Organic compound, organic light-emitting device and display panel

By introducing specific structures into organic compounds to increase the conjugation of boron and nitrogen compounds and improve solubility, the problem of performance limitations of traditional TADF materials is solved, and the luminescence efficiency and life of organic light emitting devices are improved.

CN119060079APending Publication Date: 2024-12-03TCL CHINA STAR OPTOELECTRONICS TECHNOLOGY CO LTD +1
View PDF 3 Cites 0 Cited by

Patent Information

Application Number
CN202411295330.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-13
Publication Date
2024-12-03

AI Technical Summary

Technical Problem

The luminescence efficiency and service life of existing organic electroluminescent devices are limited by the performance of traditional thermal excitation delayed fluorescence (TADF) materials, and it is difficult to significantly improve.

Method used

It provides an organic compound which introduces specific structures such as dianiline, carbazole, benzothiophene, etc. into boron nitrogen compounds to increase the overall conjugation of the molecule, and introduces tetrahydronaphthalene and Structures such as indan improve solubility and purity.

Benefits of technology

It improves the luminous efficiency and service life of organic light emitting devices, and significantly improves the performance and product quality of materials.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119060079A_ABST
    Figure CN119060079A_ABST
Patent Text Reader

Abstract

The invention discloses an organic compound, an organic light-emitting device and a display panel. The organic compound has a structure as shown in a general formula (1) or a general formula (2), according to the organic compound disclosed by the invention, structures such as A-1 (such as diphenylamine), A-2 (such as carbazole), B-1 (such as triphenylene), B-2 (such as dibenzofuran and dibenzothiophene), B-3 (such as a benzo five-membered ring) or B-4 (such as naphthalene) are introduced into a benzene ring connected with an N atom in the boron-nitrogen compound, so that the conjugacy of an arylamine structure in the boron-nitrogen compound is increased; furthermore, the overall conjugacy of organic compound molecules is higher, the material performance is improved, the luminous efficiency of the organic light-emitting device is improved, and the service life of the organic light-emitting device is prolonged.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the field of display, and in particular to an organic compound, an organic light-emitting device and a display panel. Background Art

[0002] At present, organic light-emitting diodes (OLEDs) generally have a positive electrode, a negative electrode, and an organic layer between the positive electrode and the negative electrode, and use the organic material of the organic layer to convert electrical energy into light energy, thereby realizing organic electroluminescence. In order to improve the luminous efficiency and service life of the organic electroluminescent device, the organic layer is often multi-layered, and the organic material of each layer is different. Specifically, the organic layer mainly includes a hole injection layer, a hole transport layer, a light-emitting layer, an electron transport layer, an electron injection layer, etc. A voltage is applied between the positive electrode and the negative electrode of the organic electroluminescent device, the positive electrode injects holes into the organic layer, and the negative electrode injects electrons into the organic layer. The injected holes meet with the electrons to form excitons, and the excitons emit light when they transition back to the ground state, thereby realizing the luminescence of the organic electroluminescent device. Organic electroluminescent devices have the characteristics of autonomous luminescence, high brightness, high efficiency, low voltage drive, wide viewing angle, high contrast, and high response. Therefore, organic electroluminescent devices have broad application prospects.

[0003] In order to improve the luminous efficiency of organic electroluminescent devices, various luminescent material systems based on fluorescence and phosphorescence have been developed. Among them, organic electroluminescent devices using fluorescent materials have the characteristics of high reliability, but under electrical excitation, due to the branching ratio of the singlet excited state and the triplet excited state of the exciton is 1:3, the internal electroluminescent quantum efficiency will be limited to 25%; organic electroluminescent devices using phosphorescent materials have achieved almost 100% internal electroluminescent quantum efficiency, but phosphorescent materials usually use metal complexes containing iridium and platinum, the raw materials are expensive and the synthesis is complicated, and phosphorescent organic electroluminescent devices will also produce a Roll-off effect, that is, the luminous efficiency decreases rapidly with the increase of current or brightness, which limits its application under high brightness.

[0004] In order to overcome the above problems, current luminescent materials are generally various material combinations based on organic compounds, such as composite excited state materials, thermally activated delayed fluorescence (TADF) materials, etc., which attempt to use reverse internal conversion to achieve high efficiency comparable to phosphorescent organic electroluminescent devices. However, the performance improvement of traditional organic compounds with TADF is limited in terms of efficiency and lifespan, resulting in difficulty in improving the luminous efficiency and service life of organic electroluminescent devices using organic compounds with TADF.

[0005] Therefore, an organic compound, an organic electroluminescent device and a display panel are urgently needed to solve the above technical problems. Summary of the invention

[0006] The present application provides an organic compound, an organic light-emitting device and a display panel, which can improve the technical problem that the luminous efficiency and life of the organic light-emitting device of the current organic compound with TADF are difficult to improve.

[0007] The present application provides an organic compound having a structure as shown in general formula (1) or general formula (2):

[0008]

[0009] Wherein, Ar1 has a structure represented by formula (X-1) or formula (X-2):

[0010]

[0011] A1 and A2 have a structure represented by any one of formula (A-1), formula (A-2) or R0, and at least one of A1 and A2 is selected from the structure represented by formula (A-1) or formula (A-2):

[0012]

[0013] R0 means (R3) n3 or (R4) n4 ;

[0014] Ar2 has a structure represented by any one of formula (B-1) to formula (B-4):

[0015]

[0016] X is selected from O, S, N-CH3, N-Ph or C(CH3)2;

[0017] n1, n2, n3, n4 and n5 are independently selected from any integer from 1 to 11;

[0018] R1, R2, R3, R4 and R5 are independently selected from -H, -D, a linear alkyl group having 1 to 20 carbon atoms, a linear alkoxy group having 1 to 20 carbon atoms, a linear thioalkoxy group having 1 to 20 carbon atoms, a branched alkyl group having 3 to 20 carbon atoms, a cyclic alkyl group having 3 to 20 carbon atoms, a branched alkoxy group having 3 to 20 carbon atoms, a cyclic alkoxy group having 3 to 20 carbon atoms, a branched thioalkoxy group having 3 to 20 carbon atoms, a cyclic thioalkoxy group having 3 to 20 carbon atoms, a silyl group, a keto group having 1 to 20 carbon atoms , an alkoxycarbonyl group having 2 to 20 carbon atoms, an aryloxycarbonyl group having 7 to 20 carbon atoms, an olefin group having 1 to 20 carbon atoms, -CN, carbamoyl, haloformyl, formyl, isocyano, isocyanate, thiocyanate, isothiocyanate, hydroxyl, nitro, -CF3, -Cl, -Br, -F, a substituted or unsubstituted aromatic group having 6 to 30 ring atoms, a substituted or unsubstituted heteroaromatic group having 5 to 30 ring atoms, a substituted or unsubstituted aryloxy group having 6 to 30 ring atoms, and a substituted or unsubstituted heteroaryloxy group having 5 to 30 ring atoms;

[0019] When n1 is greater than or equal to 2, two adjacent R1s may or may not form a ring with each other; when n2 is greater than or equal to 2, two adjacent R2s may or may not form a ring with each other; when n3 is greater than or equal to 2, two adjacent R3s may or may not form a ring with each other; when n4 is greater than or equal to 2, two adjacent R4s may or may not form a ring with each other; when n5 is greater than or equal to 2, two adjacent R5s may or may not form a ring with each other.

[0020] In some embodiments, the organic compound has a structure as shown in any one of Formula (2-1) to Formula (2-22):

[0021]

[0022]

[0023]

[0024]

[0025] In some embodiments, R1, R2, R3, R4 and R5 are independently selected from -H, -D, a linear alkyl group having 1 to 10 carbon atoms, a branched alkyl group having 3 to 10 carbon atoms, a cyclic alkyl group having 3 to 10 carbon atoms.

[0026] In some embodiments, R1, R2, R3, R4, and R5 are independently selected from -H, -D, a straight chain alkyl group having 1 to 4 carbon atoms, a branched chain alkyl group having 3 to 5 carbon atoms.

[0027] In some embodiments, the structure represented by formula (B-2) includes as well as At least one of .

[0028] In some embodiments, the organic compound is selected from the compounds represented by the following Formula 1 to Formula 260:

[0029]

[0030]

[0031]

[0032]

[0033]

[0034]

[0035]

[0036]

[0037]

[0038]

[0039]

[0040] The present application also provides an organic light-emitting device, the organic light-emitting device comprising:

[0041] a first electrode;

[0042] A second electrode is disposed opposite to the first electrode; and

[0043] an organic functional layer, located between the first electrode and the second electrode;

[0044] Wherein, the material of the organic functional layer includes one or more of the organic compounds.

[0045] In some embodiments, the organic functional layer includes at least a light-emitting layer, the light-emitting layer includes a host material and a guest material, the guest material includes the organic compound, and the host material includes a condensed aromatic derivative or a heteroaromatic compound.

[0046] In some embodiments, the host material includes one or more of anthracene derivatives, pyrene derivatives, naphthalene derivatives, pentacene derivatives, phenanthrene compounds, fluoranthene compounds, carbazole derivatives, dibenzofuran derivatives, ladder-type furan compounds, and pyrimidine derivatives.

[0047] The present application also provides a display panel, which includes the organic light-emitting device.

[0048] The organic compound of the present application increases the conjugation of the aromatic amine structure in the boron nitrogen compound by introducing structures such as A-1 (such as diphenylamine), A-2 (such as carbazole), B-1 (such as triphenylene), B-2 (such as dibenzofuran, dibenzothiophene), B-3 (such as benzo pentacyclic ring) or B-4 (such as naphthalene) on the benzene ring connected to the N atom in the boron nitrogen compound, thereby making the overall conjugation of the organic compound molecule greater, improving the material properties, increasing the luminous efficiency of the organic light-emitting device and extending the service life of the organic light-emitting device. BRIEF DESCRIPTION OF THE DRAWINGS

[0049] Figure 1 is a schematic structural diagram of an organic light-emitting device provided in an embodiment of the present application;

[0050] Figure 2 It is a schematic diagram of the structure of another organic light-emitting device provided in an embodiment of the present application.

[0051] Figure 3 It is the nuclear magnetic resonance hydrogen spectrum of the organic compound M258 provided in the examples of the present application. DETAILED DESCRIPTION

[0052] The technical solutions in the embodiments of the present application will be described below in conjunction with the drawings in the embodiments of the present application. In addition, it should be understood that the specific implementation methods described herein are only used to illustrate and explain the present application, and are not used to limit the present application. In the present application, unless otherwise stated, the directional words used, such as "upper" and "lower", generally refer to the upper and lower parts of the device in actual use or working state, specifically the drawing direction in the drawings; while "inside" and "outside" refer to the outline of the device. In the present application, "optionally", "optional", and "optional" refer to optional, that is, to any one of the two parallel solutions of "yes" or "no". If multiple "optional" appear in a technical solution, if there is no special explanation and there is no contradiction or mutual restriction, each "optional" is independent. In the present application, the technical features described in an open manner include closed technical solutions composed of the listed features, and also include open technical solutions containing the listed features.

[0053] In the present application, aromatic group, aromatic series and aromatic ring system have the same meaning and can be interchanged.

[0054] In the present application, heteroaromatic group, heteroaromatic series and heteroaromatic ring system have the same meaning and can be interchanged.

[0055] In the present application, "substituted" means that a hydrogen atom in a substituted group is replaced by a substituent.

[0056] In the present application, when the same substituent appears multiple times, it can be independently selected from different groups. If the general formula contains multiple R, then R can be independently selected from different groups.

[0057] In the present application, "substituted or unsubstituted" means that the defined group may be substituted or unsubstituted. When the defined group is substituted, it should be understood that the defined group may be substituted by one or more substituents R, wherein R is selected from but not limited to: deuterium atom, cyano, isocyano, nitro or halogen, alkyl containing 1-20 carbon atoms, heterocyclic group containing 3-20 ring atoms, aromatic group containing 6-20 ring atoms, heteroaromatic group containing 5-20 ring atoms, -NR'R", silane, carbonyl, alkoxycarbonyl, aryloxycarbonyl, carbamoyl, haloformyl, formyl, isocyanate, thiocyanate, isothiocyanate, hydroxyl, trifluoromethyl, and the above groups may be further substituted by substituents acceptable in the art; it is understood that R' and R" in -NR'R" are independently selected from but not limited to: H, deuterium atom, , cyano, isocyano, nitro or halogen, alkyl containing 1-10 carbon atoms, heterocyclic group containing 3-20 ring atoms, aromatic group containing 6-20 ring atoms, heteroaromatic group containing 5-20 ring atoms. Preferably, R is selected from but not limited to: deuterium atom, cyano, isocyano, nitro or halogen, alkyl containing 1-10 carbon atoms, heterocyclic group containing 3-10 ring atoms, aromatic group containing 6-20 ring atoms, heteroaromatic group containing 5-20 ring atoms, silane group, carbonyl group, alkoxycarbonyl group, aryloxycarbonyl group, carbamoyl group, haloformyl group, formyl group, isocyanate group, thiocyanate group, isothiocyanate group, hydroxyl group, trifluoromethyl group, and the above groups can also be further substituted by substituents acceptable in the art.

[0058] In the present application, "ring atoms" refers to the number of atoms in the atoms constituting the ring itself of a structural compound (e.g., a monocyclic compound, a condensed ring compound, a cross-linked compound, a carbocyclic compound, a heterocyclic compound) obtained by atoms bonding to form a ring. When the ring is substituted by a substituent, the atoms contained in the substituent are not included in the ring atoms. The same is true for the "ring atoms" described below, unless otherwise specified. For example, the number of ring atoms of a benzene ring is 6, the number of ring atoms of a naphthalene ring is 10, and the number of ring atoms of a thienyl group is 5.

[0059] In the present application, "aryl or aromatic group" refers to an aromatic hydrocarbon group derived from an aromatic ring compound by removing a hydrogen atom, which can be a monocyclic aromatic group, a condensed aromatic group, or a polycyclic aromatic group. For a polycyclic ring, at least one is an aromatic ring system. For example, "substituted or unsubstituted aromatic group having 6 to 40 ring atoms" refers to an aromatic group containing 6 to 40 ring atoms, preferably a substituted or unsubstituted aromatic group having 6 to 30 ring atoms, more preferably a substituted or unsubstituted aromatic group having 6 to 18 ring atoms, and particularly preferably a substituted or unsubstituted aromatic group having 6 to 14 ring atoms, and the aromatic group is optionally further substituted; suitable examples include, but are not limited to: phenyl, biphenyl, terphenyl, naphthyl, anthracenyl, phenanthrenyl, fluoranthenyl, triphenylene, pyrenyl, perylene, naphthyl, fluorenyl, dinaphthylenyl, acenaphthene and its derivatives. It is understood that multiple aromatic groups may also be interrupted by short non-aromatic units (e.g. <10% non-H atoms, such as C, N or O atoms), such as acenaphthene, fluorene, or 9,9-diarylfluorene, triarylamine, diaryl ether system should also be included in the definition of aromatic group.

[0060] In the present application, "heteroaryl or heteroaromatic group" means that at least one carbon atom is replaced by a non-carbon atom on the basis of an aryl group, and the non-carbon atom can be an N atom, an O atom, an S atom, etc. For example, "substituted or unsubstituted heteroaryl having 5 to 40 ring atoms" means a heteroaryl having 5 to 40 ring atoms, preferably a substituted or unsubstituted heteroaryl having 6 to 30 ring atoms, more preferably a substituted or unsubstituted heteroaryl having 6 to 18 ring atoms, and particularly preferably a substituted or unsubstituted heteroaryl having 6 to 14 ring atoms, and the heteroaryl group is optionally further substituted, and suitable examples include but are not limited to: thienyl, furanyl, pyrrolyl, imidazolyl, oxadiazolyl, triazolyl, imidazolyl, pyridyl, bipyridyl, pyrimidine yl, triazine, acridinyl, pyridazinyl, pyrazinyl, quinolyl, isoquinolyl, quinazolinyl, quinoxalinyl, phthalazinyl, pyridopyrimidinyl, pyridopyrazinyl, benzothienyl, benzofuranyl, indolyl, pyrroloimidazolyl, pyrrolopyrrolyl, thienopyrrolyl, thienothiphenyl, furopyrrolyl, furofuranyl, thienofuranyl, benzisoxazolyl, benzisothiazolyl, benzimidazolyl, o-naphthyl, phenanthridinyl, primary pyridyl, quinazolinone, dibenzothienyl, dibenzofuranyl, carbazolyl and derivatives thereof.

[0061] In the present application, "alkyl" may refer to a linear, branched and / or cyclic alkyl group. The carbon number of the alkyl group may be 1 to 50, 1 to 30, 1 to 20, 1 to 10 or 1 to 6. Phrases containing this term, such as "C 1-9"Alkyl" refers to an alkyl group containing 1 to 9 carbon atoms, and each occurrence may be independently C1 alkyl, C2 alkyl, C3 alkyl, C4 alkyl, C5 alkyl, C6 alkyl, C7 alkyl, C8 alkyl or C9 alkyl. Non-limiting examples of alkyl groups include methyl, ethyl, n-propyl, isopropyl, n-butyl, sec-butyl, tert-butyl, isobutyl, 2-ethylbutyl, 3,3-dimethylbutyl, n-pentyl, isopentyl, neopentyl, tert-pentyl, cyclopentyl, 1-methylpentyl, 3-methylpentyl, 2-ethylpentyl, 4-methyl-2-pentyl, n-hexyl, 1-methylhexyl, 2-ethylhexyl, 2-butylhexyl, cyclohexyl, 4-methylcyclohexyl, 4-tert-butylcyclohexyl, n-heptyl, 1-methylheptyl, 2,2-dimethylheptyl, 2-ethylheptyl, 2-butylheptyl, n-octyl, tert-octyl, 2-ethyloctyl, 2-butyloctyl, 2-hexyloctyl 2-Hexyldecyl, 2-octyldecyl, 2-undecyl, 2-ethyldecyl, 2-butyldecyl, 2-hexyldecyl, 2-octyldecyl, 2-undecyl, 2-ethyldodecyl, 2-butyldodecyl, 2-hexyldodecyl, 2-octyldodecyl, 2-tridecyl, 2-tetradecyl, 2-pentadecyl, 2-hexadecyl, 2-ethylhexadecyl, 2-butylhexadecyl, 2-hexylhexadecyl, 2-octylhexadecyl, 2-heptadecyl, 2-octylhexadecyl, 2-octadecyl, 2-octadecyl, 2-nonadecyl, 2-ethyleicosyl, 2-butyleicosyl, 2-hexyleicosyl, 2-octyleicosyl, 2-heneicosyl, 2-heneicosyl, 2-heconicosyl, 2-docosyl, 2-tricosyl, 2-tetracosyl, 2-pentacosyl, 2-hexacosyl, 2-heptacosyl, 2-octacosyl, 2-nonacosyl, 2-triacontyl, etc.

[0062] In the present application, the substituent abbreviations correspond to: n-normal, sec-secondary, i-iso, t-tertiary, o-ortho, m-meta, p-para, Me methyl, Et ethyl, Pr propyl, Bu butyl, Am n-pentyl, Hx hexyl, Cy cyclohexyl.

[0063] In the present application, "amino" refers to an amine derivative having the structural characteristics of the formula -N(X)2, wherein each "X" is independently H, substituted or unsubstituted alkyl, substituted or unsubstituted cycloalkyl, substituted or unsubstituted heterocyclyl, etc. Non-limiting types of amines include -NH2, -N(alkyl)2, -NH(alkyl), -N(cycloalkyl)2, -NH(cycloalkyl), -N(heterocyclyl), -NH(heterocyclyl), -N(aryl), -NH(aryl), -N(alkyl)(aryl), -N(alkyl)(heterocyclyl), -N(cycloalkyl)(heterocyclyl), -N(aryl)(heteroaryl), -N(alkyl)(heteroaryl), etc.

[0064] In the present application, unless otherwise defined, hydroxyl refers to -OH, carboxyl refers to -COOH, carbonyl refers to -C(=O)-, amino refers to -NH2, formyl refers to -C(=O)H, haloformyl refers to -C(=O)Z (wherein Z represents halogen), carbamoyl refers to -C(=O)NH2, isocyanate refers to -NCO, and isothiocyanate refers to -NCS.

[0065] In the present application, the term "alkoxy" refers to a group having a structure of "-O-alkyl", i.e., an alkyl group as defined above is connected to other groups via an oxygen atom. Phrases containing the term, suitable examples include, but are not limited to, methoxy (-O-CH3 or -OMe), ethoxy (-O-CH2CH3 or -OEt) and tert-butoxy (-OC(CH3)3 or -OtBu).

[0066] In the present application, "*" connected to a single bond indicates a connection or fusion site.

[0067] In the present application, when a linking site is not specified in a group, it means that an optional linking site in the group can be used as a linking site.

[0068] In the present application, when the fusion site is not specified in the group, it means that any fusion site in the group can be used as the fusion site, and preferably two or more sites in the ortho position in the group are fusion sites.

[0069] In the present application, when a group contains multiple substituents with the same symbol, the substituents may be the same or different from each other, for example The six Rs on the benzene ring may be the same as or different from each other.

[0070] In the present application, the single bond to which the substituent is connected runs through the corresponding ring, indicating that the substituent can be connected to any position of the ring, for example In which R is connected to any substitutable position of the benzene ring; express Can be used with The benzene ring can be fused at any position.

[0071] The cyclic alkyl group or cycloalkyl group described in the present application have the same meaning and can be interchanged.

[0072] In the present application, "adjacent groups" means that there is no substitutable site between two substituents.

[0073] In the present application, "two adjacent R1 or R3 or R5 form a ring with each other" means a ring system formed by two adjacent 1 or 3 or R5 connected to each other, and the ring system can be selected from aliphatic hydrocarbon rings, aliphatic heterocycles, aromatic hydrocarbon rings or aromatic heterocycles. Preferably,

[0074] The present application provides an organic compound having a structure as shown in general formula (1) or general formula (2):

[0075]

[0076] Wherein, Ar1 has a structure represented by formula (X-1) or formula (X-2):

[0077]

[0078] A1 and A2 have a structure represented by any one of formula (A-1), formula (A-2) or R0, and at least one of A1 and A2 is selected from the structure represented by formula (A-1) or formula (A-2):

[0079]

[0080] R0 means (R3) n3 or (R4) n4 ;

[0081] Ar2 has a structure represented by any one of formula (B-1) to formula (B-4):

[0082]

[0083] X is selected from O, S, N-CHH3, N-Ph or C(CH3)2;

[0084] n1, n2, n3, n4 and n5 are independently selected from any integer from 1 to 11;

[0085] R1, R2, R3, R4 and R5 are independently selected from -H, -D, a linear alkyl group having 1 to 20 carbon atoms, a linear alkoxy group having 1 to 20 carbon atoms, a linear thioalkoxy group having 1 to 20 carbon atoms, a branched alkyl group having 3 to 20 carbon atoms, a cyclic alkyl group having 3 to 20 carbon atoms, a branched alkoxy group having 3 to 20 carbon atoms, a cyclic alkoxy group having 3 to 20 carbon atoms, a branched thioalkoxy group having 3 to 20 carbon atoms, a cyclic thioalkoxy group having 3 to 20 carbon atoms, a silyl group, a keto group having 1 to 20 carbon atoms , an alkoxycarbonyl group having 2 to 20 carbon atoms, an aryloxycarbonyl group having 7 to 20 carbon atoms, an olefin group having 1 to 20 carbon atoms, -CN, carbamoyl, haloformyl, formyl, isocyano, isocyanate, thiocyanate, isothiocyanate, hydroxyl, nitro, -CF3, -Cl, -Br, -F, a substituted or unsubstituted aromatic group having 6 to 30 ring atoms, a substituted or unsubstituted heteroaromatic group having 5 to 30 ring atoms, a substituted or unsubstituted aryloxy group having 6 to 30 ring atoms, and a substituted or unsubstituted heteroaryloxy group having 5 to 30 ring atoms;

[0086] When n1 is greater than or equal to 2, two adjacent R1s may or may not form a ring with each other; when n2 is greater than or equal to 2, two adjacent R2s may or may not form a ring with each other; when n3 is greater than or equal to 2, two adjacent R3s may or may not form a ring with each other; when n4 is greater than or equal to 2, two adjacent R4s may or may not form a ring with each other; when n5 is greater than or equal to 2, two adjacent R5s may or may not form a ring with each other.

[0087] In some embodiments, the organic compound has a structure as shown in any one of Formula (2-1) to Formula (2-22):

[0088]

[0089]

[0090]

[0091]

[0092] In some embodiments, R1, R2, R3, R4 and R5 are independently selected from -H, -D, a linear alkyl group having 1 to 10 carbon atoms, a branched alkyl group having 3 to 10 carbon atoms, a cyclic alkyl group having 3 to 10 carbon atoms.

[0093] In some embodiments, R1, R2, R3, R4, and R5 are independently selected from -H, -D, a straight chain alkyl group having 1 to 4 carbon atoms, a branched chain alkyl group having 3 to 5 carbon atoms.

[0094] By introducing an alkyl group into the organic compound, it is beneficial to improve the solubility of the organic compound in processes such as inkjet printing, and improve the product quality of the organic light-emitting device using the organic compound.

[0095] In some embodiments, two adjacent R1s are mutually cyclic; further, two adjacent R1s are mutually cyclic to form a 6-membered aromatic ring or aliphatic ring; further, two adjacent R1s are mutually cyclic to form Wherein, * indicates the connection site.

[0096] In some embodiments, two adjacent R2s are mutually cyclic; further, two adjacent R2s are mutually cyclic to form a 6-membered aromatic ring or aliphatic ring; further, two adjacent R2s are mutually cyclic to form Wherein, * indicates the connection site.

[0097] In some embodiments, two adjacent R3s are mutually cyclic; further, two adjacent R3s are mutually cyclic to form a 6-membered aromatic ring or aliphatic ring; further, two adjacent R3s are mutually cyclic to form Wherein, * indicates the connection site.

[0098] In some embodiments, two adjacent R4s are mutually cyclic; further, two adjacent R4s are mutually cyclic to form a 6-membered aromatic ring or aliphatic ring; further, two adjacent R4s are mutually cyclic to form Wherein, * indicates the connection site.

[0099] In some embodiments, two adjacent R5s are mutually cyclic; further, two adjacent R5s are mutually cyclic to form a 6-membered aromatic ring or aliphatic ring; further, two adjacent R5s are mutually cyclic to form Wherein, * indicates the connection site.

[0100] In some embodiments, when Ar2 contains a structure represented by the formula (B-2), the structure represented by the formula (B-2) is selected from:

[0101] as well as At least one of the above is beneficial to improving the luminous efficiency and service life of an organic light-emitting device using the organic compound.

[0102] In some embodiments, the organic compound is a blue light emitting material.

[0103] In some embodiments, the organic compound is selected from the compounds represented by the following Formula 1 to Formula 260:

[0104]

[0105]

[0106]

[0107]

[0108]

[0109]

[0110]

[0111]

[0112]

[0113]

[0114]

[0115] The organic compound provided in the embodiment of the present application is a boron-containing biphenyl organic compound. By further introducing structures such as A-1 (such as diphenylamine), A-2 (such as carbazole), B-1 (such as triphenylene), B-2 (such as dibenzofuran, dibenzothiophene), B-3 (such as benzo pentacyclic ring) or B-4 (such as naphthalene) on the benzene ring connected to the N atom in the boron nitrogen compound, the conjugation of the aromatic amine structure in the boron nitrogen compound is increased, thereby making the overall conjugation of the organic compound molecule greater, thereby improving the luminous efficiency and service life of the organic light-emitting device using the organic compound; at the same time, introducing structures such as tetralin and / or indane into the boron nitrogen compound makes the molecule more soluble in processes such as inkjet printing, facilitates compound purification, thereby improving the purity of the organic compound, and can further extend the luminous efficiency and service life of the organic light-emitting device using the organic compound.

[0116] See also Figure 1 and Figure 2 The present application also provides an organic light-emitting device, which includes: a first electrode 101, a second electrode 102, and an organic functional layer 103. The second electrode 102 is arranged opposite to the first electrode 101, and the organic functional layer 103 is located between the first electrode 101 and the second electrode 102. The material of the organic functional layer 103 includes one or more of the organic compounds described above.

[0117] In some embodiments, the first electrode 101 may be an anode, and the second electrode 102 may be a cathode.

[0118] In some embodiments, the organic light-emitting device can be used for organic light-emitting diodes, organic photovoltaic cells, organic light-emitting cells, organic field effect transistors, organic light-emitting field effect transistors, organic lasers, organic spin electronic devices, organic sensors and organic plasmon emission diodes, etc., preferably organic light-emitting diodes, organic light-emitting cells, and organic light-emitting field effect transistors.

[0119] In some embodiments, the organic light-emitting device can be applied to a variety of electronic devices, such as display panels, lighting devices, light sources, etc.

[0120] In some embodiments, the organic functional layer 103 may be a single layer. In this case, the organic functional layer 103 is a mixture layer, and the mixture layer includes a first compound and a second compound, wherein the first compound is selected from one or more of the organic compounds described above, and the second compound is selected from one or more of hole injection materials, hole transport materials, electron transport materials, hole blocking materials, luminescent guest materials, luminescent host materials, and organic dyes. Detailed descriptions of various organic functional materials included in the organic functional layer 103 are detailed in WO2010135519A1, US20090134784A1, and WO 2011110277A1, and the entire contents of these three patent documents are hereby incorporated herein by reference.

[0121] The luminescent guest material is selected from a singlet luminescent body (fluorescent luminescent body), a triplet luminescent body (phosphorescent luminescent body) and a TADF material.

[0122] When the second compound is selected from one or more of hole injection materials, hole transport materials, electron transport materials, hole blocking materials, light-emitting host materials, and organic dyes, the mass ratio of the first compound to the second compound is 1:99 to 30:70, preferably 1:99 to 10:90.

[0123] When the second compound is a light-emitting guest material, the mass ratio of the first compound to the second compound is 99:1 to 70:30, preferably 99:1 to 90:10.

[0124] In some embodiments, the organic functional layer 103 may include multiple layers. When the organic functional layer 103 is multiple layers, the organic functional layer 103 at least includes a light-emitting layer 107; preferably, the organic functional layer 103 includes a hole injection layer 104, a hole transport layer 105, a light-emitting layer 107, an electron blocking layer 106, an electron injection layer 109, an electron transport layer 108 or a hole blocking layer.

[0125] In some embodiments, the organic light-emitting device can be a blue organic light-emitting device, a green organic light-emitting device or a red organic light-emitting device, and the light-emitting layer 107 can include a host material and a guest material, the guest material is one or more of the organic compounds described above, and the host material includes a fused aromatic derivative or a heteroaromatic compound.

[0126] The light-emitting wavelength of the organic light-emitting device is between 300nm and 1000nm; further, the light-emitting wavelength of the organic light-emitting device is between 35nm0 and 900nm; further, the light-emitting wavelength of the organic light-emitting device is between 400nm and 800nm; further, the light-emitting wavelength of the organic light-emitting device is within the wavelength range of blue light.

[0127] In some embodiments, the host material includes at least one of anthracene derivatives, pyrene derivatives, naphthalene derivatives, pentacene derivatives, phenanthrene compounds, fluoranthene compounds, carbazole derivatives, dibenzofuran derivatives, ladder-type furan compounds, and pyrimidine derivatives. Preferably, the host material is a blue light host material used in a blue organic light-emitting device; when the host material is a blue light host material, the host material is preferably an anthracene organic compound.

[0128] In some embodiments, the mass ratio of the host material to the guest material is 99:1 to 70:30, such as 90:10, 85:15, 80:20, 75:25, etc.; preferably 99:1 to 90:10, such as 97:3, 96:4, 95:5, 93:7, 92:8, etc. The guest material is dispersed in the host material, and the mass ratio of the host material to the guest material is 99:1 to 70:30, which is conducive to inhibiting the crystallization of the light-emitting layer 107 and inhibiting the concentration quenching of the guest material due to high concentration, thereby improving the luminous efficiency of the organic light-emitting device.

[0129] In some embodiments, the anode is an electrode for injecting holes, and the anode can inject holes into the organic functional layer 103, such as: the anode injects holes into the hole injection layer, the hole transport layer or the light-emitting layer. The anode may include at least one of a conductive metal, a conductive metal oxide, or a conductive polymer. Preferably, the absolute value of the difference between the work function of the anode and the HOMO (Highest Occupied Molecular Orbital) energy level or valence band energy level of the light-emitting material in the light-emitting layer, or the p-type semiconductor material in the hole injection layer, the hole transport layer or the electron blocking layer is less than 0.5 eV, preferably less than 0.3 eV, and more preferably less than 0.2 eV. The material of the anode includes but is not limited to: at least one of Al, Cu, Au, Ag, Mg, Fe, Co, Ni, Mn, Pd, Pt, ITO (Indium Tin Oxide), aluminum-doped zinc oxide (AZO), etc., or other suitable and known anode materials, which can be easily selected and used by ordinary technicians in the field. The material of the anode can be deposited using any suitable technique, such as a suitable physical vapor deposition method, including radio frequency magnetron sputtering, vacuum thermal evaporation, electron beam (e-beam), etc. In some embodiments, the anode can be patterned, such as: patterned ITO conductive substrates are commercially available and can be used to prepare the organic light-emitting device of the present application.

[0130] In some embodiments, the cathode is an electrode for injecting electrons, and the cathode can inject electrons into the organic functional layer, such as: the cathode injects electrons into the electron injection layer, the electron transport layer, or the light-emitting layer. The cathode may include at least one of a conductive metal or a conductive metal oxide. Preferably, the absolute value of the difference between the work function of the cathode and the LUMO (Lowest Unoccupied Molecular Orbital) energy level or conduction band energy level of the luminescent material in the light-emitting layer, or the n-type semiconductor material as the electron injection layer, the electron transport layer or the hole blocking layer is less than 0.5 eV, preferably less than 0.3 eV, and more preferably less than 0.2 eV. All materials that can be used as cathodes of organic electronic devices may be used as cathode materials of the organic light-emitting device of the present application, and the materials of the cathode include but are not limited to: at least one of Al, Au, Ag, Ca, Ba, Mg, LiF / Al, MgAg alloy, BaF2 / Al, Cu, Fe, Co, Ni, Mn, Pd, Pt, ITO, etc. The cathode material may be deposited using any suitable technique, such as a suitable physical vapor deposition method, including radio frequency magnetron sputtering, vacuum thermal evaporation, electron beam (e-beam), and the like.

[0131] In some embodiments, the hole injection layer 104 is used to promote the injection of holes from the anode to the light-emitting layer 107, and the hole injection layer 104 includes a hole injection material, which is a material that can receive holes injected from the positive electrode at a low voltage, and preferably, the highest occupied molecular orbital (HOMO) of the hole injection material is between the work function of the material of the anode and the HOMO of the functional material of the film layer (such as the hole transport material of the hole transport layer) into which the holes are injected away from the anode. The hole injection material includes but is not limited to at least one of metal porphyrin, oligothiophene, organic material based on arylamine, organic material based on hexanitrile hexaazatriphenylene, organic material based on quinacridone, organic material based on perylene, anthraquinone, polyaniline-based and polythiophene-based conductive polymers, etc.

[0132] In some embodiments, the hole transport layer 105 can be used to transport holes to the light-emitting layer 107. The hole transport layer 105 includes a hole transport material, which receives holes transmitted from the anode or the hole injection layer and transfers the holes to the light-emitting layer. The hole transport material is a material with high hole mobility known in the art, and the hole transport material may include but is not limited to at least one of an organic material based on arylamine, a conductive polymer, a block copolymer having both a conjugated part and a non-conjugated part, and the like.

[0133] In some embodiments, the electron transport layer 108 is used to transport electrons, and the electron transport layer 108 includes an electron transport material, which receives electrons injected from the negative electrode and transfers the electrons to the light-emitting layer 107. The electron transport material is a material with high electron mobility known in the art, and the electron transport material may include but is not limited to: at least one of an Al complex of 8-hydroxyquinoline, a complex containing Alq3, an organic free radical compound, a hydroxyflavone-metal complex, 8-hydroxyquinoline lithium (LiQ), and a benzimidazole-based compound.

[0134] In some embodiments, the electron injection layer 109 is used to inject electrons, and the electron injection layer 109 includes an electron injection material, and the electron injection material preferably has the ability to transport electrons, has the effect of injecting electrons from the negative electrode, has an excellent effect of injecting electrons into the light-emitting layer 107 or the light-emitting material, and has the ability to prevent the excitons generated by the light-emitting layer 107 from moving to the hole injection layer, and also has an excellent ability to form a thin film. The electron injection material includes, but is not limited to, at least one of 8-hydroxyquinoline lithium (LiQ), fluorenone, anthraquinone dimethane, diphenoquinone, thiopyran dioxide, azole, diazole, triazole, imidazole, perylene tetracarboxylic acid, fluorenyl methane, anthrone, etc. and their derivatives, metal complex compounds, nitrogen-containing 5-membered ring derivatives, etc.

[0135] In some embodiments, the hole blocking layer is used to block holes from reaching the negative electrode, and can generally be formed under the same conditions as the hole injection layer 104. The hole blocking layer includes a hole blocking material, which includes but is not limited to at least one of diazole derivatives or triazole derivatives, phenanthroline derivatives, BCP, aluminum complexes, and the like.

[0136] In some embodiments, the organic light-emitting device further comprises a substrate 110, and the first electrode 101, the hole injection layer 104, the hole transport layer 105, the electron blocking layer 106, the light-emitting layer 107, the electron transport layer 108, the electron injection layer 109, and the second electrode 102 are sequentially stacked on the substrate 110. The substrate 110 may be a transparent substrate or an opaque substrate. When the substrate 110 is a transparent substrate, a transparent organic light-emitting device may be manufactured; the substrate 110 may be a rigid substrate or a flexible substrate with elasticity, and the material of the substrate 110 may include but is not limited to plastic, polymer, metal, semiconductor wafer or glass, etc. Preferably, the substrate 110 comprises at least one smooth surface for forming the anode on the surface. More preferably, the surface has no surface defects. Preferably, the material of the substrate 110 is a polymer film or plastic, including but not limited to polyethylene terephthalate (PET material) and polyethylene glycol (2,6-naphthalene) (PEN material), and the glass transition temperature of the substrate 110 is greater than or equal to 150°C, preferably greater than or equal to 200°C, more preferably greater than or equal to 250°C, and most preferably greater than or equal to 300°C.

[0137] In some embodiments, the organic light-emitting device may be a solution-type organic light-emitting device, that is, at least one of the organic functional layers is prepared by printing (eg, inkjet printing).

[0138] In some embodiments, the mixture layer or the luminescent layer can be formed by a printing or coating process of the composition. The printing or coating process includes inkjet printing, nozzle printing, letterpress printing, screen printing, dip coating, spin coating, blade coating, roller printing, twist roller printing, lithography, flexographic printing, rotary printing, spraying, brushing or pad printing, slit extrusion coating, etc. Preferably, it is gravure printing, nozzle printing and inkjet printing.

[0139] The composition may be a solution or a suspension, and the composition may include a dispersant and a dispersant, wherein the dispersant is one or more of the organic compounds described above, and the dispersant is used to disperse the dispersant.

[0140] In the composition, the mass fraction of the organic compound may be 0.3% to 30%, preferably 0.5% to 20%, more preferably 0.5% to 15%, further preferably 0.5% to 10%, and most preferably 1% to 5%.

[0141] When the composition is used in a printing process, the composition can be an ink, and the viscosity and surface tension of the ink are important parameters. The surface tension parameters of the appropriate ink are suitable for a specific substrate and a specific printing method. In some embodiments, the surface tension of the ink at the working temperature or at 25°C ranges from 19 dyne / cm to 50 dyne / cm; preferably 22 dyne / cm to 35 dyne / cm; more preferably 25 dyne / cm to 33 dyne / cm, which is advantageous for use in an inkjet printing process. In some embodiments, the viscosity of the ink at the working temperature or at 25°C ranges from 1 cps to 100 cps; preferably 1 cps to 50 cps; more preferably 1.5 cps to 20 cps; most preferably 4.0 cps to 20 cps, which is advantageous for use in an inkjet printing process.

[0142] In some embodiments, the Hansen solubility parameter of the dispersant is within the following range: the δd (dispersion force) of the dispersant is between 17.0 and 23.2 MPa. 1 / 2 The range is preferably 18.5 to 21.0 MPa 1 / 2 Range; δp (polar force) is 0.2~12.5MPa 1 / 2 The range is preferably 2.0 to 6.0 MPa. 1 / 2 The range of δh (hydrogen bond force) is 0.9~14.2MPa 1 / 2 The range is preferably 2.0 to 6.0 MPa. 1 / 2 range.

[0143] In some embodiments, the boiling point of the dispersant is greater than or equal to 150° C., preferably greater than or equal to 180° C., more preferably greater than or equal to 200° C., more preferably greater than or equal to 250° C., further preferably greater than or equal to 275° C., and most preferably greater than or equal to 300° C. The boiling point of the dispersant is at least greater than or equal to 150° C., which is beneficial to preventing the nozzle of the inkjet print head from being blocked during inkjet printing, and the higher the boiling point, the more beneficial it is to preventing blockage.

[0144] The dispersant may include at least one organic solvent, which may be evaporated from the solvent system to form a film containing a functional material. The organic solvent may include at least one first organic solvent, which may be selected from aromatic or heteroaromatic. Specifically, the first organic solvent may be selected from p-diisopropylbenzene, pentylbenzene, tetralin, cyclohexylbenzene, chloronaphthalene, 1,4-dimethylnaphthalene, 3-isopropylbiphenyl, p-methylisopropylbenzene, dipentylbenzene, tripentylbenzene, pentyltoluene, o-diethylbenzene, m-diethylbenzene, p-diethylbenzene, 1,2,3,4-tetramethylbenzene, 1,2,3,5-tetramethylbenzene, 1,2,4,5-tetramethylbenzene, butylbenzene, dodecylbenzene, dihexylbenzene, dibutylbenzene, p-diisopropylbenzene, cyclohexylbenzene, benzylbutylbenzene, dimethylnaphthalene, 3-isopropyl Biphenyl, p-methylisopropylbenzene, 1-methylnaphthalene, 1,2,4-trichlorobenzene, 4,4-difluorodiphenylmethane, 1,2-dimethoxy-4-(1-propenyl)benzene, diphenylmethane, 2-phenylpyridine, 3-phenylpyridine, N-methyldiphenylamine, 4-isopropylbiphenyl, α,α-dichlorodiphenylmethane, 4-(3-phenylpropyl)pyridine, benzyl benzoate, 1,1-bis(3,4-dimethylphenyl)ethane, 2-isopropylnaphthalene, quinoline, isoquinoline, methyl 2-furoate, ethyl 2-furoate, etc.

[0145] The first organic solvent can be selected from aromatic ketone solvents. Specifically, the first organic solvent can be selected from 1-tetralone, 2-tetralone, 2-(phenylepoxy)tetralone, 6-(methoxy)tetralone, acetophenone, propiophenone, benzophenone, and their derivatives, such as 4-methylacetophenone, 3-methylacetophenone, 2-methylacetophenone, 4-methylpropiophenone, 3-methylpropiophenone, 2-methylpropiophenone, etc.

[0146] The first organic solvent can be selected from aromatic ether solvents. Specifically, the first organic solvent can be selected from 3-phenoxytoluene, butoxybenzene, p-anisaldehyde dimethyl acetal, tetrahydro-2-phenoxy-2H-pyran, 1,2-dimethoxy-4-(1-propenyl)benzene, 1,4-benzodioxane, 1,3-dipropylbenzene, 2,5-dimethoxytoluene, 4-ethyl ethyl ether, 1,3-dipropoxybenzene, 1,2,4-trimethoxybenzene, 4-(1-propenyl)-1,2-dimethoxybenzene, 1,3-dimethoxybenzene, glycidyl phenyl ether, dibenzyl ether, 4-tert-butylanisole, trans-p-propenylanisole, 1,2-dimethoxybenzene, 1-methoxynaphthalene, diphenyl ether, 2-phenoxymethyl ether, 2-phenoxytetrahydrofuran, ethyl-2-naphthyl ether, etc.

[0147] The first organic solvent may be selected from aliphatic ketones. Specifically, the first organic solvent may be selected from aliphatic ketones, such as 2-nonanone, 3-nonanone, 5-nonanone, 2-decanone, 2,5-hexanedione, 2,6,8-trimethyl-4-nonanone, fenchone, phorone, isophorone, di-n-amyl ketone, etc.; or aliphatic ethers, such as amyl ether, hexyl ether, dioctyl ether, ethylene glycol dibutyl ether, diethylene glycol diethyl ether, diethylene glycol butyl methyl ether, diethylene glycol dibutyl ether, triethylene glycol dimethyl ether, triethylene glycol ethyl methyl ether, triethylene glycol butyl methyl ether, tripropylene glycol dimethyl ether, tetraethylene glycol dimethyl ether, etc.

[0148] The first organic solvent may be selected from organic ester solvents. Specifically, the first solvent may be selected from alkyl octanoate, alkyl sebacate, alkyl stearate, alkyl benzoate, alkyl phenylacetate, alkyl cinnamate, alkyl oxalate, alkyl maleate, alkyl lactone, alkyl oleate, etc. Octyl octanoate, diethyl sebacate, diallyl phthalate, isononyl isononanoate, etc. are particularly preferred.

[0149] The organic solvent may further include a second organic solvent, which may be selected from one or more of methanol, ethanol, 2-methoxyethanol, dichloromethane, chloroform, chlorobenzene, o-dichlorobenzene, tetrahydrofuran, anisole, morpholine, toluene, o-xylene, m-xylene, p-xylene, 1,4-dioxane, acetone, methyl ethyl ketone, 1,2-dichloroethane, 3-phenoxytoluene, 1,1,1-trichloroethane, 1,1,2,2-tetrachloroethane, ethyl acetate, butyl acetate, dimethylformamide, dimethylacetamide, dimethyl sulfoxide, tetralin, decalin, indene and the like.

[0150] In addition to the dispersoid and the dispersant, the composition may also include one or more components such as surfactant compounds, lubricants, wetting agents, dispersants, hydrophobic agents, adhesives, etc., for adjusting viscosity, film-forming properties, improving adhesion, etc.

[0151] The organic compound and the organic light-emitting device of the present application are further described below through specific examples.

[0152] Examples 1 to 20 provide preparation methods and characterization data for organic compounds M1, M2, M5, M6, M7, M8, M9, M10, M193, M201, M209, M233, M241, M242, M251, M252, M257, M258, M259, and M260.

[0153] Example 1

[0154] The synthetic route of organic compound M1 is as follows:

[0155]

[0156] Synthesis of intermediate 1-3:

[0157] Compound 1-1 (10 mmol), compound 1-2 (10 mmol), Pd(dba)2 (bis(dibenzylideneacetonepalladium, 0.1 mmol), TTBP (tri-tert-butylphosphine, 0.2 mmol) and sodium tert-butoxide (30 mmol) were dissolved in toluene and stirred at 100°C for 6 h under a nitrogen atmosphere; after cooling, the solvent was removed by rotary evaporation, and the mixture was extracted and washed with water. The organic phase was subjected to column chromatography to obtain intermediate 1-3 with a molar weight of 8.21 mmol and a yield of 82.1%. The atmospheric pressure solid phase analytical probe mass spectrometry (ASAP-MS) result of intermediate 1-3 was: MS (ASAP) = 337.

[0158] Synthesis of intermediate 1-5:

[0159] Compound 1-3 (10 mmol), compound 1-4 (10 mmol), Pd(dba)2 (bis(dibenzylideneacetonepalladium, 0.1 mmol), TTBP (tri-tert-butylphosphine, 0.2 mmol) and sodium tert-butoxide (30 mmol) were dissolved in toluene and stirred at 100°C for 6 h under a nitrogen atmosphere; after cooling, the solvent was removed by rotary evaporation, and the mixture was extracted and washed with water. The organic phase was subjected to column chromatography to obtain intermediate 1-5 with a molar weight of 7.28 mmol and a yield of 72.8%. The atmospheric pressure solid phase analytical probe mass spectrometry (ASAP-MS) result of intermediate 1-5 was: MS (ASAP) = 481.

[0160] Synthesis of intermediate 1-7:

[0161] Intermediate 1-5 (10 mmol), compound 1-6 (10 mmol), Pd-132 (bis(di-tert-butyl-4-dimethylaminophenylphosphine)palladium chloride, 0.1 mmol), S-Phos (2-dicyclohexylphosphine-2',6'-dimethoxy-1,1'-biphenyl, 0.2 mmol) and sodium tert-butoxide (30 mmol) were dissolved in toluene and stirred at 100°C for 6 h under a nitrogen atmosphere; after cooling, the solvent was removed by rotary evaporation, the mixture was extracted and washed with water, and the organic phase was subjected to column chromatography to obtain intermediate 1-7 with a molar weight of 8.34 mmol and a yield of 83.4%. The atmospheric pressure solid phase analytical probe mass spectrometry (ASAP-MS) result of intermediate 1-7 was: MS (ASAP) = 628.

[0162] Synthesis of intermediate 1-9:

[0163] Intermediate 1-7 (10 mmol), compound 1-8 (10 mmol), Pd2(dba)3 (0.1 mmol), S-Phos (2-dicyclohexylphosphine-2',6'-dimethoxy-1,1'-biphenyl, 0.2 mmol) and sodium tert-butoxide (30 mmol) were dissolved in toluene and stirred at 100°C for 6 h under a nitrogen atmosphere; after cooling, the solvent was removed by rotary evaporation, the mixture was extracted and washed with water, and the organic phase was subjected to column chromatography to obtain intermediate 1-9 with a molar weight of 7.58 mmol and a yield of 75.8%. The atmospheric pressure solid phase analytical probe mass spectrometry (ASAP-MS) result of intermediate 1-9 was: MS (ASAP) = 871.

[0164] Synthesis of intermediate 1-11:

[0165] Intermediate 1-9 (10 mmol) and intermediate 1-10 (10 mmol) were dissolved in a mixed solvent of 1,4-dioxane and water (21 / 2 ml), and Pd(PPh3)4 (0.1 mmol) and potassium carbonate (30 mmol) were added, and stirred at 100°C for 6 h under a nitrogen atmosphere; after cooling, most of the solvent was removed by rotary evaporation, and then the liquid was extracted and washed with water, and the organic phase was subjected to column chromatography and recrystallization to obtain intermediate 1-11 with a molar weight of 7.32 mmol and a yield of 73.2%. The atmospheric pressure solid phase analysis probe mass spectrometry (ASAP-MS) result of intermediate 1-11 was: MS (ASAP) = 1063.

[0166] Synthesis of organic compound M1:

[0167] 10 mmol of intermediate 1-11 and 100 ml of dry tert-butylbenzene were added to a 250 ml three-necked flask, cooled to -30 ° C in a N2 atmosphere, and a n-hexane solution of t-BuLi (tert-butyl lithium) (21 mmol) was added dropwise, the temperature was raised to 60 ° C for 2 hours, and the n-hexane solvent was evaporated under reduced pressure; the reaction solution was cooled to -30 ° C again, boron tribromide (21 mmol) was added, and the temperature was raised to room temperature and stirred for 0.5 hours, and then the reaction solution was cooled to 0 ° C, and 42 mmol After the addition of N,N-diisopropylethylamine is completed, the temperature is raised to room temperature with stirring, and the temperature is further raised to 120° C. with stirring for 3 hours, and the reaction solution is cooled to room temperature; sodium carbonate aqueous solution and ethyl acetate are added to quench the reaction; the aqueous phase is extracted with ethyl acetate and the organic phases are combined, and the solvent therein is evaporated to obtain a crude product, which is purified by a rapid silica gel column to obtain a pure product; recrystallization is performed with toluene and ethyl acetate to obtain a light yellow solid powder, i.e., organic compound M1, with a yield of 41.1%. The atmospheric pressure solid phase analysis probe mass spectrometry (ASAP-MS) result of organic compound M1 is: MS (ASAP) = 1037.

[0168] Example 2

[0169] The synthetic route of organic compound M2 is as follows:

[0170]

[0171] Synthesis of intermediate 2-2:

[0172] Intermediate 1-7 (10 mmol), compound 2-1 (10 mmol), Pd2(dba)3 (0.1 mmol), S-Phos (2-dicyclohexylphosphine-2',6'-dimethoxy-1,1'-biphenyl, 0.2 mmol) and sodium tert-butoxide (30 mmol) were dissolved in toluene and stirred at 100°C for 6 h under a nitrogen atmosphere; after cooling, the solvent was removed by rotary evaporation, the mixture was extracted and washed with water, and the organic phase was subjected to column chromatography to obtain intermediate 2-2 with a molar weight of 8.96 mmol and a yield of 89.6%. The atmospheric pressure solid phase analytical probe mass spectrometry (ASAP-MS) result of intermediate 2-2 was: MS (ASAP) = 869.

[0173] Synthesis of intermediate 2-3:

[0174] Intermediate 2-2 (10 mmol) and intermediate 1-10 (10 mmol) were dissolved in a mixed solvent of 1,4-dioxane and water (21 / 2 ml), and Pd(PPh3)4 (0.1 mmol) and potassium carbonate (30 mmol) were added, and stirred at 100°C for 6 h under a nitrogen atmosphere; after cooling, most of the solvent was removed by rotary evaporation, and then the liquid was extracted and washed with water, and the organic phase was subjected to column chromatography and recrystallization to obtain intermediate 2-3 with a molar weight of 8.11 mmol and a yield of 81.1%. The atmospheric pressure solid phase analysis probe mass spectrometry (ASAP-MS) result of intermediate 2-3 was: MS (ASAP) = 1061.

[0175] Synthesis of organic compound M2:

[0176] 10 mmol of intermediate 2-3 and 100 ml of dry tert-butylbenzene were added to a 250 ml three-necked flask, cooled to -30 ° C in a N2 atmosphere, and a n-hexane solution of t-BuLi (tert-butyl lithium) (21 mmol) was added dropwise, the temperature was raised to 60 ° C for 2 hours, and the n-hexane solvent was evaporated under reduced pressure; the reaction solution was cooled to -30 ° C again, boron tribromide (21 mmol) was added, and the temperature was raised to room temperature and stirred for 0.5 hours, and then the reaction solution was cooled to 0 ° C, and 42 mmol After the addition of N,N-diisopropylethylamine is completed, the temperature is raised to room temperature with stirring, and the temperature is further raised to 120°C with stirring for 3 hours, and the reaction solution is cooled to room temperature; sodium carbonate aqueous solution and ethyl acetate are added to quench the reaction; the aqueous phase is extracted with ethyl acetate and the organic phases are combined, and the solvent therein is evaporated to obtain a crude product, which is purified by a rapid silica gel column to obtain a pure product; recrystallization is performed with toluene and ethyl acetate to obtain a light yellow solid powder, i.e., organic compound M2, with a yield of 42.6%. The atmospheric pressure solid phase analysis probe mass spectrometry (ASAP-MS) result of the organic compound M1 is: MS (ASAP) = 1035.

[0177] Example 3

[0178] The synthetic route of organic compound M5 is as follows:

[0179]

[0180] Synthesis of intermediate 3-2:

[0181] Intermediate 3-1 (10 mmol) and intermediate 1-10 (10 mmol) were dissolved in a mixed solvent of 1,4-dioxane and water (21 / 2 ml), and Pd(PPh3)4 (0.1 mmol) and potassium carbonate (30 mmol) were added, and stirred at 100°C for 6 h under a nitrogen atmosphere; after cooling, most of the solvent was removed by rotary evaporation, and then the liquid was extracted and washed with water, and the organic phase was subjected to column chromatography and recrystallization to obtain intermediate 3-2 with a molar weight of 9.22 mmol and a yield of 92.2%. The atmospheric pressure solid phase analysis probe mass spectrometry (ASAP-MS) result of intermediate 3-2 was: MS (ASAP) = 375.

[0182] Synthesis of intermediate 3-4:

[0183] Compound 3-2 (10 mmol), compound 3-3 (10 mmol), Pd(dba)2 (bis(dibenzylideneacetonepalladium, 0.1 mmol), TTBP (tri-tert-butylphosphine, 0.2 mmol) and sodium tert-butoxide (30 mmol) were dissolved in toluene and stirred at 100°C for 6 h under a nitrogen atmosphere; after cooling, the solvent was removed by rotary evaporation, and the mixture was extracted and washed with water. The organic phase was subjected to column chromatography to obtain intermediate 3-4 with a molar weight of 7.68 mmol and a yield of 76.8%. The atmospheric pressure solid phase analytical probe mass spectrometry (ASAP-MS) result of intermediate 3-4 was: MS (ASAP) = 507.

[0184] Synthesis of intermediate 3-5:

[0185] Compound 3-4 (10 mmol), compound 1-4 (10 mmol), Pd(dba)2 (bis(dibenzylideneacetonepalladium, 0.1 mmol), TTBP (tri-tert-butylphosphine, 0.2 mmol) and sodium tert-butoxide (30 mmol) were dissolved in toluene and stirred at 100°C for 6 h under a nitrogen atmosphere; after cooling, the solvent was removed by rotary evaporation, and the mixture was extracted and washed with water. The organic phase was subjected to column chromatography to obtain intermediate 3-5 with a molar weight of 6.97 mmol and a yield of 69.7%. The atmospheric pressure solid phase analytical probe mass spectrometry (ASAP-MS) result of intermediate 3-5 was: MS (ASAP) = 651.

[0186] Synthesis of intermediate 3-7:

[0187] Intermediate 3-5 (10 mmol), compound 3-6 (10 mmol), Pd-132 (bis(di-tert-butyl-4-dimethylaminophenylphosphine)palladium chloride, 0.1 mmol), S-Phos (2-dicyclohexylphosphine-2',6'-dimethoxy-1,1'-biphenyl, 0.2 mmol) and sodium tert-butoxide (30 mmol) were dissolved in toluene and stirred at 100°C for 6 h under a nitrogen atmosphere; after cooling, the solvent was removed by rotary evaporation, the mixture was extracted and washed with water, and the organic phase was subjected to column chromatography to obtain intermediate 3-7 with a molar weight of 8.41 mmol and a yield of 84.1%. The atmospheric pressure solid phase analytical probe mass spectrometry (ASAP-MS) result of intermediate 3-7 was: MS (ASAP) = 742.

[0188] Synthesis of intermediate 3-8:

[0189] Intermediate 3-7 (10 mmol), compound 1-2 (10 mmol), Pd2(dba)3 (0.1 mmol), S-Phos (2-dicyclohexylphosphine-2',6'-dimethoxy-1,1'-biphenyl, 0.2 mmol) and sodium tert-butoxide (30 mmol) were dissolved in toluene and stirred at 100°C for 6 h under a nitrogen atmosphere; after cooling, the solvent was removed by rotary evaporation, the mixture was extracted and washed with water, and the organic phase was subjected to column chromatography to obtain intermediate 3-8 with a molar weight of 8.26 mmol and a yield of 82.6%. The atmospheric pressure solid phase analytical probe mass spectrometry (ASAP-MS) result of intermediate 3-8 was: MS (ASAP) = 930.

[0190] Synthesis of intermediate 3-10:

[0191] Intermediate 3-8 (10 mmol), intermediate 3-9 (10 mmol), Pd-132 (bis(di-tert-butyl-4-dimethylaminophenylphosphine)palladium chloride, 0.1 mmol), S-Phos (2-dicyclohexylphosphine-2',6'-dimethoxy-1,1'-biphenyl, 0.2 mmol) and sodium tert-butoxide (30 mmol) were dissolved in toluene and stirred at 120° C. for 3 h under a nitrogen atmosphere; after cooling, most of the solvent was removed by rotary evaporation, and then the liquid was extracted and washed with water, and the organic phase was subjected to column chromatography and recrystallization to obtain intermediate 3-10 with a molar weight of 7.33 mmol and a yield of 73.3%. The atmospheric pressure solid phase analytical probe mass spectrometry (ASAP-MS) result of intermediate 3-10 was: MS (ASAP) = 1063.

[0192] Synthesis of organic compound M5:

[0193] In a 250 ml three-necked flask, 10 mmol of intermediate 3-10 and 100 ml of dry tert-butylbenzene were added. The mixture was cooled to -30 °C in a N2 atmosphere. A n-hexane solution of t-BuLi (tert-butyl lithium) (21 mmol) was added dropwise. The temperature was raised to 60 °C for 2 hours. The n-hexane solvent was evaporated under reduced pressure. The reaction solution was cooled to -30 °C again, boron tribromide (21 mmol) was added, and the mixture was heated to room temperature and stirred for 0.5 hours. The reaction solution was then cooled to 0 °C and 42 mmol After the addition of N,N-diisopropylethylamine is completed, the temperature is raised to room temperature with stirring, and the temperature is further raised to 120°C with stirring for 3 hours, and the reaction solution is cooled to room temperature; sodium carbonate aqueous solution and ethyl acetate are added to quench the reaction; the aqueous phase is extracted with ethyl acetate and the organic phases are combined, and the solvent therein is evaporated to obtain a crude product, which is purified by a rapid silica gel column to obtain a pure product; recrystallization is performed with toluene and ethyl acetate to obtain a light yellow solid powder, i.e., organic compound M5, with a yield of 34.9%. The atmospheric pressure solid phase analysis probe mass spectrometry (ASAP-MS) result of organic compound M5 is: MS (ASAP) = 1037.

[0194] Example 4

[0195] The synthetic route of organic compound M6 is as follows:

[0196]

[0197] Synthesis of intermediate 4-2:

[0198] Intermediate 3-8 (10 mmol), intermediate 4-1 (10 mmol), Pd-132 (bis(di-tert-butyl-4-dimethylaminophenylphosphine)palladium chloride, 0.1 mmol), S-Phos (2-dicyclohexylphosphine-2',6'-dimethoxy-1,1'-biphenyl, 0.2 mmol) and sodium tert-butoxide (30 mmol) were dissolved in toluene and stirred at 120°C for 3 h under a nitrogen atmosphere; after cooling, most of the solvent was removed by rotary evaporation, and then the liquid was extracted and washed with water, and the organic phase was subjected to column chromatography and recrystallization to obtain intermediate 4-2 with a molar weight of 8.13 mmol and a yield of 81.3%. The atmospheric pressure solid phase analytical probe mass spectrometry (ASAP-MS) result of intermediate 4-2 was: MS (ASAP) = 1061.

[0199] Synthesis of organic compound M6:

[0200] 10 mmol of intermediate 4-2 and 100 ml of dry tert-butylbenzene were added to a 250 ml three-necked flask, cooled to -30 ° C in a N2 atmosphere, and a n-hexane solution of t-BuLi (tert-butyl lithium) (21 mmol) was added dropwise, the temperature was raised to 60 ° C for 2 hours, and the n-hexane solvent was evaporated under reduced pressure; the reaction solution was cooled to -30 ° C again, boron tribromide (21 mmol) was added, and the temperature was raised to room temperature and stirred for 0.5 hours, and then the reaction solution was cooled to 0 ° C, and 42 mmol After the addition of N,N-diisopropylethylamine is completed, the temperature is raised to room temperature with stirring, and the temperature is further raised to 120°C with stirring for 3 hours, and the reaction solution is cooled to room temperature; sodium carbonate aqueous solution and ethyl acetate are added to quench the reaction; the aqueous phase is extracted with ethyl acetate and the organic phases are combined, and the solvent therein is evaporated to obtain a crude product, which is purified by a rapid silica gel column to obtain a pure product; recrystallization is performed with toluene and ethyl acetate to obtain a light yellow solid powder, i.e., organic compound M5, with a yield of 30.3%. The atmospheric pressure solid phase analysis probe mass spectrometry (ASAP-MS) result of organic compound M6 is: MS (ASAP) = 1035.

[0201] Example 5

[0202] The synthetic route of organic compound M7 is as follows:

[0203]

[0204] Synthesis of intermediate 5-2:

[0205] Intermediate 3-5 (10 mmol), compound 5-1 (10 mmol), Pd-132 (bis(di-tert-butyl-4-dimethylaminophenylphosphine)palladium chloride, 0.1 mmol), S-Phos (2-dicyclohexylphosphine-2',6'-dimethoxy-1,1'-biphenyl, 0.2 mmol) and sodium tert-butoxide (30 mmol) were dissolved in toluene and stirred at 100°C for 6 h under a nitrogen atmosphere; after cooling, the solvent was removed by rotary evaporation, the mixture was extracted and washed with water, and the organic phase was subjected to column chromatography to obtain intermediate 5-2 with a molar weight of 8.03 mmol and a yield of 80.3%. The atmospheric pressure solid phase analytical probe mass spectrometry (ASAP-MS) result of intermediate 5-2 was: MS (ASAP) = 742.

[0206] Synthesis of intermediate 5-3:

[0207] Intermediate 5-2 (10 mmol), compound 1-2 (10 mmol), Pd2(dba)3 (0.1 mmol), S-Phos (2-dicyclohexylphosphine-2',6'-dimethoxy-1,1'-biphenyl, 0.2 mmol) and sodium tert-butoxide (30 mmol) were dissolved in toluene and stirred at 100°C for 6 h under a nitrogen atmosphere; after cooling, the solvent was removed by rotary evaporation, the mixture was extracted and washed with water, and the organic phase was subjected to column chromatography to obtain intermediate 5-3 with a molar weight of 7.84 mmol and a yield of 78.4%. The atmospheric pressure solid phase analytical probe mass spectrometry (ASAP-MS) result of intermediate 5-3 was: MS (ASAP) = 930.

[0208] Synthesis of intermediate 5-4:

[0209] Intermediate 5-3 (10 mmol), intermediate 3-9 (10 mmol), Pd-132 (bis(di-tert-butyl-4-dimethylaminophenylphosphine)palladium chloride, 0.1 mmol), S-Phos (2-dicyclohexylphosphine-2',6'-dimethoxy-1,1'-biphenyl, 0.2 mmol) and sodium tert-butoxide (30 mmol) were dissolved in toluene and stirred at 120°C for 3 h under a nitrogen atmosphere; after cooling, most of the solvent was removed by rotary evaporation, and then the liquid was extracted and washed with water, and the organic phase was subjected to column chromatography and recrystallization to obtain intermediate 5-4 with a molar weight of 7.17 mmol and a yield of 71.7%. The atmospheric pressure solid phase analytical probe mass spectrometry (ASAP-MS) result of intermediate 5-4 was: MS (ASAP) = 1063.

[0210] Synthesis of organic compound M7:

[0211] In a 250 ml three-necked flask, 10 mmol of intermediate 5-4 and 100 ml of dry tert-butylbenzene were added. The mixture was cooled to -30 °C in a N2 atmosphere. A n-hexane solution of t-BuLi (tert-butyl lithium) (21 mmol) was added dropwise. The temperature was raised to 60 °C for 2 hours. The n-hexane solvent was evaporated under reduced pressure. The reaction solution was cooled to -30 °C again, boron tribromide (21 mmol) was added, and the mixture was heated to room temperature and stirred for 0.5 hours. The reaction solution was then cooled to 0 °C and 42 mmol After the addition of N,N-diisopropylethylamine is completed, the temperature is raised to room temperature with stirring, and the temperature is further raised to 120°C with stirring for 3 hours, and the reaction solution is cooled to room temperature; sodium carbonate aqueous solution and ethyl acetate are added to quench the reaction; the aqueous phase is extracted with ethyl acetate and the organic phases are combined, and the solvent therein is evaporated to obtain a crude product, which is purified by a rapid silica gel column to obtain a pure product; recrystallization is performed with toluene and ethyl acetate to obtain a light yellow solid powder, i.e., organic compound M7, with a yield of 45.3%. The atmospheric pressure solid phase analysis probe mass spectrometry (ASAP-MS) result of organic compound M7 is: MS (ASAP) = 1037.

[0212] Example 6

[0213] The synthetic route of organic compound M8 is as follows:

[0214]

[0215] Synthesis of intermediate 6-1:

[0216] Intermediate 5-3 (10 mmol), intermediate 4-1 (10 mmol), Pd-132 (bis(di-tert-butyl-4-dimethylaminophenylphosphine)palladium chloride, 0.1 mmol), S-Phos (2-dicyclohexylphosphine-2',6'-dimethoxy-1,1'-biphenyl, 0.2 mmol) and sodium tert-butoxide (30 mmol) were dissolved in toluene and stirred at 120°C for 3 h under a nitrogen atmosphere; after cooling, most of the solvent was removed by rotary evaporation, and then the liquid was extracted and washed with water, and the organic phase was subjected to column chromatography and recrystallization to obtain intermediate 6-1 with a molar weight of 7.83 mmol and a yield of 78.3%. The atmospheric pressure solid phase analytical probe mass spectrometry (ASAP-MS) result of intermediate 6-1 was: MS (ASAP) = 1061.

[0217] Synthesis of organic compound M8:

[0218] 10 mmol of intermediate 6-1 and 100 ml of dry tert-butylbenzene were added to a 250 ml three-necked flask, cooled to -30 ° C in a N2 atmosphere, and a n-hexane solution of t-BuLi (tert-butyl lithium) (21 mmol) was added dropwise, the temperature was raised to 60 ° C for 2 hours, and the n-hexane solvent was evaporated under reduced pressure; the reaction solution was cooled to -30 ° C again, boron tribromide (21 mmol) was added, and the temperature was raised to room temperature and stirred for 0.5 hours, and then the reaction solution was cooled to 0 ° C, and 42 mmol After the addition of N,N-diisopropylethylamine is completed, the temperature is raised to room temperature with stirring, and the temperature is further raised to 120°C with stirring for 3 hours, and the reaction solution is cooled to room temperature; sodium carbonate aqueous solution and ethyl acetate are added to quench the reaction; the aqueous phase is extracted with ethyl acetate and the organic phases are combined, and the solvent therein is evaporated to obtain a crude product, which is purified by a rapid silica gel column to obtain a pure product; recrystallization is performed with toluene and ethyl acetate to obtain a light yellow solid powder, i.e., organic compound M8, with a yield of 41.3%. The atmospheric pressure solid phase analysis probe mass spectrometry (ASAP-MS) result of organic compound M7 is: MS (ASAP) = 1035.

[0219] Example 7

[0220] The synthetic route of organic compound M9 is as follows:

[0221]

[0222] Synthesis of intermediate 7-1:

[0223] Compound 3-2 (10 mmol), compound 1-4 (10 mmol), Pd(dba)2 (bis(dibenzylideneacetonepalladium, 0.1 mmol), TTBP (tri-tert-butylphosphine, 0.2 mmol) and sodium tert-butoxide (30 mmol) were dissolved in toluene and stirred at 100°C for 6 h under a nitrogen atmosphere; after cooling, the solvent was removed by rotary evaporation, and the mixture was extracted and washed with water. The organic phase was subjected to column chromatography to obtain intermediate 7-1 with a molar weight of 7.81 mmol and a yield of 78.1%. The atmospheric pressure solid phase analytical probe mass spectrometry (ASAP-MS) result of intermediate 7-1 was: MS (ASAP) = 519.

[0224] Synthesis of intermediate 7-2:

[0225] Compound 7-1 (10 mmol), compound 5-1 (10 mmol), Pd(dba)2 (bis(dibenzylideneacetonepalladium, 0.1 mmol), TTBP (tri-tert-butylphosphine, 0.2 mmol) and sodium tert-butoxide (30 mmol) were dissolved in toluene and stirred at 100°C for 6 h under a nitrogen atmosphere; after cooling, the solvent was removed by rotary evaporation, and the mixture was extracted and washed with water. The organic phase was subjected to column chromatography to obtain intermediate 7-2 with a molar weight of 6.33 mmol and a yield of 63.3%. The atmospheric pressure solid phase analytical probe mass spectrometry (ASAP-MS) result of intermediate 7-2 was: MS (ASAP) = 610.

[0226] Synthesis of intermediate 7-3:

[0227] Intermediate 7-2 (10 mmol), compound 1-2 (10 mmol), Pd-132 (bis(di-tert-butyl-4-dimethylaminophenylphosphine)palladium chloride, 0.1 mmol), S-Phos (2-dicyclohexylphosphine-2',6'-dimethoxy-1,1'-biphenyl, 0.2 mmol) and sodium tert-butoxide (30 mmol) were dissolved in toluene and stirred at 100°C for 6 h under a nitrogen atmosphere; after cooling, the solvent was removed by rotary evaporation, the mixture was extracted and washed with water, and the organic phase was subjected to column chromatography to obtain intermediate 7-3 with a molar weight of 8.56 mmol and a yield of 85.6%. The atmospheric pressure solid phase analytical probe mass spectrometry (ASAP-MS) result of intermediate 7-3 was: MS (ASAP) = 798.

[0228] Synthesis of intermediate 7-4:

[0229] Intermediate 7-3 (10 mmol), compound 3-9 (10 mmol), Pd2(dba)3 (0.1 mmol), S-Phos (2-dicyclohexylphosphine-2',6'-dimethoxy-1,1'-biphenyl, 0.2 mmol) and sodium tert-butoxide (30 mmol) were dissolved in toluene and stirred at 100°C for 6 h under a nitrogen atmosphere; after cooling, the solvent was removed by rotary evaporation, the mixture was extracted and washed with water, and the organic phase was subjected to column chromatography to obtain intermediate 7-4 with a molar weight of 7.41 mmol and a yield of 74.1%. The atmospheric pressure solid phase analytical probe mass spectrometry (ASAP-MS) result of intermediate 7-4 was: MS (ASAP) = 931.

[0230] Synthesis of intermediate 7-5:

[0231] Intermediate 7-4 (10 mmol), intermediate 1-8 (10 mmol), Pd-132 (bis(di-tert-butyl-4-dimethylaminophenylphosphine)palladium chloride, 0.1 mmol), S-Phos (2-dicyclohexylphosphine-2',6'-dimethoxy-1,1'-biphenyl, 0.2 mmol) and sodium tert-butoxide (30 mmol) were dissolved in toluene and stirred at 120°C for 3 h under a nitrogen atmosphere; after cooling, most of the solvent was removed by rotary evaporation, and then the liquid was extracted and washed with water, and the organic phase was subjected to column chromatography and recrystallization to obtain intermediate 7-5 with a molar weight of 7.21 mmol and a yield of 72.1%. The atmospheric pressure solid phase analytical probe mass spectrometry (ASAP-MS) result of intermediate 7-5 was: MS (ASAP) = 1174.

[0232] Synthesis of organic compound M9:

[0233] In a 250 ml three-necked flask, 10 mmol of intermediate 7-5 and 100 ml of dry tert-butylbenzene were added. The mixture was cooled to -30 °C in a N2 atmosphere. A n-hexane solution of t-BuLi (tert-butyl lithium) (21 mmol) was added dropwise. The temperature was raised to 60 °C for 2 hours. The n-hexane solvent was evaporated under reduced pressure. The reaction solution was cooled to -30 °C again, boron tribromide (21 mmol) was added, and the mixture was heated to room temperature and stirred for 0.5 hours. The reaction solution was then cooled to 0 °C and 42 mmol After the addition of N,N-diisopropylethylamine is completed, the temperature is raised to room temperature with stirring, and the temperature is further raised to 120° C. with stirring for 3 hours, and the reaction solution is cooled to room temperature; sodium carbonate aqueous solution and ethyl acetate are added to quench the reaction; the aqueous phase is extracted with ethyl acetate and the organic phases are combined, and the solvent therein is evaporated to obtain a crude product, which is purified by a rapid silica gel column to obtain a pure product; recrystallization is performed with toluene and ethyl acetate to obtain a light yellow solid powder, i.e., organic compound M9, with a yield of 26.3%. The atmospheric pressure solid phase analysis probe mass spectrometry (ASAP-MS) result of the organic compound M9 is: MS (ASAP) = 1148.

[0234] Example 8

[0235] The synthetic route of organic compound M10 is as follows:

[0236]

[0237] Synthesis of intermediate 8-2:

[0238] Intermediate 7-4 (10 mmol), intermediate 8-1 (10 mmol), Pd-132 (bis(di-tert-butyl-4-dimethylaminophenylphosphine)palladium chloride, 0.1 mmol), S-Phos (2-dicyclohexylphosphine-2',6'-dimethoxy-1,1'-biphenyl, 0.2 mmol) and sodium tert-butoxide (30 mmol) were dissolved in toluene and stirred at 120°C for 3 h under a nitrogen atmosphere; after cooling, most of the solvent was removed by rotary evaporation, and then the liquid was extracted and washed with water, and the organic phase was subjected to column chromatography and recrystallization to obtain intermediate 8-2 with a molar weight of 7.37 mmol and a yield of 73.7%. The atmospheric pressure solid phase analytical probe mass spectrometry (ASAP-MS) result of intermediate 8-2 was: MS (ASAP) = 1172.

[0239] Synthesis of organic compound M10:

[0240] In a 250 ml three-necked flask, 10 mmol of intermediate 8-2 and 100 ml of dry tert-butylbenzene were added. The mixture was cooled to -30 °C in a N2 atmosphere. A solution of t-BuLi (tert-butyl lithium) (21 mmol) in n-hexane was added dropwise. The temperature was raised to 60 °C for 2 hours. The n-hexane solvent was evaporated under reduced pressure. The reaction solution was cooled to -30 °C again, boron tribromide (21 mmol) was added, and the mixture was heated to room temperature and stirred for 0.5 hours. The reaction solution was then cooled to 0 °C and 42 mmol After the addition of N,N-diisopropylethylamine is completed, the temperature is raised to room temperature with stirring, and the temperature is further raised to 120° C. with stirring for 3 hours, and the reaction solution is cooled to room temperature; sodium carbonate aqueous solution and ethyl acetate are added to quench the reaction; the aqueous phase is extracted with ethyl acetate and the organic phases are combined, and the solvent therein is evaporated to obtain a crude product, which is purified by a rapid silica gel column to obtain a pure product; recrystallization is performed with toluene and ethyl acetate to obtain a light yellow solid powder, i.e., organic compound M10, with a yield of 28.4%. The atmospheric pressure solid phase analysis probe mass spectrometry (ASAP-MS) result of organic compound M10 is: MS (ASAP) = 1146.

[0241] Example 9

[0242] The synthetic route of organic compound M193 is as follows:

[0243]

[0244] Synthesis of intermediate 9-2:

[0245] Intermediate 1-9 (10 mmol) and intermediate 9-1 (10 mmol) were dissolved in a mixed solvent of 1,4-dioxane and water (21 / 2 ml), and Pd(PPh3)4 (0.1 mmol) and potassium carbonate (30 mmol) were added, and stirred at 100°C for 6 h under a nitrogen atmosphere; after cooling, most of the solvent was removed by rotary evaporation, and then the liquid was extracted and washed with water, and the organic phase was subjected to column chromatography and recrystallization to obtain intermediate 9-2 with a molar weight of 7.89 mmol and a yield of 78.9%. The atmospheric pressure solid phase analysis probe mass spectrometry (ASAP-MS) result of intermediate 9-2 was: MS (ASAP) = 1019.

[0246] Synthesis of organic compound M193:

[0247] 10 mmol of intermediate 9-2 and 100 ml of dry tert-butylbenzene were added to a 250 ml three-necked flask, cooled to -30 ° C in a N2 atmosphere, and a n-hexane solution of t-BuLi (tert-butyl lithium) (21 mmol) was added dropwise, the temperature was raised to 60 ° C for 2 hours, and the n-hexane solvent was evaporated under reduced pressure; the reaction solution was cooled to -30 ° C again, boron tribromide (21 mmol) was added, and the temperature was raised to room temperature and stirred for 0.5 hours, and then the reaction solution was cooled to 0 ° C, and 42 mmol After the addition of N,N-diisopropylethylamine is completed, the temperature is raised to room temperature with stirring, and the temperature is further raised to 120°C with stirring for 3 hours, and the reaction solution is cooled to room temperature; sodium carbonate aqueous solution and ethyl acetate are added to quench the reaction; the aqueous phase is extracted with ethyl acetate and the organic phases are combined, and the solvent therein is evaporated to obtain a crude product, which is purified by a rapid silica gel column to obtain a pure product; recrystallization is performed with toluene and ethyl acetate to obtain a light yellow solid powder, i.e., organic compound M193, with a yield of 35.1%. The atmospheric pressure solid phase analysis probe mass spectrometry (ASAP-MS) result of the organic compound M193 is: MS (ASAP) = 993.

[0248] Example 10

[0249] The synthetic route of organic compound M201 is as follows:

[0250]

[0251] Synthesis of intermediate 10-2:

[0252] Intermediate 1-9 (10 mmol) and intermediate 10-1 (10 mmol) were dissolved in a mixed solvent of 1,4-dioxane and water (21 / 2 ml), and Pd(PPh3)4 (0.1 mmol) and potassium carbonate (30 mmol) were added, and stirred at 100°C for 6 h under a nitrogen atmosphere; after cooling, most of the solvent was removed by rotary evaporation, and then the liquid was extracted and washed with water, and the organic phase was subjected to column chromatography and recrystallization to obtain intermediate 10-2 with a molar weight of 8.17 mmol and a yield of 81.7%. The atmospheric pressure solid phase analysis probe mass spectrometry (ASAP-MS) result of intermediate 10-2 was: MS (ASAP) = 1016.

[0253] Synthesis of organic compound M201:

[0254] In a 250 ml three-necked flask, 10 mmol of intermediate 10-2 and 100 ml of dry tert-butylbenzene were added. The mixture was cooled to -30 °C in a N2 atmosphere. A solution of t-BuLi (tert-butyl lithium) (21 mmol) in n-hexane was added dropwise. The temperature was raised to 60 °C for 2 hours. The n-hexane solvent was evaporated under reduced pressure. The reaction solution was cooled to -30 °C again, boron tribromide (21 mmol) was added, and the mixture was heated to room temperature and stirred for 0.5 hours. The reaction solution was then cooled to 0 °C and 42 mmol After the addition of N,N-diisopropylethylamine is completed, the temperature is raised to room temperature with stirring, and the temperature is further raised to 120°C with stirring for 3 hours, and the reaction solution is cooled to room temperature; sodium carbonate aqueous solution and ethyl acetate are added to quench the reaction; the aqueous phase is extracted with ethyl acetate and the organic phases are combined, and the solvent therein is evaporated to obtain a crude product, which is purified by a rapid silica gel column to obtain a pure product; recrystallization is performed with toluene and ethyl acetate to obtain a light yellow solid powder, i.e., organic compound M201, with a yield of 39.3%. The atmospheric pressure solid phase analysis probe mass spectrometry (ASAP-MS) result of the organic compound M201 is: MS (ASAP) = 990.

[0255] Embodiment 11

[0256] The synthetic route of organic compound M209 is as follows:

[0257]

[0258] Synthesis of intermediate 11-2:

[0259] Intermediate 1-9 (10 mmol) and intermediate 11-1 (10 mmol) were dissolved in a mixed solvent of 1,4-dioxane and water (21 / 2 ml), and Pd(PPh3)4 (0.1 mmol) and potassium carbonate (30 mmol) were added, and stirred at 100°C for 6 h under a nitrogen atmosphere; after cooling, most of the solvent was removed by rotary evaporation, and then the liquid was extracted and washed with water, and the organic phase was subjected to column chromatography and recrystallization to obtain intermediate 11-2 with a molar weight of 8.36 mmol and a yield of 83.6%. The atmospheric pressure solid phase analysis probe mass spectrometry (ASAP-MS) result of intermediate 11-2 was: MS (ASAP) = 967.

[0260] Synthesis of organic compound M209:

[0261] 10 mmol of intermediate 11-2 and 100 ml of dry tert-butylbenzene were added to a 250 ml three-necked flask, cooled to -30 ° C in a N2 atmosphere, and a n-hexane solution of t-BuLi (tert-butyl lithium) (21 mmol) was added dropwise. The temperature was raised to 60 ° C and the reaction was carried out for 2 hours. The n-hexane solvent was evaporated under reduced pressure; the reaction solution was cooled to -30 ° C again, boron tribromide (21 mmol) was added, and the temperature was raised to room temperature and stirred for 0.5 hours. Then the reaction solution was cooled to 0 ° C, and 42 mmol After the addition of N,N-diisopropylethylamine is completed, the temperature is raised to room temperature with stirring, and the temperature is further raised to 120°C with stirring for 3 hours, and the reaction solution is cooled to room temperature; sodium carbonate aqueous solution and ethyl acetate are added to quench the reaction; the aqueous phase is extracted with ethyl acetate and the organic phases are combined, and the solvent therein is evaporated to obtain a crude product, which is purified by a rapid silica gel column to obtain a pure product; recrystallization is performed with toluene and ethyl acetate to obtain a light yellow solid powder, i.e., organic compound M209, with a yield of 32.5%. The atmospheric pressure solid phase analysis probe mass spectrometry (ASAP-MS) result of the organic compound M209 is: MS (ASAP) = 941.

[0262] Example 12

[0263] The synthetic route of organic compound M233 is as follows:

[0264]

[0265] Synthesis of intermediate 12-2:

[0266] Intermediate 1-9 (10 mmol) and intermediate 12-1 (10 mmol) were dissolved in a mixed solvent of 1,4-dioxane and water (21 / 2 ml), and Pd(PPh3)4 (0.1 mmol) and potassium carbonate (30 mmol) were added, and stirred at 100°C for 6 h under a nitrogen atmosphere; after cooling, most of the solvent was removed by rotary evaporation, and then the liquid was extracted and washed with water, and the organic phase was subjected to column chromatography and recrystallization to obtain intermediate 12-2 with a molar weight of 6.41 mmol and a yield of 64.1%. The atmospheric pressure solid phase analysis probe mass spectrometry (ASAP-MS) result of intermediate 12-2 was: MS (ASAP) = 953.

[0267] Synthesis of organic compound M233:

[0268] 10 mmol of intermediate 12-2 and 100 ml of dry tert-butylbenzene were added to a 250 ml three-necked flask, cooled to -30 ° C in a N2 atmosphere, and a n-hexane solution of t-BuLi (tert-butyl lithium) (21 mmol) was added dropwise. The temperature was raised to 60 ° C and the reaction was carried out for 2 hours. The n-hexane solvent was evaporated under reduced pressure; the reaction solution was cooled to -30 ° C again, boron tribromide (21 mmol) was added, and the temperature was raised to room temperature and stirred for 0.5 hours. Then the reaction solution was cooled to 0 ° C, and 42 mmol After the addition of N,N-diisopropylethylamine is completed, the temperature is raised to room temperature with stirring, and the temperature is further raised to 120°C with stirring for 3 hours, and the reaction solution is cooled to room temperature; sodium carbonate aqueous solution and ethyl acetate are added to quench the reaction; the aqueous phase is extracted with ethyl acetate and the organic phases are combined, and the solvent therein is evaporated to obtain a crude product, which is purified by a rapid silica gel column to obtain a pure product; recrystallization is performed with toluene and ethyl acetate to obtain a light yellow solid powder, i.e., organic compound M233, with a yield of 33.8%. The atmospheric pressure solid phase analysis probe mass spectrometry (ASAP-MS) result of the organic compound M233 is: MS (ASAP) = 927.

[0269] Example 13

[0270] The synthetic route of organic compound M241 is as follows:

[0271]

[0272] Synthesis of intermediate 13-2:

[0273] Intermediate 1-7 (10 mmol), compound 13-1 (10 mmol), Pd2(dba)3 (0.1 mmol), S-Phos (2-dicyclohexylphosphine-2',6'-dimethoxy-1,1'-biphenyl, 0.2 mmol) and sodium tert-butoxide (30 mmol) were dissolved in toluene and stirred at 100°C for 6 h under a nitrogen atmosphere; after cooling, the solvent was removed by rotary evaporation, the mixture was extracted and washed with water, and the organic phase was subjected to column chromatography to obtain intermediate 13-2 with a molar weight of 7.22 mmol and a yield of 72.2%. The atmospheric pressure solid phase analytical probe mass spectrometry (ASAP-MS) result of intermediate 13-2 was: MS (ASAP) = 983.

[0274] Synthesis of intermediate 13-3:

[0275] Intermediate 13-2 (10 mmol) and intermediate 1-10 (10 mmol) were dissolved in a mixed solvent of 1,4-dioxane and water (21 / 2 ml), and Pd(PPh3)4 (0.1 mmol) and potassium carbonate (30 mmol) were added, and stirred at 100°C for 6 h under a nitrogen atmosphere; after cooling, most of the solvent was removed by rotary evaporation, and then the liquid was extracted and washed with water, and the organic phase was subjected to column chromatography and recrystallization to obtain intermediate 13-3 with a molar weight of 7.03 mmol and a yield of 70.3%. The atmospheric pressure solid phase analysis probe mass spectrometry (ASAP-MS) result of intermediate 13-3 was: MS (ASAP) = 1175.

[0276] Synthesis of organic compound M241:

[0277] 10 mmol of intermediate 13-3 and 100 ml of dry tert-butylbenzene were added to a 250 ml three-necked flask, cooled to -30 ° C in a N2 atmosphere, and a n-hexane solution of t-BuLi (tert-butyl lithium) (21 mmol) was added dropwise. The temperature was raised to 60 ° C and reacted for 2 hours. The n-hexane solvent was evaporated under reduced pressure; the reaction solution was cooled to -30 ° C again, boron tribromide (21 mmol) was added, and the temperature was raised to room temperature and stirred for 0.5 hours. Then the reaction solution was cooled to 0 ° C, and 42 mmol After the addition of N,N-diisopropylethylamine is completed, the temperature is raised to room temperature with stirring, and the temperature is further raised to 120°C with stirring for 3 hours, and the reaction solution is cooled to room temperature; sodium carbonate aqueous solution and ethyl acetate are added to quench the reaction; the aqueous phase is extracted with ethyl acetate and the organic phases are combined, and the solvent therein is evaporated to obtain a crude product, which is purified by a rapid silica gel column to obtain a pure product; recrystallization is performed with toluene and ethyl acetate to obtain a light yellow solid powder, i.e., organic compound M241, with a yield of 36.2%. The atmospheric pressure solid phase analysis probe mass spectrometry (ASAP-MS) result of the organic compound M241 is: MS (ASAP) = 1149.

[0278] Embodiment 14

[0279] The synthetic route of organic compound M242 is as follows:

[0280]

[0281] Synthesis of intermediate 14-2:

[0282] Intermediate 1-7 (10 mmol), compound 14-1 (10 mmol), Pd2(dba)3 (0.1 mmol), S-Phos (2-dicyclohexylphosphine-2',6'-dimethoxy-1,1'-biphenyl, 0.2 mmol) and sodium tert-butoxide (30 mmol) were dissolved in toluene and stirred at 100°C for 6 h under a nitrogen atmosphere; after cooling, the solvent was removed by rotary evaporation, the mixture was extracted and washed with water, and the organic phase was subjected to column chromatography to obtain intermediate 14-2 with a molar weight of 7.51 mmol and a yield of 75.1%. The atmospheric pressure solid phase analytical probe mass spectrometry (ASAP-MS) result of intermediate 14-2 was: MS (ASAP) = 981.

[0283] Synthesis of intermediate 14-3:

[0284] Intermediate 14-2 (10 mmol) and intermediate 1-10 (10 mmol) were dissolved in a mixed solvent of 1,4-dioxane and water (21 / 2 ml), and Pd(PPh3)4 (0.1 mmol) and potassium carbonate (30 mmol) were added, and stirred at 100°C for 6 h under a nitrogen atmosphere; after cooling, most of the solvent was removed by rotary evaporation, and then the liquid was extracted and washed with water, and the organic phase was subjected to column chromatography and recrystallization to obtain intermediate 14-3 with a molar weight of 7.63 mmol and a yield of 76.3%. The atmospheric pressure solid phase analysis probe mass spectrometry (ASAP-MS) result of intermediate 14-3 was: MS (ASAP) = 1173.

[0285] Synthesis of organic compound M242:

[0286] 10 mmol of intermediate 14-3 and 100 ml of dry tert-butylbenzene were added to a 250 ml three-necked flask, cooled to -30 ° C in a N2 atmosphere, and a n-hexane solution of t-BuLi (tert-butyl lithium) (21 mmol) was added dropwise. The temperature was raised to 60 ° C and the reaction was carried out for 2 hours. The n-hexane solvent was evaporated under reduced pressure; the reaction solution was cooled to -30 ° C again, boron tribromide (21 mmol) was added, and the temperature was raised to room temperature and stirred for 0.5 hours. Then the reaction solution was cooled to 0 ° C, and 42 mmol After the addition of N,N-diisopropylethylamine is completed, the temperature is raised to room temperature with stirring, and the temperature is further raised to 120°C with stirring for 3 hours, and the reaction solution is cooled to room temperature; sodium carbonate aqueous solution and ethyl acetate are added to quench the reaction; the aqueous phase is extracted with ethyl acetate and the organic phases are combined, and the solvent therein is evaporated to obtain a crude product, which is purified by a rapid silica gel column to obtain a pure product; recrystallization is performed with toluene and ethyl acetate to obtain a light yellow solid powder, i.e., organic compound M242, with a yield of 33.2%. The atmospheric pressure solid phase analysis probe mass spectrometry (ASAP-MS) result of the organic compound M242 is: MS (ASAP) = 1147.

[0287] Embodiment 15

[0288] The synthetic route of organic compound M251 is as follows:

[0289]

[0290] Synthesis of intermediate 15-1:

[0291] Compound 7-1 (10 mmol), compound 3-6 (10 mmol), Pd(dba)2 (bis(dibenzylideneacetonepalladium, 0.1 mmol), TTBP (tri-tert-butylphosphine, 0.2 mmol) and sodium tert-butoxide (30 mmol) were dissolved in toluene and stirred at 100°C for 6 h under a nitrogen atmosphere; after cooling, the solvent was removed by rotary evaporation, and the mixture was extracted and washed with water. The organic phase was subjected to column chromatography to obtain intermediate 15-1 with a molar weight of 6.08 mmol and a yield of 60.8%. The atmospheric pressure solid phase analytical probe mass spectrometry (ASAP-MS) result of intermediate 15-1 was: MS (ASAP) = 610.

[0292] Synthesis of intermediate 15-2:

[0293] Intermediate 15-1 (10 mmol), compound 1-2 (10 mmol), Pd-132 (bis(di-tert-butyl-4-dimethylaminophenylphosphine)palladium chloride, 0.1 mmol), S-Phos (2-dicyclohexylphosphine-2',6'-dimethoxy-1,1'-biphenyl, 0.2 mmol) and sodium tert-butoxide (30 mmol) were dissolved in toluene and stirred at 100°C for 6 h under a nitrogen atmosphere; after cooling, the solvent was removed by rotary evaporation, the mixture was extracted and washed with water, and the organic phase was subjected to column chromatography to obtain intermediate 15-2 with a molar weight of 8.17 mmol and a yield of 81.7%. The atmospheric pressure solid phase analytical probe mass spectrometry (ASAP-MS) result of intermediate 15-2 was: MS (ASAP) = 798.

[0294] Synthesis of intermediate 15-4:

[0295] Intermediate 15-2 (10 mmol), compound 15-3 (10 mmol), Pd2(dba)3 (0.1 mmol), S-Phos (2-dicyclohexylphosphine-2',6'-dimethoxy-1,1'-biphenyl, 0.2 mmol) and sodium tert-butoxide (30 mmol) were dissolved in toluene and stirred at 100°C for 6 h under a nitrogen atmosphere; after cooling, the solvent was removed by rotary evaporation, the mixture was extracted and washed with water, and the organic phase was subjected to column chromatography to obtain intermediate 15-4 with a molar weight of 7.27 mmol and a yield of 72.7%. The atmospheric pressure solid phase analytical probe mass spectrometry (ASAP-MS) result of intermediate 15-4 was: MS (ASAP) = 1041.

[0296] Synthesis of intermediate 15-6:

[0297] Intermediate 15-4 (10 mmol), intermediate 15-5 (10 mmol), Pd-132 (bis(di-tert-butyl-4-dimethylaminophenylphosphine)palladium chloride, 0.1 mmol), S-Phos (2-dicyclohexylphosphine-2',6'-dimethoxy-1,1'-biphenyl, 0.2 mmol) and sodium tert-butoxide (30 mmol) were dissolved in toluene and stirred at 120°C for 3 h under a nitrogen atmosphere; after cooling, most of the solvent was removed by rotary evaporation, and then the liquid was extracted and washed with water, and the organic phase was subjected to column chromatography and recrystallization to obtain intermediate 15-6 with a molar weight of 7.03 mmol and a yield of 70.3%. The atmospheric pressure solid phase analytical probe mass spectrometry (ASAP-MS) result of intermediate 15-6 was: MS (ASAP) = 1228.

[0298] Synthesis of organic compound M251:

[0299] 10 mmol of intermediate 15-6 and 100 ml of dry tert-butylbenzene were added to a 250 ml three-necked flask, cooled to -30 ° C in a N2 atmosphere, and a n-hexane solution of t-BuLi (tert-butyl lithium) (21 mmol) was added dropwise. The temperature was raised to 60 ° C and the reaction was carried out for 2 hours. The n-hexane solvent was evaporated under reduced pressure. The reaction solution was cooled to -30 ° C again, boron tribromide (21 mmol) was added, and the temperature was raised to room temperature and stirred for 0.5 hours. Then the reaction solution was cooled to 0 ° C, and 42 mmol After the addition of N,N-diisopropylethylamine is completed, the temperature is raised to room temperature with stirring, and the temperature is further raised to 120°C with stirring for 3 hours, and the reaction solution is cooled to room temperature; sodium carbonate aqueous solution and ethyl acetate are added to quench the reaction; the aqueous phase is extracted with ethyl acetate and the organic phases are combined, and the solvent therein is evaporated to obtain a crude product, which is purified by a rapid silica gel column to obtain a pure product; recrystallization is performed with toluene and ethyl acetate to obtain a light yellow solid powder, i.e., organic compound M251, with a yield of 34.3%. The atmospheric pressure solid phase analysis probe mass spectrometry (ASAP-MS) result of the organic compound M251 is: MS (ASAP) = 1202.

[0300] Example 16

[0301] The synthetic route of organic compound M252 is as follows:

[0302]

[0303] Synthesis of intermediate 16-2:

[0304] Intermediate 15-2 (10 mmol), compound 16-1 (10 mmol), Pd2(dba)3 (0.1 mmol), S-Phos (2-dicyclohexylphosphine-2',6'-dimethoxy-1,1'-biphenyl, 0.2 mmol) and sodium tert-butoxide (30 mmol) were dissolved in toluene and stirred at 100°C for 6 h under a nitrogen atmosphere; after cooling, the solvent was removed by rotary evaporation, the mixture was extracted and washed with water, and the organic phase was subjected to column chromatography to obtain intermediate 16-2 with a molar weight of 7.36 mmol and a yield of 73.6%. The atmospheric pressure solid phase analytical probe mass spectrometry (ASAP-MS) result of intermediate 16-2 was: MS (ASAP) = 1039.

[0305] Synthesis of intermediate 16-3:

[0306] Intermediate 16-2 (10 mmol), intermediate 15-5 (10 mmol), Pd-132 (bis(di-tert-butyl-4-dimethylaminophenylphosphine)palladium chloride, 0.1 mmol), S-Phos (2-dicyclohexylphosphine-2',6'-dimethoxy-1,1'-biphenyl, 0.2 mmol) and sodium tert-butoxide (30 mmol) were dissolved in toluene and stirred at 120°C for 3 h under a nitrogen atmosphere; after cooling, most of the solvent was removed by rotary evaporation, and then the liquid was extracted and washed with water, and the organic phase was subjected to column chromatography and recrystallization to obtain intermediate 16-3 with a molar weight of 6.35 mmol and a yield of 63.5%. The atmospheric pressure solid phase analytical probe mass spectrometry (ASAP-MS) result of intermediate 16-3 was: MS (ASAP) = 1226.

[0307] Synthesis of organic compound M252:

[0308] 10 mmol of intermediate 16-3 and 100 ml of dry tert-butylbenzene were added to a 250 ml three-necked flask, cooled to -30 ° C in a N2 atmosphere, and a n-hexane solution of t-BuLi (tert-butyl lithium) (21 mmol) was added dropwise. The temperature was raised to 60 ° C and the reaction was carried out for 2 hours. The n-hexane solvent was evaporated under reduced pressure; the reaction solution was cooled to -30 ° C again, boron tribromide (21 mmol) was added, and the temperature was raised to room temperature and stirred for 0.5 hours. Then the reaction solution was cooled to 0 ° C, and 42 mmol After the addition of N,N-diisopropylethylamine is completed, the temperature is raised to room temperature with stirring, and the temperature is further raised to 120°C with stirring for 3 hours, and the reaction solution is cooled to room temperature; sodium carbonate aqueous solution and ethyl acetate are added to quench the reaction; the aqueous phase is extracted with ethyl acetate and the organic phases are combined, and the solvent therein is evaporated to obtain a crude product, which is purified by a rapid silica gel column to obtain a pure product; recrystallization is performed with toluene and ethyl acetate to obtain a light yellow solid powder, i.e., organic compound M252, with a yield of 45.2%. The atmospheric pressure solid phase analysis probe mass spectrometry (ASAP-MS) result of the organic compound M252 is: MS (ASAP) = 1200.

[0309] Embodiment 17

[0310] The synthetic route of organic compound M257 is as follows:

[0311]

[0312] Synthesis of intermediate 17-1:

[0313] Compound 3-2 (10 mmol), compound 1-8 (10 mmol), Pd(dba)2 (bis(dibenzylideneacetonepalladium, 0.1 mmol), TTBP (tri-tert-butylphosphine, 0.2 mmol) and sodium tert-butoxide (30 mmol) were dissolved in toluene and stirred at 100°C for 6 h under a nitrogen atmosphere; after cooling, the solvent was removed by rotary evaporation, and the mixture was extracted and washed with water. The organic phase was subjected to column chromatography to obtain intermediate 17-1 with a molar weight of 7.36 mmol and a yield of 73.6%. The atmospheric pressure solid phase analytical probe mass spectrometry (ASAP-MS) result of intermediate 17-1 was: MS (ASAP) = 618.

[0314] Synthesis of intermediate 17-2:

[0315] Compound 17-1 (10 mmol), compound 1-4 (10 mmol), Pd(dba)2 (bis(dibenzylideneacetonepalladium, 0.1 mmol), TTBP (tri-tert-butylphosphine, 0.2 mmol) and sodium tert-butoxide (30 mmol) were dissolved in toluene and stirred at 100°C for 6 h under a nitrogen atmosphere; after cooling, the solvent was removed by rotary evaporation, and the mixture was extracted and washed with water. The organic phase was subjected to column chromatography to obtain intermediate 17-2 with a molar weight of 6.37 mmol and a yield of 63.7%. The atmospheric pressure solid phase analytical probe mass spectrometry (ASAP-MS) result of intermediate 17-2 was: MS (ASAP) = 762.

[0316] Synthesis of intermediate 17-3:

[0317] Intermediate 17-2 (10 mmol), compound 5-1 (10 mmol), Pd-132 (bis(di-tert-butyl-4-dimethylaminophenylphosphine)palladium chloride, 0.1 mmol), S-Phos (2-dicyclohexylphosphine-2',6'-dimethoxy-1,1'-biphenyl, 0.2 mmol) and sodium tert-butoxide (30 mmol) were dissolved in toluene and stirred at 100°C for 6 h under a nitrogen atmosphere; after cooling, the solvent was removed by rotary evaporation, the mixture was extracted and washed with water, and the organic phase was subjected to column chromatography to obtain intermediate 17-3 with a molar weight of 8.02 mmol and a yield of 80.2%. The atmospheric pressure solid phase analytical probe mass spectrometry (ASAP-MS) result of intermediate 17-3 was: MS (ASAP) = 853.

[0318] Synthesis of intermediate 17-4:

[0319] Intermediate 17-3 (10 mmol), compound 1-2 (10 mmol), Pd2(dba)3 (0.1 mmol), S-Phos (2-dicyclohexylphosphine-2',6'-dimethoxy-1,1'-biphenyl, 0.2 mmol) and sodium tert-butoxide (30 mmol) were dissolved in toluene and stirred at 100°C for 6 h under a nitrogen atmosphere; after cooling, the solvent was removed by rotary evaporation, the mixture was extracted and washed with water, and the organic phase was subjected to column chromatography to obtain intermediate 17-4 with a molar weight of 8.11 mmol and a yield of 81.1%. The atmospheric pressure solid phase analytical probe mass spectrometry (ASAP-MS) result of intermediate 17-4 was: MS (ASAP) = 1041.

[0320] Synthesis of intermediate 17-6:

[0321] Intermediate 17-4 (10 mmol), intermediate 17-5 (10 mmol), Pd-132 (bis(di-tert-butyl-4-dimethylaminophenylphosphine)palladium chloride, 0.1 mmol), S-Phos (2-dicyclohexylphosphine-2',6'-dimethoxy-1,1'-biphenyl, 0.2 mmol) and sodium tert-butoxide (30 mmol) were dissolved in toluene and stirred at 120°C for 3 h under a nitrogen atmosphere; after cooling, most of the solvent was removed by rotary evaporation, and then the liquid was extracted and washed with water, and the organic phase was subjected to column chromatography and recrystallization to obtain intermediate 17-6 with a molar weight of 7.21 mmol and a yield of 72.1%. The atmospheric pressure solid phase analytical probe mass spectrometry (ASAP-MS) result of intermediate 17-6 was: MS (ASAP) = 1083.

[0322] Synthesis of organic compound M257:

[0323] 10 mmol of intermediate 17-6 and 100 ml of dry tert-butylbenzene were added to a 250 ml three-necked flask, cooled to -30 ° C in a N2 atmosphere, and a n-hexane solution of t-BuLi (tert-butyl lithium) (21 mmol) was added dropwise. The temperature was raised to 60 ° C and the reaction was carried out for 2 hours. The n-hexane solvent was evaporated under reduced pressure; the reaction solution was cooled to -30 ° C again, boron tribromide (21 mmol) was added, and the temperature was raised to room temperature and stirred for 0.5 hours. Then the reaction solution was cooled to 0 ° C, and 42 mmol After the addition of N,N-diisopropylethylamine is completed, the temperature is raised to room temperature with stirring, and the temperature is further raised to 120°C with stirring for 3 hours, and the reaction solution is cooled to room temperature; sodium carbonate aqueous solution and ethyl acetate are added to quench the reaction; the aqueous phase is extracted with ethyl acetate and the organic phases are combined, and the solvent therein is evaporated to obtain a crude product, which is purified by a rapid silica gel column to obtain a pure product; recrystallization is performed with toluene and ethyl acetate to obtain a light yellow solid powder, i.e., organic compound M257, with a yield of 32.8%. The atmospheric pressure solid phase analysis probe mass spectrometry (ASAP-MS) result of the organic compound M257 is: MS (ASAP) = 1057.

[0324] Embodiment 18

[0325] The synthetic route of organic compound M258 is as follows:

[0326]

[0327] Synthesis of intermediate 18-2:

[0328] Intermediate 17-4 (10 mmol), intermediate 18-1 (10 mmol), Pd-132 (bis(di-tert-butyl-4-dimethylaminophenylphosphine)palladium chloride, 0.1 mmol), S-Phos (2-dicyclohexylphosphine-2',6'-dimethoxy-1,1'-biphenyl, 0.2 mmol) and sodium tert-butoxide (30 mmol) were dissolved in toluene and stirred at 120°C for 3 h under a nitrogen atmosphere; after cooling, most of the solvent was removed by rotary evaporation, and then the liquid was extracted and washed with water, and the organic phase was subjected to column chromatography and recrystallization to obtain intermediate 18-2 with a molar weight of 8.61 mmol and a yield of 86.1%. The atmospheric pressure solid phase analytical probe mass spectrometry (ASAP-MS) result of intermediate 18-2 was: MS (ASAP) = 1195.

[0329] Synthesis of organic compound M258:

[0330] 10 mmol of intermediate 18-2 and 100 ml of dry tert-butylbenzene were added to a 250 ml three-necked flask, cooled to -30 ° C in a N2 atmosphere, and a n-hexane solution of t-BuLi (tert-butyl lithium) (21 mmol) was added dropwise. The temperature was raised to 60 ° C and the reaction was carried out for 2 hours. The n-hexane solvent was evaporated under reduced pressure. The reaction solution was cooled to -30 ° C again, boron tribromide (21 mmol) was added, and the temperature was raised to room temperature and stirred for 0.5 hours. Then the reaction solution was cooled to 0 ° C, and 42 mmol After the addition of N,N-diisopropylethylamine is completed, the temperature is raised to room temperature with stirring, and the temperature is further raised to 120°C with stirring for 3 hours, and the reaction solution is cooled to room temperature; sodium carbonate aqueous solution and ethyl acetate are added to quench the reaction; the aqueous phase is extracted with ethyl acetate and the organic phases are combined, and the solvent therein is evaporated to obtain a crude product, which is purified by a rapid silica gel column to obtain a pure product; recrystallization is performed with toluene and ethyl acetate to obtain a light yellow solid powder, i.e., organic compound M258, with a yield of 38.8%. The atmospheric pressure solid phase analysis probe mass spectrometry (ASAP-MS) result of organic compound M258 is: MS (ASAP) = 1169. 1H NMR (400 MHz, CDCl3) δ9.09 (s, 1H), 8.85 (d, J = 11.8 Hz, 1H), 8.74 (s, 1H), 8.65 (d, J = 17.6 Hz, 1H), 8.52 (d, J = 14.2 Hz, 4H), 8.43 (t, J = 8.8 Hz, 2H), 8.28-8.01 (m, 3H), 7.88 (s, 2H), 7.69 (s, 3H), 7.58 (t, J = 13.7 Hz, 7H), 7.51-7.32 (m, 9H), 7.23 (d, J = 17.3 Hz, 2H), 7.01 (d, J = 58.4 Hz, 4H), 1.55 (s, 9H), 1.35 (s, 18H), 1.04 (s, 9H). Please refer to Figure 3 , Figure 3 : is the hydrogen nuclear magnetic resonance spectrum of the organic compound M258 of this example.

[0331] Embodiment 19

[0332] The synthetic route of organic compound M259 is as follows:

[0333]

[0334] Synthesis of intermediate 19-1:

[0335] Compound 7-1 (10 mmol), compound 1-1 (10 mmol), Pd(dba)2 (bis(dibenzylideneacetonepalladium, 0.1 mmol), TTBP (tri-tert-butylphosphine, 0.2 mmol) and sodium tert-butoxide (30 mmol) were dissolved in toluene and stirred at 100°C for 6 h under a nitrogen atmosphere; after cooling, the solvent was removed by rotary evaporation, and the mixture was extracted and washed with water. The organic phase was subjected to column chromatography to obtain intermediate 19-1 with a molar weight of 8.45 mmol and a yield of 84.5%. The atmospheric pressure solid phase analytical probe mass spectrometry (ASAP-MS) result of intermediate 19-1 was: MS (ASAP) = 632.

[0336] Synthesis of intermediate 19-3:

[0337] Intermediate 19-1 (10 mmol), compound 19-2 (10 mmol), Pd-132 (bis(di-tert-butyl-4-dimethylaminophenylphosphine)palladium chloride, 0.1 mmol), S-Phos (2-dicyclohexylphosphine-2',6'-dimethoxy-1,1'-biphenyl, 0.2 mmol) and sodium tert-butoxide (30 mmol) were dissolved in toluene and stirred at 100°C for 6 h under a nitrogen atmosphere; after cooling, the solvent was removed by rotary evaporation, the mixture was extracted and washed with water, and the organic phase was subjected to column chromatography to obtain intermediate 19-3 with a molar weight of 8.33 mmol and a yield of 83.3%. The atmospheric pressure solid phase analytical probe mass spectrometry (ASAP-MS) result of intermediate 19-3 was: MS (ASAP) = 840.

[0338] Synthesis of intermediate 19-4:

[0339] Intermediate 19-3 (10 mmol), compound 15-3 (10 mmol), Pd2(dba)3 (0.1 mmol), S-Phos (2-dicyclohexylphosphine-2',6'-dimethoxy-1,1'-biphenyl, 0.2 mmol) and sodium tert-butoxide (30 mmol) were dissolved in toluene and stirred at 100°C for 6 h under a nitrogen atmosphere; after cooling, the solvent was removed by rotary evaporation, the mixture was extracted and washed with water, and the organic phase was subjected to column chromatography to obtain intermediate 19-4 with a molar weight of 7.88 mmol and a yield of 78.8%. The atmospheric pressure solid phase analytical probe mass spectrometry (ASAP-MS) result of intermediate 19-4 was: MS (ASAP) = 1083.

[0340] Synthesis of organic compound M259:

[0341] 10 mmol of intermediate 19-4 and 100 ml of dry tert-butylbenzene were added to a 250 ml three-necked flask, cooled to -30 ° C in a N2 atmosphere, and a n-hexane solution of t-BuLi (tert-butyl lithium) (21 mmol) was added dropwise. The temperature was raised to 60 ° C and the reaction was carried out for 2 hours. The n-hexane solvent was evaporated under reduced pressure; the reaction solution was cooled to -30 ° C again, boron tribromide (21 mmol) was added, and the temperature was raised to room temperature and stirred for 0.5 hours. Then the reaction solution was cooled to 0 ° C, and 42 mmol After the addition of N,N-diisopropylethylamine is completed, the temperature is raised to room temperature with stirring, and the temperature is further raised to 120°C with stirring for 3 hours, and the reaction solution is cooled to room temperature; sodium carbonate aqueous solution and ethyl acetate are added to quench the reaction; the aqueous phase is extracted with ethyl acetate and the organic phases are combined, and the solvent therein is evaporated to obtain a crude product, which is purified by a rapid silica gel column to obtain a pure product; recrystallization is performed with toluene and ethyl acetate to obtain a light yellow solid powder, i.e., organic compound M259, with a yield of 38.3%. The atmospheric pressure solid phase analysis probe mass spectrometry (ASAP-MS) result of the organic compound M259 is: MS (ASAP) = 1057.

[0342] Embodiment 20

[0343] The synthetic route of organic compound M260 is as follows:

[0344]

[0345] Synthesis of intermediate 20-2:

[0346] Compound 7-1 (10 mmol), compound 20-1 (10 mmol), Pd(dba)2 (bis(dibenzylideneacetonepalladium, 0.1 mmol), TTBP (tri-tert-butylphosphine, 0.2 mmol) and sodium tert-butoxide (30 mmol) were dissolved in toluene and stirred at 100°C for 6 h under a nitrogen atmosphere; after cooling, the solvent was removed by rotary evaporation, and the mixture was extracted and washed with water. The organic phase was subjected to column chromatography to obtain intermediate 20-2 with a molar weight of 8.11 mmol and a yield of 81.1%. The atmospheric pressure solid phase analytical probe mass spectrometry (ASAP-MS) result of intermediate 20-2 was: MS (ASAP) = 652.

[0347] Synthesis of intermediate 20-3:

[0348] Intermediate 20-2 (10 mmol), compound 19-2 (10 mmol), Pd-132 (bis(di-tert-butyl-4-dimethylaminophenylphosphine)palladium chloride, 0.1 mmol), S-Phos (2-dicyclohexylphosphine-2',6'-dimethoxy-1,1'-biphenyl, 0.2 mmol) and sodium tert-butoxide (30 mmol) were dissolved in toluene and stirred at 100°C for 6 h under a nitrogen atmosphere; after cooling, the solvent was removed by rotary evaporation, the mixture was extracted and washed with water, and the organic phase was subjected to column chromatography to obtain intermediate 20-3 with a molar weight of 8.57 mmol and a yield of 85.7%. The atmospheric pressure solid phase analytical probe mass spectrometry (ASAP-MS) result of intermediate 20-3 was: MS (ASAP) = 860.

[0349] Synthesis of intermediate 20-4:

[0350] Intermediate 20-3 (10 mmol), compound 15-3 (10 mmol), Pd2(dba)3 (0.1 mmol), S-Phos (2-dicyclohexylphosphine-2',6'-dimethoxy-1,1'-biphenyl, 0.2 mmol) and sodium tert-butoxide (30 mmol) were dissolved in toluene and stirred at 100°C for 6 h under a nitrogen atmosphere; after cooling, the solvent was removed by rotary evaporation, the mixture was extracted and washed with water, and the organic phase was subjected to column chromatography to obtain intermediate 20-4 with a molar weight of 7.88 mmol and a yield of 78.8%. The atmospheric pressure solid phase analytical probe mass spectrometry (ASAP-MS) result of intermediate 20-4 was: MS (ASAP) = 1103.

[0351] Synthesis of organic compound M260:

[0352] In a 250 ml three-necked flask, 10 mmol of intermediate 20-4 and 100 ml of dry tert-butylbenzene were added. The mixture was cooled to -30 °C in a N2 atmosphere. A n-hexane solution of t-BuLi (tert-butyl lithium) (21 mmol) was added dropwise. The temperature was raised to 60 °C for 2 hours. The n-hexane solvent was evaporated under reduced pressure. The reaction solution was cooled to -30 °C again, boron tribromide (21 mmol) was added, and the mixture was heated to room temperature and stirred for 0.5 hours. The reaction solution was then cooled to 0 °C and 42 mmol After the addition of N,N-diisopropylethylamine is completed, the temperature is raised to room temperature with stirring, and the temperature is further raised to 120°C with stirring for 3 hours, and the reaction solution is cooled to room temperature; sodium carbonate aqueous solution and ethyl acetate are added to quench the reaction; the aqueous phase is extracted with ethyl acetate and the organic phases are combined, and the solvent therein is evaporated to obtain a crude product, which is purified by a rapid silica gel column to obtain a pure product; recrystallization is performed with toluene and ethyl acetate to obtain a light yellow solid powder, i.e., organic compound M260, with a yield of 45.1%. The atmospheric pressure solid phase analysis probe mass spectrometry (ASAP-MS) result of the organic compound M260 is: MS (ASAP) = 1077.

[0353] Comparative Example 1

[0354] Comparative compound 1 is used as a comparative example of the above-mentioned Examples 1 to 20, and the structural formula of comparative compound 1 is:

[0355]

[0356] As shown in Table 1, the HOMO (Highest Occupied Molecular Orbital) energy level, LUMO (Lowest Unoccupied Molecular Orbital) energy level, T1 (first excited triplet state) energy level, and S1 (first excited singlet state) energy level of compounds M1, M2, M5, M6, M7, M8, M9, M10, M193, M201, M209, M233, M241, M242, M251, M252, M257, M258, M259, M260 obtained in Examples 1 to 20 and the comparative compound 1 in Comparative Example 1 can be obtained by quantum calculation. Specifically, TD-DFT (time-dependent density functional theory) is used through Gaussian09W (Gaussian Inc.). The specific simulation method can be found in WO2011141110. First, the semi-empirical method "Ground State / Semi-empirical / Default Spin / AM1" (Charge 0 / SpinSinglet) is used to optimize the molecular geometry. Then, the energy structure of the organic molecule is calculated by the TD-DFT (time-dependent density functional theory) method "TD-SCF / DFT / Default Spin / B3PW91" and the basis set "6-31G(d)" (Charge 0 / SpinSinglet). The HOMO energy level and the LUMO energy level are calculated according to the following calibration formula, and the S1 energy level and the T1 energy level are used directly.

[0357] HOMO(eV)=((HOMO(G)×27.212)-0.9899) / 1.1206;

[0358] LUMO(eV)=((LUMO(G)×27.212)-2.0041) / 1.385;

[0359] Among them, HOMO, LUMO, T1 and S1 are the direct calculation results of Gaussian 09W, and the unit is Hartree.

[0360] Table 1 Calculation results of HOMO energy level, LUMO energy level, S1 energy level and T1 energy level of the organic compounds of Examples 1 to 20 and Comparative Example 1

[0361]

[0362]

[0363] From the results in Table 1, it can be seen that the T1 energy level and S1 energy level of the organic compounds M1, M2, M5, M6, M7, M8, M9, M10, M193, M201, M209, M233, M241, M242, M251, M252, M257, M258, M259, and M260 provided in Examples 1 to 20 of the present application are higher than those of the comparative compound 1. The above data show that compared with Compared with compound 1, the blue light emitted by the organic compounds M1, M2, M5, M6, M7, M8, M9, M10, M193, M201, M209, M233, M241, M242, M251, M252, M257, M258, M259, and M260 of the present application is more inclined to dark blue. Therefore, a blue organic light-emitting device using the organic compounds of the present application as the guest material in the light-emitting layer can obtain better color coordinates.

[0364] Organic light-emitting devices are prepared using the organic compounds M1, M2, M5, M6, M7, M8, M9, M10, M193, M201, M209, M233, M241, M242, M251, M252, M257, M258, M259, and M260 obtained in Examples 1 to 20. The preparation steps and performance test results of the organic light-emitting devices are shown below.

[0365] In the organic light-emitting device provided in the embodiment of the present application, ITO (indium tin oxide) is used as the anode, PEDOT (polyethylene dioxythiophene, Clevios TM AI4083) is used as a material for the hole injection layer, PVK (Sigma Aldrich, average Mn 25,000-50,000) is used as a material for the hole transport layer, BH-1 to BH-3 are respectively used as host materials in the light-emitting layers of the corresponding organic light-emitting devices, the organic compounds M1, M2, M5, M6, M7, M8, M9, M10, M193, M201, M209, M233, M241, M242, M251, M252, M257, M258, M259, M260 in Examples 1 to 20 and the comparative compound 1 in Comparative Example 1 are respectively used as guest materials in the light-emitting layers of the corresponding organic light-emitting devices, ET and Liq (8-hydroxyquinoline lithium) are used as materials for the electron transport layer, Al is used as a cathode, and the specific steps for preparing the organic light-emitting device are as follows:

[0366] a. Cleaning of ITO anode: Use chloroform, acetone and / or isopropyl alcohol to clean the ITO conductive glass, and then perform UV ozone treatment;

[0367] b. Forming a hole injection layer: Spin-coat the hole injection layer material PEDOT (polyethylene dioxythiophene, Clevios TM AI4083), and treated on a hot plate at 180°C for 10 minutes, the thickness of the hole injection layer was 40 nm;

[0368] c. Forming a hole transport layer: Spin-coat a toluene solution of PVK (Sigma Aldrich, Mn25,000-50,000) with a concentration of 5 mg / ml on the hole injection layer, and then treat on a hot plate at 180° C. for 60 minutes. The thickness of the hole transport layer is 20 nm.

[0369] d. Forming a light-emitting layer: in a nitrogen glove box, spin-coating a light-emitting layer material on the hole transport layer, and then treating on a hot plate at 140° C. for 10 minutes, the main material in the light-emitting layer of different organic light-emitting devices corresponds to BH-1, BH-2 or BH-3, respectively, and the guest material in the light-emitting layer of different organic light-emitting devices corresponds to one of the organic compounds M1, M2, M5, M6, M7, M8, M9, M10, M193, M201, M209, M233, M241, M242, M251, M252, M257, M258, M259, and M260, respectively, the solvent is methyl benzoate solution, the mass ratio of the main material to the guest material is 95:5, the concentration of the material of the light-emitting layer is 15 mg / ml, and the thickness of the light-emitting layer finally formed is 40 nm.

[0370] e. Forming the electron transport layer: In a vacuum chamber, above the light-emitting layer, ET and Liq are placed in different evaporation units and heated in a high vacuum (1×10 -6 ET and Liq were co-deposited at a weight ratio of 50:50 under a 200 mbar (mbar) environment to form an electron transport layer with a thickness of 20 nm;

[0371] f. Forming a cathode layer: depositing Al on the electron transport layer to obtain an Al cathode with a thickness of 100 nm;

[0372] g. Packaging: The device is packaged with UV-curable resin in a nitrogen glove box.

[0373] Organic light-emitting devices 1 to 24 and comparative elements 1 to 3 are obtained through the above steps. The guest materials used in organic light-emitting devices 1 to 20 are organic compounds M1, M2, M5, M6, M7, M8, M9, M10, M193, M201, M209, M233, M241, M242, M251, M252, M257, M258, M259 and M260, respectively, and the host material is BH-1; the guest material used in organic light-emitting devices 21 and 23 is organic compound M10, and the host materials are BH-2 and BH-3, respectively; the guest material used in organic light-emitting devices 22 and 24 is organic compound M233, and the host materials are BH-2 and BH-3, respectively; the guest material used in comparative elements 1 to 3 is comparative compound 1, and the host materials are BH-1, BH-2 and BH-3, respectively.

[0374] Among them, the chemical structures of BH-1, BH-2, BH-3, ET and Liq are as follows:

[0375]

[0376] The current-voltage (JV) characteristics of the organic light-emitting devices 1 to 24 and the comparative elements 1 to 3 were tested, and the CIE color coordinates (x, y), the driving voltage at 1 knits brightness (V@1 knits [V]), and the current density of 10 mA / cm 2 The luminous efficiency (CE@1knits[cd / A]) obtained when the luminance is reduced from the initial brightness of 1knits to 90% of the initial brightness (LT90@1knits[h]) is shown in Table 2.

[0377] Table 2 Performance data of organic light-emitting devices 1 to 24 and comparative elements 1 to 3

[0378]

[0379]

[0380] As can be seen from Table 2, the organic light-emitting devices 1 to 24 obtained by using the guest materials M1, M2, M5, M6, M7, M8, M9, M10, M193, M201, M209, M233, M241, M242, M251, M252, M257, M258, M259, and M260 in the light-emitting layer of the present application have better color coordinates than the comparative elements 1 to 3; wherein the luminous efficiency of the organic light-emitting devices 1 to 20 is 5.7 to 6.5 cd / A, the luminous efficiency is much higher than the luminous efficiency of comparison elements 1 to comparison elements 3; wherein, the time taken for the brightness of organic light-emitting devices 1 to organic light-emitting devices 24 to decrease from an initial brightness of 1 knits to 90% of the initial brightness is in the range of 130 to 173 h, which is an increase of 50% to 100% compared to the time taken for the brightness of comparison elements 1 to comparison elements 3 to decrease from an initial brightness of 1 knits to 90% of the initial brightness, indicating that the organic light-emitting devices 1 to organic light-emitting devices 24 of the present application have a significantly improved lifespan.

[0381] Compared with Comparative Example 1, the organic compound of the present application introduces a biphenyl ring + an aromatic ring, which makes the overall molecule more soluble and easier to purify, thereby improving the purity of the compound and further improving the efficiency and life of the manufactured organic light-emitting device.

[0382] In addition, the luminous efficiency of the organic light-emitting devices 1, 2, 5-10, and 17-20 of the present application are all in the range of 6.1 to 6.5 cd / A, and the lifespan is about 170 hours. This is because compared with the guest materials in other organic light-emitting devices, the overall molecular conjugation is greater, the aromatic amine life efficiency of the benzothiophene + biphenyl combination is significantly better than that of the benzothiophene + benzene combination, and the number of solubilizing groups is greater, which improves the solubility of the guest material and further improves the luminous efficiency and lifespan of the organic light-emitting device.

[0383] The organic light-emitting device provided in the embodiments of the present application uses boron nitrogen compounds and introduces aromatic amines of biphenyl + benzothiophene into the boron nitrogen compounds to make the overall conjugated group of the compound more powerful, thereby improving material properties, increasing the luminous efficiency of the organic light-emitting device and extending the service life of the organic light-emitting device.

[0384] An embodiment of the present application further discloses a display panel, which includes any of the above-mentioned organic light-emitting devices.

[0385] The display panel further includes an array substrate located on one side of the organic light-emitting device, and an encapsulation layer located on a side of the organic light-emitting device away from the array substrate and covering the organic light-emitting device. The display panel further includes a polarizer layer located on a side of the encapsulation layer away from the organic light-emitting device, and a cover layer located on a side of the polarizer layer away from the organic light-emitting device. The polarizer layer may be replaced by a color filter layer, and the color filter layer may include a plurality of color resists and a black matrix located on both sides of the color resists.

[0386] The display panel disclosed in the embodiment of the present application uses an organic light-emitting device containing a boron nitrogen compound and introduces a group into the boron nitrogen compound that makes the compound more conjugated as a whole, thereby enhancing the conjugation effect of the material used in the organic light-emitting device, improving the material properties, improving the luminous efficiency of the display panel and extending the service life of the display panel.

[0387] The above is a detailed introduction to an organic compound, an organic light-emitting device and a display panel provided in the embodiments of the present application. Specific examples are used herein to illustrate the principles and implementation methods of the present application. The description of the above embodiments is only used to help understand the method of the present application and its core idea. At the same time, for technical personnel in this field, according to the idea of ​​the present application, there will be changes in the specific implementation methods and application scope. In summary, the content of this specification should not be understood as a limitation on the present application.

Claims

1. An organic compound, characterized in that The organic compound has a structure as shown in general formula (1) or general formula (2): Wherein, Ar1 has a structure represented by formula (X-1) or formula (X-2): A1 and A2 have a structure represented by any one of formula (A-1), formula (A-2) or R0, and at least one of A1 and A2 has a structure represented by formula (A-1) or formula (A-2): R0 means (R3) n3 or (R4) n4 ; Ar2 has a structure represented by any one of formula (B-1) to formula (B-4): X is selected from O, S, N-CH3, N-Ph or C(CH3)2; n1, n2, n3, n4 and n5 are independently selected from any integer from 1 to 11; R1, R2, R3, R4 and R5 are independently selected from -H, -D, a linear alkyl group having 1 to 20 carbon atoms, a linear alkoxy group having 1 to 20 carbon atoms, a linear thioalkoxy group having 1 to 20 carbon atoms, a branched alkyl group having 3 to 20 carbon atoms, a cyclic alkyl group having 3 to 20 carbon atoms, a branched alkoxy group having 3 to 20 carbon atoms, a cyclic alkoxy group having 3 to 20 carbon atoms, a branched thioalkoxy group having 3 to 20 carbon atoms, a cyclic thioalkoxy group having 3 to 20 carbon atoms, a silyl group, a keto group having 1 to 20 carbon atoms , an alkoxycarbonyl group having 2 to 20 carbon atoms, an aryloxycarbonyl group having 7 to 20 carbon atoms, an olefin group having 1 to 20 carbon atoms, -CN, carbamoyl, haloformyl, formyl, isocyano, isocyanate, thiocyanate, isothiocyanate, hydroxyl, nitro, -CF3, -Cl, -Br, -F, a substituted or unsubstituted aromatic group having 6 to 30 ring atoms, a substituted or unsubstituted heteroaromatic group having 5 to 30 ring atoms, a substituted or unsubstituted aryloxy group having 6 to 30 ring atoms, and a substituted or unsubstituted heteroaryloxy group having 5 to 30 ring atoms; When n1 is greater than or equal to 2, two adjacent R1s may or may not form a ring with each other; when n2 is greater than or equal to 2, two adjacent R2s may or may not form a ring with each other; when n3 is greater than or equal to 2, two adjacent R3s may or may not form a ring with each other; when n4 is greater than or equal to 2, two adjacent R4s may or may not form a ring with each other; when n5 is greater than or equal to 2, two adjacent R5s may or may not form a ring with each other.

2. The organic compound according to claim 1, characterized in that The organic compound has a structure as shown in any one of the general formulas (2-1) to (2-22):

3. The organic compound according to claim 2, characterized in that R1, R2, R3, R4 and R5 are independently selected from -H, -D, a linear alkyl group having 1 to 10 carbon atoms, a branched alkyl group having 3 to 10 carbon atoms, a cyclic alkyl group having 3 to 10 carbon atoms.

4. The organic compound according to claim 3, characterized in that R1, R2, R3, R4 and R5 are independently selected from -H, -D, a straight chain alkyl group having 1 to 4 carbon atoms, a branched chain alkyl group having 3 to 5 carbon atoms.

5. The organic compound according to claim 1, characterized in that The structure represented by the formula (B-2) includes as well as At least one of .

6. The organic compound according to claim 1, characterized in that The organic compound is selected from the compounds represented by Formula 1 to Formula 260:

7. An organic light-emitting device, characterized in that: include: a first electrode; a second electrode, arranged opposite to the first electrode; and an organic functional layer, located between the first electrode and the second electrode; The material of the organic functional layer includes one or more of the organic compounds as described in any one of claims 1 to 6.

8. The organic light-emitting device according to claim 7, characterized in that: The organic functional layer at least includes a light-emitting layer, the light-emitting layer includes a host material and a guest material, the guest material includes the organic compound, and the host material includes a condensed aromatic derivative or a heteroaromatic compound.

9. The organic light emitting device according to claim 8, characterized in that: The host material includes one or more of anthracene derivatives, pyrene derivatives, naphthalene derivatives, pentacene derivatives, phenanthrene compounds, fluoranthene compounds, carbazole derivatives, dibenzofuran derivatives, ladder-type furan compounds, and pyrimidine derivatives.

10. A display panel, characterized in that: The organic light emitting device comprises the organic light emitting device as claimed in any one of claims 7 to 9.

Citation Information

Patent Citations

  • Carbazole-containing materials in phosphorescent light emitting diodes

    US20090134784A1

  • Metal complexes with boron-nitrogen heterocycle containing ligands for use in organic light emitting devices

    WO2010135519A1

  • Fibers in therapy and cosmetics

    WO2011110277A1