Glass energy-saving structure and implementation method

By using a combined structure of composite glass, spacer strips and sealant in existing buildings, the gas spacer layer and adhesive layer are formed, which solves the heat and sun protection problems of ordinary hollow glass windows, achieving more efficient energy-saving effects and a better building appearance.

CN119900448APending Publication Date: 2025-04-29TIANJIN CSG ENERGY CONSERVATION GLASS CO LTD +1
View PDF 10 Cites 0 Cited by

Patent Information

Application Number
CN202510057245.6
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2025-01-14
Publication Date
2025-04-29

AI Technical Summary

Technical Problem

The ordinary insulating glass windows in existing buildings have poor heat protection effects, poor thermal insulation in winter, high power consumption of air conditioners, and limited durability and sun protection ability of energy-saving films, making it difficult to meet the requirements of lighting and sun protection at the same time.

Method used

A combined structure of composite glass, spacer strips and sealant is adopted. The spacer strips are arranged around the existing glass to form a gas spacer layer. The sealant is arranged on the side of the spacer strips away from the gas spacer layer, and the thermal insulation performance and sun protection ability of the glass are improved by bonding methods.

Benefits of technology

It significantly improves the thermal insulation performance of glass, reduces the power consumption of air conditioners in summer and heating energy consumption in winter, improves the appearance of the building, meets the requirements of lighting and sun protection, and is easy to operate and has strong adaptability.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119900448A_ABST
    Figure CN119900448A_ABST
Patent Text Reader

Abstract

The invention provides a glass energy-saving structure and an implementation method. The glass energy-saving structure comprises composite glass, spacing bars and sealant, and the spacing bars are arranged on the periphery of existing glass; the size of the composite glass corresponds to that of the existing glass, the composite glass is arranged on the other side of the existing glass through the spacing bar, a gas spacing layer is formed among the composite glass, the existing glass and the spacing bar, and the sealant is arranged on the side, away from the gas spacing layer, of the spacing bar and between the composite glass and the existing glass. And the composite glass is arranged on one indoor side. The energy-saving effect can be improved, the hollow cavity is formed in the position, a certain distance away from the edge, of the periphery of the indoor face of the existing glass, and therefore the heat preservation performance of the glass is improved, and air conditioner power consumption in summer and heating energy consumption in winter are reduced. Compared with a method for pasting an energy-saving film, the energy-saving effect is more remarkable and lasting.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the field of glass structures, and in particular relates to a glass energy-saving structure and an implementation method. Background Art

[0002] At present, a large number of existing buildings use ordinary insulating glass windows, which have poor heat protection effect, poor winter insulation, high power consumption for air conditioning, and poor human comfort. As energy-saving design standards in Beijing and other regions gradually improve, doors and windows of old buildings no longer meet relevant energy-saving design requirements. For example, the current standard GB55015-2021 "General Specification for Building Energy Conservation and Renewable Energy Utilization" requires energy-saving renovation to diagnose heat transfer coefficient, air tightness, and solar heat gain coefficient.

[0003] Applying energy-saving film to glass is currently a widely used renovation solution for existing buildings, but this solution has the problem of poor durability. After 3-5 years, due to the heat absorption of the film, bubbles and debonding will appear on the film, seriously affecting the appearance of the building; the film can improve the problem of indoor sun exposure to a certain extent, but it cannot improve the thermal insulation capacity. The power consumption of air conditioning in summer and heating in winter are still very high; the film is difficult to meet the requirements of lighting and sun protection at the same time, and the improvement in sun protection ability is limited. It cannot completely block infrared rays like Low-E film. HYPERLINK "https: / / analytics.zhihuiya.com / patent-view / abst?patentId=c3391217-9654-47c4-94b8-197fa364ae77&shareId=19878F78-DCB3-7B4D-B459-391B3CB52666&from=EXPORT&signature=Q3eruLgj+zD95TJzwzz3ml3HDYGzQx3n25cR7P2dWhA=&expire=94608000&date=20240428T033636Z&version=1.0" Relevant patch modification solutions are disclosed in CN211923061U, CN106593220A and CN204738692U. Summary of the invention

[0004] In view of this, the present invention aims to provide a glass energy-saving structure and implementation method to solve at least one technical problem in the background technology.

[0005] To achieve the above object, the technical solution of the present invention is achieved as follows: A glass energy-saving structure, comprising composite glass, spacer strips, and sealant, wherein the spacer strips are arranged around the existing glass; The size of the composite glass corresponds to the size of the existing glass, and the composite glass is arranged on the other side of the existing glass through a spacer bar. A gas spacing layer is formed between the composite glass, the existing glass and the spacer bar. The sealant is arranged on the side of the spacer bar away from the gas spacing layer and between the composite glass and the existing glass. The composite glass is arranged on the side inside the room.

[0006] Furthermore, the distance between the spacer and the four edges of the composite glass is not less than 2 mm, preferably 3-5 mm; The spacer is a composite butyl rubber spacer containing a molecular sieve inside, or a common spacer (such as a stainless steel spacer, an aluminum bar, etc.) is used, and adhesive is provided on both sides thereof, and the adhesive is butyl rubber; The width of the spacer is between 3-20 mm, preferably 9-12 mm; The distance between the four sides of the composite glass and the existing glass exposed outside is not less than 3mm, preferably 3-5mm.

[0007] Furthermore, a support block is arranged in the sealant at the lower side of the composite glass, preferably two support blocks are symmetrically arranged, and the distance between one end of the support block and the side edge of the existing glass is 1 / 4 of the side length of the existing glass.

[0008] The support block is made of plastic or acrylic.

[0009] Furthermore, the sealant can be selected from silicone structural sealant or polysulfide sealant according to the usage scenario.

[0010] A method for implementing a glass energy-saving structure comprises the following steps: S1: Clean the existing glass surface, measure the length and width of the existing glass, and measure and mark the position of the spacer strips; S2: placing the composite glass on the workbench assembly, placing the spacer strips on the shaft frame, pasting the spacer strips around the composite glass, and setting the spacer strips on the composite glass through a code strip device to obtain a composite glass pasted with the spacer strips; S3: Heat the spacer bar, align the composite glass with the spacer bar to the marked position in step S1, place the support block at the bottom of the composite glass, apply pressure evenly, and glue the four sides of the composite glass.

[0011] Step S2 also includes rolling up the electrostatic film of the composite glass from the four edges respectively, and then gradually uncovering it completely towards the middle. If marks are found at a local position, it needs to be wiped clean with a dust-free cloth and anhydrous ethanol; The workbench assembly in step S2 includes a base, a rotating tube, a rotating screw, a sliding head, and a support table; The rotating table is fixedly arranged on the base, the inner thread of the rotating tube is provided with a rotating screw, the upper end of the rotating screw is rotatably provided with a sliding head, the sliding head is provided with a supporting table, the supporting table is provided with an annular table, and the composite glass is arranged on the annular table during processing.

[0012] Furthermore, an annular buffer pad is provided on the annular table, and the annular buffer pad is a rubber pad or a cotton pad.

[0013] Preferably, a locking bolt is provided on one side of the sliding head, and the end of the locking bolt abuts against the rotating screw rod. The locking bolt can relatively fix the sliding head and the rotating screw rod so that the sliding head will not slide any more.

[0014] Preferably, the support platform is provided with a plurality of handles along the circumference, and an operator can rotate the support platform at the end of the sliding head and the rotating screw through the handles.

[0015] Further, the shaft frame in step S2 is arranged on one side of the workbench assembly, and the shaft frame includes a side plate, a fixed shaft, an I-shaped wheel, a guide roller, and an output roller; The fixed shaft is arranged between the two side plates, and the I-shaped wheel is rotatably arranged on the fixed shaft; The guide roller is rotatably arranged between the two side plates and arranged above the spool; The two output rollers are rotatably arranged between the two side plates, the centers of the two output rollers are perpendicular to the ground, and the distance between the two output rollers is the same as the thickness of the spacer bar.

[0016] Furthermore, the code bar device in step S2 includes a housing, a first slot and a second slot are provided at the bottom of the housing, and two first cylinders and two second cylinders are symmetrically provided on the housing through the first slot; The shell is provided with a first rotating wheel through the second slot.

[0017] Furthermore, a third slot is provided on one side of the bottom of the shell, a second rotating wheel is provided in the third slot, two mounting rods are symmetrically provided on the other side of the shell, and a chuck is provided on the shell through the two mounting rods; The chuck is U-shaped, and slots are arranged on both sides of the U-shaped chuck, and the slots are matched with the mounting rods, and mounting nuts are arranged at the ends of the mounting rods. The present application achieves better effect by laminating the chuck with the composite glass.

[0018] Further, the heating temperature of step S3 is 45-55°C; In step S3, the support blocks are symmetrically placed at the bottom of the composite glass, and pressure is applied evenly to ensure that the patch is in full contact with the existing glass and to check whether there is any loose connection. If necessary, a rubber hammer is used to hammer to ensure that there is no loose connection, and the pressing time is at least 2 minutes.

[0019] In step S3, before sealing, masking tape needs to be pasted on the edge of the composite glass and the edge of the window frame. During sealing, the speed of gluing is controlled to ensure that the sealant is filled with no empty glue. After gluing, it is necessary to use a scraper for trimming, and then remove the masking tape to ensure the beauty of the seal.

[0020] Compared with the prior art, the glass energy-saving structure and implementation method described in the present invention have the following advantages: 1. The present invention can improve the energy-saving effect. By using aluminum strip spacers for bonding, a hollow cavity can be formed around the existing glass room at a certain distance from the edge, thereby improving the thermal insulation performance of the glass and reducing the power consumption of air conditioning in summer and heating in winter. Compared with the method of applying energy-saving film, the energy-saving effect of the present invention is more significant and lasting.

[0021] 2. This application can improve the appearance of the building. The spacer strip bonding method will not cause bubbles or debonding, which will not affect the appearance of the building. In contrast, the durability of energy-saving films is poor, usually only 3-5 years, and bubbles and debonding are prone to occur, which seriously affects the appearance of the building.

[0022] 3. This application can meet the requirements of lighting and sun protection. The use of spacer strip bonding method can meet the requirements of lighting and sun protection at the same time. In contrast, it is difficult to meet the requirements of lighting and sun protection at the same time by applying energy-saving film. The sun protection ability is limited and it cannot completely block infrared rays like Low-E film.

[0023] 4. The application is easy to operate, and the spacer strip bonding method is easy to operate, which is suitable for scenes with narrow installation space and small operating space. In contrast, the operation of pasting energy-saving film is more complicated and requires professional personnel to install, which increases construction cost and time.

[0024] 5. This application has strong adaptability, and the spacer bonding method can be selected according to the thickness of the hollow cavity to be obtained, which has strong adaptability. In contrast, the energy-saving film has poor adaptability and needs to be selected according to different glass types and needs, which increases the difficulty of construction. BRIEF DESCRIPTION OF THE DRAWINGS

[0025] The accompanying drawings constituting a part of the present invention are used to provide a further understanding of the present invention. The exemplary embodiments of the present invention and their descriptions are used to explain the present invention and do not constitute an improper limitation of the present invention. In the accompanying drawings: Figure 1 It is an overall schematic diagram of a glass energy-saving structure according to an embodiment of the present invention; Figure 2 It is a cross-sectional schematic diagram of a glass energy-saving structure according to an embodiment of the present invention; Figure 3 A schematic diagram of a workbench assembly and a shaft frame according to an embodiment of the present invention; Figure 4A schematic diagram of a code bar device according to an embodiment of the present invention; Figure 5 It is a bottom schematic diagram of the code bar device according to an embodiment of the present invention.

[0026] Description of reference numerals: 1. Gas spacer layer; 2. Composite glass; 3. Existing glass; 4. Spacer strip; 5. Sealant; 6. Base; 7. Rotating tube; 8. Rotating screw; 9. Sliding head; 10. Support platform; 11. Ring platform; 12. Locking bolt; 13. Handle; 14. Side plate; 15. Fixed shaft; 16. I-wheel; 17. Guide roller; 18. Output roller; 19. Shell; 20. First slot; 21. First cylinder; 22. Second cylinder; 23. First rotating wheel; 24. Third slot; 25. Second rotating wheel; 26. Chuck; 27. U-shaped chuck; 28. Slot; 29. ​​Mounting nut; 30. Second slot; 31. Support block; 32. Glass frame. DETAILED DESCRIPTION

[0027] It should be noted that, in the absence of conflict, the embodiments of the present invention and the features in the embodiments may be combined with each other.

[0028] In the description of the present invention, it should be understood that the terms "center", "longitudinal", "lateral", "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside", "outside" and the like indicate positions or positional relationships based on the positions or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present invention and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as limiting the present invention. In addition, the terms "first", "second", and the like are only used for descriptive purposes, and cannot be understood as indicating or implying relative importance or implicitly indicating the number of technical features indicated. Thus, features defined as "first", "second", and the like may explicitly or implicitly include one or more of the features. In the description of the present invention, unless otherwise specified, "multiple" means two or more.

[0029] In the description of the present invention, it should be noted that, unless otherwise clearly specified and limited, the terms "installed", "connected", and "connected" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection, or it can be indirectly connected through an intermediate medium, or it can be the internal communication of two components. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood by specific circumstances.

[0030] The present invention will be described in detail below with reference to the accompanying drawings and in conjunction with embodiments.

[0031] Example 1 like Figure 1-5 As shown, a glass energy-saving structure includes a composite glass 2, a spacer bar 4, and a sealant 5, wherein the spacer bar 4 is arranged around the existing glass 3; The size of the composite glass 2 corresponds to the size of the existing glass, and the composite glass 2 is arranged on the other side of the existing glass 3 through the spacer bar 4, and a gas spacing layer 1 is formed between the composite glass 2, the existing glass 3, and the spacer bar 4. The sealant 5 is arranged on the side of the spacer bar 4 away from the gas spacing layer 1, and between the composite glass 2 and the existing glass 3. The composite glass 2 is arranged on the side inside the room.

[0032] The spacing between the spacer bar 4 and the four edges of the composite glass 2 is not less than 2 mm, preferably 3-5 mm; adhesive is provided on both sides of the spacer bar 4, and the adhesive is butyl adhesive; the width of the spacer bar 4 is between 3-20 mm, preferably 9-12 mm; the spacing between the four edges of the composite glass 2 and the existing glass 3 exposed to the outside (the size outside the glass frame 32) is not less than 3 mm, preferably 3-5 mm.

[0033] Two support blocks 31 are symmetrically arranged in the sealant 5, and the distance between one end of the support block 31 and the existing glass 3 (such as Figure 1 , L) is 1 / 4 of the side length of the existing glass 3. The support block 31 is made of plastic or acrylic material.

[0034] A method for implementing a glass energy-saving structure comprises the following steps: S1: cleaning the surface of an existing glass 3, measuring the length and width of the existing glass 3, and measuring and marking the position of a spacer strip 4; S2: placing a composite glass 2 on a workbench assembly, placing the spacer strip 4 on an axis frame, and attaching adhesive strips around the composite glass 2, wherein the spacer strip 4 is arranged on the adhesive strip of the composite glass 2 by a code strip device, and the composite glass 2 attached with the spacer strip 4 is obtained; S3: heating the composite glass 2 attached with the spacer strip 4, and then aligning the composite glass 2 attached with the spacer strip 4 with a manual suction cup to the marked position in step S1, symmetrically placing a support block 31 at the bottom of the composite glass 2, and applying uniform pressure to glue the composite glass 2 around. Step S2 also includes rolling up the electrostatic film of the composite glass 2 from the four edges respectively, and then gradually peeling it off completely towards the middle. If marks are found in some local positions, they need to be wiped clean with a dust-free cloth and anhydrous ethanol; the workbench assembly in step S2 includes a base 6, a rotating tube 7, a rotating screw 8, a sliding head 9, and a support table 10; the rotating table is fixedly arranged on the base 6, the rotating tube 7 has an internal thread with a rotating screw 8, the upper end of the rotating screw 8 is rotatably provided with a sliding head 9, a support table 10 is arranged on the sliding head 9, and a ring table 11 is arranged on the support table 10, and the composite glass 2 is arranged on the ring table 11 during processing.

[0035] An annular cushion is provided on the annular platform 11, and the annular cushion is a rubber cushion or a cotton cushion. A locking bolt 12 is provided on one side of the sliding head 9, and the end of the locking bolt 12 abuts against the rotating screw 8. The locking bolt 12 can relatively fix the sliding head 9 and the rotating screw 8, and thus no longer slide. The support platform 10 is provided with a plurality of handles 13 along the circumference, and the operator can rotate the support platform 10 at the end of the sliding head 9 and the rotating screw 8 through the handles 13.

[0036] The shaft frame in step S2 is set on one side of the workbench assembly, and the shaft frame includes a side plate 14, a fixed shaft 15, an I-shaped wheel 16, a guide roller 17, and an output roller 18; the fixed shaft 15 is set between the two side plates 14, and the I-shaped wheel 16 is rotatably set on the fixed shaft 15; the guide roller 17 is rotatably set between the two side plates 14 and is set above the I-shaped wheel 16; the two output rollers 18 are rotatably set between the two side plates 14, the centers of the two output rollers 18 are perpendicular to the ground, and the distance between the two output rollers 18 is the same as the thickness of the spacer bar 4.

[0037] The barcode reader in step S2 includes a housing 19 , a first slot 20 and a second slot 30 are provided at the bottom of the housing 19 , two first cylinders 21 and two second cylinders 22 are symmetrically provided in sequence on the housing 19 through the first slot 20 ; and a first rotating wheel 23 is provided on the housing 19 through the second slot 30 .

[0038] A third slot 24 is provided on one side of the bottom of the housing 19, a second rotating wheel 25 is provided in the third slot 24, two mounting rods are symmetrically provided on the other side of the housing 19, and a chuck 26 is provided on the housing 19 through the two mounting rods; The chuck 26 is U-shaped, and a clamping groove 28 is provided on both sides of the U-shaped chuck 2726. The clamping groove 28 cooperates with the mounting rod, and the end of the mounting rod is provided with a mounting nut 29. The present application is bonded to the composite glass 2 through the chuck 26, and the effect is better.

[0039] The heating temperature of step S3 is 45-55°C; in step S3, the support block 31 is symmetrically placed on the bottom of the composite glass 2, and pressure is applied evenly to ensure that the patch is in full contact with the existing glass 3 and to check whether there is a virtual connection. If necessary, a rubber hammer is used to hammer to ensure that there is no virtual connection, and the pressing time is at least 2 minutes. Before sealing in step S3, masking tape is applied to the edge of the composite glass 2 and the edge of the window frame. The speed of gluing is controlled during sealing to ensure that the sealant is filled with no empty glue. After gluing, a scraper is used for trimming, and then the masking tape is removed to ensure the beauty of the sealant.

[0040] Example 2 In the specific implementation, the spacer strip 4 is bonded to the existing glass 3 at a certain distance from the edge. The thickness and type of the spacer strip 4 can be selected according to the thickness of the hollow cavity to be obtained. For scenes with narrow installation space and small operation space, for example, 3mm, butyl strips can be selected. For scenes with large installation space, aluminum strip type spacer strips 4 can be used. Such spacer strips 4 are thick and have good thermal insulation performance.

[0041] 1. Surface treatment: clean the oil, dust, etc. on the old wall and glass surface to ensure that the pasting surface is dry and flat.

[0042] 2. Measurement and positioning: According to the frame size of the construction site, accurately measure the patch position and mark it, measure the length and width of the existing glass 3 exposed to the outside, and calculate the size of the composite glass 2.

[0043] 3. Patch installation: Place the composite film glass on the workbench, roll up the electrostatic film on the film glass from the four edges, and then gradually uncover it completely towards the middle. If marks are found in some local areas, wipe them clean with dust-free cloth and anhydrous ethanol.

[0044] Put the spacer bar 4 on the shaft frame, and wind the spacer bar 4 on the I-shaped wheel 16 of the shaft frame. The spacer bar 4 passes through the top of the guide roller 17 and is transmitted from the middle of the two output rollers 18, so that the spacer bar 4 can be smoothly output from the I-shaped roller and can ensure that the spacer bar 4 does not reverse. The spacer bar 4 must rotate forward and not reverse. Reversal makes it easy for the bar to fall to the ground and stick to other debris and dust, which hinders the adhesion between the spacer bar 4 and the glass, causing a channel inside and outside the insulating glass to leak.

[0045] The height of the support platform 10 is adjusted according to the height of the I-wheel 16, so that the locking bolt 12 is in contact with the rotating screw 8, so that the sliding head 9 is fixedly set above the rotating screw 8, and the rotating screw 8 is driven by the handle 13 to adjust the height of the support platform 10, and the locking bolt 12 is loosened to allow the sliding head 9 to rotate along the end of the rotating screw 8, and the composite glass 2 is placed on the annular buffer pad of the annular platform 11. The composite glass 2 can be damaged by the annular buffer pad, and the handle 13 is turned to allow the sliding head 9 to rotate along the end of the rotating screw 8 to drive the rotating head to rotate, and the side of the rubber strip (non-adhesive surface, do not touch the adhesive surface) is pinched with fingers, and applied from right to left. The end of the rubber strip should be cut into a right angle. The end of the spacer bar 4 is 5-6mm away from the end of the glass, and the outer edge is parallel to the edge of the glass and 3-5mm away from the edge. The chuck 26 of the code bar device is fitted with the composite glass 2, and the spacer bar 4 passes through the two first cylinders 21 and the two second cylinders 22. The first rotating wheel 23 can make the spacer bar 4 slide more smoothly, and the second rotation slides along the composite glass 2. The code bar device can make the spacer bar 4 and the composite glass 2 fit better.

[0046] Adjust the distance between the glass edge and the spacer 4 on the baffle under the code stripper. It is best to adjust it to 3 to 5 mm. The spacing between the two first cylinders 21 is 1 mm, and the spacing between the two second cylinders 22 is 1 mm. If the pressure is adjusted too large, the code strip 4 will fall outward. If the pressure is too small, the code strip 4 will fall inward. Remember to adjust the code stripper smoothly before operation. When starting to code, the code strip is straight and smooth, leaving 5 mm at the corner, and slightly bent at a 90-degree angle at the edge of the glass. The two sides of the 90-degree angle are the same size as the edge of the glass. The last connecting corner needs to be connected and sealed with a disc-shaped adhesive strip.

[0047] Use a hot hair dryer to heat the butyl glue on the surface of the spacer strip 4 (temperature 50°C) to ensure good adhesion. Use a manual suction cup to align the patch to the predetermined position, apply pressure evenly, ensure that the patch is in full contact with the existing glass 3, and check whether the butyl glue has any virtual joints. If necessary, use a rubber hammer to hammer it to ensure that there are no virtual joints in the butyl glue (pressing time is at least 2 minutes). Before sealing, masking tape needs to be applied to the edge of the glass and the edge of the window frame. When sealing, control the speed of gluing to ensure that the sealant is filled without empty glue. After gluing, it is necessary to use a scraper to trim it, and then remove the masking tape to ensure the beauty of the sealant.

[0048] Comparative Example 1 The composite glass 2 is directly attached to the existing glass 3 without providing a gas interlayer 1 .

[0049] Table 1 Performance parameters of windows of Example 1 and Comparative Example 1 The life of the structure using this application is long: the same life as the external curtain wall glass, and no quality problems will occur during this period. In terms of optical and thermal performance: on the basis of the original building, the high-performance LOW-E modification meets the high transmittance while having a lower K value and SHGC value. The thermal transmittance gIR can be reduced by 50%, SHGC by 25%, and the K value heat transfer coefficient by 40%. The safety of this application: high impact resistance, no breakage due to impact. This application is beautiful: no discoloration, wrinkles, debonding, or bubbles after long-term use. The thermal insulation of this application: the heat transfer coefficient is more than 20% higher than that of the original curtain wall glass. This application reduces noise: the noise is reduced by 5-10 decibels, and the human ear perception is reduced by 50%.

[0050] The above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principle of the present invention should be included in the protection scope of the present invention.

Claims

1. A glass energy-saving structure, characterized in that: It includes composite glass, spacer strips and sealant, and the spacer strips are arranged around the existing glass; The size of the composite glass corresponds to the size of the existing glass, and the composite glass is arranged on the other side of the existing glass through a spacer bar. A gas spacing layer is formed between the composite glass, the existing glass and the spacer bar. The sealant is arranged on the side of the spacer bar away from the gas spacing layer and between the composite glass and the existing glass. The composite glass is arranged on the side inside the room.

2. A glass energy-saving structure according to claim 1, characterized in that: The distance between the spacer and the four edges of the composite glass is not less than 2 mm, preferably 3-5 mm; Adhesive glue is provided on both sides of the spacer strip; The width of the spacer is between 3-20 mm, preferably 9-12 mm; The distance between the four sides of the composite glass and the existing glass exposed outside is not less than 3mm, preferably 3-5mm.

3. The glass energy-saving structure according to claim 1, characterized in that: A supporting block is arranged in the sealant at the lower end of the composite glass.

4. The glass energy-saving structure according to claim 3, characterized in that: The support block is made of plastic or acrylic.

5. A method for implementing a glass energy-saving structure according to any one of claims 1 to 4, characterized in that: The steps include: S1: Clean the existing glass surface, measure the length and width of the existing glass, and measure and mark the position of the spacer strips; S2: placing the composite glass on the workbench assembly, placing the spacer strips on the shaft frame, pasting the spacer strips around the composite glass, and setting the spacer strips on the composite glass through a code strip device to obtain a composite glass pasted with the spacer strips; S3: Heat the spacer bar, align the composite glass with the spacer bar to the marked position in step S1, place the support block at the bottom of the composite glass, apply pressure evenly, and glue the four sides of the composite glass.

6. The implementation method of a glass energy-saving structure according to claim 5, characterized in that: Step S2 also includes rolling up the electrostatic film of the composite glass from four peripheral edges respectively, and then gradually uncovering it completely towards the middle.

7. The method for implementing a glass energy-saving structure according to claim 5, characterized in that: The workbench assembly in step S2 includes a base, a rotating tube, a rotating screw, a sliding head, and a support table; The rotating table is fixedly arranged on the base, the inner thread of the rotating tube is provided with a rotating screw, the upper end of the rotating screw is provided with a sliding head, the sliding head is provided with a supporting table, the supporting table is provided with a ring table, and the composite glass is provided on the ring table during processing; The annular table is provided with an annular buffer pad, which is a rubber pad or a cotton pad; A locking bolt is provided on one side of the sliding head, and the end of the locking bolt abuts against the rotating screw rod, so that the sliding head and the rotating screw rod can be relatively fixed by the locking bolt; The support platform is provided with a plurality of handles along the circumference, and the operator can rotate the support platform at the end of the sliding head and the rotating screw through the handles.

8. The method for implementing a glass energy-saving structure according to claim 5, characterized in that: The shaft frame in step S2 is arranged on one side of the workbench assembly, and the shaft frame includes a side plate, a fixed shaft, an I-shaped wheel, a guide roller, and an output roller; The fixed shaft is arranged between the two side plates, and the I-shaped wheel is rotatably arranged on the fixed shaft; The guide roller is rotatably arranged between the two side plates and arranged above the spool; The two output rollers are rotatably arranged between the two side plates, the centers of the two output rollers are perpendicular to the ground, and the distance between the two output rollers is the same as the thickness of the spacer bar.

9. The method for implementing a glass energy-saving structure according to claim 5, characterized in that: The code bar device in step S2 includes a housing, a first slot and a second slot are provided at the bottom of the housing, and two first cylinders and two second cylinders are symmetrically provided on the housing through the first slot; The shell is provided with a first rotating wheel through the second slot; A third slot is provided on one side of the bottom of the shell, a second rotating wheel is provided in the third slot, two mounting rods are symmetrically provided on the other side of the shell, and a chuck is provided on the shell through the two mounting rods; The chuck is U-shaped, and two sides of the U-shaped chuck are provided with clamping grooves, which cooperate with the mounting rod, and the end of the mounting rod is provided with a mounting nut.

10. The implementation method of a glass energy-saving structure according to claim 5, characterized in that: The heating temperature of step S3 is 45-55°C; In step S3, the support block is symmetrically placed on the bottom of the composite glass, and pressure is applied evenly to ensure that the patch is in full contact with the existing glass and to check whether there is any loose connection. If necessary, a rubber hammer is used to hammer to ensure that there is no loose connection. In step S3, before sealing, masking tape needs to be pasted on the edge of the composite glass and the edge of the window frame. During sealing, the speed of gluing is controlled to ensure that the sealant is filled with no empty glue. After gluing, it is necessary to use a scraper for trimming, and then remove the masking tape to ensure the beauty of the seal.

Citation Information

Patent Citations

  • Building glass's transformation structure

    CN204738692U

  • Sunlight room multi-screen heat insulation device

    CN211923061U

  • Construction method for performing energy conservation transformation for glass of existing building

    CN102661058A

  • Energy saving and noise reduction glass window transformed through existing glass window and transformation method of energy saving and noise reduction glass window

    CN106593220A

  • Negative-pressure hollow glass, manufacturing method and application

    CN112431519A