High-flatness FPC thin plate single-face pattern hole filling manufacturing method
Through the bonding of the carrier board and the circuit board and the vacuum adsorption and flattening treatment, the wrinkles and blocking problems of thin circuit boards during the filling process are solved, the processing efficiency is improved and the completion quality is enhanced, and the filling of high flatness is achieved Hole effect.
Patent Information
- Application Number
- CN202411176439.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-26
- Publication Date
- 2024-12-03
- Estimated Expiration
- 2044-08-26
AI Technical Summary
Thin circuit boards are prone to wrinkles and blocking problems during single-sided graphic hole filling process, and strengthening of conventional fixtures will cause the inclusion of potions in the board, affecting the quality of the product.
The bearing method of the carrier plate with rigid characteristics and ultra-thin circuit board is adopted. The carrier plate is formed by a hot press roller film press, and the vacuum adsorption table is flattened. The hole filling processing is carried out in combination with the graphic hole filling processing line to ensure that Flatness of circuit board during hole filling process.
It effectively reduces product wrinkles and plate blocking problems, improves processing efficiency, avoids the hidden potions in the board, and enhances the reinforcement effect of the dry film protective film, reducing the risk of shedding.
Smart Images

Figure CN119072012A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the field of printed circuit board manufacturing technology, and in particular to a method for manufacturing single-sided pattern hole filling of an FPC thin plate with high flatness. Background Art
[0002] Circuit board can be called printed circuit board or printed circuit board, which is an important electronic component, a support for electronic components, and a provider of electrical connections for electronic components. Due to the development trend of circuit boards, thin circuit boards (i.e. thin plates) have gradually appeared on the market, and their board structure has a thinner thickness feature than conventional circuit boards.
[0003] At present, for circuit boards with a thickness of less than 0.15mm, the thin plates with single-sided patterned hole filling lines in the industry often use a special fixture with double-sided tape to fill the holes. The product is electroplated by covering the whole board with dry film on one side and patterning the circuit on the other side. The thinner the circuit board, the worse the support strength of the circuit board when using conventional fixtures for patterned hole filling. The circuit board will have quality problems such as wrinkles and blockages in the hole filling lines. In addition, even if a reinforced fixture is reluctantly used to improve the problem that thin boards are not convenient for patterned hole filling, it will also make the circuit board more prone to the problem of hidden chemicals in the board, greatly affecting the molding quality of the circuit board. Summary of the invention
[0004] Based on this, it is necessary to provide a method for making a single-sided patterned hole-filling FPC sheet with high flatness in view of the deficiencies in the prior art.
[0005] A method for making a single-sided patterned hole-filling FPC sheet with high flatness comprises the following steps:
[0006] Step 1: Cut the carrier board, cut a copper-clad board that is not smaller than the circuit board, and use the roll material micro-adhesive film;
[0007] Step 2: Carrier board forming, using a hot-pressing roller laminator to stick a micro-adhesive film on both sides of the copper-clad laminate to form it into a rigid carrier board;
[0008] Step 3: Expose the circuit board. Expose the pattern circuit on one side of the circuit board and expose the entire board on the other side.
[0009] Step 4: PCB film pasting: Double-sided yellow glue, dry film and dry film protective film are pasted on both sides of the PCB in sequence, and the dry film protective film on the exposed side of the whole board is retained, and the dry film protective film on the exposed side of the graphic circuit is torn off;
[0010] Step 5: Development, both sides of the circuit board are developed;
[0011] Step 6: Flatten, place the developed circuit board on the vacuum adsorption table, and flatten the board surface through vacuum adsorption. When placing the circuit board, make sure that the exposed side of the circuit board is facing down;
[0012] Step 7: laminating the carrier board, laminating the carrier board from top to bottom on the upper surface of the circuit board that has been flattened by adsorption, that is, the micro-adhesive film of the carrier board and the dry film protective film of the circuit board are closely attached to form a combined board body to be processed for pattern filling;
[0013] Step 8: Graphic hole filling, remove the combined board from the vacuum adsorption table and send it to the graphic hole filling processing line for graphic hole filling processing;
[0014] Step 9: Unloading and separating boards. Unloading and unloading the assembled boards that have completed the pattern-filled hole processing from the processing line, and separating the circuit board from the carrier board, thereby obtaining a finished thin circuit board with pattern-filled holes.
[0015] Furthermore, the copper-clad laminate in step 1 is made of copper-free material and has a thickness of 0.6 mm.
[0016] Furthermore, the dry film protective film in step 4 is a release film, and the adhesion between the dry film protective film and the micro-mucosal film is smaller than the adhesion between the dry film and the micro-mucosal film.
[0017] Furthermore, when the film is pasted in step 4, a conductor plate is also pasted on one end of the circuit board, and the width of the conductor plate is consistent with the width of the circuit board.
[0018] Furthermore, the steps 3 to 6 are repeated once, and in step 7, the circuit board and the other side of the carrier are bonded together to form a combined board body supported by the carrier and with the circuit boards bonded on both sides to be processed with pattern filling.
[0019] In summary, the beneficial effects of the method for making a single-sided patterned hole filling FPC thin plate with high flatness of the present invention are: by designing a carrier plate with rigid characteristics to fit with an ultra-thin circuit board, the circuit board can be kept flat during the patterned hole filling process, which greatly reduces the risk of product wrinkles and board blockage during processing; and compared with conventional fixture clamping, the combined plate body formed by the carrier plate and the circuit board can not only effectively improve the problem of the quality of the finished circuit board due to the presence of chemicals in the board, but also can simultaneously support two circuit boards for patterned hole filling processing, greatly improving the processing efficiency; adding a wire board to the board head of the circuit board not only makes the circuit board easier to be pulled and thus smoothly transmitted on the production and processing line, but also can play a certain reinforcement role on the dry film protective film, reducing the risk of the dry film protective film falling off; the present invention is highly practical and has a strong promotional significance. BRIEF DESCRIPTION OF THE DRAWINGS
[0020] Figure 1It is a schematic diagram of the cross-sectional structure of a carrier board in a method for manufacturing a single-sided patterned hole-filling FPC sheet with high flatness according to the present invention;
[0021] Figure 2 It is a schematic diagram of the cross-sectional structure of a circuit board after film lamination in a method for making a single-sided patterned hole-filling FPC sheet with high flatness according to the present invention;
[0022] Figure 3 The present invention is a schematic diagram of the cross-sectional structure of a combined plate body in a method for manufacturing a single-sided patterned hole-filling FPC thin plate with high flatness. DETAILED DESCRIPTION
[0023] In order to further understand the features, technical means and specific objectives and functions achieved by the present invention, and analyze the advantages and spirit of the present invention, a further understanding is obtained through the following detailed description of the present invention in combination with the accompanying drawings and specific implementation methods.
[0024] like Figures 1 to 3 As shown, the present invention provides a method for making a single-sided patterned hole-filling FPC sheet with high flatness, comprising the following steps:
[0025] Step 1: Cut the carrier board 10, cut a 0.6mm thick copper-free copper-clad board 11, and use the roll micro-adhesive film 12;
[0026] Step 2: forming the carrier board 10, using a hot-pressing roller laminating machine to attach a micro-adhesive film 12 to both sides of the copper-clad laminate 11, so as to form the carrier board 10 into a rigid one;
[0027] Step 3: Exposure of the circuit board 21, respectively, one side of the two circuit boards 21 is subjected to pattern line exposure, and the other side is subjected to whole board exposure;
[0028] Step 4: Laminating the circuit board 21, first laminating the wire board (not shown) with the same width on one end of the two circuit boards, and then laminating the double-sided yellow glue (not shown), the dry film 22 and the dry film protective film 23 on both sides of the two circuit boards 21 in turn, wherein the dry film protective film 23 is a release film, and the adhesion between the dry film protective film 23 and the micro-mucosal film 12 is less than the adhesion between the dry film 22 and the micro-mucosal film 12, wherein the dry film protective film 23 on the exposed side of the whole board is retained, and the dry film protective film 23 on the exposed side of the pattern circuit is torn off;
[0029] Step 5: Development, both sides of the two circuit boards 21 are developed;
[0030] Step 6: Flattening, placing one of the developed circuit boards 21 on a vacuum adsorption table, and flattening the board surface by vacuum adsorption. When placing the circuit board 21, ensure that the exposed side of the pattern circuit of the circuit board 21 faces downward;
[0031] Step 7: Laminating the carrier 10, laminating the carrier 10 from top to bottom on the upper surface of the circuit board 21 flattened by adsorption, that is, the micro-adhesive film 12 of the carrier 10 is tightly attached to the dry film protective film 23 of the circuit board 21, and then taking the carrier 10 with the circuit board 21 attached on one side from the vacuum adsorption table, and then placing another circuit board 21 on the vacuum adsorption table to flatten it and laminating the other side of the carrier 10 thereto, and finally forming a combined board body 30 to be processed by pattern filling;
[0032] Step 8: Pattern hole filling, removing the combined plate body 30 from the vacuum adsorption table and sending it to the pattern hole filling processing line for pattern hole filling processing;
[0033] Step 9: Unloading and separating the boards. Unloading and unloading the assembled board 30 that has completed the pattern-filled hole processing from the processing line, and separating the circuit board 21 from the carrier board 10, thereby obtaining a finished thin circuit board 21 with pattern-filled holes.
[0034] In summary, the beneficial effects of the method for making a single-sided patterned hole filling FPC thin plate with high flatness of the present invention are: by designing a carrier board 10 with rigid characteristics to fit with an ultra-thin circuit board 21, the circuit board 21 can remain flat during the patterned hole filling process, greatly reducing the risk of product wrinkles and board blockage during processing; and compared with conventional fixture clamping, the combined board body 30 formed by the carrier board 10 and the circuit board 21 can not only effectively improve the problem of the potion hidden in the board affecting the quality of the finished product of the circuit board 21, but also can simultaneously support two circuit boards 21 for patterned hole filling processing, greatly improving the processing efficiency; adding a wire board to the board head of the circuit board 21 not only makes the circuit board 21 easier to be pulled and thus smoothly transmitted on the production and processing line, but also can play a certain reinforcement role on the dry film protective film 23, reducing the risk of the dry film protective film 23 falling off; the present invention is highly practical and has a strong promotional significance.
[0035] The above-mentioned embodiment only expresses one implementation method of the invention, and its description is relatively specific and detailed, but it cannot be understood as limiting the scope of the invention patent. It should be pointed out that for ordinary technicians in this field, several modifications and improvements can be made without departing from the inventive concept, which all belong to the protection scope of the invention. Therefore, the protection scope of the invention patent shall be based on the attached claims.
Claims
1. A method for making single-sided patterned holes on a high-flatness FPC sheet. It is characterized in that The steps include: Step 1: Cut the carrier board, cut a copper-clad board that is not smaller than the circuit board, and use the roll material micro-adhesive film; Step 2: Carrier board forming, using a hot-pressing roller laminator to stick a micro-adhesive film on both sides of the copper-clad laminate to form it into a rigid carrier board; Step 3: Expose the circuit board. Expose the pattern circuit on one side of the circuit board and expose the entire board on the other side. Step 4: PCB film pasting: Double-sided yellow glue, dry film and dry film protective film are pasted on both sides of the PCB in sequence, and the dry film protective film on the exposed side of the whole board is retained, and the dry film protective film on the exposed side of the graphic circuit is torn off; Step 5: Development, both sides of the circuit board are developed; Step 6: Flatten, place the developed circuit board on the vacuum adsorption table, and flatten the board surface through vacuum adsorption. When placing the circuit board, make sure that the exposed side of the circuit board is facing down; Step 7: laminating the carrier board, laminating the carrier board from top to bottom on the upper surface of the circuit board that has been flattened by adsorption, that is, the micro-adhesive film of the carrier board and the dry film protective film of the circuit board are closely attached to form a combined board body to be processed for pattern filling; Step 8: Graphic hole filling, remove the combined board from the vacuum adsorption table and send it to the graphic hole filling processing line for graphic hole filling processing; Step 9: Unloading and separating boards. Unloading and unloading the assembled boards that have completed the pattern-filled hole processing from the processing line, and separating the circuit board from the carrier board, thereby obtaining a finished thin circuit board with pattern-filled holes.
2. The method for making a single-sided patterned hole-filling FPC sheet with high flatness as claimed in claim 1, Features: The copper clad laminate in step 1 is made of copper-free material and has a thickness of 0.6 mm.
3. The method for making a single-sided patterned hole-filling FPC sheet with high flatness as claimed in claim 1, Features: The dry film protective film in step 4 is a release film, and the adhesion between the dry film protective film and the micro-mucosal film is smaller than the adhesion between the dry film and the micro-mucosal film.
4. The method for making a single-sided patterned hole-filling FPC sheet with high flatness as claimed in claim 1, Features: When the film is pasted in step 4, a conductor plate is also pasted on one end of the circuit board, and the width of the conductor plate is consistent with the width of the circuit board.
5. The method for making a single-sided patterned hole-filling FPC sheet with high flatness as claimed in claim 1, Features: The steps 3 to 6 are repeated once, and in step 7, the circuit board and the other side of the carrier board are bonded together to form a combined board body supported by the carrier board and bonded to the circuit boards on both sides to be processed with patterned holes.
Citation Information
Patent Citations
Sandwich structure for ultrathin laminated board processing and laminated board manufacturing method
CN105934110A
Carrier for manufacturing substrate and method of manufacturing substrate using the same
TW201124027A
Method of manufacturing wiring substrate and method of manufacturing electronic component device