Anti-deformation quick demolding plastic uptake box mold
The design of the blister box mold, which features automatic mold closing, uniform material distribution, and automatic demolding, solves the problems of mold skewing and deformation, thereby improving the yield rate and production efficiency of blister boxes.
Patent Information
- Application Number
- CN202610133248.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-01-30
- Publication Date
- 2026-04-14
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
Existing blister box molds are prone to mold skewing and misalignment during the molding process, which can cause deformation of the blister box preform inside the mold cavity and reduce the yield of molded products.
The system employs an automatic mold closing assembly and a spiral extrusion material distribution assembly, combined with a demolding assembly, to achieve precise opening and closing of the upper and lower molds and uniform material distribution. It utilizes servo motors and electric push rods for automated control, incorporates a heater to maintain material flowability, and uses demolding ejector pins to achieve automatic demolding.
It effectively prevents mold deformation during mold closing, ensures uniform material distribution, improves the yield of molded products, avoids deformation and defects caused by manual operation, and improves production efficiency.
Smart Images

Figure CN121848647A_ABST
Abstract
Description
Technical Field
[0001] This invention belongs to the field of blister box production technology, and in particular relates to a blister box mold that prevents deformation and allows for quick demolding. Background Technology
[0002] Blister boxes broadly refer to all blister-type plastic packaging, while narrowly they specifically refer to box-shaped blister products with a connected lid and bottom. They can be divided into double blister packs, blister packs with insert cards, and other types. They are made by heating and softening plastic sheets such as PVC, PET, PP, and PS, and then vacuum adsorbing them into molds. The production process covers plate making, printing, punching, folding, and other stages. They are mainly used in the packaging of electronic products, medical devices, food, toys, cosmetics, and other fields, and have the advantages of transparency, adaptability to irregularly shaped products, and automated packaging.
[0003] In existing technology (patent application CN220280473U, entitled "A Vacuum Forming Mold for Easy Material Discharge"), a vacuum generator controlled by an electromagnetic valve is used to create negative pressure within the suction cup, thereby firmly holding the mold body. The electrically controlled suction cup boasts extremely strong holding force, uniform and adjustable magnetic force distribution, and is suitable for various heavy-duty machining processes, roughing, and finishing. Continuous operation generates no heat, preventing heat-induced deformation of the mold body. Simultaneously, the strong and uniform suction force ensures the highest machining accuracy, thus achieving rapid demolding. However, in implementing this technical solution, at least the following problems were found in the existing technology: During the production of blister boxes, mold forming methods are used according to the design requirements of the blister boxes. Currently, most of the mold forming methods are manual, which involves manually closing the mold blanks in the upper and lower mold cavities. This method also has the problem of uneven material distribution, which can easily lead to skewed or misaligned mold closing and deformation of the blister box blanks in the mold cavity, thus reducing the yield of blister boxes. Summary of the Invention
[0004] This application aims to at least address the technical problem in the prior art that it is impossible to achieve efficient molding and demolding of the blister box preform within the mold cavity using a combination of uniform extrusion and adaptive top-pressure demolding under conditions of automatic mold closing triggering. To this end, this application proposes a deformation-resistant and rapid demolding blister box mold.
[0005] To achieve the above objectives, the specific technical solution of the present invention is as follows: A blister box mold for preventing deformation and quick demolding includes a fixed frame, on which a storage tank with a feeding tube is placed vertically, and a support platform is placed horizontally at the bottom inside the fixed frame, with a sliding cylinder frame placed vertically around the bottom of the support platform. The top of the inner side of the fixed frame is horizontally provided with an upper mold, and the middle of the inner side of the fixed frame is slidably provided with a lower mold that is used in conjunction with the upper mold. The fixed frame is provided with a mold closing assembly for opening and closing the upper mold and the lower mold, and includes a servo motor horizontally provided on the outside of the fixed frame. The storage tank is provided with a fabric feeding assembly that supplies material to the upper mold, and includes a spiral frame that rotates inside the storage tank. The lower mold is provided with a demolding assembly, and includes a sealing sleeve embedded in the lower mold.
[0006] Preferably, the mold clamping assembly further includes an electric push rod fixed to the output shaft of a servo motor via a coupling, and a double-sided gear is sleeved on the piston rod of the electric push rod, with a driven bevel gear provided on the inner side of the double-sided gear.
[0007] Preferably, a threaded rod that rotates with the fixed frame is longitudinally arranged inside the bevel gear, a threaded sleeve is threadedly connected to the threaded rod, and a connecting piece that is fixed to the lower mold is fixed on the inner side of the threaded sleeve. The connecting piece slides with the reserved sliding opening on the fixed frame.
[0008] Preferably, the upper mold has main conductive blocks fixed around its top four sides, and the lower mold has auxiliary conductive blocks fixed around its bottom four sides, which are triggered by the main conductive blocks. The main conductive blocks and auxiliary conductive blocks are distributed in an axially symmetrical manner along the longitudinal axes of the upper mold and the lower mold, respectively.
[0009] Preferably, the fabric assembly further includes a secondary bevel gear disposed outside the double-sided gear, the secondary bevel gear being sleeved with the spiral frame, and an electrically controlled valve being connected to the storage tank.
[0010] Preferably, the inner end of the electric control valve is connected to a feeding pipe, and the inner end of the feeding pipe is connected to a fabric rack. The fabric rack is equipped with a one-way valve, and the upper mold has a fabric hole that communicates with the fabric rack.
[0011] Preferably, the storage tank has a double-layer cavity, and a heater is fixed inside the storage tank. The heater is connected to a curved panel embedded in the storage tank on the outside. The curved panel has a flow equalization hole, and a temperature probe is embedded on the outside of the storage tank and extends into the double-layer cavity.
[0012] Preferably, the demolding assembly further includes a demolding ejector pin that slides within a sealing sleeve, and the top of the demolding ejector pin is horizontally positioned with a demolding bracket for demolding from the lower mold.
[0013] Preferably, the bottom of the ejector pin is fixed with a lifting plate, and a storage groove hidden from the lifting plate is provided on the support platform. A T-shaped slide block fixed to the lifting plate slides inside the slide frame and slides with the support platform. A compression spring is sleeved on the T-shaped slide block.
[0014] Preferably, one side of the lower mold is connected to a cooling pipe, and a cooling channel connected to the cooling pipe is opened inside the lower mold. The other side of the lower mold is connected to a cooling exhaust pipe, and both the cooling pipe and the cooling exhaust pipe are equipped with manual valves.
[0015] The blister box mold for preventing deformation and quick demolding according to the present invention has the following advantages: 1. This type of blister box mold with anti-deformation and quick demolding uses an automatic mold closing component to achieve precise opening and closing operations of the upper and lower molds, replacing the traditional manual mold closing method. This prevents misalignment or skewing of the upper and lower molds, thus preventing deformation. It also forces the main conductive block and the auxiliary conductive block to fit together and be energized, providing triggering conditions for the material feeding component and achieving continuity between mold closing and material feeding operations.
[0016] 2. This type of blister box mold for preventing deformation and quick demolding uses a material feeding assembly and a spiral extrusion method to pressurize and extrude the material added to the storage tank. Combined with a material feeding frame, it achieves a uniform material distribution effect, ensuring that the material is evenly and effectively delivered to the mold cavities of the upper and lower molds to prevent material feeding interruption and deformation. A one-way valve is used to perform zoned opening and closing operations on the material distributed to each mold cavity, avoiding material distribution in idle mold cavities. Furthermore, a heater and a sandwich cavity are used to keep the material added to the storage tank warm, improving the extrusion fluidity of the material and ensuring smooth material distribution.
[0017] 3. This type of anti-deformation and fast demolding blister box mold utilizes the height difference generated by the opening and closing of the lower mold through the demolding component. This forces the demolding ejector pin on the demolding ejector to apply top pressure to the blister box mold blank formed in the lower mold, thereby forcing the blister box mold blank to automatically demold, replacing the manual demolding method. This ensures the integrity of the blister box mold blank after molding, avoids deformation and defects caused by manual demolding, and improves the yield of molded blister box mold blanks. Attached Figure Description
[0018] To more clearly illustrate the technical solutions of the embodiments of the present invention, the accompanying drawings used in the embodiments will be briefly introduced below. It should be understood that the following drawings only show some embodiments of the present invention and should not be regarded as a limitation of the scope. For those skilled in the art, other related drawings can be obtained from these drawings without creative effort.
[0019] Figure 1 This is an initial state diagram of a blister box mold structure for preventing deformation and quick demolding according to the present invention; Figure 2 This is a diagram showing the mold-closed state of a blister box mold structure for preventing deformation and quick demolding according to the present invention; Figure 3This is a partial sectional view of the structure of a blister box mold for preventing deformation and quick demolding according to the present invention; Figure 4 This is an initial state diagram of the fixing frame, upper mold, lower mold, and mold closing assembly of the present invention; Figure 5 This is a diagram showing the mold closing assembly structure in the mold closing state of the present invention; Figure 6 This is a side sectional view of the structure of the fixing frame, storage tank, upper mold and fabric assembly of the present invention; Figure 7 This is a bottom cross-sectional view of the structure of the storage tank, upper mold and fabric assembly of the present invention; Figure 8 This is an exploded cross-sectional view of the storage tank structure of the present invention; Figure 9 This is a side view of the structure of the support platform, slide frame, lower mold, and demolding assembly of the present invention; Figure 10 This is a side sectional view of the support platform, slide frame, and demolding assembly structure of the present invention; Figure 11 This is a partial top sectional view of the lower mold structure of the present invention.
[0020] Explanation of markings in the diagram: 1. Fixed frame; 2. Storage tank; 3. Feeding pipe; 4. Support platform; 5. Slide frame; 6. Upper mold; 7. Lower mold; 81. Servo motor; 82. Electric push rod; 83. Double-sided gear; 84. Driven bevel gear; 85. Threaded rod; 86. Threaded sleeve; 87. Connecting part; 91. Secondary bevel gear; 92. Screw frame; 93. Electric control valve; 94. Feeding pipe; 95. Fabric placing frame; 9 6. One-way valve; 97. Fabric feeding hole; 101. Sealing sleeve; 102. Demolding ejector pin; 103. Demolding ejector frame; 104. Lifting plate; 105. Storage groove; 106. T-shaped slide; 107. Compression spring; 11. Main conductive block; 12. Secondary conductive block; 13. Interlayer cavity; 14. Heater; 15. Curved panel; 16. Temperature probe; 17. Cooling pipe; 18. Cooling channel; 19. Cooling exhaust pipe. Detailed Implementation
[0021] The present invention will now be described in detail with reference to the accompanying drawings and specific embodiments: like Figures 1-11 As shown, the present invention provides a blister box mold for quick demolding and deformation prevention, including a fixed frame 1, a storage tank 2 with a feeding pipe 3 is longitudinally placed on the fixed frame 1, a manual valve is provided on the feeding pipe 3 to facilitate the opening and feeding operation of the feeding pipe 3, and a support platform 4 is horizontally placed at the bottom of the inner side of the fixed frame 1, and a slide cylinder frame 5 is longitudinally placed around the bottom of the support platform 4. A PLC controller is fixed at the bottom of the fixed frame 1 for the automatic control of the components. An upper mold 6 is horizontally placed on the top of the inner side of the fixing frame 1, and a lower mold 7 that is used in conjunction with the upper mold 6 slides in the middle of the inner side of the fixing frame 1. Limiting ribs are provided in the mold cavity between the upper mold 6 and the lower mold 7 to optimize the design of the inner mold cavity of the upper mold 6 and the lower mold 7, and to limit the forming of the blister box mold blank in the mold cavity, preventing the blister box mold blank from deforming. At the same time, the upper mold 6 and the lower mold 7 are also positioned by positioning heads and positioning grooves to prevent misalignment, further ensuring the tightness and fit of the mold closing of the upper mold 6 and the lower mold 7.
[0022] The fixed frame 1 is equipped with a mold closing assembly for opening and closing the upper mold 6 and the lower mold 7, and includes a servo motor 81 horizontally placed on the outside of the fixed frame 1, and an electric push rod 82 fixed to the output shaft of the servo motor 81 by a coupling. A double-sided gear 83 is sleeved on the piston rod of the electric push rod 82, and a driven bevel gear 84 is provided on the inner side of the double-sided gear 83. The electric push rod 82 adjusts the meshing stroke between the double-sided gear 83 and the driven bevel gear 84. First, control the electric push rod 82 to open and drive the double-sided gear 83 to move forward and engage with the bevel gear 84. Then, control the servo motor 81 to open and drive the bevel gear 84 to rotate linearly forward through the engaged double-sided gear 83. A threaded rod 85, which rotates with the fixed frame 1, is longitudinally placed inside the bevel gear 84. A threaded sleeve 86 is threadedly connected to the threaded rod 85, and a connecting piece 87, which is fixed to the lower mold 7, is fixed inside the threaded sleeve 86. The connecting piece 87 slides with the reserved sliding opening on the fixed frame 1. The reserved sliding opening plays a role in limiting the sliding of the connecting piece 87 to prevent it from shaking or tilting during the displacement of the lower mold 7 driven by the connecting piece 87. The threaded rod 85 on the bevel gear 84 rotates linearly forward, driving the threaded sleeve 86 to move upward. The threaded sleeve 86, through the connecting piece 87, drives the lower mold 7 to move towards the upper mold 6, which is in a fixed state, until the lower mold 7 and the upper mold 6 are successfully closed. At this point, the servo motor 81 is paused, and the electric push rod 82 is closed and drives the double-sided gear 83 to move backward and disengage from the meshing part of the bevel gear 84 back to the initial position. This automatic mold closing method achieves precise opening and closing operations for the upper mold 6 and the lower mold 7, replacing the traditional manual mold closing method. This prevents misalignment or skewing of the upper and lower molds during mold closing and also serves to prevent deformation.
[0023] The upper mold 6 has main conductive blocks 11 fixed around its top, and the lower mold 7 has auxiliary conductive blocks 12 fixed around its bottom, which are triggered by the main conductive blocks 11. When the lower mold 7 and the upper mold 6 are successfully closed, the main conductive blocks 11 on the upper mold 6 are forced to come into contact with the auxiliary conductive blocks 12 on the lower mold 7 and become energized. This triggers the electric push rod 82 and the servo motor 81 to reopen in succession, which facilitates the subsequent material placement work in the mold cavities of the lower mold 7 and the upper mold 6 and improves the continuity of the operation process. The main conductive blocks 11 and auxiliary conductive blocks 12 are distributed in an axially symmetrical manner along the longitudinal axis of the upper mold 6 and the lower mold 7, respectively, so that the main conductive blocks 11 and auxiliary conductive blocks 12 are reasonably distributed and ensure that the four sets of main conductive blocks 11 and auxiliary conductive blocks 12 are tightly attached and accurately triggered.
[0024] like Figures 1-11 As shown, the storage tank 2 is equipped with a material feeding assembly that supplies material to the upper mold 6, and includes a spiral frame 92 that rotates inside the storage tank 2, as well as a secondary bevel gear 91 located outside the double-sided gear 83. The secondary bevel gear 91 is sleeved with the spiral frame 92. The meshing stroke between the double-sided gear 83 and the secondary bevel gear 91 is adjusted by an electric push rod 82. The storage tank 2 is connected to an electric control valve 93, and a metering sensor is installed on the electric control valve 93 to accurately and quantitatively control the metering of the material passing through the electric control valve 93, so as to prevent excessive material overflow and material waste. When the four sets of main conductive blocks 11 and auxiliary conductive blocks 12 are in contact with the power supply, the electric push rod 82 and the servo motor 81 are triggered to restart in succession. The electric push rod 82, which is triggered to restart, drives the double-sided gear 83 to move backward and engage with the meshing part of the auxiliary bevel gear 91. Then, the servo motor 81, which is triggered to restart in succession, drives the spiral frame 92 on the auxiliary bevel gear 91 to rotate linearly through the meshing double-sided gear 83. The spiral frame 92 squeezes the material added to the storage tank 2 upward in a spiral. The inner end of the electric control valve 93 is connected to the feeding pipe 94, and the inner end of the feeding pipe 94 is connected to the material rack 95. The material rack 95 is equipped with a one-way valve 96, which performs zoned opening and closing operations on the material to each mold cavity, avoiding material waste caused by material feeding in idle mold cavities, and also causing trouble for subsequent mold cavity cleaning. In addition, the upper mold 6 has a material feeding hole 97 connected to the material rack 95. The material feeding hole 97 is distributed in a circumferential shape along the longitudinal axis of the mold cavities of the lower mold 7 and the upper mold 6, which improves the rationality of material feeding in the material feeding hole 97 and forces the material to be fully and effectively squeezed and flow into each mold cavity of the lower mold 7 and the upper mold 6. The material being spirally extruded upwards by the spiral frame 92 is fed into the material rack 95 through the feeding pipe 94 by the electrically controlled valve 93, which is in the open state. Based on the number of blister box preforms formed in the mold cavities of the lower mold 7 and the upper mold 6, the four sets of one-way valves 96 on the material rack 95 are opened accordingly. The material in the open channel of the material rack 95 then reaches the mold cavity of the successfully closed lower mold 7 and the upper mold 6 through the material feeding hole 97 for forming. The spiral extrusion method is used to apply pressure to the material added to the storage tank 2 and extrude it. Combined with the uniform partitioning material distribution method, the material is evenly and effectively delivered to the mold cavity of the upper mold 6 and the lower mold 7 to prevent interruption of material feeding, deformation, and reduce the defect rate of blister box preforms in the mold cavity. The storage tank 2 has a jacketed cavity 13, and a heater 14 is fixed inside the storage tank 2. The outside of the heater 14 is connected to a curved panel 15 embedded in the storage tank 2. The curved panel 15 has flow equalization holes to equalize the heat source generated by the heater 14, so as to prevent turbulence at the curved panel 15. A temperature probe 16 is embedded on the outside of the storage tank 2 and extends into the jacketed cavity 13. The probe controls the heater 14 to turn on and supplies the generated heat into the jacketed cavity 13 in the storage tank 2 through the flow equalization holes on the curved panel 15. The temperature probe 16 monitors the temperature of the heat reaching the jacketed cavity 13 in real time, continuously heating the material in the storage tank 2 to ensure that the material always maintains a smooth flow state and to prevent the material from condensing and causing flow stagnation.
[0025] like Figures 1-11 As shown, the lower mold 7 is provided with a demolding assembly, including a sealing sleeve 101 embedded in the lower mold 7, and a demolding ejector pin 102 sliding in the sealing sleeve 101. The top of the demolding ejector pin 102 is horizontally provided with a demolding bracket 103 for demolding from the lower mold 7. The sealing sleeve 101 provides a sealing and sliding function for the demolding ejector pin 102 to prevent material leakage in the mold cavities of the lower mold 7 and the upper mold 6. The bottom of the ejector pin 102 is fixed with a lifting plate 104, and the support platform 4 is provided with a storage groove 105 that is hidden from the lifting plate 104. A T-shaped slide block 106 fixed to the lifting plate 104 slides inside the slide frame 5 and slides with the support platform 4. A compression spring 107 is sleeved on the T-shaped slide block 106. The compression spring 107 provides elastic buffering for the T-shaped slide block 106, thereby achieving the damping sliding effect of the T-shaped slide block 106. During the closing of the lower mold 7 and the upper mold 6, the upward-moving lower mold 7, through several sealing sleeves 101, drives several ejector pins 102 to move upward as well. Then, the ejector pins 102 drive the ejector frame 103 to move upward as well. Until the lower mold 7 and the upper mold 6 are successfully closed, the ejector frame 103, which moves upward with the lower mold 7, is forced by the downward extrusion force generated by the upper mold 6 when the mold is closed. This forces the ejector frame 103 to drive several ejector pins 102 to slide downward within several sealing sleeves 101. Then, the ejector pins 102 drive the lifting plate 104 to move downward toward the receiving groove 105 on the support platform 4. At the same time, the downward-moving lifting plate 104 drives four T-shaped slide blocks 106 to slide down within four slide cylinder frames 5 until the ejector frame 103 is pressed down and hidden into the mold cavity of the lower mold 7, preparing for subsequent demolding. After the blister box mold blank is molded, the lower mold 7, which is in the downward reset state, drives several ejector pins 102 to move downward again through several sealing sleeves 101. The upper mold 6 loses the downward pressing force on the ejector frame 103. The ejector pins 102 that continue to move downward drive the lifting plate 104 to move downward and reset into the storage groove 105. The lifting plate 104 that has moved down to the position continues to drive the four T-shaped slides 106 to slide down in the four slide cylinder frames 5 and stretch the four compression springs 107 on them. Under the upward pushing force generated by the four slide cylinder frames 5 on the four T-shaped slides 106, the ejector frame 103 in the lower mold cavity is forced to move upward and lift through the ejector pins 102 that are pushing upward, and the blister box mold blank formed in the mold cavity is pushed upward and demolded. By utilizing the height difference generated by the opening and closing of the lower mold 7, top pressure is applied to the blister box mold blank formed inside the lower mold 7, forcing the blister box mold blank inside to automatically demold, replacing the manual demolding method, ensuring the integrity of the blister box mold blank after molding, avoiding the deformation and defects of the blister box mold blank caused by manual demolding, and improving the molding yield of blister box mold blanks. A cooling pipe 17 is connected to one side of the lower mold 7, and a cooling channel 18 connected to the cooling pipe 17 is opened inside the lower mold 7. After the blister box mold blank is molded, the cold source is supplied to the cooling channel 18 inside the lower mold 7 through the cooling pipe 17 by the external cold source pipe, so as to quickly cool and form the blister box mold blank in the mold cavity of the lower mold 7 and the upper mold 6. A cooling exhaust pipe 19 is connected to the other side of the lower mold 7, and a manual valve is provided on both the cooling pipe 17 and the cooling exhaust pipe 19. After the lower mold 7 and the demolding ejector 103 are lowered and reset to the initial state, the cold source in the cooling channel 18 inside the lower mold 7 is discharged through the cooling exhaust pipe 19, so that the lower mold 7 returns to the initial temperature and is ready for the next batch of blister box mold blanks to be formed.
[0026] The working principle of a blister box mold with anti-deformation and quick demolding: First, control the electric push rod 82 to open and drive the double-sided gear 83 to move forward and engage with the bevel gear 84. Then, control the servo motor 81 to open and drive the threaded rod 85 on the bevel gear 84 to rotate linearly forward through the engaged double-sided gear 83. The threaded rod 85 drives the threaded sleeve 86 to move upward. The threaded sleeve 86 drives the lower mold 7 to move towards the upper mold 6, which is in a fixed state, through the connecting piece 87. At this time, the moving lower mold 7 drives several demolding pins 102 to move upward through several sealing sleeves 101. Then, the demolding pins 102 drive the demolding bracket 103 to move upward. As the lower mold 7 and the upper mold 6 are successfully closed, the demolding ejector 103, which moves upward with the lower mold 7, is forced by the downward squeezing force generated by the upper mold 6 when the mold is closed. This forces the demolding ejector 103 to drive several demolding ejector pins 102 to slide downward within several sealing sleeves 101. Subsequently, the several demolding ejector pins 102 drive the lifting plate 104 to move downward toward the receiving groove 105 on the support platform 4. At the same time, the downward-moving lifting plate 104 drives four T-shaped slide blocks 106 to slide down within four sliding cylinder frames 5 until the demolding ejector 103 is pressed down and hidden into the mold cavity of the lower mold 7. The servo motor 81 is then paused, and the electric push rod 82 is then closed and drives the double-sided gear 83 to move backward and disengage from the meshing part of the bevel gear 84 to the initial position. Then, material is added unidirectionally to the storage tank 2 through the feeding pipe 3. As the lower mold 7 and the upper mold 6 are successfully closed, the main conductive block 11 on the upper mold 6 is forced to come into contact with the auxiliary conductive block 12 on the lower mold 7 and be energized. This triggers the electric push rod 82 and the servo motor 81 to restart in succession. The electric push rod 82, which is triggered to restart, drives the double-sided gear 83 to move backward and engage with the meshing part of the auxiliary bevel gear 91. Then, the servo motor 81, which is triggered to restart in succession, drives the spiral frame 92 on the auxiliary bevel gear 91 to rotate linearly through the meshing double-sided gear 83. The spiral frame 92 squeezes the material added to the storage tank 2 upward in a spiral. At the same time, the heater 14 is turned on and the heat generated is supplied into the jacket cavity 13 in the storage tank 2 through the flow equalization hole on the curved panel 15. The temperature probe 16 monitors the temperature of the heat reaching the jacket cavity 13 in real time, and continuously heats the material in the storage tank 2 to ensure that the material in it always maintains a smooth flow. Subsequently, the material that is spirally squeezed upward by the spiral frame 92 is fed into the material rack 95 through the feeding pipe 94 by the open electric control valve 93. In advance, according to the number of blister box blanks formed in the mold cavities of the lower mold 7 and the upper mold 6, the four sets of one-way valves 96 on the material rack 95 are opened accordingly. The material in the open channel of the material rack 95 then reaches the mold cavity of the successfully closed lower mold 7 and upper mold 6 through the material hole 97 for forming operation. After the blister box mold blank is molded, the cold source is first supplied to the cooling channel 18 in the lower mold 7 through the cooling pipe 17 by the external cold source pipe. This allows for rapid cooling and molding of the blister box mold blank in the mold cavities of the lower mold 7 and the upper mold 6. Conversely, the electric push rod 82 is first controlled to reopen and drive the double-sided gear 83 to move forward and engage with the bevel gear 84. Then, the servo motor 81 is controlled to reopen and drive the threaded rod 85 on the bevel gear 84 to reverse linearly through the engaged double-sided gear 83. The threaded rod 85 drives the threaded sleeve 86 to move downward. The threaded sleeve 86 drives the lower mold 7 to move downward synchronously through the connecting piece 87 and move away from the upper mold 6. Then, the lower mold 7 and the upper mold 6 are successfully separated. At the same time as the lower mold 7 and the upper mold 6 are successfully separated, the main conductive block 11 on the upper mold 6 is also forced to separate from the auxiliary conductive block 12 on the lower mold 7, so that the main conductive block 11 and the auxiliary conductive block 12 are in a de-energized state, the triggering conditions of the electric push rod 82 and the servo motor 81 are released, and the electric push rod 82 and the servo motor 81 are successively controlled to shut down again. Meanwhile, the lower mold 7, in its lower reset state, drives several ejector pins 102 to move downwards again via several sealing sleeves 101. The upper mold 6 loses its downward pressure on the ejector frame 103. The ejector pins 102, continuing to move downwards, drive the lifting plate 104 to move down and reset into the receiving groove 105. The lifting plate 104, now in its lowered position, then drives the four T-shaped slide blocks 106 to slide down within the four slide cylinder frames 5, stretching the four compression springs 107 on them. Under the upward pushing pressure generated by the cylinder frame 5 on the four T-shaped slide blocks 106, the demolding ejector pins 102, which are pushed upward, force the demolding ejector frame 103 in the mold cavity of the lower mold 7 to move upward and push the molded blister box mold blank in the mold cavity upward and demold it. At this time, the lower mold 7 and the demolding ejector frame 103 both move downward and reset to the initial state. Then, the cold source in the cooling channel 18 in the lower mold 7 is discharged through the cooling pipe 19, so that the lower mold 7 returns to the initial temperature and is ready for the next batch of blister box mold blanks to be formed.
[0027] It should be noted that the specific models and specifications of the servo motor 81, electric push rod 82, electric control valve 93, check valve 96, main conductive block 11, auxiliary conductive block 12, heater 14 and temperature probe 16 need to be selected and determined according to the actual specifications of the device. The specific selection calculation method adopts the existing technology in this field, so it will not be elaborated in detail.
[0028] The power supply circuits for the servo motor 81, electric push rod 82, electric control valve 93, check valve 96, main conductive block 11, auxiliary conductive block 12, heater 14, and temperature probe 16 are clear to those skilled in the art and will not be described in detail here.
[0029] It is understood that the present invention has been described through some embodiments, and those skilled in the art will recognize that various changes or equivalent substitutions can be made to these features and embodiments without departing from the spirit and scope of the invention. Furthermore, under the teachings of the present invention, these features and embodiments can be modified to adapt to specific situations and materials without departing from the spirit and scope of the invention. Therefore, the present invention is not limited to the specific embodiments disclosed herein, and all embodiments falling within the scope of the claims of this application are within the protection scope of the present invention.
Claims
1. A blister box mold for preventing deformation and quick demolding, comprising a fixing frame (1), characterized in that: The fixed frame (1) has a storage tank (2) with a feeding pipe (3) placed vertically on it, and a support platform (4) is placed horizontally at the bottom of the inner side of the fixed frame (1). Slide racks (5) are placed vertically around the bottom of the support platform (4). The top of the inner side of the fixed frame (1) is horizontally provided with an upper mold (6), and the middle of the inner side of the fixed frame (1) is slidably provided with a lower mold (7) used in conjunction with the upper mold (6). The fixed frame (1) is provided with a mold closing assembly for opening and closing the upper mold (6) and the lower mold (7), and includes a servo motor (81) horizontally provided on the outside of the fixed frame (1). The storage tank (2) is provided with a fabric feeding assembly that supplies material to the upper mold (6), and includes a spiral frame (92) that rotates inside the storage tank (2). The lower mold (7) is provided with a demolding assembly, and includes a sealing sleeve (101) embedded in the lower mold (7).
2. The blister box mold for preventing deformation and quick demolding according to claim 1, characterized in that: The mold clamping assembly also includes an electric push rod (82) fixed to the output shaft of a servo motor (81) via a coupling, and a double-sided gear (83) is sleeved on the piston rod of the electric push rod (82), and a bevel gear (84) is provided on the inner side of the double-sided gear (83).
3. The blister box mold for anti-deformation and quick demolding according to claim 2, characterized in that: The threaded rod (85) is longitudinally placed inside the bevel gear (84) and rotates with the fixed frame (1). A threaded sleeve (86) is threadedly connected to the threaded rod (85), and a connecting piece (87) fixed to the lower mold (7) is fixed on the inner side of the threaded sleeve (86). The connecting piece (87) slides with the reserved sliding opening on the fixed frame (1).
4. The blister box mold for preventing deformation and quick demolding according to claim 3, characterized in that: The upper mold (6) has a main conductive block (11) fixed around its top, and the lower mold (7) has a secondary conductive block (12) fixed around its bottom, which is conductively triggered by the main conductive block (11). The main conductive block (11) and the secondary conductive block (12) are distributed in an axially symmetrical manner along the longitudinal axis of the upper mold (6) and the lower mold (7), respectively.
5. The blister box mold for anti-deformation and quick demolding according to claim 4, characterized in that: The fabric assembly also includes a secondary bevel gear (91) disposed outside the double-sided gear (83), the secondary bevel gear (91) being sleeved with the spiral frame (92), and an electric control valve (93) connected to the storage tank (2).
6. The blister box mold for anti-deformation and quick demolding according to claim 5, characterized in that: The inner end of the electric control valve (93) is connected to the feeding pipe (94), and the inner end of the feeding pipe (94) is connected to the fabric rack (95). The fabric rack (95) is equipped with a one-way valve (96), and the upper mold (6) has a fabric hole (97) that communicates with the fabric rack (95).
7. The blister box mold for anti-deformation and quick demolding according to claim 6, characterized in that: The storage tank (2) has a sandwich cavity (13) inside, and a heater (14) is fixed inside the storage tank (2). The heater (14) is connected to a curved panel (15) embedded in the storage tank (2) on the outside. A flow equalization hole is opened on the curved panel (15), and a temperature probe (16) is embedded on the outside of the storage tank (2) and extends into the sandwich cavity (13).
8. The blister box mold for anti-deformation and quick demolding according to claim 7, characterized in that: The demolding assembly also includes a demolding ejector pin (102) that slides within a sealing sleeve (101), and the top of the demolding ejector pin (102) is horizontally provided with a demolding ejector bracket (103) for demolding from the lower mold (7).
9. A blister box mold for quick demolding and deformation prevention according to claim 8, characterized in that: The bottom of the ejector pin (102) is fixed with a lifting plate (104), and the support platform (4) is provided with a storage groove (105) that is hidden from the lifting plate (104). The slide frame (5) has a T-shaped slide block (106) that is fixed to the lifting plate (104) and slides with the support platform (4). A compression spring (107) is sleeved on the T-shaped slide block (106).
10. A blister box mold for quick demolding and deformation prevention according to claim 9, characterized in that: The lower mold (7) is connected to a cooling pipe (17) on one side, and a cooling channel (18) connected to the cooling pipe (17) is provided inside the lower mold (7). The lower mold (7) is connected to a cooling pipe (19) on the other side, and a manual valve is provided on both the cooling pipe (17) and the cooling pipe (19).
Citation Information