Manufacturing method of carbon fiber composite material mobile phone backboard

Through carbon fiber composite materials and high-temperature molding technology, the weight and corrosion resistance of traditional mobile phone back panel materials are solved, lightweight design and efficient molding are achieved, and production efficiency and product life are improved.

CN119078219AInactive Publication Date: 2024-12-06LIANYUNGANG SHENYING CARBON BIKE CO LTD
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
CN202411464200.2
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-10-21
Publication Date
2024-12-06
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

The back panel materials of traditional mobile phones are prone to plastic deformation, are not resistant to acid and alkali corrosion, are simple in shape, heavier in weight, and have low molding process efficiency.

Method used

Using carbon fiber composite materials, the high-temperature molding process of preformed molds and silicone, combined with prepreg cloth and engraving technology of carbon fiber and resin, the lightweight design and efficient molding of the back panel of the mobile phone is achieved.

Benefits of technology

It realizes the lightweight, corrosion-resistant and diverse appearance of the carbon fiber mobile phone back panel, reduces the subsequent surface treatment process, and improves the production efficiency and product service life.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

The invention discloses a manufacturing method of a carbon fiber composite material mobile phone backboard. The method comprises the following steps: (1) preparing a pre-forming mold; (2) molding a pre-molding core mold; (3) preparing a carbon fiber mobile phone backboard forming die; (4) preparing raw materials; (5) preparing a carbon fiber mobile phone backboard preform; (6) forming the carbon fiber mobile phone backboard; (7) processing; and (8) surface treatment. Compared with a traditional mold pressing mode, the mold pressing and silica gel forming mode is adopted, so that the carbon fiber mobile phone backboard is light and thin in thickness and brighter in appearance, meanwhile, it can be guaranteed that lines of the appearance of the mobile phone backboard are clearer, the laying layer structure is 3k oblique / C45 / C0 / 3k oblique, disordered lines and distortion are avoided, subsequent surface treatment and other processes are conveniently reduced, and the production efficiency is improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of new material application, and in particular to a method for manufacturing a carbon fiber composite material mobile phone back panel. Background Art

[0002] Traditional mobile phone back panels are mostly made of glass, ceramics, metal and plastic materials, which have the disadvantages of easy plastic deformation, acid and alkali corrosion resistance, and drop resistance. In addition, due to the simple shape of glass, ceramics and metal, it is impossible to achieve curved surfaces and beautiful shapes, and the weight is heavy. Carbon fiber composite materials have excellent high specific strength, high specific modulus, light weight, corrosion resistance, strong designability, no plastic change, dimensional stability, and easy processing. To solve the shortcomings and disadvantages of traditional mobile phone back panels. However, the traditional molding process has the disadvantages of direct molding, easy distortion of fabric texture, or direct molding, long molding time, and low molding efficiency. Summary of the invention

[0003] The technical problem to be solved by the present invention is to provide a method for manufacturing a carbon fiber composite material mobile phone back panel with strong design, simple process and obvious weight reduction effect in view of the shortcomings of the prior art.

[0004] The technical problem to be solved by the present invention is achieved through the following technical solutions. The present invention is a method for manufacturing a carbon fiber composite material mobile phone back panel, and the steps of the method are as follows: (1) Preparation of preform mold According to the shape and shape of the mobile phone back panel, make a preform mold that is 5~10mm smaller than the outer contour of the mobile phone back panel; (2) Forming of preform core mold Heat the preform mold to 50-100°C, then evenly apply a water-based mold release agent in the mold cavity, fill the entire mold cavity with raw silicone, and then place it on a flat hot press for curing at 150-250°C for 1-3 hours to obtain a preform core mold; (3) Preparation of carbon fiber mobile phone back panel molding die According to the shape and shape of the mobile phone back panel, a mobile phone back panel forming mold with a 1:1 size to the outer contour of the mobile phone back panel is manufactured; (4) Raw material preparation The carbon fiber and resin are mixed in a certain proportion and molded to obtain a carbon fiber prepreg, and then the prepreg shape design is performed using computer-aided design software, and the obtained carbon fiber prepreg is carved into a desired mobile phone back panel shape using an engraving machine; (5) Preparation of carbon fiber mobile phone back panel preform The carbon fiber prepreg having the shape of the mobile phone back panel obtained in step (4) is laid on the preform core mold obtained above according to the set structure ply sequence to obtain a carbon fiber mobile phone back panel preform; (6) Carbon fiber mobile phone back panel molding Heat the carbon fiber mobile phone back panel forming mold to 50-100°C, then evenly brush the oily release agent in the mold cavity, put the above-mentioned carbon fiber mobile phone back panel preform, then put the preform core mold, and cover the mold, then put it in a flat vulcanizer for curing at 150-250°C for 40-180 minutes, then put the mold on a cooling table to cool down to 50-80°C, finally open the mold, and take out the formed mobile phone back panel blank; (7) Processing Remove the excess part of the mobile phone back panel blank and perform CNC processing according to the finished product size; (8) Surface treatment According to the product identification and appearance requirements, the surface of the mobile phone back panel can be polished, painted and labeled.

[0005] The technical problem to be solved by the present invention can be further achieved by the following technical solution. For the method for manufacturing the carbon fiber composite material mobile phone back panel described above, in step (1), the preform mold is 4 to 8 mm smaller than the outer contour of the mobile phone back panel.

[0006] The technical problem to be solved by the present invention can be further achieved by the following technical solution. For the method for manufacturing the carbon fiber composite material mobile phone back panel described above, the resin used in step (4) is any one of epoxy resin, phenolic resin, bismaleimide resin, unsaturated polyester, and thermoplastic resin.

[0007] The technical problem to be solved by the present invention can be further achieved by the following technical solution. For the method for manufacturing the carbon fiber composite material mobile phone back panel as described above, the surface treatment in step (8) also includes performing a bright finish or texture treatment on the surface of the mobile phone back panel.

[0008] The technical problem to be solved by the present invention can be further achieved by the following technical scheme. For the method for manufacturing the carbon fiber composite material mobile phone back panel described above, the thickness of the carbon fiber composite material mobile phone back panel manufactured by this method is 0.5~2mm.

[0009] Compared with the prior art, the present invention adopts a molding + silicone molding method to produce a carbon fiber composite material mobile phone back panel. This molding method can make the appearance of the carbon fiber mobile phone back panel brighter, and at the same time ensure that the texture of the mobile phone back panel is clearer and has no random texture or distortion, which is convenient for reducing subsequent surface treatment processes and helps to improve production efficiency. DETAILED DESCRIPTION

[0010] In order to make the purpose, technical solution and advantages of the embodiments of the present invention clearer, the technical solution in the present invention will be clearly and completely described below in combination with the embodiments of the present invention. Obviously, the described embodiments are part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0011] A method for manufacturing a carbon fiber composite material mobile phone back panel, wherein the carbon fiber composite material mobile phone back panel is manufactured by using a resin-impregnated carbon fiber prepreg cloth + silicone + high-temperature molding process, and the specific steps of the method are as follows: (1) Preparation of preform mold According to the shape and shape of the mobile phone back panel, the production of the preform mold is the basis of the entire process. It needs to be accurately produced according to the design drawings of the mobile phone back panel to ensure that the final product can perfectly fit the mobile phone body while maintaining the required appearance and dimensional accuracy. A preform mold that is 5~10mm smaller than the outer contour of the mobile phone back panel needs to be made; preferably, the preform mold is 4~8mm smaller than the outer contour of the mobile phone back panel; the preform mold is a certain size smaller than the outer contour of the mobile phone back panel (such as 4~8mm) to take into account the expansion of the material during high-temperature molding and the needs of subsequent processing. Secondly, the material of the preform mold needs to have good heat resistance and wear resistance to ensure stability and durability for long-term use; (2) Forming of preform core mold Heat the preform mold to 50-100°C, then evenly apply a water-based release agent in the mold cavity, fill the entire mold cavity with raw silicone, and place it on a flat hot press at 150-250°C for 1-3 hours to cure and shape it. Then, a preform core mold is obtained, which is used to support and shape the subsequent molding process to ensure that the carbon fiber material can be cured in the predetermined shape. The molding of the preform core mold is one of the key steps in making the carbon fiber mobile phone back panel. The selection of silicone and the curing conditions (such as temperature and time) are crucial to the quality and stability of the core mold. (3) Preparation of carbon fiber mobile phone back panel molding die According to the shape and shape of the mobile phone back panel, a mobile phone back panel forming mold with a 1:1 size to the outer contour of the mobile phone back panel needs to be made; The production of the mobile phone back panel molding mold needs to be carried out strictly in accordance with the design size of the mobile phone back panel. This mold will be used in the final molding process to ensure that the carbon fiber mobile phone back panel can have the required appearance and dimensional accuracy. The material and manufacturing process of the molding mold also need to take into account factors such as heat resistance, wear resistance and stability; (4) Raw material preparation Carbon fiber and resin are mixed in a certain proportion and molded to obtain carbon fiber prepreg, with a ply structure of 3k oblique / C45 / C0 / 3k oblique... This alternating plying method can effectively improve the strength and toughness of the material, and then the shape of the mobile phone back panel is absolutely unfolded through computer software, and the obtained carbon fiber prepreg is engraved with the desired mobile phone back panel shape through an engraving machine to ensure that the shape and size of the carbon fiber prepreg are consistent with the design requirements of the mobile phone back panel; Preferably, the resin used is any one of epoxy resin, phenolic resin, bismaleimide resin, unsaturated polyester, and thermoplastic resin; The mixing ratio of carbon fiber and resin has an important influence on the performance of the final product. Different types of resins have different physical and chemical properties. For example, epoxy resin has good adhesion and corrosion resistance, while phenolic resin has high heat resistance and mechanical strength. In actual application, it can be selected according to actual needs. (5) Preparation of carbon fiber mobile phone back panel preform By spreading the shape of the mobile phone back panel obtained above and laying it on the preformed core mold obtained above according to the set structure laying order, a carbon fiber mobile phone back panel preform can be obtained; During this process, the quality and accuracy of the paving needs to be strictly controlled to ensure that the final product has the required performance and appearance; (6) Carbon fiber mobile phone back panel molding Heat the carbon fiber mobile phone back panel molding mold to 50-100°C, then evenly brush the oily release agent in the mold cavity, put the above-mentioned carbon fiber mobile phone back panel preform, then put in the preform core mold and cover mold, and then put it in a flat vulcanizer at 150-250°C for 40-180 minutes of curing, place the mold on a cooling table to cool to 50-80°C, then open the mold and take out the molded mobile phone back panel blank; (7) Processing Remove the excess part of the mobile phone back panel blank and perform CNC processing according to the finished product size. During this process, the processing accuracy and surface quality need to be strictly controlled to ensure that the finished product can meet the design requirements and usage needs; (8) Surface treatment: The surface of the mobile phone back panel can be polished, painted and labeled according to the product identification and appearance requirements, or the surface of the mobile phone back panel can be polished or textured as needed. This can not only improve the appearance and texture of the product, but also enhance the brand identification and personalized characteristics of the product.

[0012] The thickness of the carbon fiber composite mobile phone back panel produced by this method is 0.5~2mm. It not only has the advantages of light weight, corrosion resistance, diverse appearance, noise reduction and sound insulation, but also has a simple structure and strong designability during production. The subsequent surface treatment and other processes are simple, which can not only improve production efficiency, but also reduce production costs.

[0013] Compared with the traditional molding method, the present invention adopts the molding method of molding + silicone, which makes the thickness of the carbon fiber mobile phone back plate thinner and brighter in appearance, and at the same time ensures that the texture of the mobile phone back plate is clearer. The ply structure is 3k oblique / C45 / C0 / 3k oblique, and there is no random grain distortion, which is convenient for reducing subsequent surface treatment processes and improving production efficiency. The carbon fiber mobile phone back panel produced by the present invention has the following characteristics: First: Lightweight Carbon fiber is a lightweight material with excellent strength and stiffness. Compared with traditional materials such as plastic or metal, the carbon fiber mobile phone back panel is lighter and easier to carry and wear for a long time; Second: Long service life Carbon fiber mobile phone back panel is impact-resistant, high and low temperature-resistant, waterproof, chemical corrosion-resistant, easy to clean, etc., making it more durable and longer service life than traditional materials such as plastic; Third: Compared with traditional materials, carbon fiber prepreg has been modified for electrical and thermal conductivity, which further optimizes the heat dissipation performance of carbon fiber composite materials. Therefore, the carbon fiber mobile phone back panel can bring better user experience to users.

Claims

1. A method for manufacturing a carbon fiber composite material mobile phone back panel, characterized in that: The steps of this method are as follows: (1) Preparation of preform mold According to the shape and shape of the mobile phone back panel, make a preform mold that is 5~10mm smaller than the outer contour of the mobile phone back panel; (2) Forming of preform core mold Heat the preform mold to 50-100°C, then evenly apply a water-based mold release agent in the mold cavity, fill the entire mold cavity with raw silicone, and then place it on a flat hot press for curing at 150-250°C for 1-3 hours to obtain a preform core mold; (3) Preparation of carbon fiber mobile phone back panel molding die According to the shape and shape of the mobile phone back panel, a mobile phone back panel forming mold with a 1:1 size to the outer contour of the mobile phone back panel is manufactured; (4) Raw material preparation The carbon fiber and resin are mixed in a certain proportion and molded to obtain a carbon fiber prepreg, and then the prepreg shape design is performed using computer-aided design software, and the obtained carbon fiber prepreg is carved into a desired mobile phone back panel shape using an engraving machine; (5) Preparation of carbon fiber mobile phone back panel preform The carbon fiber prepreg having the shape of the mobile phone back panel obtained in step (4) is laid on the preform core mold obtained above according to the set structure ply sequence to obtain a carbon fiber mobile phone back panel preform; (6) Carbon fiber mobile phone back panel molding Heat the carbon fiber mobile phone back panel forming mold to 50-100°C, then evenly brush the oily release agent in the mold cavity, put the above-mentioned carbon fiber mobile phone back panel preform, then put the preform core mold, and cover the mold, then put it in a flat vulcanizer for curing at 150-250°C for 40-180 minutes, then put the mold on a cooling table to cool down to 50-80°C, finally open the mold, and take out the formed mobile phone back panel blank; (7) Processing Remove the excess part of the mobile phone back panel blank and perform CNC processing according to the finished product size; (8) Surface treatment According to the product identification and appearance requirements, the surface of the mobile phone back panel can be polished, painted and labeled.

2. The method for manufacturing a carbon fiber composite material mobile phone back panel according to claim 1, characterized in that: In step (1), the preform mold is 4 to 8 mm smaller than the outer contour of the mobile phone back panel.

3. The method for manufacturing a carbon fiber composite material mobile phone back panel according to claim 1, characterized in that: The resin used in step (4) is any one of epoxy resin, phenolic resin, bismaleimide resin, unsaturated polyester and thermoplastic resin.

4. The method for manufacturing a carbon fiber composite material mobile phone back panel according to claim 1, characterized in that: The surface treatment in step (8) also includes glossing or texture treatment on the surface of the back panel of the mobile phone.

5. The method for manufacturing a carbon fiber composite material mobile phone back panel according to claim 1, characterized in that: The thickness of the carbon fiber composite material mobile phone back panel produced by this method is 0.5~2mm.

Citation Information

Patent Citations

  • Carbon fiber composite material product and manufacturing method thereof

    CN101532253A

  • Carbon fiber shell and surface coating preparation method thereof

    CN105500595A

  • Carbon fiber and glass fiber mobile phone rear cover forming process and mobile phone rear cover

    CN114193809A

  • Manufacturing method of earphone shell made of carbon fiber composite material

    CN117734192A