that are configured to integrate multiple devices (e.g., chips / die that may be heterogeneous (e.g., may have different sizes and configurations)) in a single integrated package. In addition, AP substrates may be combined on PLP substrates. Panel-level substrates typically provide locations for multiple chips, dies, or AP substrates to be placed on its surface, such as on one side or on both sides, and multiple inter-device electrical interconnect paths extending through the body of the PLP substrate.
[0033] It is worth noting that the size of the panel-level substrate is not limited to the size of the wafer. For example, the panel-level substrate can be rectangular or have other shapes. Specifically, the panel-level substrate can provide a larger surface area than the surface area of a typical wafer, such as 1000 cm 2 For example, the panel-level substrate may have a size of 30 cm x 30 cm or more, 60 cm x 30 cm or more, 60 cm x 60 cm or more.
[0034] The present disclosure relates to methods and apparatus for testing package substrates that are configured to integrate multiple devices in an integrated package and include at least one inter-device electrical interconnect path. It should be understood that the methods and apparatus described herein that employ the principle of controlling charge by morphology can be used for all SEM-related applications with electronic components and morphology. According to an embodiment of the present disclosure, a test system, a test device, or a test method can detect and / or classify defective electrical connections in a package substrate, such as open circuits, short circuits, leakage defects, or other. In particular, a test method and a test system can provide non-contact testing. Contact pad spacings of 60µm or less, or even about 10µm or less, are difficult or even impossible for mechanical probing. In addition, small contact pads must not be damaged by any scratches. Non-contact testing is beneficial.
[0035] According to specific embodiments of the present disclosure, electron beam testing and / or electron beam inspection provides testing of contact pads of 60 μm or less, or even about 10 μm or less. Voltage contrast test imaging may be provided. Testing may be provided at or between "surface contacts" of a package substrate.
[0036] A "surface contact point" can be understood as an endpoint of an electrical interconnect path exposed on the surface of a package substrate, such that an electron beam can be directed to the surface contact point for contactless charging or probing of the electrical interconnect path. A "surface contact point" can be an intermediate contact point in a complex network. In addition, a "surface contact point" can be on the top side of the substrate or on the bottom side of the substrate. For example, a "surface contact point" can be set at the V pin for powering the device. DD Line or V SS Connect to V DD Line or V SS Line. V SS Represents the voltage applied to the source of the transistor. V DD Represents the voltage applied to the drain of the transistor. The surface contact point is configured to electrically contact a chip, die, smaller package, or other electrical component such as a capacitor, resistor, coil, etc., to be placed on the surface of the package substrate, such as by soldering. These electrical components may also include active electrical components, such as a transformer that changes the voltage in the package area. In some embodiments, the surface contact point may be or may include a solder bump.
[0037] According to an embodiment of the present disclosure, 100% of the electrical interconnect paths are tested. The cost of ownership of device packages such as processor, memory, etc. (microelectronic device) chips is mainly determined by the high integration of microelectronic devices. Therefore, it is disadvantageous in terms of manufacturing cost to mount a defective microelectronic device to a defective packaging substrate. A completely defect-free packaging substrate is required before mounting the microelectronic device.
[0038] According to one embodiment, a method for testing a package substrate is provided, wherein the package substrate is a panel-level package substrate or an advanced package substrate. The package substrate is tested using at least one electron beam column. The method includes placing the package substrate on a platform in a vacuum chamber. In addition, the method includes placing at least one electron beam column having a landing energy U pe , a first beam diameter BD1 and a first impact angle θ1 are directed to one or more first surface contact points on the packaging substrate. In addition, the method includes directing an electron beam having at least one of a second beam diameter BD2 and a second impact angle θ2 to one or more second surface contact points different from the one or more first surface contact points. When performing the method, at least one of the following situations applies: i) the first impact angle θ1 is different from the second impact angle θ2, and ii) the second beam diameter BD2 is different from the first beam diameter BD1. In addition, the method includes detecting signal electrons emitted when the electron beam impacts, for testing at least a first inter-device electrical interconnect path of the packaging substrate.
[0039] According to an embodiment of the present disclosure, testing of features of a packaging substrate (e.g., electrical interconnect paths) can be provided, wherein charging of the features and / or the packaging substrate can be controlled. The charge on the packaging substrate or a corresponding portion thereof (specifically, the surface contact points) can be controlled by a change in at least one of the impact angle θ of the electron beam on the surface contact points and the beam diameter. Thus, non-contact electrical testing using an electron beam can be provided. The test can include a voltage signal reading, i.e., a voltage comparison measurement when a signal electron (e.g., a secondary electron) is detected. The test locations (i.e., surface contact points) of an advanced packaging substrate or a panel-level packaging substrate can be charged without contact to avoid damage to the surface contact points.
[0040] 1 illustrates in schematic cross-sectional view an apparatus 100 for testing a package substrate 10 according to an embodiment described herein. The apparatus 100 includes a vacuum chamber 110, which may be a test chamber specifically configured for testing or may be one vacuum chamber of a larger vacuum system, such as a processing chamber of a package substrate manufacturing or processing system.
[0041] As shown in FIG. 1 , the package substrate 10 includes a first inter-device electrical interconnection path 20 extending between a first surface contact point 21 and a second surface contact point 22 of the package substrate 10. Optionally, the first inter-device electrical interconnection path 20 may extend between three or more surface contact points, which may be disposed on the same surface or on two opposite surfaces of the package substrate. The inter-device electrical interconnection path 20 depicted in FIG. 1 extends only between the first surface contact point 21 and the second surface contact point 22 disposed on the top surface of the package substrate, but the present invention is not limited to such an inter-device electrical interconnection path, and the inter-device electrical interconnection path may be a complex network of through holes, pillars and / or wires extending through the package substrate and having multiple surface contact points.
[0042] The package substrate 10 may include a plurality of inter-device electrical interconnection paths 20 for connecting a plurality of devices to be placed on the package substrate 10. In FIG. 1 , three inter-device electrical interconnection paths are exemplarily depicted, but if there is no short circuit between two electrical interconnection paths, the package substrate 10 may include thousands or tens of thousands of such inter-device electrical interconnection paths that are generally electrically isolated from each other.
[0043] According to a specific embodiment described herein, the packaging substrate 10 is placed on a platform 105 in a vacuum chamber 110. The platform can be movable, in particular in the z direction (i.e., in a direction perpendicular to the platform surface) and / or in the x direction and the y direction (i.e., in the plane of the platform surface). The platform 105 is disposed in the vacuum chamber and is configured to support the packaging substrate, which is one of a panel-level packaging substrate and an advanced packaging substrate. An electron beam 111 is directed to a first surface contact point 21. The electron beam can be scanned to be directed to a second surface contact point 22. Signal electrons 113 emitted from the second surface contact point 22 are detected to test the first device-to-device electrical interconnect path 20. The signal electrons can be secondary electrons and / or backscattered electrons. For example, it can be determined whether the first device-to-device electrical interconnect path 20 has an "open circuit" defect.
[0044] Alternatively or additionally, the electron beam 111 is directed to another surface contact point 27, which is not an endpoint of the first inter-device electrical interconnection path 20, that is, belongs to the second inter-device electrical interconnection path 23, which can extend through the packaging substrate and is adjacent to the first inter-device electrical interconnection path 20. Signal electrons emitted from the other surface contact point 27 are detected to test the first inter-device electrical interconnection path 20. The signal electrons can be secondary electrons and / or backscattered electrons. For example, it can be determined whether the first inter-device electrical interconnection path 20 has a "short circuit" defect.
[0045] In particular, by detecting the signal electrons 113 emitted when the electron beam 111 strikes the package substrate (in particular, by determining the energy of the signal electrons 113 depending on the potential of the second surface contact point 22 or the other surface contact point 27), it is possible to determine in a "voltage comparison measurement" whether the first inter-device electrical interconnect path 20 is defective. In particular, defective connections in the package substrate, such as open circuits, short circuits, and / or leakage defects, can be determined and classified.
[0046] In some embodiments that may be combined with other embodiments described herein, one or more electrical connections extending between surface contacts on different sides of a substrate are inspected. In still other embodiments, a first plurality of electrical connections extending between surface contacts on a first side of a substrate, a second plurality of electrical connections extending between surface contacts on a second side of a substrate, and / or a third plurality of electrical connections extending between surface contacts on different sides of a substrate are inspected. For example, one or more electron beam columns (not shown) may be provided on both sides of a substrate so that surface contacts on both sides of the substrate may be charged and / or discharged to inspect and test the respective electrical connections.
[0047] According to the embodiments described herein, both charging and probing are provided with an electron beam, in particular a scanning electron beam. Other test methods such as electrical and / or mechanical probing cannot provide the throughput provided by the methods and systems described herein. The methods and systems described herein rely on non-contact charging and electron beam probing. In addition, the contact reliability of electrical and / or mechanical testers decreases as the size of the surface contact points to be tested in the advanced packaging substrate decreases and the density and number increase. For example, contact pad sizes of 30 μm or less are difficult to perform mechanical probing. In addition, the topography of the packaging substrate and the topography of the surface contact points of the packaging substrate may cause problems for other test methods, such as capacitive detectors or electric field detectors. It is more advantageous to have a charging electron beam, for example, compared to flood-type electron gun charging. In view of the complexity of the packaging substrate, the ability to charge locally improves the available test procedures compared to charging the entire area using a flood-type electron gun. In addition, local charging reduces the total charge accumulated on the packaging substrate. Further, different charges in different regions can result in a reduction in the total charge provided on the substrate. For example, if one region is positively charged and another region is negatively charged, the total charge can be kept close to neutral. According to some embodiments, which can be combined with other embodiments described herein, patterns of different charges may be provided on portions of the packaging substrate.
[0048] The test method described herein is applicable to the testing of package substrates integrated within a multi-device package, and is particularly applicable to the testing of panel-level package substrates (PLP substrates) or advanced package substrates (AP substrates), and uses an electron beam for both charging the inter-device electrical interconnect path 20 and for reading the charged circuit voltage, specifically by probing the second surface contact point and / or the additional surface contact point. In other words, both "electrical driving" and "probing" are accomplished with an electron beam, so that defects can be found reliably and quickly. Testing by electron beam charging and electron beam probing (e.g., using an EBT column or an EBR column) is independent of topography, fast, and flexible in terms of contact point location, size, and geometry, while the topography of the package substrate may be a problem for other test methods such as capacitors or electric field detectors.
[0049] A packaging substrate such as a PLP substrate may include a plurality of inter-device connections, such as 5,000 or more, 10,000 or more, 20,000 or more, or even 50,000 or more. The connections may include through silicon vias (TSVs), for example, provided in a silicon interposer, other conductors extending through the packaging substrate, and / or may include multi-die interconnect bridges that may be embedded in the packaging substrate. The packaging substrate may be a multi-layer substrate that includes electrical interconnects arranged in multiple layers on top of each other, such as in the form of a layer stack.
[0050] In some specific embodiments, the packaging substrate 10 includes a plurality of inter-device electrical interconnect paths extending between corresponding first and second surface contact points and optional additional contact points, and the method may include testing the plurality of inter-device electrical interconnect paths sequentially or in parallel. The "sequential testing" described herein refers to the sequential testing of a plurality of inter-device electrical interconnect paths of the packaging substrate. For example, 5,000 or more inter-device electrical interconnect paths are tested one after another. The "parallel testing" described herein may refer to the synchronous testing of two or more inter-device electrical interconnect paths. The "parallel testing" described herein may also refer to testing a plurality of inter-device electrical interconnect paths by scanning an electron beam in a field of view to charge a plurality of first surface contact points, while scanning an electron beam in a field of view to detect a plurality of corresponding second surface contact points.
[0051] While conventional PCBs typically include relatively large flat metal pads that form surface contacts for testing, the package substrates tested according to the embodiments described herein may include a large number of small, convex solder bumps to be tested, which makes testing more challenging. In particular, the first surface contact point 21 and the second surface contact point 22 may each have a maximum dimension of 25 μm or less, in particular 10 μm or less. For example, the first and second surface contact points may be substantially circular, in particular hemispherical, having a diameter of 25 μm or less, in particular 10 μm or less. According to some embodiments that may be combined with other embodiments described herein, the surface contact point may have a three-dimensional topography, in particular a substantially hemispherical shape.
[0052] Compared to mechanical testers, the electron beam can be precisely directed to such a small surface area because the electron beam can be focused to a very small probing diameter and can be precisely directed to a predetermined point on the substrate, for example using a scanning deflector, with an accuracy in the sub-micrometer range. While other testers may slip or slide from a surface contact point with convex geometries, the electron beam can be accurately focused onto arbitrary geometries.
[0053] As shown in FIG1 , a charged particle beam column 120 can be disposed on a first side of the platform 105. In some embodiments that can be combined with other embodiments described herein, the charged particle beam column 120 can have an electron source 121 for generating an electron beam, and beam optical elements, such as a scanning deflector 122 and / or an objective lens 124, for directing the first electron beam onto a substrate placed on the platform 105. The objective lens 124 can be an electrostatic objective lens (as shown in FIG1 ), a magnetic objective lens, or a magneto-electrostatic objective lens.
[0054] The device 100 further includes an electron detector 140 for detecting the signal electrons 113 emitted when the second electron beam strikes the packaging substrate, and an analysis unit 141 configured to determine whether the first device-to-device electrical interconnect path 20 is defective based on the signal electrons 113. In some embodiments, the analysis unit 141 can be configured to determine whether the electrical interconnect path has a defect, such as a short circuit, an open circuit, and / or a leakage, based on the detected signal electrons. Optionally, the analysis unit 141 can be configured to classify any detected defects. In some embodiments, the analysis unit 141 can be configured to determine whether there is a short circuit or leakage between two or more electrical interconnect paths based on the signal electrons detected from subsequent measurements. In some embodiments, the signal electrons 113 detected by the electron detector 140 can provide information about the potential of the substrate location where the signal electrons 113 are emitted or reflected, and the analysis unit 141 can be configured to determine whether the first device-to-device electrical interconnect path 20 is defective based on the information. The analysis unit 141 can be further configured to classify the determined defects. Specifically, the test may include determining by the analysis unit 141 whether the first inter-device electrical interconnection path 20 has any of a short circuit, an open circuit, and / or leakage. An "open circuit" is understood as an open electrical interconnection path that does not actually electrically connect the first surface contact point 21 and the second surface contact point 22. A "short circuit" is understood as an electrical connection between two electrical interconnection paths that are actually electrically separated.
[0055] In some embodiments that may be combined with other embodiments described herein, the electron detector 140 includes an Everhard-Thornley detector. An energy filter 142 for the signal electrons 113 may be arranged in front of the electron detector 140, specifically in front of the Everhard-Thornley detector, as schematically depicted in FIG. 1 . The energy filter may include a grid electrode configured to be set at a predetermined potential. The energy filter 142 may allow low-energy signal electrons to be suppressed. The energy filter 142 may suppress signal electrons that are not related to the voltage contrast measurement to be performed. In some embodiments, the energy filter 142 may suppress signal electrons emitted from uncharged surface areas and may only allow signal electrons emitted from charged surface contacts to pass. Therefore, the signal current detected by the electron detector may depend on the energy of the signal electrons, which indicates whether the detected surface contact point is defective.
[0056] In some embodiments, the device 100 may include a scanning controller 123 connected to a scanning deflector 122 of the charged particle beam column 120. The scanning deflector 122 may be configured to scan the electron beam on the substrate surface. The electron beam may be directed to a portion of the packaging substrate (e.g., with a first beam detection diameter). The portion of the packaging substrate may be an area of the packaging substrate where the electron beam scans the area of the packaging substrate. The electron beam may be raster scanned on a portion of the packaging substrate. For example, one or more scanning deflectors 122 may scan the electron beam on a portion of the packaging substrate. The portion of the packaging substrate may also be a surface contact point. The electron beam may be vector scanned to one or more surface contact points of the packaging substrate. For example, one or more scanning deflectors may be used to vector scan the electron beam to one or more surface contact points.
[0057] For example, the scanning controller 123 can be configured to control the scanning deflector so that the electron beam is sequentially directed to the paired first and second surface contacts for testing the corresponding inter-device electrical interconnect paths extending between the corresponding first and second surface contact pairs. This allows for rapid and reliable testing of multiple electrical interconnect paths extending through the package substrate.
[0058] According to some embodiments that may be combined with other embodiments described herein, the electron beam may be vector scanned to separate locations, such as surface contact points of a packaging substrate, for charging, and may be vector scanned to separate locations for detecting signal electrons. Alternatively, the electron beam may be vector scanned to various locations, such as surface contact points of a packaging substrate, for charging, and may be raster scanned over an area of the packaging substrate for detecting signal electrons. According to some embodiments that may be combined with other embodiments described herein, the electron beam of a charged particle beam column may be scanned to one or more locations on a packaging substrate for charging and for detection of signal electrons.
[0059] As shown in FIG1 , the electron source 121 is connected to a power supply 130. The power supply can provide a high voltage to the electron source to emit an electron beam, i.e., a primary electron beam, from the electron source. According to some embodiments that can be combined with other embodiments described herein, the voltage provided by the power supply 130 can be changed to change the energy of the electron beam, thereby changing the landing energy U of the electron beam on the packaging substrate. pe In general, in order to perform the method of testing the package substrate, a suitable working point is first selected. The working point includes the landing energy U pe , working parameters such as the working distance between the detection and the packaging substrate, the detection size, and the electron beam current.
[0060] According to some embodiments that can be combined with other embodiments described herein, one or more power supplies can be connected to various components of the electron beam column. For example, the power supply can be connected to the electron source (as shown in FIG. 1 ), the extractor of the electron source, the anode of the electron source, the deceleration electrode configured to decelerate the electrons before striking the package substrate, and / or the platform 105. The landing energy of the electron beam on the package substrate is determined by the potential difference between the potential of the emitter tip of the electron source and the potential of the package substrate or the potential of the platform 105, respectively. Therefore, one or more power supplies can be provided to change the landing energy of the electron beam.
[0061] With reference to FIG. 1 , in accordance with an embodiment that may be combined with other embodiments described herein, the device 100 includes a controller 180 configured to control a scanning deflector 122 and an objective lens 124. Thus, the controller 180 may be connected to the scanning deflector 122 and the objective lens 124, for example, via a physical connection or a wireless connection. Specifically, the controller is configured to control the scanning deflector 122 and the objective lens 124 for: a) directing an electron beam having a first beam diameter and a first impact angle θ1 to one or more first surface contact points on a packaging substrate, (b) directing an electron beam (111) to one or more second surface contact points different from the one or more first surface contact points with at least one of a second beam diameter and a second impact angle θ2, wherein at least one of the following applies: i) the first impact angle θ1 is different from the second impact angle θ2, and ii) the second beam diameter is different from the first beam diameter.
[0062] Furthermore, according to some embodiments, which can be combined with other embodiments described herein, the controller can be connected to the power supply 130, the scanning controller 123, the analysis unit 141, and the platform 105. The controller can also be connected to the detector 140. Furthermore, the controller can be connected to the objective lens 124, for example, to control and / or adjust the focus of the objective lens.
[0063] Controller 180 includes a central processing unit (CPU), a memory, and, for example, a support circuit. To facilitate control of the equipment for testing the package substrate, the CPU may be one of any form of general-purpose computer processor that can be used in an industrial environment to control various chambers and subprocessors. Memory 112 is coupled to CPU 114. The memory or computer-readable medium may be one or more easily accessible memories, such as random access memory, read-only memory, hard disk, or any other form of digital storage device located locally or remotely. Support circuits may be coupled to the CPU to support the processor in a conventional manner. These circuits include caches, power supplies, clock circuits, input and output systems, and related subsystems, etc. Inspection processing instructions are typically stored in the memory as software routines commonly referred to as recipes. The software routines may also be stored and / or executed by a second CPU (not shown) located at a remote end of the hardware controlled by the CPU. When the software program is executed by the CPU, the general-purpose computer is converted into a special-purpose computer (controller) to control the operation of equipment such as landing energy control, platform positioning, and charged particle beam scanning in test operations. Although the methods and / or processes of the present disclosure are discussed as being implemented as software routines, some of the method steps disclosed therein may be performed in hardware and by a software controller. Thus, embodiments of the present invention may be implemented in software executed on a computer system, as well as in hardware implemented as an application specific integrated circuit or other type of hardware, or a combination of software and hardware.
[0064] According to one embodiment, an apparatus for testing a package substrate using any of the methods described herein is provided. The apparatus may include a controller 180. According to any of the embodiments described herein, the controller may perform a method for testing a package substrate. The controller includes a processor and a memory storing instructions that, when executed by the processor, cause the apparatus to perform a method according to an embodiment of the present disclosure.
[0065] 2A and 2B illustrate enlarged cross-sectional views of a package substrate during the test method described herein. The package substrate 10 may be an AP substrate or a PLP substrate for manufacturing a multi-die integrated package and includes a first die connection interface for attaching a first die 201 and a second die connection interface for attaching a second die 202. A plurality of inter-device electrical interconnect paths (four of which are exemplarily illustrated in FIGS. 2A and 2B) extend between corresponding first surface contacts of the first die connection interface and corresponding second surface contacts of the second die connection interface. The surface contacts may be formed as or include solder bumps having a three-dimensional geometry (e.g., substantially hemispherical).
[0066] In FIG. 2A , a first inter-device electrical interconnect path 20 extending between a first surface contact 21 and a second surface contact 22 is tested by directing a charging electron beam 111 onto the first surface contact 21 and directing the electron beam onto the second surface contact 22. Since the first surface contact 21 is electrically connected to the second surface contact 22 via the first inter-device electrical interconnect path 20, the second surface contact 22 should be at the same potential as the first surface contact 21 after the first surface contact 21 is charged. Signal electrons 113 emitted from the second surface contact 22 are detected, and the signal electrons 113 carry information about the potential of the second surface contact 22, which should be equal to the potential of the first surface contact 21. If it is determined that the potential of the second surface contact 22 is different from the potential of the first surface contact 21, a defect is detected. The detected voltage contrast can be used to characterize the defect. In addition, the detected voltage contrast of subsequent measurements of adjacent electrical interconnect paths can be compared to find short circuits or leakage between different electrical interconnect paths.
[0067] After the test of the first inter-device electrical interconnection path 20, the electron beam 111 can be directed to two surface contact points of the second inter-device electrical interconnection path 23, for example by scanning the electron beam (vector scanning) to other positions by a corresponding scanning deflector and / or by moving the platform supporting the package substrate. Subsequently, multiple inter-device electrical interconnection paths can be tested with the charging electron beam and the detection electron beam. Therefore, multiple test points can be tested sequentially and / or in parallel.
[0068] 2B, an open circuit 151 exists in the first inter-device electrical interconnect path 20. The open circuit 151 is determined because after or during the charging of the first surface contact 21 by the charging electron beam 111, the second surface contact 22 is not charged.
[0069] 2B , there is a short circuit 152 between the second inter-device electrical interconnect path 23 and the third inter-device electrical interconnect path 24. The short circuit can be determined because the third inter-device electrical interconnect path 24 is charged together with the second inter-device electrical interconnect path 23, which can be detected by a probing electron beam directed to a point 27 of the third inter-device electrical interconnect path 24 after or during the charging of the second inter-device electrical interconnect path 23.
[0070] For evaluation and defect classification, measured signals of adjacent interconnect paths and / or previously collected data can be compared, allowing the identification of opens, shorts, and leakages in the package substrate.
[0071] 3 is a schematic top view of a package substrate 10 under test as described herein. The top surface of the package substrate has a plurality of surface contact points arranged in a two-dimensional pattern. The package substrate 10 includes a first die connection interface 31 for attaching a first die (specifically by flip chip mounting), a second die connection interface 32 for attaching a second die (specifically by mounting), and optional additional die connection interfaces, which can be arranged adjacent to each other in pairs. The first die connection interface 31 can include a plurality of first surface contact points, for example, formed as solder bumps, and the second die connection interface 32 can include a plurality of second surface contact points, for example, formed as solder bumps.
[0072] In some specific embodiments, each first surface contact point of the first die connection interface 31 is connected to a corresponding second surface contact point of the second die connection interface 32 via an inter-device electrical interconnection path. For the sake of clarity, only the inter-device electrical interconnection paths connecting the first and second die connection interfaces are depicted. According to some embodiments that can be combined with other embodiments described herein, the first surface contact point can be connected to a second surface contact point. Alternatively, the first surface contact point can be connected to two or more second surface contact points. Two or more second surface contact points can be detected with an electron beam, for example, after a charge has been applied to the first surface contact point.
[0073] According to the test method described herein, the charged electron beam 111 is directed (specifically focused) on the first surface contact point of the first die connection interface 31, and the charged electron beam 111 is directed (specifically focused) on the associated second surface contact point of the second die connection interface 32. The signal electrons emitted from the second surface contact point are detected to test whether there is an "open circuit" defect in the electrical interconnect path connecting the first and second surface contact points. Thereafter, the other surface contact points of the first and second die connection interfaces can be tested, specifically in pairs.
[0074] Alternatively or additionally, it may be possible to test in parallel or sequentially whether charging of one inter-device electrical interconnect path causes charging of a surface contact point of another inter-device electrical interconnect path, such that a "short" defect may be determined. For example, an electron beam may be raster scanned over a portion of a packaging substrate to generate an image of the portion of the packaging substrate. The image may be evaluated, for example, by pattern recognition.
[0075] 4A-4D illustrate enlarged cross-sectional views of a package substrate that may be tested according to the methods described herein.
[0076] The package substrate 10 shown in Fig. 4A has surface contacts on two main surfaces of the package substrate. For example, a first plurality of inter-device electrical interconnection paths may extend between first and second surface contacts exposed on the upper substrate surface, and a second plurality of inter-device electrical interconnection paths may extend between first and second surface contacts exposed on the lower substrate surface.
[0077] At least one inter-device electrical interconnect path in the package substrate 10 shown in FIG. 4B extends between at least three surface contact points 25 , ie, a first surface contact point, a second surface contact point, and at least a third surface contact point.
[0078] At least one inter-device electrical interconnect path in the package substrate 10 shown in Fig. 4C extends between at least three surface contacts 25, which are exposed on different main surfaces of the substrate in a complex connection network. Such inter-device electrical interconnect paths can be configured to connect three or more dies to each other through the package substrate.
[0079] The package substrate 10 shown in FIG4D has at least one interconnection bridge 29 embedded in the package substrate 10. At least one inter-device electrical interconnection path extends through at least one interconnection bridge 29. Specifically, multiple inter-device electrical interconnection paths extending between the first die connection interface and the second die connection interface of the package substrate extend through the interconnection bridge. The interconnection bridge can be embedded in the package substrate during the manufacture of the package substrate. The interconnection bridge can be a bridge chip embedded in the package substrate for increasing the connection speed between multiple dies.
[0080] According to some embodiments that can be combined with other embodiments described herein, the test method and / or device according to the present disclosure can be used during and / or after the manufacture of the packaging substrate. For example, the test can be applied on a packaging substrate that does not yet include all layers or structures. For example, the test can be performed after the manufacture of the redistribution layer (RDL) and / or after the manufacture of the via layer. RDL testing and / or via testing can be provided. In addition, the completed packaging substrate can be tested.
[0081] 5 illustrates two graphs 500A and 500B illustrating the total electron yield as a function of the primary beam energy (i.e., the landing energy of the electron beam on the packaging substrate). Graph 500A shows the total electron yield as a function of the primary beam energy when the impact angle θ is θ=0°. Graph 500B shows the total electron yield as a function of the primary beam energy when the impact angle θ is θ>0° (e.g., θ=90°). As can be seen from FIG. 5, the number of electrons emitted from the surface of the packaging substrate per irradiated electron (i.e., the total electron yield) is energy-dependent. Line 501 corresponds to a total electron yield of 1. Therefore, the number of electrons reaching the surface of the packaging substrate is the same as the number of signal electrons emitted or scattered from the surface of the packaging substrate. For each of graphs 500A and 500B, there are two neutral energy values. For graph 500A, there is a first neutral energy value E whose total electron yield is equal to 1 (i.e., no charging) N1 and the second neutral energy value E N2 Accordingly, for graph 500B, there is a first neutral energy value E whose total electron yield is equal to 1 (ie, no charging). N1 ' and the second neutral energy value E N2 '. If the total electron yield σ is σ>1, positive charging occurs. A total electron yield greater than 1 is related to the fact that the number of electrons leaving the surface is greater than the number of electrons hitting the surface. Therefore, the packaging substrate or structure is positively charged. If the total electron yield σ is σ<1, negative charging occurs. A total electron yield less than 1 is related to the fact that the number of electrons leaving the surface is less than the number of electrons hitting the surface. Therefore, the packaging substrate or structure is negatively charged.
[0082] Furthermore, according to some embodiments, which can be combined with other embodiments described herein, the surface of the package substrate may be read using an electron beam having one of the neutral energy values, ie, signal electrons may be detected.
[0083] According to some embodiments, which can be combined with other embodiments described herein, the landing energy U pe Directing an electron beam having a first beam diameter BD1, a first beam diameter BD1, and a first impact angle θ1 to one or more first surface contact points on a package substrate can be a charging operation. The charging operation "writes" charge to an electrical interconnect path or a network of electrical interconnect paths. In addition, directing an electron beam having at least one of a second beam diameter BD2 and a second impact angle θ2 to one or more second surface contact points different from the one or more first surface contact points can be an operation of detecting signal electrons. The electron beam at the second landing energy can "read" the charge of an electrical interconnect path or a network of electrical interconnect paths.
[0084] According to some embodiments, which can be combined with other embodiments described herein, during detection of signal electrons (i.e., reading charge), charging of portions of a package substrate is reduced or avoided. In particular, when detecting signal electrons (e.g., when detecting previously provided charge), the influence of the charge of an electrical interconnect path or a network of electrical interconnect paths is avoided or minimized.
[0085] For example, a network of electrical interconnect paths may include 5 surface contact points (or any number greater than 2). Charge may be applied, i.e., "written", to a first surface contact point. The charge applied to the network of electrical interconnect paths may be "read" at a second surface contact point. It is beneficial to not change the charge of the network of electrical interconnect paths having 5 surface contact points when "reading" the charge on the second to fifth surface contact points. Thus, charge generation may be reduced or avoided while detecting signal electrons by using a neutral energy value for the landing energy.
[0086] The neutral energy value depends on the material. The material of the package substrate or the material of the surface of the package substrate is known, and the landing energy can be adapted to the package substrate material for the method of testing the package substrate. For a typical package substrate or a typical surface contact point on the package substrate, the first neutral energy value (e.g., E of graph 500A) is N1 and / or E of Chart 500B N1 ') can be several hundred eV. The second neutral energy value (e.g., E N2 and / or Chart 500B E N2 ') can be between 2keV and 5keV. Specifically, the second neutral energy value E of graph 500A N2 It can be between 2keV and 3keV. The second neutral energy value E of graph 500B N2 'Can be between 3.5keV and 5keV.
[0087] According to some embodiments that can be combined with other embodiments described herein, the landing energy U of the test method pe You can choose E N2 pe <E N2 ', as shown in Figure 5. Alternatively, the landing energy U of the test method pe You can choose E N1 ' pe <E N1 The landing energy can be adjusted depending on the test strategy, the material of the package substrate and / or the material of the surface contact point.
[0088] According to a specific embodiment of the present disclosure, a test structure (e.g., a region of a package substrate), in particular, a surface contact point, can be charged positively or negatively by electron beam impact. In particular, the total electron yield can be controlled according to the impact angle θ of the electron beam on the surface contact point.
[0089] The charging effect employed in the embodiments described herein is described with exemplary reference to Figures 6A to 6C. Figures 6A to 6C illustrate schematic side views of exemplary surface contacts onto which an electron beam 111 is directed, resulting in emission of signal electrons 113.
[0090] FIG. 6A illustrates the landing energy E N2 pe <E N2 ' and the impact angle θ is θ=0° to guide the electron beam 111 to the surface contact point. Therefore, as shown in the area 502 in FIG5 , the total electron yield is less than 1, thereby generating negative charges.
[0091] FIG. 6B illustrates the landing energy E N2 pe <E N2 ' and the impact angle θ is θ>0° (specifically 80°≤θ≤90°) to guide the electron beam 111 to the surface contact point. Therefore, as shown in area 503 in FIG. 5 , the total electron yield is greater than 1, thereby generating positive charges.
[0092] According to some embodiments, which can be combined with other embodiments described herein, the total electron yield can be controlled according to the beam diameter BD of the electron beam directed onto the surface of the contact point. N2 pe < E N2 ' and the beam diameter substantially corresponds to the diameter D of the surface contact point to guide the electron beam 111 to the surface contact point. As shown in Figure 6C, the total number of electrons leaving the substrate is greater than the total number of electrons introduced by the primary electron beam, resulting in a total electron yield greater than 1, thereby positive charging occurs.
[0093] It should be understood that the total electron yield can be controlled based on the primary energy level (i.e., the landing energy relative to the secondary electron yield). The test point potential can be determined. The voltage contrast principle can be used for defect detection. According to some embodiments that can be combined with other embodiments described herein, the landing energy can be set to a desired landing energy and positioned at one or more surface contacts as described herein or a test point on the packaging substrate. The electron beam remains on the corresponding surface contact point of the packaging substrate for a defined time to positively or negatively charge the portion of the packaging substrate relative to the environment of the portion of the packaging substrate. For example, the environment of the tested surface contact point can be one or more adjacent surface contacts.
[0094] According to some embodiments that can be combined with other embodiments described herein, one or more first surface contact points and / or one or more second surface contact points are positively charged during a first test sequence and negatively charged during a subsequent second test sequence. Positive or negative charges can be applied to different test sequences. In addition, changing from positively charged to negatively charged (or vice versa) reduces the total charge accumulated on the package substrate. The test accuracy can be improved by reducing the total charge accumulated on the package substrate. For example, the change from negative charge to positive charge can be made by increasing the impact angle θ, as exemplarily described with reference to FIG. 6B. Additionally or alternatively, the change from negative charge to positive charge can be made by increasing the beam diameter BD, as exemplarily described with reference to FIG. 6C.
[0095] Fig. 7A and Fig. 7B illustrate images of package substrates for illustrating the test method according to an embodiment of the present disclosure. The image 600 shown in Fig. 7A may relate to the first portion of the package substrate to which the electron beam of the charged particle beam column 120 is directed. According to some embodiments that may be combined with other embodiments described herein, the field of view and field size of the electron beam column of the method for testing the package substrate may be in the range of 25mm to 80mm. Therefore, the field of view may be advantageously selected to cover a panel on the package substrate without platform movement.
[0096] Image 600 shows a positively charged surface contact 602, and a surface contact 603. Surface contact 603 may be uncharged or may be negatively charged. Surface contact 603 is at a negative potential relative to surface contact 602. Electrons emitted from a more negative region are accelerated away from the packaging substrate, or experience less deceleration due to the positive charge on the packaging substrate. Therefore, electrons emitted from a more negative region have higher energy than electrons emitted from a less negative region or a positive region. In addition, the positive charge on the packaging substrate region may hinder electron emission. The total number of electrons in the positively charged region may be reduced.
[0097] According to some embodiments that can be combined with other embodiments described herein, the higher energy of electrons from a more strongly negatively charged area of the packaging substrate allows higher energy electrons to pass through an energy filter (see, e.g., energy filter 142 in FIG. 1 ) compared to other areas of the packaging substrate. As a result, more electrons reach the electron detector 140. The brighter areas in FIG. 7A refer to higher energy electrons.
[0098] According to some embodiments that can be combined with other embodiments described herein, a portion of a packaging substrate as referred to herein may involve an area, such as the area of image 600 shown in FIG. 7A. The portion of the packaging substrate typically includes one or more first surface contact points and / or one or more second surface contact points, as described herein. An image is generated by raster scanning an electron beam over a field of view or a portion of a field of view. This area can be scanned by an electron beam, similar to scanning an image. According to some embodiments that can be combined with other embodiments described herein, a portion of a packaging substrate as referred to herein may also be one or more beam positions on a surface contact point, where the electron beam contacts the packaging substrate. One or more beam positions can be addressed by an electron beam column by vector scanning to each beam position. FIG. 7A and FIG. 7B represent beam position 604 and beam position 614 with white circles, respectively. Exemplarily, beam position 604 and beam position 614 are displayed on the surface contact points of the packaging substrate.
[0099] According to some embodiments, which can be combined with other embodiments described herein, charging of a portion of a package substrate can be provided over an area and / or at a separate beam position. Additionally or alternatively, reading, such as testing, of a portion of a package substrate can be provided over an area and / or at a separate beam position.
[0100] In the image 600, a portion or region of the package substrate is shown in which a plurality of surface contacts are positively charged (e.g., the dark lines of surface contacts 602 shown in FIG. 7A), while FIG. 7B shows an image of a read region or read or tested surface contacts. The more positive surface contacts 612, the darker the image 610 is, and the more negative surface contacts 613, the lighter the image 610 is. In addition, FIG. 7B illustrates beam positions 614 that can be used in a vector scan test procedure as white circles.
[0101] Image 610 shows a line of positively charged surface contacts, however it is interrupted on the right hand side.Thus, considering the charging of the entire line as shown in FIG7, the interrupted line of surface contacts 612 can be analyzed as a defect.
[0102] 7A and 7B describe charging by directing an electron beam onto a first portion of a packaging substrate (specifically, including one or more first surface contacts), and reading (i.e., detecting signal electrons) by directing an electron beam onto a second portion of the packaging substrate (specifically, including one or more second surface contacts). As can be seen from image 600, signal electrons are generated during charging of a portion of the packaging substrate (e.g., a field of view region or a surface contact point within the field of view). Thus, detection signal electrons for testing at least a first device-to-device electrical interconnect path can be provided while charging a portion of the packaging substrate and / or reading a charge directed to the other end of the device-to-device electrical interconnect path in the second region of the packaging substrate.
[0103] For example, FIGS. 8A and 8B illustrate an image 700 of a portion of a packaging substrate during charging, in which signal electrons are detected, and an image 710 of an uncharged area of the packaging substrate, in which signal electrons are detected. In the example shown in FIG. 8A , a first surface contact point 702 is negatively charged by the electron beam. As a result, a second surface contact point 704 also shows a negative charge, while other surface contact points 705 are not negatively charged. Even if one contact or surface contact point is charged, two adjacent contacts or adjacent surface contact points will also show the charge provided on one of the contacts. The design of the packaging substrate may include redundant connections or defects, such as short circuits, that may be included in the packaging substrate.
[0104] The image 710 shown in FIG8B illustrates two contacts or surface contacts 715 that are connected to the contacts (i.e., surface contacts 702 and surface contacts 704) in FIG8A as connections for the electrical connection paths between the devices. The other surface contacts 712 are at a lower potential. Even though the images 700 and 710 shown in FIG8A and FIG8B are used to illustrate the testing method according to the specific embodiments described herein, the testing method can also be applied without imaging, i.e., charging and reading with an electron beam at beam position 706 and beam position 716, respectively. Beam position 706 and beam position 716 are shown as white circles in FIG8A and FIG8B.
[0105] 11 illustrates a block diagram for explaining a method of testing a packaging substrate according to an embodiment of the present disclosure. The packaging substrate is a panel of packaging substrates or an advanced packaging substrate. The test may be performed using at least one electron beam from at least one electron beam column.
[0106] At operation 801, a field of view is defined. The field of view is defined to generate a scanning electron microscope (SEM) image using an electron beam of an electron beam column. For example, the field of view or a high-resolution SEM image may have a field of view having a size of 20 mm or more and / or 60 mm or less, respectively. For example, the SEM image may have a field of view of up to about 40 mm x 40 mm. According to some embodiments that may be combined with other embodiments described herein, the resolution of an image (e.g., a SEM image) for initial imaging, for charging, or for defect detection may have a resolution of 0.1 μm to 2 μm.
[0107] At operation 802, at least one electron beam column has a landing energy U pe , a first beam diameter BD1, and a first impact angle θ1 are directed onto one or more first surface contact points on the package substrate. In addition, an electron beam having at least one of a second beam diameter BD2 and a second impact angle θ2 is directed onto one or more second surface contact points different from the one or more first surface contact points, wherein at least one of the following applies: i) the first impact angle θ1 is different from the second impact angle θ2, and ii) the second beam diameter BD2 is different from the first beam diameter BD1. Typically, the electron beam is scanned over the field of view defined in operation 801. By scanning the field of view with a landing energy close to or at a neutral energy value, substrate charging can be reduced or avoided.
[0108] At operation 803, beam positioning and reference potentials may be determined from the image generated at operation 802. In particular, reference potentials may be generated at charging locations, test locations, read locations, and / or surface contact points. No charge is accumulated at these locations, i.e., during the imaging of operation 802, a "no defect" condition may be generated as a reference. In the absence of charge accumulation, defects in the electrical interconnect path do not directly affect the generated image.
[0109] According to some embodiments that can be combined with other embodiments described herein, the image generated at operation 802 can be analyzed, for example, by pattern recognition. The analysis can calibrate the electron beam position. Thus, surface contact points can be addressed with calibrated beam positions, such as vector scanning. Further distortion calibration of the electron beam in the field of view (FOV) can be avoided, in particular the field of view is significantly larger than that of SEM images with a field of view of 1 mm or less.
[0110] At operation 804, an electron beam is directed to one or more first surface contact points to be charged and one or more second surface contact points to be charged that are different from the one or more first surface contact points. The one or more first surface contact points and / or the one or more second surface contact points can be positively or negatively charged. For example, a negative charge can be provided by an electron beam having an impact angle θ of 0° ≤ θ < 45, specifically 0° ≤ θ < 22.5°, more specifically 0° ≤ θ < 10° at each surface contact point. For example, the impact angle θ can be θ < 5°. It should be noted that a smaller impact angle provides more negative charge, as described exemplary with reference to FIG. 6A.
[0111] A positive charge can be provided by an electron beam having an impact angle θ of 45° ≤ θ2 ≤ 90, specifically 67.5° ≤ θ2 ≤ 90, more specifically 80° ≤ θ ≤ 90° at each surface contact point. For example, the impact angle θ can be 85° ≤ θ ≤ 90°. It should be noted that a larger impact angle provides more positive charge, as described exemplary with reference to FIG. 6B. Additionally or alternatively, a positive charge can be provided by directing the electron beam to each surface contact point with a beam diameter BD of 0.5×D < BD ≤ D, specifically 0.75×D < BD ≤ D (where D is the diameter of the corresponding surface contact point). For example, the beam diameter BD can be 0.9×D < BD ≤ D. It should be noted that by increasing the beam diameter BD from BD = 0.5×D to BD = D, the positive charge can be increased, as described exemplary with reference to FIG. 6C.
[0112] For example, at operation 804, if there are no defects in the electrical interconnect path, all test points (i.e., selected surface contact points) of the connected network or electrical interconnect path can be charged to the same potential.
[0113] At operation 805, signal electrons are detected to test one or more electrical interconnect paths of the package substrate. For example, a voltage contrast image between a good reference die and a test die can be compared. Additionally or alternatively, according to an embodiment that can be combined with other embodiments described herein, a voltage difference can be generated compared to the reference image generated at operation 802.
[0114] Differences in the voltage contrast image indicate the presence of a defect. The voltage difference at a predetermined beam position corresponding to a surface contact point, for example, can be evaluated. An image including voltage contrast information can be generated. Pattern recognition can be provided on at least a portion of the image to evaluate the deviation of the interconnect path network compared to the desired package substrate. Additionally or alternatively, the voltage of the surface contact point to be tested (i.e., “read”) can be measured by determining signal electrons, specifically using a detector with an energy filter. The surface contact point can be measured, for example, the voltage contrast of the surface contact point can be measured.
[0115] According to a specific embodiment of the present disclosure, a measurement of a first surface contact point may be provided at a first beam position and a measurement of a second surface contact point may be provided at a second beam position. A vector scan may be provided to move the electron beam from the first beam position to the second beam position, i.e., directly move the electron beam from the first beam position to the second beam position. Only a few surface contact points, such as two surface contact points, or a small number (<20) of surface contact points, corresponding to the beam positions may be required to measure an electrical interconnect path network.
[0116] Specific embodiments of the present disclosure may include the generation of SEM images. The apparatus for testing according to embodiments of the present disclosure may be configured to generate SEM images. The resolution of the image may be 3 µm or less and / or 0.1 µm or more. For example, beam positioning settings for beam positions on surface contact points may be based on SEM images and may be provided automatically. No electron beam distortion calibration is required because positioning may be calculated from the SEM image. Individual beam positions may be calibrated by pattern recognition (i.e., by utilizing unique features of the package substrate during pattern recognition) for electron beam alignment.
[0117] FIG9 illustrates another embodiment of a method for testing a package substrate, wherein the package substrate is a panel-level package substrate or an advanced package substrate. According to one embodiment, the method includes placing a package substrate 10 on a platform 105 in a vacuum chamber 110, as shown in operation 901. In operation 902, at least one electron beam column having a landing energy U pe An electron beam 111 having a first beam diameter BD1, a first impact angle θ1 and a second beam diameter BD2 is directed onto one or more first surface contact points on the packaging substrate. At operation 903, an electron beam 111 having at least one of a second beam diameter BD2 and a second impact angle θ2 is directed onto one or more second surface contact points. The one or more second surface contact points are different from the one or more first surface contact points. In addition, at least one of the following situations applies: i) the first impact angle θ1 is different from the second impact angle θ2, and (ii) the second beam diameter BD2 is different from the first beam diameter BD1. At operation 904, signal electrons 113 emitted upon electron beam impact are detected to test at least a first inter-device electrical interconnect path 20 of the packaging substrate.
[0118] According to some embodiments that may be combined with other embodiments described herein, the first impact angle θ1 is 0°≤θ1<45°. Specifically, the first impact angle θ1 may be 0°≤θ1<22.5°. Typically, the first impact angle θ1 is 0°≤θ1<10°. According to an example, the first impact angle θ1 may be 0°≤θ1<5°.
[0119] According to some embodiments that can be combined with other embodiments described herein, the second impact angle θ2 is 45° ≤ θ2 ≤ 90. Specifically, the second impact angle θ2 can be 67.5° ≤ θ2 ≤ 90. Generally, the second impact angle θ2 is 80° ≤ θ2 < 90°. According to one example, the second impact angle θ2 can be 85° ≤ θ2 < 90°.
[0120] According to some embodiments that can be combined with other embodiments described herein, one or more first surface contact points have a first diameter D1 and the first beam diameter BD1 is BD1 ≤ 0.25×D1. Specifically, the first beam diameter BD1 can be BD1 ≤ 0.10×D1. For example, the first beam diameter BD1 can be BD1 ≤ 0.05×D1.
[0121] According to some embodiments that can be combined with other embodiments described herein, one or more second surface contact points have a second diameter D2 and the second beam diameter BD2 is 0.5×D2 < BD2 ≤ D2. Specifically, the second beam diameter BD2 can be 0.75×D2 < BD2 ≤ D2. For example, the second beam diameter BD2 can be 0.9×D2 < BD2 ≤ D2. Generally, the first diameter D1 of one or more first surface contact points corresponds to the second diameter D2 of one or more second surface contact points. In other words, the first diameter D1 can be substantially the same as the second diameter D2. The term "substantially the same" can be understood to be the same within a tolerance T of T ≤ 10% (specifically T ≤ 5%).
[0122] According to some embodiments that can be combined with other embodiments described herein, the electron beam 111 is directed to a first relative position of one or more first surface contact points. In addition, the electron beam 111 is directed to a second relative position of one or more second surface contact points. The second relative position is different from the first relative position. "The relative position of the surface contact point" can be understood to refer to the selected position of a particular surface contact point.
[0123] FIG. 9 illustrates a schematic side view of a surface contact point, and FIG. 10 shows a schematic top view of a surface contact point. Referring to FIG. 9 and FIG. 10 , the “relative position of the surface contact point” is explained, which can be applied to the first relative position of one or more first surface contact points and the second relative position of one or more second surface contact points described herein. As exemplarily shown in FIG. 9 , the surface contact point described herein generally has a convex morphology with a diameter D and an apex AP. In particular, the apex AP can be a central apex, such as the central apex of a hemispherical contact point, as exemplarily shown in FIG. 9 and FIG. 10 . It should be understood that the surface contact point with a diameter D and an apex AP illustrated in FIG. 9 and FIG. 10 can also be applied to one or more first surface contact points with a first diameter D1 and a first apex AP1 and one or more second surface contact points with a second diameter D2 and a second apex AP2, as described herein. In other words, the diameter D shown in FIG. 9 and FIG. 10 can be replaced by the first diameter D1 or the second diameter D2. Therefore, the apex AP shown in FIG. 9 and FIG. 10 can be replaced by the first apex AP1 or the second apex AP2.
[0124] According to some embodiments that can be combined with other embodiments described herein, one or more first surface contact points have a convex shape with a first diameter D1 and a first vertex AP1. In particular, the first vertex AP1 can be a central first vertex. The electron beam can be directed to a first relative position of the one or more first surface contact points. Typically, the first relative position is located within a first area A1 around the first vertex AP1, where A1 ≤ (D1 / 4) 2 ×π. The first area A1 is exemplarily indicated in FIG. 10. Specifically, the first relative position may be within the first area A1 surrounding the first vertex AP1, where A1≤(D1 / 8) 2 ×π. More specifically, the first relative position may be within a first area A1 surrounding the first vertex AP1, where A1≤(D1 / 10) 2 ×π.
[0125] According to some embodiments that can be combined with other embodiments described herein, one or more second surface contact points have a convex morphology, the convex morphology having a second diameter D2 and a second vertex AP2. In particular, the second vertex AP2 can be a central second vertex. The electron beam can be directed to a second relative position of the one or more second surface contact points. The second relative position is located within a second area A2 around the second vertex AP2, where [(D2 / 2) 2 ×π-(D2 / 4) 2 ×π]≤A2≤[(D2 / 2) 2 ×π-(D2 / 8) 2×π]. The second area A2 is exemplarily indicated in Fig. 10. As exemplarily shown in Fig. 10, a typical second area A2 is an annular area.
[0126] According to some embodiments that can be combined with other embodiments described herein, the landing energy U of the electron beam pe Selected as E N2 pe <E N2 '. E N2 is the second neutral energy value corresponding to the landing energy with a total electron yield of 1 at an impact angle θ = 0°. E N2 ' is the second neutral energy value corresponding to the landing energy with a total electron yield of 1 when the impact angle θ = 90°. Usually, the landing energy U pe Choose in E N2 and E N2 ' is between ±25%. That is, the landing energy U pe It may be [E N2 +0.25×E N2 ] pe <[E N2 '-0.25×E N2 ].
[0127] According to some embodiments that can be combined with other embodiments described herein, the landing energy U of the electron beam pe Selected as E N1 ' pe <E N1 . E N1 is the first neutral energy value corresponding to the landing energy with a total electron yield of 1 at an impact angle θ = 0°. E N1 is the first neutral energy value corresponding to the landing energy with a total electron yield of 1 at an impact angle θ = 90°. Specifically, the landing energy U pe You can choose to N1 ' and E N1 ±25% between the two. That is, the landing energy U pe It may be [E N1 '+0.25×E N1 '] pe <[E N1 -0.25×E N1 ].
[0128] According to some embodiments that may be combined with other embodiments described herein, the method further includes scanning the electron beam to one or more first surface contacts and one or more second surface contacts on the packaging substrate to charge and detect signal electrons. Typically, the one or more first surface contacts and the one or more second surface contacts are formed as metal pads covered by solder bumps having a diameter of 25 μm or less (specifically 10 μm or less). As exemplarily described with reference to Figures 4A to 4D, the packaging substrate typically includes a plurality of inter-device electrical interconnect paths extending between corresponding first surface contacts and second surface contacts. Therefore, the method typically also includes testing a plurality of inter-device electrical interconnect paths. Testing of the plurality of inter-device electrical interconnect paths can be performed sequentially and / or in parallel.
[0129] According to some embodiments that can be combined with other embodiments described herein, the package substrate tested by the method described herein includes 5000 or more inter-device electrical interconnect paths, some or all of which are tested. Specifically, the package substrate tested by the method described herein may include 20000 or more (specifically 50000 or more) inter-device electrical interconnect paths, some or all of which are tested.
[0130] According to some embodiments that may be combined with other embodiments described herein, the method includes obtaining information about one or more potentials from the energy of the signal electrons. Obtaining the information may include energy filtering the signal electrons. In addition, the method generally includes determining whether the first inter-device electrical interconnect path is defective based on the information. Optionally, the method may also include classifying any determined defects.
[0131] According to some embodiments, which can be combined with other embodiments described herein, the testing of the package substrate includes determining whether the first inter-device electrical interconnect path has one or more of the following defects: a short circuit, an open circuit, and / or a leakage.
[0132] The charge on the package substrate portion, in particular the charge on the surface contact points described herein, can be controlled. Additionally or alternatively, the charge is applied during some test sequences, not applied or substantially not applied during some test sequences, and the charge can be removed during some test sequences. In particular, the charge can be applied during a "write" operation. Advantageously, the charge is not applied during a "read" operation.
[0133] According to some embodiments that can be combined with other embodiments described herein, individual beam positions can be addressed by vector scanning. That is, the electron beam can be directed to various positions, for example, where no area needs to be scanned. The ability to provide charge at various beam positions and read the charge at various beam positions allows for fast test operations. In addition, multiple test sequences can be generated, in which different patterns can be "written" on various surface contact points of the packaging substrate. The pattern can be provided, for example, in the form of a checkerboard with negative charge positions and positive charge positions. As a result, the total charge on the packaging substrate is reduced. According to some embodiments that can be combined with other embodiments described herein, patterns such as a checkerboard can also be provided on regions rather than on individual positions.
[0134] According to some embodiments that can be combined with other embodiments described herein, a charge reading (i.e., detection signal electronics) at a beam position where a charge or potential is to be determined can be provided at a written beam position. For example, a charge can be applied to a first surface contact point. After a predetermined period of time, it can be measured whether a charge can be detected at the first surface contact point. Additionally or alternatively, the detection signal electronics (i.e., "reading") can be provided at a different beam position (e.g., at a second surface contact point connected to the first surface contact point to which a charge has been applied). The electrical connection between the first surface contact point and the second surface contact point provides the charge written to the first surface contact point to the second surface contact point. Therefore, if the electrical connection is not defective, the charge can be detected at the second surface contact point. Further additionally or alternatively, the detection signal electronics (i.e., "reading") can be provided at another different beam position (e.g., at a third surface contact point that is not connected to the first surface contact point). Since the third surface contact point is not connected to the first surface contact point, the charge cannot be detected for a non-defective packaging substrate. According to some embodiments that can be combined with other embodiments described herein, one or more third surface contacts adjacent to the second surface contact point and / or adjacent to the first surface contact point can be measured. Unless there is a short circuit between adjacent surface contacts, the charge provided on the first surface contact should not be detected at the one or more third surface contacts.
[0135] As described above, individual beam positions may be addressed by vector scanning, and a test sequence may be provided by directing the electron beam only to individual (i.e., different) beam positions. Furthermore, the test sequence may include a raster scan of a substrate area. Thus, a portion of the package substrate may also be referred to as a raster scanned area, wherein an image of the area is generated. In particular, a "read" operation may be provided based on an image raster scanned in an area of the package substrate.
[0136] According to some embodiments, which may be combined with other embodiments described herein, imaging of an area of a package substrate may also be provided without generating a charge, for example, by raster scanning. For example, a reference image may be generated. A reference potential may be determined from the reference image without generating a charge. Additionally or alternatively, beam positioning calibration may be provided based on the reference image.
[0137] According to yet another embodiment, defect inspection can be provided by a method of testing a package substrate according to an embodiment described herein. For example, an automatic optical inspection system (AOI system) can generate a list of potential defect locations. The list of locations can be subject to defect review. A charge can be provided on the structure of the location to be reviewed. For example, the charge can be provided by aiming an electron beam at a surface contact point or by scanning an electron beam over an area including the location to be inspected. An image can be generated to view locations or areas with potential defects. According to some embodiments that can be combined with other embodiments described herein, an image can be generated by detecting signal electrons and, in particular, including voltage contrast information.
[0138] Embodiments of the present disclosure provide one or more of the following advantages. Contactless electrical testing of a package substrate as disclosed herein can be provided, wherein charge can be controlled for electrical defect detection. In view of the flexibility of the electron beam, an increased test speed can be provided. During mass production, tests including 100% of the electrical interconnect paths can be performed. In addition, the flexibility of the electron beam allows testing and flexible settings for different AP / PLP substrate layouts. The test methods and apparatus disclosed herein also allow for scalability to smaller sizes, particularly if technology development is moving towards smaller structural sizes. Testing of the package substrate does not cause damage. In addition, embodiments of the present disclosure beneficially provide a low signal-to-noise ratio. In particular, since the neutral energy value of the package substrate as described herein can be similar to the neutral energy value of the surface contact point as described herein, the embodiments of the test method as described herein are relatively insensitive to the parasitic charge effects of the package substrate.
[0139] While the foregoing is directed to certain embodiments, other and further embodiments may be envisaged without departing from the basic scope of the foregoing, and the scope of the foregoing is determined by the claims that follow.
Claims
1. A method for testing a packaged substrate (10) with at least one electron beam column (120), the packaged substrate being a panel-level packaged substrate or an advanced packaged substrate, the method comprising the steps of: Placing the packaged substrate (10) on a platform (105) in a vacuum chamber (110); The at least one electron beam column has a landing energy U pe , directing an electron beam (111) having a first beam diameter BD1 and a first impact angle θ1 onto one or more first surface contact points on the packaging substrate; Directing the electron beam (111) having at least one of a second beam diameter BD2 and a second impact angle θ2 to one or more second surface contact points different from the one or more first surface contact points, wherein at least one of the following applies: i) The first impact angle θ1 is different from the second impact angle θ2, and ii) The second beam diameter BD2 is different from the first beam diameter BD1; and Detecting signal electrons (113) emitted upon impact of the electron beam to test at least a first inter-device electrical interconnect path (20) of the packaged substrate.
2. The method according to claim 1, wherein the first impact angle θ1 is 0° ≤ θ1 < 45°, particularly 0° ≤ θ1 < 22.5°, and wherein the second impact angle θ2 is 45° ≤ θ2 ≤ 90, particularly 67.5° ≤ θ2 ≤ 90.
3. The method according to claim 1 or 2, wherein the one or more first surface contact points have a first diameter D1, and the first beam diameter BD1 is BD1 ≤ 0.25×D1, particularly BD1 ≤ 0.10×D1.
4. The method according to any one of claims 1 to 3, wherein the one or more second surface contact points have a second diameter D2, and the second beam diameter BD2 is 0.5×D2 < BD2 ≤ D2, particularly 0.75×D2 < BD2 ≤ D2.
5. The method according to any one of claims 1 to 4, wherein the electron beam (111) is directed to a first relative position of the one or more first surface contact points, and wherein the electron beam (111) is directed to a second relative position of the one or more second surface contact points, wherein the second relative position is different from the first relative position.
6. The method according to claim 5, wherein the one or more first surface contact points have a convex topography having a first diameter D1 and a first vertex AP1, in particular a central first vertex, and wherein the first relative position is within a first area A1 around the first vertex AP1, wherein A1 ≤ (D1 / 4) 2 ×π, especially A1≤(D1 / 8) 2 ×π.
7. The method according to claim 5 or 6, wherein the one or more second surface contact points have a convex topography with a second diameter D2 and a second vertex AP2, in particular a central second vertex, and wherein the second relative position is within a second area A2 around the second vertex AP2, wherein [(D2 / 2) 2 ×π-(D2 / 4) 2 ×π]≤A2≤[(D2 / 2) 2 ×π-(D2 / 8) 2 ×π].
8. The method according to any one of claims 1 to 7, wherein the landing energy U pe Selected as E N2 pe <E N2 ', where E N2 is the second neutral energy value corresponding to the landing energy with a total electron yield of 1 when the impact angle θ=0°, and where E N2 ' is the second neutral energy value corresponding to the landing energy with a total electron yield of 1 when the impact angle θ=90°, in particular, wherein the landing energy U pe Located in E N2 and E N2 'Middle ±25%. 9. The method according to any one of claims 1 to 7, wherein the landing energy U pe Selected as E N1 pe <E N1 ', where E N1 is the first neutral energy value corresponding to the landing energy with a total electron yield of 1 when the impact angle θ=0°, and where E N1 ' is the first neutral energy value corresponding to the landing energy with a total electron yield of 1 when the impact angle θ=90°, in particular, wherein the landing energy U pe Located in E N1 and E N1 'Middle ±25%. 10. The method according to any one of claims 1 to 9, further comprising the steps of: Scanning the electron beam to the one or more first surface contact points and the one or more second surface contact points on the packaged substrate for charging and detecting the signal electrons.
11. The method according to any one of claims 1 to 10, wherein the one or more first surface contact points and the one or more second surface contact points are formed as metal pads covered with solder bumps having a diameter of 25 μm or less, particularly 10 μm or less.
12. The method according to any one of claims 1 to 11, wherein the packaged substrate includes a plurality of inter-device electrical interconnect paths extending between corresponding first surface contact points and second surface contact points, the method further comprising the steps of: Testing the plurality of inter-device electrical interconnect paths sequentially and / or in parallel.
13. The method according to any one of claims 1 to 12, wherein the packaging substrate includes 5,000 or more inter-device electrical interconnect paths, particularly 20,000 or more inter-device electrical interconnect paths, and more particularly 50,000 or more inter-device electrical interconnect paths that are all tested.
14. The method according to any one of claims 1 to 13, further comprising the following steps: deriving information about one or more potentials from the energy of the signal electrons; and Determining whether the first inter-device electrical interconnect path is defective based on the information, and optionally further comprising classifying any determined defects.
15. The method of claim 14, wherein the step of obtaining the information comprises energy filtering the signal electrons.
16. The method of any one of claims 1 to 15, wherein the step of testing comprises determining whether the first inter-device electrical interconnect path has one or more of the following defects: a short circuit, an open circuit and / or a leakage.
17. An apparatus for testing a package substrate according to the method of any one of claims 1 to 16.
18. An apparatus (100) for contactlessly testing a package substrate (10), comprising: A vacuum chamber (110); A platform (105), the platform is located in the vacuum chamber, the platform is configured to support the packaging substrate, the packaging substrate is a panel-level packaging substrate or an advanced packaging substrate; A charged particle beam column (120), the charged particle beam column being configured to generate an electron beam, the electron beam column comprising: an objective lens (124), the objective lens being configured to focus the electron beam onto the packaging substrate; a scanning deflector (122), the scanning deflector being configured to scan the electron beam to different positions on the packaging substrate; an electron detector (140) for detecting signal electrons (113) emitted when the electron beam impinges on the packaging substrate; and One or more power supplies, the one or more power supplies providing the landing energy U of the electron beam pe ; an analyzing unit (141) for determining whether the first inter-device electrical interconnect path (20) is defective based on the signal electrons (113); and A controller (180) configured to control the scanning deflector (122) and the objective lens (124) for: a) directing the electron beam (111) having a first beam diameter BD1 and a first impact angle θ1 onto one or more first surface contact points on the packaging substrate (10), and b) directing the electron beam (111) having at least one of a second beam diameter BD2 and a second impact angle θ2 onto one or more second surface contact points different from the one or more first surface contact points, wherein at least one of the following applies: i) the first impact angle θ1 is different from the second impact angle θ2, and ii) The second beam diameter BD2 is different from the first beam diameter BD1.
19. The apparatus of claim 18, wherein the electronic detector (140) comprises: E Verhard-Thornley detector; and An energy filter (142) for the signal electrons (113) in front of the Everhard-Thornley detector.
20. An apparatus according to claim 18 or 19, wherein the scan controller (123) is configured so that the electron beam is directed to pairs of first surface contacts and second surface contacts in sequence for testing corresponding inter-device electrical interconnect paths extending between corresponding pairs of the first surface contacts and second surface contacts.