Preparation method of semiconductor structure
By forming a stacking layer and a dielectric layer on the substrate of the semiconductor device, partial stacking layer is removed to form conductive columns and alignment marks, and the alignment mark quality is improved by using the isolation material dielectric layer, which solves the high cost of semiconductor device production and the misalignment of conductive columns. The problem has improved the yield and efficiency of three-dimensional memory.
Patent Information
- Application Number
- CN202411178412.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-26
- Publication Date
- 2024-12-06
- Estimated Expiration
- 2044-08-26
AI Technical Summary
During the miniaturization of feature sizes, existing semiconductor devices have high production costs and low yield. The alignment mark quality and conductive column misalignment of three-dimensional memory are serious, which affects the performance and reliability of the memory.
By forming a stacking layer and a dielectric layer on the substrate, partial stacking layer is removed to expose the substrate, forming conductive posts and alignment marks, the quality and recognizability of the alignment marks are improved by using the isolation material dielectric layer to prevent the conductive posts from being misaligned.
Improves the yield of three-dimensional memory, improves the quality of alignment marks, ensures alignment signal quality, prevents conductive column misalignment, and improves the efficiency and reliability of the device.
Smart Images

Figure CN119095378A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the field of semiconductor technology, and in particular to a method for preparing a semiconductor memory structure. Background Art
[0002] With the continuous development of science and technology, the application of semiconductor devices is becoming more and more extensive. For example, a semiconductor device may include a transistor, which generally includes a source region, a drain region, a channel region between the source region and the drain region, a gate dielectric layer at least located on the channel region, and a gate located on the gate dielectric layer. The transistor uses the electric field formed by the gate to control the amount of induced charge in the channel region, thereby changing the state of the channel region, thereby achieving the effect of controlling the drain current.
[0003] As the characteristic size of semiconductor devices shrinks, the manufacturing cost of semiconductor devices is getting higher and higher, and the yield rate is getting lower and lower. The development of planar semiconductor devices has reached a bottleneck, and semiconductor devices with three-dimensional structures have become the current mainstream development trend, such as three-dimensional NAND flash memory. However, existing semiconductor devices still have many defects, and further improvements are needed to effectively improve the performance and reliability of related semiconductor devices. Summary of the invention
[0004] The object of the present invention is to provide a method for preparing a semiconductor structure, which can improve the quality of a first alignment mark, prevent the first conductive pillar and the second conductive pillar from being misaligned, and improve the yield of a three-dimensional memory.
[0005] In order to solve the above technical problems, the present invention provides a method for preparing a semiconductor memory, which may at least include:
[0006] providing a substrate comprising a first region and a second region;
[0007] forming a first stacked layer on the first region and the second region;
[0008] removing the first stacked layer on the second area to expose the substrate on the second area;
[0009] forming a first dielectric layer on the second region;
[0010] A plurality of first conductive pillars separated from each other are formed in the first stacked layer in the first region, and a plurality of first alignment marks are formed in the first dielectric layer in the second region.
[0011] In one optional example, a top surface of the first dielectric layer may be flush with a top surface of the first stacked layer.
[0012] In one optional example, the material of the first dielectric layer may include oxide.
[0013] In one optional example, after forming the first alignment mark, the method may further include:
[0014] forming a second stacked layer on the first stacked layer in the first region and on the first dielectric layer in the second region;
[0015] Etching a portion of the second stacked layer in the second region to form a plurality of grooves with the first alignment mark exposed at the bottom thereof in the second stacked layer in the second region;
[0016] A second dielectric layer is formed in the groove.
[0017] In one optional example, the top surface of the second dielectric layer may be flush with the top surface of the second stacked layer.
[0018] In one optional example, after forming the second dielectric layer, the method may further include:
[0019] A plurality of second conductive pillars separated from each other are formed in the second stacking layer in the first region, and a second alignment mark is formed in the second dielectric layer in the second region.
[0020] In one optional example, the step of forming the first alignment mark in the first dielectric layer, or the step of forming the second alignment mark in the second dielectric layer, may include:
[0021] Etching the first dielectric layer in the second region to form a plurality of first through holes spaced apart from each other in the first dielectric layer;
[0022] sequentially forming a metal oxide layer, a barrier layer and a metal layer in the first through hole, wherein the metal oxide layer, the barrier layer and the metal layer constitute the first alignment mark;
[0023] or,
[0024] Etching the second dielectric layer in the second region to form a plurality of second through holes spaced apart from each other in the second dielectric layer;
[0025] A metal oxide layer, a barrier layer and a metal layer are sequentially formed in the second through hole, and the metal oxide layer, the barrier layer and the metal layer constitute the second alignment mark.
[0026] In one optional example, projections of the first through hole and the second through hole in a first direction may not overlap, and the first direction is a direction perpendicular to the surface of the substrate.
[0027] In one optional example, the width of the groove in the second direction may be greater than the width of the first through hole or the second through hole in the second direction, and the second direction is a direction parallel to the surface of the substrate.
[0028] In one optional example, the first alignment mark and the second alignment mark may include grid-shaped marking strips.
[0029] In one optional example, the first stacked layer and the second stacked layer may include dielectric layers and conductive layers that are alternately arranged.
[0030] In one optional example, the material of the first dielectric layer and the material of the second dielectric layer may be the same.
[0031] The method for preparing a semiconductor structure provided by the present invention comprises: providing a substrate, the substrate comprising a first region and a second region, forming a first stacked layer located on the first region and the second region, removing the first stacked layer on the second region to expose the substrate on the second region, forming a first dielectric layer located on the second region, forming a plurality of mutually separated first conductive pillars located in the first stacked layer of the first region, and forming a plurality of first alignment marks located in the first dielectric layer of the second region. In the present invention, before forming the alignment mark (the first alignment mark or the second alignment mark), the stacked layer (the first stacked layer or the second stacked layer) on the second region is first removed, and then the dielectric layer (the first dielectric layer or the second dielectric layer) is deposited, so that the alignment mark quality is improved by forming the alignment mark in the dielectric layer of the isolation material, ensuring that the alignment signal quality meets the requirements, improving the recognizability of the alignment mark, thereby preventing the first conductive pillar and the second conductive pillar from being misaligned, and finally improving the yield of the three-dimensional memory. BRIEF DESCRIPTION OF THE DRAWINGS
[0032] The accompanying drawings are used to provide a further understanding of the present application and constitute a part of the specification. Together with the following specific embodiments, they are used to explain the present application but do not constitute a limitation to the present application. In the accompanying drawings:
[0033] Figure 1 A schematic diagram of a process for preparing a semiconductor structure provided in one embodiment of the present invention;
[0034] Figure 2 to Figure 11 The method for preparing a semiconductor structure provided in one embodiment of the present invention includes: Fig.12 Schematic diagram of the structure obtained in the direction of the AA tangent shown in .
[0035] Fig.12 To use Figure 1A top view of a plurality of first alignment marks and a second alignment mark formed by a method for manufacturing a semiconductor structure is shown.
[0036] Wherein, the accompanying drawings are marked as follows:
[0037] 100-substrate, 100A-first area of the substrate, 100B-second area of the substrate, 110-first etch barrier layer, 120-first stacked layer, 121-dielectric layer, 122-conductive layer, 130-first photoresist layer, 140-first dielectric layer, 150-first hard mask layer, 160-second photoresist layer, 101-first deep trench, OP1-first through hole, 170-first conductive column, 171-metal oxide layer, 172-barrier layer, 173-metal layer, Mark1-first alignment mark, 180-second etch barrier layer, 190-second stacked layer, 102-groove, 200-second dielectric layer, 210-second hard mask layer, 220-third photoresist layer, Mark2-second alignment mark.
[0038] In the drawings, the same reference numerals are used for the same components and the drawings are not drawn to scale. DETAILED DESCRIPTION
[0039] In order to make the technical solutions and advantages of the embodiments of the present invention clearer, the technical solutions of the present invention will be further described in detail below in conjunction with the accompanying drawings and embodiments. Although the exemplary implementation methods of the present invention are shown in the accompanying drawings, it should be understood that the present invention can be implemented in various forms and should not be limited by the implementation methods described here. On the contrary, these implementation methods are provided in order to enable a more thorough understanding of the present invention and to fully convey the scope of the present invention to those skilled in the art.
[0040] In the embodiments of the present invention, the terms "first", "second", etc. are used to distinguish similar objects, and are not necessarily used to describe a specific order or sequence. It should be noted that the technical solutions recorded in the embodiments of the present invention can be combined arbitrarily without conflict.
[0041] For ease of understanding, a first direction and a second direction are defined below, wherein the first direction is a direction perpendicular to the surface of the substrate 100; the second direction is a direction parallel to the surface of the substrate 100; and Figure 2 to Figure 12 The D1 direction and the D2 direction are defined in , wherein the D2 direction corresponds to the horizontal direction, the D1 direction corresponds to the vertical direction, and the D1 direction and the D2 direction, the horizontal direction and the vertical direction are perpendicular to each other.
[0042] Please refer to Figure 1 As shown, Figure 1 FIG. 1 is a flow chart of a method for preparing a semiconductor structure provided in one embodiment of the present invention. Figure 1 As shown, the method for preparing a semiconductor structure provided in an embodiment of the present invention comprises at least the following steps:
[0043] Step S101, providing a substrate, wherein the substrate comprises a first region and a second region;
[0044] Step S102, forming a first stacked layer on the first region and the second region;
[0045] Step S103, removing the first stacked layer on the second area to expose the substrate on the second area;
[0046] Step S104, forming a first dielectric layer on the second region;
[0047] Step S105 , forming a plurality of mutually separated first conductive pillars in the first stacked layer in the first region, and forming a plurality of first alignment marks in the first dielectric layer in the second region.
[0048] In the method for preparing the semiconductor structure provided by the present invention, before forming the alignment mark (the first alignment mark or the second alignment mark), the stacked layer (the first stacked layer or the second stacked layer) on the second area is first removed, and then the dielectric layer (the first dielectric layer or the second dielectric layer) is deposited, so that the alignment mark is formed in the dielectric layer whose material is the isolation material, thereby improving the quality of the alignment mark, ensuring that the quality of the alignment signal meets the requirements, and improving the recognizability of the alignment mark, thereby preventing the first conductive column and the second conductive column from being misaligned, and ultimately improving the yield of the three-dimensional memory.
[0049] In order to enable a person skilled in the art to which the present invention belongs to easily understand the method for preparing a semiconductor structure in the embodiment of the present invention, the method for preparing a semiconductor structure proposed by the present invention will be further described below in conjunction with various structural schematic diagrams of the preparation method during the preparation process. Figure 2 to Figure 11 The method for preparing a semiconductor structure provided in one embodiment of the present invention includes: Fig.12 The schematic diagram of the structure obtained in the direction of the AA tangent shown in the figure, Fig.12 To use Figure 1 A top view of a plurality of first alignment marks and second alignment marks formed by the method for preparing the semiconductor structure shown in FIG. Figure 2 to Figure 12 The method for preparing the semiconductor structure provided in this embodiment is described in detail.
[0050] Please refer to Figure 2, perform step S101: provide a substrate 100, and divide the substrate 100 into a first area 100A, for example, as a chip area for forming a transistor, and a second area 100B, for example, as a cutting road area adjacent to the chip area. In one embodiment, the substrate 100 is any suitable substrate material known in the art, for example, it can be a silicon substrate, a germanium substrate, a silicon germanium substrate, a silicon carbide substrate, an epitaxial silicon substrate (Epitaxial Silicon Substrate), a silicon on insulator (Silicon on Insulator, referred to as SOI) substrate or a germanium on insulator (Germanium on Insulator, referred to as GOI) substrate, or a substrate composed of other suitable materials, but not limited thereto. Those skilled in the art should easily understand that various required active components and / or passive components, such as transistors and / or circuits (not shown) can be further formed on or in the substrate according to actual device requirements, but not limited thereto.
[0051] Please continue to refer to Figure 2 , execute step S102: use at least one of the deposition processes such as physical vapor deposition, chemical vapor deposition, atomic layer deposition, etc. to sequentially form a first etch stop layer 110 and a first stack layer 120 on the surface of the substrate 100 (including the substrate surfaces corresponding to the first area 100A and the second area 100B, respectively). In one embodiment, the first etch stop layer 110 may include a single layer or multiple layers of metal oxide materials. Applicable metal oxide materials may include, for example, aluminum oxide, titanium oxide, tantalum oxide, tungsten oxide or copper oxide, preferably aluminum oxide, but not limited thereto. The first stack layer 120 includes a plurality of dielectric layers 121 and a plurality of conductive layers 122 alternately arranged. And each dielectric layer 121 and the conductive layer 122 above it together form a group of dielectric-conductive layer pairs. Among them, the specific number of dielectric-conductive layer pairs can be adjusted according to actual needs, and is not limited to. Figure 2 The material of the dielectric layer 121 may be, for example, silicon oxide, silicon nitride, silicon oxynitride or any combination thereof, but is not limited thereto, and the material of the conductive layer 122 may be, for example, aluminum, titanium, tantalum, tungsten, copper, titanium nitride, titanium carbide, tantalum nitride, titanium tungsten, titanium and titanium nitride, polysilicon, doped silicon, metal silicide or any combination thereof, preferably including tungsten, but is not limited thereto.
[0052] Please refer to Figure 3 , perform step S103: using the above deposition process, first form a top surface of the first stacked layer 120 corresponding to the first area 100A and expose the top surface of the first stacked layer 120 corresponding to the second area 100B, for example, with a thickness of A photoresist layer 130 is formed on the left and right sides of the substrate 100, and then an etching process, such as at least one of a dry etching process and a wet etching process, is used to remove the corresponding first stacked layer 120 on the exposed second area 100B with the photoresist layer 130 as a mask to expose the corresponding substrate 100 on the second area 100B, and further remove the photoresist layer 130.
[0053] Please refer to Figure 4 , perform step S104: use at least one of the above deposition processes to form a first dielectric layer 140 on the substrate 100 in the second area 100B; in one embodiment, the top surface of the first dielectric layer 140 located on the second area 100B can be flush with the top surface of the first stacked layer 120 located on the first area 100A, and the material of the first dielectric layer 140 is preferably an oxide, such as silicon dioxide. Obviously, in the embodiment of the present invention, after forming the corresponding first stacked layer 120, the first alignment mark will not be directly formed in the first stacked layer 120 in the first area 100A, but the first stacked layer 120 in the second area 100B is first removed, and then the first dielectric layer 140 flush with the top surface of the first stacked layer 120 is formed, that is, to prepare for the subsequent formation of the alignment mark in the dielectric layer.
[0054] Please refer to Figure 5 , following step S104, at least one of the above deposition processes may be further used to form a first hard mask layer 150 and a second photoresist layer 160 stacked from bottom to top on the top surfaces of the first stacked layer 120 on the first area 100A and the first dielectric layer 140 on the second area 100B, and a plurality of through hole patterns are provided in the second photoresist layer 160. In one embodiment, the material of the first hard mask layer 150 may be, for example, a dielectric material such as silicon oxide, silicon nitride, silicon oxynitride, or any combination thereof, but is not limited thereto, and the material of the second photoresist layer 160 may be the same as or different from that of the first photoresist layer 130. Furthermore, the size of the corresponding through hole pattern of the second photoresist layer 160 on the first area 100A is different from that of the corresponding through hole pattern on the second area 100B, for example, the width along the second direction D2 may be different. Exemplarily, if the corresponding through-hole pattern of the second photoresist layer 160 in the first area 100A is called a first through-hole pattern, and the corresponding through-hole pattern of the second photoresist layer 160 in the second area 100B is called a second through-hole pattern, then the width of the first through-hole pattern in the second direction D2 (for example, about 63 nm) is smaller than the width of the second through-hole pattern in the second direction D2 (for example, about 240 nm), but is not limited to this.
[0055] Please refer to Figure 6, following step S104, using the second photoresist layer 160 as a mask, the first hard mask layer 150 of the first area 100A and the first stacked layer 120 and the first etch stop layer 110 thereunder, as well as the first hard mask layer 150 of the second area 100B and a portion of the first dielectric layer 140 thereunder are etched along the first direction D1, so as to form a plurality of first deep trenches 101 on the first area 100A, and simultaneously form a plurality of first through holes OP1 on the second area 100B, and then the second photoresist layer 160 may be further removed. In one embodiment, the plurality of first deep trenches 101 are subsequently used to form first conductive pillars, and the plurality of first deep trenches 101 may be arranged at intervals from each other along the second direction D2, and the plurality of first through holes OP1 are subsequently used to form first alignment marks, and the plurality of first through holes OP1 may be arranged at intervals from each other along the second direction D2, but the present invention is not limited thereto. Obviously, the width of the first deep trenches 101 in the second direction D2 is smaller than the width of the first through holes OP1 in the second direction D2.
[0056] Please refer to Figure 7, perform step S105: using at least one of the deposition processes described above, form a first conductive pillar 170 in the first deep trench 101, and form a first alignment mark Mark1 in the first through hole OP1. Specifically, the first conductive pillar 170 may include a metal oxide layer 171, a barrier layer 172, and a metal layer 173 stacked in sequence, the metal oxide layer 171 is located on the sidewall and part of the bottom of the first deep trench 101, so as to exemplarily form two oppositely arranged L-shaped structures, the barrier layer 172 is located on the surface of the metal oxide layer 171 and on the substrate 100 at the bottom of the first deep trench 101 exposed therefrom, and the metal layer 173 is located on the barrier layer 172 and fills the remaining space of the first deep trench 101. In one embodiment, the two corners of the bottom of the barrier layer 172 and the metal layer 173 are both recessed in a direction close to each other; the material of the metal oxide layer 171 may include hafnium silicon oxide, hafnium oxide, zirconium oxide, tantalum oxide, titanium oxide, etc. In this way, the metal oxide layer 171 has a higher dielectric constant, which can improve its insulation performance. The material of the barrier layer 22 can include titanium nitride, tantalum nitride, etc., so as to separate the metal oxide layer 171 from the metal layer 173, and prevent the metal ions in the metal layer 173 from diffusing into the metal oxide layer 171, thereby ensuring the insulation performance of the metal oxide layer 171. The material of the metal layer 173 is a metal material, for example, including tungsten and its alloy, but not limited to this. The shape of the first alignment mark Mark1 can be a gate-shaped mark bar, and also includes a metal oxide layer 171, a barrier layer 172 and a metal layer 173 stacked in sequence, and the materials, mutual positional relationship and structural shape of each layer of the metal oxide layer 171, the barrier layer 172 and the metal layer 173 are the same as the metal oxide layer 171, the barrier layer 172 and the metal layer 173 in the first conductive column 170, which will not be repeated here.
[0057] Obviously, the first alignment mark Mark1 in the embodiment of the present invention is specifically formed in the first dielectric layer 140 whose material is an isolation material. Under this setting, the metal layer 170 (such as metal tungsten) in the first alignment mark Mark1 can be effectively isolated by the first dielectric layer 140 (such as silicon dioxide), so as to improve the quality of the alignment mark, ensure that the quality of the alignment signal meets the requirements, and improve the recognizability of the alignment mark.
[0058] Please refer to Figure 8, following step S105, the above deposition process can be further used to sequentially form a second etch stop layer 180 and a second stack layer 190 on the top surface of the first stack layer 120 on which the first conductive pillar 170 is formed and on the top surface of the first dielectric layer 140 on which the first alignment mark Mark1 is formed. In one embodiment, the material of the second etch stop layer 180 can be the same as the material of the first etch stop layer 110 (for example, aluminum oxide), but is not limited thereto. The material and structure of the second stack layer 190 can also be the same as the material and structure of the first stack layer 120, for example, a plurality of groups of dielectric-conductive layer pairs composed of a plurality of dielectric layers and a plurality of conductive layers alternately arranged, and the number of dielectric-conductive layer pairs included in the second stack layer 190 and the first stack layer 120 can be adjusted to be the same or different according to actual needs, not to mention the number of dielectric-conductive layer pairs. Figure 2 The following are limited to those shown.
[0059] Please refer to Fig. 9 , proceeding to step S105, a portion of the second stacked layer 190 in the second area 100B and the second etch stop layer 180 thereunder are etched away by an etching process, so as to form a plurality of grooves 102 with the first alignment mark Mark1 exposed at the bottom in the second stacked layer 190 and the second etch stop layer 180 in the second area 100B. In one embodiment, the width of the groove 102 in the second direction D2 is greater than the width of the first through hole OP1 in the second direction D2, and is also greater than the width of the first alignment mark Mark1 in the second direction D2, so as to prepare for the subsequent formation of a plurality of second alignment marks Mark2.
[0060] Please refer to Fig.10 , proceeding to step S105, the groove 102 is filled by a deposition process to form a second dielectric layer 200 whose top surface is flush with the top surface of the second stacked layer 190 on the first region 100A, and the second dielectric layer 200 is also flush with the top surface of the second stacked layer 190 remaining on the second region 100B. In one embodiment, the material of the second dielectric layer 190 can be the same as that of the first dielectric layer 140 (e.g., oxide, silicon dioxide), but is not limited thereto.
[0061] Please refer to Fig.11 , and combined with Fig.12, following step S105, a second hard mask layer 210 and a third photoresist layer 220 are further sequentially deposited on the first region 100A and the second region 100B by a deposition process, so as to further form a plurality of second conductive pillars (not shown) separated from each other in the second stacked layer 190 of the first region 100A by the same process as that for forming the first conductive pillar 170 and the first alignment mark Mark1, and to form a plurality of second alignment marks Mark2 (set apart from each other) separated from each other in the second dielectric layer 200. Fig.11 The same process technology is not shown here.
[0062] It should be noted that a plurality of through-hole patterns are also provided in the third photoresist layer 220, and a portion of the plurality of through-hole patterns is also located in the first area 100A, and another portion is located in the second area 100B, and the width of the through-hole pattern located in the first area 100A along the second direction D2 is also smaller than the width of the through-hole pattern located in the second area 100B along the second direction D2. The through-hole pattern located in the first area 100A in the third photoresist layer 220 is used to form a corresponding second conductive column, and the through-hole pattern located in the second area 100B is used to form a corresponding second through hole (not shown, located in the second dielectric layer 200) and a second alignment mark Mark2 filled in the second through hole. In addition, in combination with Fig.12 As shown, the projections of the first through hole OP1 formed with the first alignment mark Mark1 and the second through hole formed with the second alignment mark Mark2 in the first direction D1 do not overlap. Obviously, since the first alignment mark Mark1 and the second alignment mark Mark2 in the embodiment of the present invention are respectively formed in the dielectric layer of the isolation material, the quality of the first alignment mark Mark1 and the second alignment mark Mark2 are improved, so that the first conductive pillar and the second conductive pillar formed based on the first alignment mark Mark1 and the second alignment mark Mark2 can be prevented from being misaligned.
[0063] In summary, the method for preparing a semiconductor structure provided by the present invention includes: providing a substrate, the substrate including a first region and a second region, forming a first stacked layer located on the first region and the second region, removing the first stacked layer on the second region to expose the substrate on the second region, forming a first dielectric layer located on the second region, forming a plurality of mutually separated first conductive pillars located in the first stacked layer of the first region, and forming a plurality of first alignment marks located in the first dielectric layer of the second region. In the present invention, before forming the alignment mark (the first alignment mark or the second alignment mark), the stacked layer (the first stacked layer or the second stacked layer) on the second region is first removed, and then the dielectric layer (the first dielectric layer or the second dielectric layer) is deposited, so that the alignment mark quality is improved by forming the alignment mark in the dielectric layer of the isolation material, ensuring that the alignment signal quality meets the requirements, improving the recognizability of the alignment mark, thereby preventing the first conductive pillar and the second conductive pillar from being misaligned, and finally improving the yield of the three-dimensional memory.
[0064] It should be noted that, in this article, relational terms such as first and second, etc. are only used to distinguish one entity or operation from another entity or operation, and do not necessarily require or imply any such actual relationship or order between these entities or operations. Moreover, the terms "include", "comprise" or any other variants thereof are intended to cover non-exclusive inclusion, so that a process, method, article or device including a series of elements includes not only those elements, but also other elements not explicitly listed, or also includes elements inherent to such process, method, article or device. In the absence of further restrictions, the elements defined by the sentence "comprise a ..." do not exclude the existence of other identical elements in the process, method, article or device including the elements.
[0065] Each embodiment in this specification is described in a related manner, and the same or similar parts between the embodiments can be referred to each other, and each embodiment focuses on the differences from other embodiments. In particular, for the device, electronic device, and computer-readable storage medium embodiments, since they are basically similar to the method embodiments, the description is relatively simple, and the relevant parts can be referred to the partial description of the method embodiments.
[0066] The above description is only a preferred embodiment of the present invention and is not intended to limit the protection scope of the present invention. Any modification, equivalent replacement, improvement, etc. made within the spirit and principle of the present invention are included in the protection scope of the present invention.
Claims
1. A method for preparing a semiconductor structure, characterized in that: include: providing a substrate comprising a first region and a second region; forming a first stacked layer on the first region and the second region; removing the first stacked layer on the second area to expose the substrate on the second area; forming a first dielectric layer on the second region; A plurality of first conductive pillars separated from each other are formed in the first stacked layer in the first region, and a plurality of first alignment marks are formed in the first dielectric layer in the second region.
2. The method for preparing a semiconductor structure according to claim 1, characterized in that: The top surface of the first dielectric layer is flush with the top surface of the first stacked layer.
3. The method for preparing a semiconductor structure according to claim 1, characterized in that: The material of the first dielectric layer includes oxide.
4. The method for preparing a semiconductor memory according to claim 2, wherein: After forming the first alignment mark, the method further includes: forming a second stacked layer on the first stacked layer in the first region and on the first dielectric layer in the second region; Etching a portion of the second stacked layer in the second region to form a plurality of grooves with the first alignment mark exposed at the bottom thereof in the second stacked layer in the second region; A second dielectric layer is formed in the groove.
5. The method for preparing a semiconductor memory according to claim 4, wherein: The top surface of the second dielectric layer is flush with the top surface of the second stacked layer.
6. The method for preparing a semiconductor memory according to claim 5, wherein: After forming the second dielectric layer, the method further includes: A plurality of second conductive pillars separated from each other are formed in the second stacking layer in the first region, and a second alignment mark is formed in the second dielectric layer in the second region.
7. The method for preparing a semiconductor structure according to claim 1 or 6, characterized in that: The step of forming the first alignment mark in the first dielectric layer, or forming the second alignment mark in the second dielectric layer, comprises: Etching the first dielectric layer in the second region to form a plurality of first through holes spaced apart from each other in the first dielectric layer; sequentially forming a metal oxide layer, a barrier layer and a metal layer in the first through hole, wherein the metal oxide layer, the barrier layer and the metal layer constitute the first alignment mark; or, Etching the second dielectric layer in the second region to form a plurality of second through holes spaced apart from each other in the second dielectric layer; A metal oxide layer, a barrier layer and a metal layer are sequentially formed in the second through hole, and the metal oxide layer, the barrier layer and the metal layer constitute the second alignment mark.
8. The method for preparing a semiconductor memory according to claim 7, wherein: Projections of the first through hole and the second through hole in a first direction do not overlap, and the first direction is a direction perpendicular to the surface of the substrate.
9. The method for preparing a semiconductor structure according to claim 8, characterized in that: The width of the groove in the second direction is greater than the width of the first through hole or the second through hole in the second direction, and the second direction is a direction parallel to the surface of the substrate.
10. The method for preparing a semiconductor structure according to claim 7, characterized in that: The first alignment mark and the second alignment mark include grid-shaped mark bars.
11. The method for preparing a semiconductor memory according to claim 7, wherein: The first stacked layer and the second stacked layer include dielectric layers and conductive layers that are alternately arranged.
12. The method for preparing a semiconductor structure according to claim 4, characterized in that: The material of the first dielectric layer is the same as that of the second dielectric layer.
Citation Information
Patent Citations
Alignment mark and manufacturing method thereof
CN102945842A
Semiconductor structure and manufacturing method thereof
CN112216790A
Methods of manufacturing semiconductor devices using alignment marks to align layers
US20160027739A1
Semiconductor memory device and fabrication method thereof
US20200176510A1
Semiconductor device having integral alignment marks with decoupling features and method for fabricating the same
US20230178494A1