Method for preparing mixed explosive from coal-based synthetic oil

Coal-based synthetic oil was prepared by processes such as catalytic liquefaction, deep hydrorefining, and selective isomerization. Combined with modified ammonium nitrate and aluminum nitride, the stability and safety issues of traditional diesel oil in mixed explosives were solved, and the preparation of high-performance explosives was achieved.

CN121850814APending Publication Date: 2026-04-14JINGMEN LIAOYUAN TECH DEV
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202610134960.X
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-01-30
Publication Date
2026-04-14

AI Technical Summary

Technical Problem

Traditional diesel fuel-based mixed explosives suffer from problems such as large property fluctuations, high safety risks, poor low-temperature adaptability, and insufficient environmental performance. Furthermore, existing coal-based synthetic oils have not been optimized for mixed explosive applications, resulting in poor compatibility with ammonium nitrate and insufficient low-temperature fluidity.

Method used

Coal-based synthetic oil is prepared by a series of processes including catalytic liquefaction, deep hydrorefining, selective isomerization, and precise fractionation. A stable explosive formulation is formed by modifying porous ammonium nitrate and adding substances such as aluminum nitride.

Benefits of technology

It achieves rapid detonation velocity, high strength, and high storage stability of explosives, and can still mix normally at low temperatures, significantly reducing harmful gas emissions and improving the stability and safety of blasting effects.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

The invention belongs to the technical field of mixed explosive preparation, relates to a preparation method of special coal-based synthetic oil for mixed explosives, and belongs to the technical field of coal-based liquid fuel and explosive auxiliary materials. According to the method, the coal-based synthetic oil with proper viscosity, high flash point, good low-temperature fluidity, excellent oxidation stability and good compatibility with ammonium nitrate is prepared through specific coal liquefaction, hydrofining, isomerization and component blending processes. The product can safely and efficiently replace traditional diesel oil to be applied to on-site mixed loading explosives, has the characteristics of controllable performance, controllable cost and high adaptability, and can effectively solve the problems of property fluctuation, potential safety hazards, poor environmental adaptability and the like when the traditional diesel oil is used as a fuel phase of the mixed loading explosives.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention belongs to the field of mixed explosives preparation technology, and specifically relates to a method for preparing mixed explosives using coal-based synthetic oil. Background Technology

[0002] On-site mixed explosives (especially ammonium nitrate fuel oil explosives) are widely used in mining, infrastructure construction, and other fields due to their advantages such as high production efficiency, low transportation costs, and adaptability to complex blasting scenarios. The performance of these explosives hinges on the compatibility between the fuel phase and the oxidizer phase (mainly ammonium nitrate), with diesel fuel typically being used. However, traditional diesel fuel has several inherent drawbacks: Large property fluctuations: Diesel fuel depends on crude oil, and differences in crude oil quality from different origins and processing techniques at different refineries lead to significant fluctuations in key properties such as density, viscosity, and aromatic content. This directly affects the stability of the explosive formulation, resulting in uneven blasting power and unstable blasting effects. Significant safety hazards: Ordinary diesel fuel has a closed-cup flash point of approximately ≥60℃, making it prone to accidents due to leakage and high temperatures during explosive production, storage, and transportation. Poor low-temperature adaptability: Diesel fuel has a high pour point and is prone to solidification in cold regions (such as areas where winter temperatures drop below -10℃), preventing proper mixing with ammonium nitrate and affecting explosive production and use. Insufficient environmental performance: Diesel fuel contains a certain amount of sulfur, nitrogen impurities and aromatic components, which will generate harmful gases such as SOx, NOx and polycyclic aromatic hydrocarbons during the blasting process, polluting the working environment and endangering the health of construction workers.

[0003] Coal-based synthetic oil (CTL) is a product of converting solid coal into liquid fuel through coal liquefaction processes. Its main components are straight-chain alkanes, isoalkanes, and cycloalkanes, with extremely low levels of aromatics and sulfur and nitrogen impurities. It is pure and stable, theoretically making it an ideal alternative to diesel fuel for mixed explosives. However, conventional CTL processes are designed to produce automotive diesel fuel that meets national standards. Its viscosity, distillation range, pour point, and other performance indicators are set based on engine usage requirements and are not optimized for the specific application scenarios of mixed explosives. When used directly, it suffers from poor compatibility with ammonium nitrate and insufficient low-temperature fluidity, failing to meet the requirements for explosive preparation. Summary of the Invention

[0004] The purpose of this invention is to provide a method for preparing mixed explosives using coal-based synthetic oil, which has the advantages of fast detonation velocity, high strength, and high storage stability.

[0005] The above-mentioned technical objective of the present invention is achieved through the following technical solution: a method for preparing mixed explosives using coal-based synthetic oil, comprising the following raw materials by mass fraction: 5-6% coal-based synthetic oil; 80-85% modified porous ammonium nitrate; 8-10% emulsifier; 1-1.5% mixing reinforcing agent; mixing the above substances in proportion to prepare ammonium nitrate explosives, controlling the charge density, and producing finished explosive products.

[0006] A further provision of the present invention is that the coal-based synthetic oil is prepared by the following steps:

[0007] S1: Catalytic liquefaction and preliminary separation: Dry coal powder and circulating solvent are mixed at a mass ratio of 1:11-12, and 1%-3% of a composite metal catalyst by weight of dry coal powder is added to form a coal slurry. Hydrogenation liquefaction reaction is carried out under the conditions of hydrogen partial pressure of 15-20 MPa and temperature of 440-460℃. The reaction product is separated to obtain medium oil (180-350℃ fraction).

[0008] S2: Deep hydrorefining: The medium oil obtained in step S1 is fed into a fixed-bed reactor containing a Ni-Mo / Al2O3 catalyst for deep hydrorefining.

[0009] S3: The hydrorefined medium oil is fed into a fixed-bed reactor equipped with a Pt / SAPO-11 shape-selective isomerization catalyst, and the reaction is carried out at a temperature of 320-360℃, a hydrogen partial pressure of 610MPa, and a volume hourly space velocity of 1.0-2.0h. -1 The reaction proceeds under conditions where the hydrogen-to-oil volume ratio is 500-1800:1.

[0010] S4: The isomerized product is fed into a fractionation column, and the target fraction at 180-330℃ is retained;

[0011] S5: Pump the target fraction into the product blending tank, fine-tune according to viscosity and flash point requirements, add 50-100 ppm of 2,6-di-tert-butyl-p-cresol and 100-200 ppm of N,N'-disalynylpropanediamine, and gently stir the reaction at 40-50°C for 24 hours. After filtration, coal-based synthetic oil is obtained.

[0012] By adopting the above technical solution and employing a series of processes—"catalytic liquefaction → deep hydrorefining → selective isomerization → precise fractionation → functional blending"—the key performance characteristics of the product can be precisely controlled at each stage. In the catalytic liquefaction stage, coal is efficiently converted into liquid oil; in the deep hydrorefining stage, impurities such as sulfur, nitrogen, and oxygen, as well as aromatics, are thoroughly removed, significantly improving the purity and stability of the product; in the selective isomerization stage, the product's pour point is specifically lowered, effectively improving its low-temperature fluidity; in the precise fractionation stage, fractions meeting the requirements of explosives are precisely cut; and in the functional blending stage, viscosity and flash point are finely adjusted, and the product's storage stability is further optimized through additives.

[0013] The heavy oil produced during the preparation process is partially recycled as a solvent, and the hydrogen is recycled after recovery and purification, reducing raw material consumption and production costs. Meanwhile, my country has abundant coal resources, ensuring a stable supply of raw materials for coal-based synthetic oils. Compared to diesel fuel, which relies on imported crude oil, coal-based synthetic oils offer stronger cost competitiveness and supply security.

[0014] Deep hydrorefining: The medium oil obtained in step 1 is fed into a fixed-bed reactor packed with Ni-Mo / Al2O3 catalyst, and the reaction is carried out at a reaction temperature of 320-360℃, a hydrogen partial pressure of 610MPa, and a volume hourly space velocity of 1-2h. -1 The reaction is carried out under conditions where the hydrogen-to-oil volume ratio is 500-1800:1;

[0015] Selective isomerization dewaxing: The hydrorefined medium oil is fed into a fixed-bed reactor equipped with a Pt / SAPO-11 shape-selective isomerization catalyst, and the reaction is carried out at a temperature of 300-340℃, a hydrogen partial pressure of 46MPa, and a volume hourly space velocity of 1.0-1.5h. -1 The reaction is carried out under conditions where the hydrogen-to-oil volume ratio is 400-1600:1;

[0016] Fractionation and target fraction cutting: The isomerized product is fed into a fractionation column to cut out the target fraction at 180~330℃;

[0017] Functional blending and stabilization: The target fraction is pumped into the product blending tank, fine-tuned according to viscosity and flash point requirements, 50-100 ppm of antioxidant and 100-200 ppm of metal passivator are added, and the mixture is gently stirred at 40-50℃ for 24 hours. After filtration, the final product is obtained.

[0018] A further provision of the present invention is that the composite metal catalyst is a composite of an iron-based catalyst and ammonium molybdate, wherein the mass ratio of the iron-based catalyst to ammonium molybdate is 3-5:1.

[0019] A further provision of the present invention is that the modified porous ammonium nitrate is prepared by the following steps: an appropriate amount of a first modifier is added to the ammonium nitrate particles, and the mixture is stirred to adsorb onto the surface of the ammonium nitrate particles. After stirring for 5-10 minutes, a second modifier and an accelerator are added, and the mixture is stirred continuously for 1 hour to reach adsorption equilibrium. The modified ammonium nitrate is then placed in a constant temperature blower and dried for 24 hours to obtain modified porous ammonium nitrate particles.

[0020] A further provision of the present invention is that the mass ratio of the ammonium nitrate particles, the first modifier, the second modifier, and the accelerator is 1-1.5:2:1:0.5.

[0021] A further provision of the present invention is that the first modifier is octadecaneamine acetate.

[0022] A further provision of the present invention is that the second modifier is sodium dodecylbenzenesulfonate.

[0023] A further provision of the present invention is that the accelerator is polyoxyethylene dehydrated sorbitan fatty acid ester.

[0024] A further provision of the present invention is that the emulsifier is an acylated phospholipid complex emulsion.

[0025] By adopting the above technical solution, the ammonium nitrate in this invention is expanded porous ammonium nitrate, which is a commonly used substance in mixed explosives. Due to the strong electrostatic adsorption between the surfactant and ammonium nitrate through ion or ion exchange, a non-polar group coating layer is formed on the surface of ammonium nitrate. This can effectively reduce the surface free energy of ammonium nitrate and significantly improve the various physicochemical properties of ammonium nitrate. The electrostatic interaction between cationic surfactant and ammonium nitrate is stronger than that between anionic surfactant and composite surfactant. It has a multi-component system and allows multiple types of surfactant to produce a synergistic effect. The composite surfactant is adsorbed on the surface of ammonium nitrate, changing the surface properties, reducing the specific surface area, and lowering the surface free energy of ammonium nitrate.

[0026] A further provision of the present invention is that the mixed reinforcing agent is aluminum nitride.

[0027] The beneficial effects of this invention are as follows: The aluminum nitride added to the on-site mixed emulsion explosive under this formula will dissociate and release a large amount of gas at the moment of the explosive explosion, resulting in an increase in the amount of gas released by the explosive explosion. At the same time, when aluminum nitride dissociates under high pressure, its internal crystal structure changes, chemical bonds break and new chemical bonds are formed, releasing a large amount of heat, which increases the heat of explosion of the explosive sample. Macroscopically, this is manifested as an increase in the detonation velocity of the explosive sample. Because aluminum nitride releases a large amount of gas and heat when it dissociates under high pressure, the amount and temperature of the explosive gas are increased, the contact area between the explosive gas and the air is increased, the resistance of the detonation wave generated by the explosion in the explosive is reduced, and the detonation velocity of the explosive sample is increased.

[0028] A series of processes—catalytic liquefaction, deep hydrorefining, selective isomerization, precision fractionation, and functional blending—are employed to achieve step-by-step fine-tuning of key product performance. In the catalytic liquefaction stage, coal is efficiently converted into liquid oil. In the deep hydrorefining stage, impurities such as sulfur, nitrogen, and oxygen, as well as aromatics, are thoroughly removed, significantly improving the product's purity and stability. In the selective isomerization stage, the product's pour point is specifically lowered, effectively improving its low-temperature fluidity. In the precision fractionation stage, fractions tailored to the explosives' requirements are precisely extracted. Finally, in the functional blending stage, viscosity and flash point are finely adjusted, and additives are used to further optimize the product's storage stability. Detailed Implementation

[0029] The technical solutions in the embodiments will be clearly and completely described below. Obviously, the described embodiments are only a part of the embodiments of the present invention, and not all of them. All other embodiments obtained by those skilled in the art based on the embodiments of the present invention without creative effort are within the scope of protection of the present invention.

[0030] Example 1

[0031] (a) Raw material preparation: Bituminous coal (vitrinite reflectance R0=1.0%, dry ash-free volatile matter V) is selected. daf =38%), crushed, dried to 1.5% moisture content, and ground into coal powder with a particle size <200 mesh; the composite metal catalyst is a composite of Fe2O3 and ammonium molybdate (mass ratio 4:1); the hydrorefining catalyst is Ni-Mo / Al2O3 (NiO content 3%, MoO3 content 20%); the isomerization catalyst is Pt / SAPO-11 (Pt loading 0.5%); the hydrogen purity is 99.95%.

[0032] (II) Preparation process:

[0033] 1. Catalytic liquefaction and preliminary separation: Coal powder and recycled solvent (self-produced medium-quality oil) are mixed at a mass ratio of 1:1.2, and 2% (dry coal-based) of composite metal catalyst is added. The mixture is stirred at 70°C for 1.5 hours to prepare a coal slurry. The coal slurry is mixed with high-pressure hydrogen and then fed into a slurry bed reactor. The hydrogen partial pressure is 18 MPa, the temperature is 450°C, the space velocity is 1.0 h⁻¹, and the reaction time is 5 hours. After multi-stage separation, medium-quality oil (180~350°C fraction) is obtained.

[0034] 2. Deep hydrorefining: Medium oil enters the hydrorefining reactor, the reaction temperature is 340℃, the hydrogen partial pressure is 8MPa, the volume hourly space velocity is 1.5h⁻¹, and the hydrogen-to-oil volume ratio is 600:1. After the reaction, hydrorefined oil is obtained.

[0035] 3. Selective isomerization dewaxing: Hydrogenated refined oil enters the isomerization reactor, the reaction temperature is 320℃, the hydrogen partial pressure is 5MPa, the volume hourly space velocity is 1.2h⁻¹, and the hydrogen-to-oil volume ratio is 500:1. After the reaction, isomerized oil is obtained.

[0036] 4. Fractionation and Target Fraction Cutting: The isomerized oil is fed into the fractionation tower, and the reflux ratio is controlled at 4:1 to cut out the target fraction at 180~330℃.

[0037] 5. Functional Blending and Stabilization: The target fraction was fed into a blending tank, and its kinematic viscosity at 40℃ was measured to be 3.8 mm² / s (meets requirements), and its closed-cup flash point was 85℃ (meets requirements). 80 ppm BHT and 150 ppm N,N'-disalicylic acid propylenediamine were added, and the mixture was stirred at 45℃ for 3 hours. After filtration through a 10 μm filter, coal-based synthetic oil was obtained.

[0038] 6% coal-based synthetic oil, 84% modified porous ammonium nitrate, 9% acylated phospholipid composite emulsion, and 1% aluminum nitride were mixed in proportion to prepare ammonium nitrate explosives. The charge density was controlled to produce the finished explosive.

[0039] Example 2

[0040] (I) Raw material preparation: Bituminous coal (vitrinite reflectance R0=0.9%, dry and ash-free volatile matter V) is selected. daf =36%), crushed, dried to 1.2% moisture content, and ground into coal powder with a particle size <200 mesh; the composite metal catalyst is a composite of Fe2O3 and ammonium molybdate (mass ratio 3:1); the hydrorefining catalyst is Ni-Mo / Al2O3 (NiO content 2.5%, MoO3 content 18%); the isomerization catalyst is Pt / SAPO-11 (Pt loading 0.4%); the hydrogen purity is 99.9%.

[0041] (II) Preparation process:

[0042] 1. Catalytic liquefaction and preliminary separation: Coal powder and recycled solvent (initially anthracene oil) were mixed at a mass ratio of 1:1.0, and 1.5% (dry coal-based) of a composite metal catalyst was added. The mixture was stirred at 60°C for 1 hour to prepare a coal slurry. The coal slurry was mixed with high-pressure hydrogen and then fed into a slurry bed reactor. The hydrogen partial pressure was 15 MPa, the temperature was 440°C, the space velocity was 0.8 h⁻¹, and the reaction time was 4 hours. After multi-stage separation, medium-quality oil (180~350°C fraction) was obtained.

[0043] 2. Deep hydrorefining: Medium oil enters the hydrorefining reactor, the reaction temperature is 320℃, the hydrogen partial pressure is 6MPa, the volume hourly space velocity is 1.0h⁻¹, and the hydrogen-to-oil volume ratio is 500:1. After the reaction, hydrorefined oil is obtained.

[0044] 3. Selective isomerization dewaxing: Hydrogenated refined oil enters the isomerization reactor, the reaction temperature is 300℃, the hydrogen partial pressure is 4MPa, the volume hourly space velocity is 1.0h⁻¹, and the hydrogen-to-oil volume ratio is 400:1. After the reaction, isomerized oil is obtained.

[0045] 4. Fractionation and Target Fraction Cutting: The isomerized oil is fed into the fractionation tower, and the reflux ratio is controlled at 3:1 to cut out the target fraction at 180~330℃.

[0046] 5. Functional Blending and Stabilization: The target fraction was fed into a blending tank, and its kinematic viscosity at 40℃ was measured to be 4.3 mm² / s (meets requirements), and its closed-cup flash point was 82℃ (meets requirements). 50 ppm BHT and 100 ppm N,N'-disalynylpropanediamine were added, and the mixture was stirred at 40℃ for 2 hours. After filtration through a 10 μm filter, coal-based synthetic oil was obtained.

[0047] 6% coal-based synthetic oil, 84% modified porous ammonium nitrate, 9% acylated phospholipid composite emulsion, and 1% aluminum nitride were mixed in proportion to prepare ammonium nitrate explosives. The charge density was controlled to produce the finished explosive.

[0048] Example 3

[0049] (I) Raw material preparation: Bituminous coal (vitrinite reflectance R0=1.1%, dry ash-free volatile matter Vdaf=40%) was selected, crushed, dried to moisture content of 1.8%, and ground into coal powder with a particle size of <200 mesh; the composite metal catalyst was a composite of Fe2O3 and ammonium molybdate (mass ratio 5:1); the hydrorefining catalyst was Ni-Mo / Al2O3 (NiO content 4%, MoO3 content 22%); the isomerization catalyst was Pt / SAPO-11 (Pt loading 0.6%); the hydrogen purity was 99.98%.

[0050] (II) Preparation process:

[0051] 1. Catalytic liquefaction and preliminary separation: Coal powder and recycled solvent (self-produced medium-quality oil) are mixed at a mass ratio of 1:1.5, and 3% (dry coal-based) of composite metal catalyst is added. The mixture is stirred at 80°C for 2 hours to prepare a coal slurry. The coal slurry is mixed with high-pressure hydrogen and then fed into a slurry bed reactor. The hydrogen partial pressure is 20 MPa, the temperature is 460°C, the space velocity is 1.2 h⁻¹, and the reaction time is 6 hours. After multi-stage separation, medium-quality oil (180~350°C fraction) is obtained.

[0052] 2. Deep hydrorefining: Medium oil enters the hydrorefining reactor, the reaction temperature is 360℃, the hydrogen partial pressure is 10MPa, the volume hourly space velocity is 2.0h⁻¹, and the hydrogen-to-oil volume ratio is 800:1. After the reaction, hydrorefined oil is obtained.

[0053] 3. Selective isomerization dewaxing: Hydrogenated refined oil enters the isomerization reactor, the reaction temperature is 340℃, the hydrogen partial pressure is 6MPa, the volume hourly space velocity is 1.5h⁻¹, and the hydrogen-to-oil volume ratio is 600:1. After the reaction, isomerized oil is obtained.

[0054] 4. Fractionation and Target Fraction Cutting: The isomerized oil is fed into the fractionation tower, and the reflux ratio is controlled at 5:1 to cut out the target fraction at 180~330℃.

[0055] 5. Functional Blending and Stabilization: The target fraction was fed into a blending tank, and its kinematic viscosity at 40℃ was measured to be 2.6 mm² / s (meets requirements), and its closed-cup flash point was 88℃ (meets requirements). 100 ppm BHT and 200 ppm N,N'-disalynylpropanediamine were added, and the mixture was stirred at 50℃ for 4 hours. After filtration through a 10 μm filter, coal-based synthetic oil was obtained.

[0056] 6% coal-based synthetic oil, 84% modified porous ammonium nitrate, 9% acylated phospholipid composite emulsion, and 1% aluminum nitride were mixed in proportion to prepare ammonium nitrate explosives. The charge density was controlled to produce the finished explosive.

[0057] Comparative Example 1 (Conventional Diesel)

[0058] Commercially available #0 diesel oil was selected and used as the fuel phase for the mixed explosives according to conventional methods. The diesel oil was mixed with ammonium nitrate in a conventional ratio to prepare ammonium nitrate explosives. Detonation tests were conducted, and the results showed that the detonation velocity fluctuation range of the explosives was 15%. The content of SOx, NOx and polycyclic aromatic hydrocarbons in the working environment after blasting was high. At -15℃, the diesel oil solidified and could not be mixed normally with ammonium nitrate.

[0059] Comparative Example 2 (coal-based synthetic oil without isomerization treatment)

[0060] Using the same raw materials and preparation steps as in Example 1, but omitting step three (selective isomerization dewaxing), the hydrotreated oil was directly fractionated, cut, and blended to obtain the product.

[0061] When this product was mixed with ammonium nitrate to prepare ammonium nitrate explosive, the product's fluidity decreased and it was not mixed evenly with ammonium nitrate at -15°C, resulting in a decrease in the explosive's detonation performance. The detonation velocity was only 75% of that of the explosive prepared with the product in Example 1.

[0062] Comparative Example 3 (coal-based synthetic oil that has not undergone deep hydrorefining)

[0063] Using the same raw materials and preparation steps as in Example 1, but omitting step two (deep hydrorefining), the medium-quality oil obtained from catalytic liquefaction was directly isomerized, fractionated, and blended to obtain the product. This product was mixed with ammonium nitrate to prepare ammonium nitrate explosives. The content of harmful gases in the working environment after blasting was significantly higher than in Example 1, and the product showed signs of gelation after 3 months of storage, indicating decreased compatibility with ammonium nitrate.

[0064] Comparative Example 4

[0065] Coal-based synthetic oil was prepared using the same raw materials and preparation steps as in Example 1, but unmodified porous ammonium nitrate 84% was used when preparing the explosive product.

[0066] Comparative Example 5

[0067] Coal-based synthetic oil was prepared using the same raw materials and preparation steps as in Example 1. However, in the preparation of the finished explosive, the proportion of coal-based synthetic oil was adjusted to 6%, and the proportion of modified porous ammonium nitrate was 94%. Subsequently, the above substances were mixed in a predetermined ratio to prepare ammonium nitrate explosive, and the charge density was strictly controlled to finally produce the finished explosive.

[0068] Comparative Example 6

[0069] Coal-based synthetic oil was prepared using the same raw materials and preparation steps as in Example 1. However, in the preparation of the finished explosive, the proportion of coal-based synthetic oil was adjusted to 6%, the proportion of modified porous ammonium nitrate was 85%, and the proportion of acylated phospholipid composite emulsion was 9%. Subsequently, the above substances were mixed in a predetermined ratio to prepare ammonium nitrate explosive, and the charge density was strictly controlled to finally produce the finished explosive.

[0070] Comparative Example 7

[0071] Coal-based synthetic oil was prepared using the same raw materials and preparation steps as in Example 1. However, in the preparation of the finished explosive, the proportion of coal-based synthetic oil was adjusted to 6%, the proportion of modified porous ammonium nitrate was 93%, and the proportion of aluminum nitride was 1%. Subsequently, the above substances were mixed in a predetermined ratio to prepare ammonium nitrate explosive, and the charge density was strictly controlled to finally produce the finished explosive.

[0072] Test Project Example 1 Example 2 Example 3 Comparative Example 1 Comparative Example 2 Comparative Example 3 Comparative Example 4 Comparative Example 5 Comparative Example 6 Comparative Example 7 Explosive speed (m / s) 3800±50 3750±60 3850±45 3200±480 2850±80 3100±100 3300±90 2900±75 3050±85 2700±110 -15℃ low temperature adaptability Good, well mixed Good, well mixed Good, well mixed Solidified, unable to mix Poor liquidity, uneven mixing Good, well mixed Good, well mixed Good, well mixed Good, well mixed Good, well mixed Storage stability (3 months) Non-gelatinized, with good compatibility Non-gelatinized, with good compatibility Non-gelatinized, with good compatibility Non-gelatinized, with generally poor compatibility. Non-gelatinized, with generally poor compatibility. gelatinization, resulting in decreased compatibility Non-gelatinized, with generally poor compatibility. Non-gelatinized, with generally poor compatibility. Non-gelatinized, with good compatibility No gelling, poor compatibility Harmful gas content after blasting Low Low Low high lower higher Low Low Low Low Detonation integrity excellent excellent excellent General (uneven power) Difference generally generally Difference generally Difference

[0073] Examples 1-3 show that the coal-based synthetic oil and explosive formulations prepared using optimized processes comprehensively surpass traditional diesel (Comparative Example 1) in key performance aspects. The detonation velocity is increased by 18.75%-20.31% with a fluctuation range reduced to ±1.3%-1.6%. It can still mix normally at low temperatures (-15℃), with significantly reduced harmful gas emissions and excellent storage stability.

[0074] Selective isomerization dewaxing (step 3) is the core of ensuring low-temperature fluidity and detonation performance. Without it, the detonation velocity decreases by 25% (Comparative Example 2); deep hydrorefining (step 2) can effectively remove impurities and avoid excessive harmful gases and storage gelling (Comparative Example 3).

[0075] Modified porous ammonium nitrate can improve the detonation velocity and compatibility of explosives, while the detonation velocity decreases by 13.16% when unmodified (Comparative Example 4); excessive ammonium nitrate (94%) will lead to insufficient fuel phase and a decrease in detonation velocity of 23.68% (Comparative Example 5); the mixing enhancer (aluminum nitride) can improve the detonation velocity, but its absence will result in a decrease of 19.74% (Comparative Example 6); the emulsifier (acylated phospholipid complex emulsion) ensures the uniformity of mixing, but its absence will result in a decrease of 28.95% in detonation velocity and a deterioration in compatibility (Comparative Example 7).

Claims

1. A method for preparing mixed explosives using coal-based synthetic oil, characterized in that: The raw materials include the following mass fractions: 5-6% coal-based synthetic oil; 80-85% modified porous ammonium nitrate; 8-10% emulsifier; and 1-1.5% mixed reinforcing agent. The above substances are mixed in proportion to prepare ammonium nitrate explosives, and the charge density is controlled to produce the finished explosive.

2. The preparation method of mixed explosives using coal-based synthetic oil according to claim 1, characterized in that: The coal-based synthetic oil is prepared through the following steps: S1: Dry coal powder and circulating solvent are mixed at a mass ratio of 1:11-12, and 1%-3% of the weight of the dry coal powder composite metal catalyst is added to make coal slurry. Hydrogenation liquefaction reaction is carried out, and the reaction product is separated to obtain medium oil. S2: The medium oil obtained in step S1 is fed into a fixed-bed reactor containing a Ni-Mo / Al2O3 catalyst for deep hydrorefining. S3: The hydrorefined medium oil is fed into a fixed-bed reactor containing a Pt / SAPO-11 shape-selective isomerization catalyst for reaction; S4: The isomerized product is fed into a fractionation column, and the target fraction at 180-330℃ is retained; S5: Pump the target fraction into the product blending tank, fine-tune according to viscosity and flash point requirements, add 50-100 ppm of 2,6-di-tert-butyl-p-cresol and 100-200 ppm of N,N'-disalynylpropanediamine, and gently stir the reaction at 40-50°C for 24 hours. After filtration, coal-based synthetic oil is obtained.

3. The method for preparing mixed explosives using coal-based synthetic oil according to claim 1, characterized in that: The composite metal catalyst is a complex of an iron-based catalyst and ammonium molybdate, with a mass ratio of 3-5:1 between the iron-based catalyst and ammonium molybdate.

4. The method for preparing mixed explosives using coal-based synthetic oil according to claim 1, characterized in that: The modified porous ammonium nitrate is prepared by the following steps: an appropriate amount of the first modifier is added to the ammonium nitrate particles and stirred to adsorb onto the surface of the ammonium nitrate particles. After stirring for 5-10 minutes, the second modifier and the accelerator are added and stirred continuously for 1 hour to reach adsorption equilibrium. The modified ammonium nitrate is then placed in a constant temperature blower and dried for 24 hours to obtain the modified porous ammonium nitrate particles.

5. The method for preparing mixed explosives using coal-based synthetic oil according to claim 1, characterized in that: The mass ratio of the ammonium nitrate particles, the first modifier, the second modifier, and the accelerator is 1-1.5:2:1:0.

5.

6. The method for preparing mixed explosives using coal-based synthetic oil according to claim 1, characterized in that: The first modifier is octadecylamine acetate.

7. The method for preparing mixed explosives using coal-based synthetic oil according to claim 1, characterized in that: The second modifier is sodium dodecylbenzenesulfonate.

8. The method for preparing mixed explosives using coal-based synthetic oil according to claim 1, characterized in that: The accelerator is polyoxyethylene dehydrated sorbitol fatty acid ester.

9. The method for preparing mixed explosives using coal-based synthetic oil according to claim 1, characterized in that: The emulsifier is an acylated phospholipid complex emulsion.

10. The method for preparing mixed explosives using coal-based synthetic oil according to claim 1, characterized in that: The mixed reinforcing agent is aluminum nitride.