Method for removing and fixing uranium by using vanadium oxide and application thereof
By systematically studying the interaction mechanism between vanadium oxide and uranium, using vanadium oxide to prepare high-performance materials, solving the problem of removal and fixing of uranyl ions, achieving efficient adsorption and resource utilization of uranium, and improving material utilization efficiency. It also provides an efficient and safe treatment solution for uranium-containing wastewater.
Patent Information
- Application Number
- CN202411168777.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-10-11
- Publication Date
- 2024-11-29
AI Technical Summary
The existing technology has complex reaction mechanisms, low material utilization efficiency, great impact on coexisting ions, and difficult uranium recycling and resource utilization in the removal and fixation of uranyl ions, which have failed to effectively solve the efficient, simple separation and resource utilization of uranium in wastewater. question.
By systematically studying the efficiency of V2O5 or VO2 removal and fixing uranium in different environmental conditions, combining multiple micro-characterization methods, the interaction mechanism between vanadium and uranium is revealed, and high-performance materials are prepared using vanadium oxides to achieve uranium enrichment and Immobilization, ultrasonic dissolution, stirring, filtration, inductively coupled mass spectrometry and other steps are used to efficiently remove and resource uranium.
It realizes efficient adsorption and resource utilization of uranium, improves the utilization efficiency of materials, provides an efficient and safe treatment solution for uranium-containing wastewater, reduces treatment costs, and realizes the control of radioactive pollution.
Smart Images

Figure HDA0005079816810000011 
Figure HDA0005079816810000012 
Figure HDA0005079816810000013
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of element separation, and in particular to a method for removing and fixing uranium by utilizing vanadium oxide and application thereof. Background Art
[0002] Uranium is the main fuel for achieving highly energy-intensive nuclear fission and an important raw material for the sustainable and safe development of nuclear energy. However, the mining and use of uranium will, to a certain extent, produce uranium-containing acidic wastewater, which pollutes the environment and threatens human health. The treatment of uranium-containing acidic wastewater is conducive to promoting the ecological environment and the safe development of nuclear energy. Capturing and recovering uranium from uranium mine wastewater is of great strategic significance for pollution prevention and control. The proper treatment and disposal of uranium-containing waste is also the key to the sustainable development of nuclear energy.
[0003] Uranyl ions have a large ionic radius and are not easily captured and removed by common ion exchange materials. Hydroxyapatite materials synthesized in the prior art have a good adsorption effect on uranyl ions, but their preparation process is complicated and contains a large amount of calcium ions and phosphates that are difficult to separate. Therefore, how to efficiently and simply separate uranium products or refine them has become a key issue to be solved.
[0004] my country is a country with abundant vanadium resources, and its reserves rank first in the world. my country is also a major vanadium consumer, and the reuse of vanadium waste is of great significance. At present, vanadium waste can be extracted through mature processes such as direct acid leaching / alkaline leaching, salt-free roasting-alkaline leaching, and ammonium sulfate roasting-acid leaching. 2 O 5 . V 2 O 5 It is a typical pentavalent vanadium oxide, and VO 2 It is a common tetravalent vanadium oxide.
[0005] Vanadium-containing substances and uranyl ions have a certain reactivity. Through chemical reactions, vanadium oxides can capture uranyl ions and may form simple-structured and thermodynamically stable vanadium-uranium minerals, thereby achieving wastewater purification and uranium fixation. Vanadium-uranium minerals are ideal mineral phases for enriching and storing uranium. The softer vanadium-uranium mineral phase has a strong uranium absorption capacity and is easily soluble in dilute hydrochloric acid and accompanied by VO 4 3- Microchemical reaction. Uranium can be extracted from vanadium-uranium ore by heap leaching-reduction-precipitation, while free vanadium can be recovered and detoxified by precipitation by neutralizing the pH to 8 with lime milk.
[0006] Problems and shortcomings of the existing technology:
[0007] 1. Complex reaction mechanism: Due to the variable valence of vanadium, the reaction process between vanadium and uranium is complicated, and the existing technology has not yet fully revealed the V 2 O 5or VO 2 The interaction mechanism between uranium and uranium.
[0008] 2. Low material utilization efficiency: Under different pH conditions, V 2 O 5 or VO 2 The fixation efficiency of U(VI) may not be high, resulting in low material utilization in practical applications.
[0009] 3. Influence of coexisting ions: Coexisting ions in wastewater may affect V 2 O 5 or VO 2 As for the removal effect of U(VI), the existing research has not fully explored this issue.
[0010] 4. Uranium recovery and resource utilization: How to efficiently and simply separate uranium products and carry out mineralization recovery and resource utilization has not yet been well answered by existing technologies.
[0011] Based on the above problems, the present invention proposes a new technical solution, which systematically studies the effects of different environmental conditions on V 2 O 5 or VO 2 The removal and fixation efficiency of uranium, combined with a variety of microscopic characterization methods, revealed that V 2 O 5 or VO 2 The adsorption of uranium and the interaction mechanism between vanadium and uranium, based on the concept of "treating waste with waste", use vanadium-containing waste to prepare high-performance vanadium-based materials, and use them for uranium enrichment and immobilization, to achieve the dual goals of waste resource utilization and radioactive pollution control, and provide theoretical basis and technical support for the efficient and safe treatment of uranium-containing radioactive wastewater. Summary of the invention
[0012] In order to solve the shortcomings of the background technology, the present invention provides a method for removing and fixing uranium by using vanadium oxide and its application, which has the characteristics of simple operation and low cost.
[0013] To achieve the above object, the technical solution of the present invention is achieved as follows:
[0014] In one aspect, the present invention provides a method for removing and fixing uranium using vanadium oxide, the method comprising the steps of:
[0015] S1. Solid uranyl nitrate (UO 2 (NO 3 ) 2 6H 2 (2) mixed with deionized water and nitric acid and then ultrasonically dissolved to obtain a uranium stock solution after sufficient dissolution;
[0016] S2, dilute the uranium stock solution obtained in step S1 to obtain uranyl ions UO 2 2+ solution, adjust the pH value of the solution with nitric acid, and add V 2 O 5 , stirring, and carrying out adsorption reaction;
[0017] S3. The solution after the reaction in step S2 was collected by filtering with a 0.22 μm filter head, and the concentration of U (VI) was tested by inductively coupled plasma mass spectrometry, and the concentration of V (V) was tested by ultraviolet spectrophotometer.
[0018] Furthermore, in step S1, the solid uranyl nitrate (UO 2 (NO 3 ) 2 6H 2 O) accounts for 1% to 2% by volume; in the step S1, 0.01 mol / L sulfuric acid or hydrochloric acid is used to adjust and remove impurities from the solid ammonium nitrate solution.
[0019] Furthermore, in step S2, uranyl ions (UO 2 2+ )The solution concentration is 10-200mg / L.
[0020] Furthermore, in step S2, the pH value of the solution is adjusted to 2.0-5.0 by nitric acid. Furthermore, in step S2, V 2 O 5 The dosage concentration is 0.2-2.0g / L.
[0021] Furthermore, the adsorption reaction time of step S2 is 0.5-7h; and the stirring speed of step S2 is 600rpm.
[0022] Furthermore, the temperature of the adsorption process is controlled within 25±5°C.
[0023] On the other hand, the present invention also provides another embodiment of the above method, comprising the following steps:
[0024] (A) Take V 2 O 5 Dissolve in deionized water, stir until completely dissolved, add citric acid, continue to stir evenly, transfer to an autoclave for reaction, cool to room temperature, wash with ethanol and ultrapure water several times and collect and dry to obtain VO 2 ;
[0025] (B) Solid uranyl nitrate (UO 2 (NO 3 ) 2 6H 2(2) mixed with deionized water and nitric acid and then ultrasonically dissolved to obtain a uranium stock solution after sufficient dissolution;
[0026] (C) diluting the uranium stock solution obtained in step B to obtain uranyl ions UO 2 2+ solution, adjust the pH value of the solution with nitric acid, and add VO 2 , stirring, and carrying out adsorption reaction;
[0027] (D) The solution after the reaction in step C was collected by filtration using a 0.22 μm filter head, and the concentration of U (VI) was tested by inductively coupled plasma mass spectrometry, and the concentration of V (V) was tested by ultraviolet spectrophotometer.
[0028] Alternatively, in step (B), citric acid may not be added and a small amount of VO2 may be directly added to distilled water. 2 The powder forms a dispersion, and after standing and stratification, the supernatant is transferred to an autoclave for concentration reaction.
[0029] As a preferred solution, V 2 O 5 The mass ratio of VO to citric acid is preferably 0.63:1. In specific implementation, citric acid may not be added and a small amount of VO may be directly added to distilled water. 2 The powder forms a dispersion, and after standing and stratification, the supernatant is transferred to an autoclave for concentration reaction.
[0030] Furthermore, in step (C), the pH range of the diluted hydrochloric acid is adjusted to 1.5-4. The stirring speed of step (A) is 600 rpm. In step A, the reaction condition of the autoclave is 180° C. for 12 hours.
[0031] The present invention utilizes V 2 O 5 or VO 2 The uranyl ions in wastewater are efficiently removed while being enriched, mineralized and utilized as resources, providing a method for achieving the dual goals of waste resource regeneration and radioactive pollution control, which is original in the field of uranium-containing wastewater removal.
[0032] The method provided by the present invention has a large uranium adsorption capacity, high efficiency, simple process, easy separation (the material is immiscible with U(VI)), and high recovery rate. The method utilizes the strong uranium absorption capacity of vanadium-uranium minerals to achieve efficient adsorption of uranium in wastewater and uranium resource refining and regeneration, thereby improving material utilization efficiency and providing a theoretical basis and technical support for efficient and safe treatment of uranium-containing radioactive wastewater. BRIEF DESCRIPTION OF THE DRAWINGS
[0033] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.
[0034] Figure 1 For different V 2 O 5 Effect of dosage on U(VI) removal rate
[0035] Figure 2 Different pH values for V 2 O 5 Effect curve of removing U(VI)
[0036] Figure 3 For the coexisting ion pair V 2 O 5 Results of the test on the effect of removing U(VI) DETAILED DESCRIPTION
[0037] The principles and features of the present invention are described below. The examples given are only used to explain the present invention and are not used to limit the scope of the present invention.
[0038] The present invention is further described below in conjunction with the accompanying drawings and embodiments.
[0039] Example 1: A method for removing and fixing uranium using vanadium oxide:
[0040] S1. At room temperature, accurately weigh 2.11 g of solid uranyl nitrate (UO 2 (NO 3 ) 2 6H 2 2) is placed in a 250mL conical flask, and ultrasonically dissolved after adding 50mL deionized water and 2mL 5mol / L nitric acid. After the solid is fully dissolved, it is transferred to a 1000mL volumetric flask. Deionized water is used to wash the conical flask many times and the solution is transferred to a volumetric flask. Finally, deionized water is used to constant volume to finally obtain a 1L 1000mg / L uranium stock solution. The uranium stock solution is stored in the dark.
[0041] S2, using the uranium stock solution obtained in S1 to dilute and prepare uranyl ion UO with different initial uranyl ion concentrations (10, 20, 30, 40, 50, 100, 150, 200 mg / L) 2 2+ Solution, HNO 3The pH value of the prepared U(VI) solution was adjusted to 2.0-5.0, and V(VI) was added to form different concentrations (0.2, 0.5, 1.0, 2.0 g / L). 2 O 5 The mixed solution was placed in a magnetic stirrer and stirred at 600 rpm for 0.5-7 h. The temperature of the adsorption process was 25±5°C.
[0042] S5. After 360 min, the reaction solution was collected by filtration using a 0.22 μm filter, and the concentration of U (VI) was tested by inductively coupled plasma mass spectrometry (ICP-MS), and the concentration of V (V) was tested by ultraviolet spectrophotometer (UV).
[0043] The U content in the sample was detected to be as high as 50.62%, much higher than 34.3% (U 2 V 6 O 21 .15H 2 O theoretical uranium content). This indicates that the newly formed U 2 V 6 O 21 15H 2 O can adsorb U(VI). Figure 1 It can be seen that the most economical and efficient material addition condition is 0.5g / L, and the removal rate can reach 97% after 120 minutes. The more abundant the U(VI) concentration is, the stronger the mineralization of V(V) and U(VI) will be. 2 V 6 O 21 15H 2 O has a certain adsorption effect on U(VI), V 2 O 5 The U(VI) removal effect increased with the increase of the initial U(VI) concentration, and the concentration threshold was determined to be higher than 180 mg / L and close to 200 mg / L.
[0044] By the attached Figure 2 It can be seen that at pH 2.0, 3.0 and 4.0, the removal rate of U(VI) reached 97%. In particular, at pH = 2.0, the removal rate of V 2 O 5 The reaction with U(VI) ions has almost no pH change, and the dissolution and existence form of V(V) ions in the solution are almost unaffected by pH. 2 V 6 O 21 15H 2 The mineral precipitation structure of O is the most complete. It can be seen that the pH value of the solution has a significant effect on the removal efficiency of uranium.
[0045] Example 2: A method for removing and fixing uranium using vanadium oxide:
[0046] S1. Accurately weigh 1.8928g of V 2 O 5 (AR) was dissolved in 168 mL of deionized water and stirred with a magnetic stirrer for 15 min until completely dissolved to obtain solution A. 2.98 g of citric acid was added to solution A and stirred with a magnetic stirrer for 15 min to obtain solution B. Solution B was transferred to a 200 mL autoclave and reacted at 180 ° C for 12 hours. After the autoclave was cooled to room temperature, the dark blue material was washed several times with ethanol and ultrapure water and collected and dried to obtain VO 2 .
[0047] S2, V in "Step S2 of Example 1" 2 O 5 Replace with VO 2 VO was analyzed by X-ray photoelectron spectroscopy (XPS), X-ray powder diffraction analysis (XRD), Fourier transform infrared spectroscopy (FTIR) and other techniques. 2 The removal of U(VI) was studied and it was shown that VO 2 Low concentration U(VI) is removed by adsorption, and high concentration U(VI) is removed by enrichment and mineralization.
[0048] The analysis results show that VO 2 and V 2 O 5 Both can efficiently enrich uranium and V 2 O 5 In comparison, VO 2 The adsorption efficiency of U(VI) is faster, and the equilibrium is reached after 60 minutes of reaction. 2 It can better treat low-concentration uranium-containing wastewater. Its optimal pH condition is 4.0 and the optimal dosage is between 0.2 and 1 g / L. 2 and V 2 O 5 After reacting with uranium, it can form thermodynamically stable vanadium-uranium crystal phases such as U 2 V 6 O 21 15H 2 O, to achieve the immobilization of uranyl ions and effectively prevent the environmental migration of uranyl ions.
[0049] Test Example 1: Coexisting cations (e.g., Na + , K + , Ca 2+ Mg 2+ and Al 3+ ) or anions (such as CO3 2- and HPO 4 2- ) for V 2 O 5 Remove the influence of U(VI)
[0050] In "Example 1, step S2, HNO 3 The pH value of the prepared U(VI) solution was adjusted to 2.0-5.0", and then ions of different concentrations (0.001 mol / L, 0.01 mol / L, 0.05 mlo / L, 0.1 mol / L) were additionally added.
[0051] from Figure 3 It can be seen that:
[0052] ①With the increase of Na+ concentration, V 2 O 5 The removal effect of U(VI) is also improved. + , Ca 2+ Mg 2+ , Na + The influence on material removal U(VI) is smaller.
[0053] ② When K is present in the reaction system + , Ca 2+ and Mg 2+ ions, V 2 O 5 The removal efficiency of U(VI) increased from 97% to 99%. This is because K + and Ca 2+ Ions can promote the formation of UV mineral phases with lower solubility (K 2 (UO 2 ) 2 V 2 O 8 and Ca(UO 2 ) 2 V 2 O 8 ).
[0054] ③Al 3+ Almost no effect on V 2 O 5 Removal of U(VI).
[0055] ④ In addition, when CO is present in the reaction system 3 2- and HPO 4 2- ions, V 2 O 5 The removal effect of U(VI) will be inhibited. This is because CO3 2- The ion has a strong affinity with U(VI) and can form various complexes with U(VI), such as UO 2 CO 3 , UO 2 (CO 3 ) 2 2- , UO 2 (CO 3 ) 3 4- , thus hindering the reaction between V(V) and U(VI). 4 2- , it combines with U(VI) under acidic conditions to form neutral or positively charged ions, and the binding of U(VI) and V(V) will also be inhibited.
[0056] The above is only a preferred embodiment of the present invention and is not intended to limit the present invention. Any modifications, equivalent substitutions and improvements made within the spirit and principles of the present invention shall be included in the protection scope of the present invention. The components and preparation methods involved in the present invention can be adjusted accordingly according to the implementation method, but shall not exceed the protection scope of the invention.
Claims
1. A method for removing and fixing uranium using vanadium oxides, characterized in that: The method comprises the following steps: S1. Mix solid uranyl nitrate (UO2(NO3)2·6H2O) with deionized water and nitric acid and dissolve them by ultrasonication to obtain a uranium stock solution after they are fully dissolved; S2, dilute the uranium stock solution obtained in step S1 to obtain uranyl ions UO2 2+ solution, adjust the pH value of the solution with nitric acid, add V2O5, stir, and perform adsorption reaction; S3. The solution after the reaction in step S2 was collected by filtering with a 0.22 μm filter head, and the concentration of U (VI) was tested by inductively coupled plasma mass spectrometry, and the concentration of V (V) was tested by ultraviolet spectrophotometer.
2. A method for removing and fixing uranium using vanadium oxides as claimed in claim 1, characterized in that: Step S2: uranyl ion UO2 2+ The solution concentration is 10-200 mg / L.
3. A method for removing and fixing uranium using vanadium oxides as claimed in claim 1, characterized in that: In step S2, the pH value of the solution is adjusted by nitric acid to 2.0-5.
0.
4. A method for removing and fixing uranium using vanadium oxides as claimed in claim 1, characterized in that: The added concentration of V2O5 in step S2 is 0.2-2.0 g / L.
5. A method for removing and fixing uranium using vanadium oxides as claimed in claim 1, characterized in that: The adsorption reaction time of step S2 is 0.5-7h; the stirring speed of step S2 is 600rpm.
6. A method for removing and fixing uranium using vanadium oxides as claimed in claim 1, characterized in that: The temperature of the adsorption process was 25±5°C.
7. A method for removing and fixing uranium using vanadium oxides as claimed in claim 1, characterized in that: The method may further comprise the steps of: S1. Dissolve V2O5 in deionized water, stir until completely dissolved, add citric acid, continue to stir evenly, transfer to an autoclave for reaction, cool to room temperature, wash with ethanol and ultrapure water several times, collect and dry to obtain VO2; S2, mixing solid uranyl nitrate (UO2(NO3)2·6H2O) with deionized water and nitric acid and dissolving them by ultrasonication to obtain a uranium stock solution after full dissolution; S3, dilute the uranium stock solution obtained in step S2 to obtain uranyl ions UO2 2+ solution, adjust the pH value of the solution with nitric acid, add VO2, stir, and perform adsorption reaction; S4. The solution after the reaction in step S3 was collected by filtering with a 0.22 μm filter head, and the concentration of U (VI) was tested by inductively coupled plasma mass spectrometry, and the concentration of V (V) was tested by ultraviolet spectrophotometer.
8. A method for removing and fixing uranium using vanadium oxides as claimed in claim 7, characterized in that: The mass ratio of V2O5 to citric acid is 0.63:
1.
9. A method for removing and fixing uranium using vanadium oxides as claimed in claim 7, characterized in that: In the step S1, the reaction condition of the autoclave is 180° C. for 12 hours.
10. Use of the method for removing and fixing uranium using vanadium oxide as claimed in any one of claims 1 to 10 in removing uranium-containing wastewater.