An anti-counterfeiting element and its preparation method, and an anti-counterfeiting product.

By using a first isolation layer of the same color to cover the gaps in the anti-counterfeiting element, combined with external magnetic field control and fluid medium lubrication, the problem of color loss caused by the gaps between the magnetic pigment sheet and the inner wall of the microcavity is solved, achieving stable and easily identifiable visual effect changes and improving anti-counterfeiting capabilities.

CN120287744BActive Publication Date: 2026-11-17ZHONGCHAO SPECIAL SECURITY TECH +1
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
CN202510500133.3
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2025-04-21
Publication Date
2026-11-17
Estimated Expiration
2045-04-21

AI Technical Summary

Technical Problem

There are gaps between the existing magnetic pigment sheets and the inner wall of the microcavity, resulting in color loss and affecting the visual effect. Furthermore, the change in the size of the gaps during the movement of the magnetic pigment sheets leads to a deterioration in the observed visual effect.

Method used

The design employs a first isolation layer with the same color as the magnetic pigment structure, covering gaps to compensate for color loss. The position and angle of the magnetic pigment structure are controlled by an external magnetic field, and combined with fluid medium lubrication and protection of the magnetic pigment structure, the anti-counterfeiting effect is enhanced.

Benefits of technology

It achieves stable visual effect changes, enhances anti-counterfeiting capabilities, is easy for the public to identify, and protects the magnetic pigment structure, avoiding unexpected visual effect changes and peeling.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN120287744B_ABST
    Figure CN120287744B_ABST
Patent Text Reader

Abstract

This invention relates to the field of optical anti-counterfeiting technology, and discloses an anti-counterfeiting element, its preparation method, and an anti-counterfeiting product. The anti-counterfeiting element includes a substrate, a microstructure forming layer, a transparent protective layer, and at least one microstructure. The microstructure forming layer is located on one side surface of the substrate, and the transparent protective layer is located on the side surface of the microstructure forming layer opposite to the substrate. The microstructure includes a first groove, a first isolation layer, and at least one magnetic pigment structure. The first groove is disposed on the microstructure forming layer, and the first isolation layer covers the inner wall of the first groove, forming a microcavity with the transparent protective layer. The magnetic pigment structure is located within the microcavity, and the magnetic pigment structure has the same color as the first isolation layer. Because the first isolation layer and the magnetic pigment structure have the same color, the color of the first isolation layer itself can compensate for color loss in gaps, ensuring that the entire first microstructure area on the anti-counterfeiting element displays color, thus avoiding partial color loss in the first microstructure.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of optical anti-counterfeiting technology, specifically to an anti-counterfeiting element and its preparation method, and an anti-counterfeiting product. Background Technology

[0002] High-security or high-value-added products such as banknotes, stocks, stamps, checks, airline tickets, credit cards, and passports are generally equipped with anti-counterfeiting elements. These anti-counterfeiting elements can ensure the authenticity of the information carrier and also prevent illegal copying.

[0003] A related technology discloses an anti-counterfeiting element having a microcavity containing magnetic pigment flakes. When an external magnetic field is applied to the anti-counterfeiting element, the magnetic pigment flakes within the microcavity change their position and angle to produce a specific visual effect. Furthermore, by adjusting the external magnetic field, the position and angle of the magnetic pigment can be adjusted to obtain different visual effects.

[0004] However, the aforementioned anti-counterfeiting elements have gaps between the magnetic pigment sheet and the inner wall of the microcavity because the magnetic pigment sheet needs to move and rotate within the microcavity. Furthermore, the size of these gaps changes during the movement and rotation of the magnetic pigment sheet, which leads to color loss in the corresponding areas and a deterioration in the observed visual effect. Summary of the Invention

[0005] In view of this, the present invention provides an anti-counterfeiting element and preparation method, as well as an anti-counterfeiting product, to solve the problem that there are gaps between the existing magnetic pigment sheet and the inner wall of the microcavity, and the size of the gaps changes during the movement or rotation of the magnetic pigment sheet, which leads to the loss of color in the corresponding area, resulting in a deterioration of the observed visual effect.

[0006] In a first aspect, the present invention provides an anti-counterfeiting element, comprising:

[0007] Substrate;

[0008] A microstructure forming layer is located on one side surface of the substrate;

[0009] A transparent protective layer is located on the surface of the microstructure forming layer that faces away from the substrate;

[0010] At least one microstructure includes a first groove, a first isolation layer, and at least one magnetic pigment structure. The first groove is disposed on the microstructure forming layer, the first isolation layer covers the inner wall of the first groove, and the first isolation layer and the transparent protective layer enclose a microcavity. The magnetic pigment structure is located in the microcavity, and the magnetic pigment structure has the same color as the first isolation layer.

[0011] Beneficial effects: The first isolation layer is the same color as the magnetic pigment structure, so the color of the first isolation layer itself can compensate for the color loss in the gaps. Furthermore, even if the size of the gaps changes, because the first isolation layer covers the inner wall of the first groove, the color of the first isolation layer itself can still compensate for the color loss in the gaps, ensuring that the first microstructure area on the anti-counterfeiting element can display a specific color, avoiding the situation where some areas of the first microstructure have missing color, resulting in a deterioration in the observed visual effect. In addition, when an external magnetic field is applied to the anti-counterfeiting element, the magnetic pigment structure in the microcavity changes position and angle under the influence of the external magnetic field, thus changing the observed visual effect. Furthermore, a reverse magnetic field can be applied to reset the magnetic pigment structure in the microcavity, restoring the observed visual effect to its initial state. The visual effect of the anti-counterfeiting element provided by this application can be changed by an external magnetic field, increasing the interactive anti-counterfeiting effect and improving the anti-counterfeiting capability to meet the needs of the high-end anti-counterfeiting field. Moreover, the change in visual effect can be observed with the naked eye, making it easy for the public to identify. In addition, placing the magnetic pigment structure inside the microcavity can protect the magnetic pigment structure and prevent the influence of external temperature and physical friction on the magnetic pigment structure, thereby avoiding unexpected changes in the visual effect of the magnetic pigment structure. This ensures that the optical anti-counterfeiting element can produce stable visual effect changes, and the microcavity can also prevent the magnetic pigment structure from falling off or being lost.

[0012] In one alternative embodiment, the microstructure further includes a fluid medium that fills the microcavity.

[0013] By filling the microcavity with a fluid medium, a lubricating effect can be achieved, reducing friction between the magnetic pigment structure and the inner wall of the microcavity, thus ensuring that the magnetic pigment structure can move and rotate smoothly. In addition, the fluid can also provide a damping effect, which helps to stabilize the movement of the magnetic pigment structure. Furthermore, the fluid medium can further protect the magnetic pigment structure and reduce the impact of the external environment on the magnetic pigment structure.

[0014] In one optional embodiment, the difference in refractive index between the fluid medium and the first isolation layer is less than or equal to a first preset value.

[0015] When light passes through a medium with a large difference in refractive index, a large amount of scattering occurs. As a result, the color of the first isolation layer itself interferes with the visual expression of the magnetic pigment structure during observation, leading to uneven color observation. By making the difference between the refractive index of the first isolation layer and the refractive index of the fluid medium less than or equal to a first preset value, the scattering of light when passing through a medium with a large difference in refractive index is reduced, thereby reducing the interference caused by the color of the first isolation layer itself.

[0016] In one optional embodiment, the fluid medium is a non-polar material, while both the transparent protective layer and the microstructure forming layer are made of polar materials, and the density of the transparent protective layer is less than the density of the fluid medium.

[0017] Nonpolar materials are predominantly characterized by intermolecular forces, which are weaker than hydrogen bonds and ionic bonds. Therefore, using nonpolar materials reduces the surface tension of the fluid medium, thereby minimizing surface concavity and facilitating better filling of microcavities, which in turn benefits the subsequent fabrication of the transparent protective layer. Polar and nonpolar materials are immiscible, preventing the transparent protective layer and microstructure formation layer from slowly dissolving in the fluid medium. The density of the transparent protective layer is lower than that of the fluid medium, ensuring that the transparent protective layer floats on the surface of the fluid medium.

[0018] In one alternative embodiment, a second isolation layer is further included, which is connected to the first isolation layer and is located between the transparent protective layer and the microstructure forming layer.

[0019] The transparent protective layer is separated from the microstructure forming layer by a second isolation layer, which prevents the transparent protective layer and the microstructure from diffusing into each other and causing the protective layer to fail, thereby extending the life of the anti-counterfeiting element.

[0020] In one alternative embodiment, the first isolation layer, the second isolation layer, and the magnetic pigment structure are all Fabry-Perot resonant cavity structures, and the second isolation layer has the same color as the magnetic pigment structure.

[0021] The first isolation layer, the second isolation layer, and the magnetic pigment structure all utilize a Fabry-Perot resonant cavity structure, ensuring that each layer exhibits different visual effects from different viewing angles. The second isolation layer shares the same color as the magnetic pigment structure; therefore, the color of the second isolation layer itself compensates for color gaps in the intervening regions between adjacent microstructures. This allows the entire anti-counterfeiting element to display a specific color, preventing color loss in intervening regions and thus avoiding a deterioration in the observed visual effect.

[0022] In one alternative embodiment, the bottom wall of the first groove is a diffraction grating structure.

[0023] The desired visual effect is achieved through a diffraction grating, further enhancing the anti-counterfeiting capability of the anti-counterfeiting element and improving its naked-eye recognizability. Furthermore, since the first isolation layer is a Fabry-Perot resonant cavity structure, it enhances the diffraction characteristics of the diffraction grating, preventing the visual effect produced by the diffraction grating from being obscured by interference from the fluid medium.

[0024] In one optional embodiment, the length of the magnetic pigment structure is 5µm-50µm, the length of the first groove is less than 500µm, and the depth of the first groove is less than 100µm.

[0025] If the length of the first groove is greater than 500µm, its structure can be observed with the naked eye, affecting the observation effect. Furthermore, an excessively long first groove can cause the fluid medium within the microcavity to be easily carried out during the filling process. If the depth of the first groove is greater than 100µm, it will increase the thickness of the anti-counterfeiting element, thus affecting the manufacturing and integration of anti-counterfeiting products.

[0026] Secondly, the present invention provides a method for preparing an anti-counterfeiting element, comprising:

[0027] Provide base materials;

[0028] A microstructure forming layer is formed on one side surface of the substrate;

[0029] At least one microstructure is formed on the microstructure forming layer;

[0030] The steps of forming the microstructure include: forming a first groove on the microstructure forming layer, forming a first isolation layer on the inner wall of the first groove, providing a magnetic pigment structure, and placing the magnetic pigment structure in the first groove;

[0031] A transparent protective layer is formed on the side of the microstructure forming layer facing away from the substrate, and the transparent protective layer and the first isolation layer enclose a microcavity.

[0032] Beneficial effects: The anti-counterfeiting element is simple to prepare and easy to implement. In addition, the first isolation layer can compensate for the color loss in the gaps, so that the first microstructure area on the anti-counterfeiting element can display a specific color, avoiding the situation where some areas of the first microstructure are missing color, resulting in a deterioration of the observed visual effect. Furthermore, the anti-counterfeiting element can reversibly adjust the position and angle of the magnetic pigment structure through a magnetic field, thereby obtaining an alterable visual effect. This forms a unique advantage for public interaction with the anti-counterfeiting element. In addition, different visual effects can be obtained by adjusting the magnetic field, and the observer does not need to change the viewing angle to perform anti-counterfeiting identification, thereby improving the naked-eye recognition of the anti-counterfeiting element.

[0033] Thirdly, the present invention provides an anti-counterfeiting product, including the aforementioned anti-counterfeiting elements.

[0034] Beneficial effects: The visual effect of this anti-counterfeiting product can be changed by an external magnetic field, thereby achieving an interactive anti-counterfeiting effect, enhancing anti-counterfeiting capabilities, meeting the needs of the high-end anti-counterfeiting field, and the anti-counterfeiting product has the advantages of high efficiency, stability, and mass production capability. Attached Figure Description

[0035] To more clearly illustrate the specific embodiments of the present invention or the technical solutions in the prior art, the drawings used in the description of the specific embodiments or the prior art will be briefly introduced below. Obviously, the drawings described below are some embodiments of the present invention. For those skilled in the art, other drawings can be obtained from these drawings without creative effort.

[0036] Figure 1 This is a schematic diagram of the substrate, microstructure forming layer, first groove, and diffraction grating structure in the preparation of the anti-counterfeiting element in this embodiment of the invention.

[0037] Figure 2 This is a schematic diagram of the structure of the substrate, microstructure forming layer, first groove, diffraction grating structure, first isolation layer and second isolation layer in the preparation of anti-counterfeiting element in an embodiment of the present invention.

[0038] Figure 3 This is a schematic diagram of the structure of the substrate, microstructure forming layer, first groove, diffraction grating structure, first isolation layer, second isolation layer, fluid medium, and magnetic pigment structure in the preparation of the anti-counterfeiting element in this embodiment of the invention.

[0039] Figure 4 This is a schematic diagram of the structure of the substrate, microstructure forming layer, first groove, diffraction grating structure, first isolation layer, second isolation layer, fluid medium, magnetic pigment structure and protective layer in the preparation of anti-counterfeiting elements in this embodiment of the invention;

[0040] Figure 5 This is a schematic diagram of the structure of the first isolation layer in an embodiment of the present invention;

[0041] Figure 6 This is a schematic diagram of the anti-counterfeiting element under the action of a magnetic field in an embodiment of the present invention;

[0042] Figure 7 This is a top view of the anti-counterfeiting product according to an embodiment of the present invention;

[0043] Figure 8 This is a top view of the anti-counterfeiting product according to an embodiment of the present invention under the influence of a magnetic field.

[0044] Explanation of reference numerals in the attached figures:

[0045] 100. Anti-counterfeiting element; 101. Substrate; 102. Microstructure forming layer; 103. Transparent protective layer; 104. Microstructure; 1041. First groove; 1042. Magnetic pigment structure; 1043. Fluid medium; 1044. First isolation layer; 10441. Chromium layer; 10442. Silicon dioxide layer; 10443. Aluminum layer; 105. Second isolation layer; 106. Diffraction grating structure;

[0046] 200. Magnet;

[0047] 300. Carrier. Detailed Implementation

[0048] The present invention will be further described in detail below with reference to the accompanying drawings and embodiments. It is understood that the specific embodiments described herein are merely illustrative of the invention and not intended to limit it. It should also be noted that, for ease of description, only the parts relevant to the invention are shown in the drawings, not all structures. In the following description, descriptions of well-known structures and technologies are omitted to avoid unnecessarily obscuring the concept of the invention. Various structural schematic diagrams according to embodiments of the present invention are shown in the drawings. These figures are not drawn to scale, and some details are enlarged for clarity, and some details may be omitted. The shapes of the various regions and layers shown in the figures, as well as their relative sizes and positional relationships, are merely exemplary and may deviate from actual practices due to manufacturing tolerances or technical limitations. Furthermore, those skilled in the art can design regions / layers with different shapes, sizes, and relative positions as needed. In the context of the present invention, when a layer / element is referred to as being "on" another layer / element, the layer / element may be directly on the other layer / element, or there may be an intermediate layer / element between them. Additionally, if one layer / component is "above" another layer / component in one orientation, then when the orientation is reversed, that layer / component can be "below" that other layer / component.

[0049] In the anti-counterfeiting elements of related technologies, since the magnetic pigment sheet needs to move and rotate within the microcavity, there is a gap between the magnetic pigment sheet and the inner wall of the microcavity. During the movement and rotation of the magnetic pigment sheet, the size of the gap will change, and the gap will cause the color to be missing in the corresponding area, thus resulting in a deterioration of the observed visual effect.

[0050] Therefore, this embodiment of the invention provides an anti-counterfeiting element. The color of the first isolation layer 1044 itself can compensate for the color loss in the gaps, so that the microstructure 104 area on the anti-counterfeiting element can display a specific color, avoiding the situation where some areas of the microstructure 104 are missing color, resulting in a deterioration of the observed visual effect.

[0051] An anti-counterfeiting element provided in this embodiment of the invention, such as... Figure 4 and Figure 6As shown, the structure includes a substrate 101, a microstructure forming layer 102, and at least one microstructure 104. The microstructure forming layer 102 is located on one side surface of the substrate 101, and the transparent protective layer 103 is located on the side surface of the microstructure forming layer 102 opposite to the substrate 101. Each microstructure 104 includes a first groove 1041, a first isolation layer 1044, and at least one magnetic pigment structure 1042. The first groove 1041 is disposed on the microstructure forming layer 102, and the first isolation layer 1044 covers the inner wall of the first groove 1041. The first isolation layer 1044 and the transparent protective layer 103 enclose a microcavity. The magnetic pigment structure 1042 is located in the microcavity, and the magnetic pigment structure 1042 has the same color as the first isolation layer 1044.

[0052] Specifically, the substrate 101 serves as the carrier 300 for the microstructure forming layer 102, providing installation space and supporting the microstructure forming layer 102. The material of the substrate 101 can be polyethylene terephthalate, polyvinyl chloride, paper, or other common anti-counterfeiting substrates 101. The substrate 101 can be opaque, meaning its transmittance is less than or equal to 25%. Anti-counterfeiting elements using this type of substrate 101 need to be observed from the side of the substrate 101 with the microstructure forming layer 102. Of course, the substrate 101 can also be transparent, meaning its transmittance is greater than or equal to 75%. Anti-counterfeiting elements using this type of substrate 101 can be observed from both sides of the substrate 101, allowing the microstructure forming layer 102 to be observed through the substrate 101. The microstructure forming layer 102 serves as the carrier 300 for the microstructure 104 and provides space for forming the microstructure 104. The microstructure forming layer 102 can be a UV-curable material or other materials. Preferably, the microstructure forming layer 102 is a UV-curable material, which can be shaped by UV irradiation, facilitating the processing of the desired structure. The microstructure forming layer 102 can be opaque. Anti-counterfeiting elements using this type of microstructure forming layer 102 need to be observed from the side where the microstructure 104 is formed. Since the microstructure forming layer 102 is opaque, the anti-counterfeiting effect of the microstructure 104 cannot be observed from the side where the microstructure forming layer 102 faces the substrate 101. Of course, the microstructure forming layer 102 can also be transparent, and the substrate 101 also needs to be transparent. Anti-counterfeiting elements using this type of microstructure forming layer 102 can be observed from both sides of the anti-counterfeiting element, and the anti-counterfeiting effect of the microstructure 104 can be observed from both sides. In this embodiment, the number of microstructures 104 is not limited and can be one or more. Each microstructure 104 includes a first groove 1041, a first isolation layer 1044, and at least one magnetic pigment structure 1042. The first groove 1041 is formed on the microstructure forming layer 102, and the opening of the first groove 1041 is located on the upper surface of the microstructure forming layer 102. The first groove 1041 is used to accommodate the magnetic pigment structure 1042. Since the magnetic pigment structure 1042 needs to change its position and angle within the first groove 1041, the maximum length of the magnetic pigment structure 1042 is less than the length, width, and depth of the first microcavity. In this embodiment, the shape of the first groove 1041 and the magnetic pigment structure 1042 is not limited. Those skilled in the art can adjust the shape of the first groove 1041 and the magnetic pigment structure 1042 as needed. Preferably, in this embodiment, the first groove 1041 and the magnetic pigment structure 1042 are both cuboids. The first isolation layer 1044 is located inside the first groove 1041 and covers the inner wall of the first groove 1041. The first isolation layer 1044 and the transparent protective layer 103 enclose each other to form a microcavity.This embodiment does not limit the number of magnetic pigment structures 1042; there can be one or more. Each magnetic pigment structure 1042 has a magnetic layer and a non-magnetic layer. The magnetic layer can be a magnetic oxide or a magnetic metal. Magnetic metals include iron, cobalt, nickel, ferrochrome, or other magnetic metals. Of course, magnetic metals also include alloys with added rare earth elements. Magnetic oxides include iron oxide, chromium oxide, ferrochrome oxide, or other magnetic oxides. The non-magnetic layer can be silicon dioxide, magnesium fluoride, titanium dioxide, zinc oxide, aluminum, chromium, copper, organic materials, or other non-magnetic materials. The non-magnetic or magnetic materials in the magnetic pigment structure 1042 themselves have a specific color (visual effect), or the magnetic pigment structure 1042 contains pigments to form a specific color, so that the anti-counterfeiting element also has a specific color that can be observed with the naked eye in its initial state. When observing the anti-counterfeiting element or an object containing the optical anti-counterfeiting element, the specific color can be observed. The color includes hue, brightness, and saturation. A transparent protective layer 103 is located on the side of the microstructure forming layer 102 facing away from the substrate 101. The transparent protective layer 103 covers the first groove 1041, that is, the transparent protective layer 103 closes the opening of the first groove 1041 and forms a microcavity with the first isolation layer 1044. The microcavity is used to protect the magnetic pigment structure 1042 inside the microcavity, prevent the magnetic pigment structure 1042 inside the microcavity from being disturbed by the external environment, and prevent the magnetic pigment structure 1042 from detaching from the first groove 1041. The transparent protective layer 103 can be a UV-curable material or other materials. Preferably, the transparent protective layer 103 is a UV-curable material, which is convenient for processing the set structure. The light transmittance of the transparent protective layer 103 is greater than or equal to 75%, which allows the visual effect of the microstructure 104 to be observed through the transparent protective layer 103.

[0053] In this embodiment, the anti-counterfeiting element has a first isolation layer 1044 with the same color as the magnetic pigment structure 1042. Therefore, the color of the first isolation layer 1044 itself can compensate for the color loss in the gaps. Furthermore, even if the size of the gaps changes, since the first isolation layer 1044 covers the inner wall of the first groove 1041, the color of the first isolation layer 1044 itself can also compensate for the color loss in the gaps. This ensures that the microstructure 104 area on the anti-counterfeiting element can display a specific color, avoiding the situation where some areas of the microstructure 104 are colorless, resulting in a deterioration in the observed visual effect. Figure 6As shown, magnet 200 can provide an external magnetic field. The arcs in the figure represent magnetic field lines, and the direction indicated by the arrows on the arcs is the direction of the magnetic field. When magnet 200 is placed below the anti-counterfeiting element, the magnetic field lines penetrate the anti-counterfeiting element from bottom to top. Under the influence of the magnetic field, the magnetic pigment structure 1042 moves along the direction of the magnetic field lines until it is parallel to the tangent of the magnetic field lines. The position and angle of the magnetic pigment structure 1042 within the microcavity change under the influence of the external magnetic field, thereby changing the visual effect produced by the magnetic pigment structure 1042. That is, any one or more values ​​of hue, brightness, and saturation exhibited by the observed magnetic structure change. In addition, a reverse magnetic field can be applied to reset the magnetic pigment structure 1042 within the microcavity, restoring the visual effect produced by the magnetic pigment structure 1042 to its initial state. The visual effect of the anti-counterfeiting element provided in this application can be changed by an external magnetic field, increasing the interactive anti-counterfeiting effect and enhancing the anti-counterfeiting capability to meet the needs of the high-end anti-counterfeiting field. Furthermore, the change in the visual effect of the magnetic pigment structure 1042 can be observed with the naked eye, making it easy for the public to identify. In addition, placing the magnetic pigment structure 1042 inside the microcavity can protect the magnetic pigment structure 1042 and prevent the influence of external temperature and physical friction on the magnetic pigment structure 1042, thereby preventing unexpected changes in the visual effect of the magnetic pigment structure 1042, so as to ensure that the optical anti-counterfeiting element can produce stable visual effect changes. The microcavity can also prevent the magnetic pigment structure 1042 from falling off or being lost.

[0054] In one embodiment, such as Figure 4 and 6As shown, each microstructure 104 also includes a fluid medium 1043. The transmittance of the fluid medium 1043 is greater than or equal to 75%, meaning that the fluid medium 1043 is made of a transparent material. Of course, the fluid medium 1043 can also be partially transparent, with the remaining parts opaque. The transparent parts are used to facilitate observation of the visual effects produced by the magnetic pigment structure 1042. The fluid medium 1043 fills the microcavity, and the magnetic pigment structure 1042 is located within the fluid medium 1043. The thickness of the fluid medium 1043 is less than the depth of the first groove 1041, which is beneficial for forming a transparent protective layer 103 on the fluid medium 1043. During the formation of the transparent protective layer 103, the fluid medium 1043 is prevented from overflowing, thus avoiding waste of the fluid medium 1043. The fluid medium 1043 can be a gas, liquid, gel, or other deformable material, so that the magnetic pigment structure 1042 can move and rotate within the fluid medium 1043. The choice of material for the fluid medium 1043 does not affect the visual effects or magnetic properties of the magnetic pigment structure 1042. Filling the microcavity with fluid medium 1043 provides lubrication, reducing friction between the magnetic pigment structure 1042 and the inner wall of the first microcavity. This ensures smooth movement and rotation of the magnetic pigment structure 1042. Furthermore, the fluid provides damping, helping to stabilize the movement of the magnetic pigment structure 1042. Additionally, the fluid medium 1043 further protects the magnetic pigment structure 1042, reducing the impact of the external environment. The transmittance of the fluid medium 1043 is greater than or equal to 75%, minimizing the influence of its own color on the visual effect of the magnetic pigment structure 1042, thus ensuring clear observation of its visual effect by the public. Since the fluid medium 1043 is located within the microcavity, the microcavity protects both the fluid medium 1043 and the magnetic pigment structure 1042, preventing damage to the microcavity structure or loss of the fluid medium 1043 due to physical friction or changes in external temperature and humidity. In addition, the first isolation layer 1044 is located between the fluid medium 1043 and the inner wall of the groove, and is used to separate the fluid medium 1043 from the inner wall of the first groove 1041 to prevent the fluid medium 1043 from corroding the inner wall of the first groove 1041.

[0055] In one embodiment, the difference between the refractive index of the first isolation layer 1044 and the refractive index of the fluid medium 1043 is less than or equal to a first preset value, which is 0.2. For example, the fluid medium 1043 is made of glycerol, and the first isolation layer 1044 is made of acrylic resin. Glycerol has a refractive index of 1.47, and acrylic resin has a refractive index of 1.49. When light passes through a medium with a large difference in refractive index, a large amount of scattering occurs, which causes the color of the isolation layer itself to interfere with the visual effect of the magnetic pigment structure 1042 during observation, resulting in uneven color observation. By making the difference between the refractive index of the first isolation layer 1044 and the refractive index of the fluid medium 1043 less than or equal to 0.2, the scattering of light when passing through a medium with a large difference in refractive index is reduced, thereby reducing the interference caused by the color of the isolation layer itself.

[0056] In one embodiment, the fluid medium 1043 is a non-polar material, such as carbon tetrachloride or glycerol. Both the transparent protective layer 103 and the microstructure forming layer 102 are made of polar materials. The transparent protective layer 103 and the microstructure forming layer 102 can be made of the same material or different materials. Preferably, in this embodiment, both the transparent protective layer 103 and the microstructure forming layer 102 are made of acrylate, and the density of the transparent protective layer 103 is less than the density of the fluid medium 1043. Non-polar materials are generally characterized by intermolecular forces, which are weaker than hydrogen bonds and ionic bonds. Therefore, using non-polar materials can reduce the surface tension of the fluid medium 1043, thereby reducing the degree of concavity or depression on the surface of the fluid medium 1043, which is beneficial for better filling of the microcavities and thus facilitates the subsequent preparation of the transparent protective layer 103. The polar material is immiscible with the non-polar material, thus avoiding the situation where the transparent protective layer 103 and the microstructure forming layer 102 slowly dissolve in the fluid medium 1043. The density of the transparent protective layer 103 is less than the density of the fluid medium 1043, ensuring that the transparent protective layer 103 floats on the fluid surface.

[0057] In one embodiment, a second isolation layer 105 is further included, which is connected to the first isolation layer 1044. The anti-counterfeiting element may have a first isolation layer 1044 or a second isolation layer 105 alone, or both the first isolation layer 1044 and the second isolation layer 105 may be present. Preferably, the anti-counterfeiting element has a first isolation layer 1044 and a second isolation layer 105, which are integrally formed or can be formed independently. The second isolation layer 105 is located between the transparent protective layer 103 and the microstructure forming layer 102, that is, the second isolation layer 105 covers the surface of the microstructure forming layer 102 excluding all openings of the first groove 1041. Since both the transparent protective layer 103 and the microstructure forming layer 102 are polar materials, mutual diffusion may occur between the transparent protective layer 103 and the microstructure forming layer 102, which may lead to the failure of the protective layer. By adding the second isolation layer 105, the transparent protective layer 103 and the microstructure forming layer 102 are separated, thereby avoiding mutual diffusion between the transparent protective layer 103 and the microstructure forming layer 104, and thus extending the life of the anti-counterfeiting element.

[0058] In one embodiment, the first isolation layer 1044, the second isolation layer 105, and the magnetic pigment structure 1042 are all Fabry-Perot resonant cavity structures, meaning that the magnetic pigment structure 1042, the first isolation layer 1044, and the second isolation layer 105 are all composed of metal / dielectric / metal stacks, or dielectric / metal / dielectric stacks, wherein the dielectric can be silicon dioxide or other dielectric materials. Specifically, taking the first isolation layer 1044 as an example, as... Figure 5As shown, the first isolation layer 1044 is composed of a chromium layer 10441, a silicon dioxide layer 10442, and an aluminum layer 10443 stacked together. The magnetic pigment structure 1042 and the second isolation layer 105 can also be made of the same material as the first isolation layer 1044. Of course, the magnetic pigment structure 1042 and the second isolation layer 105 can also be made of other metals and media. Preferably, in this embodiment, the magnetic pigment structure 1042 is made of nickel / silicon dioxide / aluminum / iron / aluminum / silicon dioxide / nickel, wherein the thickness of nickel is 7nm, the thickness of silicon dioxide is 390nm, the thickness of aluminum is 40nm, and the thickness of iron is 40nm. The symmetrically distributed nickel / silicon dioxide / aluminum and aluminum / silicon dioxide / nickel structures on both sides form a Fabry-Perot structure. The magnetic pigment structure 1042 appears golden yellow when viewed from the nickel side. The iron in the middle is a magnetic layer, capable of moving and rotating under a magnetic field. The nickel on both sides also provides some magnetism, enhancing the movement and rotation capabilities of the magnetic pigment structure 1042, thereby improving the interactive anti-counterfeiting effect of the anti-counterfeiting element. Furthermore, the magnetic pigment structure 1042 also features a surface relief structure, such as a holographic diffraction structure or a submicron scale structure, which adds specific visual effects to increase the complexity of the visual effect and thus enhance the anti-counterfeiting capability of the anti-counterfeiting element. The second isolation layer 105 is the same color as the magnetic pigment structure 1042. Therefore, the color of the second isolation layer 105 itself can compensate for the color gaps in the interval areas between two adjacent microstructures 104, ensuring that the entire anti-counterfeiting element displays a specific color and avoiding the deterioration of the observed visual effect due to color gaps in the interval areas.

[0059] In one embodiment, the bottom wall of each first groove 1041 is a diffraction grating structure 106. Alternatively, the bottom wall of some of the first grooves 1041 can be a diffraction grating structure 106, or it can be omitted. The diffraction grating structure 106 consists of several triangular prisms arranged sequentially along the length of the first microcavity, and several triangular pyramids covering the entire bottom wall of the first groove 1041. Each triangular prism has a height of 0.3 μm and a bottom width of 2 μm. The diffraction grating achieves a specific visual effect, further enhancing the complexity of the visual effect presented by the anti-counterfeiting element, thereby further improving the anti-counterfeiting capability and the naked-eye recognizability of the anti-counterfeiting element. Furthermore, since the first isolation layer 1044 is a Fabry-Perot resonant cavity structure, it enhances the diffraction characteristics of the diffraction grating, avoiding interference from the fluid medium 1043, thus preventing the observation of the visual effect produced by the diffraction grating.

[0060] In one embodiment, the angle between the inner wall of the first groove 1041 and the surface of the microstructure forming layer 102 facing away from the substrate 101 is A, where 90° < A < 180°. That is, the angle between the inner wall of the first groove 1041 and the upper surface of the microstructure forming layer 102 is between 90° and 180°. Obviously, the inclined inner wall of the first groove 1041 facilitates the preparation of the first isolation layer 1044 on the inner wall of the first groove 1041, and facilitates the smooth filling of the fluid medium 1043 into the first groove 1041.

[0061] In one embodiment, the shapes of the magnetic pigment structure 1042 and the first groove 1041 are not limited. The shape of the magnetic pigment structure 1042 may be the same as or different from the shape of the first groove 1041. Preferably, in this embodiment, the shape of the first groove 1041 is the same as the shape of the magnetic pigment structure 1042, which is a cuboid. The length of the magnetic pigment structure 1042 is 5µm-50µm. The length and depth of the first groove 1041 are both greater than the maximum length of the magnetic pigment structure 1042. Since the first magnetic pigment only moves and rotates in the length and depth directions, the first groove... The width of the groove 1041 may not exceed the maximum length of the magnetic pigment structure 1042. If movement and deflection in the width direction of the first groove 1041 are required, the width of the first groove 1041 must also exceed the maximum length of the magnetic pigment structure 1042. Furthermore, the length of the first groove 1041 must be less than 500 μm, and the depth of the first groove 1041 must be less than 100 μm. If the length of the first groove 1041 exceeds 500 μm, its structure can be observed with the naked eye, affecting the observation effect. Additionally, during the filling of the fluid medium 1043, the fluid medium 1043 within the microcavity may be easily carried out. If the depth of the first groove 1041 exceeds 100 μm, the thickness of the anti-counterfeiting element will increase, thus affecting the manufacturing and integration with anti-counterfeiting products.

[0062] In one embodiment, multiple microstructures 104 form a group of microstructures 104, which are arranged at intervals along a straight line. The anti-counterfeiting element has multiple groups of microstructures 104, which are spaced apart on the microstructure forming layer 102. Adjacent microstructures 104 in different groups are aligned, and adjacent microstructures 104 in different groups can also be staggered. Of course, the multiple microstructures 104 can also be randomly arranged to reduce diffraction and avoid interference in the observation room.

[0063] Secondly, the present invention provides a method for preparing an anti-counterfeiting element, comprising the following steps:

[0064] S101 provides a substrate 101, which can be made of polyethylene terephthalate, polyvinyl chloride, paper, or other common anti-counterfeiting substrates 101, and the transmittance of the substrate 101 is less than or equal to 25%.

[0065] S102, a microstructure forming layer 102 is formed on one side surface of the substrate 101.

[0066] Specifically, the microstructure forming layer 102 can be acrylate or other polar materials. The microstructure forming layer 102 is initially liquid, and the liquid microstructure forming layer 102 material is spin-coated onto the surface of the substrate 101.

[0067] S103, a first groove 1041 is formed on the microstructure forming layer 102.

[0068] The first groove 1041 is fabricated on the microstructure forming layer 102 using a molding process. Molding methods include hot molding and UV molding, with UV molding being preferred. The UV molding machine is automated, which not only meets the requirements for embossing thickness, achieving clear and bright patterns with high positioning accuracy and reproduction, but also avoids the high temperatures of hot molding. UV molding allows for efficient, stable, and mass production of the first groove 1041.

[0069] Specifically, a master plate with the shape of the first groove 1041 is pressed into the liquid microstructure forming layer 102, and the liquid microstructure forming layer 102 is solidified and shaped by ultraviolet light irradiation. Then, the master plate is peeled off from the solidified microstructure forming layer 102 to complete the fabrication of the first groove 1041.

[0070] S104, such as Figure 1 As shown, a diffraction grating structure 106 is formed at the bottom of the first groove 1041;

[0071] The diffraction grating structure 106 can be fabricated by mechanical scribing, holographic ion beam etching, or lamination.

[0072] S105, as Figure 2 As shown, a first isolation layer 1044 and a second isolation layer 105 are formed by a deposition process, and the first isolation layer 1044 encloses and forms a second groove.

[0073] The deposition process includes physical vapor deposition and chemical vapor deposition, and a chromium layer 10441, a silicon dioxide layer 10442, and an aluminum layer 10443 are formed sequentially using the deposition process. Of course, step S105 can also be performed directly after step S103, and the first isolation layer 1044 or the second isolation layer 105 can also be fabricated separately in step S104.

[0074] S106, as Figure 3 As shown, a magnetic pigment structure 1042 is provided, and the magnetic pigment structure 1042 and the fluid medium 1043 are placed in the second groove.

[0075] S105, as shown in the figure, a transparent protective layer 103 is formed on the side surface of the second isolation layer 105 opposite to the microstructure forming layer 102.

[0076] Specifically, the transparent protective layer 103 is made of acrylic ester. The liquid transparent protective layer 103 is coated onto the surface of the second isolation layer 105 opposite to the microstructure 104 using a coating device. The liquid transparent protective layer 103 is also coated onto the fluid medium 1043. Then, the liquid transparent protective layer 103 is cured and shaped by ultraviolet light irradiation. The transparent protective layer 103 and the second groove form a second microcavity.

[0077] There are two approaches to placing the magnetic pigment structure 1042 inside the second groove. One approach is to fill the second groove with the magnetic pigment structure 1042 dispersed in the fluid medium 1043, and then evaporate the fluid medium 1043 by drying. In this case, the fluid medium 1043 inside the microcavity is air. The other approach is to fill the second groove with the magnetic pigment structure 1042 dispersed in the fluid medium 1043, retaining the solution. In this case, the microcavity consists of liquid or a mixture of liquid and air.

[0078] The method for preparing the anti-counterfeiting element provided in this embodiment is simple and easy to implement. In addition, the first isolation layer 1044 can compensate for the color loss in the gaps, so that the microstructure 104 area on the anti-counterfeiting element can display a specific color, avoiding the situation where some areas of the microstructure 104 are missing color, resulting in a deterioration of the observed visual effect. Furthermore, the anti-counterfeiting element can reversibly adjust the position and angle of the magnetic pigment structure 1042 through a magnetic field, thereby obtaining an alterable visual effect. This forms a unique advantage for public interaction with the anti-counterfeiting element. In addition, different visual effects can be obtained by adjusting the magnetic field, and the observer can perform anti-counterfeiting identification without changing the observation angle, thereby improving the naked-eye recognition of the anti-counterfeiting element.

[0079] Thirdly, the present invention provides an anti-counterfeiting product, such as... Figure 7 As shown, the device includes the aforementioned anti-counterfeiting element 100 and a carrier 300. The carrier 300 can be one of the following: banknotes, stocks, stamps, checks, airline tickets, various ticket labels, valuable documents, and various certificates. The anti-counterfeiting element can be transferred to the carrier 300 by pasting, hot stamping, or other transfer methods. In the absence of an external magnetic field, the optical anti-counterfeiting element exhibits the initial visual effect of the magnetic pigment structure 1042.

[0080] like Figure 8As shown, in this embodiment, when the magnet 200 approaches the anti-counterfeiting product, the visual effect of the optical anti-counterfeiting element changes.

[0081] The anti-counterfeiting product provided in this embodiment has an optical effect that can be changed by an external magnetic field, thereby achieving an interactive anti-counterfeiting effect, enhancing anti-counterfeiting capabilities, meeting the needs of the high-end anti-counterfeiting field, and having the advantages of high efficiency, stability, and mass production capability.

[0082] The above description does not provide detailed explanations of the technical aspects of each layer's patterning, etching, etc. However, those skilled in the art should understand that various technical means can be used to form layers and regions of the desired shape. Furthermore, to form the same structure, those skilled in the art can also design methods that are not entirely identical to those described above. Additionally, although various embodiments have been described above, this does not mean that the measures in the various embodiments cannot be used advantageously in combination.

[0083] Although embodiments of the invention have been described in conjunction with the accompanying drawings, those skilled in the art can make various modifications and variations without departing from the spirit and scope of the invention, and such modifications and variations all fall within the scope defined by the appended claims.

Claims

1. An anti-counterfeiting element, characterized in that, include: Substrate (101); A microstructure forming layer (102) is located on one side surface of the substrate (101); A transparent protective layer (103) is located on the side surface of the microstructure forming layer (102) facing away from the substrate (101); At least one microstructure (104) includes a first groove (1041), a first isolation layer (1044), and at least one magnetic pigment structure (1042). The first groove (1041) is disposed on the microstructure forming layer (102). The first isolation layer (1044) covers the inner wall of the first groove (1041), and the first isolation layer (1044) and the transparent protective layer (103) enclose a microcavity. The magnetic pigment structure (1042) is located in the microcavity, and the magnetic pigment structure (1042) has the same color as the first isolation layer (1044).

2. The anti-counterfeiting element according to claim 1, characterized in that, The microstructure (104) further includes a fluid medium (1043) that fills the microcavity.

3. The anti-counterfeiting element according to claim 2, characterized in that, The difference in refractive index between the fluid medium (1043) and the first isolation layer (1044) is less than or equal to a first preset value.

4. The anti-counterfeiting element according to claim 3, characterized in that, The fluid medium (1043) is a non-polar material, while the transparent protective layer (103) and the microstructure forming layer (102) are both made of polar materials, and the density of the transparent protective layer (103) is less than the density of the fluid medium (1043).

5. The anti-counterfeiting element according to any one of claims 1-4, characterized in that, It also includes a second isolation layer (105), which is connected to the first isolation layer (1044) and is located between the transparent protective layer (103) and the microstructure forming layer (102).

6. The anti-counterfeiting element according to claim 5, characterized in that, The first isolation layer (1044), the second isolation layer (105), and the magnetic pigment structure (1042) are all Fabry-Perot resonant cavity structures, and the second isolation layer (105) and the magnetic pigment structure (1042) have the same color.

7. The anti-counterfeiting element according to claim 1 or 6, characterized in that, The bottom wall of the first groove (1041) is a diffraction grating structure (106).

8. The anti-counterfeiting element according to claim 1, characterized in that, The length of the magnetic pigment structure (1042) is 5um-50um, the length of the first groove (1041) is less than 500um, and the depth of the first groove (1041) is less than 100um.

9. A method for preparing an anti-counterfeiting element, characterized in that, include: Provide substrate (101); A microstructure forming layer (102) is formed on one side surface of the substrate (101). At least one microstructure (104) is formed on the microstructure forming layer (102). The steps of forming the microstructure (104) include: forming a first groove (1041) on the microstructure forming layer (102), forming a first isolation layer (1044) on the inner wall of the first groove (1041), providing a magnetic pigment structure (1042), placing the magnetic pigment structure (1042) in the first groove (1041), and the magnetic pigment structure (1042) having the same color as the first isolation layer (1044); A transparent protective layer (103) is formed on the side of the microstructure forming layer (102) facing away from the substrate (101), and the transparent protective layer (103) and the first isolation layer (1044) enclose a microcavity.

10. An anti-counterfeiting product, characterized in that, Includes the anti-counterfeiting element (100) as described in any one of claims 1-8.

Citation Information

Patent Citations

  • Optical anti-counterfeiting element and preparation method thereof

    CN114590054A

  • Safety thread or strip and preparation method thereof