Efficient selective double-sided pressing plate continuous spraying device
By designing an efficient and selective double-sided plate continuous spraying device, the problem that wheel plating technology is difficult to meet thickness requirements and double-sided electroplating is solved, and efficient electroplating of products with dense tape thickness and plating zones is achieved, reducing costs and improving accuracy and efficiency.
Patent Information
- Application Number
- CN202310623685.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2023-05-30
- Publication Date
- 2024-12-03
AI Technical Summary
The existing wheel plating technology is difficult to meet the thickness requirements. The use of spraying is limited to single-sided electroplating of sheets with discontinuous electroplating cannot meet double-sided electroplating, and the cost is high, and there is difficulty in controlling tape deformation and plating zones.
A highly efficient selective double-sided pressure plate continuous spraying device was designed. The water box base, lower mold and upper mold structures were stacked in sequence to achieve double-sided electroplating of material tape using electroplating solution paths and shielding silicone boards, combined with Ceramic guide ring and water barrier adjust the flow rate of the plating solution to ensure uniformity and efficiency of the plating layer.
It realizes efficient double-sided electroplating of products with thicker material tape and dense plating zones, reduces production costs, improves the control accuracy and efficiency of plating zones, and is suitable for production lines with limited space.
Smart Images

Figure CN119061448A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of strip electroplating, and in particular to a highly efficient and selective double-sided pressing plate continuous spraying device. Background Art
[0002] At present, the most commonly used selective spraying fixture in the market is wheel plating. In recent years, there are also platen-type spraying fixtures, but they are also limited to the production of non-continuous electroplated sheets, and they are all single-sided electroplating. In view of the current production needs in the market, wheel plating can meet the production of most products, but for products with thicker strips, denser plating areas, and higher electroplating film thickness, wheel plating still has many disadvantages.
[0003] First, for products with thicker strips, surface treatment through wheel plating will increase the risk of strip deformation. When using a ferry to surface treat thicker strips, the diameter of the plating wheel and the guide wheel can be increased, as well as the inlet and outlet angles of the strip can be changed. In this way, the size of the spot plating machine and the size of the electroplating tank need to be increased to meet the demand, and the sharing performance of the production line is poor. For production lines that cannot meet the requirements of increased size and space, there is still no way to complete the production of such products.
[0004] For products with densely plated areas, the risk of infiltration will increase if wheel plating is used. Because wheel plating is continuous electroplating with the nozzles rotating around the plating wheel, there are many uncertainties. For example, the diameter production error of the plating wheel, the temperature error of the plating solution, the production and assembly error of the silicone, the production and assembly error of the positioning needle, the processing and assembly error of the spot plating machine, etc., will affect the stability of the electroplating area, especially for products with densely plated areas, the impact on the electroplating area will be more obvious.
[0005] Wheel plating can generally only plate on one side. For products that require double-sided plating, the material strip needs to be flipped over by a flip wheel and then another plating wheel is used. The film thickness that can be achieved by a single wheel is related to factors such as product structure, plating area, anode structure, plating wheel opening, production speed, and concentration of the plating solution. For the production of products that require double-sided plating with a higher film thickness, more plating wheels are needed to complete the process. In this way, the production cost will be greatly increased and the effective utilization of space will be greatly reduced. Summary of the invention
[0006] The technical problem to be solved by the present invention is: in order to solve the technical problems that the wheel plating in the prior art cannot meet the thickness requirements, the spraying is limited to the single-sided electroplating production of non-continuously plated sheets, and cannot meet the requirements of double-sided electroplating and the cost is high. The present invention provides a high-efficiency selective double-sided platen continuous spraying device, which not only solves the problems of material deformation, poor control of the plating area and low efficiency in the electroplating process of products with thicker material strips and denser plating areas. It also helps production lines with limited space to complete double-sided electroplating normally and efficiently. It has low cost and high precision. The technical solution adopted by the present invention to solve its technical problems is: a high-efficiency selective double-sided pressure plate continuous spraying device, comprising: a water box base, a lower mold water plate, a lower mold anode plate, a lower mold template, a lower mold shielding silicone plate, an upper mold shielding silicone plate, an upper mold template and an upper mold water plate, which are stacked in sequence from bottom to top, a lower mold water baffle plate is provided on one side of the lower mold template, and an upper mold water baffle plate is provided on one side of the upper mold water plate, a first electroplating liquid passage is formed between the water box base, the lower mold water plate, the lower mold anode plate, the lower mold template and the lower mold water baffle plate, a second electroplating liquid passage is formed by the water box base, the lower mold water plate, the lower mold anode plate, the lower template, the lower mold shielding silicone plate, the upper mold shielding silicone plate, the upper template, the upper mold water plate and the upper mold water baffle plate, and a metal strip to be plated is provided between the lower mold shielding silicone plate and the upper mold shielding silicone plate.
[0007] Furthermore, a lower mold anode conductive rod is arranged below the lower mold anode plate, and the metal strip serves as a cathode. During electroplating, the lower mold anode conductive rod is connected to electricity, and the current is transmitted to the lower mold anode plate to generate metal cations. The plating solution containing the metal cations reaches the lower end surface of the metal strip, and the anions and cations react to form a metal coating at the part of the lower surface of the strip that is not covered by the lower mold shielding silicone plate, thereby achieving electroplating of the lower end surface of the metal strip. The plating solution containing the metal cations continues to flow upward and reaches the upper end surface of the metal strip, and the anions and cations react to form a metal coating at the part of the upper surface of the metal strip that is not covered by the upper mold shielding silicone plate, thereby achieving electroplating of the upper end surface of the metal strip.
[0008] Furthermore, an upper mold anode plate is provided between the upper mold lower water plate and the upper mold plate, and an upper mold anode conductive plate is provided at one end of the upper mold anode plate.
[0009] Furthermore, the lower mold shielding silicone plate is positioned on the lower mold plate by a plurality of silicone shielding plate positioning pins, and the upper mold shielding silicone plate is positioned on the upper mold plate by a plurality of silicone shielding plate positioning pins.
[0010] Furthermore, a plurality of ceramic guide rings are provided on the lower template, and the plurality of ceramic guide rings are used to limit the position of the metal strip, and a metal strip placement area is formed between the plurality of ceramic guide rings.
[0011] Furthermore, the lower mold water retaining plate includes an outer water retaining plate and an inner water retaining plate which abut against each other on the sides. The inner water retaining plate is close to one side of the lower mold plate and is located on the lower side of the lower mold plate. The upper and lower spacing between the inner water retaining plate and the lower mold plate is adjustable to adjust the flow rate of the first electroplating liquid passage.
[0012] Furthermore, a first waist-shaped mounting hole is provided on the water retaining outer plate, and a second mounting hole is provided on the water retaining inner plate. The first waist-shaped mounting hole and the second mounting hole of the water retaining outer plate cooperate with each other, and the distance between the water retaining plate and the lower template is adjusted through the first waist-shaped mounting hole.
[0013] Furthermore, a water hole is provided on one side of the upper mold water lower plate close to the upper mold water retaining plate, and the upper mold water retaining plate adjusts the size of the water hole to adjust the flow rate of the second electroplating solution passage.
[0014] Furthermore, the upper mold water retaining plate is installed on the upper mold lower water plate through a second waist-shaped mounting hole, and the upper mold water retaining plate is provided with an adjustment hole, and the adjustment hole corresponds to the lower water hole. The position of the upper mold water retaining plate is adjusted through the second waist-shaped mounting hole, so that the relative position of the adjustment hole and the lower water hole is adjustable to adjust the liquid outlet size of the lower water hole.
[0015] The beneficial effect of the present invention is that the high-efficiency selective double-sided platen continuous spraying device of the present invention provides an efficient and lightweight selective double-sided platen spraying device, which not only solves the problems of strip deformation, poor plating area control and low efficiency in the electroplating process of products with thicker strips and denser plating areas. It also helps production lines with limited space to complete production tasks normally and efficiently. The jig of the present invention occupies a small space, performs continuous double-sided electroplating, and is more efficient. In addition, the shielding rubber strip of the jig of this invention is made in the form of integrated laser cutting, which is simpler, lower cost and higher precision than the traditional manual pressing of rubber molds. BRIEF DESCRIPTION OF THE DRAWINGS
[0016] The present invention is further described below in conjunction with the accompanying drawings and embodiments.
[0017] Figure 1 It is a schematic diagram of the overall structure of the highly efficient and selective double-sided platen continuous spraying device of the present invention;
[0018] Figure 2 It is a schematic diagram of the structure of the upper mold anode plate of the high-efficiency selective double-sided pressure plate continuous spraying device of the present invention;
[0019] Figure 3 It is a schematic diagram of the positioning structure of the lower mold shielding silicone plate of the high-efficiency selective double-sided pressure plate continuous spraying device of the present invention;
[0020] Figure 4It is a schematic diagram of the flow direction of the electroplating liquid of the high-efficiency selective double-sided pressure plate continuous spraying device of the present invention.
[0021] Reference numerals:
[0022] 1. Water box base; 2. Lower mold water retaining plate; 21. Water retaining outer plate; 22. Water retaining inner plate; 23. First waist-shaped mounting hole; 24. Second mounting hole; 3. Lower mold water discharge plate; 4. Lower mold anode plate; 41. Lower mold anode conductive rod; 5. Lower mold plate; 6. Lower mold shielding silicone plate; 7. Upper mold shielding silicone plate; 8. Upper mold plate; 9. Upper mold water discharge plate; 91. Water discharge hole; 10. Upper mold anode plate; 11. Upper mold anode conductive plate; 12. Upper mold water retaining plate; 121. Second waist-shaped mounting hole; 122. Adjustment hole; 13. Silicone shielding plate positioning pin; 14. Ceramic guide ring; 15. Silicone plating area hole. DETAILED DESCRIPTION
[0023] The present invention will now be described in further detail with reference to the accompanying drawings. These drawings are simplified schematic diagrams, which only illustrate the basic structure of the present invention in a schematic manner, and therefore only show the components related to the present invention.
[0024] In the description of the present invention, it should be understood that the terms "center", "longitudinal", "lateral", "length", "width", "thickness", "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside", "outside", "clockwise", "counterclockwise", "axial", "radial", "circumferential" and the like indicate positions or positional relationships based on the positions or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present invention and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as a limitation on the present invention. In addition, features defined as "first" and "second" may explicitly or implicitly include one or more of the features. In the description of the present invention, unless otherwise specified, "multiple" means two or more.
[0025] In the description of the present invention, it should be noted that, unless otherwise clearly specified and limited, the terms "installed", "connected", and "connected" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection, or it can be indirectly connected through an intermediate medium, or it can be the internal communication of two components. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.
[0026] like Figures 1 to 4As shown, it is the best embodiment of the present invention, a high-efficiency selective double-sided platen continuous spraying device, comprising: a water box base 1, a lower mold water plate 3, a lower mold anode plate 4, a lower mold template 5, a lower mold shielding silicone plate 6, an upper mold shielding silicone plate 7, an upper mold template 8, and an upper mold water plate 9 are stacked in sequence from bottom to top, a lower mold water baffle 2 is provided on one side of the lower mold template 5, an upper mold water baffle 12 is provided on one side of the upper mold water plate 9, a water box base 1, a lower mold water plate 3, a lower mold anode plate 4, a lower mold template 5 and a lower mold water plate 9 are stacked in sequence from bottom to top. A first electroplating liquid passage is formed between the mold water retaining plate 2, and a second electroplating liquid passage is formed by the water box base 1, the lower mold water plate 3, the lower mold anode plate 4, the lower mold plate 5, the lower mold shielding silicone plate 6, the upper mold shielding silicone plate 7, the upper mold plate 8, the upper mold water plate 9 and the upper mold water retaining plate 12. A metal strip to be plated is arranged between the lower mold shielding silicone plate 6 and the upper mold shielding silicone plate 7, an upper mold anode plate 10 is arranged between the upper mold water plate 9 and the upper mold plate 8, and an upper mold anode conductive plate 11 is arranged at one end of the upper mold anode plate 10.
[0027] A lower mold anode conductive rod 41 is arranged below the lower mold anode plate 4, and the metal strip serves as a cathode. During electroplating, the lower mold anode conductive rod 41 is energized, and the current is transmitted to the lower mold anode plate 4 to generate metal cations. The plating solution containing the metal cations reaches the lower end surface of the metal strip, and the anions and cations react to form a metal coating on the lower surface of the strip that is not covered by the lower mold shielding silicone plate 6, thereby achieving electroplating of the lower end surface of the metal strip. The plating solution containing the metal cations continues to flow upward and reaches the upper end surface of the metal strip, and the anions and cations react to form a metal coating on the upper surface of the metal strip that is not covered by the upper mold shielding silicone plate 7, thereby achieving electroplating of the upper end surface of the metal strip.
[0028] The lower mold shielding silicone plate 6 is positioned on the lower mold plate 5 by multiple silicone shielding plate positioning pins 13, and the upper mold shielding silicone plate 7 is positioned on the upper mold plate 8 by multiple silicone shielding plate positioning pins 13. Multiple ceramic guide rings 14 are provided on the lower mold plate 5, and the multiple ceramic guide rings 14 are used to limit the metal material strip, and a metal material strip placement area is formed between the multiple ceramic guide rings 14.
[0029] like Figure 1 and Figure 4 As shown, the entire structure of a high-efficiency selective double-sided platen continuous spraying device is supported by a water box base 1. In addition to the supporting function, the water box base 1 also plays the role of water supply. The plating liquid is injected from the water hole at the bottom of the water box base 1. When a certain pressure is reached in the water box base 1, the plating liquid can be sprayed out through the water outlet hole at the top of the water box base 1.
[0030] The position and size of the water outlet hole on the top of the water box base 1 correspond to the electroplating area of the strip to be electroplated. The electroplating liquid ejected from the water box base 1 continues to flow upward through the upper water hole on the lower die water plate 3 to reach the lower die anode plate 4. Figure 2As shown, the lower mold anode plate 4 is made of pure titanium, and the surface is platinum-plated. The lower mold anode conductive rod 41 is connected to the lower mold anode plate 4. After the lower mold anode conductive rod 41 is energized, the current is transmitted to the lower mold anode plate 4. The lower mold anode plate 4 reacts with the sprayed electroplating liquid under the action of the current to produce metal cations. The electroplating liquid with metal cations continues to ascend, passes through the upper water hole of the lower mold plate 5, and continues to ascend through the lower mold shielding silicone plate 6. The lower mold shielding silicone plate 6 is a plate with a G10 base and a surface covered with RTV silicone. It is laser cut by a precision laser machine according to the actual point plating area required to meet the function of shielding the material strip. As shown Figure 3 As shown, the position and size of the silicone plating area hole 15 on the lower mold shielding silicone plate 6 are closely related to the actual electroplated area and position, so positioning is very important. It is accurately fixed on the lower mold plate 5 by the silicone shielding plate positioning pin 13.
[0031] The product in contact with the lower mold shielding silicone plate 6 is a material strip made of metal. Under the action of the ceramic material guide ring 14, the metal material strip is continuously fed according to the step distance set in advance by the machine, that is, the material strip step distance. The material strip is energized during the transportation on the production line, and the material strip acts as a cathode. The cation-containing electroplating liquid that flows out from the lower mold shielding silicone plate 6 reaches the material strip, and the anions and cations react, so that a metal coating is formed on the lower surface of the material strip that is not shielded by the lower mold silicone shielding plate 6, that is, the place where spot plating is required, to achieve the purpose of electroplating. At this time, the electroplating liquid will continue to move upward through the material strip and reach the upper mold shielding silicone plate 7. The upper surface of the material strip is close to the upper mold shielding silicone plate 7. The upper mold shielding silicone plate 7 is also fixed on the upper mold plate 8 with a silicone shielding plate positioning pin 13 to limit the position and size of the silicone plating area hole on the upper mold shielding silicone plate 7. The upper mold shielding silicone plate 7 is covered with an upper mold plate 8, and the openings on the upper mold plate 8 correspond to the upper mold shielding silicone plate 7. The electroplating solution goes up all the time and passes through the upper mold plate 8. Above the upper mold plate 8 is an upper mold anode plate 10, and the base material of the upper mold anode plate 10 is a pure titanium mesh with platinum plated on the surface.
[0032] The upper mold anode plate 10 is equipped with an upper mold anode conductive plate 11 made of pure titanium at both ends. The external wire is connected to the upper mold anode plate 10 through the upper mold anode conductive plate 11. After the upper mold anode conductive plate 11 is energized, the current is transmitted to the upper mold anode plate 10. Under the action of the current, the upper mold anode plate 10 reacts with the upwelling electroplating solution, so that the metal in the electroplating solution produces free metal cations, so as to supplement the electroplating solution from the bottom of the upper mold plate 8 to solve the problem of insufficient metal cations in the electroplating solution caused by the formation of a metal coating under the material strip. It can ensure that the electroplating on the upper surface of the material strip is completed smoothly. Thereby achieving the purpose of high-efficiency double-sided electroplating.
[0033] The lower mold water retaining plate 2 includes a water retaining outer plate 21 and a water retaining inner plate 22 whose sides abut against each other. The water retaining inner plate 22 is close to one side of the lower template 5 and is located on the lower side of the lower template 5. The upper and lower distances between the water retaining inner plate 22 and the lower template 5 are adjustable to adjust the flow rate of the first electroplating liquid passage. A first waist-shaped mounting hole 23 is provided on the water retaining outer plate 21, and a second mounting hole 24 is provided on the water retaining inner plate 22. The first waist-shaped mounting hole 23 and the second mounting hole 24 of the water retaining outer plate 21 cooperate with each other, and the distance between the water retaining plate and the lower template 5 is adjusted through the first waist-shaped mounting hole 23.
[0034] A water hole 91 is provided on one side of the upper mold water plate 9 close to the upper mold water retaining plate 12. The upper mold water retaining plate 12 adjusts the size of the water hole 91 to adjust the flow rate of the second electroplating liquid passage. The upper mold water retaining plate 12 is installed on the upper mold water plate 9 through the second waist-shaped mounting hole 121. The upper mold water retaining plate 12 has an adjustment hole 122, and the adjustment hole 122 corresponds to the water hole 91. The position of the upper mold water retaining plate 12 is adjusted through the second waist-shaped mounting hole 121, so that the relative position of the adjustment hole 122 and the water hole 91 can be adjusted to adjust the liquid outlet size of the water hole 91.
[0035] The lower mold water retaining plate 2 and the upper mold water retaining plate 12 play a very important role in controlling the thickness of the double-sided electroplating film.
[0036] During the electroplating process of the material strip between the lower mold shielding silicone plate 6 and the upper mold shielding silicone plate 7, a device that can adjust the water leakage flow rate is formed between the three workpieces of the lower mold plate 5, the lower mold water plate 3 and the lower mold water retaining plate 2 under the lower mold shielding silicone plate 6.
[0037] The lower mold water retaining plate 2 includes two parts, one part is the lower mold water retaining outer plate 21, on which there are 6 first waist-shaped mounting holes 23, i.e. screw holes, which can be adjusted in a row. The other part is the lower mold water retaining inner plate 22, on which there are 6 second mounting holes 24 in a row. The 6 second mounting holes 24 on the lower mold water retaining inner plate 22 and the 6 first waist-shaped mounting holes 23 on the lower mold water retaining outer plate 21 are fixed together by screws, and under the action of the first waist-shaped mounting holes 23 on the lower mold water retaining outer plate 21, the cooperation between the lower mold water retaining inner plate 22 and the lower mold water retaining outer plate 21 can be adjusted. Therefore, the upper and lower spacings between the water retaining inner plate 22 and the lower mold plate 5 are adjustable, and a device that can adjust the flow rate of water leakage is formed between the three workpieces of the lower mold plate 5, the lower mold lower water plate 3 and the lower mold water retaining plate 2. The device can be used to adjust the coating thickness of the lower end face of the material strip. When the thickness of the lower end face of the material strip is too low, the inner plate water retaining inner plate 22 of the lower mold water retaining plate 2 is adjusted downward to enlarge the flow channel formed between the three workpieces of the lower mold plate 5, the lower mold water plate 3 and the lower mold water retaining plate 2, and the water discharge speed is increased, which can increase the exchange of the electroplating solution and increase the coating thickness of the lower end face of the material strip. When the coating of the lower end face of the material strip is too thick, the inner plate water retaining inner plate 22 of the lower mold water retaining plate 2 is adjusted upward to reduce the flow channel formed between the three workpieces of the lower mold plate 5, the lower mold water plate 3 and the lower mold water retaining plate 2, and the water discharge speed is slowed down, which can reduce the exchange of the electroplating solution and reduce the coating thickness of the lower end face of the material strip.
[0038] The water holes 91 of the upper mold water plate 9 are circular holes distributed on the side. When the plating solution is injected from the water box base 1 to the material strip on both sides to complete the plating, the plating solution will continue to rise, and will eventually reach the upper mold water plate 9 and flow out from the side water holes 91 of the upper mold water plate 9. The upper mold water retaining plate 12 is a plate covering the side of the upper mold water plate 9. The upper mold water retaining plate 12 has two rows of holes, the upper row of holes is the adjustment holes 122, and the lower row of holes is the second waist-shaped mounting holes 121. The upper row of adjustment holes 122 is consistent with the water holes on the side of the upper mold water plate 9, and there is a row of screw holes on the upper mold water plate 9 corresponding to the position of the second waist-shaped mounting holes 121 of the upper mold water retaining plate 12. The upper mold water retaining plate 12 and the upper mold water plate 9 are fixed in position by screws through these two holes. The upper mold water retaining plate 12 moves left and right through the second waist-shaped mounting hole 121, so that the positions of the adjustment hole 122 of the upper mold water retaining plate 12 and the water hole 91 of the upper mold water plate 9 can be changed. When the adjustment hole 122 of the upper mold water retaining plate 12 and the water hole 91 of the upper mold water plate 9 are completely aligned, the upper mold water discharge speed is the fastest, the exchange of the electroplating solution is also the fastest, and the corresponding plating thickness of the upper end surface of the material strip will increase. When the adjustment hole 122 of the upper mold water retaining plate 12 and the water hole 91 of the upper mold water plate 9 are not aligned and there is mutual shielding, the upper mold water discharge speed will be correspondingly slowed down, the exchange of the electroplating solution is also relatively slow at this time, and the corresponding plating thickness of the upper end surface of the material strip will be reduced.
[0039] In actual production, the inner plate position of the lower mold water retaining plate 2 and the position of the upper mold water retaining plate 12 can be adjusted by screws to find a position point that makes the upper and lower film thicknesses of the material strip balanced, thereby achieving effective and efficient production.
[0040] The high-efficiency selective double-sided platen continuous spraying device of the present invention provides an efficient and lightweight selective double-sided platen spraying device, which not only solves the problems of strip deformation, poor plating area control and low efficiency in the electroplating process of products with thicker strips and denser plating areas. It also helps production lines with limited space to complete production tasks normally and efficiently. The jig of the present invention occupies little space, performs continuous double-sided electroplating, and is more efficient. In addition, the shielding rubber strip of the jig of this invention is made in the form of integrated laser cutting, which is simpler, lower cost and higher precision than the traditional manual pressing of rubber molds.
[0041] Based on the above ideal embodiments of the present invention, the relevant staff can make various changes and modifications without departing from the technical concept of the present invention through the above description. The technical scope of the present invention is not limited to the contents of the specification, but must be determined according to the scope of the claims.
Claims
1. A highly efficient and selective double-sided platen continuous spraying device, characterized in that: include: A water box base (1), a lower mold water plate (3), a lower mold anode plate (4), a lower mold template (5), a lower mold shielding silicone plate (6), an upper mold shielding silicone plate (7), an upper mold template (8) and an upper mold water plate (9) are stacked in sequence from bottom to top, wherein one side of the lower mold template (5) is provided with a lower mold water retaining plate (2), one side of the upper mold water plate (9) is provided with an upper mold water retaining plate (12), and the water box base (1), the lower mold water plate (3), the lower mold anode plate (4), A first electroplating liquid passage is formed between the lower mold plate (5) and the lower mold water retaining plate (2); a second electroplating liquid passage is formed by the water box base (1), the lower mold water lower plate (3), the lower mold anode plate (4), the lower mold plate (5), the lower mold shielding silicone plate (6), the upper mold shielding silicone plate (7), the upper mold plate (8), the upper mold water lower plate (9) and the upper mold water retaining plate (12); and a metal strip to be plated is arranged between the lower mold shielding silicone plate (6) and the upper mold shielding silicone plate (7).
2. The high-efficiency selective double-sided platen continuous spraying device according to claim 1, characterized in that: A lower mold anode conductive rod (41) is arranged below the lower mold anode plate (4), and the metal strip serves as a cathode. During electroplating, the lower mold anode conductive rod (41) is energized, and the current is transmitted to the lower mold anode plate (4) to generate metal cations. The plating solution containing the metal cations reaches the lower end surface of the metal strip, and the cations and anions react to form a metal coating at the lower surface of the strip that is not shielded by the lower mold shielding silicone plate (6), thereby achieving electroplating of the lower end surface of the metal strip. The plating solution containing the metal cations continues to flow upward and reaches the upper end surface of the metal strip, and the cations and anions react to form a metal coating at the upper surface of the metal strip that is not shielded by the upper mold shielding silicone plate (7), thereby achieving electroplating of the upper end surface of the metal strip.
3. The high-efficiency selective double-sided platen continuous spraying device according to claim 1, characterized in that: An upper mold anode plate (10) is provided between the upper mold lower water plate (9) and the upper mold plate (8), and an upper mold anode conductive plate (11) is provided at one end of the upper mold anode plate (10).
4. The high-efficiency selective double-sided platen continuous spraying device according to claim 1, characterized in that: The lower mold shielding silicone plate (6) is positioned on the lower mold plate (5) through a plurality of silicone shielding plate positioning pins (13), and the upper mold shielding silicone plate (7) is positioned on the upper mold plate (8) through a plurality of silicone shielding plate positioning pins (13).
5. The high-efficiency selective double-sided platen continuous spraying device according to claim 4, characterized in that: A plurality of ceramic guide rings (14) are arranged on the lower template (5), and the plurality of ceramic guide rings (14) are used to limit the position of the metal strip, and a metal strip placement area is formed between the plurality of ceramic guide rings (14).
6. The high-efficiency selective double-sided platen continuous spraying device according to claim 1, characterized in that: The lower mold water retaining plate (2) comprises a water retaining outer plate (21) and a water retaining inner plate (22) which are abutted against each other on the side, the water retaining inner plate (22) is close to one side of the lower mold plate (5) and is located on the lower side of the lower mold plate (5), and the upper and lower spacing between the water retaining inner plate (22) and the lower mold plate (5) is adjustable to adjust the flow rate of the first electroplating solution passage.
7. The high-efficiency selective double-sided platen continuous spraying device according to claim 6, characterized in that: The water retaining outer plate (21) is provided with a first waist-shaped mounting hole (23), and the water retaining inner plate (22) is provided with a second mounting hole (24). The first waist-shaped mounting hole (23) and the second mounting hole (24) of the water retaining outer plate (21) cooperate with each other, and the spacing between the water retaining plate and the lower template (5) is adjusted through the first waist-shaped mounting hole (23).
8. The high-efficiency selective double-sided platen continuous spraying device according to claim 1, characterized in that: A water hole (91) is provided on one side of the upper mold water plate (9) close to the upper mold water retaining plate (12), and the upper mold water retaining plate (12) adjusts the size of the water hole (91) to adjust the flow rate of the second electroplating solution passage.
9. The high-efficiency selective double-sided platen continuous spraying device according to claim 8, characterized in that: The upper mold water retaining plate (12) is installed on the upper mold lower water plate (9) through a second waist-shaped mounting hole (121); an adjustment hole (122) is provided on the upper mold water retaining plate (12); the adjustment hole (122) corresponds to the lower water hole (91); the position of the upper mold water retaining plate (12) is adjusted through the second waist-shaped mounting hole (121), so that the relative position of the adjustment hole (122) and the lower water hole (91) is adjustable, so as to adjust the liquid discharge size of the lower water hole (91).