Cosmetic art paint and preparation method thereof

Through solvents without VOCs and modified diatomaceous earth, titanium dioxide sol composite materials, and cosmetic art paints combined with tetrabutyl titanate and other components, the problem of high VOCs content in the existing technology is solved, and high wear resistance and Environmentally friendly paint film reduces the concentration of harmful substances in the room.

CN119039839APending Publication Date: 2024-11-29JIANGSU MARITIME INST
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
CN202410482498.3
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-04-22
Publication Date
2024-11-29

AI Technical Summary

Technical Problem

The high content of organic solvents in existing artistic paints leads to a high content of volatile organic matter (VOCs), which affects human health. At the same time, the glue adhesive used in the manufacturing process of artificial boards also releases toxic substances such as free formaldehyde, resulting in the decoration of the room. The content of internal VOCs is high.

Method used

Using solvents and resins without VOCs, a cosmetic art paint is prepared by modifying diatomaceous earth and titanium dioxide sol composite material, combined with tetrabutyl titanate, anhydrous ethanol, ethyl silicate and graphene, and using elasticity. The ratio of acrylic emulsion, pearlescent powder, calcium carbonate, coupling agent, defoaming agent, oxidized polyethylene wax, conditioning agent, stain-resistant material and photocatalytic material is prepared by stirring and precipitation processes to form high wear resistance and water resistance paint film with corrosion resistance and photocatalytic properties.

Benefits of technology

It has achieved the reduction of the absorption and decomposition of indoor VOCs, reduced the impact on human health, and improved the wear resistance, water resistance and high temperature resistance of the paint film, and comply with national environmental protection standards.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119039839A_ABST
    Figure CN119039839A_ABST
Patent Text Reader

Abstract

The invention relates to the technical field of art paint, and discloses makeup art paint and a preparation method thereof.The makeup art paint is prepared from, by mass, 30-50 parts of elastic acrylic emulsion, 6-12 parts of pearl powder, 35-48 parts of water, 10-19 parts of calcium carbonate, 0.2-0.45 part of coupling agent, 0.1-0.3 part of defoaming agent, 0.1-0.25 part of oxidized polyethlene wax, 2-7 parts of conditioner and 3-9 parts of stain-resistant material; 8-12 parts of a photocatalytic material; the cosmetic art paint has the beneficial effects that the solvent and the resin which do not contain the VOCs are used, so that the cosmetic art paint provided by the invention does not contain the VOCs, and indoor VOCs can be absorbed by compounding the modified diatomite and the titanium dioxide sol, so that the aim of reducing the influence of the VOCs on human body health to a certain extent is fulfilled.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of artistic paints, and in particular to a color cosmetic artistic paint and a preparation method thereof. Background Art

[0002] As a new type of wall decoration paint, artistic paint is different from the single decorative effect of latex paint. It has rich three-dimensional texture and can produce different refraction effects under the illumination of light, thus enhancing the layering of the space invisibly.

[0003] In the related art, artistic paint usually includes resin, solvent, pigment, diluent, leveling agent and antioxidant. The resin can provide good adhesion, wear resistance and corrosion resistance; the solvent is used to mix the resin and pigment and allow them to flow and be applied to the surface of the object; the pigment in the artistic paint can be inorganic pigments, organic pigments, metal powders, etc. of various colors, which are used to give the artwork rich colors and texture effects; the diluent, leveling agent and antioxidant are used to improve the performance of the artistic paint.

[0004] At present, artificial boards are also one of the main materials for decorating most new houses. In the manufacturing process of artificial boards, a large amount of glue and adhesives are needed to bond the wood together. The main components of glue and adhesives are urea-formaldehyde resin glue or phenol-formaldehyde resin glue, which are the main source of free formaldehyde release and can easily lead to toxic pollution. The content of volatile organic compounds (VOCs) in the organic solvents of artistic paint is also high. Therefore, the VOCs content in the decorated room that uses artistic paint and artificial boards at the same time is high, which can easily affect people's health.

[0005] In order to address the above problems, a kind of makeup art paint is urgently needed. Summary of the invention

[0006] The object of the present invention is to provide a color cosmetic art paint to solve the problems raised in the above background technology.

[0007] To achieve the above-mentioned purpose, a cosmetic art paint is provided, comprising the following raw materials in proportion by weight: 30-50 parts of elastic acrylic emulsion, 6-12 parts of pearlescent powder, 35-48 parts of water, 10-19 parts of calcium carbonate, 0.2-0.45 parts of coupling agent, 0.1-0.3 parts of defoaming agent, 0.1-0.25 parts of oxidized polyethylene wax, 2-7 parts of conditioning agent, 3-9 parts of anti-fouling material, and 8-12 parts of photocatalytic material.

[0008] Furthermore, the coupling agent is specifically a silane coupling agent or a titanate coupling agent.

[0009] Furthermore, the defoaming agent is specifically one of organic oxane, polyether, silicon and ether grafted, amine or imine.

[0010] Furthermore, the anti-fouling material is specifically one of silica sol, pure acrylic emulsion or dimethyl silylate silica.

[0011] A method for preparing a color cosmetic art paint comprises the following steps: S1: Add elastic acrylic emulsion, pearl powder, calcium carbonate, stain-resistant material and photocatalytic material into a mixing container; S2: Stir the mixing container at a low speed of 300-500 rpm for 10 minutes, and gradually add the conditioning agent during the stirring process; S3: Continue to add coupling agent, defoamer and oxidized polyethylene wax into the mixing container; S4: Increase the stirring speed of the mixing container to 800-1000 rpm and continue mixing and stirring for 15 minutes; S5: gradually and slowly add water and continue stirring at 1000 rpm until the mixture is completely mixed.

[0012] Furthermore, the photocatalytic material is prepared by the following method: Step 1: Evenly mix tetrabutyl titanate and anhydrous ethanol, and place in an ultrasonic stirrer for 15-20 minutes to obtain an ethanol solution of tetrabutyl titanate; Step 2: Add ethyl silicate to the ethanol solution of tetrabutyl titanate obtained in step 1, and stir for 10-15 minutes; Step 3: Continue to add graphene dispersion and continue stirring until the solution is evenly mixed; Step 4: Precipitation by spin coating; Step 5: After the precipitate is stabilized, the precipitate is heat-treated in a drying oven at 45-60°C to obtain a photocatalytic precipitate; Step 6: Place the precipitate in a container and crush it to obtain a powdered photocatalytic material.

[0013] Compared with the prior art, the present invention has the following beneficial effects: By using solvents and resins that do not contain VOCs, the color cosmetic paint provided by the present application itself does not contain VOCs. The modified diatomaceous earth and titanium dioxide sol can also absorb indoor VOCs through composite use, thereby achieving the purpose of reducing the impact of VOCs on human health to a certain extent. The composite use of tetrabutyl titanate, anhydrous ethanol, ethyl silicate and graphene dispersion can make the artistic paint have higher wear resistance, water resistance, corrosion resistance, high temperature resistance and photocatalytic performance. BRIEF DESCRIPTION OF THE DRAWINGS

[0014] Figure 1 is a preparation flow chart of the present invention; Figure 2 The figure is a flow chart for preparing the photocatalytic material in the present invention. DETAILED DESCRIPTION

[0015] The technical solutions in the embodiments of the present invention will be clearly and completely described below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, rather than all the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without making creative work are within the scope of protection of the present invention.

[0016] Those skilled in the art will appreciate that, unless otherwise stated, the singular forms "a", "an" and "the" used herein may also include plural forms. It should be further understood that the term "comprising" used in the specification of the present invention refers to the presence of the features, integers, steps, operations, elements and / or components, but does not exclude the presence or addition of one or more other features, integers, steps, operations, elements, components and / or groups thereof. Example

[0017] See also Figure 1-2 As shown, a makeup art paint is provided, comprising the following steps: A cosmetic art paint comprises the following raw materials in proportion by weight: 30 parts of elastic acrylic emulsion, 6 parts of pearlescent powder, 35 parts of water, 10 parts of calcium carbonate, 0.2 parts of coupling agent, 0.1 parts of defoaming agent, 0.15 parts of oxidized polyethylene wax, 2 parts of conditioning agent, 3 parts of anti-fouling material and 8 parts of photocatalytic material.

[0018] It should be noted that, in this embodiment, the coupling agent is a titanate coupling agent, the defoaming agent is a silicon and ether grafting agent, and the anti-fouling material is a silica sol.

[0019] The preparation method of the makeup art paint of this embodiment is as follows: S1: Add elastic acrylic emulsion, pearl powder, calcium carbonate, stain-resistant material and photocatalytic material into a mixing container; S2: Stir the mixing container at a low speed of 300 rpm for 10 minutes, and gradually add the conditioning agent during the stirring process; S3: Continue to add coupling agent, defoamer and oxidized polyethylene wax into the mixing container; S4: increasing the stirring speed of the mixing container to 800 rpm and continuing mixing and stirring for 15 minutes; S5: gradually and slowly add water and continue stirring at 1000 rpm until the mixture is completely mixed.

[0020] A cosmetic art paint comprises the following raw materials in proportion by weight: 40 parts of elastic acrylic emulsion, 9 parts of pearlescent powder, 42 parts of water, 14 parts of calcium carbonate, 0.3 parts of coupling agent, 0.2 parts of defoaming agent, 0.15 parts of oxidized polyethylene wax, 4 parts of conditioning agent, 5 parts of anti-fouling material and 10 parts of photocatalytic material. Example

[0021] It should be noted that, in this embodiment, the coupling agent is a titanate coupling agent, the defoaming agent is a silicon and ether grafting agent, and the anti-fouling material is a silica sol.

[0022] The preparation method of the makeup art paint of this embodiment is as follows: S1: Add elastic acrylic emulsion, pearl powder, calcium carbonate, stain-resistant material and photocatalytic material into a mixing container; S2: Stir the mixing container at a low speed of 400 rpm for 10 minutes, and gradually add the conditioning agent during the stirring process; S3: Continue to add coupling agent, defoamer and oxidized polyethylene wax into the mixing container; S4: increasing the stirring speed of the mixing container to 800 rpm, and continuing mixing and stirring for 20 minutes; S5: gradually and slowly add water and continue stirring at 1000 rpm until the mixture is completely mixed.

[0023] A cosmetic art paint comprises the following raw materials in proportion by weight: 50 parts of elastic acrylic emulsion, 12 parts of pearlescent powder, 48 parts of water, 19 parts of calcium carbonate, 0.45 parts of coupling agent, 0.3 parts of defoaming agent, 0.25 parts of oxidized polyethylene wax, 7 parts of conditioning agent, 9 parts of anti-fouling material and 12 parts of photocatalytic material.

[0024] It should be noted that, in this embodiment, the coupling agent is a titanate coupling agent, the defoaming agent is a silicon and ether grafting agent, and the anti-fouling material is a silica sol. Example

[0025] The preparation method of the makeup art paint of this embodiment is as follows: S1: Add elastic acrylic emulsion, pearl powder, calcium carbonate, stain-resistant material and photocatalytic material into a mixing container; S2: Stir the mixing container at a low speed of 500 rpm for 15 minutes, and gradually add the conditioning agent during the stirring process; S3: Continue to add coupling agent, defoamer and oxidized polyethylene wax into the mixing container; S4: increasing the stirring speed of the mixing container to 1000 rpm and continuing mixing and stirring for 20 minutes; S5: gradually and slowly add water and continue stirring at 1000 rpm until the mixture is completely mixed.

[0026] The color cosmetic art paint of the present invention is resistant to low temperature, has a full paint film, good water resistance and acid resistance, strong scrub resistance, does not contain harmful substances such as formaldehyde, is non-toxic, and is environmentally friendly. Other properties also fully meet national standards.

[0027] Preparation Example 1: Step 1: 10 g of tetrabutyl titanate and 30 g of anhydrous ethanol were mixed evenly, and the mixture was sent into an ultrasonic stirrer for stirring for 15 minutes to obtain an ethanol solution of tetrabutyl titanate; Step 2: Add 2 g of ethyl silicate to the ethanol solution of tetrabutyl titanate obtained in step 1 and stir for 10 minutes; Step 3: Continue to add 1g of graphene dispersion and continue stirring until the solution is evenly mixed; Step 4: Precipitation by spin coating; Step 5: After the precipitate is stabilized, the precipitate is placed in a drying oven at 45°C for heat treatment to obtain a photocatalytic precipitate; Step 6: Place the precipitate in a container and crush it to obtain a powdered photocatalytic material.

[0028] Preparation Example 2: Step 1: 12 g of tetrabutyl titanate and 30 g of anhydrous ethanol were mixed evenly, and the mixture was sent into an ultrasonic stirrer for stirring for 20 min to obtain an ethanol solution of tetrabutyl titanate; Step 2: Add 2 g of ethyl silicate to the ethanol solution of tetrabutyl titanate obtained in step 1 and stir for 10 minutes; Step 3: Continue to add 1g of graphene dispersion and continue stirring until the solution is evenly mixed; Step 4: Precipitation by spin coating; Step 5: After the precipitate is stabilized, the precipitate is placed in a drying oven at 50° C. for heat treatment to obtain a photocatalytic precipitate; Step 6: Place the precipitate in a container and crush it to obtain a powdered photocatalytic material.

[0029] Preparation Example 3: Step 1: 12 g of tetrabutyl titanate and 35 g of anhydrous ethanol were mixed evenly, and the mixture was sent into an ultrasonic stirrer for stirring for 20 min to obtain an ethanol solution of tetrabutyl titanate; Step 2: Add 2 g of ethyl silicate to the ethanol solution of tetrabutyl titanate obtained in step 1 and stir for 20 minutes; Step 3: Continue to add 2g of graphene dispersion and continue stirring until the solution is evenly mixed; Step 4: Precipitation by spin coating; Step 5: After the precipitate is stabilized, the precipitate is placed in a drying oven at 60° C. for heat treatment to obtain a photocatalytic precipitate; Step 6: Place the precipitate in a container and crush it to obtain a powdered photocatalytic material.

[0030] Comparative Example 1: Based on Example 1, the photocatalytic material prepared in Preparation Example 1 was used to prepare the makeup art paint; Comparative Example 2: Based on Example 1, the photocatalytic material prepared in Preparation Example 2 was used to prepare the makeup art paint; Comparative Example 3: Based on Example 1, the photocatalytic material prepared in Preparation 3 was used to prepare the color makeup art paint.

[0031] A simulation test was conducted in a sealed test chamber with a volume of 2 cubic meters and a constant temperature of 28°C. 200g of makeup art paint was evenly applied to the inner wall of the chamber (ensuring that the application area was consistent). After 48 hours, the temperature in the sealed test chamber was tested. Concentration, according to Calculation of concentration change A total of 60 closed test chambers are provided, each with 10 as a group. When calculating the data, the lowest and highest data are removed, and then the average value is taken.

[0032] The above shows and describes the basic principles, main features and advantages of the present invention. Those skilled in the art should understand that the present invention is not limited by the above embodiments. The above embodiments and descriptions are only preferred examples of the present invention and are not intended to limit the present invention. Without departing from the spirit and scope of the present invention, the present invention may have various changes and improvements, which fall within the scope of the present invention. The scope of protection of the present invention is defined by the attached claims and their equivalents.

Claims

1. A color cosmetic paint, characterized in that: The composition comprises the following raw materials in proportion by weight: 30-50 parts of elastic acrylic emulsion, 6-12 parts of pearlescent powder, 35-48 parts of water, 10-19 parts of calcium carbonate, 0.2-0.45 parts of coupling agent, 0.1-0.3 parts of defoaming agent, 0.1-0.25 parts of oxidized polyethylene wax, 2-7 parts of conditioning agent, 3-9 parts of anti-fouling material and 8-12 parts of photocatalytic material.

2. A cosmetic art paint according to claim 1, characterized in that: The coupling agent is specifically a silane coupling agent or a titanate coupling agent.

3. A cosmetic art paint according to claim 2, characterized in that: The defoaming agent is specifically one of organic oxane, polyether, silicon and ether grafting, amine or imine.

4. A cosmetic art paint according to claim 3, characterized in that: The anti-fouling material is specifically one of silica sol, pure acrylic emulsion or dimethyl silylated silica.

5. A method for preparing a color cosmetic paint, characterized in that: The following steps are involved: S1: Add elastic acrylic emulsion, pearl powder, calcium carbonate, stain-resistant material and photocatalytic material into a mixing container; S2: Stir the mixing container at a low speed of 300-500 rpm for 10-15 minutes, and gradually add the conditioning agent during the stirring process; S3: Continue to add coupling agent, defoamer and oxidized polyethylene wax into the mixing container; S4: Increase the stirring speed of the mixing container to 800-1000 rpm, and continue mixing and stirring for 15-20 minutes; S5: gradually and slowly add water and continue stirring at 1000 rpm until the mixture is completely mixed.

6. The method for preparing a color makeup art paint according to claim 5, characterized in that: The photocatalytic material is prepared by the following method: Step 1: Evenly mix tetrabutyl titanate and anhydrous ethanol, and place in an ultrasonic stirrer for 15-20 minutes to obtain an ethanol solution of tetrabutyl titanate; Step 2: Add ethyl silicate to the ethanol solution of tetrabutyl titanate obtained in step 1, and stir for 10-15 minutes; Step 3: Continue to add graphene dispersion and continue stirring until the solution is evenly mixed; Step 4: Precipitation by spin coating; Step 5: After the precipitate is stabilized, the precipitate is heat-treated in a drying oven at 45-60°C to obtain a photocatalytic precipitate; Step 6: Place the precipitate in a container and crush it to obtain a powdered photocatalytic material.

Citation Information

Patent Citations

  • Cosmetic art paint and preparation method thereof

    CN117925024A