Packaging method and packaging equipment for cold film pasting electrode frame

By using a vacuum adsorption platform and positioning mechanism to fix the film layer during the cold-paste electrode frame packaging, and using the fill layer to eliminate the bonding height difference, the problem of wrinkles and uneven stress in the cold-paste packaging is solved, and more stable membrane electrode performance is achieved.

CN119542454APending Publication Date: 2025-02-28FTXT ENERGY TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202311114601.0
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2023-08-31
Publication Date
2025-02-28

AI Technical Summary

Technical Problem

In the existing cold-patch packaging method, the three-layer film structure is prone to wrinkles during the bonding process with the frame film, resulting in incomplete sealing and air leakage, and the stress is uneven when the female and anode frame is rolled and bonded, which affects the performance of the film electrode.

Method used

The frame film and three-layer film structure are fixed by a vacuum adsorption platform and positioning mechanism, and the reaction area of ​​the frame film is filled through the filling layer to eliminate the height difference during the bonding process, ensure that the bond is flat and wrinkled, and the frame film is subjected to uniform stress.

Benefits of technology

It effectively reduces the risk of air leakage of the membrane electrode, ensures that the reaction area remains unchanged, and improves the stability of the membrane electrode performance.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119542454A_ABST
    Figure CN119542454A_ABST
Patent Text Reader

Abstract

The invention provides a packaging method and packaging equipment for a cold film electrode frame, and relates to the technical field of fuel cells. The packaging method of the cold film electrode frame comprises the following steps: cutting to obtain a frame film of a hollow reaction area; fixing the frame film on a first vacuum adsorption platform according to the position of a first positioning mechanism, and filling a reaction area of the frame film with a filling layer; and the cut three-layer film structure is fixed to the second vacuum adsorption platform, a protective film of the frame film on the first vacuum adsorption platform is removed, after the first positioning mechanism is aligned, the first vacuum adsorption platform is turned over, and the second vacuum adsorption platform is moved to the position below the first vacuum adsorption platform and is jacked or rolled. According to the packaging method of the cold pasting film electrode frame provided by the invention, the technical problem of poor cold pasting packaging effect in the prior art is solved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of fuel cells, and in particular to a packaging method and packaging equipment for a cold film electrode frame. Background Art

[0002] The membrane electrode is the core component of the fuel cell, including the frame membrane, gas diffusion layer and three-layer membrane structure, where the three-layer membrane structure is a proton exchange membrane and an anode catalyst layer and a cathode catalyst layer respectively transferred on both sides of the proton exchange membrane by coating. The development technology of the membrane electrode includes pulping, coating, transfer, frame packaging and gas diffusion layer packaging. The frame packaging includes hot pressing packaging and cold pasting packaging. Cold pasting packaging uses pressure-sensitive adhesive frame membrane materials to directly encapsulate the frame membrane by controlling the bonding pressure and bonding speed.

[0003] The existing cold-stick packaging steps include: a punching machine punches a large piece of frame film to obtain a small piece of frame film with a hollowed-out reaction area, and a membrane electrode requires two symmetrical anode and cathode frame films; the punching machine punches the rolled three-layer membrane structure into a size larger than the frame reaction area; the three-layer membrane structure, the cathode frame film and the anode frame film are placed on the left, middle and right platforms of the bonding equipment respectively; the middle platform is turned over to make the cathode frame with glue face downward, the left platform is driven to move to the bottom of the middle platform and raised, so that the three-layer membrane structure is bonded to the cathode frame reaction area and then reset; the position of the three-layer membrane structure is adjusted, and the middle platform is turned over, and the right platform is driven to move to the bottom of the middle platform and raised, so that the anode frame is rolled from left to right and bonded to the cathode frame of the middle platform to achieve the purpose of packaging; the punching equipment punches water vapor holes on the packaged membrane electrode.

[0004] During the cold-sticking packaging process, wrinkles will appear when the three-layer membrane structure is lifted and bonded to the frame film. If the wrinkles are severe, it will lead to incomplete sealing and air leakage. Or, during the rolling and bonding process of the anode and cathode frames, the reaction zone area is squeezed and reduced due to uneven force, which affects the performance of the membrane electrode and increases the difficulty of encapsulating the gas diffusion layer. Summary of the invention

[0005] The object of the present invention is to provide a packaging method and packaging equipment for a cold-stick film electrode frame, so as to alleviate the technical problem of poor cold-stick packaging effect existing in the prior art.

[0006] In order to solve the above technical problems, the technical solution provided by the present invention is:

[0007] In a first aspect, the packaging method of the cold film electrode frame provided by the present invention comprises:

[0008] Cutting to obtain a frame film with a hollowed-out reaction area;

[0009] The frame film is fixed on the first vacuum adsorption platform according to the position of the first positioning mechanism, and the reaction area of ​​the frame film is filled with a filling layer;

[0010] The cut three-layer film structure is fixed on the second vacuum adsorption platform, the protective film of the frame film on the first vacuum adsorption platform is removed, and after the first positioning mechanism is aligned, the first vacuum adsorption platform is turned over, and the second vacuum adsorption platform is moved under the first vacuum adsorption platform and lifted or rolled.

[0011] Furthermore, the frame film is cut, and the remaining frame film at the reaction area position is retained;

[0012] The cut frame film reaction area residue is used to remove the protective film and use it as a filling layer to fill the reaction area of ​​the frame film.

[0013] Furthermore, the frame film with two hollowed-out reaction areas is cut out;

[0014] Fixing a cut frame film on the first vacuum adsorption platform according to the position of the first positioning mechanism, and filling the reaction area of ​​the frame film with a filling layer;

[0015] The cut three-layer film structure is fixed on the second vacuum adsorption platform, and the protective film of the frame film on the first vacuum adsorption platform is removed. After the first positioning mechanism is aligned, the first driving mechanism drives the first vacuum adsorption platform to flip, and the second driving mechanism drives the second vacuum adsorption platform to move to the bottom of the first vacuum adsorption platform and lift or roll it;

[0016] The second vacuum adsorption platform and the first vacuum adsorption platform are reset to remove the protective film of the three-layer membrane structure;

[0017] The first vacuum adsorption platform is turned over, and the position of another cut frame film installed by the third positioning mechanism is fixed on the third vacuum adsorption platform, and the protective film is removed. The third driving mechanism drives the third vacuum adsorption platform to move under the first vacuum adsorption platform and lift or roll it.

[0018] Furthermore, the packaged membrane electrode is shaped and punched.

[0019] In a second aspect, the packaging device provided by the present invention is used to implement the packaging method of the cold film electrode frame as described in any one of the above items, including a first vacuum adsorption platform and a first positioning mechanism;

[0020] The first positioning mechanism is arranged opposite to the first vacuum adsorption platform, and a filling layer is installed on the surface of the first vacuum adsorption platform opposite to the first positioning mechanism;

[0021] The first vacuum adsorption platform is used to fix the frame film, the filling layer is used to fill the reaction area of ​​the frame film, and the surface of the filling layer is flush with the surface of the frame film.

[0022] Furthermore, the first positioning mechanism is configured as a camera.

[0023] Furthermore, the packaging device includes a first driving mechanism, which is transmission-connected to the first vacuum adsorption platform to drive the first vacuum adsorption platform to flip.

[0024] Furthermore, the packaging equipment includes a second vacuum adsorption platform and a third vacuum adsorption platform;

[0025] The first vacuum adsorption platform is located between the second vacuum adsorption platform and the third vacuum adsorption platform.

[0026] Furthermore, the packaging device further includes a second positioning mechanism and a third positioning mechanism;

[0027] The second positioning mechanism is disposed opposite to the second vacuum adsorption platform, and the third positioning mechanism is disposed opposite to the third vacuum adsorption platform.

[0028] Furthermore, the packaging device further includes a second driving mechanism and a third driving mechanism;

[0029] The second driving mechanism is in transmission connection with the second vacuum adsorption platform to drive the second vacuum adsorption platform to move toward or away from the side of the first vacuum adsorption platform away from the first positioning mechanism, and to move toward or away from the first vacuum adsorption platform;

[0030] The third driving mechanism is transmission-connected to the third vacuum adsorption platform to drive the third vacuum adsorption platform to move toward or away from the first vacuum adsorption platform on the side away from the first positioning mechanism, and to move toward or away from the first vacuum adsorption platform.

[0031] Based on the above technical solutions, the technical effects that can be achieved by the present invention are analyzed as follows:

[0032] The packaging method of the cold-attached film electrode frame provided by the present invention includes cutting a frame film with a hollowed-out reaction area; fixing the frame film on a first vacuum adsorption platform according to the position of a first positioning mechanism, and filling the reaction area of ​​the frame film with a filling layer; fixing the cut three-layer film structure on a second vacuum adsorption platform, removing the protective film of the frame film on the first vacuum adsorption platform, and after the first positioning mechanism is aligned, the first vacuum adsorption platform is flipped, and the second vacuum adsorption platform is moved to the bottom of the first vacuum adsorption platform and lifted or rolled. The packaging method of the cold-attached film electrode frame uses the first vacuum adsorption platform to fix the frame film, and fills the filling layer at a corresponding position of the reaction area of ​​the frame film on the first vacuum adsorption platform, so as to eliminate the height difference between the frame film and the three-layer film structure during the bonding process, so that the three-layer film structure is flat and wrinkle-free during and after the bonding process, and the frame film is evenly stressed during the bonding process, and the reaction area area of ​​the frame will not be deformed after the frame is bonded, thereby reducing the risk of membrane electrode leakage, and ensuring the reaction area area of ​​the membrane electrode, so that the performance of the membrane electrode is more stable. BRIEF DESCRIPTION OF THE DRAWINGS

[0033] In order to more clearly illustrate the specific implementation methods of the present invention or the technical solutions in the prior art, the drawings required for use in the specific implementation methods or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are some implementation methods of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.

[0034] Figure 1 A schematic diagram of the structure of a packaging device provided in an embodiment of the present invention.

[0035] icon:

[0036] 100 - three-layer membrane structure; 200 - frame membrane; 210 - filling layer; 300 - first vacuum adsorption platform. DETAILED DESCRIPTION

[0037] In order to make the purpose, technical solutions and advantages of the embodiments of the present invention clearer, the technical solutions in the embodiments of the present invention will be clearly and completely described below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are part of the embodiments of the present invention, not all of the embodiments. Generally, the components of the embodiments of the present invention described and shown in the drawings here can be arranged and designed in various different configurations.

[0038] Therefore, the following detailed description of the embodiments of the present invention provided in the accompanying drawings is not intended to limit the scope of the invention claimed for protection, but merely represents selected embodiments of the present invention. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0039] It should be noted that similar reference numerals and letters denote similar items in the following drawings, and therefore, once an item is defined in one drawing, further definition and explanation thereof is not required in subsequent drawings.

[0040] In the description of the present invention, it should be noted that the terms "center", "upper", "lower", "left", "right", "vertical", "horizontal", "inside", "outside", etc. indicate positions or positional relationships based on the positions or positional relationships shown in the accompanying drawings, or the positions or positional relationships in which the product of the invention is usually placed when in use. They are only for the convenience of describing the present invention and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific position, be constructed and operated in a specific position, and therefore cannot be understood as limiting the present invention. In addition, the terms "first", "second", "third", etc. are only used to distinguish the description, and cannot be understood as indicating or implying relative importance.

[0041] In addition, the terms "horizontal", "vertical", "overhanging" and the like do not mean that the components are required to be absolutely horizontal or overhanging, but can be slightly tilted. For example, "horizontal" only means that its direction is more horizontal than "vertical", and does not mean that the structure must be completely horizontal, but can be slightly tilted.

[0042] In the description of the present invention, it is also necessary to explain that, unless otherwise clearly specified and limited, the terms "set", "install", "connect", and "connect" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection, or it can be indirectly connected through an intermediate medium, or it can be the internal communication of two elements. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.

[0043] Some embodiments of the present invention are described in detail below in conjunction with the accompanying drawings. In the absence of conflict, the following embodiments and features in the embodiments can be combined with each other.

[0044] Embodiment 1

[0045] In the existing cold-sticking packaging process, during the lifting and bonding process between the three-layer membrane structure 100 and the frame film 200, wrinkles will appear when the three-layer membrane structure 100 is bonded to the frame film 200. If the wrinkles are severe, it will lead to incomplete sealing and leakage. Alternatively, during the rolling and bonding process of the anode and cathode frames, the reaction zone area is squeezed and reduced due to uneven force, which affects the performance of the membrane electrode and increases the difficulty of packaging the gas diffusion layer.

[0046] In view of this, the packaging method of the cold-stick film electrode frame provided by the embodiment of the present invention includes cutting to obtain a frame film 200 with a hollowed-out reaction area; fixing the frame film 200 on the first vacuum adsorption platform 300 according to the position of the first positioning mechanism, and using the filling layer 210 to fill the reaction area of ​​the frame film 200; fixing the cut three-layer film structure 100 on the second vacuum adsorption platform, removing the protective film of the frame film 200 on the first vacuum adsorption platform 300, and after the first positioning mechanism is aligned, the first vacuum adsorption platform 300 is flipped over, and the second vacuum adsorption platform is moved to the bottom of the first vacuum adsorption platform 300 and lifted or rolled. The packaging method of the cold-bonded film electrode frame uses a first vacuum adsorption platform 300 to fix the frame film 200, and fills a filling layer 210 at a position corresponding to the reaction area of ​​the frame film 200 on the first vacuum adsorption platform 300, so as to eliminate the height difference between the frame film 200 and the three-layer membrane structure 100 during the bonding process, so that the three-layer membrane structure 100 is flat and wrinkle-free during and after the bonding process, and the frame film 200 is evenly stressed during the bonding process. The reaction area will not be deformed after the frame is bonded, thereby reducing the risk of membrane electrode leakage, ensuring the area of ​​the membrane electrode reaction area, and making the performance of the membrane electrode more stable.

[0047] In the optional scheme of the embodiment of the present invention, the frame film 200 with two hollowed-out reaction areas is cut; one of the cut frame films 200 is fixed on the first vacuum adsorption platform 300 according to the position of the first positioning mechanism, and the reaction area of ​​the frame film 200 is filled with a filling layer 210; the cut three-layer membrane structure 100 is fixed on the second vacuum adsorption platform, and the protective film of the frame film 200 on the first vacuum adsorption platform 300 is removed. After the first positioning mechanism is aligned, the first driving mechanism drives the first vacuum adsorption platform 300 to flip, and the second driving mechanism drives the second vacuum adsorption platform to move to the bottom of the first vacuum adsorption platform 300 and lift or roll; the second vacuum adsorption platform and the first vacuum adsorption platform 300 are reset, and the protective film of the three-layer membrane structure 100 is removed; the first vacuum adsorption platform 300 is flipped, and the position of the other cut frame film 200 installed with the third positioning mechanism is fixed on the third vacuum adsorption platform, and the protective film is removed, and the third driving mechanism drives the third vacuum adsorption platform to move to the bottom of the first vacuum adsorption platform 300 and lift or roll.

[0048] Specifically, the filling layer 210 is adhered to the first vacuum adsorption platform 300 .

[0049] The filling layer 210 is filled on the first vacuum adsorption platform 300 to ensure that the surface of the three-layer film structure 100 is flat and the reaction area of ​​the frame film 200 remains unchanged.

[0050] In an optional solution of the embodiment of the present invention, two frame films 200 are cut, and the cut frame film 200 at the reaction area is retained; one of the cut frame films 200 is fixed on the first vacuum adsorption platform 300 according to the position of the first positioning mechanism, and the cut frame film 200 reaction area residue is used to remove the protective film as the filling layer 210 to fill the reaction area of ​​the frame film 200. The packaged membrane electrode is shaped and punched.

[0051] The following is the test process and results of the comparative test between the prior art and the packaging method of the cold film electrode frame provided by this embodiment:

[0052] Test 1:

[0053] Lay the three-layer membrane structure 100 flat on the second vacuum adsorption platform according to the camera position, and evacuate the vacuum. Place the anode frame film on the first vacuum adsorption platform 300 according to the camera position, and stick the remaining material of the upper frame film 200 in the middle of the reaction area of ​​the upper frame film 200 on the first vacuum adsorption platform 300 to ensure that there is no height difference in the sticking. Set the lifting pressure of 1KG to stick the three-layer membrane structure 100 and the anode frame film, and observe the surface state of the three-layer membrane structure 100. Place the cathode frame on the third vacuum adsorption platform, set the sticking pressure of 1.5KG, complete the frame sticking, and observe the sticking effect of the frame film 200.

[0054] Test 2:

[0055] Lay the three-layer membrane structure 100 flat on the second vacuum adsorption platform according to the camera position, and evacuate it. Place the anode frame film on the first vacuum adsorption platform 300 according to the camera position, and stick the remaining upper frame film 200 in the middle of the reaction area of ​​the upper frame film 200 on the first vacuum adsorption platform 300 to ensure that there is no height difference in the sticking. Set the lifting pressure to 1.5KG, stick the three-layer membrane structure 100 and the anode frame film, and observe the surface state of the three-layer membrane structure 100. Place the cathode frame on the third vacuum adsorption platform, set the sticking pressure to 2KG, complete the frame sticking, and observe the sticking effect of the frame film 200.

[0056] Test 3:

[0057] Lay the three-layer membrane structure 100 flat on the second vacuum adsorption platform according to the camera position, and evacuate the vacuum. Place the anode frame film on the first vacuum adsorption platform 300 according to the camera position, and stick the remaining upper frame film 200 in the middle of the reaction area of ​​the upper frame film 200 on the first vacuum adsorption platform 300 to ensure that there is no height difference in the sticking. Set the lifting pressure to 2KG, stick the three-layer membrane structure 100 and the anode frame film, and observe the surface state of the three-layer membrane structure 100. Place the cathode frame on the third vacuum adsorption platform, set the sticking pressure to 2.5KG, complete the frame sticking, and observe the sticking effect of the frame film 200.

[0058] Test 4:

[0059] Lay the three-layer membrane structure 100 flat on the second vacuum adsorption platform according to the camera position, and evacuate the vacuum. Place the anode frame film on the first vacuum adsorption platform 300 according to the camera position, and stick the remaining upper frame film 200 in the middle of the reaction area of ​​the upper frame film 200 on the first vacuum adsorption platform 300 to ensure that there is no height difference in the sticking. Set the lifting pressure to 2KG, stick the three-layer membrane structure 100 and the anode frame film, and observe the surface state of the three-layer membrane structure 100. Place the cathode frame on the third vacuum adsorption platform, set the sticking pressure to 3KG, complete the frame sticking, and observe the sticking effect of the frame film 200.

[0060] Comparative test 1:

[0061] Lay the three-layer membrane structure 100 flat on the second vacuum adsorption platform according to the camera position, and evacuate it. Place the anode frame film on the first vacuum adsorption platform 300 according to the camera position, and the first vacuum adsorption platform 300 is not processed. Set the lifting pressure to 1KG, and bond the three-layer membrane structure 100 and the anode frame film, and observe the surface state of the three-layer membrane structure 100. Place the cathode frame on the third vacuum adsorption platform, set the bonding pressure to 1.5KG, complete the frame bonding, and observe the bonding effect of the frame film 200.

[0062] Comparative test 2:

[0063] Lay the three-layer membrane structure 100 flat on the second vacuum adsorption platform according to the camera position, and evacuate it. Place the anode frame film on the first vacuum adsorption platform 300 according to the camera position, and the first vacuum adsorption platform 300 is not processed. Set the lifting pressure to 1.5KG, and bond the three-layer membrane structure 100 and the anode frame film, and observe the surface state of the three-layer membrane structure 100. Place the cathode frame on the third vacuum adsorption platform, set the bonding pressure to 2KG, complete the frame bonding, and observe the bonding effect of the frame film 200.

[0064] Comparative test three:

[0065] Lay the three-layer membrane structure 100 flat on the second vacuum adsorption platform according to the camera position, and evacuate it. Place the anode frame film on the first vacuum adsorption platform 300 according to the camera position, and the first vacuum adsorption platform 300 is not processed; set the lifting pressure to 2KG, and fit the three-layer membrane structure 100 and the anode frame film, and observe the surface state of the three-layer membrane structure 100; place the cathode frame on the third vacuum adsorption platform, set the fitting pressure to 2.5KG, complete the frame fitting, and observe the fitting effect of the frame film 200.

[0066] Comparative test 4:

[0067] Lay the three-layer membrane structure 100 on the second vacuum adsorption platform according to the camera position, and evacuate it. Place the anode frame film on the first vacuum adsorption platform 300 according to the camera position, and do not process the first vacuum adsorption platform 300. Set the lifting pressure to 2KG, and bond the three-layer membrane structure 100 with the anode frame film, and observe the surface state of the three-layer membrane structure 100. Place the cathode frame on the third vacuum adsorption platform, set the bonding pressure to 3KG, complete the frame bonding, and observe the bonding effect of the frame film 200.

[0068] The bonded membrane electrode was observed to ensure that the ambient temperature during the bonding and measurement process was between 23-25°C and the humidity was between 60-70%. The three-layer membrane structure 100 was visually inspected to observe the number and length of wrinkles in the three-layer membrane structure 100. The frame membrane 200 position was measured for error using an image measuring instrument.

[0069] test Three-layer membrane structure 100 folds Border reaction area error Test 1 0 0.135mm Test 2 0 0.153mm Test 3 0 0.173mm Test 4 0 0.186mm Comparative test 1 3 0.215mm Comparative test 2 2 0.231mm Comparative test three 1 0.258mm Comparative test 4 1 0.283mm

[0070] From the above comparative test, it can be seen that after the filling layer 210 is set on the first vacuum adsorption platform 300, the number of wrinkles of the three-layer membrane structure 100 is significantly reduced, and the error of the frame reaction area is reduced, which reduces the risk of membrane electrode leakage and ensures the area of ​​the membrane electrode reaction area, making the performance of the membrane electrode more stable.

[0071] Embodiment 2

[0072] The packaging device provided in the embodiment of the present invention is used to implement the packaging method of the cold film electrode frame described in the first embodiment.

[0073] like Figure 1 As shown, the packaging device provided by the embodiment of the present invention includes a first vacuum adsorption platform 300 and a first positioning mechanism; the first positioning mechanism is arranged opposite to the first vacuum adsorption platform 300, and a filling layer 210 is installed on the surface of the first vacuum adsorption platform 300 opposite to the first positioning mechanism; the first vacuum adsorption platform 300 is used to fix the frame film 200, and the filling layer 210 is used to fill in the reaction area of ​​the frame film 200, and the surface of the filling layer 210 is flush with the surface of the frame film 200.

[0074] In an optional solution of the embodiment of the present invention, the filling layer 210 is configured as the residual material of the reaction area of ​​the frame film 200 after the protective film is removed.

[0075] Specifically, the first vacuum adsorption platform 300 is provided with adsorption holes and a vacuum pump, and the frame film 200 is fixed by the cooperation of the vacuum pump and the adsorption holes.

[0076] The filling layer 210 uses more than 200 pieces of frame film that were originally discarded, which is easy to obtain and saves cost investment.

[0077] In an optional solution of the embodiment of the present invention, the first positioning mechanism is configured as a camera.

[0078] Specifically, the frame film 200 itself has adhesive, and can be used directly after removing the protective film, without the need for auxiliary materials such as tape or double-sided tape, which further ensures the flatness of the fit. The camera automatically aligns the first vacuum adsorption platform 300 through visual photography.

[0079] When the packaging device is used, the frame film 200 is placed on the first vacuum adsorption platform 300 according to the position of the camera, so as to achieve the alignment of the camera to the frame film 200 .

[0080] In an optional solution of the embodiment of the present invention, the packaging device includes a first driving mechanism, which is transmission-connected to the first vacuum adsorption platform 300 to drive the first vacuum adsorption platform 300 to flip.

[0081] Specifically, when the packaging device is used, the support surface of the first vacuum adsorption platform 300 is firstly set to face upward, so that the operator can place the frame film 200 on the support surface of the first vacuum adsorption platform 300; then the first driving mechanism turns the first vacuum adsorption platform 300 180° to face the support surface downward, so that the three-layer membrane structure 100 and the frame film 200 adsorbed on the first vacuum adsorption platform 300 can be bonded together; then the first driving mechanism drives the first vacuum adsorption platform 300 to reset, so that the operator can check the bonding of the three-layer membrane structure 100; then the first driving mechanism again turns the first vacuum adsorption platform 300 180° to face the support surface downward, so that another frame film 200 can be bonded to the frame film 200 adsorbed on the first vacuum adsorption platform 300; finally, the first driving mechanism drives the first vacuum adsorption platform 300 to reset, so that the operator can check the membrane electrode.

[0082] The first driving mechanism realizes the flipping movement of the first vacuum adsorption platform 300, which is convenient for operators to load, fit and inspect.

[0083] In an optional solution of the embodiment of the present invention, the packaging equipment includes a second vacuum adsorption platform and a third vacuum adsorption platform; the first vacuum adsorption platform 300 is located between the second vacuum adsorption platform and the third vacuum adsorption platform.

[0084] Specifically, the second vacuum adsorption platform and the third vacuum adsorption platform both have an adsorption and fixing function, and fix the three-layer film structure 100 and another frame film 200 respectively.

[0085] The second vacuum adsorption platform and the third vacuum adsorption platform realize the fixing function of the three-layer film structure 100 and another frame film 200 .

[0086] In an optional solution of the embodiment of the present invention, the packaging equipment further includes a second positioning mechanism and a third positioning mechanism; the second positioning mechanism is arranged opposite to the second vacuum adsorption platform, and the third positioning mechanism is arranged opposite to the third vacuum adsorption platform.

[0087] Specifically, the second positioning mechanism and the third positioning mechanism are both configured as cameras, and the cameras are automatically aligned through a visual photography platform.

[0088] The camera realizes the positioning function of the materials fixed on the second vacuum adsorption platform and the third vacuum adsorption platform.

[0089] In an optional scheme of an embodiment of the present invention, the packaging equipment also includes a second driving mechanism and a third driving mechanism; the second driving mechanism is transmission-connected to the second vacuum adsorption platform to drive the second vacuum adsorption platform to move toward or away from the side of the first vacuum adsorption platform 300 away from the first positioning mechanism, and to move toward or away from the first vacuum adsorption platform 300; the third driving mechanism is transmission-connected to the third vacuum adsorption platform to drive the third vacuum adsorption platform to move toward or away from the side of the first vacuum adsorption platform 300 away from the first positioning mechanism, and to move toward or away from the first vacuum adsorption platform 300.

[0090] The second driving mechanism realizes the driving effect on the second vacuum adsorption platform, and the third driving mechanism realizes the driving effect on the third vacuum adsorption platform.

[0091] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the present invention, rather than to limit it. Although the present invention has been described in detail with reference to the aforementioned embodiments, those skilled in the art should understand that they can still modify the technical solutions described in the aforementioned embodiments, or replace some or all of the technical features therein with equivalents. However, these modifications or replacements do not cause the essence of the corresponding technical solutions to deviate from the scope of the technical solutions of the embodiments of the present invention.

Claims

1. A packaging method for a cold film electrode frame, characterized in that: include: Cutting to obtain a frame film with a hollowed-out reaction area; The frame film is fixed on the first vacuum adsorption platform according to the position of the first positioning mechanism, and the reaction area of ​​the frame film is filled with a filling layer; The cut three-layer film structure is fixed on the second vacuum adsorption platform, the protective film of the frame film on the first vacuum adsorption platform is removed, and after the first positioning mechanism is aligned, the first vacuum adsorption platform is turned over, and the second vacuum adsorption platform is moved under the first vacuum adsorption platform and lifted or rolled.

2. The packaging method of the cold film electrode frame according to claim 1, characterized in that: Cut the frame film and keep the remaining frame film at the reaction area; The cut frame film reaction area residue is used to remove the protective film and use it as a filling layer to fill the reaction area of ​​the frame film.

3. The packaging method of the cold film electrode frame according to claim 1, characterized in that: Cutting to obtain two frame films with hollowed-out reaction areas; Fixing a cut frame film on the first vacuum adsorption platform according to the position of the first positioning mechanism, and filling the reaction area of ​​the frame film with a filling layer; The cut three-layer film structure is fixed on the second vacuum adsorption platform, and the protective film of the frame film on the first vacuum adsorption platform is removed. After the first positioning mechanism is aligned, the first driving mechanism drives the first vacuum adsorption platform to flip, and the second driving mechanism drives the second vacuum adsorption platform to move to the bottom of the first vacuum adsorption platform and lift or roll it; The second vacuum adsorption platform and the first vacuum adsorption platform are reset to remove the protective film of the three-layer membrane structure; The first vacuum adsorption platform is turned over, and the position of another cut frame film installed by the third positioning mechanism is fixed on the third vacuum adsorption platform, and the protective film is removed. The third driving mechanism drives the third vacuum adsorption platform to move under the first vacuum adsorption platform and lift or roll it.

4. The packaging method of the cold film electrode frame according to claim 3 is characterized in that: The packaged membrane electrode is punched and cut into shape.

5. A packaging device for implementing the packaging method of the cold film electrode frame according to any one of claims 1 to 4, characterized in that: include: A first vacuum adsorption platform and a first positioning mechanism; The first positioning mechanism is arranged opposite to the first vacuum adsorption platform, and a filling layer is installed on the surface of the first vacuum adsorption platform opposite to the first positioning mechanism; The first vacuum adsorption platform is used to fix the frame film, the filling layer is used to fill the reaction area of ​​the frame film, and the surface of the filling layer is flush with the surface of the frame film.

6. The packaging device according to claim 5, characterized in that The first positioning mechanism is configured as a camera.

7. The packaging device according to claim 5, characterized in that: The packaging device includes a first driving mechanism, which is transmission-connected to the first vacuum adsorption platform to drive the first vacuum adsorption platform to flip.

8. The packaging device according to any one of claims 5 to 7, characterized in that: The packaging equipment includes a second vacuum adsorption platform and a third vacuum adsorption platform; The first vacuum adsorption platform is located between the second vacuum adsorption platform and the third vacuum adsorption platform.

9. The packaging device according to claim 8, characterized in that: The packaging device also includes a second positioning mechanism and a third positioning mechanism; The second positioning mechanism is disposed opposite to the second vacuum adsorption platform, and the third positioning mechanism is disposed opposite to the third vacuum adsorption platform.

10. The packaging device according to claim 9, characterized in that The packaging device also includes a second driving mechanism and a third driving mechanism; The second driving mechanism is in transmission connection with the second vacuum adsorption platform to drive the second vacuum adsorption platform to move toward or away from the side of the first vacuum adsorption platform away from the first positioning mechanism, and to move toward or away from the first vacuum adsorption platform; The third driving mechanism is transmission-connected to the third vacuum adsorption platform to drive the third vacuum adsorption platform to move toward or away from the first vacuum adsorption platform on the side away from the first positioning mechanism, and to move toward or away from the first vacuum adsorption platform.