Electronic device
The concave structure is formed through laser drilling process and plasma etching process, which solves the problem of high impedance between the connecting pad and the conductive material in the electronic device, and improves the reliability and quality of the electronic device.
Patent Information
- Application Number
- CN202410266833.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2023-06-05
- Filing Date
- 2024-03-08
- Publication Date
- 2024-12-06
AI Technical Summary
The impedance between the existing electronic devices is high in the connection pad and other conductive materials, which affects their reliability and quality. Especially in the process of lightweight and thinning, it is difficult to effectively reduce the damage and impedance of the connection pad.
The laser drilling process is used in combination with plasma etching process to form a concave structure of the joint pad and the metal layer, reducing residues and reducing impedance, and improving the connection ability of the joint pad to other conductive materials.
It effectively reduces the impedance between the connecting pad and other conductive materials, improves the electrical properties and subsequent capabilities of the connecting pad, and enhances the reliability and quality of the electronic device.
Smart Images

Figure CN119092467A_ABST
Abstract
Description
Technical Field
[0001] The present disclosure relates to an electronic device, and more particularly to an electronic device capable of reducing impedance. Background Art
[0002] Electronic devices or spliced electronic devices have been widely used in different fields such as communication, display, automobile or aviation. With the rapid development of electronic devices, electronic devices are developing towards being lighter and thinner, so the reliability or quality requirements of electronic devices are higher. Summary of the invention
[0003] The present disclosure provides an electronic device, which can reduce the damage of a pad (or a metal layer) or reduce the impedance between the pad (or a metal layer) and other conductive materials.
[0004] According to an embodiment of the present disclosure, an electronic device includes a chip, a protective layer, a packaging layer, and a circuit structure. The chip has a base layer and at least one pad. The at least one pad is arranged on a first side of the base layer. The protective layer is arranged on the first side and has at least one opening. The at least one opening exposes a portion of at least one pad. The packaging layer surrounds the chip and the protective layer. The circuit structure is arranged on the packaging layer and electrically connected to the chip. The at least one pad has a concave surface. A portion of the circuit structure contacts the concave surface. BRIEF DESCRIPTION OF THE DRAWINGS
[0005] The accompanying drawings are included to provide a further understanding of the present disclosure, and are incorporated in and constitute a part of this specification. The drawings illustrate embodiments of the present disclosure and together with the description serve to explain the principles of the present disclosure.
[0006] Figures 1A to 1F is a cross-sectional schematic diagram of a method for manufacturing an electronic device according to a first embodiment of the present disclosure;
[0007] Figure 2 is a cross-sectional schematic diagram of a method for manufacturing an electronic device according to a second embodiment of the present disclosure;
[0008] Figure 3 is a cross-sectional schematic diagram of a method for manufacturing an electronic device according to a third embodiment of the present disclosure;
[0009] Figure 4 is a cross-sectional schematic diagram of a manufacturing method of an electronic device according to a fourth embodiment of the present disclosure;
[0010] Figure 5 A cross-sectional schematic diagram of an electronic device according to a fifth embodiment of the present disclosure;
[0011] Figure 6 A cross-sectional schematic diagram of an electronic device according to a sixth embodiment of the present disclosure;
[0012] Figure 7is a cross-sectional schematic diagram of an electronic device according to a seventh embodiment of the present disclosure;
[0013] Figure 8 It is a cross-sectional schematic diagram of an electronic device according to an eighth embodiment of the present disclosure.
[0014] Description of Figure Numbers
[0015] 10, 10c, 10d, 10e, 10f, 10g: electronic devices;
[0016] 100: chip;
[0017] 100a: first side;
[0018] 100b: second side;
[0019] 100c, 200a: side surface;
[0020] 100d: cambered surface;
[0021] 100s: basal layer;
[0022] 110: pad;
[0023] 111: concave;
[0024] 112, 411, 711, 712, 851, 852: surface;
[0025] 200: protective layer;
[0026] 210, 210a, 441, 501, 502: opening;
[0027] 211: First opening;
[0028] 300, 300c: encapsulation layer;
[0029] 310, 320, 421, 422, 740: through holes;
[0030] 400: Circuit structure;
[0031] 410, 410c: first metal layer;
[0032] 412: Depression;
[0033] 420: first insulating layer;
[0034] 430: second metal layer;
[0035] 440: second insulating layer;
[0036] 500, 710: insulation layer;
[0037] 600, 720, 722, 724, 726: conductive bumps;
[0038] 610, 730, 731, 855: connection pads;
[0039] 700, 700e, 700f, 700g: intermediary layer;
[0040] 750: metal layer;
[0041] 760, 761, 762, 800, 801, 802, 803: electronic components;
[0042] 850: Circuit board;
[0043] CS1, CS1a, CS2, CS2a, CS2c: chip structure;
[0044] H1, H3: height;
[0045] H2, H4: depth;
[0046] L: cutting line;
[0047] P: plasma etching process;
[0048] R1, R2: residues;
[0049] RL: release layer;
[0050] S1: first seed layer;
[0051] S2: second seed layer;
[0052] sub: carrier board;
[0053] UF: primer;
[0054] W1, W2, W5, W6: width;
[0055] W3: top width;
[0056] W4: bottom width;
[0057] X, Z: direction. DETAILED DESCRIPTION
[0058] The present disclosure can be understood by referring to the following detailed description in conjunction with the accompanying drawings. It should be noted that in order to make it easier for readers to understand and for the simplicity of the drawings, the multiple drawings in the present disclosure only depict a portion of the electronic device, and the specific elements in the drawings are not drawn according to the actual scale. In addition, the number and size of each element in the figure are only for illustration and are not intended to limit the scope of the present disclosure.
[0059] In the following description and claims, the words “including” and “comprising” are open-ended words, and thus should be interpreted as meaning “including but not limited to…”.
[0060] It should be understood that when an element or a film layer is referred to as being "on" or "connected to" another element or film layer, it may be directly on or directly connected to the other element or layer, or there may be an intervening element or film layer between the two (indirect case). Conversely, when an element is referred to as being "directly on" or "directly connected to" another element or film layer, there may be no intervening element or film layer between the two.
[0061] Although the terms "first", "second", "third" ... can be used to describe a variety of components, the components are not limited to these terms. These terms are only used to distinguish a single component from other components in the specification. The same terms may not be used in the claims, but may be replaced by first, second, third ... according to the order of the components declared in the claims. Therefore, in the following description, the first component may be the second component in the claims.
[0062] In the text, the terms "about", "approximately", "substantially", and "roughly" generally mean within 10%, within 5%, within 3%, within 2%, within 1%, or within 0.5% of a given value or range. The numbers given here are approximate numbers, that is, in the absence of specific descriptions of "about", "approximately", "substantially", and "roughly", the meanings of "about", "approximately", "substantially", and "roughly" can still be implied.
[0063] In some embodiments of the present disclosure, terms such as "connection" and "interconnection" may refer to two structures being in direct contact, or two structures not being in direct contact, with other structures disposed between the two structures, unless otherwise specified. Such terms may also include situations where both structures are movable or both structures are fixed. In addition, the term "coupling" includes any direct and indirect electrical connection means.
[0064] In some embodiments of the present disclosure, an optical microscope (OM), a scanning electron microscope (SEM), an α-step, an ellipsometer, or other suitable methods may be used to measure the area, width, thickness, or height of each element, or the distance or spacing between elements. Specifically, according to some embodiments, a scanning electron microscope may be used to obtain a cross-sectional structural image including the element to be measured, and the area, width, thickness, or height of each element, or the distance or spacing between elements may be measured.
[0065] In some embodiments of the present disclosure, "roughness" means that when observed by SEM, multiple surface protrusions and multiple surface depressions can be seen on the surface, and the peak of each of the multiple surface protrusions and the trough of each of the multiple surface depressions have a height difference of at least 0.1 to 5 μm. The determination of "roughness" herein may include using SEM, transmission electron microscope (TEM), etc., to observe the surface undulations at an appropriate same magnification, and taking a unit length (e.g., 10 μm) to compare the undulations. Here, "appropriate magnification" means that at least one surface can see at least 5 peaks of surface protrusions and at least 5 troughs of surface depressions under the field of view of this magnification. The value of the reference line L is taken as 0, the side toward the peak point Rp1-Rp5 is a positive value, and the side toward the trough point Rv1-Rv5 is a negative value. The numerical difference between the peak point Rp1 and the trough point Rv1, the numerical difference between the peak point Rp2 and the trough point Rv2, the numerical difference between the peak point Rp3 and the trough point Rv3, the numerical difference between the peak point Rp4 and the trough point Rv4, and the numerical difference between the peak point Rp5 and the trough point Rv5 are calculated respectively. The roughness Rz is obtained by summing up the above five groups of numerical differences and taking the average value thereof. Therefore, the roughness Rz can be expressed by the following formula, wherein the extension direction of the reference line L is perpendicular to the normal direction of the electronic device:
[0066]
[0067] The electronic device disclosed herein may include a power management device, a display device, an antenna device, a communication device, a sensing device or a splicing device, but is not limited thereto. The electronic device may be a bendable or flexible electronic device. The electronic device may, for example, include liquid crystal (LC), light emitting diodes, quantum dots (QD), fluorescence, phosphorescence, other suitable materials, or any combination of the above materials, but is not limited thereto; the light emitting diode may, for example, include an organic light emitting diode (OLED), a sub-millimeter light emitting diode (mini LED), a micro light emitting diode (micro LED) or a quantum dot light emitting diode (quantum dot, QD, which may be, for example, QLED, QDLED), but is not limited thereto. The antenna device may, for example, be a phased array antenna, but is not limited thereto. The splicing device may, for example, be a display splicing device or an antenna splicing device, but is not limited thereto. It should be noted that the electronic device may be any combination of the aforementioned, but is not limited thereto. The following will illustrate the contents of the disclosure using an electronic device, but the disclosure is not limited thereto.
[0068] It should be noted that the following embodiments may replace, reorganize, or mix features in several different embodiments to complete other embodiments without departing from the spirit of the present disclosure. Features between embodiments may be mixed and matched as long as they do not violate the spirit of the invention or conflict with each other.
[0069] Reference will now be made in detail to exemplary embodiments of the present disclosure, examples of which are illustrated in the accompanying drawings. Whenever possible, the same reference numerals are used in the drawings and the description to refer to the same or like parts.
[0070] The manufacturing method of the electronic device disclosed herein can be applied, for example, to a wafer-level package (WLP) process or a panel-level package (PLP) process, and can be a chip-first or chip-last redistribution layer first (RDL first) manufacturing method. The following description is made by taking the chip-first redistribution layer first manufacturing method as an example, but is not limited thereto.
[0071] Figures 1A to 1F This is a cross-sectional diagram of a method for manufacturing an electronic device according to a first embodiment of the present disclosure. Figure 1F, the electronic device 10 of this embodiment may include a chip 100, a protective layer 200, a packaging layer 300 and a circuit structure 400. The chip 100 has a base layer 100s and at least one pad 110. The at least one pad 110 is disposed on the base layer 100s. The chip 100 includes a first side, and further, the first side 100a of the base layer 100s on which the pad 110 is disposed may be referred to as the first side of the chip 100. The protective layer 200 is disposed on the first side 100a of the base layer 100s and has at least one opening 210. The at least one opening 210 exposes a portion of the at least one pad 110. The packaging layer 300 surrounds the chip 100 and the protective layer 200. The circuit structure 400 is disposed on the packaging layer 300 and is electrically connected to the chip 100. The at least one pad 110 has a concave surface 111. A portion of the circuit structure 400 contacts the concave surface 111. The electronic device 10 of the present embodiment may be applied to a power module, a semiconductor packaging device, a display device, a light emitting device, a backlight device, an antenna device, a sensing device or a splicing device, but is not limited thereto.
[0072] Then, the manufacturing method of the electronic device 10 of this embodiment will be described below. In this embodiment, the manufacturing method of the electronic device 10 may include but is not limited to the following steps and their sequence:
[0073] First, please refer to Figure 1A , provide the chip 100 on a carrier with a release layer (not shown), form an insulating layer 500 on the chip 100, and form a protective layer 200 on the chip 100 and the insulating layer 500. Specifically, the base layer 100s of the chip 100 has a first side 100a, a second side 100b and a side surface 100c, wherein the first side 100a and the second side 100b are opposite to each other, and the side surface 100c connects the first side 100a and the second side 100b. The chip 100 includes at least one pad 110 ( Figure 1A Four pads 110 are schematically shown, but not limited thereto), and the pads 110 are disposed on the first side 100a of the base layer 100s. The pads 110 have a surface 112 away from the base layer 100s. The pads 110 have a height H1, and the height H1 is, for example, the maximum height of the pads 110 measured along the direction Z (i.e., the normal direction of the chip 100 or the normal direction of the base layer 100s). In the present embodiment, the base layer 100s may include organic materials, glass, wafers, silicon substrates, doped silicon substrates, gallium nitride, other suitable substrate materials, or combinations thereof, but not limited thereto. In the present embodiment, the material of the pads 110 may include aluminum, titanium, copper, molybdenum, silver, gold, tantalum, other suitable conductive materials, or combinations thereof, but not limited thereto.
[0074] The insulating layer 500 is disposed on the first side 100a of the base layer 100s, and the insulating layer 500 is disposed between the chip 100 and the protective layer 200. The insulating layer 500 has an opening 501 and an opening 502. The opening 501 exposes a portion of the pad 110, and the opening 502 exposes a portion of the chip 100. In the present embodiment, the material of the insulating layer 500 may include silicon oxide, silicon nitride, aluminum oxide, polyimide (PI), photosensitive polyimide (PSPI), other suitable inorganic materials, other suitable organic materials, or a combination thereof, but is not limited thereto. In some embodiments, along the Z direction, the insulating layer 500 may be a single layer or a multi-layer stack, and the thickness of the insulating layer 500 may be between 0.5 micrometers (μm) and 10 micrometers. In some embodiments, the coefficient of thermal expansion (CTE) of the insulating layer 500 may be 0.01 ppm / ° C. to 5 ppm / ° C., and the Young's modulus may be 100 GPa to 300 GPa, but is not limited thereto.
[0075] The protective layer 200 is disposed on the insulating layer 500, in the opening 501 and in the opening 502, and the protective layer 200 can cover the portion of the pad 110 and the portion of the chip 100 exposed by the insulating layer 500. The protective layer 200 can reduce the occurrence of cracks in the chip 100 during the subsequent singulation process. In the present embodiment, the material of the protective layer 200 may include an organic material. For example, the material of the protective layer 200 may be polyimide, photosensitive polyimide, epoxy resin, ajinomoto build-up layer (ABF), other suitable polymer materials or a combination thereof, but not limited thereto. In some embodiments, along the Z direction, the thickness of the protective layer 200 is between 5 micrometers (μm) and 30 micrometers, and the material of the protective layer 200 may also include a filling material with a particle size of 0.05 micrometers (μm) to 20 micrometers, but not limited thereto. In some embodiments, the coefficient of thermal expansion (CTE) of the protective layer 200 may be 10ppm / °C to 40ppm / °C, the Young's modulus may be 3GPa to 15GPa, and the tensile strength may be 50MPa to 110MPa, but not limited thereto. The above design can reduce the risk of cracking of the chip 100 during the singulation process, but not limited thereto.
[0076] Next, please refer to Figure 1B, at least one opening 210 ( Figure 1B Four openings 210 are schematically shown, but not limited thereto), to expose a portion of the pad 110 and form a concave surface 111 of the pad 110, so as to manufacture the chip structure CS1.
[0077] Specifically, the first surface treatment process may include laser drilling, plasma etching, chemical etching or a combination thereof, but is not limited thereto. The step of forming at least one opening 210 and the concave surface 111 may include the following steps: firstly, laser drilling is performed on the protective layer 200 to form a first opening 211 that can expose a portion of the surface 112 of the pad 110; then, plasma etching is performed on the first opening 211 to remove the residue R1 in the first opening 211 (for example, the metal oxide on the pad 110 and / or the residual part of the protective layer remaining in the first opening 211 after the drilling process), and the opening 210 and the concave surface 111 of the pad 110 are formed. Therefore, compared to the general method of performing the first surface treatment process using only the laser drilling process, the first surface treatment process of this embodiment uses the laser drilling process combined with the plasma etching process P, which can reduce the damage of the pad 110 or reduce the residue R1 in the opening 210, thereby reducing the impedance (or contact resistance) between the pad 110 and other conductive materials, improving the electrical properties of the pad 110, or improving the bonding ability between the pad 110 and other conductive materials. According to some embodiments, the first surface treatment process may include the use of a gas, such as oxygen, carbon monoxide, carbon dioxide, a fluorine-containing gas, a sulfur-containing gas, a passivation gas, a reducing gas, or a combination thereof, but is not limited thereto. According to some embodiments, the first surface treatment process may further include a cleaning step of the first opening 211 after the plasma etching process P, and the cleaning step includes the use of a solvent or a gas, but is not limited thereto. Through the first surface treatment process, the electrical properties of the pad 110 can be improved or the bonding ability between the pad 110 and other conductive materials can be improved, but is not limited thereto.
[0078] The first opening 211 and the opening 210 of the protective layer 200 have a width W1 and a width W2, respectively. The width W1 is, for example, the maximum width measured along the direction X (i.e., the horizontal direction in the figure) from the top of the first opening 211, and the width W2 is, for example, the maximum width measured along the direction X from the top of the opening 210. In the present embodiment, the width W2 of the opening 210 may be greater than the width W1 of the first opening 211, but is not limited thereto.
[0079] In the present embodiment, the plasma etching process P may include at least one plasma etching step. For example, the plasma etching process P may be, for example, a plasma etching step performed once using a plasma etching method with a high etching rate; or the plasma etching process P may also be, for example, a plasma etching method with a high etching rate is first used to perform a first plasma etching step, and then a plasma etching method with a low etching rate is used to perform a second plasma etching step (i.e., two plasma etching steps are performed). In the present embodiment, the plasma etching method with a high etching rate may include inductively coupled plasma-capacitive coupled plasma (ICP-CCP) or inductively coupled plasma-reactive-ion etching (ICP-RIE), and the plasma etching method with a low etching rate may include high density plasma (HDP), but is not limited thereto. In addition, in the present embodiment, the plasma etching process P may, for example, use a fluorine-based gas, but is not limited thereto.
[0080] The concave surface 111 of the pad 110 is, for example, a surface of the pad 110 that is concave from the surface 112 toward the chip 100. The concave surface 111 may be connected to the surface 112, the concave surface 111 and the surface 112 are not coplanar, and the concave surface 111 may overlap the opening 210 in the direction Z. The concave surface 111 has a depth H2, wherein the depth H2 is, for example, the minimum distance between the surface 112 of the pad 110 and the bottom of the concave surface 111 measured along the direction Z. In the present embodiment, the depth H2 of the concave surface 111 of at least one pad 110 may be 30 nanometers (nm) to 70 nanometers to ensure that the depth H2 of the concave surface 111 is not too deep to affect the conductivity of the pad 110, but the invention is not limited thereto. In the present embodiment, the ratio of the depth H2 of the concave surface 111 of at least one pad 110 to the height H1 of at least one pad 110 may be 1% to 15% (i.e., 1%≤H2 / H1≤15%), or 3% to 10% (i.e., 3%≤H2 / H1≤10%), to ensure that the depth H2 of the concave surface 111 is not too deep to affect the conductivity of the pad 110, but is not limited thereto.
[0081] Next, please also refer to Figure 1B and Figure 1C Specifically, a cutting tool is used to cut along the Figure 1B The cutting line L in Figure 1B The large chip structure CS1 shown is cut into Figure 1C The chip structure CS2 of the small piece is shown.
[0082] Next, please refer to Figures 1D to 1F First, a carrier board sub and a release layer RL disposed on the carrier board sub are provided; then, the carrier board sub is turned upside down as shown in FIG. Figure 1C The chip structure CS2 is shown, and the chip structure CS2 that is turned upside down is fixed on the release layer RL; then, a packaging layer 300 is formed on the carrier sub and the release layer RL, so that the packaging layer 300 can surround the chip 100 and the protective layer 200; then, the release layer RL and the carrier sub are removed, and the chip structure CS2 is turned upside down again; then, a circuit structure 400 is formed on the packaging layer 300, so that the circuit structure 400 can be electrically connected to the chip 100; then, a conductive bump (conductive stud) 600 is formed on the circuit structure (conductive stud) 600, and a connection pad (connection pad) 610 is formed on the conductive bump 600.
[0083] For details, please refer to Figure 1D After forming the encapsulation layer 300 and removing the release layer RL and the carrier sub, a first seed layer S1 is formed on the encapsulation layer 300, a first metal layer 410 is formed on the first seed layer S1, and a first insulating layer 420 is formed on the first metal layer 410. The thickness of the first seed layer S1 may be between 0.1 micrometers and 1 micrometers. By providing the seed layer on the insulating layer, the bonding force between the subsequent film layer and the insulating layer can be improved, but it is not limited to this. The thickness of the first metal layer 410 may be between 5 micrometers and 25 micrometers. Specifically, in the cross-sectional view, the encapsulation layer 300 may at least contact the side surface 100c of the chip 100. The first seed layer S1 may be disposed on the protective layer 200, on the encapsulation layer 300, and in the opening 210. The first metal layer 410 may be disposed on the first seed layer S1 and in the opening 210. The first metal layer 410 has a surface 411 away from the chip 100 along the Z direction. The first metal layer 410 can be electrically connected to the pad 110 of the chip 100 through the first seed layer S1. The first metal layer 410 has a height H3, and the height H3 is, for example, the height of the first metal layer 410 measured along the direction Z. In the present embodiment, the height H3 of the first metal layer 410 can be 5 microns to 25 microns (i.e., 5μm≤H3≤25μm), or 10 microns to 20 microns (i.e., 10μm≤H3≤20μm), but is not limited thereto. The roughness (Rz) of the surface 411 of the first metal layer 410 can be 0.1 microns to 5 microns, but is not limited thereto. The first insulating layer 420 can cover part of the protective layer 200 and part of the encapsulation layer 300. In detail, the first insulating layer 420 can directly contact part of the protective layer 200 and part of the encapsulation layer 300.
[0084] Please continue to refer to Figure 1E , a through hole 421 ( Figure 1E Two through holes 421 are schematically shown, but not limited thereto), to expose a portion of the first metal layer 410 and form a recess 412 of the first metal layer 410. Specifically, the second surface treatment process may include a laser drilling process, a plasma etching process P, and a micro etching process (micro etching), but not limited thereto. Among them, the steps of forming the through hole 421 and the recess 412 may include the following steps: first, a laser drilling process is performed on the first insulating layer 420 to form a first through hole 422 that can expose a portion of the surface 411 of the first metal layer 410; then, a plasma etching process P is performed on the first through hole 422 to remove the residue R2 in the first through hole 422 (for example, the metal oxide on the first metal layer 410 and / or the residual portion of the first insulating layer remaining in the first through hole 422 after the drilling process), and form the through hole 421 and the recess 412 of the first metal layer 410; then, a micro-etching process (for example, wet etching) is performed on the through hole 421 to improve its bonding ability by adjusting the surface roughness of the recess 412. Therefore, compared to the general method of only using a laser drilling process to perform the second surface treatment process, the second surface treatment process of the present embodiment uses a laser drilling process combined with a plasma etching process P, which can reduce damage to the first metal layer 410 or reduce the residue R2 in the through hole 421, thereby reducing the impedance (or contact resistance) between the first metal layer 410 and other conductive materials, improving the electrical properties of the first metal layer 410, or improving the adhesion between the first metal layer 410 and other conductive materials.
[0085] The through hole 421 of the first insulating layer 420 has a top width W3 and a bottom width W4. The top width W3 is, for example, the maximum width of the top of the through hole 421 measured along the direction X, and the bottom width W4 is, for example, the maximum width of the bottom of the through hole 421 measured along the direction X. In the present embodiment, the ratio of the bottom width W4 to the top width W3 may be 0.3 to 0.5 (i.e., 0.3≤W4 / W3≤0.5), but is not limited thereto.
[0086] The recess 412 of the first metal layer 410 is, for example, a groove of the first metal layer 410 that is concave from the surface 411 toward the chip 100. The recess 412 may be connected to the surface 411, the recess 412 and the surface 411 are not coplanar, and the recess 412 may overlap the through hole 421 in the direction Z. The recess 412 has a depth H4, wherein the depth H4 is, for example, the minimum distance between the surface 411 of the first metal layer 410 and the bottom of the recess 412 measured along the direction Z. In the present embodiment, the depth H4 of the recess 412 of the first metal layer 410 may be 0.1 micrometer to 5 micrometers (i.e., 0.1μm≤H4≤5μm), or 0.5 micrometer to 3 micrometers (i.e., 0.5μm≤H4≤3μm), to ensure that the depth H4 of the recess 412 is not too deep to affect the conductivity of the first metal layer 410, but is not limited thereto.
[0087] Please continue to refer to Figure 1F After forming the through hole 421 of the first insulating layer 420 and the recess 412 of the first metal layer 410, a second seed layer S2 is formed on the first insulating layer 420, a second metal layer 430 is formed on the second seed layer S2, and a second insulating layer 440 is formed on the second metal layer 430. Specifically, the second seed layer S2 may be disposed on the first insulating layer 420 and in the through hole 421. The second metal layer 430 may be disposed on the second seed layer S2 and in the through hole 421. The second metal layer 430 may be electrically connected to the first metal layer 410 through the second seed layer S2. The second insulating layer 440 may cover a portion of the first insulating layer 420. The second insulating layer 440 has an opening 441 ( Figure 1F Two openings 441 are schematically shown, but not limited thereto), and the openings 441 may expose a portion of the second metal layer 430 .
[0088] In the present embodiment, the circuit structure 400 may be a redistribution layer (RDL) or a redistribution structure (RDL structure), and the circuit structure 400 may be electrically connected to other chips or electronic units through solder balls, connection pads or other bonding elements. In the present embodiment, the circuit structure 400 may include a stack structure of at least one metal layer (i.e., a first metal layer 410 and a second metal layer 430) and at least one insulating layer (i.e., a first insulating layer 420 and a second insulating layer 440), and the circuit structure 400 may redistribute the circuits and / or further increase the circuit fan-out area, or the circuit structure 400 may allow different electronic components to be electrically connected to each other through the redistribution layer or redistribution structure of the circuit structure 400. For example, the circuit structure 400 may adjust the contact pad spacing and thus adjust the circuit fan-out area, for example, the spacing between two adjacent contact pads of the circuit structure contacting one end of the chip is smaller than the spacing between two adjacent contact pads of the circuit structure away from one end of the chip, but the present invention is not limited thereto.
[0089] For example, if Figure 1F As shown, the circuit structure 400 may include a first seed layer S1, a first metal layer 410, a first insulating layer 420, a second seed layer S2, a second metal layer 430 and a second insulating layer 440. The first seed layer S1 is disposed on the pad 110. The first metal layer 410 is disposed on the first seed layer S1, the first metal layer 410 may contact the concave surface 111 of the pad 110, and the first metal layer 410 has a recess 412. The first insulating layer 420 is disposed on the first metal layer 410 and includes a through hole 421. The second seed layer S2 is disposed on the first metal layer 410. The second metal layer 430 is disposed on the second seed layer S2 and the first insulating layer 420, the second metal layer 430 may contact the recess 412 of the first metal layer 410, and the second metal layer 430 may be electrically connected to the first metal layer 410 through the through hole 421 of the first insulating layer 420. The second insulating layer 440 is disposed on the second metal layer 430 .
[0090] Although Figure 1F The circuit structure 400 exemplarily includes two seed layers (i.e., a first seed layer S1 and a second seed layer S2), two metal layers (i.e., a first metal layer 410 and a second metal layer 430), two insulating layers (i.e., a first insulating layer 420 and a second insulating layer 440), two through holes 421, two openings 441, and two recesses 412. However, the present disclosure does not limit the number of seed layers, metal layers, insulating layers, through holes, openings, and recesses in the circuit structure. It should be understood that the residue R2 in each through hole (e.g., the residual portion of the insulating layer remaining in the through hole after the metal oxide and / or drilling process) needs to be reduced, or each through hole may overlap the recess of the metal layer in the direction Z.
[0091] In the present embodiment, the silicon content of the interface between the first seed layer S1 and the pad 110 is less than 1% to reduce the impedance (or contact resistance) between the first metal layer 410 and the pad 110; and the silicon content and / or carbon content of the interface between the second seed layer S2 and the first metal layer 410 is less than 1% to reduce the impedance (or contact resistance) between the second metal layer 430 and the first metal layer 410. For example, elemental analysis can be performed by scanning electron microscopy at an appropriate magnification, such as a magnification of 20 microns per unit length. For example, an area of a suitable size can be selected at the interface between the second seed layer S2 and the first metal layer 410 for elemental analysis. The area of the area can be 1 micron*1 micron, 3 microns*3 microns or 5 microns*5 microns, and the area needs to cover both the film layer to be analyzed and the interface between the two film layers.
[0092] In the present embodiment, the first seed layer S1 and the second seed layer S2 may be a single-layer or multi-layer metal layer, and the materials of the first seed layer S1 and the second seed layer S2 may include tantalum, titanium, copper, aluminum, nickel, indium-tin oxide (ITO), other suitable conductive materials or a combination thereof, but not limited thereto. The first metal layer 410 and the second metal layer 430 may be a single-layer structure or a multi-layer structure, and the materials of the first metal layer 410 and the second metal layer 430 may include copper, titanium, chromium, aluminum, gold, nickel, tin, silver and other metal alloys, other suitable conductive materials or a combination thereof, but not limited thereto. The first insulating layer 420 and the second insulating layer 440 may be a single-layer structure or a multi-layer structure, and the materials of the first insulating layer 420 and the second insulating layer 440 may include photosensitive polyimide, Ajinomoto laminated film, other suitable insulating materials or a combination thereof, but not limited thereto.
[0093] In the present embodiment, the manufacturing method of the circuit structure 400 may include providing a stack structure of at least one metal layer and at least one insulating layer, and may include process steps such as yellow light, etching, surface treatment, laser, and electroplating. Among them, the surface treatment includes roughening the surface of the insulating layer or the surface of the metal layer so that the insulating layer or the metal layer can have a rough surface and improve its bonding ability. In the present embodiment, the method for determining the rough surface may be, for example: using a scanning electron microscope (Scanning Electron Microscope, SEM) or a transmission electron microscope (Transmission electron microscope, TEM) and other tools, at an appropriate magnification, taking a unit length (for example, 10 microns) to observe and compare the peak and valley fluctuations of the surface, when the peak and valley fluctuations of the surface have a distance difference of 0.15 microns to 1 micron, it is determined to be a rough surface.
[0094] Please continue to refer to Figure 1F After forming the opening 441 of the second insulating layer 440, a conductive bump 600 is formed in the opening 441 of the second insulating layer 440, and a connection pad 610 is formed on the conductive bump 600. The conductive bump 600 can electrically connect the circuit structure 400 and the connection pad 610, and the chip 100 can be electrically connected to the connection pad 610 through the pad 110, the circuit structure 400 and the conductive bump 600. At this point, the electronic device 10 of this embodiment can be substantially completed.
[0095] Other embodiments will be listed below for illustration. It must be noted that the following embodiments use the component numbers and some contents of the previous embodiments, wherein the same numbers are used to represent the same or similar components, and the description of the same technical contents is omitted. The description of the omitted parts can be referred to the previous embodiments, and the following embodiments will not be repeated.
[0096] Figure 2 It is a cross-sectional schematic diagram of a manufacturing method of an electronic device according to a second embodiment of the present disclosure. Figure 2 To continue Figure 1A and replace Figure 1B steps. Figure 2 Examples and Figures 1A to 1F The same or similar components in the embodiments can be made of the same materials or methods, so the following description of the same and similar parts in the two embodiments will not be repeated, and the differences between the two embodiments will be mainly described.
[0097] Specifically, please refer to Figure 2 When performing the first surface treatment process, the protective layer 200 is first subjected to a laser drilling process to form an opening 210a that can expose the insulating layer 500, the opening 501 and the pad 110; then, the opening 501 is subjected to a plasma etching process P to remove the residue R1 in the opening 501 (for example, the metal oxide on the pad 110 and / or the residual portion of the protective layer remaining in the opening 501 after the drilling process), and to form a concave surface 111 of the pad 110 to obtain the chip structure CS1a.
[0098] The opening 501 of the insulating layer 500 and the opening 210a of the protective layer 200 have a width W5 and a width W6, respectively. The width W5 is, for example, the maximum width measured along the direction X (i.e., the horizontal direction in the figure) at the top of the opening 501, and the width W6 is, for example, the maximum width measured along the direction X at the top of the opening 210a. In the present embodiment, the width W6 of the opening 210a may be greater than the width W5 of the opening 501, but is not limited thereto.
[0099] Figure 3 It is a cross-sectional schematic diagram of a manufacturing method of an electronic device according to a third embodiment of the present disclosure. Figure 3 To continue Figure 1B and replace Figure 1C steps. Figure 3 Examples and Figures 1A to 1F The same or similar components in the embodiments can be made of the same materials or methods, so the following description of the same and similar parts in the two embodiments will not be repeated, and the differences between the two embodiments will be mainly described.
[0100] Specifically, please refer to Figure 3 In the chip structure CS2a of the cut piece, the side surface 200a of the protective layer 200 is an inclined surface, and the intersection of the first side 100a and the side surface 100c of the base layer 100s of the chip 100 has a curved surface 100d. The protective layer 200 can expose the curved surface 100d of the chip 100. When the chip 100 has the curved surface 100d, the contact area can be increased, thereby improving the bonding ability with the packaging layer 300, but it is not limited thereto.
[0101] Figure 4 It is a cross-sectional schematic diagram of a manufacturing method of an electronic device according to a fourth embodiment of the present disclosure. Figure 4 To continue Figure 1A and replace Figures 1B to 1D steps, or Figure 4 To continue Figure 2 and replace Figure 1C to Figure 1D steps. Figure 4 Examples and Figures 1A to 1F as well as Figure 2 The same or similar components in the embodiments can be made of the same materials or methods, so the following description of the same and similar parts in the two embodiments will not be repeated, and the differences between the two embodiments will be mainly described.
[0102] Specifically, a singulation process is first performed to utilize a cutting tool and along Figure 2 The cutting line L in Figure 2 The large chip structure CS1a shown is cut into small chip structures CS2c. Figure 1D The steps are as follows: providing a carrier (not shown) and a release layer (not shown) disposed on the carrier; fixing the chip structure CS2c turned upside down on the release layer; forming a packaging layer 300c on the carrier and the release layer so that the packaging layer 300c can surround the chip 100 and the protective layer 200; removing the release layer and the carrier, and fixing the chip structure CS2c surrounded by the packaging layer 300c on the interposer 700; forming a circuit structure 400c on the packaging layer 300 so that the circuit structure 400c can be electrically connected to the chip 100, so as to obtain the following Figure 4 The electronic device 10c is shown.
[0103] Please refer to Figure 4 In the electronic device 10c of the present embodiment, the interposer 700 may include an insulating layer 710, a plurality of conductive bumps (i.e., conductive bumps 720, conductive bumps 722, and conductive bumps 724), and a plurality of connection pads 730. The conductive bumps 720, conductive bumps 722, and conductive bumps 724 penetrate the insulating layer 710, and the plurality of connection pads 730 are disposed on the conductive bumps 720, conductive bumps 722, and conductive bumps 724, respectively.
[0104] The packaging layer 300c is disposed on the interposer 700. The packaging layer 300c may cover the side surface 100c of the chip 100 and expose the second side 100b of the chip 100. The packaging layer 300c may include a through hole 310 and a through hole 320 penetrating the packaging layer 300c. The through hole 310 may expose the conductive bump 720, and the through hole 320 may expose the conductive bump 724.
[0105] The circuit structure 400c may include a first seed layer S1c, a first metal layer 410c, and a first insulating layer 420c. The first seed layer S1c is disposed on the packaging layer 300c, in the through holes 310 and 320, on the protection layer 200, in the opening 210a, and in the opening 501. The first metal layer 410 may be disposed on the first seed layer S1, in the through holes 310 and 320, in the opening 210a, and in the opening 501. The first insulating layer 420 is disposed on the first metal layer 410, and the first insulating layer 420 may cover a portion of the protection layer 200 and a portion of the packaging layer 300c.
[0106] The first metal layer 410c can be electrically connected to the pad 110 of the chip 100 through the opening 210a and the opening 501. The first metal layer 410c can also be electrically connected to the conductive bump 720 (or the conductive bump 724) through the through hole 310 (or the through hole 320). In other words, the chip 100 can be electrically connected to the connection pad 730 through the pad 110, the opening 501, the opening 210a, the first metal layer 410c and the conductive bump 720 (or the conductive bump 724). In addition, the chip 100 can also be electrically connected to the connection pad 730 through the conductive bump 722. Alternatively, according to some embodiments, the surface of the conductive bump 722 away from the chip 100 may not have the connection pad 730, and in a direction perpendicular to the Z direction (i.e., the X direction), the width of the conductive bump 722 is greater than or equal to the width of the chip 100, and the width referred to is, for example, the maximum width. Through the above design, the conductive bump 722 can increase the heat dissipation capacity of the electronic device, but is not limited thereto.
[0107] Figure 5 This is a cross-sectional diagram of an electronic device according to a fifth embodiment of the present disclosure. Figure 5 and Figure 4The electronic device 10d of this embodiment is Figure 4 The electronic device 10d of the present embodiment is similar to the electronic device 10c in the embodiment, but the difference between the two is that the electronic device 10d of the present embodiment further includes an electronic component 800. Specifically, the electronic component 800 replaces Figure 4 The electronic component 800 is disposed in the packaging layer 300c, and the electronic component 800 can be electrically connected to the corresponding first metal layer 410 and the conductive bump 720. In some embodiments, the electronic component 800 can also be replaced by Figure 1F The electronic device 10. The electronic component 800 may include silicon, doped silicon, a conductor, a capacitor, an inductor or other suitable components. In addition, in the electronic device 10d of the present embodiment, the second side 100b of the base layer 100s of the chip 100 may have an accommodation space R, so that part of the conductive bump 722 may extend into the accommodation space R. This design may improve the bonding capability or the heat dissipation effect, but is not limited thereto.
[0108] Figure 6 This is a cross-sectional diagram of an electronic device according to a sixth embodiment of the present disclosure. Figure 6 and Figure 1F The electronic device 10e of this embodiment and Figure 1F The electronic device 10e of the embodiment is similar to the electronic device 10 in the embodiment, but the difference between the two is that the electronic device 10e of the present embodiment also includes electronic components 801, electronic components 802, electronic components 803, interposer 700e and circuit board 850. Through the stacking of components, a structure in which the chip is set on the interposer and the interposer is set on the circuit board can be realized, such as CoIoS (chip on interposer on substrate), wherein the interposer may include glass, silicon wafer, redistribution structure, PSPI, ABF carrier, a combination of the above or other suitable insulating layers or dielectric layers. In addition, the electronic device 10e may further include a primer UF, which may be filled between the electronic component 801 and the interposer 700e, or the primer UF may be filled between the interposer 700e and the circuit board 850, and the primer UF may contact the side surface of the electronic component.
[0109] Specifically, please refer to Figure 6 The circuit board 850 has a surface 851 and a surface 852 opposite to each other. The circuit board 850 may include a connection pad 855, and the connection pad 855 is disposed on the surface 852 of the circuit board 850.
[0110] The interposer 700e is disposed on the surface 851 of the circuit board 850. The interposer 700e may include an insulating layer 710, a plurality of connection pads 730, and a plurality of through holes 740. The insulating layer 710 has a surface 711 and a surface 712 opposite to each other. The plurality of connection pads 730 are respectively disposed on the surface 712 of the insulating layer 710, so that the interposer 700e can be bonded to the surface 851 of the circuit board 850 through the plurality of connection pads 730. The plurality of through holes 740 respectively penetrate the insulating layer 710, and the plurality of through holes 740 can extend from the surface 711 to the surface 712 of the insulating layer 710. The plurality of through holes 740 are filled with conductive materials, and the plurality of through holes 740 can be electrically connected to the corresponding connection pads 610 and the corresponding connection pads 730, respectively.
[0111] Electronic component 801, electronic component 802, electronic component 803, and Figure 1F The electronic device 10 includes a connection pad 610, and an electronic component 801, an electronic component 802, an electronic component 803 and Figure 1F The electronic device 10 can be bonded to the surface 711 of the insulating layer 710 of the intermediary layer 700e through the connection pad 610. In some embodiments, at least one of the electronic component 801, the electronic component 802, and the electronic component 803 can also be replaced by Figure 1F An electronic device 10.
[0112] Figure 7 This is a cross-sectional diagram of an electronic device according to the seventh embodiment of the present disclosure. Figure 7 and Figure 6 The electronic device 10f of this embodiment and Figure 6 The electronic device 10e in the embodiment is similar to the electronic device 10e in the embodiment, but the difference between the two is that in the electronic device 10f of the present embodiment, the intermediate layer 700f is a redistribution layer or a redistribution structure.
[0113] Specifically, please refer to Figure 7, the intermediary layer 700f is disposed on the surface 851 of the circuit board 850. The intermediary layer 700f may include an insulating layer 710, a plurality of conductive bumps 726, a plurality of connection pads 730, a plurality of connection pads 731, a plurality of through holes 740, and a plurality of metal layers 750. The insulating layer 710 has a surface 711 and a surface 712 opposite to each other. The plurality of connection pads 730 are respectively disposed on the surface 712 of the insulating layer 710, so that the intermediary layer 700f can be bonded to the surface 851 of the circuit board 850 through the plurality of connection pads 730. The plurality of connection pads 731 are respectively disposed on the surface 711 of the insulating layer 710. The plurality of conductive bumps 726 are respectively disposed on the corresponding connection pads 731. The plurality of metal layers 750 are respectively disposed in the insulating layer 710. The plurality of through holes 740 respectively penetrate a portion of the insulating layer 710. The plurality of through holes 740 are filled with conductive materials, and the plurality of through holes 740 can electrically connect the metal layers 750 of different layers.
[0114] In some embodiments, the intermediate layer 700f can be manufactured using a manufacturing method similar to the circuit structure 400 in the electronic device 10f (including a laser drilling process in the second surface treatment process combined with a plasma etching process P) to reduce damage to the metal layer 750 or reduce residues in the through hole 740, thereby reducing the impedance (or contact resistance) between the metal layer 750 and other conductive materials, improving the electrical properties of the metal layer 750, or improving the bonding ability between the metal layer 750 and other conductive materials.
[0115] Electronic component 801, electronic component 802 and Figure 1F The electronic device 10 includes a connection pad 610 and a conductive bump 600 disposed on the connection pad 610, and an electronic component 801, an electronic component 802 and Figure 1F The electronic device 10 can be bonded to the connection pad 731 of the interposer 700e through the connection pad 610 and the conductive bump 726. In some embodiments, at least one of the electronic component 801 and the electronic component 802 can also be replaced by Figure 1F An electronic device 10.
[0116] Figure 8 This is a cross-sectional diagram of an electronic device according to an eighth embodiment of the present disclosure. Figure 8 and Figure 7 The electronic device 10g of this embodiment and Figure 7The electronic device 10f is similar to the electronic device 10g in the embodiment, but the difference between the two is that: in the electronic device 10g of the present embodiment, the intermediate layer 700g also includes an electronic component 760, an electronic component 761 and an electronic component 762. For example, the electronic component can be, for example, a capacitor, a silicon-through-hole substrate, a chip, a circuit board, a combination of the above or other suitable electronic components. The electronic component 801 can be electrically connected to the electronic component 802 through the electronic component 760. Through the above design, the electrical signal transmission path, noise or chip offset can be reduced, thereby improving the quality of the electronic device, but is not limited to this.
[0117] Specifically, please refer to Figure 8 , electronic components 760, 761, and 762 are embedded in the insulating layer 710 of the interposer 700g. Figure 1F The electronic device 10 can be electrically connected to the electronic components 760, 761 and 762 through the connection pads 610, the conductive bumps 726 and the connection pads 731. The electronic components 760, 761 and 762 can be electrically connected to the circuit board 850 through the connection pads 730.
[0118] In some embodiments, at least one of the electronic component 760, the electronic component 761, and the electronic component 762 may also be replaced by Figure 1F An electronic device 10.
[0119] In summary, in the electronic device of the disclosed embodiment, since the first surface treatment process is a laser drilling process combined with a plasma etching process, the damage to the pad can be reduced or the residue in the opening can be reduced (for example, the silicon content of the interface between the first metal layer and the pad is less than 1%), thereby reducing the impedance (or contact resistance) between the pad and other conductive materials (for example, the first metal layer), improving the electrical properties of the pad, or improving the bonding ability between the pad and other conductive materials (for example, the first metal layer). In addition, since the second surface treatment process is a laser drilling process combined with a plasma etching process, the damage to the first metal layer in the circuit structure can be reduced or the residue in the through hole can be reduced (for example, the silicon content and / or carbon content of the interface between the second metal layer and the first metal layer is less than 1%), thereby reducing the impedance (or contact resistance) between the first metal layer and other conductive materials (for example, the second metal layer), improving the electrical properties of the first metal layer, or improving the bonding ability between the first metal layer and other conductive materials (for example, the second metal layer).
[0120] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the present disclosure, rather than to limit them. Although the present disclosure has been described in detail with reference to the aforementioned embodiments, those skilled in the art should understand that they can still modify the technical solutions described in the aforementioned embodiments, or replace some or all of the technical features therein by equivalents. However, these modifications or replacements do not cause the essence of the corresponding technical solutions to deviate from the scope of the technical solutions of the embodiments of the present disclosure.
Claims
1. An electronic device, It is characterized in that include: A chip comprises a base layer and at least one pad, wherein the at least one pad is disposed on a first side of the base layer; a protective layer disposed on the first side and having at least one opening, wherein the at least one opening exposes a portion of the at least one pad; A packaging layer, surrounding the chip and the protective layer; as well as A circuit structure, disposed on the packaging layer and electrically connected to the chip; The at least one pad has a concave surface, and a portion of the circuit structure contacts the concave surface.
2. The electronic device according to claim 1, It is characterized in that The depth of the concave surface of the at least one pad is 30 nanometers to 70 nanometers.
3. The electronic device according to claim 1, It is characterized in that The ratio of the depth of the concave surface of the at least one pad to the height of the at least one pad is 1% to 15%.
4. The electronic device according to claim 3, It is characterized in that The ratio is 3% to 10%.
5. The electronic device according to claim 1, It is characterized in that The at least one opening of the protection layer overlaps the concave surface of the at least one pad.
6. The electronic device according to claim 1, It is characterized in that The circuit structure comprises: A first metal layer having a recess; a first insulating layer, disposed on the first metal layer and comprising a through hole; and a second metal layer, disposed on the first insulating layer and electrically connected to the first metal layer through the through hole of the first insulating layer; and A second insulating layer, disposed on the second metal layer; The through hole overlaps the recess of the first metal layer.
7. The electronic device according to claim 6, It is characterized in that The depth of the recess is 0.1 micrometer to 5 micrometers.
8. The electronic device according to claim 6, It is characterized in that The first metal layer contacts the concave surface of the at least one pad.
9. The electronic device according to claim 6, It is characterized in that The second metal layer contacts the recess of the first metal layer.
10. The electronic device according to claim 1, It is characterized in that The chip also has a side surface connected to the first side, and the protection layer has a side surface. The side surface of the protection layer is an inclined surface, the junction between the side surface of the chip and the first side has a curved surface, and the packaging layer contacts the curved surface.