High-paintiness composite energetic film transduction element

By introducing Cu film as a barrier layer into the composite energy-containing film and combining the design of metal bridge chips and NTC thermistors, the problems of low energy output and poor temperature resistance in the prior art are solved. It realizes high-stop feeling and high-efficiency transducer elements with long storage time.

CN119043090AActive Publication Date: 2024-11-29ZHONGBEI UNIV
View PDF 7 Cites 0 Cited by

Patent Information

Application Number
CN202411376777.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-30
Publication Date
2024-11-29
Estimated Expiration
2044-09-30

AI Technical Summary

Technical Problem

The existing composite energy-containing films have low energy release energy at low energy input, and are not resistant to high temperatures and are unstable, making it difficult to achieve high sudden feeling.

Method used

Using an energy-containing film composed of Al film, Cu film and CuO film, combined with the structural design of metal bridge chip, ceramic electrode plug and NTC thermistor, a nickel-chromium bridge film was prepared through magnetron sputtering technology, and in Al A Cu film is added as a barrier layer on the layer to improve the film performance.

Benefits of technology

A higher energy output is achieved, the maximum flame height reaches 5mm, which extends storage time, and high insensitivity requirements are achieved through parallel NTC thermistors to ensure that the components do not fire at 2A4W5min.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119043090A_ABST
    Figure CN119043090A_ABST
Patent Text Reader

Abstract

The invention provides a high-pause composite energetic film transduction element, and belongs to the technical field of initiating explosive devices. The invention discloses a high-pause composite energetic film transduction element, which mainly comprises an energetic film, a metal bridge chip, a ceramic electrode plug and an NTC (Negative Temperature Coefficient) thermistor, the energetic film is formed by compounding an Al film, a Cu film and a CuO film. The Cu film is added between the Al film and the CuO film, so that the performance aging of the composite film can be inhibited, the flame power after long-term storage is improved, and the storage time is prolonged. And the metal bridge chip is connected in parallel with the NTC thermistor, so that 2A4W5min non-ignition can be realized, and the high insensitive requirement is realized.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of pyrotechnics, and in particular to a high-intensity composite energetic film transducer element. Background Art

[0002] Initiators are disposable components and devices that contain explosives and burn or explode when stimulated by external factors to ignite the gunpowder, detonate the explosives, or perform mechanical work. Bridge-type initiators are the most widely used initiators, and are divided into bridge-wire type and bridge-membrane type.

[0003] With the combination of bridge-type ignition devices and MEMS technology, the bridge-film ignition bridge has the characteristics of mass production, micro-integration, high safety, and low cost. According to the material of the bridge-film ignition bridge, it can be divided into metal film bridge, semiconductor film bridge, and composite energetic film bridge. Among them, the composite energetic film ignition bridge is the research focus of film ignition bridge at home and abroad.

[0004] Composite energetic thin films refer to nano-sized particles embedded in a certain thin film material, or multi-layer thin films with a single-layer thickness in the nanometer range, which are periodically constructed in a direction perpendicular to the substrate according to a certain thickness (usually satisfying a certain chemical reaction stoichiometry). The thickness of a single periodic film of the composite energetic thin film ranges from a few nanometers to hundreds of nanometers, the total number of periods ranges from a few to hundreds, and the total thickness of the multi-layer film can reach a few microns to tens of microns. Composite energetic thin films are divided into chemical reaction multilayer films (such as Al / CuO, Al / MoO 3 、Al / Fe 2 O 3 The two types of composite energetic films can undergo violent exothermic reactions at relatively low energy inputs, accompanied by the formation of plasma, and can self-propagate. In addition, the composite reactive films that are currently being studied are usually Al systems, which are prone to oxidation, are not resistant to high temperatures, are unstable, and do not release high energy.

[0005] Therefore, how to obtain a high-sensitivity composite energetic thin film transducer element is a technical problem that needs to be solved at present. Summary of the invention

[0006] The object of the present invention is to provide a high-sensitivity composite energetic thin film transducer element to solve the above technical problems.

[0007] In order to achieve the above-mentioned object of the invention, the present invention provides the following technical solutions:

[0008] The present invention provides a high-sensitivity composite energetic thin film transducer element, which is mainly composed of an energetic thin film, a metal bridge chip, a ceramic electrode plug and an NTC thermistor; the energetic thin film is composited by an Al film, a Cu film and a CuO film;

[0009] The metal bridge chip comprises Al 2 O 3 Ceramic substrate layer, photoresist layer, Ni-Cr film layer and Au pad layer;

[0010] The energetic film is sputtered on the Au pad layer.

[0011] Furthermore, the ceramic electrode plug is cylindrical, and a groove is provided on both the upper surface and the lower surface of the cylinder. The groove on the upper surface is used to encapsulate the metal bridge chip, and the groove on the lower surface is used to encapsulate the NTC thermistor.

[0012] Furthermore, the ceramic electrode plug is formed by sintering a ceramic shell and an electrode.

[0013] Furthermore, the Au pad layer has a groove in the middle, which together with the Ni-Cr film layer forms a metal bridge area, and the metal bridge area is double V-shaped with an angle of 90°;

[0014] The dimensions of the metal bridge area are: 455-465 μm in length, 225-230 μm in width, and 0.80-0.85 μm in thickness.

[0015] Furthermore, the metal bridge chip is connected to the electrode through a silicon-aluminum wire, and the surface of the silicon-aluminum wire is coated with conductive silver paste.

[0016] Further, the NTC thermistor is attached to the groove on the lower surface of the ceramic electrode plug by epoxy resin glue;

[0017] The NTC thermistor is connected to the electrode via a solder sheet.

[0018] Furthermore, in the energetic film, the Cu film is disposed as a barrier layer between the Al film and the CuO film;

[0019] The thickness of the Al film is 80-100 nm, the thickness of the Cu film is 8-12 nm, and the thickness of the CuO is 150-200 nm;

[0020] The modulation period of the energetic film is 238-312 nm, and the number of periods is 10.

[0021] Furthermore, in the metal bridge chip, Al 2 O 3The thickness of the ceramic base layer is 500 μm, the thickness of the photoresist layer is 1-2 μm, the thickness of the Ni-Cr film layer is 0.80-0.85 μm, and the thickness of the Au pad layer is 1-3 μm.

[0022] Furthermore, the depth of the groove on the upper surface of the ceramic electrode plug is 0.5 to 1 mm, and the depth of the groove on the lower surface is 0.5 to 1 mm.

[0023] Beneficial effects of the present invention:

[0024] 1. Compared with the traditional metal bridge, the composite energetic thin film metal bridge provided by the present invention replaces the first-level artificially coated detonator of the traditional metal bridge with the composite energetic thin film layer formed by magnetron sputtering deposition, which is more controllable and safer.

[0025] 2. By designing the modulation period and modulation ratio, the output energy of the transducer element can achieve the effect of reliable ignition with a gap of 1mm, and the maximum flame height is 5mm.

[0026] 3. Adding Cu film between Al film and CuO film can inhibit the performance aging of the composite film, improve the flame power after long storage, and extend the storage time.

[0027] 4. The NTC thermistor is connected in parallel in the bridge area, which can reach 2A4W5min without ignition, realizing high insensitivity requirements. BRIEF DESCRIPTION OF THE DRAWINGS

[0028] Figure 1 This is a schematic diagram of the structure of the high-density composite energetic thin film transducer element obtained by the present invention;

[0029] Figure 2 It is a schematic structural diagram of the metal bridge chip of the present invention;

[0030] Figure 3 is a top view of the metal bridge chip of the present invention;

[0031] Among them, 1-energy-containing film; 2-metal bridge chip; 3-conductive silver paste; 4-ceramic electrode plug; 5-epoxy resin glue; 6-NTC thermistor; 7-tin sheet; 8-electrode; 9-Au pad layer; 10-Ni-Cr film layer; 11-photoresist layer; 12-Al 2 O 3 Ceramic base layer. DETAILED DESCRIPTION

[0032] In order to make the technical problems, technical solutions and beneficial effects to be solved by the present invention more clearly understood, the present invention is further described in detail below in conjunction with the accompanying drawings and embodiments. It should be understood that the specific embodiments described herein are only used to explain the present invention and are not used to limit the present invention.

[0033] like Figure 1-3 As shown, a high-sensitivity composite energetic thin film transducer element is mainly composed of an energetic thin film 1, a metal bridge chip 2, a ceramic electrode plug 4 and an NTC thermistor 6; the energetic thin film 1 is a composite of an Al film, a Cu film and a CuO film;

[0034] The metal bridge chip 2 comprises Al 2 O 3 Ceramic base layer 12, photoresist layer 11, Ni-Cr thin film layer 10 and Au pad layer 9;

[0035] The energetic film 1 is sputtered on the Au pad layer 9 .

[0036] Specifically, an insulating layer is disposed between the energetic film 1 and the Au pad layer 9, and the insulating layer is a CuO layer with a thickness of 300 nm.

[0037] Specifically, the ceramic electrode plug 4 is cylindrical, and a groove is provided on both the upper surface and the lower surface of the cylinder. The groove on the upper surface is used to encapsulate the metal bridge chip 2 , and the groove on the lower surface is used to encapsulate the NTC thermistor 6 .

[0038] Specifically, the ceramic electrode plug 4 is formed by sintering a ceramic shell and an electrode 8, and the ceramic shell is processed with metallized vias.

[0039] Specifically, the Au pad layer 9 has a groove in the middle, and together with the Ni-Cr film layer 10, forms a metal bridge area. Figure 3 The middle shaded part shows a double V shape with an angle of 90°;

[0040] The size of the metal bridge area is: 455-465 μm in length, 225-230 μm in width, and 0.80-0.85 μm in thickness; preferably, the size of the metal bridge area is: 460 μm in length, 230 μm in width, and 0.83 μm in thickness.

[0041] Specifically, the metal bridge chip 2 is connected to the electrode 8 via a silicon-aluminum wire, and the surface of the silicon-aluminum wire is coated with a conductive silver paste 3.

[0042] Specifically, the NTC thermistor 6 is attached to the groove on the lower surface of the ceramic electrode plug 4 by epoxy resin glue 5;

[0043] The NTC thermistor 6 is connected to the electrode 8 via the solder sheet 7, so that the NTC thermistor 6 and the metal bridge region form a parallel circuit.

[0044] Specifically, in the energetic film 1, the Cu film is disposed as a barrier layer between the Al film and the CuO film;

[0045] The thickness of the Al film is 80-100 nm, the thickness of the Cu film is 8-12 nm, and the thickness of CuO is 150-200 nm; preferably, the thickness of the Al film is 90 nm, the thickness of the Cu film is 10 nm, and the thickness of CuO is 180 nm.

[0046] Specifically, the modulation period of the energetic film is 238-312 nm, preferably 280 nm; the number of periods is 10, and the total thickness is 2.8 μm.

[0047] Specifically, in the metal bridge chip 2, Al 2 O 3 The thickness of the ceramic base layer 12 is 500 μm, the thickness of the photoresist layer 11 is 1-2 μm, preferably 2 μm; the thickness of the Ni-Cr film layer 10 is 0.80-0.85 μm, preferably 0.83 μm; the thickness of the Au pad layer 9 is 1-3 μm, preferably 2 μm.

[0048] Specifically, the depth of the groove on the upper surface of the ceramic electrode plug 4 is 0.5-1 mm, preferably 0.5 mm; the depth of the groove on the lower surface is 0.5-1 mm, preferably 0.5 mm.

[0049] Example 1

[0050] The method for preparing the highly insensitive composite energetic thin film transducer element comprises the following steps:

[0051] Step 1: Prepare a nickel-chromium bridge film using magnetron sputtering technology. First, a 500 μm thick, 95% Al 2 O 3 A 1 μm photoresist layer 11 is coated on the ceramic base layer 12 by a coating machine, and a 0.83 μm Ni—Cr thin film layer 10 is sputtered by a magnetron sputtering method.

[0052] Step 2: Use a mask to cover the bridge area, sputter a 2 μm Au pad layer 9 on the Ni-Cr film layer 10, and finally obtain the shape of the pad and the shape of the Ni-Cr metal bridge area by a stripping process. Finally, cut into a single Ni-Cr metal bridge chip 2.

[0053] Step 3: In order to prevent the Al layer in the energetic film 1 from short-circuiting the nickel-chromium metal bridge, a 300nm CuO layer is first sputtered on the surface of the nickel-chromium metal bridge as an insulating layer, and then a 90nm Al layer, a 10nm Cu layer, and a 180nm CuO layer are alternately sputtered thereon to form an Al / Cu / CuO composite energetic film.

[0054] Step 4: Encapsulate the metal bridge chip 2 on the ceramic electrode plug 4. A groove with a depth of 0.5 mm is machined between the two electrodes of the ceramic electrode plug 4, and the metal bridge chip 2 is placed therein. Using an ultrasonic welding process, a silicon aluminum wire is used to connect the pad of the metal bridge chip 2 to the electrode 8. In order to improve the strength of the welding wire, the welding wire is wrapped with a conductive silver paste 3 and heat-dried at 150°C for 1 hour.

[0055] Step 5: dig a 0.5 mm deep groove at the bottom of the ceramic electrode plug 4 for encapsulating the NTC thermistor 6. The encapsulation process is as follows: first, paste the NTC thermistor 6 in the groove with epoxy resin 5, connect the NTC thermistor 6 and the electrode 8 with solder sheet 7, and then encapsulate and cure.

[0056] Example 2

[0057] The method for preparing the highly insensitive composite energetic thin film transducer element comprises the following steps:

[0058] Step 1: Prepare a nickel-chromium bridge film using magnetron sputtering technology. First, a 500 μm thick, 95% Al 2 O 3 A 2 μm photoresist layer 11 is coated on the ceramic base layer 12 by a coating machine, and a 0.85 μm Ni—Cr thin film layer 10 is sputtered by a magnetron sputtering method.

[0059] Step 2: Use a mask to cover the bridge area, sputter a 1 μm Au pad layer 9 on the Ni-Cr film layer 10, and finally obtain the shape of the pad and the shape of the Ni-Cr metal bridge area by a stripping process. Finally, cut into a single Ni-Cr metal bridge chip 2.

[0060] Step 3: In order to prevent the Al layer in the energetic film 1 from short-circuiting the nickel-chromium metal bridge, a 300nm CuO layer is first sputtered on the surface of the nickel-chromium metal bridge as an insulating layer, and then an 80nm Al layer, a 12nm Cu layer, and a 200nm CuO layer are alternately sputtered thereon to form an Al / Cu / CuO composite energetic film.

[0061] Step 4: Encapsulate the metal bridge chip 2 on the ceramic electrode plug 4. A groove with a depth of 0.5 mm is machined between the two electrodes of the ceramic electrode plug 4, and the metal bridge chip 2 is placed therein. Using an ultrasonic welding process, a silicon aluminum wire is used to connect the pad of the metal bridge chip 2 to the electrode 8. In order to improve the strength of the welding wire, the welding wire is wrapped with a conductive silver paste 3 and heat-dried at 150°C for 1 hour.

[0062] Step 5: dig a 0.5 mm deep groove at the bottom of the ceramic electrode plug 4 for encapsulating the NTC thermistor 6. The encapsulation process is as follows: first, paste the NTC thermistor 6 in the groove with epoxy resin 5, connect the NTC thermistor 6 and the electrode 8 with solder sheet 7, and then encapsulate and cure.

[0063] The above is only a preferred embodiment of the present invention. It should be pointed out that for ordinary technicians in this technical field, several improvements and modifications can be made without departing from the principle of the present invention. These improvements and modifications should also be regarded as the scope of protection of the present invention.

Claims

1. A high-density composite energetic thin film transducer element, characterized in that: It is mainly composed of an energetic film, a metal bridge chip, a ceramic electrode plug and an NTC thermistor; the energetic film is a composite of an Al film, a Cu film and a CuO film; The metal bridge chip comprises an Al2O3 ceramic base layer, a photoresist layer, a Ni-Cr film layer and an Au pad layer which are compounded in sequence from bottom to top; The energetic film is sputtered on the Au pad layer.

2. The high-density composite energetic thin film transducer element according to claim 1, characterized in that: The ceramic electrode plug is cylindrical, and a groove is provided on both the upper surface and the lower surface of the cylinder. The groove on the upper surface is used to package the metal bridge chip, and the groove on the lower surface is used to package the NTC thermistor.

3. The high-density composite energetic thin film transducer element according to claim 1 or 2, characterized in that: The ceramic electrode plug is formed by sintering a ceramic shell and an electrode.

4. The high-density composite energetic thin film transducer element according to claim 1, characterized in that: The Au pad layer has a groove in the middle, which together with the Ni-Cr film layer forms a metal bridge area, and the metal bridge area is double V-shaped with an angle of 90°; The dimensions of the metal bridge area are: 455-465 μm in length, 225-230 μm in width, and 0.80-0.85 μm in thickness.

5. The high-density composite energetic thin film transducer element according to claim 1 or 4, characterized in that: The metal bridge chip is connected to the electrode through a silicon-aluminum wire, and the surface of the silicon-aluminum wire is coated with conductive silver paste.

6. The high-density composite energetic thin film transducer element according to claim 5, characterized in that: The NTC thermistor is attached to the groove on the lower surface of the ceramic electrode plug by epoxy resin glue; The NTC thermistor is connected to the electrode via a solder sheet.

7. The high-density composite energetic thin film transducer element according to claim 1, characterized in that: In the energetic film, the Cu film is arranged as a barrier layer between the Al film and the CuO film; The thickness of the Al film is 80-100 nm, the thickness of the Cu film is 8-12 nm, and the thickness of the CuO is 150-200 nm; The modulation period of the energetic film is 238-312 nm, and the number of periods is 10.

8. The high-density composite energetic thin film transducer element according to claim 1, characterized in that: In the metal bridge chip, the thickness of the Al2O3 ceramic base layer is 500 μm, the thickness of the photoresist layer is 1-2 μm, the thickness of the Ni-Cr film layer is 0.80-0.85 μm, and the thickness of the Au pad layer is 1-3 μm.

9. The high-density composite energetic thin film transducer element according to claim 2, characterized in that: The depth of the groove on the upper surface of the ceramic electrode plug is 0.5 to 1 mm, and the depth of the groove on the lower surface is 0.5 to 1 mm.

Citation Information

Patent Citations

  • Semiconductor bridge chip and preparation method thereof

    CN110137090A

  • Composite energetic thin film semiconductor bridge

    CN112254586A

  • Method for inhibiting generation of ordered intermetallic compound in phase change process of Al-Ni nano multilayer film

    CN113481467A

  • High-insensitivity integrated non-contact ignition assembly

    CN115752123A

  • Transduction element based on amorphous alloy

    CN116497258A