Impermeable construction method suitable for small depth bay
By using a combination of steel mesh and liquid asphalt in anti-seepage construction, the problem of waterproof and anti-seepage failure caused by vibration and aging in the case of small depth openings is solved, and better crack resistance and aging delay effect are achieved.
Patent Information
- Application Number
- CN202510339710.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2025-03-21
- Publication Date
- 2025-06-13
AI Technical Summary
The existing anti-seepage trim layer is susceptible to vibration and aging when the depth is small, resulting in waterproof and anti-seepage failure.
The combination of steel bar mesh and liquid asphalt is used for anti-seepage construction. The steel bar mesh is used as the stress skeleton, and the liquid asphalt is automatically leveled and fills the gaps to form a high-strength waterproof and impermeable structure.
It improves crack resistance, delays the aging speed of waterproof and impermeable structure, and solves the problem that the anti-seepage trim layer is prone to failure under the small depth opening.
Smart Images

Figure CN120139460A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of building construction, and particularly refers to an anti-seepage construction method applicable to small bay depths and bay widths. Background Art
[0002] In the construction of building construction, it is inevitable that some fine cracks will appear in the concrete pouring. In the construction of positions such as kitchens and bathrooms with small bay depths, small moving loads but high anti-seepage requirements, multiple anti-seepage measures are often required.
[0003] In the existing anti-seepage finishing construction, the waterproof and anti-seepage structures are all solid materials. During use, in the case of small bay depths and bay widths, vibrations or aging are likely to occur, resulting in cracks, causing the anti-seepage materials to crack or break, and losing the waterproof and anti-seepage function. Summary of the Invention
[0004] The purpose of the present invention is to overcome the defects of the prior art, and provide an anti-seepage construction method applicable to small bay depths and bay widths, so as to solve the problem that the conventional anti-seepage finishing in the prior art is greatly affected by vibrations and aging in the case of small bay depths and bay widths, resulting in easy failure of waterproof and anti-seepage.
[0005] To achieve the above purpose, the present invention provides an anti-seepage construction method applicable to small bay depths and bay widths. Based on the situation of small bay depths and bay widths in building construction, it is used for high-grade waterproof and anti-seepage and decorative construction on the floor slab between walls after the secondary structure construction. The construction method includes the following steps:
[0006] S1. Chisel a connecting groove on the floor slab;
[0007] S2. Lay a steel mesh on the floor slab;
[0008] S3. Pour liquid asphalt onto the floor slab until it reaches the top of the steel mesh;
[0009] S4. Place a separation layer on the top of the steel mesh;
[0010] S5. Lay a bottom layer of mortar on the top of the separation layer;
[0011] S6. Lay a decorative surface layer on the bottom layer of mortar;
[0012] S7. Complete the construction.
[0013] By adopting this technical solution, the solid material waterproof and anti-seepage structure in the original anti-seepage decorative layer construction is adjusted to a form combined with a steel mesh and liquid asphalt. The steel mesh serves as the stress-bearing framework sheet, and the liquid asphalt automatically levels and fills the gaps. Thus, a complete high-strength waterproof and anti-seepage structure is formed after the liquid asphalt and the steel mesh are consolidated. Compared with the anti-seepage decorative layer formed by the original waterproof and anti-seepage structure, it has better crack resistance, and the aging speed of the waterproof and anti-seepage structure is slowed down by the long aging time of the asphalt itself, so as to solve the problem of waterproof and anti-seepage failure caused by the anti-seepage decorative layer being vulnerable to vibration and aging in the case of small bay depths and spans.
[0014] Further, step S1 includes:
[0015] Strip-shaped communication grooves are chiseled uniformly along the surface of the bottom plate, and any two communication grooves are ensured to be parallel to each other.
[0016] By adopting this technical solution, communication grooves are opened on the bottom plate for the liquid asphalt to flow, increasing the connection area between the liquid asphalt and the bottom plate, thereby enhancing the connection effect between the liquid asphalt and the bottom plate after consolidation, and providing a prerequisite for avoiding the influence of subsequent laying of bottom steel bars on the flow of liquid asphalt.
[0017] Further, step S1 also includes:
[0018] After chiseling the communication grooves on the surface of the bottom plate, the debris on the surface of the bottom plate is cleaned.
[0019] By adopting this technical solution, the fragments formed by chiseling the communication grooves and the original debris on the bottom plate are prevented from affecting the construction of the anti-seepage decorative layer.
[0020] Further, step S2 includes:
[0021] The bottom steel bars are placed uniformly on the bottom plate, and it is ensured that the bottom steel bars are perpendicular to the communication grooves;
[0022] The top steel bars are placed uniformly on the bottom steel bars, and it is ensured that the top steel bars are perpendicular to the bottom steel bars;
[0023] The bottom steel bars and the top steel bars together form a steel mesh.
[0024] By adopting this technical solution, after the bottom steel bars are set to be perpendicular to the communication grooves, the communication grooves can span multiple bottom steel bars, avoiding the formation of a bottom-closed space between adjacent bottom steel bars that affects the flow of liquid asphalt, thus ensuring the automatic leveling and gap-filling effect of the liquid asphalt after pouring; setting the top steel bars perpendicular to the bottom steel bars can provide the best two-way support effect.
[0025] Further, step S2 also includes:
[0026] Electric heating wires are evenly wound on the bottom steel bars and top steel bars forming the steel bar mesh.
[0027] By adopting this technical solution, the steel bar mesh is enabled to have the ability of overall heating. When the temperature is relatively low, power can be supplied to the electric heating wires to make itself heat up, increasing the fluidity of the liquid asphalt, thereby ensuring the effects of automatic leveling and gap filling of the liquid asphalt.
[0028] Further, before pouring the liquid asphalt onto the bottom plate in step S3, it further includes:
[0029] An anti-seepage plate is set up on the surface of the wall side wall along the circumference of the bottom plate, with its bottom end supported on the surface of the bottom plate and its top end at the same height as the kicker of the secondary structure construction.
[0030] By adopting this technical solution, setting the anti-seepage plate realizes circumferential anti-seepage, and cooperating with the consolidation of the liquid asphalt can ensure the overall waterproof and anti-seepage effect.
[0031] Further, the top surface height of the anti-seepage plate is higher than the top surface height of the steel bar mesh.
[0032] By adopting this technical solution, it is ensured that the anti-seepage plate can play the role of circumferential anti-seepage.
[0033] Further, both the upper and lower surfaces of the separation layer in step S4 are rough surfaces.
[0034] By adopting this technical solution, setting the separation layer as a rough surface can increase the upper and lower surface areas, thereby increasing its connection strength with the lower liquid asphalt and the connection strength with the upper bottom mortar, and further ensuring the overall structural strength of the anti-seepage decorative layer.
[0035] Compared with the prior art, the present invention has the following beneficial effects:
[0036] The solid material waterproof and anti-seepage structure in the original anti-seepage decorative layer construction is adjusted to the form of cooperation between the steel bar mesh and the liquid asphalt. With the steel bar mesh as the stress skeleton sheet, the liquid asphalt automatically levels and fills the gaps, so as to form a complete high-strength waterproof and anti-seepage structure after the consolidation of the liquid asphalt and the steel bar mesh. Compared with the anti-seepage decorative layer formed by the original waterproof and anti-seepage structure, it has better anti-cracking performance, and the aging speed of the waterproof and anti-seepage structure is slowed down by the long aging time of the asphalt itself, so as to solve the problem of waterproof and anti-seepage failure caused by the anti-seepage decorative layer being easily affected by vibration and aging in the case of small bay and room depth. Description of the Drawings
[0037] Figure 1 It is a schematic flow chart of the anti-seepage construction method applicable to small bay and room depth in the present invention;
[0038] Figure 2Schematic diagram of the completion of step S1 in the anti-seepage construction method applicable to small depth and bay in the present invention;
[0039] Figure 3 Schematic diagram of the completion of step S2 in the anti-seepage construction method applicable to small depth and bay in the present invention;
[0040] Figure 4 Schematic diagram of the layout of the anti-seepage plate before step S3 in the anti-seepage construction method applicable to small depth and bay in the present invention;
[0041] Figure 5 Schematic diagram of the completion of step S3 in the anti-seepage construction method applicable to small depth and bay in the present invention;
[0042] Figure 6 Schematic diagram of the completion of step S4 in the anti-seepage construction method applicable to small depth and bay in the present invention;
[0043] Figure 7 Schematic diagram of the completion of steps S5 - S7 in the anti-seepage construction method applicable to small depth and bay in the present invention;
[0044] Figure 8 is Figure 7 Lateral sectional view schematic diagram.
[0045] Explanation of reference numerals: 1, wall; 2, floor slab; 3, connecting groove; 4, steel mesh; 41, bottom layer steel bars; 42, top layer steel bars; 5, anti-seepage plate; 6, liquid asphalt; 7, separation layer; 8, bottom layer mortar; 9, decorative surface layer. Detailed implementation manners
[0046] The present invention will be further described below in conjunction with the accompanying drawings and specific embodiments.
[0047] Please overview the attached Figures 1-8 , the present invention provides an anti-seepage construction method applicable to small depth and bay. Based on the situation of small depth and bay in building construction, it is used for high-grade waterproof and anti-seepage and decorative construction on the floor slab 2 between the walls 1 after secondary structure construction. The construction method includes the following steps: S1, chisel a connecting groove 3 on the floor slab 2; S2, lay a steel mesh 4 on the floor slab 2; S3, pour liquid asphalt 6 onto the floor slab 2 until it reaches the top of the steel mesh 4; S4, place a separation layer 7 on the top of the steel mesh 4; S5, lay a bottom layer mortar 8 on the top of the separation layer 7; S6, lay a decorative surface layer 9 on the bottom layer mortar 8; S7, complete the construction;
[0048] The solid material waterproof and impermeable structure in the original anti-seepage decorative layer construction is adjusted to the form of cooperation between the steel mesh 4 and the liquid asphalt 6. The steel mesh 4 is used as the stress skeleton sheet, and the liquid asphalt 6 automatically levels and fills the gaps. Thus, a complete high-strength waterproof and impermeable structure is formed after the liquid asphalt 6 and the steel mesh 4 are consolidated. Compared with the anti-seepage decorative layer formed by the original waterproof and impermeable structure, it has better crack resistance, and the aging speed of the waterproof and impermeable structure is slowed down by the characteristic that the asphalt itself has a long aging time, so as to solve the problem of waterproof and impermeable failure caused by the anti-seepage decorative layer being easily affected by vibration and aging in the case of small depth and bay.
[0049] Please refer to the appendix Figure 2 , step S1 includes chiseling strip-shaped connecting grooves 3 uniformly on the surface of the bottom plate 2 and ensuring that any two connecting grooves 3 are parallel to each other; opening connecting grooves 3 on the bottom plate 2 for the liquid asphalt 6 to flow, increasing the connection area between the liquid asphalt 6 and the bottom plate 2, thereby increasing the connection effect between the liquid asphalt 6 and the bottom plate 2 after consolidation, and providing a prerequisite for avoiding the influence of the subsequent laying of the bottom layer steel bars 41 on the flow of the liquid asphalt 6;
[0050] Furthermore, step S1 also includes cleaning the sundries on the surface of the bottom plate 2 after chiseling the connecting grooves 3 on the surface of the bottom plate 2; avoiding the influence of the broken blocks formed by chiseling the connecting grooves 3 and the original sundries on the bottom plate 2 on the construction of the anti-seepage decorative layer.
[0051] Please refer to the appendix Figure 3 , step S2 includes uniformly placing the bottom layer steel bars 41 on the bottom plate 2 and ensuring that the bottom layer steel bars 41 are perpendicular to the connecting grooves 3; after the bottom layer steel bars 41 are set to be perpendicular to the connecting grooves 3, the connecting grooves 3 can span multiple bottom layer steel bars 41, avoiding the formation of a bottom-closed space between adjacent bottom layer steel bars 41 that affects the flow of the liquid asphalt 6, thereby ensuring the automatic leveling and gap filling effect of the liquid asphalt 6 after pouring; uniformly placing the top layer steel bars 42 on the bottom layer steel bars 41 and ensuring that the top layer steel bars 42 are perpendicular to the bottom layer steel bars 41; setting the top layer steel bars 42 perpendicular to the bottom layer steel bars 41 can provide the best two-way support effect; the bottom layer steel bars 41 and the top layer steel bars 42 jointly form the steel mesh 4;
[0052] Furthermore, step S2 also includes uniformly winding heating wires on the bottom layer steel bars 41 and the top layer steel bars 42 that form the steel mesh 4; enabling the steel mesh 4 to have the ability to heat as a whole, and when the temperature is low, the heating wires can be electrified to make itself heat, increasing the fluidity of the liquid asphalt 6, thereby ensuring the automatic leveling and gap filling effect of the liquid asphalt 6.
[0053] Please refer to the appendix Figures 4-5, before pouring the liquid asphalt 6 onto the bottom plate 2 in step S3, it further includes setting an anti-seepage plate 5 on the side wall surface of the wall 1 along the circumferential direction of the bottom plate 2, with the bottom end supported on the surface of the bottom plate 2 and the top end at the same height as the kicker of the secondary structure construction; setting the anti-seepage plate 5 realizes circumferential anti-seepage, and cooperating with the consolidation of the liquid asphalt 6 can ensure the overall waterproof and anti-seepage effect; the top surface height of the anti-seepage plate 5 is higher than the top surface height of the steel mesh 4; ensuring that the anti-seepage plate 5 can play a role in circumferential anti-seepage.
[0054] Please refer to the appendix Figure 6 , both the upper and lower surfaces of the separation layer 7 are rough surfaces; setting the separation layer 7 as a rough surface can increase the upper and lower surface areas, thereby increasing its connection strength with the lower liquid asphalt 6 and the connection strength with the upper bottom mortar 8, and further ensuring the overall structural strength of the anti-seepage decorative layer.
[0055] The present invention has been described in detail above in combination with the embodiments of the accompanying drawings. Those of ordinary skill in the art can make various variations to the present invention according to the above description. Therefore, certain details in the embodiments should not constitute a limitation to the present invention, and the present invention will take the scope defined by the appended claims as the protection scope of the present invention.
Claims
1. A method for waterproofing and anti-seepage construction suitable for small depth and span, based on the situation of small depth and span in building construction, used for high-level waterproofing, anti-seepage and decoration construction on the bottom plate between walls after secondary structure construction, characterized in that: The construction method comprises the following steps: S1. Drill a connecting groove on the bottom plate; S2. Lay a steel mesh on the bottom plate; S3, pouring liquid asphalt onto the bottom plate to the top of the steel mesh; S4. Place a spacer layer on top of the steel mesh; S5. Lay the base mortar on the top of the separation layer; S6. Lay the decorative surface layer on the base mortar; S7. Complete the construction.
2. The anti-seepage construction method applicable to small-depth spans according to claim 1 is characterized in that: Step S1 includes: Strip-shaped connecting grooves are evenly distributed along the surface of the bottom plate, and it is ensured that any two connecting grooves are parallel to each other.
3. The anti-seepage construction method applicable to small-depth spans according to claim 2 is characterized in that: Step S1 also includes: After chiseling the connecting grooves on the surface of the base plate, clean the debris on the surface of the base plate.
4. The anti-seepage construction method applicable to small-depth spans according to claim 1, characterized in that: Step S2 includes: Place the bottom steel bars evenly on the bottom plate and ensure that the bottom steel bars are perpendicular to the connecting grooves; Place the top steel bars evenly on the bottom steel bars and ensure that the top steel bars are perpendicular to the bottom steel bars; The bottom layer of steel bars and the top layer of steel bars together form a steel mesh.
5. The anti-seepage construction method applicable to small-depth spans according to claim 4 is characterized in that: Step S2 also includes: Electric heating wires are evenly wound around the bottom steel bars and the top steel bars forming the steel mesh.
6. The anti-seepage construction method applicable to small-depth spans according to claim 1, characterized in that: Step S3, before pouring the liquid asphalt onto the base plate, also includes: An anti-seepage board is set up on the wall side wall surface along the circumference of the bottom plate, the bottom end of which is supported on the bottom plate surface and the top end is at the same height as the secondary structure construction skirting line.
7. The anti-seepage construction method applicable to small-depth spans according to claim 6, characterized in that: In step S3, the top surface height of the anti-seepage plate is higher than the top surface height of the steel mesh.
8. The anti-seepage construction method applicable to small-depth spans according to claim 1, characterized in that: In step S4, both the upper and lower surfaces of the separation layer are rough surfaces.