Solar cell module

By designing the special thickness distribution and lamination treatment of the support members and filler materials in the solar cell module, the flexibility and strength of the module are improved, the problem of insufficient flexibility and strength in the prior art is solved, and the material cost is reduced.

CN119032428APending Publication Date: 2024-11-26KYOCERA CORP
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202380032866.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2022-04-28
Filing Date
2023-04-20
Publication Date
2024-11-26

Smart Images

  • Figure CN119032428A_ABST
    Figure CN119032428A_ABST
Patent Text Reader

Abstract

The solar cell module includes a first protective layer, a solar cell portion, a support member, and a filler. The first protective layer has a first surface and a second surface opposite to the first surface. The solar cell part includes a plurality of solar cell elements provided in a state of facing the second surface of the first protective layer. The support member is provided in a state of being adjacent to the solar cell section. The support member includes an inner portion provided so as to face the second surface of the first protective layer, and an outer portion provided so as to extend outward from the inner portion. The filler is in contact with the second surface of the first protective layer, and is provided so as to cover the inner portion and the solar cell section. The thickness of the filling material between the solar cell part and the support member is greater than the thickness of the filling material between two adjacent solar cell elements among the plurality of solar cell elements.
Need to check novelty before this filing date? Find Prior Art

Description

[0001] Cross-references of related applications

[0002] This application claims the benefit of priority based on Japanese Patent Application No. 2022-075028 (filed on April 28, 2022), the disclosure of which is incorporated herein by reference in its entirety. Technical Field

[0003] The present disclosure relates to a solar cell module. Background Art

[0004] A solar cell module is known in which a plurality of solar cell elements arranged in a plane and electrically connected are located between a surface protective layer and a back protective layer (for example, see Patent Document 1). In the solar cell module, the plurality of solar cell elements are covered with a filler material having ethylene vinyl acetate copolymer (EVA) as a main component.

[0005] Prior Art Literature

[0006] Patent Literature

[0007] Patent Document 1: International Publication No. 2021 / 070743 Summary of the invention

[0008] A solar cell module is disclosed.

[0009] In one embodiment, a solar cell module comprises a first protective layer, a solar cell unit, a supporting member and a filling material. The first protective layer has a first surface and a second surface on the side opposite to the first surface. The solar cell unit includes a plurality of solar cell elements arranged in a state facing the second surface of the first protective layer. The supporting member is arranged in a state adjacent to the solar cell unit. The supporting member includes an inner portion arranged in a state facing the second surface of the first protective layer, and an outer portion arranged in a state extending from the inner portion to the outside. The filling material is in contact with the second surface of the first protective layer and is arranged in a state covering the inner portion and the solar cell unit. The thickness of the filling material between the solar cell unit and the supporting member is greater than the thickness of the filling material between two adjacent solar cell elements among the plurality of solar cell elements.

[0010] In addition, in one embodiment, the solar cell module includes a first protective layer, a solar cell unit, a supporting member, and a filling material. The first protective layer has a first surface and a second surface on the side opposite to the first surface. The solar cell unit is arranged in a state opposite to the second surface of the first protective layer. The supporting member is arranged in a state adjacent to the solar cell unit. The supporting member includes an inner portion arranged in a state opposite to the second surface of the first protective layer, and an outer portion arranged in a state extending from the inner portion to the outside. The filling material is in contact with the second surface of the first protective layer, and is arranged in a state covering the inner portion and the solar cell unit. The thickness of the filling material increases as it goes from the solar cell unit to the supporting member. BRIEF DESCRIPTION OF THE DRAWINGS

[0011] Figure 1 It is a plan view showing an example of the appearance of the solar cell module according to the first embodiment when viewed from above.

[0012] Figure 2 Yes means Figure 1 FIG. 1 is a diagram showing an example of a virtual cross-section of a solar cell module taken along line Ib-Ib.

[0013] Figure 3 (a) is a diagram showing an example of a structure when a first element surface of a solar cell element is viewed from above. Figure 3 (b) is a diagram showing an example of the structure when the second element surface of the solar cell element is viewed from above.

[0014] Figure 4 (a) to Figure 4 (c) are diagrams illustrating a cross-sectional state during manufacturing in a first specific example of the method for manufacturing a solar cell module according to the first embodiment.

[0015] Figure 5 (a) and Figure 5 (b) are diagrams illustrating a cross-sectional state during manufacturing in a second specific example of the method for manufacturing the solar cell module according to the first embodiment.

[0016] Figure 6 It is a diagram illustrating a state where the solar cell module according to the first embodiment is bent.

[0017] Figure 7 This is a diagram showing an example of a virtual cross section of a solar cell module according to the second embodiment.

[0018] Figure 8 It is enlarged to show Figure 7 Figure 2 shows the area enclosed by the dotted line.

[0019] Fig. 9(a) and Fig. 9 (b) are diagrams illustrating a cross-sectional state during manufacturing in a first specific example of the method for manufacturing a solar cell module according to the second embodiment.

[0020] Fig.10 (a) and Fig.10 (b) are diagrams illustrating a cross-sectional state during manufacturing in a second specific example of the method for manufacturing a solar cell module according to the second embodiment.

[0021] Fig.11 This is a diagram showing an example of a virtual cross section of a solar cell module according to the third embodiment.

[0022] Fig.12 (a) and Fig.12 (b) are diagrams illustrating the state of a cross section during the manufacturing process of the solar cell module according to the third embodiment.

[0023] Fig.13 (a) is a plan view showing an example of the appearance of a solar cell module according to the fourth embodiment when viewed from above. Fig.13 (b) is along Fig.13 (a) is a diagram showing an example of a virtual cross-section of a solar cell module along line IIb-IIb.

[0024] Fig.14 It is a plan view showing an example of the appearance of a solar cell module according to the fifth embodiment when viewed from above.

[0025] Fig.15 (a) is a plan view showing an example of the appearance of a solar cell module according to the sixth embodiment when viewed from above. Fig.15 (b) means Fig.15 (a) is a diagram showing an example of a virtual cross-section of a solar cell module taken along line IIIb-IIIb.

[0026] Fig.16 (a) is a diagram showing an example of the structure of a solar cell module according to the seventh embodiment when viewed from above. Fig.16 (b) means Fig.16 (a) is a diagram showing an example of a virtual cross-section of a solar cell module along line IVb-IVb.

[0027] Fig.17 (a) is a diagram showing an example of the structure of a solar cell portion according to the seventh embodiment when viewed from above. Fig.17 (b) means Fig.17(a) is a diagram showing an example of a virtual cross-section of a solar cell portion along the Vb-Vb line. DETAILED DESCRIPTION

[0028] The inventors have created a technique for improving the flexibility and strength of a solar cell module. In this regard, first to seventh embodiments will be described below with reference to the drawings.

[0029] In the drawings, parts having the same or similar structures and functions are marked with the same symbols, and repeated descriptions are omitted in the following description. Figures 1 to 17 In (b), a right-handed XYZ coordinate system is added. In this XYZ coordinate system, the short side direction of the front face 10f of the solar cell panel 10 is set to the +X direction, the long side direction of the front face 10f is set to the +Y direction, and the normal direction of the front face 10f orthogonal to both the +X direction and the +Y direction is set to the +Z direction.

[0030] <1-1. Solar cell module>

[0031] based on Figures 1 to 3 The solar cell module 100 according to the first embodiment will be described with reference to (b).

[0032] like Figure 1 as well as Figure 2 As shown, the solar cell module 100 includes, for example, a solar cell panel 10. The solar cell panel 10 mainly includes, for example: a light receiving surface (also referred to as a front surface) 10f on which light is incident; and a back surface 10b located on the opposite side of the front surface 10f. In the first embodiment, the front surface 10f is in a state of facing the +Z direction. The back surface 10b is in a state of facing the -Z direction. The +Z direction is set to, for example, the direction toward the sun at mid-sky. Figure 1 In the example of FIG. 1 , the front surface 10 f has a rectangular shape as an example of a rectangular shape.

[0033] The solar cell module 100 may further include a terminal box (not shown) for extracting the electric power generated by the solar cell panel 10 to the outside.

[0034] like Figure 1 as well as Figure 2 As shown, the solar cell panel 10 includes, for example, a surface protection layer 1 , a back surface protection layer 2 , a solar cell section 3 , a filler 4 , and a support member 5 .

[0035] <1-1-1. Surface protection layer>

[0036] Surface protection layer 1, such as the first surface 1f and the second surface 1s of the monitor (refer to Figure 2). In the first embodiment, the first surface 1f is in a state of constituting the front surface 10f of the solar cell panel 10, for example. That is, the surface protection layer 1 has a rectangular shape as an example of a rectangular shape. Figure 1 as well as Figure 2 In the example of , the first surface 1f is exposed to a space (also referred to as an external space) 200 outside the solar cell module 100. In addition, the second surface 1s is a surface on the opposite side to the first surface 1f.

[0037] The surface protection layer 1 has, for example, light transmittance. Specifically, the surface protection layer 1 has, for example, light transmittance for light of a specific range of wavelengths. The specific range of wavelengths, for example, includes wavelengths of light that can be photoelectrically converted by the solar cell unit 3. If the specific range of wavelengths includes wavelengths of light with high irradiation intensity among sunlight, the photoelectric conversion efficiency of the solar cell module 100 can be improved.

[0038] The material of the surface protection layer 1 is, for example, a weather-resistant resin. In other words, the surface protection layer 1 is, for example, a layer composed of a weather-resistant resin. Here, weather resistance means, for example, a property that is difficult to cause deformation, discoloration, and deterioration when used outdoors. By using a resin as the material of the surface protection layer 1, the surface protection layer 1 has, for example, a property of reducing the infiltration of water such as water droplets from the external space 200 of the solar cell module 100 into the solar cell section 3, and moisture easily passes from the filling material 4 to the external space 200 (also called moisture permeability and waterproofness). Here, the weather-resistant resin includes, for example, a fluorine-based resin. The fluorine-based resin includes, for example, a fluorinated ethylene propylene copolymer (Fluorinated Ethylene Propylene: FEP), an ethylene tetrafluoroethylene copolymer (Ethylene Tetrafluoroethylene: ETFE), and an ethylene chlorotrifluoroethylene copolymer (Ethylene Chlorotrifluoroethylene: ECTFE). Here, for example, the surface protection layer 1 can be composed of two or more layers of weather-resistant resin. In this case, the fluorine-based resin used for the surface protection layer 1 may be, for example, two or more types of resins. For this purpose, for example, the fluorine-based resin used for the surface protection layer 1 may include at least one type of resin among FEP, ETFE, and ECTFE.

[0039] The thickness of the surface protection layer 1 is set to, for example, about 0.05 millimeters (mm) to about 0.5 mm. As such, the surface protection layer 1 is not only composed of a resin with a relatively low density and moisture permeability, but also thin, so the surface protection layer 1 is light. For this reason, for example, compared with a structure in which a dense glass having a thickness of about 1 mm or more is used instead of the surface protection layer 1, the solar cell module 100 can be made lighter and thinner.

[0040] In addition, the material of the surface protection layer 1 can replace the fluorine resin or use acrylic resin and polycarbonate resin together with the fluorine resin. In the case of using acrylic resin and polycarbonate, the thickness of the resin is, for example, about 0.03mm to 0.6mm. The surface protection layer 1 can be composed of multiple types of resins.

[0041] <1-1-2. Solar cell section>

[0042] The solar cell section 3 is, for example, located between the surface protection layer 1 and the back protection layer 2. In other words, the solar cell section 3 is in a state of being opposed to the surface protection layer 1 in the Z direction, and is also in a state of being opposed to the back protection layer 2 in the Z direction. Figure 1 as well as Figure 2 As shown, the solar cell section 3 includes, for example, a plurality of solar cell elements 31. The plurality of solar cell elements 31 are located between the second surface 1s of the surface protection layer 1 and the back surface protection layer 2. In the first embodiment, the plurality of solar cell elements 31 are arranged two-dimensionally. Figure 1 as well as Figure 2 In the example of FIG. 1 , the plurality of solar cell elements 31 are arranged in a planar manner along the second surface 1s of the surface protection layer 1. Alternatively, the plurality of solar cell elements 31 may be arranged one-dimensionally.

[0043] The solar cell section 3, for example, further has a plurality of first wiring members 32, a second wiring member 33, and a third wiring member 34. The solar cell section 3, for example, includes a plurality of (here, 2) solar cell strings 30. The plurality of solar cell strings 30, for example, are arranged in the X direction. The plurality of solar cell strings 30, for example, respectively include a plurality of (here, 5) solar cell elements 31 and a plurality of first wiring members 32. In each solar cell string 30, the plurality of solar cell elements 31, for example, are arranged in the Y direction. The plurality of first wiring members 32, for example, are in a state of electrically connecting two adjacent solar cell elements 31 among the plurality of solar cell elements 31. The second wiring member 33 is in a state of electrically connecting two adjacent solar cell strings 30 among the plurality of solar cell strings 30. Figure 1 as well as Figure 2In the example, two third wiring members 34 are respectively connected to two solar cell strings 30. The third wiring member 34 connected to the solar cell string 30 located closest to the end in the -X direction and the third wiring member 34 connected to the solar cell string 30 located closest to the end in the +X direction are in a state of being led out to the outside of the solar cell panel 10.

[0044] Each of the plurality of solar cell elements 31 can convert light energy into electrical energy. Each of the plurality of solar cell elements 31 has: a surface (also referred to as a first element surface) 31f located on the front side; and a surface (also referred to as a second element surface) 31s on the opposite side of the first element surface 31f. Figure 2 In the example of , the first element surface 31f is in a state facing the +Z direction, and the second element surface 31s is in a state facing the -Z direction. In this case, for example, the first element surface 31f mainly functions as a surface for incident light (also called a light-receiving surface), and the second element surface 31s mainly functions as a surface for no incident light (also called a non-light-receiving surface).

[0045] In the first embodiment, as Figure 3 (a) and Figure 3 As shown in (b) of FIG. 8 , each of the plurality of solar cell elements 31 includes a semiconductor substrate 310 , a first output extraction electrode 311 , a first collector electrode 312 , a second output extraction electrode 313 , and a second collector electrode 314 .

[0046] The semiconductor substrate 310 uses, for example, a crystalline semiconductor such as crystalline silicon, an amorphous semiconductor such as amorphous silicon, or a compound semiconductor using four elements of copper, indium, gallium, and selenium, or two elements of cadmium and tellurium. Here, it is assumed that the semiconductor substrate 310 uses crystalline silicon. In this case, the semiconductor substrate 310 mainly includes: a region having a first conductivity type (also referred to as a first conductivity type region); and a region having a second conductivity type opposite to the first conductivity type (also referred to as a second conductivity type region). The first conductivity type region is, for example, located on the second element surface 31s side of the semiconductor substrate 310 in the -Z direction. The second conductivity type region is, for example, located on the surface portion of the first element surface 31f side of the semiconductor substrate 310 in the +Z direction. Here, for example, when the first conductivity type is p-type, the second conductivity type becomes n-type. In addition, for example, when the first conductivity type is n-type, the second conductivity type becomes p-type. As a result, the semiconductor substrate 310 has a pn junction located at the interface between the first conductivity type region and the second conductivity type region. The thickness of the semiconductor substrate 310 is, for example, approximately 0.15 mm to 0.5 mm.

[0047] The first output extraction electrode 311 and the first collector electrode 312 are located, for example, on the surface of the semiconductor substrate 310 on the first element surface 31f side. The first output extraction electrode 311 is, for example, a bus bar electrode. The first collector electrode 312 is, for example, a finger electrode. Figure 3 In the example (a), five substantially parallel first output extraction electrodes 311 are provided on the first element surface 31f side of the semiconductor substrate 310, and a plurality of substantially parallel first collector electrodes 312 are provided substantially orthogonal to the five first output extraction electrodes 311. Figure 3 In the example of (a), the first output extraction electrode 311 has a long strip shape long in the Y direction, and the first collector electrode 312 has a linear shape long in the X direction. In addition, in the area where the first output extraction electrode 311 and the first collector electrode 312 are not formed on the second conductive type area of ​​the semiconductor substrate 310, for example, an insulating film as a reflection prevention film 315 in a state containing silicon nitride or the like can be provided. Here, for example, in the case where the main component of the first output extraction electrode 311 is silver, the first output extraction electrode 311 can be formed by, for example, applying a silver paste into a desired shape by screen printing or the like and then firing it. The so-called main component refers to the component with the largest (high) content ratio (also referred to as the content rate) among the contained components. The silver paste, for example, uses a metal paste containing a metal powder containing silver as a main component, an organic carrier, and a glass material. For example, when the main component of the first collector electrode 312 is silver, the first collector electrode 312 can be formed by applying silver paste into a desired shape by screen printing or the like and then firing it, similarly to the first output extraction electrode 311. The first output extraction electrode 311 and the first collector electrode 312 can be formed in different processes or in the same process.

[0048] The second output extraction electrode 313 and the second collector electrode 314 are located, for example, on the surface of the semiconductor substrate 310 on the second element surface 31s side. The second output extraction electrode 313 is, for example, a bus bar electrode. Figure 3In the example (b), five columns of second output extraction electrodes 313 substantially parallel to each other along the +Y direction are provided on the second element surface 31s side of the semiconductor substrate 310. The second collector electrode 314 is located on the second element surface 31s side of the semiconductor substrate 310, on substantially the entire surface of the region where the second output extraction electrode 313 is not formed, except for the portion where the second output extraction electrode 313 and the second collector electrode 314 are connected to each other by overlapping. The five columns of second output extraction electrodes 313 each include, for example, four electrodes arranged in a row. In addition, for example, a thin film of an oxide or nitride such as aluminum oxide may exist in a desired pattern between the first conductive type region of the semiconductor substrate 310 and the second output extraction electrode 313 and the second collector electrode 314 as a passivation film. Here, for example, when the main component of the second output extraction electrode 313 is silver, the second output extraction electrode 313 can be formed by applying silver paste into a desired shape by screen printing or the like and then firing it, similarly to the first output extraction electrode 311. For example, when the main component of the second collector electrode 314 is aluminum, the second collector electrode 314 can be formed by applying aluminum paste into a desired shape by screen printing or the like and then firing it. The aluminum paste is, for example, a metal paste containing a metal powder containing aluminum as a main component, an organic vehicle, and glass frit.

[0049] The first wiring member 32 is in a state of electrically connecting, for example, a first output extraction electrode 311 of one solar cell element 31 and a second output extraction electrode 313 of another solar cell element 31 next to the one solar cell element 31 . Figure 3 (a) and in Figure 3 In the example of (b), the outer edges of the plurality of first wiring members 32 respectively attached to the solar cell elements 31 are virtually drawn by two-dot chain lines. Figure 1 To Figure 3In the example of (b), the first wiring member 32 has a long strip shape that is long in the Y direction. Here, the first wiring member 32 is, for example, in a state of being bonded to the first output extraction electrode 311 and the second output extraction electrode 313. Specifically, for example, there is a portion (also referred to as a first bonding portion) 321 that is located between the first wiring member 32 and the first output extraction electrode 311 and bonds the first wiring member 32 and the first output extraction electrode 311. For this reason, for example, the first wiring member 32 is in a state of being bonded to the first output extraction electrode 311 of one solar cell element 31 via the first bonding portion 321. In addition, for example, there is a portion (also referred to as a second bonding portion) 322 that is located between the first wiring member 32 and the second output extraction electrode 313 and bonds the first wiring member 32 and the second output extraction electrode 313. For this reason, for example, the first wiring member 32 is in a state of being bonded to the second output extraction electrode 313 of another solar cell element 31 next to one solar cell element 31 via the second bonding portion 322. The first wiring member 32 is, for example, a metal body having a conductive wire or strip shape. The materials of the first bonding portion 321 and the second bonding portion 322 are, for example, low-melting-point alloys such as solder or low-melting-point single metals. More specifically, the first wiring member 32 is, for example, a copper foil having a thickness of about 0.1 mm to 0.2 mm and a width of about 1 mm to 2 mm, and is in a state where the entire surface of the first wiring member 32 is covered with solder. The first wiring member 32 is, for example, in a state where it is electrically connected to the first output extraction electrode 311 and the second output extraction electrode 313 by soldering. In this case, for example, the solder between the first wiring member 32 and the first output extraction electrode 311 constitutes the first bonding portion 321. In addition, for example, the solder between the first wiring member 32 and the second output extraction electrode 313 constitutes the second bonding portion 322.

[0050] <1-1-3. Filling materials>

[0051] The filling material 4 is in a state of covering the solar cell section 3 between the surface protection layer 1 and the back protection layer 2. In other words, the filling material 4 is in a state of covering the plurality of solar cell elements 31 between the surface protection layer 1 and the back protection layer 2. From another point of view, the filling material 4 is in a state of covering and filling the solar cell section 3 in, for example, the region (also referred to as the gap region) 10g between the surface protection layer 1 and the back protection layer 2.

[0052] The filler 4 has a first surface 4f located on the surface and a second surface 4s located on the opposite side of the first surface 4f. The first surface 4f of the filler 4 is in contact with the second surface 1s of the surface protection layer 1, and the second surface 4s of the filler 4 is in contact with the back protection layer 2.

[0053] In the first embodiment, the filler 4 includes, for example, a filler (also referred to as a first filler) 41 located on the front face 10f side and a filler (also referred to as a second filler) 42 located on the back face 10b side. The first filler 41 is, for example, in a state of constituting the first face 4f and in a state of covering the entire surface of the surface protection layer 1 side of the solar cell section 3. In other words, the first filler 41 is, for example, in a state of covering the plurality of solar cell elements 31 between the surface protection layer 1 and the plurality of solar cell elements 31. The second filler 42 is, for example, in a state of constituting the second face 4s and in a state of covering the entire surface of the back face protection layer 2 side of the solar cell section 3. In other words, the second filler 42 is, for example, in a state of covering the plurality of solar cell elements 31 between the back face protection layer 2 and the plurality of solar cell elements 31. For this reason, in the first embodiment, the solar cell section 3 is, for example, in a state of being surrounded and sandwiched by the first filler 41 and the second filler 42. Thus, for example, the posture of the solar cell section 3 can be maintained by the filler 4.

[0054] In addition, the filler 4 has, for example, light transmittance. Here, the filler 4 has, for example, light transmittance to light of the above-mentioned specific range of wavelengths. Here, for example, as long as at least the first filler 41 of the first filler 41 and the second filler 42 constituting the filler 4 has light transmittance, incident light from the front face 10f side can reach the solar cell section 3.

[0055] The material of the first filling material 41 is, for example, ethylene vinyl acetate copolymer (EVA), polyvinyl butyral (PVB) and other polyvinyl acetals and acid-modified resins. Here, for example, if the material of the first filling material 41 is relatively cheap EVA, the performance of protecting multiple solar cell elements 31 can be easily achieved. The acid-modified resin is, for example, a modified polyolefin resin that can be formed by acid-based grafting modification of a resin such as polyolefin. The acid that can be used in the grafting modification of the acid-modified resin can be, for example, acrylic acid, methacrylic acid, maleic acid, fumaric acid, itaconic acid, maleic anhydride, nadic anhydride, itaconic anhydride and citraconic anhydride. The material of the second filling material 42 can be, for example, polyvinyl acetals such as EVA and PVB and acid-modified resins, like the first filling material 41. The first filling material 41 and the second filling material 42 can be composed of two or more types of materials.

[0056] The second filler 42 may contain a pigment, for example. For example, when a white pigment is contained, light transmitted through the solar cell section 3 can be reflected by the second filler 42 and re-enter the solar cell section 3. This can improve the power generation efficiency of the solar cell module 100.

[0057] In addition, the filler 4 may not include the second filler 42 but may include only the first filler 41 . In this case, the first filler 41 covers the solar cell section 3 between the front surface protection layer 1 and the back surface protection layer 2 .

[0058] <1-1-4. Back protective layer>

[0059] The back protective layer 2 is, for example, in a state of constituting the back side 10b of the solar cell panel 10. The back protective layer 2 is, for example, in a state of being opposed to the second surface 1s of the surface protective layer 1. The back protective layer 2 is in contact with the filler 4 on the side opposite to the surface protective layer 1 relative to the filler 4. The back protective layer 2 is provided in a state of being opposed to the solar cell section 3 and the inner portion 51 of the support member 5 in the Z direction. As described later, the inner portion 51 is a portion on the solar cell section 3 side relative to the outer portion 52 of the support member 5 in the X direction.

[0060] The back protective layer 2 can protect the solar cell section 3 from the back side 10b, for example. The back protective layer 2 uses, for example, a back sheet constituting the back side 10b. The thickness of the back sheet is, for example, set to about 0.15 mm to 0.5 mm. The material of the back sheet is, for example, a resin. The resin is, for example, the same material as the surface protective layer 1. The back protective layer 2 has the same or similar shape as the surface protective layer 1 when viewed from the back side 10b. For example, it is assumed that when viewed from the back side 10b, both the surface protective layer 1 and the back protective layer 2 have a rectangular shape.

[0061] <1-1-5. Supporting member>

[0062] The support member 5 is a member for improving the rigidity of the solar cell panel 10, and has, for example, higher rigidity than the total rigidity of the surface protection layer 1, the back protection layer 2, and the filler 4. The material of the support member 5 can be, for example, metal, and as a more specific example, aluminum or stainless steel can be used.

[0063] When the main surface of the surface protection layer 1 is viewed from above, the support member 5 is arranged adjacent to the solar cell section 3 with a gap. In other words, when the view is observed along the Z direction, the support member 5 is arranged adjacent to the solar cell section 3 with a gap. Hereinafter, observation along the Z direction is also referred to as viewing from above. The support member 5 includes an inner portion 51 and an outer portion 52, and the inner portion 51 is arranged between the surface protection layer 1 and the back protection layer 2 in a state covered by the filling material 4. In other words, the inner portion 51 is in a state opposite to the surface protection layer 1 in the Z direction, in a state opposite to the back protection layer 2 in the Z direction, and in a state covered by the filling material 4.

[0064] The outer portion 52 is in a state of extending from the inner portion 51 to the side opposite to the solar cell section 3 (ie, the outer side), and is, for example, in a state of not being covered by the filler 4. Figure 1 as well as Figure 2 In the example of , in a plan view, the outer portion 52 is in a state of extending from the inner portion 51 to the outer sides of the surface protection layer 1 and the back protection layer 2. That is, the outer portion 52 is in a state of not being opposed to the surface protection layer 1 in the Z direction, and is also in a state of not being opposed to the back protection layer 2 in the Z direction. In a plan view, the inner portion 51 of the support member 5 is located on the solar cell section 3 side (i.e., the inner side) relative to the outer portion 52 of the support member 5.

[0065] exist Figure 1 as well as Figure 2 In the example of FIG. 5 , the support member 5 has a plate-like shape, and has a rectangular shape in a plan view. Figure 2 In the example of , the ZX cross section of the support member 5 also has a rectangular shape. The corners of the support member 5 can be appropriately chamfered. The long side direction of the support member 5 (here, the Y direction) is, for example, along one side of the surface protection layer 1. In addition, the long side direction of the support member 5 is, for example, along the arrangement direction of the plurality of solar cell elements 31 contained in one solar cell string 30 (here, the Y direction). That is, the long side direction of the support member 5 is, for example, along the long side direction of the first wiring member 32 (here, the Y direction).

[0066] exist Figure 1 as well as Figure 2 In the example of , the solar cell panel 10 includes two supporting members 5. The two supporting members 5 are respectively arranged along the two sides located on both sides of the surface protection layer 1 in the X direction. The two sides located on both sides of the X direction here include one side extending along the Y direction at the end of the -X direction in the surface protection layer 1, and one side extending along the Y direction at the end of the +X direction. That is, one supporting member 5 is located at the end of the -X direction of the surface protection layer 1 and has a rectangular shape with the long side direction in the Y direction, and the other supporting member 5 is located at the end of the +X direction of the surface protection layer 1 and has a rectangular shape with the long side direction in the Y direction. The length of the long side direction (here is the Y direction) of the supporting member 5 is, for example, approximately equal to the length of the surface protection layer 1. The width of the short side direction (here is the X direction) of the supporting member 5 is, for example, set to more than tens of mm. The width of the inner part 51 of the supporting member 5 is, for example, set to more than 20% and less than 80% of the width of the supporting member 5. This allows the support member 5 to be integrated with the filler 4 with relatively high adhesive strength. The thickness of the support member 5 is larger than the thickness of the solar cell section 3 and is set to about 1 mm to 5 mm, for example.

[0067] The outer portion 52 of the support member 5 is mounted on an external building material or other installation target member. For example, a mounting hole (not shown) may be formed in the outer portion 52. The mounting hole penetrates the outer portion 52 in the Z direction. The solar cell panel 10 can be mounted on the installation target member by passing the mounting screw through the mounting hole and screwing it into the installation target member. Figure 1 as well as Figure 2 In the example of , since the two supporting members 5 are respectively located on both sides of the solar cell panel 10, the two supporting members 5 on both sides of the solar cell panel 10 can be fixed to the installation object member. Therefore, the solar cell panel 10 can be more firmly installed on the installation object member. The supporting member 5 can also be said to be a mounting member.

[0068] In addition, Figure 1 In the example, the rigid support member 5 is not mainly located on both sides of the solar cell panel 10 in the Y direction. That is, the support member 5 is not substantially located at the end of the solar cell panel 10 extending along the X direction in the +Y direction, nor is it substantially located at the end of the solar cell panel 10 extending along the X direction in the -Y direction. Figure 6 As shown, by applying an external force F1 to the supporting member 5, the solar cell panel 10 can be bent in an arc shape when viewed in the direction along the Y direction. In other words, when viewed with the line of sight along the Y direction, the solar cell panel 10 can be bent in an arc shape. For example, the solar cell panel 10 can be bent to a state along an arc with a radius of several hundred mm (for example, 500 mm). Accordingly, it is easy to install the solar cell panel 10 on a curved installation object member.

[0069] <1-1-6. Thickness of Filler 4>

[0070] like Figure 2 As shown, the thickness of the filling material 4 is smaller in the solar cell section 3 and larger between the solar cell section 3 and the supporting member 5. Here, thickness W1 and thickness W3 are introduced. Thickness W1 is the thickness (maximum value) of the filling material 4 between the solar cell section 3 and the supporting member 5. Thickness W3 is the thickness (maximum value) of the filling material 4 between two adjacent solar cell elements 31 among the multiple solar cell elements 31 belonging to the solar cell section 3. Figure 2 As shown, the thickness W1 is, for example, larger than the thickness W3. The difference between the thickness W1 and the thickness W3 may be, for example, 0.1 mm or more, 0.5 mm or more, or 1 mm or more.

[0071] Focusing on the distance between the surface protective layer 1 and the back protective layer 2, the distance between the surface protective layer 1 and the back protective layer 2 is smaller in the solar cell section 3 and larger between the solar cell section 3 and the supporting member 5. In other words, the distance (maximum value) between the surface protective layer 1 and the back protective layer 2 between the solar cell section 3 and the supporting member 5 is larger than the distance (maximum value) between the surface protective layer 1 and the back protective layer 2 in the solar cell section 3.

[0072] Here, an example of the thickness distribution of the portion 4a between the solar cell section 3 and the support member 5 in the filler 4 is described. The portion 4a mentioned here is a portion of the filler 4 that is located between the solar cell section 3 and the support member 5 and is provided in a state of being continuous from the surface protection layer 1 to the back protection layer 2. Figure 2 In the example, the thickness W1 of the portion 4a at the end of the support member 5 is greater than the thickness W2 of the portion 4a at the end of the solar cell section 3. The difference between the thickness W1 and the thickness W2 may be, for example, 0.1 mm or more, 0.5 mm or more, or 1 mm or more.

[0073] like Figure 2 As shown, the thickness of the portion 4a of the filling material 4, for example, in at least a portion of the region R1 between the support member 5 and the solar cell section 3, gradually increases as it goes from the solar cell section 3 to the support member 5 along the X direction. That is, the thickness of the portion 4a of the filling material 4 in the region R1 increases monotonically as it goes from the solar cell section 3 to the support member 5 along the X direction. In other words, as the position in the X direction approaches the support member 5 from the solar cell section 3, the thickness of the portion 4a of the filling material 4 at that position gradually increases. In short, the thickness of the portion 4a in the region R1 gradually increases as it goes to the outside along the X direction. The increase in the thickness of the entire region R1 can be, for example, more than 0.1 mm, more than 0.5 mm, or more than 1 mm. The shape of the portion 4a of the filling material 4 is the same in the Y direction, for example.

[0074] In addition, Figure 2 In the example shown in FIG. 1 , the first surface 4 f and the second surface 4 s of the filler 4 have shapes that are line-symmetrical with respect to the XY plane. However, the drawings are merely schematic illustrations and the present invention is not necessarily limited to this.

[0075] <1-2. Characteristics of Solar Cell Modules>

[0076] According to the present embodiment, the inner portion 51 of the rigid support member 5 is covered by the filler 4 between the surface protection layer 1 and the back protection layer 2. Therefore, the rigidity of the solar cell panel 10 can be improved. Figure 1In the example, since the support member 5 is provided so as to be continuous between the ends of the solar cell panel 10 in the Y direction at the ends of the solar cell panel 10 in the X direction, the rigidity in the Y direction can be particularly improved.

[0077] On the other hand, the support member 5 is not substantially located on both sides of the solar cell panel 10 in the Y direction. That is, the support member 5 is not substantially located at the end of the solar cell panel 10 extending in the X direction in the +Y direction, nor is it substantially located at the end of the solar cell panel 10 extending in the X direction in the -Y direction. Therefore, when the solar cell panel 10 is observed with the line of sight along the Y direction, it is possible to bend the solar cell panel 10 in an arc shape (refer to Figure 6 ). In such a flexed state, a relatively large stress is generated in the portion between the support member 5 and the solar cell section 3 in the solar cell panel 10. More specifically, a large stress is generated in the portion near the inner end surface 5a of the support member 5 in the solar cell panel 10. The inner end surface 5a mentioned here is the end surface of the support member 5 on the solar cell section 3 side.

[0078] In the present embodiment, the thickness of the filling material 4 is larger between the supporting member 5 and the solar cell section 3, and smaller in the solar cell section 3. In other words, the thickness W1 is greater than the thickness W3. For this reason, the strength of the solar cell panel 10 can be improved between the supporting member 5 and the solar cell section 3. Therefore, the solar cell panel 10 can appropriately cope with the stress caused by bending. In addition, since the filling material 4 is thinner at the solar cell section 3, the flexibility of the solar cell panel 10 can be improved. That is, the flexibility and strength of the solar cell panel 10 can be taken into account. In addition, compared with the structure in which the thickness W3 is increased to the same extent as the thickness W1, the volume of the filling material 4 can be reduced, and therefore, the material cost of the filling material 4 can be reduced.

[0079] like Figure 2 As shown, if the thickness W1 of the portion 4a of the filling material 4 is greater than the thickness W2, the strength of the solar cell panel 10 can be improved near the inner end surface 5a of the support member 5. For this reason, the solar cell panel 10 can more appropriately cope with the stress caused by bending. In addition, if the thickness of the portion 4a in the region R1 gradually increases as it goes from the solar cell section 3 to the support member 5, the stress at the portion 4a can be effectively dispersed.

[0080] <1-3. First Specific Example of Manufacturing Solar Cell Module According to First Embodiment>

[0081] Next, based on Figure 4 (a) to Figure 4 (c) will now be described an example of a method for manufacturing the solar cell module 100 .

[0082] First, a surface protection layer 1 is prepared. Here, for example, as the surface protection layer 1, a film made of a resin having a rectangular front and back surface and weather resistance is prepared. As the resin having weather resistance, for example, a fluorine-based resin is used. As the fluorine-based resin, for example, FEP, ETFE or ECTFE is used. Here, for example, a treatment for activating the surface by corona treatment or plasma treatment is implemented on the second surface 1s as a single surface of the surface protection layer 1. Thereby, in the lamination process described later, the adhesion between the surface protection layer 1 and the filler 4 can be improved.

[0083] Next, for example, Figure 4 (b) and Figure 4 As shown in (c), the surface protection layer 1, the sheet 41s, the sheet 41t, the solar cell unit 3, the support member 5, the sheet 42s, the sheet 42t, and the back surface protection layer 2 are stacked to form a stacked body 10s.

[0084] In the laminate 10s, the solar cell section 3 is located between two supporting members 5, which are arranged side by side with a gap in the X direction. In addition, at this time, it is appropriate to provide wiring for leading from the solar cell section 3 to the outside of the solar cell panel 10 and connecting to a terminal box or the like. For example, a plurality of solar cell elements 31 of the solar cell section 3 are connected to each other through a first wiring member 32 and a second wiring member 33. In addition, a third wiring member 34 is connected to the solar cell section 3.

[0085] The sheet 41s and the sheet 41t are sheets made of a resin (EVA, etc.) that is the material of the first filling material 41. The sheet 41s is located between the surface protection layer 1 and the solar cell section 3 and between the surface protection layer 1 and the support member 5. That is, the sheet 41s is located on the surface protection layer 1, and the solar cell section 3 and the support member 5 are located on the sheet 41s. When viewed from above, the sheet 41s has a rectangular shape as an example of a rectangular shape.

[0086] In a plan view, the sheet 41t is located on the sheet 41s between the support member 5 and the solar cell section 3. Figure 4 (b) and Figure 4 In the example of (c), two supporting members 5 are provided, and therefore two pieces 41t are provided. When viewed from above, each piece 41t has, for example, a strip-like shape that is long in the Y direction. Figure 4 (b) and Figure 4 In the example (c), the width of each sheet 41t is narrower than the distance between the support member 5 and the solar cell section 3. Figure 4 (b) and Figure 4In the example of (c), the sheet 41 t is provided in a state where it does not face both the supporting member 5 and the solar cell section 3 in the Z direction.

[0087] The sheet 42s and the sheet 42t are sheets made of a resin (EVA, etc.) that is the material of the second filling material 42. The sheet 42s and the sheet 42t may contain a pigment. The sheet 42s is located between the back protective layer 2 and the solar cell portion 3 and between the back protective layer 2 and the supporting member 5. That is, the sheet 42s is provided in a state where both ends thereof are opposed to the supporting member 5. When viewed from above, the sheet 42s has a rectangular shape as an example of a rectangular shape.

[0088] In a plan view, the sheet 42t is located on the sheet 42s between the support member 5 and the solar cell section 3. Figure 4 (b) and Figure 4 In the example of (c), two support members 5 are provided, so two pieces 42t are provided. When viewed from above, each piece 42t has a long strip shape that is long in the Y direction. Figure 4 (b) and Figure 4 In the example of (c), the width of each sheet 42t is narrower than the interval between the support member 5 and the solar cell section 3. Figure 4 (b) and Figure 4 In the example of (c), the sheet 42 t is provided in a state where it does not face both the supporting member 5 and the solar cell section 3 in the Z direction.

[0089] The back protection layer 2 is located on the sheet 42s and the sheet 42t.

[0090] As described above, in the laminate 10s, the sheet 41t and the sheet 42t are located between the support member 5 and the solar cell section 3 in a plan view. Therefore, the total thickness of the sheet between the support member 5 and the solar cell section 3 is greater than the total thickness of the sheet in the region facing the solar cell section 3 by the amount of the sheet 41t and the sheet 42t.

[0091] In addition, Figure 4 In the example of (c), the sheet 42s and the back surface protection layer 2 are shown in a flat plate shape, but when they have flexibility or softness, the center portion thereof bends toward the front surface protection layer 1 side.

[0092] Next, for example, a lamination process is performed on the stack 10s. Here, for example, a laminating device (laminator) is used to integrate the stack 10s. For example, in the laminator, the stack 10s is placed on a heating plate in a chamber, and the pressure in the chamber is reduced from 50 Pascals (Pa) to about 150 Pa, and the stack 10s is heated from 100 degrees Celsius (100°C) to about 200 degrees Celsius (200°C). At this time, the sheets 41s, 41t, 42s, and 42t are heated to a state where they can flow to a certain extent. In this state, in the chamber, the stack 10s is integrated by pressing the stack 10s in the Z direction with a pressing body such as a diaphragm.

[0093] As described above, in the lamination process, the sheet 41t and the sheet 42t are provided on the stacked body 10s. That is, the total thickness of the sheet increases between the support member 5 and the solar cell section 3. Therefore, the thickness of the filler 4 can be increased more easily between the support member 5 and the solar cell section 3.

[0094] Furthermore, if the sheet 41t and the sheet 42t are provided, the gap caused by the difference in thickness between the supporting member 5 and the solar cell element 31 can be reduced between the supporting member 5 and the solar cell section 3 in the stack 10s. As a result, the pressing body of the laminator can also press the stack 10s with sufficient pressure between the supporting member 5 and the solar cell section 3. In other words, the uneven pressure distribution caused by the difference in thickness between the supporting member 5 and the solar cell element 31 can be reduced. Therefore, the molten sheet can also press the surface protective layer 1, the supporting member 5, the solar cell section 3, and the back protective layer 2 with sufficient pressure between the supporting member 5 and the solar cell section 3. As a result, the filler 4 can bond these with a higher bonding strength.

[0095] In the above example, in the lamination process, the sheet 42t is located on the sheet 42s, but it may be located between the sheet 42s and the sheet 41t. In addition, the sheet 41t is located on the sheet 41s, but it may be located between the sheet 41s and the surface protection layer 1. In addition, between the solar cell section 3 and the support member 5, a plurality of sheets 41t may be stacked in the Z direction, or a plurality of sheets 42t may be stacked in the Z direction. In addition, only one of the sheet 41t and the sheet 42t may be provided.

[0096] In the above example, the sheet 41s and the sheet 41t are separate sheets, but they may be integrated. That is, the thickness of the sheet in the area between the support member 5 and the solar cell section 3 is greater than the thickness of the sheet in the area facing the solar cell section 3. The same applies to the sheet 42s and the sheet 42t.

[0097] After the lamination process, a terminal box or the like may be appropriately mounted on the solar cell panel 10. At this time, for example, wiring drawn from the solar cell section 3 to the outside of the solar cell panel 10 is appropriately connected to terminals in the terminal box. Thus, the solar cell module 100 is assembled.

[0098] In the above example, the solar cell panel 10 including the support member 5 is integrated by lamination. Therefore, the solar cell panel 10 is easier to assemble than a structure in which an external frame (not shown) is attached to the solar cell panel 10 by screws or the like instead of the support member 5.

[0099] <1-4. Second Specific Example of Manufacturing Solar Cell Module According to First Embodiment>

[0100] like Figure 5 (a) and Figure 5 As shown in (b), in the lamination process, the sheet 41t and the sheet 42t may not be provided on the laminate 10s. In this case, Figure 5 As shown in (b) of FIG. 1 , the pressing surface 400s of the pressing body 400 of the laminator may have a height difference shape. The pressing surface 400s is a surface that contacts the laminated body 1os to press the laminated body 1os.

[0101] exist Figure 5 In the example of (b), the pressing body 400 includes a diaphragm 410, a first release sheet 420, and a second release sheet 421. The material of the diaphragm 410 is an elastic member such as silicone rubber that is easily elastically deformed. The diaphragm 410 is larger than the stacked body 10s in a plan view and is provided in a state opposite to the entire stacked body 10s.

[0102] The first mold release sheet 420 is a mold release sheet, for example, a film for mold release such as a silicon coating can be formed on the surface of a sheet-like substrate. The first mold release sheet 420. The first mold release sheet 420 is located on the laminate 10s side relative to the membrane 410. The first mold release sheet 420 is arranged in a state of overlapping with the membrane 410. The first mold release sheet 420 is larger than the laminate 10s when viewed from above, and is arranged in a state opposite to the entire laminate 10s.

[0103] The second release sheet 421 is a sheet having a releasable property. For example, a film for release such as a silicon coating can be formed on the surface of a sheet-like substrate to obtain the second release sheet 421. The second release sheet 421 is located on the laminate 10s side relative to the first release sheet 420. The second release sheet 421 is provided in a state of overlapping with the first release sheet 420.

[0104] When viewed from above, the second release sheet 421 has, for example, a strip-like shape that is long in the Y direction. The width of the second release sheet 421 in the X direction is narrower than the interval between the two support members 5 and is greater than the width of the solar cell section 3. The second release sheet 421 is in a state of being opposed to the stacked body 10s in the Z direction between the two support members 5, and is not opposed to the support member 5 in the Z direction. In addition, the second release sheet 421 is in a state of being opposed to the entire solar cell section 3 in the Z direction. The length of the second release sheet 421 in the Y direction is, for example, greater than the length of the stacked body 10s in the Y direction.

[0105] The thickness of such a pressing body 400 is smaller in the region opposite to the supporting member 5 in the Z-axis direction, and is larger in the region opposite to the solar cell section 3 in the Z-axis direction. For this reason, the surface of the pressing body 400 on the stacking body 10s side, i.e., the pressing surface 400s, has a height difference on both sides of the second release sheet 421, and the portion of the pressing surface 400s corresponding to the second release sheet 421 protrudes toward the stacking body 10s side by the thickness of the second release sheet 421. In other words, the pressing surface 400s has a first region 401s opposite to the supporting member 5, and a second region 402s located closer to the stacking body 10s side than the first region 401s and corresponding to the solar cell section 3, and the height difference between the first region 401s and the second region 402s is located between the supporting member 5 and the solar cell section 3 in the X-axis direction. The pressing surface 400s of such a pressing body 400 has a height difference on both sides of the second release sheet 421. Figure 2 The illustrated filler material 4 has a thickness distribution corresponding to the height difference shape.

[0106] In the lamination process, the pressing body 400 initially presses the back protective layer 2 at the second region (i.e., the second release sheet 421) facing the solar cell section 3, and then presses the back protective layer 2 at the first region on the side of the support member 5. Therefore, the molten sheet easily flows toward the support member 5 side and flows between the support member 5 and the solar cell section 3. Therefore, the thickness of the filling material 4 between the support member 5 and the solar cell section 3 can be easily increased.

[0107] In addition, since the melted sheet flows into between the support member 5 and the solar cell section 3, the volume of the sheet between the support member 5 and the solar cell section 3 increases, and the pressing body 400 can press the laminate 10s with a more uniform pressure distribution. As a result, between the support member 5 and the solar cell section 3, the filler 4 also bonds the surface protection layer 1, the support member 5, the solar cell section 3, and the back protection layer 2 with a higher bonding strength.

[0108] <1-5. Summary of the First Implementation Method>

[0109] In the solar cell module 100 according to the first embodiment, for example, the thickness W1 of the filler 4 between the support member 5 and the solar cell section 3 is greater than the thickness W3 of the filler 4 between the solar cell elements 31. For this reason, the strength of the solar cell panel 10 can be improved between the support member 5 and the solar cell section 3. As a result, the solar cell panel 10 can withstand the stress applied to the portion between the support member 5 and the solar cell section 3 due to the deflection caused by the external force F1. In addition, since the thickness W3 is small, the flexibility of the solar cell panel 10 can be improved.

[0110] <1-6. Number of Solar Cell Element Arrangements>

[0111] exist Figure 1 In the example, the number of solar cell elements 31 arranged in the X direction is 2, which is an even number. In other words, the number of solar cell elements 31 arranged in the direction perpendicular to the long side direction of the support member 5 is an even number. In addition, the widths of the solar cell elements 31 in the X direction are substantially equal to each other. For this reason, there is no solar cell element 31 in the center of the solar cell panel 10 in the X direction. That is, the center of the solar cell panel 10 corresponds to the portion between the solar cell elements 31.

[0112] However, when the solar cell panel 10 is bent by the external force F1 (see also Figure 6 ), a relatively large stress is also applied to the center of the solar cell panel 10 in the X direction. In addition, when a load such as snow is applied to the solar cell panel 10 while the supporting member 5 is mounted on the mounting object member, the solar cell panel 10 will also bend in an arc shape when viewed from the Y direction. In such a case, a relatively large stress is also applied to the center of the solar cell panel 10 in the X direction.

[0113] exist Figure 1 In the example of , there is no solar cell element 31 in the center of the solar cell panel 10. Therefore, even when the solar cell panel 10 is bent by an external force F1 or a load such as snow, the stress applied to each solar cell element 31 is relatively small. Therefore, the possibility of adverse conditions such as performance degradation of the solar cell element 31 caused by stress can be reduced.

[0114] <2. Other Implementation Methods>

[0115] The present disclosure is not limited to the above-described first embodiment, and various changes and improvements can be made without departing from the gist of the present disclosure.

[0116] <2-1. Second Embodiment>

[0117] <2-1-1. Solar cell module>

[0118] In the first embodiment described above, for example, Figure 7 as well as Figure 8 As shown, the portion (corresponding to the first portion) 4b between the support member 5 and the surface protection layer 1 in the filler 4 may have a thickness distribution (corresponding to a given first thickness distribution) described below. The first thickness distribution is a thickness distribution in which the thickness W4 at the end of the solar cell section 3 side of the portion 4b is greater than the thickness W5 at the end of the outer portion 52 side of the portion 4b. The difference between the thickness W4 and the thickness W5 may be, for example, 0.01 mm or more, 0.05 mm or more, or 0.1 mm or more.

[0119] like Figure 7 as well as Figure 8 As shown, the thickness of the portion 4b of the filling material 4 can gradually decrease as it goes from the inner end face 5a to the outer end face 5b in at least the region R2 among the regions opposite to the support member 5 in the Z direction. The outer end face 5b mentioned here is the end face of the support member 5 on the side opposite to the solar cell portion 3 in the X direction. It can also be said that the thickness of the portion 4b can decrease monotonically as it goes from the inner end face 5a to the outer end face 5b in the region R2. The reduction in thickness in the entire region R2 can be, for example, more than 0.01 mm, more than 0.05 mm, or more than 0.1 mm.

[0120] exist Figure 7 as well as Figure 8 In the example, the thickness of the portion 4a of the filler 4 gradually increases as it goes from the solar cell portion 3 to the support member 5, and the thickness of the portion 4b of the filler 4 gradually decreases as it goes from the inner end face 5a to the outer end face 5b. For this reason, the first surface 4f of the filler 4 has a convex shape bulging toward the +Z direction near the inner end face 5a of the support member 5. Specifically, the first surface 4f bulges into a smooth mountain shape, for example. The shapes of the portions 4a and 4b of the filler 4 are the same, for example, in the Y direction.

[0121] like Figure 7 as well as Figure 8 As shown, the portion (corresponding to the second portion) 4c between the support member 5 and the back protective layer 2 in the filler 4 may also have a thickness distribution (corresponding to the second thickness distribution) described below. The second thickness distribution is a thickness distribution in which the thickness W6 at the end of the portion 4c on the solar cell section 3 side is greater than the thickness W7 at the end of the portion 4c on the outer portion 52 side. The difference between the thickness W6 and the thickness W7 may be, for example, 0.01 mm or more, 0.05 mm or more, or 0.1 mm or more.

[0122] like Figure 7 as well as Figure 8 As shown, the thickness of the portion 4c of the filling material 4 may gradually decrease from the inner end face 5a to the outer end face 5b in at least the region R3 among the regions that are opposite to the supporting member 5 in the Z direction. In other words, the thickness of the portion 4c may decrease monotonically from the inner end face 5a to the outer end face 5b in the region R3. The amount of reduction in the thickness of the entire region R3 may be, for example, greater than 0.01 mm, greater than 0.05 mm, or greater than 0.1 mm. In addition, in Figure 7 as well as Figure 8 In the example, the second surface 4s of the filling material 4 has a convex shape bulging in the -Z direction near the inner end surface 5a of the support member 5. Specifically, the second surface 4s bulges into a smooth mountain shape, for example. The shape of the portion 4c of the filling material 4 is the same in the Y direction, for example.

[0123] Here, the description will focus on the distance between the surface protective layer 1 and the back protective layer 2. That is, the distance between the surface protective layer 1 and the back protective layer 2 at the position of the inner end surface 5a of the support member 5 is larger than the distance between the surface protective layer 1 and the back protective layer 2 at the end in the X direction of the surface protective layer 1 or the end in the X direction of the back protective layer 2. The distance between the surface protective layer 1 and the back protective layer 2 is the largest near the inner end surface 5a of the support member 5.

[0124] In addition, the thickness of the structure composed of the filler 4 and the support member 5 is described. That is, the thickness of the structure at the position of the inner end surface 5a of the support member 5 is greater than the thickness of the structure at the end of the surface protection layer 1 in the X direction or the end of the back protection layer 2 in the X direction. The thickness of the structure becomes the largest near the inner end surface 5a of the support member 5.

[0125] <2-1-2. Characteristics of Solar Cell Modules>

[0126] According to the second embodiment, the thickness W4 of the portion 4b of the filling material 4 is greater than the thickness W5. For this reason, the thickness of the solar cell panel 10 near the inner end surface 5a of the support member 5 can be further increased, and the strength of the solar cell panel 10 near the inner end surface 5a can be further improved. Therefore, even if the external force F1 is increased and the solar cell panel 10 is bent more, the solar cell panel 10 can withstand the stress. In addition, since the thickness W5 of the filling material 4 is less than the thickness W4, the material cost of the filling material 4 can be reduced compared to a structure in which the thickness W5 of the filling material 4 is increased to the same degree as the thickness W4.

[0127] exist Figure 7 as well as Figure 8In the example, the thickness W6 of the portion 4c of the filling material 4 is greater than the thickness W7. For this reason, the thickness of the solar cell panel 10 near the inner end surface 5a of the support member 5 can be further increased, and the strength of the solar cell panel 10 near the inner end surface 5a can be further improved. Therefore, even if the external force F1 is increased to cause the solar cell panel 10 to bend more, the solar cell panel 10 can withstand its stress. In addition, since the thickness W7 of the filling material 4 is less than the thickness W6, the material cost of the filling material 4 can be reduced compared to a structure in which the thickness W7 of the filling material 4 is increased to the same degree as the thickness W6.

[0128] In addition, Figure 7 as well as Figure 8 In the example shown in FIG. 1 , the first surface 4 f and the second surface 4 s of the filler 4 have shapes that are line-symmetrical with respect to the XY plane. However, the drawings are merely schematic illustrations and the present invention is not necessarily limited to this.

[0129] In addition, for example, the thickness of either part 4b or part 4c of the filling material 4 may be uniform. That is, either part 4b or part 4c may have a flat plate shape with uniform thickness. This is because if either part 4b or part 4c has the above-mentioned thickness distribution, the strength of the solar cell panel 10 can be improved near the inner end surface 5a.

[0130] <2-1-3. First Specific Example of the Method for Manufacturing the Solar Cell Module According to the Second Embodiment>

[0131] based on Fig. 9 (a) and Fig. 9 (b) will be used to describe an example of a lamination process in the method for manufacturing the solar cell module 100 according to the second embodiment.

[0132] For example, Fig. 9 (a) and Fig. 9 As shown in (b), the laminate 10s is formed by laminating the surface protection layer 1, the sheet 41s, the sheet 41u, the solar cell section 3, the support member 5, the sheet 42s, the sheet 42u and the back protection layer 2. That is, compared with the first specific example of the first embodiment, the sheet 41u and the sheet 42u are used instead of the sheet 41t and the sheet 42t.

[0133] The sheet 41u is a sheet made of a resin (EVA, etc.) that is a part of the material of the first filler 41. The sheet 41u is located on the sheet 41s, for example. Fig. 9 (a) and Fig. 9In the example (b), since two supporting members 5 are provided, two sheets 41u are provided. When viewed from above, each sheet 41u has, for example, a strip-like shape that is long in the Y direction. The sheet 41u is located in the area that spans the inner end surface 5a of the supporting member 5 in the X direction. That is, the outer portion of the sheet 41u in the X direction is located between the surface protection layer 1 and the supporting member 5, and the inner portion of the sheet 41u in the X direction is located further inward than the inner end surface 5a of the supporting member 5. The inner portion of the sheet 41u is provided, for example, in a state that it is not opposed to the solar cell portion 3 in the Z direction. In addition, the outer end of the sheet 41u in the X direction is located inwardly relative to, for example, the end of the surface protection layer 1 in the X direction and the end of the sheet 41s.

[0134] The sheet 42u is a sheet made of a resin (EVA, etc.) that is a part of the material of the second filling material 42. The sheet 42u is located on the sheet 42s, for example. Fig. 9 (a) and Fig. 9 In the example of (b), two supporting members 5 are provided, and therefore two sheets 42u are provided. When observed from above, each sheet 42u has, for example, a long strip shape that is long in the Y direction. The sheet 42u is located in the area that spans the inner end surface 5a of the supporting member 5 in the X direction. That is, the outer portion of the sheet 42u in the X direction is located between the back protective layer 2 and the supporting member 5, and the inner portion of the sheet 42u in the X direction is located further inward than the inner end surface 5a of the supporting member 5. The inner portion of the sheet 42u is provided, for example, in a state that it is not opposed to the solar cell portion 3 in the Z direction. In addition, the outer end of the sheet 42u in the X direction is located inwardly relative to, for example, the end of the back protective layer 2 in the X direction and the end of the sheet 42s.

[0135] Next, for example, a lamination process is performed on the laminated body 10s. Here, for example, a laminating device (laminator) is used to integrate the laminated body 10s. In this way, the laminated body 10s can be manufactured. Figure 7 as well as Figure 8 A solar cell panel 10 is shown.

[0136] In the laminated body 10s, the sheet 41u is provided in a state of straddling the inner end surface 5a of the support member 5. Therefore, the thickness W4 of the portion 4b of the filler material 4 can be increased more easily. In addition, since the outer end of the sheet 41u is located inside the end of the surface protection layer 1 and the end of the sheet 41s in a plan view, the thickness W5 of the portion 4b can be reduced more easily than the thickness W4.

[0137] In the laminate 10s, the sheet 42u is provided so as to straddle the inner end surface 5a of the support member 5. Therefore, the thickness W6 of the portion 4c of the filler material 4 can be increased more easily. In addition, since the outer end of the sheet 42u is located inside the end of the back protective layer 2 and the end of the sheet 41s in a plan view, the thickness W7 of the portion 4c can be reduced more easily than the thickness W6.

[0138] <2-1-4. Second Specific Example of the Method for Manufacturing the Solar Cell Module According to the Second Embodiment>

[0139] like Fig.10 (a) and Fig.10 As shown in (b), in the lamination process, the sheet 41u and the sheet 42u may not be provided on the laminate 1os. In this case, Fig.10 As shown in (b) of FIG. 4 , the pressing surface 400s of the pressing body 400 may have a height difference shape. Fig.10 In the example of (b), the pressing body 400 and Figure 5 Compared with the pressing body 400 of (b), it further includes a third release sheet 422.

[0140] The third release sheet 422 is a sheet having a releasable property. For example, a film for release such as a silicon coating can be formed on the surface of a sheet-like substrate to obtain the third release sheet 422. The third release sheet 422 is located on the laminate 10s side relative to the first release sheet 420. The third release sheet 422 is provided in a state of overlapping with the first release sheet 420.

[0141] exist Fig.10 In the example of (b), since two supporting members 5 are provided in the laminate 10s, two third release sheets 422 are provided. The third release sheet 422 has, for example, a strip-shaped shape that is long in the Y direction, and is provided in a state that is opposed to the end of the back protective layer 2 in the X direction in the Z direction. The inner end 422a of the third release sheet 422 on the second release sheet 421 side is located between the end of the back protective layer 2 and the inner end surface 5a of the supporting member 5 in the X direction. The outer end 422b of the third release sheet 422 on the side opposite to the second release sheet 421 is located outside relative to the end of the back protective layer 2 in the X direction.

[0142] The thickness of such a pressing body 400 is smaller in the area opposite to the inner end surface 5a of the supporting member 5 in the Z direction. For this reason, the pressing surface 400s of the pressing body 400 has a concave shape in the area opposite to the inner end surface 5a of the supporting member 5 in the Z direction. More specifically, the pressing surface 400s has: a first area 401s opposite to the inner end surface 5a of the supporting member 5; a second area 402s located closer to the stack 1os side than the first area 401s and opposite to the solar cell portion 3; and a third area 403s located closer to the stack 10s side than the first area 401s and opposite to the end of the back protective layer 2. The pressing surface 400s of such a pressing body 400 has a concave shape opposite to the inner end surface 5a of the supporting member 5. Figure 7 as well as Figure 8 The illustrated filler material 4 has a thickness distribution corresponding to the height difference shape.

[0143] Such a pressing body 400 presses the regions at both ends of the back protective layer 2 in the X direction and the region facing the solar cell section 3 during the lamination process, and then presses the back protective layer 2 in the region near the inner end surface 5a of the support member 5. For this reason, the molten sheet flows from both sides in the X direction to the vicinity of each inner end surface 5a. As a result, the thickness of the filler 4 can be easily increased near the inner end surface 5a of the support member 5.

[0144] In addition, in the laminator, the support surface of the support body (not shown) supporting the surface protection layer 1 may have the same height difference shape as the pressing surface 400s of the pressing body 400. That is, the support body may include the first release sheet 420, the second release sheet 421, and the third release sheet 422 of the pressing body 400 in a reversed state.

[0145] <2-2. Third embodiment>

[0146] <2-2-1. Solar cell module>

[0147] In the first embodiment and the second embodiment, Fig.11 As shown, the end 2a of the back protective layer 2 in the X direction can be located on the solar cell portion 3 side relative to the end 1a of the surface protective layer 1 in the X direction. End 1a can be said to be an end on the supporting member 5 side of the surface protective layer 1, and end 2a can be said to be an end on the supporting member 5 side of the back protective layer 2. More specifically, the end 2a of the back protective layer 2 in the -X direction can be located on the solar cell portion 3 side relative to the end 1a of the surface protective layer 1 in the -X direction, and the end 2a of the back protective layer 2 in the +X direction can be located on the solar cell portion 3 side relative to the end 1a of the surface protective layer 1 in the +X direction. In other words, the width of the back protective layer 2 in the X direction can be smaller than the width of the surface protective layer 1 in the X direction. In addition, as Fig.11As shown in the figure, the end 42a of the filler 4 on the back protective layer 2 side and the outer part 52 side may be located on the solar cell section 3 side relative to the end 41a of the filler 4 on the surface protective layer 1 side and the outer part 52 side. Specifically, the end 42a of the filler 4 in the -X direction and -Z direction is located on the solar cell section 3 side relative to the end 41a of the filler 4 in the -X direction and +Z direction, and the end 42a of the filler 4 in the +X direction and -Z direction is located on the solar cell section 3 side relative to the end 41a of the filler 4 in the +X direction and +Z direction.

[0148] As a more specific example, Fig.11 As shown in the figure, the back protection layer 2 can be provided avoiding the region facing each supporting member 5 in the Z direction, and the filling material 4 can be provided avoiding the region facing each supporting member 5 in the Z direction, which is closer to the -Z direction (i.e., the side opposite to the surface protection layer 1) than each supporting member 5. That is, the filling material 4 and the back protection layer 2 may not be provided in the region facing the supporting member 5 in the Z direction, which is closer to the -Z direction than the supporting member 5.

[0149] In such a structure, the entire surface of the support member 5 in the -Z direction is exposed to the outside of the solar cell module 100. Fig.11 In the example of FIG. 1 , the mounting target member 300 to which the support member 5 in the +X direction is fixed and the fastening member 301 to which they are fixed are shown by virtual lines. Fig.11 In the example, the mounting object member 300 is opposed to the supporting member 5 in the Z direction and contacts the supporting member 5. The fastening member 301 is, for example, a screw that penetrates the supporting member 5 in the Z direction. The supporting member 5 can be pressed against the mounting object member 300 and fixed by the fastening member 301. Fig.11 Although not shown in the figure, the supporting member 5 in the −X direction can be attached to the attachment target member in the same manner as the supporting member 5 in the +X direction, for example.

[0150] exist Fig.11 In the example of , the filler 4 and the back protection layer 2 are not provided between the installation object member 300 and the support member 5. Therefore, even if the thickness of the filler 4 and the back protection layer 2 changes due to the thermal expansion, thermal contraction, and aging degradation of the filler 4 and the back protection layer 2, the interval between the support member 5 and the installation object member 300 does not change. Therefore, the loosening of the fastening member 301 caused by the change in the thickness of the filler 4 and the back protection layer 2 can be suppressed, and the solar cell module 100 can be more firmly fixed to the installation object member 300 with higher reliability.

[0151] Furthermore, since the facing area between the support member 5 and the mounting object member 300 can be increased, the support member 5 can be more firmly fixed to the mounting object member 300. In other words, since the facing area between the support member 5 and the mounting object member 300 can be ensured even if the width of the support member 5 in the X direction is narrowed, the solar cell module 100 can be miniaturized.

[0152] In addition, Fig.11 In the example of , a part of the filling material 4 is provided between the surface protection layer 1 and each supporting member 5. Therefore, even if water such as rain water falls from the external space 200 to the front face 10f of the solar cell panel 10, it is difficult for the water to enter between the surface protection layer 1 and each supporting member 5. On the other hand, since it is difficult for rain water to reach the back face 10b of the solar cell panel 10, the amount of water entering between the back face protection layer 2 and each supporting member 5 is originally small. Therefore, the solar cell section 3 can also be appropriately protected from water.

[0153] <2-2-2. Method for manufacturing solar cell module according to third embodiment>

[0154] Next, based on Fig.12 (a) and Fig.12 (b) will be used to describe an example of a lamination process in the method for manufacturing the solar cell module 100 according to the third embodiment.

[0155] For example, Fig.12 (a) and Fig.12 As shown in (b), the surface protection layer 1, the sheet 41s, the sheet 41t, the solar cell unit 3, the support member 5, the sheet 42s, the sheet 42t and the back protection layer 2 are stacked to form a stacked body 1os. Fig.12 (a) and Fig.12 As shown in (b), in the laminated body 10s involved in the third embodiment, the sheet 42s that is the material of the filler 4 is not provided between the support member 5 and the back protective layer 2. That is, the width of the sheet 42s in the X direction is smaller than the width of the sheet 41s in the X direction, more specifically, smaller than the interval between the two support members 5. In addition, the width of the sheet 42s is wider than the width of the solar cell section 3 in the X direction. The sheet 42s is provided in a state of being opposed to the solar cell section 3 in the Z direction and not being opposed to the support member 5 in the Z direction.

[0156] In addition, if Fig.12 (a) and Fig.12As shown in (b), the width of the back protective layer 2 in the X direction is narrower than the width of the surface protective layer 1 in the X direction. The width of the back protective layer 2 in the X direction may be, for example, the same as the interval between the two supporting members 5, or may be narrower than the interval. In other examples described later, the width of the back protective layer 2 in the X direction may be wider than the interval between the supporting members 5 and narrower than the width of the surface protective layer 1 in the X direction.

[0157] Next, for example, a lamination process is performed on the laminated body 10s. Here, for example, a laminating device (laminator) is used to integrate the laminated body 10s. In this way, the laminated body 10s can be manufactured. Fig.11 A solar cell panel 10 is shown.

[0158] In addition, Fig.12 (a) and Fig.12 In the example of (b), the sheet 41t and the sheet 42t are provided, but for example, Figure 5 (a) and Figure 5 As shown in (b), the sheet 41t and the sheet 42t are not provided. In this case, the width of the sheet 42s is also set to Fig.12 (a) and Fig.12 The width shown in (b).

[0159] <2-2-3. Other examples of the third embodiment>

[0160] exist Fig.11 In the example, the filler 4 and the back protection layer 2 are not located in the entire region opposite to each supporting member 5 in the -Z direction. However, the present invention is not limited thereto. The back protection layer 2 and a portion of the filler 4 may be located in the region. Fig.11 In the example, on the side of the support member 5 in the -X direction, a portion of the filler 4 and a portion of the back protective layer 2 are indicated by a two-dot chain line as being located in the region. In this case, too, when viewed from above, the end 2a of the back protective layer 2 in the -X direction is located on the solar cell section 3 side relative to the end 1a of the surface protective layer 1 in the -X direction, and the end 42a of the filler 4 on the back protective layer 2 side and the outer portion 52 side is located on the solar cell section 3 side relative to the end 41a of the filler 4 on the surface protective layer 1 side and the outer portion 52 side. In addition, although Fig.11 Although not shown in the figure, on the side of the supporting member 5 in the +X direction, a part of the filling material 4 and a part of the back surface protection layer 2 are also provided in this region.

[0161] Such a structure can also increase the area of ​​the portion of each supporting member 5 exposed on the back protective layer 2 side. For this reason, the opposing area between the supporting member 5 and the installation target member can be increased, and the solar cell module 100 can be more firmly fixed to the installation target member. Alternatively, even if the width of the supporting member 5 in the X direction is narrowed in the solar cell module 100, the opposing area between the supporting member 5 and the installation target member can be ensured, so the solar cell module 100 can be miniaturized.

[0162] <2-3. Fourth embodiment>

[0163] In the above-mentioned first embodiment to the above-mentioned third embodiment, Fig.13 (a) and Fig.13 As shown in (b) of FIG. 1 , a plurality of support members 5 may be arranged side by side with a gap in the Y direction. Fig.13 In the example (a), four supporting members 5 are arranged in the Y direction on both sides of the solar cell panel 10 in the X direction. That is, the four supporting members 5 are arranged side by side with a gap in the Y direction at the end portion of the solar cell panel 10 extending in the Y direction, which is the end portion of the solar cell panel 10 in the -X direction, and the other four supporting members 5 are arranged side by side with a gap in the Y direction at the end portion of the solar cell panel 10 extending in the Y direction, which is the end portion of the solar cell panel 10 in the +X direction. Fig.13 In the example (a), the four support members 5 on one side of the solar cell panel 10 are arranged in a state of facing the four support members 5 on the other side of the solar cell panel 10 in the X direction. That is, the eight support members 5 are arranged in a matrix of 4 rows and 2 columns.

[0164] refer to Fig.13 (b) shows the thickness of the portion 4d between two adjacent support members 5 in the Y direction of the filling material 4 (equivalent to the third portion). The portion 4d may have a thickness distribution (equivalent to the third thickness distribution) described below. The third thickness distribution is a thickness distribution in which the thickness W8 of the portion 4d at the end of one side of two adjacent support members 5 is greater than the thickness W9 of the portion 4d at the center between the two support members 5. The difference between the thickness W8 and the thickness W9 may be, for example, greater than 0.1 mm, greater than 0.5 mm, or greater than 1 mm.

[0165] exist Fig.13 In the example (b), the portion 4 d of the filling material 4 has a thickness distribution in which the thickness gradually decreases toward the center between the two supporting members 5 in at least a partial region R4 between two supporting members 5 adjacent in the Y direction.

[0166] According to the fourth embodiment, since the plurality of support members 5 are arranged side by side with a gap in the Y direction, the solar cell panel 10 can be bent in an arc shape when viewed with the line of sight along the X direction. In this bent state, a greater stress is generated in the solar cell panel 10 near the end faces 5c on both sides of the Y direction of each support member 5. The end faces 5c on both sides of the Y direction mentioned here include: the end face 5c of the support member 5 located on one side of the Y direction and intersecting the Y direction; and the end face 5c of the support member 5 located on the other side of the Y direction and intersecting the Y direction.

[0167] like Fig.13 As shown in (b), the thickness of the portion 4d of the filling material 4 is larger on the side of the supporting member 5 and smaller in the center between the supporting members 5. For this reason, the strength of the solar cell panel 10 can be improved near the end surface 5c of the supporting member 5. Therefore, the solar cell panel 10 can cope with the stress caused by the above-mentioned deflection. In addition, since the filling material 4 is thinner in the center between the supporting members 5, the flexibility of the solar cell panel 10 can also be improved. In addition, compared to the structure in which the thickness W9 is increased to the same level as the thickness W8, the material cost of the filling material 4 can also be reduced.

[0168] For example, in the lamination process, by newly providing a resin sheet that is the material of the filler 4 only at the end portion between the supporting members 5, the thickness distribution of the portion 4d of the filler 4 can be easily achieved. Alternatively, in the lamination process, for example, by forming a height difference shape corresponding to the thickness distribution of the portion 4d as the pressing surface 400s of the pressing body 400, the thickness distribution of the portion 4d can be achieved.

[0169] In addition, similar to the second embodiment, the first surface 4f of the filling material 4 can have a convex shape bulging in the +Z direction near the end surface 5c of the supporting member 5, and the second surface 4s of the filling material 4 can have a convex shape bulging in the -Z direction near the end surface 5c of the supporting member 5.

[0170] <2-4. Fifth embodiment>

[0171] In the above-mentioned first embodiment to the above-mentioned fourth embodiment, as Fig.14 As shown in FIG. 1 , the support member 5 may be located only on one side of the rectangular solar cell panel 10. In other words, the support member 5 may be located only on the rectangular surface protection layer 1 and the back surface protection layer 2. Fig.14In the example, the support member 5 is provided only on one side of the solar cell panel 10 in the -X direction. Even with this structure, the rigidity of the solar cell panel 10 can be improved compared to a structure without the support member 5. In addition, the solar cell panel 10 is integrated by lamination. Therefore, the solar cell panel 10 is easy to assemble.

[0172] Furthermore, since the support members 5 are not provided on three sides of the solar cell panel 10, the solar cell panel 10 can be easily bent in more directions. That is, the flexibility of the solar cell panel 10 can be improved.

[0173] <2-5. Sixth Implementation Method>

[0174] In the above-mentioned first embodiment to the above-mentioned fifth embodiment, for example, Fig.15 (a) and Fig.15 As shown in (b) of FIG. 1 , the solar cell module 100 may further include a reinforcing fiber member 60. The reinforcing fiber member 60 includes, for example, aramid fibers such as Kevlar fibers (registered trademark) and fiber members such as carbon fibers, and is provided between the surface protection layer 1 and the back protection layer 2 in a state covered by the filling material 4. For example, the entire reinforcing fiber member 60 is covered by the filling material 4. Fig.15 In the example of (a), the reinforcing fiber member 60 is provided along the side of the solar cell panel 10 where the supporting member 5 is not provided. Fig.15 In the example of (a), since the two supporting members 5 are respectively located on the sides of the solar cell panel 10 in the X direction (equivalent to the first side), the two reinforcing fiber members 60 are respectively located on the sides of the solar cell panel 10 in the Y direction (equivalent to the second side). The so-called sides of the X direction include: one side located at the end of the solar cell panel 10 in the -X direction and extending in the Y direction; and one side located at the end of the solar cell panel 10 in the +X direction and extending in the Y direction. The so-called sides of the Y direction include: one side located at the end of the solar cell panel 10 in the -Y direction and extending in the X direction; and one side located at the end of the solar cell panel 10 in the +Y direction and extending in the X direction. The reinforcing fiber member 60 has a long strip shape in the X direction and is arranged in a state that does not overlap with the solar cell section 3 when viewed from above. That is, the reinforcing fiber member 60 is arranged in a state that does not face the solar cell section 3 in the Z direction.

[0175] The length of the longitudinal direction of the reinforcing fiber member 60 (ji, the length in the X direction) may be, for example, more than 1 / 2, more than 2 / 3, or more than 3 / 4 of the width in the X direction of the solar cell panel 10. Both ends of the reinforcing fiber member 60 in the X direction may abut against the supporting member 5, respectively.

[0176] The reinforcing fiber member 60 is easy to deform, but has high strength. Therefore, the reinforcing fiber member 60 can improve the strength of the solar cell panel 10 without reducing its flexibility. Fig.15 In the example (a), since the reinforcing fiber member 60 is located at the edge of the solar cell panel 10 where the supporting member 5 is not provided, the portion with low strength can be improved by the reinforcing fiber member 60. Therefore, the strength in the peripheral area of ​​the solar cell panel 10 can be improved as a whole by the supporting member 5 and the reinforcing fiber member 60.

[0177] <2-6. Seventh Implementation Method>

[0178] In the above-mentioned first embodiment to the above-mentioned sixth embodiment, for example, Fig.16 (a) to Fig.17 As shown in (b), the solar cell section 3 can be changed to a solar cell section 3B having a plurality of thin film solar cell regions 31B each including a thin film semiconductor and a transparent electrode. The thin film semiconductor includes, for example, a silicon-based, compound-based, or other type of semiconductor. The silicon-based thin film semiconductor uses, for example, a semiconductor utilizing amorphous silicon or thin film polycrystalline silicon. The compound-based thin film semiconductor uses, for example, a compound semiconductor having a chalcopyrite structure such as a CIS semiconductor or a CIGS semiconductor, a compound semiconductor having a perovskite structure, a compound semiconductor having a kesterite structure, or a cadmium telluride (CdTe) semiconductor. The CIS semiconductor is a compound semiconductor comprising copper (Cu), indium (In), and selenium (Se). The CIGS semiconductor is a compound semiconductor comprising Cu, In, gallium (Ga), and Se. Here, an example of providing a plurality of thin film solar cell regions 31B on the substrate 6 is given for illustration.

[0179] like Fig.16 (a) to Fig.17 As shown in (b), the solar cell section 3B has: a substrate 6; and a plurality of solar cell regions 31B arranged in a plane on the substrate 6. Here, the so-called plane arrangement means that the plurality of solar cell regions 31B are arranged along a virtual or actual plane, and the plurality of solar cell regions 31B are arranged in a plane. Fig.17 (a) and Fig.17In the example (b), a plurality of solar cell regions 31B are arranged side by side on the substrate 6 along the surface of the substrate 6. The substrate 6 is, for example, a transparent glass substrate having a thickness of about 0.5 mm to 2 mm. Here, for example, it is assumed that the solar cell section 3B includes N (N is a natural number greater than 2) solar cell regions 31B. In this case, for example, if the N solar cell regions 31B are electrically connected in series, the larger the value N, the larger the output voltage of the solar cell section 3B. Fig.17 (a) and Fig.17 In (b), an example of arranging a plurality of (seven in this case) solar cell regions 31B in the +Y direction is shown. Here, for example, each solar cell region 31B has an elongated shape with a long side in the +X direction. In this case, for example, if the width of the solar cell region 31B in the +Y direction is several millimeters (mm) to 1 centimeter (cm), dozens to hundreds of solar cell regions 31B can be arranged in parallel in the solar cell section 3B.

[0180] The plurality of solar cell regions 31B are respectively as follows, for example Fig.17 As shown in (b), the first electrode layer 8a, the semiconductor layer 8b and the second electrode layer 8c are provided. In addition, in the solar cell section 3B, for example, Fig.17 As shown in (b), there are connecting portions 9 and transparent portions 7 between adjacent solar cell regions 31B. Here, for example, if the second electrode layer 8c is a layer (also referred to as a translucent electrode layer) having a higher light transmittance than the semiconductor layer 8b for light of a specific range of wavelengths, then in each solar cell region 31B, the incident light will pass through the second electrode layer 8c. Thus, for example, the incident light passing through the surface protective layer 1 will pass through the second electrode layer 8c and irradiate the semiconductor layer 8b. At this time, for example, the incident light will be absorbed in the semiconductor layer 8b. Here, for example, in the case where the back protective layer 2 contains a translucent material like the surface protective layer 1, if the first electrode layer 8a is a layer (translucent electrode layer) having a higher light transmittance than the semiconductor layer 8b for light of a specific range of wavelengths, then the incident light passing through the back protective layer 2 will pass through the first electrode layer 8a and irradiate the semiconductor layer 8b.

[0181] The first electrode layer 8a is, for example, located on the surface of the substrate 6 facing the +Z direction. The first electrode layer 8a is, for example, an electrode (also referred to as a first electrode) that can collect charges generated by photoelectric conversion corresponding to light irradiation in the semiconductor layer 8b. If the material of the first electrode layer 8a is, for example, a transparent conductive oxide (TCO: Transparent Conductive Oxide) that is translucent to light in a specific range of wavelengths, the light in the specific range of wavelengths will pass through the back protective layer 2 and the first electrode layer 8a and enter the semiconductor layer 8b. TCO includes, for example, indium tin oxide (ITO: Indium Tin Oxide), fluorine-doped tin oxide (FTO: Fluorine-doped tin oxide) or zinc oxide (ZnO). When zinc oxide is used as TCO, TCO may contain aluminum (A1), boron (B) or gallium (Ga) as needed. Fig.17 In the example of (b), seven first electrode layers 8a are arranged side by side along the +Y direction plane on the substrate 6. Here, the first electrode layer 8a of the mth solar cell region 31Bm (m is a natural number from 1 to 6) and the portion of the first electrode layer 8a of the (m+1)th solar cell region 31B(m+1) extending to the mth solar cell region 31Bm are arranged side by side with a gap (also referred to as the first gap) G1 sandwiched therebetween. For example, the first electrode layer 8a of the first solar cell region 31B1 and the portion of the first electrode layer 8a of the second solar cell region 31B2 extending to the first solar cell region 31B1 are arranged side by side with the first gap G1 sandwiched therebetween. Each first gap G1 has a long side direction along the +X direction. Here, in each first gap G1, there is a first groove portion P1 with the surface of the substrate 6 as the bottom surface.

[0182] The semiconductor layer 8b is located between the first electrode layer 8a and the second electrode layer 8c. Here, the semiconductor layer 8b of the mth solar cell region 31Bm is provided in a state where it extends to the end of the portion of the first electrode layer 8a of the (m+1)th solar cell region 31B(m+1) extending in the -Y direction next to it in the +Y direction. For example, the semiconductor layer 8b of the first solar cell region 31B1 is provided in a state where it extends to the end of the portion of the first electrode layer 8a of the second solar cell region 31B2 extending in the -Y direction next to it. The semiconductor layer 8b contains, for example, the above-mentioned thin film semiconductor.

[0183] The second electrode layer 8c is located on the semiconductor layer 8b. The second electrode layer 8c is an electrode (also referred to as a second electrode) that can collect charges generated by photoelectric conversion in the semiconductor layer 8b in response to light irradiation. The material of the second electrode layer 8c is the same as that of the first electrode layer 8a, and a transparent conductive oxide (TCO) that is translucent to light of a specific wavelength range can be used. Fig.17 In the example of (b), seven second electrode layers 8c are arranged side by side along the +Y direction plane. Here, the portion of the second electrode layer 8c of the mth solar cell region 31Bm extending toward the (m+1)th solar cell region 31B(m+1) and the second electrode layer 8c of the (m+1)th solar cell region 31B(m+1) are arranged side by side with a gap (also referred to as the second gap) G2 sandwiched therebetween. For example, the portion of the second electrode layer 8c of the first solar cell region 31B1 extending toward the +Y direction and the second electrode layer 8c of the second solar cell region 31B2 are arranged side by side with a gap (the second gap) G2 sandwiched therebetween. Each second gap G2 has a long side direction along the +X direction. Here, in each second gap G2, there is a third groove portion P3 with the first electrode layer 8a as the bottom surface. Here, for example, between the mth solar cell region 31Bm and the (m+1)th solar cell region 31B(m+1) adjacent to each other in the +Y direction, the second gap G2 exists at a position further deviated in the +Y direction than the first gap G1. For this purpose, for example, the inter-cell region 31ga between the mth solar cell region 31Bm and the (m+1)th solar cell region 31B(m+1) adjacent to each other in the +Y direction is provided from the edge of the first gap G1 in the -Y direction to the edge of the second gap G2 in the +Y direction.

[0184] The connection portion 9 is in a state of electrically connecting two adjacent solar cell regions 31B in series among the plurality of solar cell regions 31B. Fig.17In the example of (b), the mth connection portion 9m is provided in a state of penetrating between the semiconductor layer 8b and the transparent portion 7. The mth connection portion 9m is in a state of electrically connecting the mth solar cell region 31Bm and the (m+1)th solar cell region 31B(m+1). For example, the first connection portion 91 is in a state of electrically connecting the first solar cell region 31B1 and the second solar cell region 31B2. More specifically, the mth connection portion 9m is in a state of electrically connecting the second electrode layer 8c of the mth solar cell region 31Bm and the first electrode layer 8a of the (m+1)th solar cell region 31B(m+1). For example, the first connection portion 91 is in a state of electrically connecting the second electrode layer 8c of the first solar cell region 31B1 and the first electrode layer 8a of the second solar cell region 31B2. Thus, a plurality of solar cell regions 31B are electrically connected in series. In addition, the connection portion 9 exists in the second groove portion (not shown), wherein the second groove portion has the end surface of the semiconductor layer 8b facing the +Y direction and the end surface of the transparent portion 7 facing the -Y direction as two side surfaces, and the surface of the first electrode layer 8a facing the -Z direction as the bottom surface. Each second groove portion has a long side direction along the +X direction. And, the connection portion 9 is filled in the second groove portion.

[0185] The transparent portion 7 has a higher light transmittance than the semiconductor layer 8b for light of a specific wavelength range. The transparent portion 7 can be formed, for example, by locally heating a portion of a semiconductor layer having a perovskite structure. Here, the mth transparent portion 7m is located between the mth connecting portion 9m of the mth solar cell region 31Bm and the (m+1)th solar cell region 31B(m+1). For example, the first transparent portion 71 is located between the first connecting portion 91 of the first solar cell region 31B1 and the second solar cell region 31B2. Fig.17 In the example of (b), the mth transparent portion 7m is located between the mth connecting portion 9m and the third groove portion P3 of the mth solar cell region 31Bm, wherein the third groove portion P3 is located between the mth solar cell region 31Bm and the (m+1)th solar cell region 31B(m+1). For example, the first transparent portion 71 is located between the first connecting portion 91 and the third groove portion P3 of the first solar cell region 31B1, wherein the third groove portion P3 is located between the first solar cell region 31B1 and the second solar cell region 31B2. The transparent portion 7 may be composed of an opaque semiconductor layer, for example, and may be the same as the semiconductor layer 8b.

[0186] In the first solar cell region 31B1, the first electrode layer 8a has a portion (also referred to as the first extension portion) 8ae extending further in the -Y direction than the semiconductor layer 8b and the second electrode layer 8c. In the seventh solar cell region 31B7, the semiconductor layer 8b and the second electrode layer 8c extend further in the +Y direction than the first electrode layer 8a, and the second electrode layer 8c has a portion (also referred to as the second extension portion) 8ce extending further in the +Y direction than the semiconductor layer 8b. On the first extension portion 8ae, a wiring member for output of the first polarity (also referred to as the first output wiring member) 32a is in a state of being electrically connected. Here, the first output wiring member 32a is, for example, in a state of being bonded to the first extension portion 8ae which is a part of the electrode of the first solar cell region 31B1. Specifically, for example, there is a portion (also referred to as the third bonding portion) 321B located between the first output wiring member 32a and the first extension portion 8ae and in a state of bonding the first output wiring member 32a and the first extension portion 8ae. exist Fig.17 In the example of (a), the first output wiring member 32a is provided along the end edge in the -Y direction of the first solar cell region 31B1. On the second extension portion 8ce, the output wiring member (also referred to as the second output wiring member) 32b is in a state of being electrically connected to the second polarity. Here, the second output wiring member 32b is, for example, in a state of being joined to the second extension portion 8ce which is a part of the electrode of the seventh solar cell region 31B7. Specifically, for example, there is a portion (also referred to as the fourth joining portion) 322B which is located between the second output wiring member 32b and the second extension portion 8ce and is in a state of joining the second output wiring member 32b and the second extension portion 8ce. In Fig.17 In the example of (a), the second output wiring member 32b is provided along the end side in the +Y direction of the seventh solar cell region 31B7.

[0187] The first output wiring member 32a and the second output wiring member 32b are, for example, respectively made of a metal body having a wire shape or a strip shape and being conductive. The materials of the third joint portion 321B and the fourth joint portion 322B are, for example, low-melting-point alloys such as solder or low-melting-point single metals. More specifically, for example, the first output wiring member 32a and the second output wiring member 32b are respectively made of copper foil having a thickness of about 0.1 mm to 0.2 mm and a width of about 1 mm to 2 mm, and the entire surface of the first output wiring member 32a and the second output wiring member 32b is covered with solder. The first output wiring member 32a is, for example, in a state of being electrically connected to the first extension portion 8ae by soldering. In addition, the second output wiring member 32b is, for example, in a state of being electrically connected to the second extension portion 8ce by soldering. In this case, for example, the solder between the first output wiring member 32a and the first extension portion 8ae constitutes the third joint portion 321B. In addition, for example, the solder between the second output wiring member 32b and the second extension portion 8ce constitutes the fourth bonding portion 322B. Hereinafter, the third bonding portion 321B and the fourth bonding portion 322B are appropriately referred to as "bonding portions". In addition, here, for example, if the first polarity is a negative pole, the second polarity becomes a positive pole. For example, if the first polarity is a positive pole, the second polarity becomes a negative pole. And, the first output wiring member 32a and the second output wiring member 32b are each, for example, in a state of being led out to the outside via a through hole penetrating the back protective layer 2.

[0188] Here, for example, the substrate 6 in the solar cell section 3B may be set as the back protective layer 2. In addition, in the above example, the plurality of solar cell regions 31B are arranged in parallel along the Y direction, but this is not necessarily limited to this. The arrangement direction of the plurality of solar cell regions 31B may be the X direction, which can be changed as appropriate.

[0189] <3. Others>

[0190] In the first to seventh embodiments, for example, the back protective layer 2 may be omitted. In this structure, since the free acid (e.g., acetic acid) generated in the filler 4 is released from the filler 4 in the -Z direction in a gaseous state, it is possible to reduce the adverse conditions of the solar cell section 3 caused by the free acid.

[0191] In the first embodiment to the seventh embodiment, the two supporting members 5 may be located on both sides of the solar cell panel 10 in the Y direction instead of in the X direction. The solar cell panel 10 can be bent when viewed with the line of sight along the X direction. In this case, the number of arrangements of the solar cell elements 31 in the Y direction may be an even number. Accordingly, the central part of the solar cell panel 10 in the Y direction corresponds to the part between the solar cell elements 31. For this reason, the stress generated in the solar cell element 31 can be reduced compared to the structure in which the number of arrangements is an odd number.

[0192] Furthermore, in the third to sixth embodiments, the thickness W1 of the filler 4 need not necessarily be greater than the thickness W2 and the thickness W3. This is because the effects of the third to sixth embodiments are not necessarily based on the thickness distribution of the filler 4.

[0193] As described above, the solar cell module is described in detail. The above description is illustrative in all situations, and the present disclosure is not limited to this. In addition, the above various examples can be used in combination as long as they are not contradictory to each other. And it is known that countless examples that are not exemplified can be conceived without departing from the scope of the present disclosure.

[0194] The present disclosure includes the following contents.

[0195] In one embodiment, (1) a solar cell module comprises: a first protective layer having a first surface and a second surface opposite to the first surface; a solar cell portion comprising a plurality of solar cell elements arranged in a state opposite to the second surface of the first protective layer; a supporting member arranged in a state adjacent to the solar cell portion, comprising an inner portion arranged in a state opposite to the second surface of the first protective layer, and an outer portion arranged in a state extending outward from the inner portion; and a filling material connected to the second surface of the first protective layer and arranged in a state covering the inner portion and the solar cell portion, wherein a thickness between the solar cell portion and the supporting member is greater than a thickness between two adjacent solar cell elements among the plurality of solar cell elements.

[0196] (2) In the solar cell module of (1) above, the number of arrayed solar cell elements is an even number.

[0197] (3) A solar cell module comprises: a first protective layer having a first surface and a second surface opposite to the first surface; a solar cell portion arranged to be opposite to the second surface of the first protective layer; a supporting member arranged to be adjacent to the solar cell portion, comprising an inner portion arranged to be opposite to the second surface of the first protective layer, and an outer portion arranged to extend outward from the inner portion; and a filling material which is in contact with the second surface of the first protective layer and is arranged to cover the inner portion and the solar cell portion, and whose thickness increases as it goes from the solar cell portion to the supporting member.

[0198] (4) Based on the solar cell module of any one of (1) to (3) above, the first part of the filling material located between the inner part of the supporting member and the first protective layer has a given first thickness distribution, and in the given first thickness distribution, the thickness of the first part at the end on the solar cell part side is greater than the thickness of the first part at the end on the outer part side.

[0199] (5) A solar cell module according to any one of (1) to (4), further comprising: a second protective layer which is in contact with the filling material on the side opposite to the first protective layer relative to the filling material and is arranged to face the solar cell portion.

[0200] (6) Based on the solar cell module of (5) above, the second protective layer is arranged in a state opposite to the inner portion of the supporting member, and the second portion of the filling material located between the inner portion of the supporting member and the second protective layer has a given second thickness distribution, in which the thickness of the second portion at the end on the solar cell part side is greater than the thickness of the second portion at the end on the outer portion side.

[0201] (7) In the solar cell module of (5) or (6) above, an end of the filler on the second protective layer side and the outer portion side is located on the solar cell portion side relative to an end on the first protective layer side and the outer portion side.

[0202] (8) In the solar cell module of (7) above, an end of the second protective layer on the support member side is located on the solar cell portion side relative to an end of the first protective layer on the support member side.

[0203] (9) In the solar cell module of (7) or (8) above, the filler and the second protective layer are provided on the side of the support member opposite to the first protective layer, avoiding a region facing the support member.

[0204] (10) In the solar cell module according to any one of (1) to (9) above, the first protective layer has a rectangular shape, and the plurality of support members are arranged side by side with intervals therebetween along one side of the first protective layer.

[0205] (11) Based on the solar cell module of (10) above, a third part as a part of the filling material is located between two adjacent supporting members among the plurality of supporting members, and the third part has a given third thickness distribution. In the third thickness distribution, the thickness of the third part at the end of one side of the two supporting members is greater than the thickness of the third part at the center position between the two supporting members.

[0206] (12) In the solar cell module according to any one of (1) to (11) above, the first protective layer has a rectangular shape, and the support member is located only on one side of the first protective layer.

[0207] (13) A solar cell module according to any one of (1) to (12) above, further comprising a carbon fiber component, wherein the first protective layer has a rectangular shape, the supporting component is located on the first side of the first protective layer, and the carbon fiber component is arranged on the second side of the first protective layer where the supporting component is not arranged in a state covered by the filling material.

[0208] Explanation of symbols

[0209] 1 Surface protection layer

[0210] 1a The end of the surface protection layer 1 on the support member 5 side

[0211] 1f Side 1

[0212] 1s Side 2

[0213] 2 Back protective layer

[0214] 2a The end of the back protection layer 2 on the supporting member 5 side

[0215] 3,3B Solar cell unit

[0216] 31 Solar cell elements

[0217] 4 Filling materials

[0218] Section 4a

[0219] 4b Part 1 (Part)

[0220] 4c Part 2 (Part)

[0221] 4d Part 3 (Part)

[0222] 41a The end of the filler 4 on the surface protection layer 1 side and the outer portion 52 side

[0223] 42a The end of the filler material 4 on the back protection layer 2 side and the outer portion 52 side.

[0224] 5 Supporting components

[0225] 60 Fiber-reinforced components

[0226] 100 Solar cell modules.

Claims

1. A solar cell module comprising: A first protective layer having a first surface and a second surface opposite to the first surface; a solar cell section including a plurality of solar cell elements disposed so as to face the second surface of the first protective layer; a supporting member disposed adjacent to the solar cell portion; and Filling material, The supporting member includes an inner portion disposed in a state facing the second surface of the first protective layer, and an outer portion disposed in a state extending outward from the inner portion. The filling material is in contact with the second surface of the first protective layer and is provided in a state of covering the inner portion and the solar cell portion. The thickness of the filling material between the solar cell section and the support member is greater than the thickness of the filling material between two adjacent solar cell elements among the plurality of solar cell elements.

2. The solar cell module according to claim 1, wherein: The number of arrays of the plurality of solar cell elements is an even number.

3. A solar cell module comprising: A first protective layer having a first surface and a second surface opposite to the first surface; a solar cell section disposed so as to face the second surface of the first protective layer; and a supporting member disposed so as to be adjacent to the solar cell section; and Filling material, The supporting member includes an inner portion disposed in a state facing the second surface of the first protective layer, and an outer portion disposed in a state extending outward from the inner portion. The filling material is in contact with the second surface of the first protective layer and is provided in a state of covering the inner portion and the solar cell portion. The thickness of the filling material increases as going from the solar cell portion toward the support member.

4. The solar cell module according to any one of claims 1 to 3, wherein: A first portion of the filling material between the inner portion of the supporting member and the first protective layer has a given first thickness distribution, In the given first thickness distribution, the thickness of the first portion at an end on the solar cell section side is greater than the thickness of the first portion at an end on the outer portion side.

5. The solar cell module according to any one of claims 1 to 4, wherein: The solar cell module further includes a second protective layer that is in contact with the filler on a side opposite to the first protective layer with respect to the filler and is provided in a state facing the solar cell section.

6. The solar cell module according to claim 5, wherein: The second protective layer is provided in a state of being also opposed to the inner portion of the supporting member, A second portion of the filling material between the inner portion of the supporting member and the second protective layer has a given second thickness distribution, In the second thickness distribution, the thickness of the second portion at an end on the solar cell section side is greater than the thickness of the second portion at an end on the outer portion side.

7. The solar cell module according to claim 5 or 6, wherein: An end of the filler on the second protective layer side and the outer portion side is located on the solar cell portion side relative to an end of the filler on the first protective layer side and the outer portion side.

8. The solar cell module according to claim 7, wherein: An end of the second protective layer on the support member side is located on the solar cell portion side with respect to an end of the first protective layer on the support member side.

9. The solar cell module according to claim 7 or 8, wherein: The filling material and the second protective layer are provided on the side of the support member opposite to the first protective layer, avoiding a region facing the support member.

10. The solar cell module according to any one of claims 1 to 9, wherein The first protective layer has a rectangular shape, The plurality of support members are provided in a state of being arranged side by side with intervals therebetween along one side of the first protective layer.

11. The solar cell module according to claim 10, wherein: The third portion, which is a part of the filling material, is located between two adjacent supporting members among the plurality of supporting members. The third portion has a given third thickness distribution, In the third thickness distribution, the thickness of the third portion at one end of the two supporting members is greater than the thickness of the third portion at a center position between the two supporting members.

12. The solar cell module according to any one of claims 1 to 11, wherein: The first protective layer has a rectangular shape, The supporting member is located only on one side of the first protective layer.

13. The solar cell module according to any one of claims 1 to 12, wherein: The solar cell module further comprises a reinforcing fiber member. The first protective layer has a rectangular shape, The supporting member is located at the first side of the first protective layer, The reinforcing fiber member is provided on the second side of the first protective layer where the supporting member is not provided, in a state covered with the filling material.