High-voltage conductive polymer solid-liquid mixed aluminum electrolytic capacitor and preparation method thereof
By using components such as temperature conduction columns and elastic strips in aluminum electrolytic capacitors to improve heat derivation efficiency, the problems of poor contact between the aluminum shell and insufficient thermal conductivity of the electrolyte are solved, efficient heat dissipation and rapid impregnation are achieved, and aluminum electrolytic capacitors are supported. high-pressure development.
Patent Information
- Application Number
- CN202411335544.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-24
- Publication Date
- 2024-12-03
AI Technical Summary
The caps of existing aluminum electrolytic capacitors are difficult to fully contact with the aluminum shell, resulting in low thermal conductivity and the thermal conductivity of the electrolyte is not enough to meet the needs of high-pressure development. At the same time, the electrolyte is prone to chemical and physical changes in high temperature environments, affecting the capacitor. stability.
A high-voltage conductive polymer solid-liquid mixed aluminum electrolytic capacitor was designed, and the heat transfer efficiency was improved by using components such as temperature conduction columns and elastic strips. The heat in the middle of the macronucleus was exported through the temperature conduction columns, and the heat was passed through the elastic strips and extrusion sleeves. Export external heat to the aluminum shell to increase the heat dissipation speed, and at the same time drive the rotating column to rotate during the impregnation process to increase the flow rate of the electrolyte and shorten the impregnation time.
It effectively improves the heat dissipation performance of aluminum electrolytic capacitors, enhances the support capacity for high voltage, shortens the impregnation time during the production process, and improves the stability and production efficiency of the capacitor.
Smart Images

Figure CN119069263A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of aluminum electrolytic capacitors, and specifically discloses a high-voltage conductive polymer solid-liquid mixed aluminum electrolytic capacitor and a preparation method thereof. Background Art
[0002] High-voltage conductive polymer solid-liquid hybrid aluminum electrolytic capacitor is a technical product that combines the advantages of traditional aluminum electrolytic capacitors and conductive polymer capacitors. The electrolytic capacitor is based on aluminum electrolytic capacitors and is also composed of elements, aluminum shells and rubber plugs. The elements contain components such as electrolytic paper, electrodes and positive and negative aluminum foils. The electrolytic capacitor mainly improves the conductivity and electrical performance of the electrolytic capacitor by sequentially impregnating the elements with solid polymer electrolytes and traditional liquid electrolytes, meeting the development needs of high-voltage electrolytic capacitors. In order to ensure that the elements of existing aluminum electrolytic capacitors are completely intactly inserted into the aluminum shell, the element diameter is usually smaller than the aluminum shell. Shell, which results in the element not being completely in contact with the aluminum shell, and the thermal conductivity between the two is low. Therefore, the existing aluminum electrolytic capacitors need electrolyte as an auxiliary thermal conductive medium to meet their own heat dissipation needs. When the voltage stored in the aluminum electrolytic capacitor becomes higher and higher, its heat generation in the working state will further increase, and the thermal conductivity of the electrolyte is lower than that of traditional thermally conductive solid materials. Therefore, it is difficult to completely replace traditional thermally conductive solid materials. Moreover, when the electrolyte is in a high temperature environment for a long time, the chemical and physical properties of the electrolyte are prone to change, causing the electrolyte to undergo thermal expansion, volatilization, and vaporization, which will undoubtedly hinder the high-voltage development of aluminum electrolytic capacitors. Summary of the invention
[0003] In order to overcome the disadvantages of the existing aluminum electrolytic capacitor that the element is difficult to completely contact with the aluminum shell and the thermal conductivity is low, the present invention provides a high-voltage conductive polymer solid-liquid hybrid aluminum electrolytic capacitor and a preparation method thereof.
[0004] The technical solution of the present invention is: a high-voltage conductive polymer solid-liquid hybrid aluminum electrolytic capacitor, including an aluminum shell, a top plug and a base are installed in the aluminum shell, the lower side of the top plug is slidably connected to the top plate, a rotating column is rotatably connected in the base, and an elastic member is installed between the two, the rotating column is fixedly connected to a centrally symmetrically distributed temperature-conducting column, the temperature-conducting column is extruded and matched with the top plate, an element is arranged on the outside of the temperature-conducting column, an elastic strip is fixed to the outside of the element, an extrusion sleeve is slidably connected in the aluminum shell, and the aluminum shell, the top plate, the base and the elastic strip are all extruded and matched with the extrusion sleeve.
[0005] Furthermore, the top plug is made of rubber material, the top plate, the base, the rotating column, the elastic strip, the extrusion sleeve and the symmetrically distributed temperature-conducting columns are all made of metal heat-conducting materials, and the upper side of the top plate is provided with symmetrically distributed annular protrusions for increasing the extrusion force between the top plug and the top plate.
[0006] Furthermore, the elastic strip includes an adhesive portion, and the adhesive portion is provided with evenly distributed grooves for preventing the glue from flowing in all directions.
[0007] Furthermore, a fixing needle is slidably connected to a side of the elastic strip away from the adhesive portion, a rubber plug is provided on the base, and the fixing needle is limitedly matched with the rubber plug.
[0008] Furthermore, the extrusion sleeve is composed of a vertical portion and an elastic portion, and an extrusion sheet evenly distributed in the circumferential direction is installed between the vertical portion and the elastic portion.
[0009] Furthermore, the element is wound by electrolytic paper and centrally symmetrically distributed aluminum foil, the centrally symmetrically distributed aluminum foil is divided into two types, anode and cathode, the aluminum foil is fixed with a conductive column and a card block, the conductive column penetrates the top plug and the top plate, and the three are sealed together, the rotating column is fixed with centrally symmetrically distributed buckles, and the buckles are limitedly matched with the adjacent card blocks.
[0010] Furthermore, the conductive column and the clamping block on the same aluminum foil are located in the same vertical line, so as to maintain the squeezing force between the adjacent aluminum foils and the adjacent electrolytic papers in a relatively balanced state.
[0011] Furthermore, the outer side of the buckle is provided with symmetrically distributed inclined surfaces, and the upper side thereof is provided with an opening, the size of the upper opening is larger than the bottom area of the adjacent clamping block, and the fitting part between the clamping block and the adjacent buckle has a certain elasticity.
[0012] Furthermore, it also includes a cone, which is sealingly and slidably connected in the rotating column, the cone penetrates the lower side of the rotating column, the rotating column is provided with an elastic limiting plate that cooperates with the cone, an air guide hole is provided in the cone, and a sealing cylinder that seals with the rotating column is fixedly connected in the aluminum shell.
[0013] A method for preparing a high-voltage conductive polymer solid-liquid hybrid aluminum electrolytic capacitor is applied to the above-mentioned high-voltage conductive polymer solid-liquid hybrid aluminum electrolytic capacitor. The specific preparation method is as follows: S1: etching the aluminum foil of the anode to form micro pits on the surface of the aluminum foil of the anode; S2: chemically forming the aluminum foil of the anode to form an aluminum oxide layer on the surface of the aluminum foil of the anode; S3: The mechanical claws clamp the base and clamp the rotating column and the base. After the electrolytic paper is clamped between the symmetrically distributed temperature-conducting columns, the mechanical claws drive the base and the rotating column to rotate together, and the electrolytic paper and the aluminum foil are wound into a shape to form an element; S4: After the element is made, the elastic strip is bonded to the outside of the element, and the fixing needle is inserted into the rubber plug on the base; S5: Move the base, the element and the elastic strip together to the manipulator of the impregnation area, and sequentially perform dispersion liquid impregnation, drying, polymer electrolyte impregnation, drying, and electrolyte impregnation on the element; S6: During the impregnation process, the element is always kept in a high pressure state. At this time, the robot controls the rotating column to drive the components on it to reciprocate along the base, so that the element is continuously loosened and tightened; S7: After the impregnation is completed, the vertical assembly is carried out. After the base, element and elastic strip are reset, the robot removes the base and adjacent parts, and installs them into the aluminum shell in the order of base, extrusion sleeve and top plug; S8: Aging of the aluminum shell and adjacent components is performed, and finally various real-time tests are performed on the entire device, and parameter labels are affixed.
[0014] Compared with the prior art, the present invention has at least the following beneficial effects: the present invention conducts heat from the middle of the element to the outside by the thermal conductive column, conducts heat generated outside the element by the elastic strip, and conducts heat to the aluminum shell through components such as the base and the extrusion sleeve. The heat conduction speed is increased by closely fitting the various layers of components, thereby providing a heat dissipation foundation for the high-voltage development of high-voltage conductive polymer solid-liquid hybrid aluminum electrolytic capacitors.
[0015] During the impregnation process, the present invention actively drives the rotating column to rotate along the base, thereby increasing the flow rate of the electrolyte in the element during the impregnation process, thereby increasing the efficiency of the element impregnation process, shortening the time required for element impregnation, and improving the overall time required for the production of the device.
[0016] The present invention replaces the cross structure at the bottom of the traditional aluminum shell with components such as a cone, which effectively prevents the aluminum shell from bursting due to accumulated air pressure and increases the resistance of the aluminum shell to external accidents. BRIEF DESCRIPTION OF THE DRAWINGS
[0017] Figure 1 It is a schematic diagram of the three-dimensional structure of the present invention; Figure 2 It is a three-dimensional structural schematic diagram of the aluminum shell, the top plug and the extrusion sleeve of the present invention; Figure 3 is a cross-sectional view of the top plug, top plate and extrusion sleeve of the present invention; Figure 4 An exploded view of the top plug, the element and the extrusion sleeve of the present invention; Figure 5 It is a three-dimensional structural schematic diagram of the base, elastic strip and extrusion sleeve of the present invention; Figure 6 This is a diagram of the relaxed state of the extrusion sleeve, the vertical portion and the extrusion sheet of the present invention; Figure 7 This is a schematic diagram of the base, electrolytic paper and aluminum foil of the present invention before winding; Figure 8 It is a schematic diagram of the three-dimensional structure of the rotating column, the elastic member and the temperature conducting column of the present invention; Fig. 9 It is a schematic diagram of the three-dimensional structure of the rotating column, the temperature conducting column and the buckle of the present invention; Fig.10 It is an exploded view of the rotating column, cone and elastic limiting plate of the present invention.
[0018] Markings in the figure are: 1-aluminum shell, 2-top plug, 3-base, 4-element, 5-elastic strip, 6-extrusion sleeve, 7-cone, 21-top plate, 31-rotating column, 32-elastic part, 33-temperature conduction column, 34-buckle, 41-electrolytic paper, 42-aluminum foil, 43-conductive column, 44-block, 51-adhesive part, 52-fixing needle, 61-vertical part, 62-extrusion sheet, 71-elastic limit sheet, 72-air guide hole. DETAILED DESCRIPTION
[0019] The present invention is described in detail below in conjunction with the accompanying drawings and specific embodiments, but is not intended to limit the present invention. It should be noted that the illustrations provided in the following embodiments are only schematic illustrations of the basic concept of the present invention, and the drawings only show components related to the present invention rather than being drawn according to the number, shape and size of components in actual implementation. The shape, quantity and proportion of each component in actual implementation may be changed at will, and the component layout may also be more complicated. In the present invention, except for the element 4 and its components, all other components are covered with an insulating layer, which will not affect the working principle of the element 4.
[0020] Embodiment 1: There is a gap between the element and the aluminum shell of the existing aluminum electrolytic capacitor, which will affect the thermal conductivity between the two. Although the existing aluminum electrolytic capacitor can make up for part of the above-mentioned thermal conductivity gap by filling the electrolyte, the thermal conductivity efficiency of the electrolyte is always lower than the thermal conductivity efficiency of the direct contact between the heat conductor and the heating element, which will undoubtedly restrict the development of aluminum electrolytic capacitors towards high voltage.
[0021] In addition to the above problems, when producing aluminum electrolytic capacitors, the existing device usually fixes the wound element 4 with tape after the element 4 is wound. This causes the gap between the electrolytic paper 41 and the aluminum foil 42 in the element 4 to always remain fixed. Since the distance between the electrolytic paper 41 and the aluminum foil 42 in the element 4 affects the capacitance value, the gap between the electrolytic paper 41 and the aluminum foil 42 needs to be smaller. This results in the subsequent processing steps of the element 4 by the existing impregnation device: the impregnation processing efficiency is low. The existing device usually needs to be impregnated under high pressure for more than 1.5 hours during impregnation to ensure that the polymer electrolyte and the electrolyte penetrate a large area of the etched part of the anode aluminum foil 42, resulting in a long impregnation time, which has a certain impact on the rapid manufacture of the device.
[0022] In view of the above two problems, the present invention proposes a high-voltage conductive polymer solid-liquid hybrid aluminum electrolytic capacitor. Figure 1-Figure 8 , including an aluminum shell 1, a top plug 2 and a base 3 are installed in the aluminum shell 1, and silicone grease is filled between the aluminum shell 1 and the base 3 to increase the contact area between the two and improve the heat dissipation efficiency. The top plug 2 is made of rubber material, and the lower side of the top plug 2 is slidably connected with a top plate 21. The top plate 21, the base 3, the rotating column 31, the elastic strip 5, the extrusion sleeve 6 and the two temperature-conducting columns 33 are all made of metal heat-conducting materials. The upper side of the top plate 21 is provided with symmetrically distributed annular protrusions. When the upper part of the aluminum shell 1 is annularly extruded by the existing pressing device so that the aluminum shell 1 and the top plug 2 are tightly fitted, the top plug 2 is deformed by force and stuck between the two annular protrusions of the top plate 21, which is used to increase the extrusion force applied by the top plate 21 to the top plug 2, thereby ensuring that the aluminum shell 1 and the top plate 2 1 and the top plug 2, a rotating column 31 is rotatably connected in the base 3, and an elastic member 32 is installed between the two, the elastic member 32 is a torsion spring, and the initial state of the elastic member 32 is a stored force state, which is used to increase the force to limit the torsion of the rotating column 31, thereby preventing the element 4 from loosening from the inside, and the rotating column 31 is fixedly connected to two centrally symmetrically distributed temperature conducting columns 33, and the temperature conducting columns 33 are used to conduct the heat of the element 4 outward, and the temperature conducting columns 33 are squeezed and matched with the top plate 21 to increase the contact area between the temperature conducting columns 33 and the top plate 21, thereby improving the heat exchange efficiency between the temperature conducting columns 33 and the top plate 21, and the element 4 is arranged on the outside of the temperature conducting column 33, and the element 4 is wound around the temperature conducting column 33 as shown in Figure 3 , Figure 4 and Figure 7As shown, an elastic strip 5 is fixed to the outside of the element 4, and the elastic strip 5 includes an adhesive portion 51. The inner surface of the adhesive portion 51 is provided with evenly distributed grooves, and the grooves are used to accommodate excess glue during adhesion to prevent the glue from flowing around and affecting the stability inside the device. The elastic strip 5 is adhered to the outermost side of the element 4 through the adhesive portion 51, replacing the existing adhesive tape to provide a stable limiting force to the outside of the element 4 to prevent the outside of the element 4 from loosening. The front side of the elastic strip 5 is slidably connected to a fixing needle 52, and a rubber plug is provided on the front side of the base 3. The fixing needle 52 is inserted into the rubber plug to fix one side of the elastic strip 5, and then the elastic strip 5 and the element 4 are fixed. The aluminum shell 1 is slidably connected to an extrusion sleeve 6, and the extrusion sleeve 6 is composed of a vertical portion 61 and an elastic portion (as shown in FIG. Figure 6 As shown in the figure, the vertical portion 61 is a rigid body, which is used to fit tightly with the aluminum shell 1 for heat conduction. A number of extrusion sheets 62 evenly distributed in the circumferential direction are installed between the vertical portion 61 and the elastic portion. Therefore, when the extrusion sleeve 6 is extruded, the elastic portion is deformed first, and then the extrusion sheet 62 is deformed. When the extrusion sleeve 6 is squeezed by the top plate 21 and the base 3 at the same time, the vertical portion 61 fits with the aluminum shell 1, and the elastic portion of the extrusion sleeve 6 fits with the elastic strip 5.
[0023] Reference Figure 7-Figure 9 The element 4 is wound by electrolytic paper 41 and two aluminum foils 42 symmetrically distributed in the center. The two aluminum foils 42 are divided into two types, the anode and the cathode. A conductive column 43 is fixedly connected to the upper side of the aluminum foil 42, and a clamping block 44 is fixedly connected to the lower side of the aluminum foil 42. The two are located in the same vertical line to prevent the conductive column 43 and the clamping block 44 from excessively squeezing the surrounding electrolytic paper 41, resulting in uneven distribution of electrolyte in the electrolytic paper 41. The conductive column 43 penetrates the top plug 2 and the top plate 21, and the three are sealed. The rotating column 31 is fixedly connected to the center of the electrolytic paper 41. There are two symmetrically distributed buckles 34, and an opening is set on the upper side of each buckle, the size of which is larger than the bottom area of the adjacent buckle 44. The joint between the buckle 44 and the adjacent buckle 34 has a certain elasticity. The outer side of the buckle 34 is provided with two symmetrically distributed inclined surfaces, which are used to enable the buckle 44 to be wound on the upper side of the rotating column 31. After passing through the upper inclined surface of the adjacent buckle 34, the buckle 34 quickly snaps into the adjacent buckle 34. The buckle 34 drives the aluminum foil 42 to rotate with the rotating column 31 by pushing the adjacent buckle 44 to move.
[0024] In the process of producing the device, the staff first etches and forms the anode aluminum foil 42 to form micro pits on the surface of the anode aluminum foil 42, and then prepares to wind the production element 4. The staff controls the manipulator of the existing winding device to grab a base 3, and fixes the base 3 and the rotating column 31 thereon by the manipulator (so that the base 3 and the rotating column 31 thereon remain relatively static), and inserts the temperature conducting column 33 into the middle of the electrolytic paper 41 to be wound (refer to Figure 7), and then the robot directly drives the base 3 and other parts to rotate. During the process of the base 3 and the temperature-conducting column 33 on it winding the electrolytic paper 41, the staff controls other conveying devices to insert two aluminum foils 42 into the gap of the wound electrolytic paper 41. The temperature-conducting column 33 drives the two adjacent aluminum foils 42 to wind together through the electrolytic paper 41, so that the electrolytic paper 41 and the aluminum foil 42 are wound together layer by layer to form the element 4. During the winding process of the aluminum foil 42, the block 44 gradually moves to the vicinity of the buckle 34, and the block 44 first contacts the outside of the buckle 34. During the rotation process, the block 44 is squeezed by the adjacent inclined surface on the buckle 34 and gradually moves to the upper side of the buckle 34. The block 44 is compressed upward to store force, and then the block 44 moves downward from the opening on the upper side of the buckle 34 and is inserted Into the buckle 34, when the element 4 is wound, the staff operates another robot to clamp the elastic strip 5 to the outside of the element 4, and apply glue on the adhesive part 51 of the elastic strip 5, and then the staff operates the robot to make the adhesive part 51 stick to the outside of the outermost electrolytic paper 41, and wind the elastic strip 5 around the outside of the element 4. At this time, the elastic strip 5 is in a power storage state, and the elastic strip 5 provides an outer tightening force for the element 4 to prevent the components in the element 4 from loosening. After the elastic strip 5 is wrapped around the outside of the element 4, the staff pushes the fixing needle 52 to move through the robot, and pushes the fixing needle 52 into the adjacent rubber plug to complete the connection between the elastic strip 5 and the base 3. Then the staff removes the base 3, the element 4 and the elastic strip 5 from the robot at the winding position.
[0025] When the element 4 is completed, the staff transports the base 3, the element 4, the elastic strip 5 and other parts to the impregnation robot. The impregnation robot first clamps the base 3 and puts the parts into the liquid of the impregnation device. During the impregnation process, in addition to the steps of pressurization in the normal production process, the robot slowly and reciprocatingly rotates the rotating column 31 on the base 3, and the angle of each reciprocating rotation of the rotating column 31 is about 180°. When the robot drives the rotating column 31 to rotate clockwise ( Figure 1 From a top-down perspective), the elastic member 32 twists and stores force, and the rotating column 31 drives the electrolytic paper 41 and the aluminum foil 42 to rotate through the temperature conducting column 33 and the buckle 34. The rotation of the electrolytic paper 41 and the aluminum foil 42 reduces the winding tightness, and the element 4 spreads out while stretching the elastic strip 5 outward, and the outermost electrolytic paper 41 drives the elastic strip 5 to rotate together, so that the elastic strip 5 twists and expands, and the elastic strip 5 gradually accumulates force. At this time, because the winding of the electrolytic paper 41 and the aluminum foil 42 becomes loose, the gap between the two is larger, which makes it easier for the liquid to penetrate from the gap, shortening the overall impregnation time of the element 4. When the manipulator drives the rotating column 31 to rotate counterclockwise ( Figure 1From a top-down perspective), the elastic force of the elastic member 32 is gradually released, and the rotating column 31 drives the electrolytic paper 41 and the aluminum foil 42 to rotate and tighten through the components such as the temperature conducting column 33 and the buckle 34, so that the tightness of the winding of the electrolytic paper 41 and the aluminum foil 42 increases. The elastic strip 5 is also released and reset in the reverse direction according to the above principle. Because the winding of the electrolytic paper 41 and the aluminum foil 42 becomes tighter, the electrolytic paper 41 and the aluminum foil 42 squeeze the liquid between them during the winding process, so that the liquid flows outward and impacts the etched surface of the anode aluminum foil 42, prompting the liquid to impact into the micro-pits on the etched surface of the anode aluminum foil 42, prompting the micro-air film inside to be broken and discharged as soon as possible, thereby increasing the impregnation efficiency of the element 4 and increasing the bonding rate of the anode aluminum foil 42 and the liquid.
[0026] During the above-mentioned impregnation process, the manipulator reciprocates to control the rotation of the rotating column 31 to drive the flow of liquid, making the impregnation process of the element 4 smoother and more stable, shortening the time required for the complete impregnation of the element 4, and when the impregnation of the element 4 is completed, the manipulator actively controls the rotating column 31 to rotate and reset. At this time, the elastic force of the elastic member 32 and the elastic strip 5 is only used to maintain the wound element 4 from loosening, and is not used as the power for actively winding the element 4. The staff controls the element 4 to be impregnated with the dispersion liquid, the polymer electrolyte and the electrolyte respectively according to the above-mentioned steps, and after the dispersion liquid and the polymer electrolyte are impregnated, the existing drying device is used to dry and heat the element 4 to form a solid electrolyte layer in the element 4. After the element 4 is impregnated with the electrolyte, the staff takes the element 4 from the manipulator of the impregnation device Next, the device is prepared to be assembled as a whole. The staff first applies some silicone grease on the bottom of the aluminum shell 1 to increase the contact area between the base 3 and the bottom of the aluminum shell 1. Then the staff inserts the base 3, extrusion sleeve 6, top plate 21 and top plug 2 into the aluminum shell 1 in sequence. At this time, because the elastic part of the extrusion sleeve 6 is made of elastic material, the resistance between the extrusion sleeve 6 and the elastic strip 5 is small, and after insertion, the extrusion sleeve 6 remains in contact with the aluminum shell 1 and the elastic strip 5 under the elastic force of the elastic part thereof. After all parts are installed in the aluminum shell 1, the staff controls the existing pressing machine to extrude the upper part of the aluminum shell 1 along a circular path, so that the aluminum shell 1 is deformed and the top plug 2 is squeezed. After the top plug 2 is deformed under pressure, it is embedded between the two annular protrusions of the top plate 21 to increase the sealing effect between the top plug 2 and the aluminum shell 1.
[0027] When the device is assembled, the elastic strip 5 is wound on the outside of the element 4, and the two thermal conductive columns 33 are inserted in the center of the element 4, and they work together to conduct the heat generated by the element 4 during the working process to the outside. The heat is first transferred to the top plate 21, the base 3 and the extrusion sleeve 6, and then the heat is transferred to the aluminum shell 1 by the top plug 2, the base 3 and the extrusion sleeve 6 to dissipate outward. Because the top plate 21, the elastic strip 5 and the element 4 are kept in a fitted state, the top plate 21 and the elastic strip 5 are more efficient in conducting the heat generated by the element 4, and the extrusion sleeve 6 is squeezed by the top plate 21, the elastic strip 5 and the base 3, and the extrusion sheet 62 is compressed and stored. The extrusion sheet 62 squeezes the elastic part of the extrusion sleeve 6 to deform to a state of being in fit with the elastic strip 5. The extrusion sheet 62 also squeezes the vertical part 61 to keep it in fit with the aluminum shell 1. Therefore, the heat transfer efficiency between the elastic strip 5 and the aluminum shell 1 and the extrusion sleeve 6 is higher, thereby ensuring that the elastic strip 5, the thermal conductive column 33, the extrusion sleeve 6 and other components cooperate with each other to effectively dissipate heat from the element 4.
[0028] After the vertical assembly is completed, the staff will carry out aging and other steps on the device. After completing all the processes, they will conduct various real-time tests on the device as a whole, affix parameter labels, and finally pack the device in batches.
[0029] Embodiment 2: The bottom of the existing aluminum electrolytic capacitor usually needs to be designed with a cross structure. The cross structure is used to reduce the connection strength of the bottom of the aluminum shell. When the electrolyte in the aluminum electrolytic capacitor is unbalanced and vaporized, the vaporized electrolyte will expand rapidly in the aluminum shell. At this time, the expanding gas will first burst the bottom of the aluminum shell, so as to avoid the gradual accumulation of air pressure in the aluminum shell and a large-scale explosion. However, because the cross structure reduces the overall structural strength of the bottom of the aluminum electrolytic capacitor, if non-internal reasons are encountered, such as foreign objects applying a certain pressure to the cross structure of the aluminum shell in an accidental situation, it will also cause damage to this position, causing the aluminum electrolytic capacitor to leak.
[0030] Therefore, in view of the above problems, based on Example 1, Fig. 9 and Fig.10 , also includes a cone 7, which is composed of a piston and a conical needle. The cone 7 is sealingly and slidably connected in the rotating column 31. The conical needle of the cone 7 penetrates the lower side of the rotating column 31. The rotating column 31 is provided with an elastic limiting piece 71. The elastic limiting piece 71 limits the cone 7 by its own elastic force, hindering the cone 7 from moving downward. An air guide hole 72 is provided in the cone 7 to assist the internal gas to be discharged outwardly. A sealing cylinder that is sealed with the rotating column 31 is fixed in the aluminum shell 1. The sealing cylinder is coaxial with the rotating column 31 and the cone 7, and is used to limit the flow of gas to prevent the gas from diffusing to a large extent to the lower side of the rotating column 31 through the air guide hole 72, causing the cone 7 to lose the thrust of the gas.
[0031] Because there is no cross structure on the aluminum shell 1, the resistance of the aluminum shell 1 to external forces is not affected. When the electrolyte between the electrolytic paper 41 and the aluminum foil 42 vaporizes due to an accident, the gas flows into the cavity on the upper side of the cone 7 in the rotating column 31. The cone 7 is pushed downward by the gas. When the thrust exerted on the cone 7 is greater than the extrusion force of the elastic limit plate 71, the cone 7 squeezes the elastic limit plate 71 and moves downward until the lower end of the cone 7 pierces the aluminum shell 1. At this time, the gas is discharged outward from the air guide hole 72 to avoid large-scale explosion of the aluminum electrolytic capacitor. After the staff finds that the cone 7 protrudes out of the aluminum shell 1, they recover and replace the device.
[0032] Example 3: A method for preparing a high voltage conductive polymer solid-liquid hybrid aluminum electrolytic capacitor, referring to Figure 1-Figure 10 , a high-voltage conductive polymer solid-liquid hybrid aluminum electrolytic capacitor used in the above-mentioned embodiment 2, the specific preparation method is as follows: S1: etching the aluminum foil 42 of the anode to form micro pits on the surface of the aluminum foil 42 of the anode; S2: chemically forming the aluminum foil 42 of the anode so that an aluminum oxide layer is formed on the surface of the aluminum foil 42 of the anode; S3: The mechanical claws clamp the base 3 and clamp the rotating column 31 and the base 3. After the electrolytic paper 41 is clamped between the symmetrically distributed temperature conducting columns 33, the mechanical claws drive the base 3 and the rotating column 31 to rotate together, and the electrolytic paper 41 and the aluminum foil 42 are wound into shape to form the element 4. S4: After the element 4 is manufactured, the elastic strip 5 is bonded to the outer side of the element 4, and the fixing needle 52 is inserted into the rubber plug on the base 3; S5: moving the base 3, the element 4 and the elastic strip 5 together to the impregnation area manipulator, and sequentially performing dispersion liquid impregnation, drying, polymer electrolyte impregnation, drying, and electrolyte impregnation on the element 4; S6: During the impregnation process, the element 4 is always kept in a high pressure state. At this time, the manipulator controls the rotating column 31 to drive the components on it to reciprocate along the base 3, so that the element 4 is continuously relaxed and wound up; S7: After the impregnation is completed, the assembly is performed, and after the base 3, the element 4 and the elastic strip 5 are reset, the robot removes the base 3 and adjacent parts, and installs the base 3, the extrusion sleeve 6 and the top plug 2 into the aluminum shell 1 in the order; S8: Perform aging and other steps on the aluminum shell 1 and adjacent components, and finally perform various real-time tests on the entire device and attach parameter labels.
[0033] It should be understood that the above description is only for exemplary purposes and is not intended to limit the present invention. Those skilled in the art will understand that variations of the present invention will be included within the scope of protection claimed by the present invention.
Claims
1. A high-voltage conductive polymer solid-liquid hybrid aluminum electrolytic capacitor, comprising an aluminum shell (1), a top plug (2) and a base (3) installed in the aluminum shell (1), a top plate (21) slidably connected to the lower side of the top plug (2), characterized in that: The invention also comprises a rotating column (31), the rotating column (31) being rotatably connected to the base (3), and an elastic member (32) being installed between the two, the rotating column (31) being fixedly connected to a centrally symmetrically distributed temperature conducting column (33), the temperature conducting column (33) being extrusion-fitted with the top plate (21), an element (4) being arranged on the outside of the temperature conducting column (33), an elastic strip (5) being fixedly connected to the outside of the element (4), an extrusion sleeve (6) being slidably connected to the inside of the aluminum shell (1), and the aluminum shell (1), the top plate (21), the base (3) and the elastic strip (5) are all extrusion-fitted with the extrusion sleeve (6).
2. A high voltage conductive polymer solid-liquid hybrid aluminum electrolytic capacitor according to claim 1, characterized in that: The top plug (2) is made of rubber material, the top plate (21), the base (3), the rotating column (31), the elastic strip (5), the extrusion sleeve (6) and the symmetrically distributed heat-conducting columns (33) are all made of metal heat-conducting material, and the top side of the top plate (21) is provided with symmetrically distributed annular protrusions for increasing the extrusion force between the top plug (2) and the top plate (21).
3. A high voltage conductive polymer solid-liquid hybrid aluminum electrolytic capacitor according to claim 2, characterized in that: The elastic strip (5) comprises an adhesive portion (51), and the adhesive portion (51) is provided with evenly distributed grooves for preventing glue from flowing in all directions.
4. The high voltage conductive polymer solid-liquid hybrid aluminum electrolytic capacitor according to claim 3, characterized in that: A fixing needle (52) is slidably connected to a side of the elastic strip (5) away from the adhesive portion (51), a rubber plug is provided on the base (3), and the fixing needle (52) is limitedly matched with the rubber plug.
5. The high voltage conductive polymer solid-liquid hybrid aluminum electrolytic capacitor according to claim 4, characterized in that: The extrusion sleeve (6) is composed of a vertical portion (61) and an elastic portion, and an extrusion sheet (62) evenly distributed in the circumferential direction is installed between the vertical portion (61) and the elastic portion.
6. A high voltage conductive polymer solid-liquid hybrid aluminum electrolytic capacitor according to claim 5, characterized in that: The element (4) is wound by electrolytic paper (41) and aluminum foil (42) distributed symmetrically at the center. The aluminum foil (42) distributed symmetrically at the center is divided into two types: an anode and a cathode. The aluminum foil (42) is fixedly connected with a conductive column (43) and a clamping block (44). The conductive column (43) penetrates the top plug (2) and the top plate (21), and the three are sealed together. The rotating column (31) is fixedly connected with a clamping buckle (34) distributed symmetrically at the center. The clamping buckle (34) is limitedly matched with the adjacent clamping block (44).
7. A high voltage conductive polymer solid-liquid hybrid aluminum electrolytic capacitor according to claim 6, characterized in that: The conductive column (43) and the clamping block (44) on the same aluminum foil (42) are located in the same vertical line, so as to maintain a relatively balanced state of the extrusion force between adjacent aluminum foils (42) and adjacent electrolytic papers (41).
8. The high voltage conductive polymer solid-liquid hybrid aluminum electrolytic capacitor according to claim 7, characterized in that: The outer side of the buckle (34) is provided with symmetrically distributed inclined surfaces, and the upper side thereof is provided with an opening, the size of the upper opening being larger than the bottom area of the adjacent clamping block (44), and the fitting portion between the clamping block (44) and the adjacent buckle (34) has a certain elasticity.
9. The high-voltage conductive polymer solid-liquid hybrid aluminum electrolytic capacitor according to claim 8, characterized in that: The invention also comprises a cone (7), wherein the cone (7) is sealingly slidably connected to the rotating column (31), the cone (7) penetrates the lower side of the rotating column (31), the rotating column (31) is provided with an elastic limiting piece (71) which is limitedly matched with the cone (7), an air guide hole (72) is provided in the cone (7), and a sealing cylinder which is sealingly matched with the rotating column (31) is fixedly connected to the aluminum shell (1).
10. A method for preparing a high-voltage conductive polymer solid-liquid hybrid aluminum electrolytic capacitor, applied to the high-voltage conductive polymer solid-liquid hybrid aluminum electrolytic capacitor according to claim 9, characterized in that: The specific preparation method is as follows: S1: etching the aluminum foil (42) of the anode to form micro pits on the surface of the aluminum foil (42) of the anode; S2: chemically treating the aluminum foil (42) of the anode so that an aluminum oxide layer is formed on the surface of the aluminum foil (42) of the anode; S3: The mechanical claws clamp the base (3) and clamp the rotating column (31) and the base (3). After the electrolytic paper (41) is clamped between the symmetrically distributed temperature conducting columns (33), the mechanical claws drive the base (3) and the rotating column (31) to rotate together, and the electrolytic paper (41) and the aluminum foil (42) are rolled into shape to form an element (4); S4: After the element (4) is manufactured, the elastic strip (5) is bonded to the outer side of the element (4), and the fixing pin (52) is inserted into the rubber plug on the base (3); S5: moving the base (3), the element (4) and the elastic strip (5) together to the impregnation area manipulator, and sequentially performing the following operations on the element (4): impregnation with dispersion liquid, drying, impregnation with polymer electrolyte, drying, and impregnation with electrolyte; S6: During the impregnation process, the element (4) is always kept in a high pressure state. At this time, the robot controls the rotating column (31) to drive the components on it to reciprocate along the base (3), so that the element (4) is continuously loosened and tightened; S7: After the impregnation is completed, the assembly is performed vertically. After the base (3), the element (4) and the elastic strip (5) are reset, the robot removes the base (3) and adjacent parts and installs the base (3), the extrusion sleeve (6) and the top plug (2) into the aluminum shell (1) in the order of the base (3); S8: The aluminum shell (1) and adjacent parts are subjected to aging and other steps, and finally the entire device is subjected to various real-time tests and parameter labels are affixed.