A riveting process and equipment for ultra-thin silicon steel sheets
By using ultra-thin silicon steel sheet riveting equipment and processes, and by utilizing interference fit and embedded interlocking structures, combined with online quality monitoring, the problems of deformation and connection strength during the riveting process of ultra-thin silicon steel sheets have been solved, and the stable production of high-performance motors has been achieved.
Patent Information
- Application Number
- CN202511218972.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2025-08-28
- Publication Date
- 2026-11-10
- Estimated Expiration
- 2045-08-28
AI Technical Summary
Existing riveting processes are insufficient to achieve adequate connection strength on ultra-thin silicon steel sheets while avoiding material deformation, which can lead to unstable motor performance and potential product quality issues.
Using ultra-thin silicon steel sheet riveting equipment and processes, the stability and connection strength of the riveting process are ensured through the interference fit between the riveting punch and the positioning structure and the embedded interlocking structure, combined with online quality monitoring.
Stable riveting of ultra-thin silicon steel sheets has been achieved, avoiding deformation, improving the connection strength and production reliability of the motor, and ensuring the mass production of high-performance motors.
Smart Images

Figure CN121036439B_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of metal sheet stamping technology, specifically to a riveting process and equipment for ultra-thin silicon steel sheets. Background Technology
[0002] In the modern motor manufacturing industry, in pursuit of higher energy efficiency, lower core losses, and overall lightweight and compact motor design, motor designers are increasingly inclined to use ultra-thin silicon steel sheets (e.g., 0.1 mm thick) as the core lamination material. The design of such high-performance motors often strives for perfection, with extremely strict dimensional tolerances; for example, the radial width (yoke width) of the stator or rotor may be designed to be very narrow.
[0003] However, firmly riveting these ultra-thin, precision silicon steel sheets together to form a core with sufficient structural strength remains a major technical challenge for the industry. Existing riveting processes suffer from the following drawbacks: Square or V-shaped snap-fitting process: This method uses significant plastic deformation to compress the material and form snap-fit points. When processing ultra-thin silicon steel sheets, this compression can easily lead to uneven material flow, causing the narrow diameter portion of the silicon steel sheet to expand and produce wavy deformation. This deformation can severely affect subsequent winding processes and even lead to uneven air gaps in the motor, ultimately affecting the overall performance and quality of the motor.
[0004] Traditional circular snap-fitting process: This process works reasonably well for materials thicker than 0.2mm. However, when applied to silicon steel sheets thinner than 0.1mm, the material's plastic deformation is extremely limited due to its thinness. This results in insufficient friction and locking force at the snap-fit points, meaning inadequate riveting force. Consequently, the iron core is highly susceptible to single or multiple sheets detaching during subsequent production and handling processes, and even in high-frequency vibration environments like motors, posing a serious product quality hazard.
[0005] Therefore, there is an urgent need for a new riveting technology that can be specifically designed for ultra-thin silicon steel sheets, ensuring sufficient riveting force while avoiding harmful deformation of the sheet body, thereby enabling stable and reliable mass production of high-performance motor cores. Summary of the Invention
[0006] In order to overcome the shortcomings and deficiencies of the existing technology, the purpose of this invention is to provide an ultra-thin silicon steel sheet riveting process that can ensure connection strength without causing deformation of the sheet, as well as a matching high-precision riveting device with online quality monitoring function.
[0007] This invention is achieved through the following technical solution: In a first aspect, the present invention discloses an ultra-thin silicon steel sheet riveting device, comprising: The rivet punch, the rivet fixture located below the rivet punch, and several rivet point punches set on the lower end face of the rivet punch and parallel to the rivet punch; The rivet fixture is provided with a positioning structure for interference fit with the stamped silicon steel sheet, and the inner diameter of the positioning structure is 3μm to 7μm longer than the diameter of the rivet punch.
[0008] In conjunction with the first aspect, the rivet point punch is further described as having a cylindrical structure, and the connection between the lower end face and the side face of the rivet point punch is provided with an annular inclined surface that can realize both punching and extrusion forming functions.
[0009] In conjunction with the first aspect, furthermore, the inner diameter of the positioning structure is 5 μm longer than the diameter of the rivet punch.
[0010] Secondly, the present invention also discloses a riveting process for an ultra-thin silicon steel sheet riveting device, which includes the following steps: S100. Place the silicon steel sheet between the rivet fixture and the rivet punch; S200. The rivet punch presses down to impact the silicon steel sheet, punching out a first circular silicon steel sheet that corresponds to the shape of the rivet punch. The rivet punch punches out several through holes on the first circular silicon steel sheet, and the first circular silicon steel sheet is interference-fitted to the positioning structure. S300. Repeat steps S100 to S200, whereby the second silicon steel sheet stamped out by the rivet punch adheres to the first silicon steel sheet and pushes the first silicon steel sheet downward toward the positioning structure. At the same time, the rivet punch stamps the second silicon steel sheet to form a rivet structure, so that the rivet structure is embedded in the through hole stamped out by the first silicon steel sheet for engagement. S400. Repeat step S300, where the subsequent silicon steel sheet pushes the aforementioned silicon steel sheet downwards into the rivet fixture, while adjacent rivet structures interlock and engage with each other.
[0011] In conjunction with the second aspect, the positioning structure is further described as a vertically penetrating columnar through-hole; The riveting process further includes step S500: after the silicon steel sheets in the positioning structure reach the corresponding number, the silicon steel sheet at the bottom of the positioning structure is detached from the positioning structure.
[0012] In conjunction with the second aspect, the process further includes the following online quality monitoring step S600: S601. During the process of embedding the rivet structure into the through hole, the instantaneous pressure value and displacement value of the rivet point punch are collected simultaneously to form a pressure-displacement dataset; S602. Based on the dataset, the quality of this riveting is determined using a preset quality determination algorithm; S603. Classify the finished riveted products as qualified or unqualified according to the determination result.
[0013] In combination with the second aspect, further, the quality determination algorithm includes a riveting work determination step, which comprises: pre-setting a standard riveting work interval through statistical analysis of the pressure-displacement data set of historical qualified products ; collecting pressure in real time during the current riveting process with respect to displacement as a function ; performing integration on within the effective riveting stroke to calculate the actual riveting work consumed in the current riveting process ; comparing whether falls within the standard interval , and determining that the riveting work is qualified if the condition is satisfied ; The calculation of the actual riveting work follows the definite integral rule:
[0014] wherein, is the actual riveting work; is the instantaneous pressure collected by the sensor when the riveting point punch is at the displacement point ; is the instantaneous displacement of the riveting point punch; is the displacement point at the start of riveting; is the displacement point at the end of riveting.
[0015] In combination with the second aspect, further, the quality determination algorithm further includes a forming gradient stability determination step, which is executed on the basis that the riveting work determination is qualified, and comprises: identifying the key forming section where the main plastic deformation of the material occurs in the pressure-displacement curve ; calculating the gradient function of the pressure-displacement curve within this section ; calculating the standard deviation of the gradient function within this section ; comparing with a preset maximum allowable gradient fluctuation threshold , and determining that the forming process is stable if ; The calculation formula of the gradient function is:
[0016] Standard deviation The calculation formula is:
[0017]
[0018] in, For the rivet point punch at the displacement point The instantaneous pressure collected by the sensor at that time; The average gradient within the critical forming section; The standard deviation of the gradient within the critical forming section; This is the starting displacement point for the critical forming section; This is the end displacement point of the critical forming section.
[0019] In conjunction with the second aspect, the final quality determination is derived from a multi-factor weighted Gaussian model, which includes the following steps: Extract n key feature parameters ; For each feature parameter According to its ideal target value and acceptable deviation The individual quality scores are calculated using the Gaussian function. ; Each feature is assigned a score based on its importance to the final product performance. Assign a weight coefficient ; Calculate the weighted sum of all individual scores to obtain the final overall quality score. ; Will With the set minimum passing score In comparison, if If so, it will ultimately be determined to be a qualified product; Overall quality score The calculation formula is:
[0020]
[0021] in, For the first Individual quality scores for each feature; For the first The weight coefficients of each feature; For the first The actual measured values of the key features in this study; For the first The ideal target value for each feature; For the first Acceptable standard deviation of key features; The total number of key features used for evaluation; Natural exponential function .
[0022] Thirdly, the present invention also discloses a computer device comprising a memory, a processor, and a computer program stored in the memory and executable on the processor, the processor running the computer program to implement the riveting process as described above.
[0023] Fourthly, the present invention also discloses a computer-readable storage medium having a computer program stored thereon, the program being executed by a processor to implement the riveting process as described above.
[0024] The beneficial effects of this invention are: This invention discloses an ultra-thin silicon steel sheet riveting device, riveting process, method, computer equipment, and storage medium. By precisely guiding the material into the positioning structure for forming, it completely solves the deformation problem caused by radial extrusion in traditional processes. During the riveting process, the physically embedded interlocking structure provides a connection strength far exceeding that of traditional friction-type riveting points, eliminating the risk of sheet falling off. This solves the key technical bottleneck of ultra-thin silicon steel sheet riveting and provides a feasible technical path for the large-scale production of high-performance, lightweight motors. Attached Figure Description
[0025] The present invention will be further described with reference to the accompanying drawings, but the embodiments in the drawings do not constitute any limitation on the present invention. For those skilled in the art, other drawings can be obtained based on the following drawings without creative effort.
[0026] Figure 1 This is a schematic diagram of the riveting device provided in an embodiment of the present invention.
[0027] Figure 2 This is a partial structural schematic diagram of a riveting device provided in an embodiment of the present invention.
[0028] Figure 3 This is a flowchart of a riveting process provided in an embodiment of the present invention.
[0029] Figure 4 This is a schematic diagram of the structure of an electronic device provided in an embodiment of the present invention.
[0030] Figure 5 This is a schematic diagram of a storage medium provided in an embodiment of the present invention. Detailed Implementation
[0031] To make the above-mentioned objects, features, and advantages of the present invention more apparent and understandable, specific embodiments of the present invention will be described in detail below with reference to the accompanying drawings. Many specific details are set forth in the following description to provide a thorough understanding of the present invention. However, the present invention can be practiced in many other ways different from those described herein, and those skilled in the art can make similar modifications without departing from the spirit of the present invention. Therefore, the present invention is not limited to the specific embodiments disclosed below.
[0032] In the description of this invention, it should be understood that the terms "center," "longitudinal," "lateral," "length," "width," "thickness," "upper," "lower," "front," "rear," "left," "right," "vertical," "horizontal," "top," "bottom," "inner," "outer," "clockwise," "counterclockwise," "axial," "radial," and "circumferential" indicate the orientation or positional relationship based on the orientation or positional relationship shown in the accompanying drawings. They are used only for the convenience of describing this invention and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, or be constructed and operated in a specific orientation. Therefore, they should not be construed as limitations on this invention.
[0033] Furthermore, the terms "first" and "second" are used for descriptive purposes only and should not be construed as indicating or implying relative importance or implicitly specifying the number of technical features indicated. Thus, a feature defined as "first" or "second" may explicitly or implicitly include at least one of that feature. In the description of this invention, "a plurality of" means at least two, such as two, three, etc., unless otherwise explicitly specified.
[0034] Example 1 like Figure 1 and Figure 2 As shown, this embodiment discloses an ultra-thin silicon steel sheet riveting device, which includes: The rivet punch 100, the rivet fixture 101 located below the rivet punch 100, and a plurality of rivet point punches 102 disposed on the lower end face of the rivet punch 100 and parallel to the rivet punch 100. The rivet fixture 101 is provided with a positioning structure 103 for interference fit with the stamped silicon steel sheet. The inner diameter of the positioning structure 103 is 3μm to 7μm longer than the diameter of the rivet punch 100.
[0035] Preferably, the inner diameter of the positioning structure 103 is 5 μm longer than the diameter of the rivet punch 100 to achieve the optimal interference fit between the circular silicon steel sheet and the positioning structure 103. With this diameter difference, the stamped or cut circular silicon steel sheet can be pushed into the positioning structure 103 for interference fit under the action of the rivet punch 100. If the circular silicon steel sheet continues to be pushed downwards by an external force into the positioning structure 103, the circular silicon steel sheet can be moved without damaging its structural integrity; in another case, the circular silicon steel sheet can be temporarily "fixed" to the positioning structure 103 under the action of friction.
[0036] The working process of the above-mentioned riveting equipment is as follows: S100. Place the silicon steel sheet between the rivet fixture 101 and the rivet punch 100; S200. The rivet punch 100 presses down to impact the silicon steel sheet, and punches out a first circular silicon steel sheet corresponding to the shape of the rivet punch 100. The rivet punch 102 punches out several through holes on the first circular silicon steel sheet, and at the same time, the first circular silicon steel sheet is interference-fitted to the positioning structure 103. S300. Repeat steps S100 to S200, whereby the second silicon steel sheet stamped out by the rivet punch 100 is attached to the first silicon steel sheet and the first silicon steel sheet is pushed down towards the positioning structure 103. At the same time, the rivet punch 102 stamps the second silicon steel sheet to form a rivet structure, so that the rivet structure is embedded in the through hole stamped out by the first silicon steel sheet for engagement. S400. Repeat step S300, where the subsequent silicon steel sheet pushes the aforementioned silicon steel sheet downwards towards the rivet fixture 101, while adjacent rivet structures interlock and engage with each other.
[0037] The embodiment adopts an embedded fit of "one protrusion and one hole", which precisely guides the flow direction of the silicon steel sheet material into the pre-opened positioning structure 103, avoiding radial compression in all directions, thereby ensuring the flatness and dimensional accuracy of the silicon steel sheet. In addition, except for the first circular silicon steel sheet, the subsequent circular silicon steel sheets form an embedded structure similar to mortise and tenon through the rivet point protrusion 102. The connection strength no longer depends solely on the frictional force generated by material deformation, but on the mutual nesting of the structure. Therefore, the riveting strength is higher and more reliable, which can fully meet the requirements of production and use.
[0038] Furthermore, the rivet point punch 102 has a cylindrical structure, and the connection between the lower end face and the side face of the rivet point punch 102 is provided with an annular inclined surface that can realize both punching and extrusion forming functions. Figure 2It can be seen that the riveting point punch 102 of this shape can punch the circular silicon steel sheets other than the first circular silicon steel sheet to form a trapezoidal protruding structure, and adjacent circular silicon steel sheets form a mortise-and-tenon-like embedded structure through the trapezoidal protruding structure.
[0039] Further, the riveting process further includes step S500: after the number of silicon steel sheets in the positioning structure 103 reaches the corresponding quantity, the silicon steel sheet at the bottommost end of the positioning structure 103 is separated from the positioning structure 103, so as to realize the blanking of the circular silicon steel sheets.
[0040] Embodiment 2 In this embodiment, the process further includes the following on-line quality monitoring step S600: S601. During the process of embedding the riveting structure into the through hole, synchronously collect the instantaneous pressure value and displacement value of the riveting point punch 102 to form a pressure-displacement data set; S602. Based on the data set, judge the quality of the current riveting through a preset quality judgment algorithm; S603. According to the judgment result, classify the riveted finished products into qualified products or unqualified products.
[0041] Further, the quality judgment algorithm includes a riveting work judgment step, which comprises: Perform statistical analysis on the pressure-displacement data sets of historical qualified products to pre-set a standard riveting work interval ; During the current riveting process, collect the pressure in real time with respect to displacement as a function ; By performing integration within the effective riveting stroke , calculate the actual riveting work consumed in the current riveting process ; Compare whether it falls within the standard interval , and if the condition is satisfied , the riveting work is judged to be qualified; The calculation of the actual riveting work follows the definite integral rule:
[0042] wherein, is the actual riveting work; is the instantaneous pressure collected by the sensor when the riveting point punch 102 is at the displacement point ; is the instantaneous displacement of the riveting point punch 102; is the displacement point at which riveting starts; is the displacement point at the end of riveting.
[0043] In this embodiment, the riveting work fully represents the total energy consumed to cause plastic deformation of the rivet structure and embed it into the through hole, and this energy value is a comprehensive evaluation of the entire riveting process.
[0044] If W_actual<W_min, it indicates that the energy is insufficient, and defects such as incomplete riveting and loose fit may exist. If , it indicates that the consumed energy is too large, and problems such as inaccurate positioning, abnormal material size or die wear may exist, and even implicit damage may be caused to the ultra-thin silicon steel sheet. This method can effectively screen out defective products with abnormal energy.
[0045] Further, the quality determination algorithm further includes a forming gradient stability determination step, which is executed on the basis that the riveting work determination is qualified, and includes: Identifying the key forming section where the main plastic deformation of the material occurs in the pressure-displacement curve ; calculating the gradient function of the pressure-displacement curve within this section ; calculating the standard deviation of the gradient function within this section ; comparing the with a preset maximum allowable gradient fluctuation threshold , and if , determining that the forming process is stable; the calculation formula of the gradient function is:
[0046] the calculation formula of the standard deviation is:
[0047]
[0048] wherein, is the instantaneous pressure collected by the sensor when the punch 102 at the rivet point is at the displacement point ; is the average gradient within the key forming section; is the standard deviation of the gradient within the key forming section; is the starting displacement point of the key forming section; is the ending displacement point of the key forming section.
[0049] In this embodiment, the gradient This represents the "work hardening rate" or "deformation resistance" of a material during deformation. In an ideal and smooth riveting process, the deformation resistance should increase smoothly.
[0050] Standard deviation This quantifies the degree of discreteness or volatility of this gradient. An excessively large... The value indicates a sudden pressure change or fluctuation during the forming process, which may indicate micro-tears, uneven flow, or "stick-slip" phenomena between the material and the mold. This step is specifically used to identify defective products that meet the energy requirements (total work is acceptable) but have unstable processes and potential problems.
[0051] Furthermore, the final quality determination is derived using a multi-factor weighted Gaussian model, a step that includes: Extract n key feature parameters ; For each feature parameter According to its ideal target value and acceptable deviation The individual quality scores are calculated using the Gaussian function. ; Each feature is assigned a score based on its importance to the final product performance. Assign a weight coefficient ; Calculate the weighted sum of all individual scores to obtain the final overall quality score. ; Will With the set minimum passing score In comparison, if If so, it will ultimately be determined to be a qualified product; Overall quality score The calculation formula is:
[0052]
[0053] in, For the first Individual quality scores for each feature; For the first The weight coefficients of each feature; For the first The actual measured values of the key features in this study; For the first The ideal target value for each feature; For the first Acceptable standard deviation of key features; The total number of key features used for evaluation; Natural exponential function .
[0054] In this embodiment, a single-dimensional judgment may have omissions. This model integrates information from multiple dimensions to form a comprehensive quality evaluation system. The Gaussian function ensures that the further the parameters deviate from their ideal values, the lower the score, and the penalty is non-linear, consistent with the general principles of industrial quality control. The introduction of weighting coefficients allows the model to be flexibly adjusted for different application scenarios, greatly improving the accuracy and robustness of the judgment results. It can not only judge "qualified / unqualified," but also output continuous scores. It can also be used to grade qualified products or to analyze the long-term health trends of production lines, providing data support for preventive maintenance.
[0055] Example 3 Please refer to Figure 4 The diagram illustrates a structural schematic of a computer device provided by some embodiments of this application. The electronic device 20 includes a processor 200, a memory 201, a bus 202, and a communication interface 203. The processor 200, the communication interface 203, and the memory 201 are connected via the bus 202. The memory 201 stores a computer program that can run on the processor 200. The processor 200 is used to operate according to the instructions to perform the steps of the riveting process described in any one of embodiments 1 and 2.
[0056] The memory 201 may include high-speed random access memory (RAM) or non-volatile memory, such as at least one disk storage device. Communication between this system network element and at least one other network element is achieved through at least one communication interface 203 (which can be wired or wireless), such as the Internet, wide area network, local area network, or metropolitan area network.
[0057] Bus 202 can be an ISA bus, PCI bus, or EISA bus, etc. The bus can be divided into an address bus, a data bus, a control bus, etc. The memory 201 is used to store programs. After receiving an execution instruction, the processor 200 executes the program. The riveting process disclosed in any of the foregoing embodiments of this application can be applied to the processor 200, or implemented by the processor 200.
[0058] The processor 200 may be an integrated circuit chip with signal processing capabilities. During implementation, each step of the aforementioned riveting process can be completed by the integrated logic circuitry in the hardware of the processor 200 or by instructions in software form. The processor 200 may be a general-purpose processor, including a central processing unit (CPU), a network processor (NP), etc.; it may also be a digital signal processor (DSP), an application-specific integrated circuit (ASIC), an off-the-shelf programmable gate array (FPGA), or other programmable logic devices, discrete gate or transistor logic devices, or discrete hardware components. It can implement or execute the methods, steps, and logic block diagrams disclosed in the embodiments of this application. The general-purpose processor may be a microprocessor or any conventional processor. The steps of the riveting process disclosed in the embodiments of this application can be directly manifested as execution by a hardware decoding processor, or execution by a combination of hardware and software modules in the decoding processor. The software modules may reside in random access memory, flash memory, read-only memory, programmable read-only memory, electrically erasable programmable memory, registers, or other mature storage media in the art. The storage medium is located in memory 201. The processor 200 reads the information in memory 201 and, in conjunction with its hardware, completes the above-mentioned riveting process steps.
[0059] Example 4 This embodiment also provides a computer-readable storage medium corresponding to the riveting process provided in the foregoing embodiments. Please refer to [link / reference]. Figure 5 The computer-readable storage medium shown is an optical disc containing a computer program (i.e., program product 30) that, when run by a processor, performs the riveting process provided in any of the aforementioned embodiments.
[0060] It should be noted that examples of the computer-readable storage medium may also include, but are not limited to, phase-change memory (PRAM), static random access memory (SRAM), dynamic random access memory (DRAM), other types of random access memory (RAM), read-only memory (ROM), electrically erasable programmable read-only memory (EEPROM), flash memory or other optical and magnetic storage media, which will not be elaborated here.
[0061] The computer-readable storage medium provided in the above embodiments of this application and the riveting process provided in the embodiments of this application are based on the same application concept and have the same beneficial effects as the methods adopted, run or implemented by the application stored therein.
[0062] It should be noted that in the above text, the terms "comprising," "including," or any other variations thereof are intended to cover non-exclusive inclusion, such that a process, method, article, or apparatus that comprises a list of elements includes not only those elements but also other elements not expressly listed, or elements inherent to such a process, method, article, or apparatus. Without further limitations, an element defined by the phrase "comprising one..." does not exclude the presence of other identical elements in the process, method, article, or apparatus that includes that element. Furthermore, it should be noted that the scope of the methods and apparatuses in the embodiments of this application is not limited to performing functions in the order shown or discussed, but may also include performing functions substantially simultaneously or in the reverse order, depending on the functions involved. For example, the described methods may be performed in a different order than described, and various steps may be added, omitted, or combined. Additionally, features described with reference to certain examples may be combined in other examples.
[0063] Through the above description of the embodiments, those skilled in the art can clearly understand that the methods of the above embodiments can be implemented by means of software plus necessary general-purpose hardware platforms. Of course, they can also be implemented by hardware, but in many cases the former is a better implementation method. Based on this understanding, the technical solution of this application, in essence, or the part that contributes to the prior art, can be embodied in the form of a software product. This computer software product is stored in a storage medium (such as ROM / RAM, magnetic disk, optical disk) and includes several instructions to cause a terminal (which may be a mobile phone, computer, server, air conditioner, or network device, etc.) to execute the methods described in the various embodiments of this application.
[0064] In summary, the FPC micro-optical module packaging system, method, computer device, and storage medium for AI glasses of the present invention, by pre-positioning micro-handles that can be manipulated by non-contact force on the optical elements to be stacked, and by monitoring the imaging quality in real time through a closed-loop feedback system after the elements are stacked and uncured optical adhesive is injected, and by using optical tweezers array technology to manipulate the handles to fine-tune the elements until the optimal position is reached, and then instantly curing the adhesive to complete the encapsulation, can effectively solve the problems of low yield and high production cost caused by tolerance accumulation and stress influence.
[0065] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the present invention, and are not intended to limit the scope of protection of the present invention. Although the present invention has been described in detail with reference to preferred embodiments, those skilled in the art should understand that modifications or equivalent substitutions can be made to the technical solutions of the present invention without departing from the essence and scope of the technical solutions of the present invention.
Claims
1. A riveting device for ultra-thin silicon steel sheets, characterized in that, include: The rivet punch, the rivet fixture located below the rivet punch, a plurality of rivet point punches set on the lower end face of the rivet punch and parallel to the rivet punch, and a sensor for synchronously acquiring the instantaneous pressure value and displacement value of the rivet point punches. The rivet fixture is provided with a positioning structure for interference fit with the stamped silicon steel sheet, and the inner diameter of the positioning structure is 3μm to 7μm longer than the diameter of the rivet punch. The rivet point punch has a cylindrical structure, and the connection between the lower end face and the side face of the rivet point punch is provided with an annular inclined surface that can realize both punching and extrusion forming functions. It also includes a control processor configured to execute a quality determination algorithm to determine the riveting quality based on the pressure-displacement dataset collected by the sensor; the quality determination algorithm includes a forming gradient stability determination step and a determination step based on a multi-factor weighted Gaussian model; The step of determining the stability of the forming gradient includes: In the pressure-displacement curve, the key forming sections where the material undergoes major plastic deformation are identified; Calculate the gradient function of the pressure-displacement curve within this section. ; Calculate the gradient function Standard deviation within this range ,in The instantaneous pressure collected by the sensor. It is an instantaneous displacement; Will With the preset maximum allowable gradient fluctuation threshold If a comparison is made, If so, the forming process is considered stable; The determination step based on the multi-factor weighted Gaussian model includes: extract Key feature parameters ; For each feature parameter According to its ideal target value and acceptable standard deviation The individual quality scores are calculated using the Gaussian function. Its calculation formula is ; Weight coefficients assigned to each feature The overall quality score is obtained by calculating the weighted sum of all individual scores. ;Will With the set minimum passing score In comparison, if If it does, it will ultimately be judged as a qualified product.
2. The ultra-thin silicon steel sheet riveting equipment according to claim 1, characterized in that, The inner diameter of the positioning structure is 5 μm longer than the diameter of the rivet punch.
3. A method for riveting ultra-thin silicon steel sheets, characterized in that, The method, performed using the ultra-thin silicon steel sheet riveting equipment as described in claim 1 or 2, includes the following steps: S100. Place the silicon steel sheet between the rivet fixture and the rivet punch; S200. The rivet punch presses down to impact the silicon steel sheet, punching out a first circular silicon steel sheet that corresponds to the shape of the rivet punch. The rivet punch punches out several through holes on the first circular silicon steel sheet, and the first circular silicon steel sheet is interference-fitted to the positioning structure. S300. Repeat steps S100 to S200, whereby the second silicon steel sheet stamped out by the rivet punch adheres to the first silicon steel sheet and pushes the first silicon steel sheet downward toward the positioning structure. At the same time, the rivet punch stamps the second silicon steel sheet to form a rivet structure, so that the rivet structure is embedded in the through hole stamped out by the first silicon steel sheet for engagement. S400. Repeat step S300, where the subsequent silicon steel sheet pushes the aforementioned silicon steel sheet downwards towards the rivet fixture, while the adjacent rivet structures interlock and cooperate with each other. S600. During the process of embedding the rivet structure into the through hole in steps S300 and S400 above, the control processor synchronously collects the instantaneous pressure value and displacement value of the rivet point punch through the sensor, and executes the quality judgment algorithm to classify the riveted finished product as qualified or unqualified.
4. The riveting method for ultra-thin silicon steel sheets according to claim 3, characterized in that, The positioning structure is a columnar through hole that runs vertically through the center. The riveting method further includes step S500: after the silicon steel sheets in the positioning structure reach the corresponding number, the silicon steel sheet at the bottom of the positioning structure is detached from the positioning structure.
5. The riveting method for ultra-thin silicon steel sheets according to claim 3, characterized in that, The quality assessment algorithm includes a riveting performance assessment step, which includes: By statistically analyzing historical pressure-displacement datasets of qualified products, a standard riveting work range is pre-defined. ; Pressure was collected in real time during this riveting process. Regarding displacement function ; Through the Effective riveting stroke Integrate within the unit to calculate the actual riveting effort consumed in this riveting operation. ; compare whether it falls within the standard range , if the condition is satisfied , it is determined that the riveting operation is qualified; Actual riveting work The calculation follows the rule of definite integrals: in, For actual riveting work; For the rivet point punch at the displacement point The instantaneous pressure collected by the sensor at that time; This refers to the instantaneous displacement of the rivet point punch; This is the displacement point at which the riveting begins; This is the displacement point at which the riveting ends.
6. An electronic device, characterized in that, It includes a memory, a processor, and a computer program stored in the memory and executable on the processor, the processor running the computer program to implement the ultrathin silicon steel sheet riveting method as described in any one of claims 3-5.
Citation Information
Patent Citations
Pen type ignition coil iron core and buckling-riveting device thereof
CN102360782A
Manufacturing method of amorphous motor iron core
CN115301800A
Optimized determination of rivet-free riveting process parameters
CN116882091A