Composite material fatigue damage early warning method

By dividing the fatigue life process into cyclic windows, calculating and normalizing the acoustic emission energy and hysteresis energy increments, and establishing a benchmark consistency relationship, the problem of real-time monitoring of composite material damage state was solved, and damage early warning and life prediction were realized.

CN122754342BActive Publication Date: 2026-11-10HARBIN INST OF TECH
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
CN202611208044.2
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2026-08-11
Publication Date
2026-11-10
Estimated Expiration
2046-08-11

AI Technical Summary

Technical Problem

How to characterize the damage state of composite materials in real time, continuously and reliably during fatigue loading, especially to address the problems of their hidden nature, suddenness, coupling of multiple damage mechanisms and complex damage evolution paths.

Method used

The fatigue life process is divided into multiple cycle windows. The increment of effective acoustic emission energy and the increment of hysteresis energy in each cycle window are calculated. A benchmark consistency relationship between the normalized hysteresis energy increment and the benchmark effective acoustic emission energy is established through normalization. The benchmark residual value is calculated using the benchmark consistency relationship, and the actual residual is compared to determine the damage state.

Benefits of technology

It enables real-time early warning of fatigue damage in composite materials, and can perform damage state judgment, stage transition identification, and instability propagation early warning, thereby improving the accuracy and reliability of damage monitoring.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN122754342B_ABST
    Figure CN122754342B_ABST
Patent Text Reader

Abstract

The present application relates to the technical field of material damage testing, and a composite material fatigue damage early warning method, comprising: dividing a fatigue life process into multiple cycle windows, calculating effective acoustic emission energy increments in each cycle window, and calculating hysteresis energy increments in each cycle window; performing normalization processing on the effective acoustic emission energy increments and the hysteresis energy increments, establishing a reference consistency relationship between normalized hysteresis energy increments and reference effective acoustic emission energy; in a stable fatigue cycle interval, comparing the reference effective acoustic emission energy with normalized effective acoustic emission energy increments to obtain a reference residual value; in any cycle window after the stable fatigue cycle interval, comparing normalized effective acoustic emission energy increments in the cycle window with the reference effective acoustic emission energy to obtain a comparison residual; and comparing the comparison residual with the reference residual value in the stable fatigue cycle interval to determine a damage state. The present application can early warn fatigue damage of a composite material.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of material damage testing technology, and in particular to a method for early warning of fatigue damage in composite materials. Background Technology

[0002] Fiber-reinforced composite materials possess advantages such as high specific strength, high specific stiffness, corrosion resistance, fatigue resistance, and strong designability, and have been widely used in aerospace, rail transportation, wind turbine blades, ship structures, and lightweight automotive structures. During long-term service, composite structures are typically subjected to various factors including cyclic loading, temperature changes, assembly stress, impact damage, and environmental aging, making them prone to progressive damage such as matrix cracking, fiber / matrix interface debonding, delamination, fiber fracture, and localized crushing. Due to the characteristics of composite material damage—including its insidious nature, sudden onset, multiple coupled damage mechanisms, and complex damage evolution paths—how to characterize the damage state in real-time, continuously, and reliably during fatigue loading is a crucial issue in the health monitoring and life assessment of composite structures.

[0003] Therefore, there is an urgent need for a method that can provide early warning of fatigue damage in composite materials. Summary of the Invention

[0004] This invention provides a method for early warning of fatigue damage in composite materials, which can provide early warning of fatigue damage in composite materials.

[0005] In a first aspect, embodiments of the present invention provide a method for early warning of fatigue damage in composite materials, comprising: The fatigue life process is divided into multiple cyclic windows. The effective acoustic emission energy increment and hysteresis energy increment within each cyclic window are calculated. Each cyclic window includes at least one fatigue cycle, and one fatigue cycle corresponds to a periodic change in the fatigue load signal. The effective acoustic emission energy increment and the hysteresis energy increment are normalized respectively to obtain the normalized effective acoustic emission energy increment and the normalized hysteresis energy increment, and a benchmark consistency relationship is established between the normalized hysteresis energy increment and the benchmark effective acoustic emission energy. Within a predetermined stable fatigue cycle interval, each cycle window performs the following: calculating the baseline effective acoustic emission energy using the baseline consistency relationship and the normalized hysteresis energy increment, and comparing the baseline effective acoustic emission energy with the normalized effective acoustic emission energy increment to obtain the baseline residual value; In any cycle window after the stable fatigue cycle interval, the reference effective acoustic emission energy is calculated based on the reference consistency relationship and the normalized hysteresis energy increment, and the normalized effective acoustic emission energy increment in the cycle window is compared with the reference effective acoustic emission energy to obtain the comparison residual; The damage state is determined by comparing the comparative residual with the baseline residual value within the stable fatigue cycle interval.

[0006] Secondly, embodiments of the present invention also provide a composite material fatigue damage early warning device for implementing any one of the above methods, the device comprising: The incremental calculation module is used to divide the fatigue life process into multiple cyclic windows, calculate the effective acoustic emission energy increment in each cyclic window, and calculate the hysteresis energy increment in each cyclic window; wherein, each cyclic window includes at least one fatigue cycle, and one fatigue cycle corresponds to the fatigue load signal changing periodically once; The benchmark establishment module is used to normalize the effective acoustic emission energy increment and the hysteresis energy increment respectively to obtain the normalized effective acoustic emission energy increment and the normalized hysteresis energy increment, and to establish a benchmark consistency relationship between the normalized hysteresis energy increment and the benchmark effective acoustic emission energy. The benchmark residual module is used to perform the following for each cycle window within a predetermined stable fatigue cycle range: calculate the benchmark effective acoustic emission energy using the benchmark consistency relationship and the normalized hysteresis energy increment, and compare the benchmark effective acoustic emission energy with the normalized effective acoustic emission energy increment to obtain the benchmark residual value; The comparison residual module is used to calculate the benchmark effective acoustic emission energy based on the benchmark consistency relationship and the normalized hysteresis energy increment in any cycle window after the stable fatigue cycle interval, and compare the normalized effective acoustic emission energy increment in the cycle window with the benchmark effective acoustic emission energy to obtain the comparison residual; The early warning module is used to compare the comparison residual with the benchmark residual value within the stable fatigue cycle interval to determine the damage state.

[0007] Thirdly, embodiments of the present invention also provide an electronic device, including a memory and a processor, wherein the memory stores a computer program, and when the processor executes the computer program, it implements the method described in any embodiment of this specification.

[0008] Fourthly, embodiments of the present invention also provide a computer-readable storage medium having a computer program stored thereon, which, when executed in a computer, causes the computer to perform the methods described in any embodiment of this specification.

[0009] Compared with the prior art, the present invention has at least the following beneficial effects: In this embodiment, the fatigue life process is first divided into multiple cyclic windows. Within each cyclic window, one or more acoustic emission events accumulate energy, and simultaneously, a certain amount of hysteresis energy also accumulates. Through these artificially defined cyclic windows, the increments of effective acoustic emission energy and hysteresis energy are correlated within the same time period. To eliminate the influence of different specimen sizes, load levels, stress levels, and structural forms on the energy dimensions, the increments of effective acoustic emission energy and hysteresis energy are normalized. Based on the normalized hysteresis energy increment and the benchmark consistency relationship, the benchmark effective acoustic emission energy can be obtained. Since the increments of effective acoustic emission energy and hysteresis energy are not completely synchronized throughout the fatigue life process, comparing the actual normalized effective acoustic emission energy increment with the calculated benchmark effective acoustic emission energy yields the residual. The residual values ​​at different stages exhibit certain regularities. Therefore, multiple benchmark residuals calculated within the stable fatigue cycle interval are selected as benchmarks and compared with the comparative residuals within the subsequent cycle window. Based on the difference between the comparative residuals and the benchmark residuals, the life of the composite material can be predicted, and damage status can be judged, stage transition can be identified, and instability propagation can be warned. Attached Figure Description

[0010] To more clearly illustrate the technical solutions in the embodiments of the present invention or the prior art, the drawings used in the description of the embodiments or the prior art will be briefly introduced below. Obviously, the drawings described below are some embodiments of the present invention. For those skilled in the art, other drawings can be obtained based on these drawings without creative effort.

[0011] Figure 1 This is a flowchart of a fatigue damage early warning method for composite materials provided in an embodiment of the present invention. Detailed Implementation

[0012] To make the objectives, technical solutions, and advantages of the embodiments of the present invention clearer, the technical solutions of the embodiments of the present invention will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are some embodiments of the present invention, but not all embodiments. All other embodiments obtained by those skilled in the art based on the embodiments of the present invention without creative effort are within the scope of protection of the present invention.

[0013] The following describes the specific implementation of the above concept.

[0014] See Figure 1 This invention provides a method for early warning of fatigue damage in composite materials, comprising: The fatigue life process is divided into multiple cyclic windows. The effective acoustic emission energy increment and hysteresis energy increment within each cyclic window are calculated. Each cyclic window includes at least one fatigue cycle, and one fatigue cycle corresponds to a periodic change in the fatigue load signal. The effective acoustic emission energy increment and the hysteresis energy increment are normalized respectively to obtain the normalized effective acoustic emission energy increment and the normalized hysteresis energy increment, and a benchmark consistency relationship is established between the normalized hysteresis energy increment and the benchmark effective acoustic emission energy. Within a predetermined stable fatigue cycle interval, each cycle window performs the following: calculating the baseline effective acoustic emission energy using the baseline consistency relationship and the normalized hysteresis energy increment, and comparing the baseline effective acoustic emission energy with the normalized effective acoustic emission energy increment to obtain the baseline residual value; In any cycle window after the stable fatigue cycle interval, the reference effective acoustic emission energy is calculated based on the reference consistency relationship and the normalized hysteresis energy increment, and the normalized effective acoustic emission energy increment in the cycle window is compared with the reference effective acoustic emission energy to obtain the comparison residual; The damage state is determined by comparing the comparative residual with the baseline residual value within the stable fatigue cycle interval.

[0015] In this embodiment, the fatigue life process is first divided into multiple cyclic windows. Within each cyclic window, one or more acoustic emission events accumulate energy, and simultaneously, a certain amount of hysteresis energy also accumulates. Through these artificially defined cyclic windows, the increments of effective acoustic emission energy and hysteresis energy are correlated within the same time period. To eliminate the influence of different specimen sizes, load levels, stress levels, and structural forms on the energy dimensions, the increments of effective acoustic emission energy and hysteresis energy are normalized. Based on the normalized hysteresis energy increment and the benchmark consistency relationship, the benchmark effective acoustic emission energy can be obtained. Since the increments of effective acoustic emission energy and hysteresis energy are not completely synchronized throughout the fatigue life process, comparing the actual normalized effective acoustic emission energy increment with the calculated benchmark effective acoustic emission energy yields the residual. The residual values ​​at different stages exhibit certain regularities. Therefore, multiple benchmark residuals calculated within the stable fatigue cycle interval are selected as benchmarks and compared with the comparative residuals within the subsequent cycle window. Based on the difference between the comparative residuals and the benchmark residuals, the life of the composite material can be predicted, and damage status can be judged, stage transition can be identified, and instability propagation can be warned.

[0016] In this embodiment, acoustic emission data is acquired through fatigue loading tests. For example, fatigue loading is applied to composite material specimens or composite material structures, and the loading methods include, but are not limited to, tension-tension fatigue, compression-compression fatigue, tension-compression fatigue, bending fatigue, fatigue of open structures, fatigue of connected structures, or amplitude-variable fatigue. During the fatigue loading process, load signals, displacement signals, number of cycles, loading frequency, cycle phase information, and raw acoustic emission waveform signals are acquired simultaneously.

[0017] Acoustic emission sensors are placed on the surface of composite material specimens or structures. One or more sensors can be arranged according to the expected damage area, sensor sensitivity, structural dimensions, and wave propagation path. The acoustic emission acquisition system records information such as the trigger time, raw waveform, channel number, amplitude, energy, duration, rise time, count, peak frequency, and average frequency for each acoustic emission event. The fatigue testing machine synchronously records the load-displacement curve for each cycle.

[0018] Before fatigue testing, background noise acquisition and lead breakage calibration can be performed. Background noise acquisition is used to determine the ambient noise level, mechanical noise frequency band, and initial acquisition threshold; lead breakage calibration is used to check the coupling status of the acoustic emission sensor, channel sensitivity, and multi-channel response consistency.

[0019] In some embodiments of the present invention, before calculating the effective acoustic emission energy increment within each cyclic window, the method further includes: Acoustic emission events obtained during composite material fatigue testing are synchronously assigned to fatigue cycles, so that each acoustic emission event is assigned to a corresponding fatigue cycle number; wherein, the fatigue cycle number corresponds to the number of periodic changes in the fatigue load signal.

[0020] In this embodiment, in order to calculate the effective acoustic emission energy increment within the loop window, it is necessary to know the loop window in which each acoustic emission event is located, and it is necessary to know the fatigue cycle in which the acoustic emission event is located (the loop window includes at least one fatigue cycle). Therefore, the fatigue cycles of the acoustic emission events need to be synchronously assigned.

[0021] Specifically, for the first Each acoustic emission event is triggered at the following time: Based on fatigue load signals The periodic changes, determine Fatigue cycle number Further based on In the The relative position within each cycle determines its cycle phase. The cyclic phase can be divided into the loading rise segment, the peak load neighborhood, the unloading segment, and the valley load neighborhood, or it can be represented by a phase angle from 0° to 360°.

[0022] Through the above processing, acoustic emission events in a continuous time series can be transformed into a cyclic synchronous acoustic emission event sequence. This sequence contains not only the waveform and energy characteristics of the acoustic emission events, but also their corresponding fatigue cycle numbers and cycle phase information.

[0023] In some embodiments of the present invention, calculating the effective acoustic emission energy increment within each cyclic window includes: Based on the validity criteria extracted from the original acoustic emission waveform, a validity score is established for each acoustic emission event; The weights of acoustic emission events are determined based on the effectiveness score, and the effective acoustic emission energy increment is calculated based on the weights of the acoustic emission events and the energy of the acoustic emission events.

[0024] To further improve the accuracy of the data, the validity of the acoustic emission signals is determined. Specifically, the acquired raw acoustic emission waveforms are preprocessed. Preprocessing methods include, but are not limited to, DC component removal, normalization, bandpass filtering, waveform truncation, endpoint correction, abnormal saturation waveform removal, and noise band suppression.

[0025] Subsequently, validity criteria are extracted based on the original acoustic emission waveform. These validity criteria include at least two categories: time-domain criteria, including peak value, root mean square value, kurtosis, skewness, duration, rise time, waveform factor, impulse factor, and margin factor; frequency-domain criteria, including dominant frequency, peak frequency, spectral centroid, effective bandwidth energy percentage, spectral entropy, and power spectral density; time-frequency domain criteria, including short-time Fourier transform energy distribution, continuous wavelet transform energy distribution, wavelet packet energy, empirical mode decomposition mode energy, or variational mode decomposition mode energy; multi-channel consistency criteria, including trigger consistency of the same event across multiple channels, reasonableness of arrival time difference, inter-channel correlation coefficient, and spatial attenuation law; cyclic phase reasonableness criteria, including whether the acoustic emission event is concentrated in the peak load neighborhood, the loading rise segment, or other preset damage-sensitive phase intervals; and signal-to-noise ratio criteria, including the ratio of event energy to background noise energy, the ratio of effective bandwidth energy to noise bandwidth energy, and the correlation coefficient between the reconstructed waveform and the original waveform.

[0026] For the Based on acoustic emission events, an effectiveness score is constructed. : in, This is the normalized signal-to-noise ratio metric. As a normalized kurtosis or shock index, This is a normalized effective frequency band energy percentage indicator. To normalize the multi-channel consistency index, To normalize the rationality index of cyclic phase, For waveform correlation or waveform reconstruction quality indicators, to These are the weighting coefficients.

[0027] when Greater than or equal to the preset threshold When, the acoustic emission event is determined to be a valid damage acoustic emission event; when Less than If an event is deemed invalid, it is classified as either a suspected noise event or an invalid event. Suspected noise events can be directly discarded or assigned a lower weight for subsequent calculations. Clearly invalid events are assigned a weight of 0.

[0028] Furthermore, the effective acoustic emission energy increment can be obtained in the following way: The fatigue life process is divided into several cyclic windows. Each cyclic window may contain a single fatigue cycle or several consecutive fatigue cycles. For cases with low acoustic emission event density or long fatigue life, a sliding window approach is preferred to improve energy sequence stability.

[0029] For the For each fatigue cycle window, calculate the effective acoustic emission energy increment within that window: in, For the first The energy of an acoustic emission event can be obtained from the output of the acoustic emission system or from the integral of the square of the amplitude of the original waveform. For the first The validity weights of each event; the summation range is those belonging to the first event. All acoustic emission events within a fatigue cycle window.

[0030] Event weight Validity can be scored Determined. For example, when hour, Take 1; when hour, Setting it to 0; alternatively, a continuous weighting method can be used: in, This represents the maximum validity score for acoustic emission events within the current test or window. Using continuous weights helps avoid the erroneous deletion of valid events due to a single threshold.

[0031] According to each loop window The cumulative effective acoustic emission energy can be further obtained: in, From fatigue to the first The window number of the looping window.

[0032] In this embodiment, the hysteresis energy increment is determined by the following method: Based on the load-displacement data collected by the fatigue testing machine, the load-displacement closed curve for each fatigue cycle is extracted. The hysteresis energy of a single cycle can be expressed as: in, For fatigue load, For displacement, The fatigue cycles are numbered. For discrete sampled data, the area enclosed by the load-displacement curves can be calculated using the trapezoidal integral method.

[0033] For the For each fatigue cycle window, calculate the hysteresis energy increment within that window: in, Belongs to the A fatigue cycle window. The average hysteresis energy within this window can also be used as the window hysteresis energy index.

[0034] To eliminate the influence of different specimen sizes, load levels, stress levels, and structural forms on the energy dimensions, the effective acoustic emission energy increment and hysteresis energy increment were normalized respectively: in, and These are reference values ​​for acoustic emission energy and hysteresis energy, respectively. The reference values ​​can be the average value during the initial stable fatigue phase, the maximum value over the entire lifespan, or the average value within a preset calibration range. and These are the normalized effective acoustic emission energy increment and the normalized hysteresis energy increment, respectively.

[0035] In some embodiments of the present invention, the stable fatigue cycle interval is determined based on at least one of the following indicators: hysteresis energy, displacement amplitude, stiffness change rate, or effective acoustic emission energy growth rate.

[0036] The stable fatigue cycle interval is determined based on hysteresis energy, displacement amplitude, stiffness change rate, effective acoustic emission energy growth rate, or a combination thereof. The stable fatigue cycle interval typically lies after the initial rapid adjustment phase of fatigue and before the instability propagation phase, and can be determined using the aforementioned indicators. Within this interval, fatigue damage in composite materials primarily accumulates steadily, and there is a relatively stable synchronous relationship between the increment of hysteresis energy and the increment of effective acoustic emission energy.

[0037] In some embodiments of the present invention, the benchmark consistency relationship is represented by a linear model, a multinomial model, an exponential model, a power function model, or a nonparametric regression model.

[0038] In a preferred embodiment, a linear benchmark consistency relationship is employed:

[0039] in, The baseline effective acoustic emission energy is predicted based on hysteresis energy, and α and β are parameters obtained by fitting data from the stable fatigue cycle interval.

[0040] In another implementation, considering the effect of the normalized number of fatigue life cycles, the following baseline relationship is adopted: in, For the first The normalized loop number corresponding to each loop window This is a constant term.

[0041] In another implementation, a nonlinear reference relationship is used: in, This is the mapping function obtained by calibration from stable fatigue cycle interval data.

[0042] In some embodiments of the present invention, the step of comparing the comparative residual with the benchmark residual value within the stable fatigue cycle interval to determine the damage state includes: In this embodiment, for any cycle window after the stable fatigue cycle interval, the reference effective acoustic emission energy is calculated based on the established reference consistency relationship. and the actual normalized effective acoustic emission energy increment and By comparison, the contrast residuals are obtained: The relative residual form can also be used: in, To prevent extremely small positive numbers with a denominator of zero.

[0043] when or When the residual mean is compared to the near-steady-state phase, it indicates that the effective acoustic emission energy and hysteresis energy maintain a baseline consistency, and fatigue damage is in a stable accumulation state; when or When the acoustic emission damage activity increases continuously and exceeds the statistical threshold of the stable stage, it indicates that the acoustic emission damage activity is abnormally enhanced relative to the mechanical energy consumption, suggesting that the internal damage has entered an accelerated expansion stage or is approaching the unstable failure stage.

[0044] Further, the step of comparing the comparative residual with the benchmark residual value within the stable fatigue cycle interval to determine the damage state includes: The residual threshold is determined based on the mean and standard deviation of the multiple benchmark residual values; When the comparison residuals of multiple consecutive cycle windows exceed the residual threshold, it is determined that the fatigue damage of the composite material has entered the accelerated expansion stage from the stable accumulation stage. When the comparison residuals of multiple consecutive cycle windows exceed the residual threshold and the rate of change continues to increase, or when the cumulative amount of the comparison residuals exceeds the preset instability threshold, it is determined that the structure has entered the near-instability failure stage and outputs a fatigue damage warning signal.

[0045] The fatigue damage stage of composite materials can be determined by comparing the changing trend of residuals, continuous exceeding of limits, sudden changes in slope, or cumulative growth.

[0046] Specifically, first, the mean residual value within the stable fatigue cycle interval is calculated. and standard deviation Set the residual threshold: in, This is the threshold coefficient, which can be a value between 2 and 5 depending on the required early warning sensitivity.

[0047] In subsequent loop windows or continuous m The number of windows exceeded the threshold. At that time, it was determined that the fatigue damage of the composite material had entered the accelerated propagation stage from the stable accumulation stage. Among them, This is the number of consecutive windows, which can be an integer between 2 and 10, depending on the fatigue test data density and monitoring stability.

[0048] when or Not only did it continuously exceed the threshold And its rate of change If the residual continues to increase, or if the accumulated residual exceeds the preset instability threshold, the structure is determined to be in the stage of imminent instability and failure, and a fatigue damage warning signal is output.

[0049] Fatigue injury can be classified into the following levels: Initial adjustment or early damage stage: Hysteresis energy and effective acoustic emission energy change rapidly, but a stable and consistent relationship has not yet been established. This mainly corresponds to initial contact adjustment, gap closure, early microcrack initiation, and local damage adjustment. Stable damage accumulation stage: The increment of hysteresis energy and the increment of effective acoustic emission energy satisfy the baseline consistency relationship, and the acoustic-mechanical energy consistency residual fluctuates within the statistical threshold range. Accelerated damage propagation stage: The acoustic-mechanical energy consistency residual continuously exceeds the limit, and the effective acoustic emission energy shows an abnormal enhancement relative to the hysteresis energy, indicating enhanced internal crack propagation, interface debonding, delamination, or fiber fracture activity. Near instability failure stage: The acoustic-mechanical energy consistency residual increases rapidly, the residual change rate continues to rise, and is accompanied by significant changes in hysteresis energy, displacement amplitude, or stiffness degradation, outputting an instability warning signal.

[0050] This invention provides a composite material fatigue damage early warning device. The device can be implemented via software, hardware, or a combination of both. From a hardware perspective, a hardware architecture diagram of the electronic device housing the composite material fatigue damage early warning device provided in this invention includes, in addition to a processor, memory, network interface, and non-volatile memory, other hardware such as a forwarding chip responsible for processing messages. Taking software implementation as an example, as a logical device, it is formed by the CPU of the electronic device reading the corresponding computer program from the non-volatile memory into memory and running it. The composite material fatigue damage early warning device provided in this embodiment includes: The incremental calculation module is used to divide the fatigue life process into multiple cyclic windows, calculate the effective acoustic emission energy increment in each cyclic window, and calculate the hysteresis energy increment in each cyclic window; wherein, each cyclic window includes at least one fatigue cycle, and one fatigue cycle corresponds to the fatigue load signal changing periodically once; The benchmark establishment module is used to normalize the effective acoustic emission energy increment and the hysteresis energy increment respectively to obtain the normalized effective acoustic emission energy increment and the normalized hysteresis energy increment, and to establish a benchmark consistency relationship between the normalized hysteresis energy increment and the benchmark effective acoustic emission energy. The benchmark residual module is used to perform the following for each cycle window within a predetermined stable fatigue cycle range: calculate the benchmark effective acoustic emission energy using the benchmark consistency relationship and the normalized hysteresis energy increment, and compare the benchmark effective acoustic emission energy with the normalized effective acoustic emission energy increment to obtain the benchmark residual value; The comparison residual module is used to calculate the benchmark effective acoustic emission energy based on the benchmark consistency relationship and the normalized hysteresis energy increment in any cycle window after the stable fatigue cycle interval, and compare the normalized effective acoustic emission energy increment in the cycle window with the benchmark effective acoustic emission energy to obtain the comparison residual; The early warning module is used to compare the comparison residual with the benchmark residual value within the stable fatigue cycle interval to determine the damage state.

[0051] This invention can be applied to unidirectional composite materials, plain-weave composite materials, three-dimensional woven composite materials, open-cell composite material structures, mechanically connected composite material structures, and complex composite material load-bearing structures. For cases requiring spatial or mechanistic verification, the damage stage identified by the acoustic-mechanical energy consistency residual can be verified by combining digital image correlation, fiber optic strain monitoring, infrared thermography, ultrasonic testing, microscopic observation, or CT scan results. However, the aforementioned additional detection methods are not necessary conditions for implementing this invention.

[0052] It is understood that the structures illustrated in the embodiments of the present invention do not constitute a specific limitation on a composite material fatigue damage early warning device. In other embodiments of the present invention, a composite material fatigue damage early warning device may include more or fewer components than illustrated, or combine some components, or split some components, or have different component arrangements. The illustrated components may be implemented in hardware, software, or a combination of software and hardware.

[0053] The information interaction and execution process between the modules in the above-mentioned device are based on the same concept as the method embodiment of the present invention, and the specific details can be found in the description of the method embodiment of the present invention, and will not be repeated here.

[0054] This invention also provides an electronic device, including a memory and a processor. The memory stores a computer program, and when the processor executes the computer program, it implements a composite material fatigue damage early warning method according to any embodiment of this invention.

[0055] This invention also provides a computer-readable storage medium storing a computer program, which, when executed by a processor, causes the processor to perform a composite material fatigue damage early warning method according to any embodiment of this invention.

[0056] Specifically, a system or apparatus equipped with a storage medium may be provided, on which software program code implementing the functions of any of the embodiments described above is stored, and the computer (or CPU or MPU) of the system or apparatus may read and execute the program code stored in the storage medium.

[0057] In this case, the program code read from the storage medium can itself implement the function of any of the above embodiments, and therefore the program code and the storage medium storing the program code constitute part of the present invention.

[0058] Storage media embodiments for providing program code include floppy disks, hard disks, magneto-optical disks, optical disks (such as CD-ROM, CD-R, CD-RW, DVD-ROM, DVD-RAM, DVD-RW, DVD+RW), magnetic tapes, non-volatile memory cards, and ROMs. Alternatively, program code can be downloaded from a server computer via a communication network.

[0059] Furthermore, it should be clear that not only can the program code read by the computer be executed, but also the operating system or other components operating on the computer can be instructed based on the program code to perform some or all of the actual operations, thereby realizing the function of any of the embodiments described above.

[0060] Furthermore, it is understood that the program code read from the storage medium is written to the memory set in the expansion board inserted into the computer or to the memory set in the expansion module connected to the computer. Then, based on the instructions of the program code, the CPU or other components installed on the expansion board or expansion module execute some and all of the actual operations, thereby realizing the function of any of the above embodiments.

[0061] It should be noted that, in this document, relational terms such as "first" and "second" are used only to distinguish one entity or operation from another, and do not necessarily require or imply any such actual relationship or order between these entities or operations. Furthermore, the terms "comprising," "including," or any other variations thereof are intended to cover non-exclusive inclusion, such that a process, method, article, or apparatus that comprises a list of elements includes not only those elements but also other elements not expressly listed, or elements inherent to such a process, method, article, or apparatus. Without further limitations, an element defined by the phrase "comprising one..." does not exclude the presence of other identical elements in the process, method, article, or apparatus that includes said element.

[0062] Those skilled in the art will understand that all or part of the steps of the above method embodiments can be implemented by hardware related to program instructions. The aforementioned program can be stored in a computer-readable storage medium. When the program is executed, it performs the steps of the above method embodiments. The aforementioned storage medium includes various media that can store program code, such as ROM, RAM, magnetic disk, or optical disk.

[0063] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the present invention, and not to limit them; although the present invention has been described in detail with reference to the foregoing embodiments, those skilled in the art should understand that modifications can still be made to the technical solutions described in the foregoing embodiments, or equivalent substitutions can be made to some of the technical features; and these modifications or substitutions do not cause the essence of the corresponding technical solutions to deviate from the spirit and scope of the technical solutions of the embodiments of the present invention.

Claims

1. A method for early warning of fatigue damage in composite materials, characterized in that, include: The fatigue life process is divided into multiple cyclic windows. The effective acoustic emission energy increment and hysteresis energy increment within each cyclic window are calculated. Each cyclic window includes at least one fatigue cycle, and one fatigue cycle corresponds to a periodic change in the fatigue load signal. The effective acoustic emission energy increment and the hysteresis energy increment are normalized respectively to obtain the normalized effective acoustic emission energy increment and the normalized hysteresis energy increment, and a benchmark consistency relationship is established between the normalized hysteresis energy increment and the benchmark effective acoustic emission energy. Within a predetermined stable fatigue cycle interval, each cycle window performs the following: calculating the baseline effective acoustic emission energy using the baseline consistency relationship and the normalized hysteresis energy increment, and comparing the baseline effective acoustic emission energy with the normalized effective acoustic emission energy increment to obtain the baseline residual value; In any cycle window after the stable fatigue cycle interval, the reference effective acoustic emission energy is calculated based on the reference consistency relationship and the normalized hysteresis energy increment, and the normalized effective acoustic emission energy increment in the cycle window is compared with the reference effective acoustic emission energy to obtain the comparison residual; The damage state is determined by comparing the comparative residual with the baseline residual value within the stable fatigue cycle interval. The calculation of the effective acoustic emission energy increment within each cyclic window includes: Based on the validity criteria extracted from the original acoustic emission waveform, a validity score is established for each acoustic emission event; The weight of the acoustic emission event is determined based on the validity score, and the effective acoustic emission energy increment is calculated based on the weight of the acoustic emission event and the energy of the acoustic emission event. The validity discrimination index includes at least one of the following: time domain index, frequency domain index, time-frequency domain index, multi-channel consistency index, cyclic phase rationality index, and signal-to-noise ratio index.

2. The method for early warning of fatigue damage in composite materials according to claim 1, characterized in that, Before calculating the effective acoustic emission energy increment within each cyclic window, the method further includes: Acoustic emission events obtained during composite material fatigue testing are synchronously assigned to fatigue cycles, so that each acoustic emission event is assigned to a corresponding fatigue cycle number; wherein, the fatigue cycle number corresponds to the number of periodic changes in the fatigue load signal.

3. The method for early warning of fatigue damage in composite materials according to claim 1, characterized in that, The stable fatigue cycle range is determined based on at least one of the following indicators: hysteresis energy, displacement amplitude, stiffness change rate, or effective acoustic emission energy growth rate.

4. The method for early warning of fatigue damage in composite materials according to claim 1, characterized in that, The benchmark consistency relationship can be represented by a linear model, a multinomial model, an exponential model, a power function model, or a nonparametric regression model.

5. The method for early warning of fatigue damage in composite materials according to claim 1, characterized in that, The step of comparing the comparative residual with the benchmark residual value within the stable fatigue cycle interval to determine the damage state includes: The residual threshold is determined based on the mean and standard deviation of the multiple benchmark residual values; When the comparison residuals of multiple consecutive cycle windows exceed the residual threshold, it is determined that the fatigue damage of the composite material has entered the accelerated expansion stage from the stable accumulation stage. When the comparison residuals of multiple consecutive cycle windows exceed the residual threshold and the rate of change continues to increase, or when the cumulative amount of the comparison residuals exceeds the preset instability threshold, it is determined that the structure has entered the near-instability failure stage and outputs a fatigue damage warning signal.

6. A fatigue damage early warning device for composite materials, characterized in that, The apparatus for implementing the method as described in any one of claims 1-5 comprises: The incremental calculation module is used to divide the fatigue life process into multiple cyclic windows, calculate the effective acoustic emission energy increment in each cyclic window, and calculate the hysteresis energy increment in each cyclic window; wherein, each cyclic window includes at least one fatigue cycle, and one fatigue cycle corresponds to the fatigue load signal changing periodically once; The benchmark establishment module is used to normalize the effective acoustic emission energy increment and the hysteresis energy increment respectively to obtain the normalized effective acoustic emission energy increment and the normalized hysteresis energy increment, and to establish a benchmark consistency relationship between the normalized hysteresis energy increment and the benchmark effective acoustic emission energy. The benchmark residual module is used to perform the following for each cycle window within a predetermined stable fatigue cycle range: calculate the benchmark effective acoustic emission energy using the benchmark consistency relationship and the normalized hysteresis energy increment, and compare the benchmark effective acoustic emission energy with the normalized effective acoustic emission energy increment to obtain the benchmark residual value; The comparison residual module is used to calculate the benchmark effective acoustic emission energy based on the benchmark consistency relationship and the normalized hysteresis energy increment in any cycle window after the stable fatigue cycle interval, and compare the normalized effective acoustic emission energy increment in the cycle window with the benchmark effective acoustic emission energy to obtain the comparison residual; The early warning module is used to compare the comparison residual with the benchmark residual value within the stable fatigue cycle interval to determine the damage state.

7. An electronic device comprising a memory and a processor, wherein the memory stores a computer program, and the processor, when executing the computer program, implements the method as described in any one of claims 1-5.

8. A computer-readable storage medium having a computer program stored thereon, which, when executed in a computer, causes the computer to perform the method of any one of claims 1-5.

Citation Information

Patent Citations

  • Metallic material fatigue loading testing and fatigue damage nondestructive testing analytical method

    CN104634879A

  • Tire abnormal state early warning method and system based on multi-sensor fusion

    CN121848866A