Lithium ion battery pack early internal short circuit diagnosis method and system based on dynamic time warping of incremental capacity

Through dynamic time regulation method based on incremental capacity, detecting the micro-short-circuit monomer of the lithium-ion battery pack and estimating its short-circuit resistance, the problem of low accuracy and efficiency of micro-short-circuit fault diagnosis in the prior art is solved, and more efficient diagnosis and More accurate short-circuit resistance evaluation.

CN119087269APending Publication Date: 2024-12-06ELECTRIC POWER RES INST STATE GRID SHANXI ELECTRIC POWER

Patent Information

Application Number
CN202411284551.5
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-13
Publication Date
2024-12-06

AI Technical Summary

Technical Problem

The existing micro-short circuit fault diagnosis methods for lithium-ion battery packs have the problem that qualitative detection cannot quantitatively describe the severity of short circuits and the quantitative diagnostic accuracy are affected by the accuracy of the equivalent circuit model, and the calculation efficiency is low, making it difficult to effectively deploy in actual BMS.

Method used

Using a dynamic time regulation method based on incremental capacity, the median IC curve is obtained by sorting the terminal voltage, the DTW distance between each monomer and the median IC curve is calculated, the micro-short-circuit monomer is detected, and the maximum charging voltage variation is estimated. Its short-circuit current and short-circuit resistance avoid the need to build a battery model.

Benefits of technology

It improves the accuracy and computing efficiency of micro-short circuit fault diagnosis, reduces the computational burden of BMS, avoids dependence on high-quality model parameters, and simplifies the deployment of diagnostic models.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119087269A_ABST
    Figure CN119087269A_ABST
Patent Text Reader

Abstract

The invention discloses a lithium ion battery pack early-stage internal short circuit diagnosis method and system based on dynamic time warping of incremental capacity, and the method comprises the following steps: sorting the terminal voltages of all monomers in a lithium ion battery pack in an ascending order to obtain a median terminal voltage, and obtaining a median IC curve based on the median terminal voltage; obtaining a DTW distance between the IC curve of each monomer and the median IC curve, and detecting a micro-short-circuit monomer based on the DTW distance; and estimating the short-circuit current and the short-circuit resistance of the micro-short-circuit cell based on the change of the maximum charging voltage MCV. According to the invention, micro-short circuit detection and quantitative evaluation of the energy storage lithium ion battery pack are realized without establishing a battery model.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to early internal short circuit fault diagnosis of energy storage lithium ion battery packs, belongs to the field of lithium ion battery fault diagnosis, and specifically relates to an early internal short circuit fault diagnosis method and system for lithium ion battery packs based on dynamic time regularization of incremental capacity. Background Art

[0002] Lithium-ion batteries have the advantages of high power density, low self-discharge rate and long cycle life, and have been widely used in electric vehicles and grid energy storage. However, due to its poor tolerance to abuse, external environment and operating conditions, lithium-ion battery systems may experience various faults, leading to accelerated battery degradation and even safety accidents characterized by thermal runaway, which has aroused public concerns about the safety of lithium-ion batteries. In the past few years, battery pack thermal runaway accident analysis reports from different research institutions have shown that internal short circuit is one of the main causes of thermal runaway in lithium-ion batteries. Internal short circuits usually have a long evolution and development process before deteriorating into thermal runaway. In the early internal short circuit (i.e., micro short circuit), the equivalent short circuit resistance is large, and the changes in the battery's electrothermal parameters caused by the short circuit are not obvious, which is highly concealed. This also makes it difficult to detect early micro short circuit faults. Therefore, timely diagnosis of early micro short circuit faults is a crucial and challenging task to ensure the safe and stable operation of lithium-ion batteries.

[0003] Existing diagnostic methods for micro short circuits in battery packs can be divided into two categories based on diagnostic effects: qualitative detection and quantitative diagnosis. Qualitative detection methods cannot quantitatively calculate short-circuit current and short-circuit resistance, that is, they cannot give a quantitative description of the severity of the short circuit. Existing quantitative diagnostic methods have the following limitations: (1) Existing methods require the establishment of an equivalent circuit model for each battery cell in the battery pack. The equivalent circuit model of lithium-ion batteries is difficult to reflect the internal reaction mechanism of the battery, and its accuracy is greatly affected by the model parameters, so that the accuracy of the diagnostic results is limited by the accuracy of the model itself and is easily interfered by the model parameters. (2) Existing methods need to calculate the short-circuit current and short-circuit resistance of each cell in the battery pack one by one. This method of indiscriminately calculating short-circuit resistance lacks specificity. For battery packs consisting of hundreds or thousands of cells, it will increase the computational burden of the battery management system (BMS). Therefore, how to improve the accuracy and computational efficiency of micro short circuit fault diagnosis in battery packs is an urgent problem to be solved. Summary of the invention

[0004] In view of the shortcomings of the prior art, the present invention proposes a method and system for early internal short circuit diagnosis of lithium-ion battery packs based on dynamic time warping of incremental capacity, which can realize micro-short circuit detection and quantitative evaluation of energy storage lithium-ion battery packs without establishing a battery model.

[0005] To achieve the above object, the present invention provides the following solutions:

[0006] A method for early internal short circuit diagnosis of a lithium-ion battery pack based on dynamic time warping of incremental capacity comprises the following steps:

[0007] Arrange the terminal voltages of all cells in the lithium-ion battery pack in ascending order to obtain a median terminal voltage, and obtain a median IC curve based on the median terminal voltage;

[0008] Obtaining a DTW distance between the IC curve of each monomer and the median IC curve, and detecting a micro-short-circuit monomer based on the DTW distance;

[0009] The short-circuit current and the short-circuit resistance of the micro-short-circuit cell are estimated based on the change of the maximum charging voltage MCV.

[0010] Preferably, the median IC curve and the IC curve of each monomer are obtained by numerical differentiation method, specifically:

[0011]

[0012] Among them, IC EVI represents the extracted incremental capacity value, Q represents the battery charging capacity, V is the terminal voltage under constant current charging mode, Q2 and Q1 represent the battery charging capacity at two different times with a voltage interval of ΔV, and Q2-Q1 represents the change in charging capacity within the voltage interval ΔV.

[0013] Preferably, the method for obtaining the DTW distance between the IC curve of each monomer and the median IC curve comprises:

[0014] The median IC curve and the IC curve of a certain monomer are represented as C med and C;

[0015] According to C med Construct the distance matrix A by using the Euclidean distance between any two points in C;

[0016] Based on the distance matrix A, the DTW distance D(C med ,C);

[0017] Among them, C med =[c med (1),c med (2),...,c med(M)], C=[c(1),c(2),...,c(N)];

[0018] Among them, c med (M) represents the Mth value of the median IC curve, c(N) represents the Nth value of the monomer IC curve, and M and N represent the lengths of the median IC curve and the monomer IC curve, respectively;

[0019]

[0020] Among them, d ij Represents the i-th sample point c in the median IC curve med (i) The Euclidean distance from the jth sample point c(j) in the IC curve of the monomer is calculated as: d ij =||c med (i)-c(j)||2,1≤i≤M,1≤j≤N;

[0021] Based on the distance matrix A, the DTW distance D(C med ,C) methods include:

[0022] Find an optimal regular path W in the distance matrix A best , so that C med The cumulative distance value from C is minimized, and the optimal regular path W bes for:

[0023]

[0024] Where K represents the total number of regular paths, and k represents the regular path number;

[0025] DTW distance D(C med ,C) is:

[0026]

[0027] Among them, W k Represents the position of the regularized path W in the distance matrix A, A(i,j) k It means that the starting point of the kth regular path is located in the i-th row and j-th column of matrix A.

[0028] Preferably, the method for obtaining the short-circuit current and short-circuit resistance of the micro-short-circuit monomer includes:

[0029]

[0030] Among them, I MSC is the micro short-circuit current, Q loss,p is the estimated power loss at the end of the pth charging of the micro-short-circuit monomer, Q loss,p-1is the estimated power loss at the end of the p-1th charging of the micro-short-circuit monomer, T p is the time when the pth charging ends, T p-1 is the time when the p-1th charging ends;

[0031]

[0032] Among them, R MSC Indicates micro short circuit resistance, U M It is the average voltage between the end times of two adjacent cycle charging.

[0033] The present invention also provides a lithium-ion battery pack early internal short circuit diagnosis system based on dynamic time regulation of incremental capacity, comprising: an IC curve calculation module, a short-circuit monomer detection module and a current resistance estimation module;

[0034] The IC curve calculation module is used to sort the terminal voltages of all cells in the lithium-ion battery pack in ascending order to obtain a median terminal voltage, and obtain a median IC curve based on the median terminal voltage;

[0035] The short-circuit monomer detection module is used to obtain the DTW distance between the IC curve of each monomer and the median IC curve, and detect a micro-short-circuit monomer based on the DTW distance;

[0036] The current resistance estimation module is used to estimate the short-circuit current and short-circuit resistance of the micro-short-circuit monomer based on the change of the maximum charging voltage MCV.

[0037] Preferably, the median IC curve and the IC curve of each monomer are obtained by numerical differentiation method, specifically:

[0038]

[0039] Among them, IC EVI represents the extracted incremental capacity value, Q represents the battery charging capacity, V is the terminal voltage under constant current charging mode, Q2 and Q1 represent the battery charging capacity at two different times with a voltage interval of ΔV, and Q2-Q1 represents the change in charging capacity within the voltage interval ΔV.

[0040] Preferably, the short-circuit monomer detection module includes: a preset unit, a matrix construction unit and a distance calculation unit;

[0041] The preset unit is used to represent the median IC curve and the IC curve of a certain monomer as C med and C;

[0042] The matrix construction unit is used to med Construct the distance matrix A by using the Euclidean distance between any two points in C;

[0043] The distance calculation unit is used to obtain the DTW distance D(C) based on the distance matrix A. med ,C);

[0044] Among them, C med =[c med (1),c med (2),...,c med (M)], C=[c(1),c(2),...,c(N)];

[0045] Among them, c med (M) represents the Mth value of the median IC curve, c(N) represents the Nth value of the monomer IC curve, and M and N represent the lengths of the median IC curve and the monomer IC curve, respectively;

[0046]

[0047] Among them, d ij Represents the i-th sample point c in the median IC curve med (i) The Euclidean distance from the jth sample point c(j) in the IC curve of the monomer is calculated as: d ij =||c med (i)-c(j)||2,1≤i≤M,1≤j≤N;

[0048] Based on the distance matrix A, the DTW distance D(C med ,C) methods include:

[0049] Find an optimal regular path W in the distance matrix A best , so that C med The cumulative distance value from C is minimized, and the optimal regular path W bes for:

[0050]

[0051] Where K represents the total number of regular paths, and k represents the regular path number;

[0052] DTW distance D(C med ,C) is:

[0053]

[0054] Among them, W k Represents the position of the regularized path W in the distance matrix A, A(i,j) k It means that the starting point of the kth regular path is located in the i-th row and j-th column of matrix A.

[0055] Preferably, the process of obtaining the short-circuit current and short-circuit resistance of the micro-short-circuit monomer includes:

[0056]

[0057] Among them, I MSC is the micro short-circuit current, Q loss,p is the estimated power loss at the end of the pth charging of the micro-short-circuit monomer, Q loss,p-1 is the estimated power loss at the end of the p-1th charging of the micro-short-circuit monomer, T p is the time when the pth charging ends, T p-1 is the time when the p-1th charging ends;

[0058]

[0059] Among them, R MSC Indicates micro short circuit resistance, U M It is the average voltage between the end times of two adjacent charging cycles.

[0060] Compared with the prior art, the present invention has the following beneficial effects:

[0061] (1) As mentioned above, the existing micro-short circuit diagnosis method requires the establishment of an equivalent circuit model of a lithium-ion battery. However, the equivalent circuit model of a lithium-ion battery is difficult to reflect the internal reaction mechanism of the battery, and its accuracy is greatly affected by the model parameters, so that the accuracy of the diagnosis result is limited by the accuracy of the model itself and is easily interfered by the model parameters. In contrast, the method of the present invention does not need to establish a battery model in the process of detecting micro-short circuit cells in the battery pack and calculating their short-circuit resistance, thereby avoiding the difficulty of establishing an accurate battery model and improving the diagnosis accuracy. (2) The existing quantitative diagnosis method needs to calculate the short-circuit resistance of all cells in the battery, and judge which cells have micro-short circuits based on the calculation results. This method lacks pertinence and has a large number of unnecessary calculations. In contrast, the method proposed in the present invention adopts a technical route of first detection and then quantitative evaluation, which makes the short-circuit resistance estimation process more pertinent, can avoid a large number of unnecessary calculations, improve the diagnosis efficiency, and reduce the calculation burden of the BMS. (3) The method proposed in the present invention does not require pre-offline training of the diagnosis model during the fault diagnosis process, thereby avoiding the use of a large amount of training data and not relying on high-quality training data, which is conducive to the deployment and promotion of the diagnosis method in actual BMS. BRIEF DESCRIPTION OF THE DRAWINGS

[0062] In order to more clearly illustrate the technical solution of the present invention, the following briefly introduces the drawings required for use in the embodiments. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative labor.

[0063] Figure 1 A schematic flow chart of a method for diagnosing early internal short circuits of a lithium-ion battery pack based on dynamic time warping of incremental capacity according to an embodiment of the present invention;

[0064] Figure 2 It is a schematic diagram of the principle of estimating micro short-circuit resistance based on the maximum charging voltage change according to an embodiment of the present invention;

[0065] Figure 3 Schematic diagram of the DTW distance of each monomer when no micro short circuit occurs in cycle 1 according to an embodiment of the present invention;

[0066] Figure 4 Schematic diagram of the DTW distance of each monomer when no micro short circuit occurs in cycle 2 according to an embodiment of the present invention;

[0067] Figure 5 Schematic diagram of the DTW distance of each monomer when the short-circuit resistance is 300Ω in cycle 3 according to an embodiment of the present invention;

[0068] Figure 6 Schematic diagram of the DTW distance of each monomer when the short-circuit resistance is 200Ω in cycle 5 according to an embodiment of the present invention;

[0069] Figure 7 Schematic diagram of the DTW distance of each monomer when the short-circuit resistance is 100Ω in cycle 7 according to an embodiment of the present invention;

[0070] Figure 8 Schematic diagram of the DTW distance of each monomer when the short-circuit resistance is 50Ω in cycle 9 according to an embodiment of the present invention;

[0071] Fig. 9 Schematic diagram of the DTW distance of each monomer when the short-circuit resistance is 10Ω in cycle 11 of the embodiment of the present invention;

[0072] Fig.10 Schematic diagram of the DTW distance of each monomer when the short-circuit resistance is 5Ω in cycle 13 according to an embodiment of the present invention. DETAILED DESCRIPTION

[0073] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0074] In order to make the above-mentioned objects, features and advantages of the present invention more obvious and easy to understand, the present invention is further described in detail below with reference to the accompanying drawings and specific embodiments.

[0075] Embodiment 1

[0076] The present invention proposes a method for early internal short circuit diagnosis of lithium-ion battery packs based on dynamic time warping of incremental capacity. The overall framework of the proposed diagnostic method is as follows Figure 1 As shown. Figure 1 As shown in the figure, the proposed method includes three main steps: First, the terminal voltages of all cells in the battery pack are sorted in ascending order to obtain the median terminal voltage, based on which the median IC curve is further obtained, which is used as a reference standard to represent the state of normal cells in the battery pack. Then, the DTW distance between the IC curve of each cell and the median IC curve is obtained, and the cells with a distance index greater than the threshold are diagnosed as micro-short-circuited cells. Finally, for the detected micro-short-circuited cells, their short-circuit current and short-circuit resistance are estimated based on the change of the maximum charging voltage (MCV).

[0077] It can be seen that the method of the present invention does not need to establish a battery model in the process of detecting micro-short-circuited cells in the battery pack and calculating their short-circuit resistance, thus avoiding the difficulty of establishing an accurate battery model. In addition, the method proposed in the present invention adopts a technical route of first detecting and then quantitatively evaluating, which makes the short-circuit resistance estimation process more targeted, can avoid a large number of unnecessary calculations, and improve diagnostic efficiency. The following is a detailed description of the extraction of IC curves, micro-short circuit detection based on DTW, and short-circuit resistance estimation based on maximum charging voltage changes. :

[0078] In this embodiment, if Figure 1 As shown, after obtaining the median terminal voltage between the cells in the lithium-ion battery pack, it is necessary to extract the median IC curve therefrom. In addition, it is necessary to calculate the IC curve of each cell based on the terminal voltage of each cell. The present invention uses numerical differentiation method to obtain the IC curve, and the calculation formula is as follows:

[0079]

[0080] Among them, IC EVIrepresents the extracted incremental capacity value, Q represents the battery charging capacity, and V is the terminal voltage in constant current charging mode. Formula (1) represents the calculation of IC based on equal voltage interval ΔV, Q2 and Q1 represent the charging capacity of the battery at two different times with a voltage interval of ΔV, and Q2-Q1 represents the change in charging capacity within the voltage interval ΔV. The present invention calculates IC based on the equal voltage interval (EVI) method. In order to fully capture the characteristics of the IC curve, ΔV is set to 1mV.

[0081] The IC curve calculated based on the numerical differentiation method is easily affected by measurement noise. Therefore, it is necessary to use a suitable filter to obtain a smooth IC curve. The present invention uses a moving average filter to smooth the IC curve. The moving average filter smoothes the signal by calculating the average value of the signal in a preset window. Given a time-varying signal s contaminated by noise, the moving average filter can be designed as:

[0082]

[0083] Among them, s r represents the value of the original signal s at the rth moment, is the corresponding filtered value, 2N p +1 is the window size of the sliding filter and N p is an integer, l is the time lag number, s r-l is the value of the original signal at the rlth moment.

[0084] In this embodiment, it should be noted that the length of the median IC curve is not equal to the length of the IC curve of each monomer. Therefore, the present invention uses DTW to measure the similarity between the IC curve of each monomer and the median IC curve to detect the micro-short-circuited monomer in the battery pack. DTW is a data sequence similarity measurement method with high accuracy and strong robustness. It can match the data points of the data sequence by bending the time domain of the data sequence, which can not only obtain better morphological measurement effects, but also measure the similarity of two data sequences of unequal lengths.

[0085] The present invention expresses the median IC curve and the IC curve of a certain monomer as C med and C:

[0086] C med =[c med (1),c med (2),...,c med (M)] (3)

[0087] C=[c(1),c(2),...,c(N)] (4)

[0088] where c med (M) represents the Mth value of the median IC curve, c(N) represents the Nth value of the monomer IC curve, M and N represent the length of the median IC curve and the monomer IC curve respectively. The distance matrix A is constructed based on the Euclidean distance between any two points of the two curves as follows:

[0089]

[0090] where d ij Represents the i-th sample point c in the median IC curve med (i) The Euclidean distance from the jth sample point c(j) in the IC curve of the monomer is calculated as follows:

[0091] d ij =||c med (i)-c(j)||2,1≤i≤M,1≤j≤N (6)

[0092] At this time, the DTW distance D(C med ,C) can be defined as: Find an optimal regular path W in the distance matrix A best , so that C med The cumulative distance between and C is minimized. The optimal regularized path W best It can be defined by the following formula:

[0093]

[0094] Where K represents the total number of regular paths and k represents the regular path number. Therefore, the mathematical definition of DTW can be given as:

[0095]

[0096] In the above formula, W k Represents the position of the regularized path W in the distance matrix A, A(i,j) k It means that the starting point of the kth regular path is located at the i-th row and j-th column of the matrix A. In order to ensure the uniqueness of the solution of the DTW mathematical definition, three constraints are given to formula (8):

[0097] (1) Boundary property: optimal regular path W best The boundary points of are determined. That is, W1=(1,1), W k =(M,N).

[0098] (2) Monotonicity, ensuring W best The search direction. That is, for a given W k =(i,j) and W k+1 =(i * ,j *), there must be i * ≥i,j * ≥j. Here i* and j* indicate that the starting point of the next regular path in the search process is located in the i*th row and j*th column of matrix A.

[0099] (3) Continuity, W best The search can only be done on adjacent nodes. k =(i,j) and W k+1 =(i * ,j * ),

[0100] Must have * ≤i+1,j * ≤j+1.

[0101] Based on the three constraints given, the dynamic programming method can be used to solve formula (8). Here is the state transition equation of dynamic programming, which represents the iterative formula for calculating the DTW distance:

[0102] DTW(i,j)=d ij +min[DTW(i-1,j-1),DTW(i-1,j),DTW(i,j-1)] (9)

[0103] Based on the above process, the present invention can obtain the DTW distance between the IC curve of each monomer and the median IC curve. The monomer with a DTW distance less than the threshold is considered to be a normal monomer. On the contrary, the monomer with a DTW distance greater than the threshold is diagnosed as a micro-short-circuit monomer.

[0104] In this embodiment, after detecting a micro-short-circuited cell in the battery pack, the present invention further estimates its short-circuit current and short-circuit resistance to quantitatively evaluate the severity and evolution stage of the micro-short circuit, which helps the battery management system to take targeted countermeasures.

[0105] Observe the charging voltage curve of the micro-short-circuit monomer in two adjacent charge and discharge cycles separately, such as Figure 2 As shown. It can be seen from the figure that the maximum charging voltage (MCV 2) of the micro-short-circuit monomer in the next charge and discharge cycle (i.e., the second charge and discharge cycle, recorded as Cycle 2) is significantly lower than the maximum charging voltage (MCV 1) in the previous charge and discharge cycle (i.e., the first charge and discharge cycle, recorded as Cycle 1). This change in the maximum charging voltage is caused by the additional energy consumption of the micro-short-circuit monomer by the short-circuit resistance. Assume that at the end of the second charge of the battery pack, the micro-short-circuit monomer is removed from the battery pack and charged separately so that its maximum charging voltage is the same as the maximum charging voltage at the end of the first charging cycle, as shown in Figure 2As shown by the dotted line in , the present invention defines the charging time Δt required at this time as the remaining charging time of the micro-short-circuit monomer.

[0106] In the actual operation of the energy storage lithium-ion battery pack, it is impossible to take out the micro-short-circuit monomer separately and charge it to obtain the remaining charging time Δt. Therefore, the remaining charging time Δt is theoretically unknown. However, it can be noted that if the maximum charging voltage MCV 2 of the next cycle is interpolated on the charging voltage curve of the previous cycle, and the corresponding moment is recorded as t, then the time interval from the moment t to the end of charging in the previous cycle is equal to the remaining charging time Δt. Therefore, the remaining charging time Δt of the micro-short-circuit monomer in the current cycle can be obtained by interpolating the maximum charging voltage of the current cycle on the charging voltage curve of the previous cycle.

[0107] After obtaining the remaining charging time Δt of the micro-short-circuited monomer in the current charge and discharge cycle, the power loss of the micro-short-circuited monomer in the current charge and discharge cycle can be further obtained by multiplying it with the charging current of the battery pack. This power loss is caused by the short-circuit resistance, that is:

[0108] Q loss,p =I·Δt (10)

[0109] Where Q loss,p is the power loss of the micro-short-circuit monomer at the end of p times of charging, and I is the charging current. The rate of change of power loss over time is the short-circuit current of the micro-short-circuit monomer, so we have

[0110]

[0111] Among them, I MSC is the micro short-circuit current, Q loss,p is the estimated power loss at the end of the pth charging of the micro-short-circuit monomer, Q loss,p-1 is the estimated power loss at the end of the p-1th charge of the micro-short-circuit monomer, T p is the time when the pth charging ends, T p-1 is the time when the p-1th charge is completed. Based on the obtained micro short-circuit current, the micro short-circuit resistance can be further calculated by the following formula. The smaller the short-circuit resistance, the greater the heat generation power of the battery short circuit, and the greater the possibility of thermal runaway.

[0112]

[0113] Among them, R MSC Indicates micro short circuit resistance, U M It is the average voltage between the end times of two adjacent cycle charging.

[0114] In this embodiment, the present invention is tested on a battery pack consisting of 8 cylindrical lithium-ion battery cells connected in series to verify the effectiveness of the technology. The cell specification parameters are shown in Table 1.

[0115] Table 1 Specifications of lithium-ion batteries

[0116]

[0117] The battery pack was charged at a constant current of 0.5C. When the maximum cell terminal voltage reached the charge cut-off voltage of 4.2V, the battery pack stopped charging to prevent the cell from overcharging. Then the battery pack was discharged for dynamic stress test. When the minimum cell terminal voltage reached the discharge cut-off voltage of 2.75V, the battery pack stopped discharging to prevent the cell from over-discharging. A total of 14 charge and discharge cycles were performed on the battery pack.

[0118] The present invention simulates micro short circuit faults by connecting external resistors in parallel at both ends of the battery. This method can not only better control the triggering time and position of the micro short circuit, but also simulate the evolution process of the micro short circuit, and has good controllability and repeatability.

[0119] Specifically, in order to simulate the evolution of micro-short circuits, short-circuit resistors of different amplitudes and corresponding manual switches are connected in series and then connected in parallel to both ends of monomer 4 and monomer 8. By closing different switches, short-circuit resistors of different amplitudes can be connected in parallel to both ends of the battery to simulate the occurrence and evolution of micro-short circuits. The smaller the short-circuit resistance, the larger the short-circuit current, indicating that the short circuit is more serious. The parallel short-circuit resistors corresponding to each charge and discharge cycle are shown in Table 2.

[0120] Table 2 Short-circuit resistance corresponding to different charge and discharge cycles

[0121]

[0122]

[0123] Next, the DTW distance between the IC curve of each cell and the median IC curve is calculated, and compared with a predetermined threshold to detect micro-short-circuited cells. Specifically, for the battery pack used in the present invention, the fault detection threshold is set to 35. It should be noted that in actual use, the fault detection threshold can be flexibly adjusted according to the battery type, application scenario, etc. to improve the sensitivity of the fault detection algorithm. The DTW distance of each cell in the battery pack at different charge and discharge cycles is as follows: Figures 3 to 10 As shown, the dotted line represents the threshold. Figures 3 to 10It can be observed that in the first two cycles, the DTW distances of all monomers are lower than the threshold, which indicates that all monomers are in a normal state and no micro-short circuit occurs in the first two cycles. Starting from the third cycle, the DTW distances corresponding to monomers 4 and 8 exceed the threshold. On the contrary, the DTW distances of other monomers have been lower than the threshold, which indicates that from the third cycle, a micro-short circuit occurs in monomers 4 and 8, while other monomers are still in a normal state. In addition, it can be observed that as the short-circuit resistance decreases, the DTW distances of monomers 4 and 8 show an increasing trend, which indicates that as the micro-short circuit worsens, the DTW distance of the micro-short-circuited monomer will gradually increase. The above diagnostic results are consistent with the aforementioned fault injection situation, which shows that the proposed method can accurately detect micro-short-circuited monomers in the lithium-ion battery pack, proving the effectiveness of the proposed method. Observing the fault detection results obtained from the 4th, 6th, 8th, 10th, 12th and 14th charge and discharge cycles, the same conclusion can be drawn. For simplicity, the present invention will not be repeated.

[0124] After detecting the micro-short-circuited cells in the battery pack, the short-circuit resistance is further estimated using the method proposed above to quantify the severity and evolution stage of the micro-short circuit. The true value, estimated value and relative error of the short-circuit resistance of micro-short-circuited cells 4 and 8 are listed in Table 3. As shown in Table 3, for micro-short-circuited cells 4, the maximum relative error of the short-circuit resistance estimation result is 3.85%, and for micro-short-circuited cells 8, the maximum relative error of the short-circuit resistance estimation result is 4.26%. In addition, it can be found from Table 3 that as the actual short-circuit resistance connected in parallel at both ends of the battery decreases, the relative error of the estimation result shows a decreasing trend. This is because as the short-circuit resistance decreases, the short-circuit current gradually increases, and the fault characteristics caused by the micro-short circuit will become more and more obvious. The above short-circuit resistance estimation error is within an acceptable range, which proves the effectiveness of the micro-short circuit quantitative evaluation method proposed in the present invention.

[0125] Table 3 Micro short circuit resistance estimation results

[0126]

[0127] Embodiment 2

[0128] The present invention also provides a lithium-ion battery pack early internal short circuit diagnosis system based on dynamic time regulation of incremental capacity, comprising: an IC curve calculation module, a short-circuit monomer detection module and a current resistance estimation module;

[0129] The IC curve calculation module is used to sort the terminal voltages of all cells in the lithium-ion battery pack in ascending order to obtain a median terminal voltage, and obtain a median IC curve based on the median terminal voltage;

[0130] The short-circuit monomer detection module is used to obtain the DTW distance between the IC curve of each monomer and the median IC curve, and detect a micro-short-circuit monomer based on the DTW distance;

[0131] The current resistance estimation module is used to estimate the short-circuit current and short-circuit resistance of the micro short-circuit monomer based on the change of the maximum charging voltage MCV.

[0132] In this embodiment, the median IC curve and the IC curve of each monomer are obtained by numerical differentiation method, specifically:

[0133]

[0134] Among them, IC EVI represents the extracted incremental capacity value, Q represents the battery charging capacity, V is the terminal voltage under constant current charging mode, Q2 and Q1 represent the battery charging capacity at two different times with a voltage interval of ΔV, and Q2-Q1 represents the change in charging capacity within the voltage interval ΔV.

[0135] In this embodiment, the short-circuit monomer detection module includes: a preset unit, a matrix construction unit and a distance calculation unit;

[0136] The preset unit is used to represent the median IC curve and the IC curve of a monomer as C med and C;

[0137] The matrix construction unit is used to med Construct the distance matrix A by using the Euclidean distance between any two points in C;

[0138] The distance calculation unit is used to obtain the DTW distance D(C med ,C);

[0139] Among them, C med =[c med (1),c med (2),...,c med (M)], C=[c(1),c(2),...,c(N)];

[0140] Among them, c med (M) represents the Mth value of the median IC curve, c(N) represents the Nth value of the monomer IC curve, and M and N represent the lengths of the median IC curve and the monomer IC curve, respectively;

[0141]

[0142] Among them, d ij Represents the i-th sample point c in the median IC curve med(i) The Euclidean distance from the jth sample point c(j) in the IC curve of the monomer is calculated as: d ij =||c med (i)-c(j)||2,1≤i≤M,1≤j≤N;

[0143] Based on the distance matrix A, the DTW distance D(C med ,C) methods include:

[0144] Find an optimal regular path W in the distance matrix A best , so that C med The cumulative distance value from C is minimized, and the optimal regular path W bes for:

[0145]

[0146] Where K represents the total number of regular paths, and k represents the regular path number;

[0147] DTW distance D(C med ,C) is:

[0148]

[0149] Among them, W k Represents the position of the regularized path W in the distance matrix A, A(i,j) k It means that the starting point of the kth regular path is located in the i-th row and j-th column of matrix A.

[0150] In this embodiment, the process of obtaining the short-circuit current and short-circuit resistance of the micro-short-circuit monomer includes:

[0151]

[0152] Among them, I MSC is the micro short-circuit current, Q loss,p is the estimated power loss at the end of the pth charging of the micro-short-circuit monomer, Q loss,p-1 is the estimated power loss at the end of the p-1th charging of the micro-short-circuit monomer, T p is the time when the pth charging ends, T p-1 is the time when the p-1th charging ends;

[0153]

[0154] Among them, R MSC Indicates micro short circuit resistance, U M It is the average voltage between the end times of two adjacent charging cycles.

[0155] The embodiments described above are only descriptions of the preferred embodiments of the present invention and are not intended to limit the scope of the present invention. Without departing from the design spirit of the present invention, various modifications and improvements made to the technical solutions of the present invention by ordinary technicians in this field should all fall within the protection scope determined by the claims of the present invention.

Claims

1. A method for early internal short circuit diagnosis of lithium-ion battery pack based on dynamic time warping of incremental capacity, characterized in that: The following steps are involved: Arrange the terminal voltages of all cells in the lithium-ion battery pack in ascending order to obtain a median terminal voltage, and obtain a median IC curve based on the median terminal voltage; Obtaining a DTW distance between the IC curve of each monomer and the median IC curve, and detecting a micro-short-circuit monomer based on the DTW distance; The short-circuit current and the short-circuit resistance of the micro-short-circuit cell are estimated based on the change of the maximum charging voltage MCV.

2. The method for early internal short circuit diagnosis of lithium-ion battery pack based on dynamic time warping of incremental capacity according to claim 1, characterized in that: The median IC curve and the IC curve of each monomer were obtained by numerical differentiation method, specifically: Among them, IC EVI represents the extracted incremental capacity value, Q represents the battery charging capacity, V is the terminal voltage under constant current charging mode, Q2 and Q1 represent the battery charging capacity at two different times with a voltage interval of ΔV, and Q2-Q1 represents the change in charging capacity within the voltage interval ΔV.

3. The method for early internal short circuit diagnosis of lithium-ion battery pack based on dynamic time warping of incremental capacity according to claim 1, characterized in that: The method of obtaining the DTW distance between the IC curve of each monomer and the median IC curve includes: The median IC curve and the IC curve of a certain monomer are represented as C med and C; According to C med Construct the distance matrix A by using the Euclidean distance between any two points in C; Based on the distance matrix A, the DTW distance D(C med ,C); Among them, C med =[c med (1),c med (2),...,c med (M)], C=[c(1),c(2),...,c(N)]; Among them, c med (M) represents the Mth value of the median IC curve, c(N) represents the Nth value of the monomer IC curve, and M and N represent the lengths of the median IC curve and the monomer IC curve, respectively; Among them, d ij Represents the i-th sample point c in the median IC curve med (i) The Euclidean distance from the jth sample point c(j) in the IC curve of the monomer is calculated as: d ij =||c med (i)-c(j)||2,1≤i≤M,1≤j≤N; Based on the distance matrix A, the DTW distance D(C med ,C) methods include: Find an optimal regular path W in the distance matrix A best , so that C med The cumulative distance value from C is minimized, and the optimal regularized path W bes for: Where K represents the total number of regular paths, and k represents the regular path number; DTW distance D(C med ,C) is: Among them, W k Represents the position of the regularized path W in the distance matrix A, A(i,j) k It means that the starting point of the kth regular path is located in the i-th row and j-th column of matrix A.

4. The method for early internal short circuit diagnosis of lithium-ion battery pack based on dynamic time warping of incremental capacity according to claim 1, characterized in that: The method for obtaining the short-circuit current and short-circuit resistance of the micro-short-circuit monomer includes: Among them, I MSC is the micro short-circuit current, Q loss,p is the estimated power loss at the end of the pth charging of the micro-short-circuit monomer, Q loss,p-1 is the estimated power loss at the end of the p-1th charging of the micro-short-circuit monomer, T p is the time when the pth charging ends, T p-1 is the time when the p-1th charging ends; Among them, R MSC Indicates micro short circuit resistance, U M It is the average voltage between the end times of two adjacent charging cycles.

5. A lithium-ion battery pack early internal short circuit diagnosis system based on dynamic time warping of incremental capacity, characterized in that: include: IC curve calculation module, short-circuit monomer detection module and current resistance estimation module; The IC curve calculation module is used to sort the terminal voltages of all cells in the lithium-ion battery pack in ascending order to obtain a median terminal voltage, and obtain a median IC curve based on the median terminal voltage; The short-circuit monomer detection module is used to obtain the DTW distance between the IC curve of each monomer and the median IC curve, and detect a micro-short-circuit monomer based on the DTW distance; The current resistance estimation module is used to estimate the short-circuit current and short-circuit resistance of the micro-short-circuit monomer based on the change of the maximum charging voltage MCV.

6. The lithium-ion battery pack early internal short circuit diagnosis system based on dynamic time warping of incremental capacity according to claim 5, characterized in that: The median IC curve and the IC curve of each monomer were obtained by numerical differentiation method, specifically: Among them, IC EVI represents the extracted incremental capacity value, Q represents the battery charging capacity, V is the terminal voltage under constant current charging mode, Q2 and Q1 represent the battery charging capacity at two different times with a voltage interval of ΔV, and Q2-Q1 represents the change in charging capacity within the voltage interval ΔV.

7. The lithium-ion battery pack early internal short circuit diagnosis system based on dynamic time warping of incremental capacity according to claim 5, characterized in that: The short-circuit monomer detection module includes: a preset unit, a matrix construction unit and a distance calculation unit; The preset unit is used to represent the median IC curve and the IC curve of a certain monomer as C med and C; The matrix construction unit is used to med Construct the distance matrix A by using the Euclidean distance between any two points in C; The distance calculation unit is used to obtain the DTW distance D(C) based on the distance matrix A. med ,C); Among them, C med =[c med (1),c med (2),...,c med (M)], C=[c(1),c(2),...,c(N)]; Among them, c med (M) represents the Mth value of the median IC curve, c(N) represents the Nth value of the monomer IC curve, and M and N represent the lengths of the median IC curve and the monomer IC curve, respectively; Among them, d ij Represents the i-th sample point c in the median IC curve med (i) The Euclidean distance from the jth sample point c(j) in the IC curve of the monomer is calculated as: d ij =||c med (i)-c(j)||2,1≤i≤M,1≤j≤N; Based on the distance matrix A, the DTW distance D(C med ,C) The process includes: Find an optimal regular path W in the distance matrix A best , so that C med The cumulative distance value from C is minimized, and the optimal regular path W bes for: Where K represents the total number of regular paths, and k represents the regular path number; DTW distance D(C med ,C) is: Among them, W k Represents the position of the regularized path W in the distance matrix A, A(i,j) k It means that the starting point of the kth regular path is located in the i-th row and j-th column of matrix A.

8. The lithium-ion battery pack early internal short circuit diagnosis system based on dynamic time warping of incremental capacity according to claim 5, characterized in that: The process of obtaining the short-circuit current and short-circuit resistance of the micro-short-circuit monomer includes: Among them, I MSC is the micro short-circuit current, Q loss,p is the estimated power loss at the end of the pth charging of the micro-short-circuit monomer, Q loss,p-1 is the estimated power loss at the end of the p-1th charging of the micro-short-circuit monomer, T p is the time when the pth charging ends, T p-1 is the time when the p-1th charging ends; Among them, R MSC Indicates micro short circuit resistance, U M It is the average voltage between the end times of two adjacent charging cycles.

Citation Information

Patent Citations

  • Battery internal short circuit quantitative diagnosis method based on peak area of incremental capacity curve

    CN112924884A

  • Method for detecting internal short circuit of single lithium ion battery

    CN116540109A

  • Lithium battery health characteristic evaluation method and device based on DTW-TWP method

    CN117368775A

  • Lithium ion battery pack micro short circuit fault diagnosis method considering inconsistency

    CN117607704A

  • Method for estimating health state of lithium ion battery based on feature extraction and BP neural network

    CN117783913A

Cited By

  • Method and apparatus for detecting and evaluating gradual fault in lithium battery, device and storage medium

    WO2026076832A1