Yarn coloring process and yarn thereof

By using slurry and drafting of water-based polyurethane and accelerator in the yarn coloring process, the efficiency and cost problems of the traditional high-temperature and high-pressure dyeing process are solved, and the high strength and color of the yarn are achieved Fastness simplifies process flow and reduces energy consumption.

CN119041128AInactive Publication Date: 2024-11-29FUJIAN CHENGDONG NEW MATERIAL TECH CO LTD
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
CN202410999928.9
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-24
Publication Date
2024-11-29
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

The traditional yarn coloring process requires high temperature and high pressure, resulting in low production efficiency, high cost, and long processing time for a single process.

Method used

A yarn coloring process is adopted to slurry by using water-based polyurethane, accelerator and color paste at room temperature, combined with drafting and winding, the yarn is colored at room temperature, and can be dried or Air-drying and speeding up drying.

Benefits of technology

The dyeing process is simplified, the yarn preparation efficiency is improved, the strength and color fastness of the yarn are improved, the drying speed is accelerated, and the color fastness can reach level 4.5 or above, reducing energy consumption and processing time.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure SMS_1
    Figure SMS_1
  • Figure SMS_2
    Figure SMS_2
Patent Text Reader

Abstract

The invention discloses a yarn coloring process and a yarn thereof, and relates to the technical field of yarn coloring. The yarn coloring process comprises the following steps that S0, slurry is prepared, the slurry is prepared from, by mass, 85%-90% of waterborne polyurethane, 0.2%-3% of an accelerant, 1%-2% of color paste and the balance water, and the raw materials are evenly mixed and placed in a slurry tank; the yarn is output from a creel and transferred into a sizing agent tank to be subjected to sizing, an extrusion roller used for guaranteeing uniform sizing of the yarn is arranged in the sizing agent tank, and the yarn passes through the sizing agent at the normal temperature state so that the surface of the yarn can be coated with colors; s2, drafting, namely passively drawing the yarns through a drafting roller; and S3, winding, wherein the drafted yarn is wound and stored through a hydraulic winding machine. The yarn coloring process is short in processing flow and high in yarn preparing and processing efficiency, the yarn traction speed is increased through automatic yarn equipment, and the yarn preparing efficiency is guaranteed; in addition, the yarn can be colored in a normal-temperature state.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of yarn coloring, in particular to a yarn coloring process and yarn thereof. Background Art

[0002] The traditional dyeing process is carried out in a dyeing vat, and is usually processed in the following steps: loosening the tube, loading the yarn, entering the vat, dyeing, adding reduction cleaning, hand-feeling treatment, dehydration, drying, and tightening the tube. This process requires high temperature and high pressure to make the dyeing meet the requirements; and when the temperature is increased, this process alone will take 3-6 hours from the beginning to the end of the treatment. Whether it is preparation efficiency, tools used, labor costs, or site costs, they are all high. In order to solve the above problems, this case was proposed. Summary of the invention

[0003] The invention provides a yarn coloring process and yarn thereof, which overcomes the shortcomings described in the background technology.

[0004] The technical solution adopted by the present invention to solve its technical problem is: A yarn coloring process comprises the following steps: S0: Prepare slurry, which includes the following raw materials by mass fraction: 85-90% waterborne polyurethane, 0.2-3% accelerator, 1-2% color paste, and the rest is water. Mix the raw materials evenly and place them in a slurry tank; S1: Sizing, transferring the yarn from the creel output to the slurry tank for sizing. The slurry tank is provided with a squeezing roller for ensuring uniform sizing of the yarn. The yarn passes through the slurry at room temperature so that the yarn surface is coated with color; S2: drafting, passively drawing the yarn through the drafting roller; S3: Winding: The stretched yarn is wound and stored by a hydraulic winder.

[0005] In traditional technology, whether it is dyes or pigments, they must be colored at high temperatures. The present invention realizes coloring at room temperature. The yarns produced under natural drying are still stable in some performance parameters. Heating and drying or air drying effectively accelerate the drying speed, which is convenient for subsequent yarn winding and molding. Taking color fastness as an example, natural drying (without heating and drying or air drying) can also reach level 4, but the cycle of preparing yarns becomes longer.

[0006] A preferred technical solution: Step S11 is further provided between step S1 and step S2: drying, in which the moisture on the yarn is evaporated and taken away by a drying device, thereby improving the dryness of the yarn surface.

[0007] A preferred technical solution: Step S11 is further provided between step S1 and step S2: air drying, wherein air convection is used through air drying equipment to remove moisture on the surface of the yarn, thereby improving the dryness of the yarn surface.

[0008] A preferred technical solution: the color of the color paste is any color.

[0009] A preferred technical solution: The color of the color paste is fluorescent green.

[0010] A preferred technical solution: multiple drafting rollers are provided, and the yarn is pulled and stretched by different drafting rollers, and the direction of the yarn is adjusted by a plurality of mesh structures for controlling the direction of the yarn.

[0011] A better technical solution: the creel outputs a plurality of yarns at the same time and processes the yarn coloring process to obtain the required yarn.

[0012] A yarn, the surface of which is covered with a slurry layer at room temperature.

[0013] A preferred technical solution: the color of the yarn is fluorescent green.

[0014] By adopting the above technical solution, the beneficial effects of the present invention are: The yarn coloring process of the present invention has a short processing flow, high efficiency in preparing and processing yarns, and the yarn pulling speed is increased by automated yarn equipment to ensure yarn preparation efficiency; and the present invention can color the yarns at room temperature. The yarns prepared by the yarn coloring process of the present invention have improved yarn strength, and the color fastness can reach above level 4.5. DETAILED DESCRIPTION

[0015] Example 1 This embodiment provides a yarn coloring slurry in a yarn coloring process, wherein the slurry comprises the following raw materials in mass fractions: 85-90% waterborne polyurethane, 0.2-3% accelerator, 1-2% color paste, and the remainder water.

[0016]

[0017] The normal proportion of water and other substances (waterborne polyurethane, accelerator, color paste) in the raw materials is usually 50% each, and the accelerator is usually between 0.2% and 0.5%. If waterborne polyurethane is added, if the amount added is large, it will increase the hardness. The accelerator is within 0.2-3%. The higher the content, the better the adhesion of the color paste and the better the color fixation effect.

[0018] The yarn coloring slurry in this embodiment, water-based polyurethane 85-90%, can be 85%, 87%, 88%, 90% in the above table, can also be any point value between 85-90%; accelerator 0.2-3%, can be 0.2%, 0.3%, 0.4%, 0.5%, 1%, 2%, 3% in the above table, can also be any point value between 0.2-3%; color paste 1-2%, can be 1%, 1.5%, 1.8%, 2% in the above table, can also be any point value between 1-2%.

[0019] The specific accelerator is -150 accelerator, which is a multifunctional cross-linking accelerator with 100% active content. Adding it to the aqueous emulsion dispersion at 0.5-3% can significantly improve its water resistance, chemical resistance, high temperature resistance and adhesion on special substrates. This type of accelerator is a multifunctional cross-linking agent, and its appearance is a colorless and transparent liquid; its scope of use: used to improve the water resistance, washing resistance, chemical resistance and high temperature resistance of film-forming materials; alcohol resistance, washing resistance, chemical resistance and wear resistance; can generally improve the adhesion of water-based systems on non-porous substrates; improve the water resistance and washing resistance of water-based printing inks; anti-stickiness and high temperature resistance.

[0020] It should be added before the coating is used. Due to its excellent miscibility, it can be stirred manually or mechanically. After adding this accelerator, it can be cured naturally at room temperature.

[0021] Example 2 This embodiment provides a yarn coloring process, comprising the following steps: S0: Prepare slurry, which includes the following raw materials by mass fraction: 85-90% waterborne polyurethane, 0.2-3% accelerator, 1-2% color paste, and the rest is water. The raw materials are mixed evenly and placed in a slurry tank; the slurry can adopt any of the yarn coloring slurry formulas in Example 1; S1: Sizing, transferring the yarn from the creel output to the slurry tank for sizing. The slurry tank is provided with a squeezing roller for ensuring uniform sizing of the yarn. The yarn passes through the slurry at room temperature so that the yarn surface is coated with color; S2: drafting, passively drawing the yarn through the drafting roller; S3: Winding, the stretched yarn is wound and stored by a hydraulic winder, which is more stable than a winder with frequency conversion.

[0022] Furthermore, step S11 is provided between step S1 and step S2: drying, in which the moisture on the yarn is evaporated and taken away by a drying device, thereby improving the dryness of the yarn surface.

[0023] Furthermore, the color of the color paste can be any color.

[0024] Furthermore, the color of the color paste is fluorescent green.

[0025] Furthermore, a plurality of drafting rollers are provided, and the yarn is pulled and stretched by cooperating with different drafting rollers, and the direction of the yarn is adjusted by cooperating with a plurality of mesh structures for controlling the direction of the yarn.

[0026] Furthermore, the creel outputs a plurality of yarns at the same time and the yarns are processed by the yarn coloring process to obtain the required yarns.

[0027] Example 3 This embodiment provides a yarn coloring process. The difference between this embodiment and embodiment 2 is that: further, a step S11 is provided between step S1 and step S2: air drying, in which air convection is used to carry away moisture on the yarn surface through air drying equipment, thereby improving the dryness of the yarn surface.

[0028] In this embodiment, the drying equipment in Example 2 is replaced by an air-drying equipment. Regardless of whether it is a drying equipment or an air-drying equipment, its purpose is to speed up the yarn preparation efficiency, increase the drying speed of the yarn, and facilitate winding and molding.

[0029] Example 4 This embodiment provides a yarn, the surface of which is coated with a slurry layer at room temperature.

[0030] Furthermore, the color of the yarn is fluorescent green. The color fastness of the yarn of the present invention can reach above level 4 when the color is fluorescent green, while the color fastness of the colored yarn made in the traditional technology to fluorescent green is not level 4, but usually level 2-3.5.

[0031] According to tests, the yarn prepared by the yarn coloring process of the present invention has improved strength, a color fastness of more than 4.5 levels, and an anti-UV light irradiation test of more than 300 hours.

[0032] Compared with the yarn in the prior art, the yarn has improved strength and better wear resistance. For weaving, the products made of optimized yarn weaving (taking shoe uppers as an example) have improved tensile strength, wear resistance and folding resistance.

[0033] Traditionally, the physical properties of the upper are usually improved through post-processing. The present invention enables the yarn to have the corresponding effect in the pre-process, which to a certain extent reduces the preparation cycle of the upper and improves the manufacturing efficiency.

[0034] The present invention solves the pain point that traditional dyeing and coloring require high temperature and high pressure to color. Among them, high temperature refers to about 130°C. Taking nylon as an example, its coloring temperature is about 110-135°C, and the coloring temperature of polyester is about 135°C; high pressure is 2kg-3KG of pressure to color. The yarns tested so far can be colored at room temperature, such as cotton, linen, nylon, polyester, monofilament, aramid, polyurethane, TPU, and fish silk. The complex process of dyeing is simplified, the processing flow of traditional technology is eliminated, and the energy consumption required for preparation is reduced to a certain extent.

[0035] Further, some data parameters of the yarn produced by the present invention can be known by referring to the following table, wherein the test method is the standard implemented by the test specification:

[0036] As can be seen from the above table, the yarn produced by the present invention has different degrees of improvement in strength and wear resistance compared with ordinary polyester yarn and ordinary cationic yarn.

[0037] The above are only preferred embodiments of the present invention, and therefore cannot be used to limit the scope of the present invention. That is, equivalent changes and modifications made according to the patent scope of the present invention and the contents of the specification should still fall within the scope of the present invention.

Claims

1. A yarn coloring process, It is characterized in that The following steps are involved: S0: Prepare slurry, which includes the following raw materials by mass fraction: 85-90% waterborne polyurethane, 0.2-3% accelerator, 1-2% color paste, and the rest is water. Mix the raw materials evenly and place them in a slurry tank; S1: Sizing, transferring the yarn from the creel output to the slurry tank for sizing. The slurry tank is provided with a squeezing roller for ensuring uniform sizing of the yarn. The yarn passes through the slurry at room temperature so that the yarn surface is coated with color; S2: drafting, passively drawing the yarn through the drafting roller; S3: Winding: The stretched yarn is wound and stored by a hydraulic winder.

2. The yarn coloring process according to claim 1, It is characterized in that A step S11 is further provided between the step S1 and the step S2: drying, in which the moisture on the yarn is evaporated and taken away by a drying device, thereby improving the dryness of the yarn surface.

3. The yarn coloring process according to claim 1, It is characterized in that A step S11 is further provided between the step S1 and the step S2: air drying, wherein air convection is used to remove moisture on the surface of the yarn through air drying equipment, thereby improving the dryness of the yarn surface.

4. The yarn coloring process according to claim 1, It is characterized in that The color of the color paste is any color.

5. The yarn coloring process according to claim 1, It is characterized in that The color of the color paste is fluorescent green.

6. The yarn coloring process according to claim 1, It is characterized in that A plurality of drafting rollers are provided, and the yarn is pulled and stretched by the cooperation of different drafting rollers, and the direction of the yarn is adjusted by the cooperation of a plurality of mesh structures for controlling the direction of the yarn path.

7. The yarn coloring process according to claim 1, It is characterized in that The creel simultaneously outputs a plurality of yarns which are processed by the yarn coloring process to obtain the required yarn.

8. A kind of yarn, It is characterized in that The yarn is obtained by the yarn coloring process according to any one of claims 1 to 7, and the surface of the yarn is coated with a slurry layer at room temperature.

9. The yarn according to claim 8, It is characterized in that The color of the yarn is fluorescent green.

Citation Information

Patent Citations

  • Pigment dyeing method of denim yarn

    CN102605649A

  • Processing process of belt membrane yarn

    CN107304501A

  • Ribbon with leather-like hand feeling and preparation method thereof

    CN114318877A

  • Fluorescent Coating Yarn and Dovie Fabric woven by a Fluorescent Coating Yarn

    KR1020180011031A

  • Process to pigment flame-resistant yarn

    US5076809A