A method for processing hidden patterns and a product with hidden patterns
By using film and screen printing technology to prepare hidden patterns, the problems of high equipment cost and environmental pollution have been solved, achieving efficient and low-cost preparation of hidden patterns and improved visual effects.
Patent Information
- Application Number
- CN202411472961.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-10-22
- Publication Date
- 2026-11-17
- Estimated Expiration
- 2044-10-22
AI Technical Summary
Existing hidden pattern coating processes and equipment are costly, require long preparation times, and pose environmental pollution problems.
Hidden patterns are prepared using film and screen printing technology. Through the combination of multiple layers of ink and metal film, combined with baking, coating and lamination processes, hidden pattern layers and visible pattern layers are formed, avoiding the use of high-cost photolithography equipment and high-pollution processes.
It reduces the cost and time of mold making and prototyping, reduces environmental pollution, achieves efficient preparation of hidden patterns, and enhances the visual effect through the light transmittance and texture of the metal film.
Smart Images

Figure CN119305326B_ABST
Abstract
Description
Technical Field
[0001] This invention belongs to the field of vacuum coating technology, and particularly relates to a method for processing hidden patterns and a product with hidden patterns. Background Technology
[0002] Traditional vacuum coating processes evaporate or sputter metals, alloys, or compounds in a vacuum, causing them to solidify and deposit on the material being coated (called a substrate, sheet, or matrix), forming a thin film on the surface of the material. This gives the material many new and good physical and chemical properties, and also enriches the appearance of the material. However, this process also places increasingly higher demands on the processing equipment.
[0003] The existing hidden pattern coating process usually uses photolithography equipment to process nanoimprint master molds. This process is costly, takes a long time to make molds and samples, and is also harmful to the environment. Summary of the Invention
[0004] The purpose of this invention is to overcome the shortcomings of the prior art and provide a method for processing hidden patterns and a product with hidden patterns, which solves the problems of high equipment cost, long preparation time and pollution in the prior art for the coating process of hidden patterns.
[0005] To achieve the above objectives, the technical solution adopted by the present invention is as follows: Firstly, a method for processing hidden patterns is provided, including the following steps: Draw graphic digital images; The digital image of the pattern is output onto a film. A screen printing plate is made from the prepared film; The screen printing plate prints pattern ink on the surface of the sheet, and the pattern ink forms a hidden pattern layer on the surface of the sheet. The sheet on which the hidden pattern layer is formed is baked to dry the pattern ink. A metal film is uniformly deposited on the surface of the dried sheet and the pattern ink; A protective film capable of adhering to the surface of the metal film is laid on the sheet, and the metal film and the pattern ink on the sheet are peeled off through the protective film; A base color ink is printed on the side of the protective film opposite to the metal film and the pattern ink, and the base color ink forms an external pattern layer on the protective film. The protective film forming the external pattern layer is laminated on both sides, and the laminated protective film is cut using a forming device to obtain the finished product.
[0006] Optionally, the film has an OD value ≥ 3.5.
[0007] Optionally, the sheet on which the hidden pattern layer is formed is baked at a temperature of 75°C to 85°C for a time of 27 to 35 minutes.
[0008] Optionally, the adhesive strength of the protective film is ≥600gf / 25mm.
[0009] Optionally, the pattern ink is a peelable ink.
[0010] Optionally, the sheet material is any one or more of PC material, PET material, aluminum plate, and acrylic.
[0011] Optionally, the light transmittance of the metal film is 40% to 70%.
[0012] In a second aspect, a hidden pattern product is provided, which is manufactured using the hidden pattern processing method described in the first aspect. The hidden pattern product includes a hidden pattern layer and an exposed pattern layer, a protective film is disposed between the hidden pattern layer and the exposed pattern layer, and a metal film is disposed between the hidden pattern layer and the protective film.
[0013] Optionally, a laminating protective layer is provided on the side of the hidden pattern layer and the visible pattern layer opposite to the protective film.
[0014] Compared with the prior art, the beneficial effects achieved by the present invention are as follows: (1) Compared with other hidden texture processing technology, the hidden pattern processing method in this technical solution does not require the use of high-priced photolithography equipment to process nano-imprint master molds. The effect of hidden patterns can be achieved through a variety of traditional and mature printing technologies, which can effectively reduce the production cost and time cost of mold making and sampling. Moreover, from the perspective of environmental impact, it does not involve high pollution such as etching, plating removal, and chemical film removal. (2) By utilizing the light transmittance of the metal film, the hidden pattern layer can be made visible at different angles under different lighting conditions, and the hidden pattern layer can have a certain metallic texture, making the hidden pattern product of this material more prominent in terms of both hiding and display effects. Attached Figure Description
[0015] The present invention will be further described below with reference to the accompanying drawings and embodiments.
[0016] Figure 1 This is a flowchart illustrating the hidden pattern processing method in a preferred embodiment of the present invention; Figure 2 This is a structural schematic diagram of the hidden pattern product in a preferred embodiment of the present invention; The layers are: 1. Hidden pattern layer; 2. Exposed pattern layer; 3. Protective film; 4. Metallic film; 5. Adhesive protective layer. Detailed Implementation
[0017] The present invention will now be described in further detail with reference to the accompanying drawings and embodiments. These drawings are simplified schematic diagrams, which are only used to illustrate the basic structure of the present invention and therefore only show the components relevant to the present invention.
[0018] It should be noted that if directional indicators (such as up, down, bottom, top, etc.) are involved in this embodiment, these directional indicators are only used to explain the relative positional relationship and movement of the components in a specific posture. If the specific posture changes, the directional indicators will also change accordingly. The terms "first" and "second" are used for descriptive purposes only and should not be construed as indicating or implying relative importance or implicitly specifying the number of indicated technical features. Therefore, features defined with "first" and "second" may explicitly or implicitly include one or more of that feature. Unless otherwise explicitly specified and limited, the terms "set," "connected," and "linked" should be interpreted broadly. For example, they can refer to a fixed connection, a detachable connection, or an integral connection; they can refer to a direct connection or an indirect connection through an intermediate medium; they can refer to the internal connection of two components. For those skilled in the art, the specific meaning of the above terms in this invention can be understood according to the specific circumstances. Example 1
[0019] like Figure 1 As shown, a method for processing hidden patterns includes the following steps: Draw graphic digital images; The digital image of the pattern is output onto a film. A screen printing plate is made from the prepared film; Printing pattern ink on the surface of the sheet using the screen printing plate, thereby forming a hidden pattern layer 1 on the surface of the sheet using the pattern ink; The sheet on which the hidden pattern layer 1 is formed is baked to dry the pattern ink. A metal film 4 is uniformly deposited on the surface of the dried sheet and the pattern ink; A protective film 3 that can adhere to the surface of the metal film 4 is laid on the sheet, and the metal film 4 and the pattern ink on the sheet are peeled off through the protective film 3; A base color ink is printed on the side of the protective film 3 that is opposite to the metal film 4 and the pattern ink, and the base color ink forms an external pattern layer 2 on the protective film 3; The protective film 3 that forms the external pattern layer 2 is laminated on both sides, and the laminated protective film 3 is cut by a forming device to obtain the finished product.
[0020] Specifically, digital image processing is quick, requires no mold making or proofing, and can be created in various styles as needed. The digital image can be output to a film using a film output machine, and different mesh counts of screen printing plates can be made based on the film exposure to achieve different levels of detail. Then, a semi-automatic screen printing machine uses these screen printing plates to print the image ink onto the film. After the ink dries, it forms a hidden image on the film. Finally, a vacuum coating machine uses existing technology to coat the film and the remaining image ink with one or more layers of metal film. 4. Subsequently, the surface of the sheet is surface-treated using a laminating machine in the prior art, so that the protective film 3 can adhere to the metal film 4 and / or the dried graphic ink. After lamination, the laminating machine can peel the protective film 3 off the sheet at the discharge port and perform a winding operation. Since the adhesion strength between the metal film 4 and the graphic ink, and the adhesion strength between the protective film 3 and the metal film 4 and the graphic ink are much greater than the adhesion strength between the graphic ink and the sheet, when the protective film 3 is peeled off, the metal film 4 and the graphic ink will also be completely peeled off from the sheet surface, ensuring that all graphic ink within the range is peeled off without any residue. Subsequently, a semi-automatic screen printing machine is used to print the base color ink on the surface of the protective film 3 torn from the sheet. Then, a laminating machine is used to perform a double-sided lamination operation on the protective film 3 after the base color ink has been printed, to protect the formed hidden pattern layer 1 and the visible pattern layer 2. Finally, the protective film 3, after the double-sided lamination operation, is cut using existing forming equipment to meet usage requirements. Because the metal film 4 has a certain light transmittance, the hidden pattern layer 1 formed by the graphic ink can be observed through the metal film 4 at different viewing angles, and the hidden graphic area also has a distinct metallic texture, resulting in a noticeable effect.
[0021] Meanwhile, compared with other hidden texture processing technologies in the industry, it does not require the use of high-priced photolithography equipment to process nano-imprint master molds, which can effectively reduce the production cost and time cost of mold making and prototyping. Moreover, from the perspective of environmental impact, the semi-automatic screen printing machine, film output machine, laminating machine and forming equipment are all relatively mature printing equipment in the existing technology, and there is no high pollution such as etching, plating removal and chemical film removal.
[0022] As mentioned above, the transmittance can be adjusted according to the required concealment effect. The coating target material used in the vacuum coating machine is mainly composed of titanium powder, silicon powder, and titanium powder, which can effectively improve the uniformity of the metal film 4. At the same time, the number, order, and thickness of the metal film 4 should be adjusted according to the transmittance requirements. The lower the transmittance, the stronger the concealment effect, and vice versa. In this technical solution, preferably, the transmittance of the metal film 4 is 40% to 70%.
[0023] Furthermore, the film used in the digital image input must have an OD value ≥ 3.5, and the film surface must be free of scratches and creases. A higher OD value means the film has a stronger light-blocking effect, ensuring that only specific areas of light pass through, achieving precise exposure control. At the same time, a higher OD value can effectively reduce the impact of stray light on exposure, resulting in clearer images and better product quality.
[0024] The sheet material after the hidden pattern layer 1 is formed on its surface is baked at a temperature of 75°C to 85°C for 27 to 35 minutes. Within this range, the drying process of the pattern ink can be effectively accelerated. Compared with lower or higher baking temperatures and longer or shorter baking times, this range can significantly shorten the production cycle and improve printing production efficiency while ensuring the drying quality of the pattern ink. Preferably, in this technical solution, the sheet material is baked at 80°C for 30 minutes.
[0025] Preferably, the protective film 3 has an adhesion strength ≥ 600gf / 25mm, enabling it to adhere firmly to the surface of the metal film 4. This ensures that when the protective film 3 is peeled off, all graphic ink within the specified area will be completely removed without residue. Simultaneously, the high adhesion of the protective film 3 allows it to remain stable in normal production environments, ensuring its continuous and stable function throughout the entire production process.
[0026] In this embodiment, the pattern ink is a peelable ink, and the sheet material is any one or more of PC material, PET material, aluminum plate, and acrylic. Example 2
[0027] like Figure 2 As shown, based on Embodiment 1, a hidden pattern product is realized by the aforementioned hidden pattern processing method, including a hidden pattern layer 1 and an exposed pattern layer 2, a protective film 3 is provided between the hidden pattern layer 1 and the exposed pattern layer 2, a metal film 4 is provided between the hidden pattern layer 1 and the protective film 3, and a laminating protective layer 5 is provided on the side of the hidden pattern layer 1 and the exposed pattern layer 2 opposite to the protective film 3.
[0028] Specifically, the metal film 4 is a single layer or multiple layers, and the adhesive protective layer 5 is the product of double-sided lamination on the protective film 3 after the printing of the base color ink by the laminating machine. It can protect the hidden pattern layer 1 and the visible pattern layer 2.
[0029] Based on the preferred embodiments of the present invention described above, those skilled in the art can make various changes and modifications without departing from the inventive concept. The technical scope of this invention is not limited to the contents of the specification, but must be determined according to the scope of the claims.
Claims
1. A method for processing hidden patterns, characterized in that, Includes the following steps: Draw graphic digital images; The digital image of the pattern is output onto a film. A screen printing plate is made from the prepared film; Printing pattern ink on the sheet surface of the screen printing plate, thereby forming a hidden pattern layer on the surface of the sheet through the pattern ink (1); The sheet on which the hidden pattern layer (1) is formed is baked to dry the pattern ink; A metal film is uniformly deposited on the surface of the dried sheet and the pattern ink (4). A protective film (3) that can adhere to the surface of the metal film (4) is laid on the sheet, and the metal film (4) and the pattern ink on the sheet are peeled off through the protective film (3); A base color ink is printed on the side of the protective film (3) that is opposite to the metal film (4) and the pattern ink, and an external pattern layer (2) is formed on the protective film (3) by the base color ink. The protective film (3) forming the external pattern layer (2) is laminated on both sides, and the laminated protective film (3) is cut by a forming device to obtain the finished product; The film has an OD value ≥ 3.5; The pattern ink is a peelable ink; The light transmittance of the metal film (4) is 40% to 70%.
2. The method for processing hidden patterns according to claim 1, characterized in that: The sheet on which the hidden pattern layer (1) is formed is baked at a temperature of 75°C to 85°C for 27 to 35 minutes.
3. The method for processing hidden patterns according to claim 1, characterized in that: The adhesive force of the protective film (3) is ≥600gf / 25mm.
4. The method for processing hidden patterns according to claim 1, characterized in that: The sheet material is any one or more of PC material, PET material, aluminum plate, and acrylic.
5. A product with a hidden pattern, characterized in that: The product is manufactured using the hidden pattern processing method described in any one of claims 1-4. The hidden pattern product includes a hidden pattern layer (1) and an exposed pattern layer (2). A protective film (3) is provided between the hidden pattern layer (1) and the exposed pattern layer (2). A metal film (4) is provided between the hidden pattern layer (1) and the protective film (3).
6. The hidden pattern product according to claim 5, characterized in that: The hidden pattern layer (1) and the visible pattern layer (2) are provided with a mounting protective layer (5) on the side opposite to the protective film (3).
Citation Information
Patent Citations
Screen printing plate manufacturing method
CN106274027A
Intelligent surface with metal appearance and automobile
CN116252723A