Elastic fiber, elastic fiber covering yarn and laddering manufacturing method of elastic fiber covering yarn

By extending the guide wires multiple times and winding treatment of thermoplastic polyurethane fibers, the thread density and elongation of break of elastic fibers and yarns are improved, and the problem of residual and recycling of toxic reagents in the production of existing elastic fibers is solved, and the problem of the problem of residual and recycling of toxic reagents is achieved. Higher service life and environmental benefits.

CN119082971AInactive Publication Date: 2024-12-06SAN FANG CHEM IND
View PDF 6 Cites 0 Cited by

Patent Information

Application Number
CN202411168303.4
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2021-06-30
Filing Date
2021-09-29
Publication Date
2024-12-06
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

The reagents used in the production process of existing elastic fibers are toxic and irritating, and may cause allergic reactions in textiles, difficult to recover, pollute the environment during combustion, and their optical resistance, weather resistance and elongation at break are poor. , affects service life.

Method used

Using a wire extraction manufacturing method, the elastic fiber raw materials and yarn wrap raw materials are processed by multiple extensions of the guide wire, including the use of thermoplastic polyurethane fibers, through multiple guide wire and winding steps to improve the wire density and elongation of break, and Reduce environmental impact using highly recyclable materials.

Benefits of technology

Improves the wire density and elongation of break for elastic fibers and yarns, extends service life, and reduces environmental pollution through highly recyclable materials, simplifies the manufacturing process and reduces costs.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119082971A_ABST
    Figure CN119082971A_ABST
Patent Text Reader

Abstract

The invention relates to an elastic fiber, an elastic fiber covering yarn and a laddering manufacturing method of the elastic fiber covering yarn. The laddering manufacturing method of the elastic fiber comprises the following steps that an elastic fiber raw material is provided, the elastic fiber raw material is provided with a core part and a sheath part, and the sheath part wraps the core part; enabling the elastic fiber raw material to pass through a first godet roller to carry out first extension godet, wherein the speed of the first godet roller is 500-1500m / min; the elastic fiber raw material passes through a second silk guide roller to be subjected to second-time extending silk guide, and the speed of the second silk guide roller ranges from 1200 m / min to 2400 m / min; and enabling the elastic fiber raw material to pass through a third godet roller to carry out third extension godet, wherein the speed of the third godet roller is 1300-2600m / min.
Need to check novelty before this filing date? Find Prior Art

Description

[0001] The present invention is a divisional application with application number 202111153733.5, application date September 29, 2021, and invention name “Elastic fiber, elastic fiber covered yarn and spinning method thereof”. Technical Field

[0002] The invention relates to an elastic fiber, an elastic fiber covered yarn and a spinning method thereof. Background Art

[0003] In the production process of conventional elastic fibers, many reagents are toxic and irritating, especially toluene diisocyanate and bisphenol methylene-4,4-diisocyanate. The reagents remaining in the elastic fiber textile can cause allergic reactions; conventional elastic fibers are difficult to recycle, and they are prone to produce hydrocyanic acid when burned, which pollutes the environment. Furthermore, conventional elastic fibers have poor rotation and light resistance, weather resistance, elongation at break, and deformation rate after stretching, which also affects their service life.

[0004] Therefore, it is necessary to provide an innovative and progressive elastic fiber, elastic fiber covered yarn and its spinning method to solve the above-mentioned conventional deficiencies. Summary of the invention

[0005] The present invention relates to a method for producing elastic fibers. In one embodiment, the method comprises the following steps: providing an elastic fiber raw material, the elastic fiber raw material having a core and a sheath, the sheath covering the core; allowing the elastic fiber raw material to pass through a first wire guide roller for a first stretching and wire drawing, the speed of the first wire guide roller being 500-1500 m / min; allowing the elastic fiber raw material to pass through a second wire guide roller for a second stretching and wire drawing, the speed of the second wire guide roller being 1200-2400 m / min; and allowing the elastic fiber raw material to pass through a third wire guide roller for a third stretching and wire drawing, the speed of the third wire guide roller being 1300-2600 m / min.

[0006] The present invention relates to an elastic fiber, which is manufactured by the spinning method as described above. In one embodiment, the elastic fiber comprises: a core and a sheath. The sheath covers the core. The elastic fiber has a linear density of 50-300 deniers and a breaking elongation of 200-400%.

[0007] The present invention relates to a method for producing elastic fiber covered yarn. In one embodiment, the method comprises the following steps: providing an elastic fiber covered yarn raw material, the elastic fiber covered yarn raw material having an elastic fiber and a plurality of peripheral fibers, the plurality of peripheral fibers surrounding the elastic fiber; allowing the elastic fiber covered yarn raw material to pass through a first wire guide roller for a first extension wire guide, the speed of the first wire guide roller being 2000-4500 m / min; and allowing the elastic fiber covered yarn raw material to pass through a second wire guide roller for a second extension wire guide, the speed of the second wire guide roller being 2500-4500 m / min.

[0008] The present invention relates to an elastic fiber covered yarn, which is manufactured by the spinning manufacturing method as described above. In one embodiment, the elastic fiber covered yarn comprises: an elastic fiber; and a plurality of peripheral fibers. The plurality of peripheral fibers surround the elastic fiber. The elastic fiber covered yarn has a linear density of 50-300 deniers and a breaking elongation of 20-150%. BRIEF DESCRIPTION OF THE DRAWINGS

[0009] Figure 1 A schematic diagram showing the flow of a spinning method for producing elastic fibers according to an embodiment of the present invention.

[0010] Figure 2 A schematic diagram showing the flow of a spinning method for producing elastic fiber covered yarn according to an embodiment of the present invention.

[0011] Description of reference numerals:

[0012] S11~S14: Steps

[0013] S21~S23: Steps DETAILED DESCRIPTION

[0014] Figure 1 A schematic diagram showing the process flow of a spinning method for producing elastic fibers according to an embodiment of the present invention. Figure 1 First, referring to step S11, an elastic fiber raw material is provided, wherein the elastic fiber raw material has a core and a sheath, wherein the sheath covers the core. The radius ratio of the core to the sheath is 1:9 to 9:1. In one embodiment, the spinning temperature of the elastic fiber raw material may be 160-240°C. In one embodiment, the spinning temperature of the elastic fiber raw material may be 180-220°C.

[0015] Referring to step S12, the elastic fiber raw material is passed through a first wire guide roller for the first extension wire guide, and the speed of the first wire guide roller is 500-1500 m / min. In one embodiment, the first wire guide roller may have two symmetrical rollers, and the elastic fiber raw material passes between the two symmetrical rollers to extend the wire guide. In one embodiment, the speed of the first wire guide roller is 550-1300 m / min. In one embodiment, the temperature of the first wire guide roller is 10-75°C. In one embodiment, the temperature of the first wire guide roller is 15-60°C.

[0016] Referring to step S13, the elastic fiber raw material is passed through a second wire guide roller for a second extension wire guide, and the speed of the second wire guide roller is 1200-2400 m / min. In one embodiment, the second wire guide roller may have two symmetrical rollers, and the elastic fiber raw material passes between the two symmetrical rollers for extension wire guide. In one embodiment, the speed of the second wire guide roller is 1300-2000 m / min. In one embodiment, the temperature of the second wire guide roller is 10-75°C. In one embodiment, the temperature of the second wire guide roller is 15-60°C. In one embodiment, the speed of the second wire guide roller may be higher than the speed of the first wire guide roller.

[0017] Referring to step S14, the elastic fiber raw material is passed through a third wire guide roller for a third extension wire drawing, and the speed of the third wire guide roller is 1300-2600 m / min. In one embodiment, the third wire guide roller may have two symmetrical rollers, and the elastic fiber raw material passes between the two symmetrical rollers for extension wire drawing. In one embodiment, the speed of the third wire guide roller is 1350-2500 m / min. In one embodiment, the temperature of the third wire guide roller is 10-75°C. In one embodiment, the temperature of the third wire guide roller is 15-60°C. In one embodiment, the speed of the third wire guide roller may be higher than the speed of the second wire guide roller. In one embodiment, the above speed is the circumferential velocity of the wire guide roller.

[0018] In one embodiment, after the third wire drawing step, a winding step is further included, wherein the elastic fiber material is wound by a winding roller, and the speed of the winding roller is 1250-2250 m / min. In one embodiment, the speed of the winding roller is 1450-2150 m / min. In one embodiment, the speed of the winding roller may be less than the speed of the third wire drawing roller.

[0019] The present invention provides an elastic fiber, which is manufactured by the spinning manufacturing method as described above. In one embodiment, the elastic fiber includes: a core and a sheath. The sheath covers the core. The linear density of the elastic fiber is 50-300 deniers, and the elongation at break is 200-400%. In one embodiment, the elongation at break is 250%-350%. In one embodiment, the material of the core can be thermoplastic polyurethane. In one embodiment, the material of the sheath can be thermoplastic polyurethane fiber, polyester fiber or nylon fiber, but is not limited to the above.

[0020] In one embodiment, the elastic fiber has a deformation rate of 0-30% after being stretched by 30-250%. Therefore, the deformation rate of the elastic fiber of the present invention after being stretched is quite small, which can increase the service life. In one embodiment, the hardness of the elastic fiber is from 80A to 80D on the Shore A scale. In one embodiment, the hardness of the elastic fiber is from 80A to 75D on the Shore A scale. In one embodiment, the hardness of the elastic fiber is from 80A to 70D on the Shore A scale.

[0021] Therefore, by using the spinning method for producing elastic fibers of the present invention, the deformation rate of the elastic fibers of the present invention after stretching is quite small, which can increase the service life. In addition, due to the high recyclability of thermoplastic polyurethane, the elastic fibers of the present invention can be recycled and granulated after use, which has environmental benefits. Moreover, the recycled thermoplastic polyurethane particles obtained by recycling and granulation can be added to the manufacturing process of the elastic fibers of the present invention to further enhance the environmental benefits and save manufacturing costs. Furthermore, the spinning method for producing elastic fibers of the present invention is simple, and the cost of the raw materials of the thermoplastic polyurethane elastic fibers is lower than that of the conventional lycra elastic fibers.

[0022] Figure 2 A schematic diagram showing the process flow of a spinning method for producing elastic fiber covered yarn according to another embodiment of the present invention. Figure 2 First, referring to step S21, an elastic fiber wrapped yarn material is provided, wherein the elastic fiber wrapped yarn material has an elastic fiber and a plurality of peripheral fibers, wherein the plurality of peripheral fibers surround the elastic fiber. In one embodiment, the elastic fiber may be the elastic fiber mentioned above, which will not be described here. In one embodiment, the plurality of peripheral fibers contact the elastic fiber together through a plurality of spray points, and the elasticity of each peripheral fiber may be lower than that of the elastic fiber.

[0023] In one embodiment, the conventional materials of the several peripheral fibers include: polyethylene terephthalate, polybutylene terephthalate, nylon 6 or nylon 66, but are not limited to the above. The materials of the several peripheral fibers also include recycled materials. The mixed weight ratio of the conventional materials and recycled materials of the several peripheral fibers ranges from 55%:45% to 100%:0%. In one embodiment, the mixed weight ratio of the conventional materials and recycled materials of the several peripheral fibers ranges from 60%:40% to 90%:10%. In one embodiment, the mixed weight ratio of the conventional materials and recycled materials of the several peripheral fibers ranges from 70%:30% to 85%:15%. In one embodiment, due to the high recyclability of thermoplastic polyurethane, the elastic fiber of the present invention can be recycled and granulated into recycled materials after use, and the recycling granulation temperature is 240-320°C. In one embodiment, the recycling granulation temperature is 280-300°C.

[0024] In one embodiment, the plurality of peripheral fibers surround the elastic fiber in a manner including: single covered yarn (SCY), double covered yarn (DCY), air-jet covered yarn (ACY) or air textured yarn (ATY), but not limited to the above.

[0025] In one embodiment, the drawing temperature of the elastic fiber covered yarn raw material is 240-320° C. In one embodiment, the drawing temperature of the elastic fiber covered yarn raw material is 280-300° C.

[0026] Referring to step S22, the elastic fiber yarn raw material is passed through a first wire guide roller for the first extension wire guide, and the speed of the first wire guide roller is 2000-4500 m / min. In one embodiment, the first wire guide roller may have two symmetrical rollers, and the elastic fiber yarn raw material passes between the two symmetrical rollers for extension wire guide. In one embodiment, the speed of the first wire guide roller is 2500-4500 m / min. In one embodiment, the temperature of the first wire guide roller is 10-75°C. In one embodiment, the temperature of the first wire guide roller is 15-60°C.

[0027] Referring to step S23, the elastic fiber yarn raw material is passed through a second wire guide roller for a second extension wire guide, and the speed of the second wire guide roller is 2500-4500 m / min. In one embodiment, the second wire guide roller may have two symmetrical rollers, and the elastic fiber raw material passes between the two symmetrical rollers for extension wire guide. In one embodiment, the speed of the second wire guide roller is 3000-4000 m / min. In one embodiment, the temperature of the second wire guide roller is 10-75°C. In one embodiment, the temperature of the second wire guide roller is 15-60°C. In one embodiment, the speed of the second wire guide roller may be higher than the speed of the first wire guide roller.

[0028] In one embodiment, after the second drawing and guiding step, a winding step is further included, wherein the elastic fiber material is wound by a winding roller, and the speed of the winding roller is 2500-5000 m / min. In one embodiment, the speed of the winding roller is 3000-5000 m / min. In one embodiment, the speed of the winding roller may be higher than the speed of the second guiding roller.

[0029] The present invention provides an elastic fiber covered yarn, which is manufactured by the above-mentioned spinning manufacturing method. In one embodiment, the elastic fiber covered yarn includes: an elastic fiber and a plurality of peripheral fibers. The plurality of peripheral fibers surround the elastic fiber. The elastic fiber covered yarn has a linear density of 50-300 deniers and a breaking elongation of 20-150%. In one embodiment, the breaking elongation is 30%-120%.

[0030] Therefore, by using the spinning method for producing the elastic fiber covered yarn of the present invention, the elastic fiber covered yarn of the present invention has a very excellent elongation at break. In addition, due to the high recyclability of the thermoplastic polyurethane, the elastic fiber of the present invention can be recycled and granulated after use, which has environmental benefits. Moreover, the recycled thermoplastic polyurethane particles obtained by recycling and granulation can be added to the manufacturing process of the elastic fiber covered yarn of the present invention to further enhance the environmental benefits and save manufacturing costs. Furthermore, the spinning method for producing the elastic fiber covered yarn of the present invention is simple, and the cost of the thermoplastic polyurethane elastic fiber raw material is lower than that of the conventional lycra elastic fiber.

[0031] [Invention Example 1]

[0032] A thermoplastic polyurethane elastic fiber raw material is used, wherein the material of the core part is thermoplastic polyurethane, and the material of the sheath part is thermoplastic polyurethane. The spinning temperature of the thermoplastic polyurethane elastic fiber raw material is 190°C.

[0033] The stretching and threading steps of the thermoplastic polyurethane elastic fiber are as follows: the elastic fiber raw material is stretched and threaded for the first time through the first thread guide roller, the speed of the first thread guide roller is 550 m / min, and the temperature of the first thread guide roller is 60° C.; the elastic fiber raw material is stretched and threaded for the second time through the second thread guide roller, the speed of the second thread guide roller is 1200 m / min, and the temperature of the second thread guide roller is 55° C.; the elastic fiber raw material is stretched and threaded for the third time through the third thread guide roller, the speed of the third thread guide roller is 1650 m / min, and the temperature of the third thread guide roller is 55° C. The thermoplastic polyurethane elastic fiber is wound at a speed of 1550 m / min.

[0034] According to the test, the linear density of the thermoplastic polyurethane elastic fiber is 50-300 deniers, the elongation at break is 200-400%, the deformation rate of the thermoplastic polyurethane elastic fiber is 0-30% after being stretched 30-250%, and the hardness of the thermoplastic polyurethane elastic fiber is 95A according to DIN ISO 7619-1.

[0035] [Invention Example 2]

[0036] The thermoplastic polyurethane elastic fiber is recycled and granulated to make thermoplastic polyurethane recycled granules, which are added to the conventional material of the several peripheral fibers. The spinning temperature of the elastic fiber yarn raw material is 240°C.

[0037] The stretching and guiding steps of the thermoplastic polyurethane elastic fiber yarn are as follows: the elastic fiber yarn raw material is passed through the first wire guide roller for the first stretching and guiding, the speed of the first wire guide roller is 2600 m / min, and the temperature of the first wire guide roller is 50° C.; the elastic fiber yarn raw material is passed through the second wire guide roller for the second stretching and guiding, the speed of the second wire guide roller is 3500 m / min, and the temperature of the second wire guide roller is 50° C. The thermoplastic polyurethane elastic fiber is wound at a speed of 3000 m / min.

[0038] According to tests, the linear density of the thermoplastic polyurethane elastic fiber wrapped yarn is 50-300 deniers, and the elongation at break is 20-150%.

[0039] The above embodiments are only for explaining the principle and efficacy of the present invention, but not for limiting the present invention. The modifications and changes made by those skilled in the art to the above embodiments still do not violate the spirit of the present invention. The scope of rights of the present invention shall be as listed in the claims.

Claims

1. A method for producing elastic fiber covered yarn by spinning, comprising the following steps: Providing an elastic fiber covered yarn material, the elastic fiber covered yarn material having an elastic fiber and a plurality of peripheral fibers, wherein the plurality of peripheral fibers surround the elastic fiber; Passing the elastic fiber covered yarn raw material through a first guide roller for first stretching and guiding, wherein the speed of the first guide roller is 2000-4500 m / min; and The elastic fiber covered yarn material is passed through a second guide roller for second stretching and guide-threading, and the speed of the second guide roller is 2500-4500 m / min.

2. The spinning method for producing elastic fiber covered yarn as described in claim 1, wherein the speed of the first guide wire roll is 2500-4000 m / min, and the speed of the second guide wire roll is 3000-4000 m / min.

3. The spinning method for producing elastic fiber covered yarn according to claim 1 further comprises a winding step, wherein the elastic fiber covered yarn is wound by a winding roller, and the speed of the winding roller is 2500-5000 m / min.

4. The spinning method for producing elastic fiber covered yarn as claimed in claim 3, wherein the speed of the winding roller is 3000-5000 m / min.

5. The method for producing elastic fiber covered yarn by spinning as claimed in claim 1, wherein the spinning temperature of the elastic fiber covered yarn raw material is 240-320°C.

6. The method for producing elastic fiber covered yarn by spinning as claimed in claim 5, wherein the spinning temperature of the elastic fiber covered yarn raw material is 280-300°C.

7. The method for producing elastic fiber covered yarn by spinning as claimed in claim 1, wherein the temperature of the first guide roller is 10-75°C, and the temperature of the second guide roller is 10-75°C.

8. The method for producing elastic fiber covered yarn according to claim 7, wherein the temperature of the first guide roller is 15-60°C, and the temperature of the second guide roller is 15-60°C.

9. The method for producing elastic fiber covered yarn according to claim 1, wherein the conventional materials of the plurality of peripheral fibers include: Polyethylene terephthalate, polybutylene terephthalate, nylon 6 or nylon 66.

10. The method for producing elastic fiber covered yarn according to claim 9, wherein the material of the plurality of peripheral fibers further comprises recycled material.

11. The method for producing elastic fiber covered yarn according to claim 10, wherein the weight ratio of the conventional material to the recycled material of the plurality of peripheral fibers ranges from 55%:45% to 100%:0%.

12. The method for producing elastic fiber covered yarn according to claim 1, wherein the plurality of peripheral fibers surround the elastic fiber in a manner comprising: Single covered yarn, double covered yarn, air covered yarn or air textured covered yarn.

13. An elastic fiber covered yarn produced by the spinning method according to claim 1, comprising: - elastic fiber; and several peripheral fibers surrounding the elastic fibers; The elastic fiber covered yarn has a linear density of 50-300 deniers and an elongation at break of 20-150%.

14. The elastic fiber covered yarn according to claim 13, wherein the elongation at break is 30% to 120%.

Citation Information

Patent Citations

  • Preparing method of thermoplastic polyurethane monofilaments

    CN109853071A

  • Method for producing polyacetal fiber

    CN110869547A

  • Method for manufacturing thermoplastic polyurethane fibers

    CN111575817A

  • Core-sheath type composite elastic fiber, elastic multifilament fiber and elastic fabric

    CN212357468U

  • Process for the production of Elastic Core-Spun Yarns

    GB1157704A