A method and apparatus for controlling the heat-affected zone in laser processing based on instantaneous liquid film jet-suction switching

By switching between instantaneous liquid film injection and negative pressure suction, a liquid film is formed and removed during laser processing, which solves the problems of low cooling efficiency and poor processing quality in laser processing. It achieves a balance between high-efficiency cooling and dry processing, and is suitable for high-repetition-rate continuous processing.

CN123060296APending Publication Date: 2026-11-10HENAN ACADEMY OF SCIENCES
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611532722.0
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-09-30
Publication Date
2026-11-10

AI Technical Summary

Technical Problem

Existing laser processing technologies suffer from problems such as low cooling efficiency, light path scattering and energy attenuation, molten pool interference, and waste liquid residue in controlling the heat-affected zone. In particular, it is difficult to balance efficient cooling and dry processing quality in high-repetition-rate continuous processing.

Method used

By employing a method of switching between instantaneous liquid film injection and negative pressure suction, a cooling liquid film is formed in front of the pulsed laser and immediately suctioned after the laser, ensuring that the liquid film exists briefly during the processing cycle. The control device sprays the cooling medium to form a liquid film before the laser is emitted and generates negative pressure after the laser to remove the medium and byproducts, avoiding interference from the continuous existence of the liquid film.

Benefits of technology

It achieves a balance between efficient cooling and dry machining quality, is suitable for high-repetition-rate continuous machining, reduces light path scattering, energy attenuation and waste liquid residue, and improves machining quality.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123060296A_ABST
    Figure CN123060296A_ABST
Patent Text Reader

Abstract

This invention belongs to the field of laser precision machining technology, and particularly relates to a method for controlling the heat-affected zone (HAZ) in laser machining based on instantaneous liquid film spray-absorption switching. The method includes: within a first time window before pulsed laser emission, a cooling medium is sprayed onto the workpiece to be processed via a control device to form a cooling liquid film, with the pulsed laser focus located in the center region of the liquid film; the pulsed laser focus passes through the cooling liquid film to process the workpiece to be processed; within a second time window after the pulsed laser processing ends, the control device stops spraying and generates negative pressure to extract the cooling medium and processing byproducts from the workpiece surface; the workpiece surface is kept dry during the processing waiting period; wherein the first and second time windows do not overlap with the pulsed laser processing time, and their sum is less than a single processing cycle. This invention balances efficient cooling with dry machining quality.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention belongs to the field of laser precision machining technology, and particularly relates to a method and device for controlling the heat-affected zone of laser machining based on instantaneous liquid film jet-suction switching. Background Technology

[0002] Laser processing, due to its non-contact, high efficiency, and high precision characteristics, is widely used in fields such as microelectronics, aerospace, and precision medical devices. However, the large amount of heat generated during laser processing diffuses into the substrate material, forming a heat-affected zone (HAZ). This leads to changes in the material's microstructure, increased residual stress, and the initiation of microcracks, affecting processing quality. Therefore, effectively controlling the width of the HAZ is a key technical problem that urgently needs to be solved in the field of laser precision machining.

[0003] Existing heat-affected zone (HAZ) control technologies mainly include dry gas-assisted machining and continuous liquid cooling machining. Dry gas-assisted machining uses compressed air or inert gas to purge and cool the machining area. However, the low specific heat capacity of the gas limits the cooling efficiency, resulting in a typically large HAZ width. Continuous liquid cooling machining utilizes the high specific heat capacity and latent heat of vaporization of liquids to improve cooling efficiency. However, the continuous presence of liquid in the machining area causes light scattering and energy attenuation, interferes with the stability of the molten pool, and leaves waste liquid residue after machining. Liquid-assisted methods such as water-guided lasers also suffer from problems such as laser transmission and cooling coupling constraints, heat backflow, and bubble interference. Existing laser and liquid timing control schemes are mostly designed for single pre-cooling scenarios and fail to periodically switch between liquid film jetting and negative pressure suction within the laser pulse interval. They also cannot actively remove the heated liquid and machining byproducts from the workpiece surface after the pulse ends, making it difficult to balance efficient cooling with dry machining quality, and are particularly unsuitable for high-repetition-rate continuous machining. Summary of the Invention

[0004] The purpose of this invention is to provide a method and apparatus for controlling the heat-affected zone in laser processing based on instantaneous liquid film jet-suction switching, so as to solve the above-mentioned problems.

[0005] To achieve the above objectives, the present invention provides the following solution: A method for controlling the heat-affected zone in laser processing based on instantaneous liquid film jet-suction switching, comprising the following steps: Within the first time window before the pulsed laser is emitted, a cooling medium is sprayed onto the workpiece to be processed area by a control device and the cooling medium forms a cooling liquid film. The focus of the pulsed laser is located in the central region of the liquid film. The focal point of the pulsed laser passes through the coolant film to process the area of ​​the workpiece to be processed; During the second time window after the pulsed laser processing ends, the control device stops spraying the cooling medium and generates negative pressure to remove the cooling medium and processing byproducts from the workpiece surface. During the processing waiting period, keep the surface of the workpiece dry; There is no overlap between the first time window, the second time window, and the pulsed laser processing time, and the sum of the first time window, the second time window, and the pulsed laser processing time is less than the time of a single processing cycle.

[0006] In operation, within the first time window before the pulsed laser emission, a cooling medium is sprayed onto the workpiece's processing area via a control device, forming a coolant film. The focus of the pulsed laser is located in the center of this coolant film. The laser beam passes through the coolant film to process the workpiece's processing area. Within the second time window after the pulsed laser processing ends, the control device stops spraying the cooling medium and generates negative pressure to remove the cooling medium and processing byproducts from the workpiece surface. During the processing wait period, the workpiece surface remains dry. The first and second time windows, as well as the pulsed laser processing time, do not overlap, and their total duration is less than the time of a single processing cycle. This timing control ensures the coolant film exists only briefly before and after the pulse, balancing efficient cooling with high-quality dry processing.

[0007] Preferably, the first time window is 0.5ms to 5ms, the second time window is 0.05ms to 3ms, and there is a lag time window between the second time window and the end time of pulsed laser processing, which is less than the critical time for solidification of the workpiece molten pool.

[0008] A coolant film is formed within 0.5ms to 5ms before the pulsed laser emission. After the pulse ends, suction is not initiated immediately, but rather after a lag window shorter than the critical solidification time of the molten pool, followed by a second time window of 0.05ms to 3ms. This ensures that the heated cooling medium and byproducts are removed before the molten pool completely solidifies, cutting off the path of heat conduction to the matrix and improving the control effect of the heat-affected zone.

[0009] Preferably, the Reynolds number Re of the coolant film is less than 2300, the thickness of the coolant film is 0.05 mm to 0.5 mm, and the surface fluctuation of the coolant film is less than 10% of the average thickness of the coolant film.

[0010] The cooling medium forms a stable laminar flow coolant film in the workpiece's processing area, with the film thickness and surface fluctuations limited within a set range. This ensures that the coolant film stably surrounds the laser focus when the laser beam penetrates it, reducing light scattering and energy attenuation, and preventing film rupture or fluctuations that could degrade processing quality.

[0011] Preferably, the critical time for solidification of the workpiece molten pool is determined by the following formula: t critical =k·(L² / α) Among them, t criticalThis refers to the critical time for the solidification of the workpiece's molten pool. k is a geometric factor, and the value of k ranges from 0.5 to 2.0; α is the thermal diffusivity; L is the size of the molten pool.

[0012] Based on the thermal diffusivity α of the workpiece material and the characteristic size L of the molten pool, the critical solidification time of the molten pool is calculated in conjunction with the geometric factor k, and the lag time window of the second time window is determined accordingly. This provides a quantitative basis for the suction lag time, enabling the control method to be adapted to different materials and improving the consistency of heat-affected zone control.

[0013] A laser processing heat-affected zone control device based on instantaneous liquid film spray-suction switching, used to implement the aforementioned control method, includes: a fixed plate, fixedly installed below the laser processing head; a sleeve coaxially fixed to the bottom surface of the fixed plate, the sleeve penetrating the fixed plate; an inner ring body coaxially sleeved on the outer side of the sleeve; an annular water cavity circumferentially formed within the inner ring body; a nozzle circumferentially arranged at the bottom end of the annular water cavity; an outer ring body circumferentially arranged on the outer side of the inner ring body; a cavity between the outer ring body and the inner ring body; both the inner and outer ring bodies are fixedly connected to the fixed plate; the lower diameter of the outer ring body is gradually reduced; a slit is left between the bottom end of the outer ring body and the sleeve; a cooling medium forms a cooling liquid film in the workpiece's processing area through the slit; a water inlet pipe is connected to the annular water cavity; and a suction pipe is connected to the cavity.

[0014] The cooling medium enters the annular water chamber through the inlet pipe and is sprayed out by the nozzle, forming a coolant film on the workpiece surface through a slit. Negative pressure is generated in the cavity through the suction pipe, drawing the cooling medium and byproducts away from the slit. This achieves coaxial integration of spraying and suction, forming an instantaneous liquid film and actively peeling it off.

[0015] Preferably, the nozzle is made of microporous sintered metal or porous ceramic structure, and the nozzle orifice diameter is 50μm~100μm.

[0016] The cooling medium is ejected through the microporous structure of the nozzle, forming a coolant film in the workpiece's processing area. The microporous structure helps generate a stable laminar liquid film, reduces film fluctuations, and improves the uniformity of film coverage.

[0017] Preferably, the width of the cavity is 0.5mm-2mm.

[0018] The cavity width between the outer and inner rings is limited to 0.5mm-2mm. During negative pressure suction, the gas-liquid mixture enters the suction tube through this cavity. Properly controlling the suction channel size ensures efficient negative pressure suction and prevents insufficient suction due to an excessively wide channel or blockage due to an excessively narrow channel.

[0019] Preferably, the angle between the lower part of the outer ring and the workpiece is 15° to 45°.

[0020] The lower part of the outer ring tapers and forms an angle of 15° to 45° relative to the workpiece surface, creating a directional suction flow field on the workpiece surface during negative pressure suction. Optimizing the suction angle improves the extraction efficiency of cooling medium and processing byproducts, reducing residue.

[0021] Preferably, the ratio of the inner diameter of the sleeve to the thickness of the coolant film is 5:1 to 20:1.

[0022] The laser beam passes through the inner hole of the sleeve and through the coolant film to process the workpiece. Ensuring the laser transmission through-hole matches the thickness of the coolant film allows the coolant film to stably envelop the laser focus without obstructing the effective processing optical path, thus controlling laser energy attenuation.

[0023] Preferably, the width of the slit is 0.5mm-2mm.

[0024] The cooling medium is ejected from the inner ring through the nozzle and forms a coolant film in the workpiece's processing area through the slit between the bottom of the outer ring and the sleeve. The width and thickness of the coolant film formation area are controlled to ensure a stable distribution of the coolant film around the laser focus.

[0025] Compared with the prior art, the present invention has the following advantages and technical effects: This invention utilizes a cooling medium to form a coolant film within a first time window before pulsed laser emission. The pulsed laser focus passes through this film to process the workpiece area, absorbing the heat generated during processing. Within a second time window after pulsed laser processing, the spraying stops and negative pressure is generated to remove the cooling medium and processing byproducts from the workpiece surface. The workpiece surface remains dry during the processing wait period. The first and second time windows do not overlap with the pulsed laser processing time, and their combined duration is less than a single processing cycle. Therefore, this invention improves cooling efficiency using a liquid medium while avoiding light scattering, energy attenuation, molten pool interference, and waste liquid residue caused by continuous liquid presence. It also actively removes processing byproducts, achieving both high-efficiency cooling and dry processing quality, making it suitable for high-repetition-rate continuous processing. Attached Figure Description

[0026] To more clearly illustrate the technical solutions in the embodiments of the present invention or the prior art, the drawings used in the embodiments will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For those skilled in the art, other drawings can be obtained based on these drawings without creative effort: Figure 1 This is a schematic diagram of the overall structure of the device in this invention; Figure 2This is a system connection diagram of the present invention; The components are: 1. Laser processing head; 2. Pulsed laser; 3. Workpiece; 4. Coolant film; 5. Water inlet pipe; 6. Suction pipe; 7. Outer ring body; 8. Inner ring body; 9. Nozzle; 10. Sleeve; 11. Fixing plate. Detailed Implementation

[0027] The technical solutions of the embodiments of the present invention will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only some embodiments of the present invention, and not all embodiments. Based on the embodiments of the present invention, all other embodiments obtained by those skilled in the art without creative effort are within the scope of protection of the present invention.

[0028] To make the above-mentioned objects, features and advantages of the present invention more apparent and understandable, the present invention will be further described in detail below with reference to the accompanying drawings and specific embodiments.

[0029] Reference Figures 1 to 2 This invention discloses a method for controlling the heat-affected zone in laser processing based on instantaneous liquid film jet-suction switching, the steps of which are as follows: Within the first time window before the pulsed laser is emitted, a cooling medium is sprayed onto the workpiece to be processed area by a control device and the cooling medium forms a cooling liquid film. The focus of the pulsed laser is located in the central region of the liquid film. The focal point of the pulsed laser passes through the coolant film to process the area of ​​the workpiece to be processed; During the second time window after the pulsed laser processing ends, the control device stops spraying the cooling medium and generates negative pressure to remove the cooling medium and processing byproducts from the workpiece surface. During the processing waiting period, keep the surface of the workpiece dry; There is no overlap between the first time window, the second time window, and the pulsed laser processing time, and the sum of the first time window, the second time window, and the pulsed laser processing time is less than the time of a single processing cycle.

[0030] The scheme was further optimized. The first time window is 0.5ms to 5ms, the second time window is 0.05ms to 3ms, and there is a lag time window between the second time window and the end time of pulsed laser processing. The lag time window is smaller than the critical time for solidification of the workpiece molten pool.

[0031] Specifically, when the workpiece 3 is made of brittle materials such as glass, quartz, or sapphire, the cooling medium is a low surface tension fluorinated liquid with a surface tension not exceeding 15 mN / m, a liquid film thickness of 0.05 mm to 0.1 mm, a first time window of 0.5 ms to 1 ms, a second time window of 0.05 ms to 0.1 ms, a negative pressure suction flow rate of 10 m / s to 15 m / s, and a critical solidification time of the molten pool of 0.01 ms to 1 ms.

[0032] When the material of workpiece 3 is metallic, the first time window is 1ms to 5ms; the second time window is 0.5ms to 3ms; and the critical time for solidification of the molten pool is 0.05ms to 5ms.

[0033] Further optimization of the scheme resulted in a Reynolds number Re < 2300 for the coolant film, a coolant film thickness of 0.05 mm to 0.5 mm, and a surface fluctuation amplitude of the coolant film of less than 10% of the average thickness of the coolant film.

[0034] The critical time for solidification of the workpiece molten pool is determined by the following formula for further optimization: t critical =k·(L² / α) Among them, t critical This refers to the critical time for the solidification of the workpiece's molten pool. k is a geometric factor, and the value of k ranges from 0.5 to 2.0; α is the thermal diffusivity; L is the size of the molten pool.

[0035] A laser processing heat-affected zone control device based on instantaneous liquid film spray-suction switching, used to implement the above-mentioned control method, includes: a fixed plate 11, fixedly installed below the laser processing head 1, a sleeve 10 coaxially fixed to the bottom surface of the fixed plate 11, the sleeve 10 penetrating the fixed plate 11, an inner ring body 8 coaxially sleeved on the outer side of the sleeve 10, an annular water cavity is opened in the inner circumferential direction of the inner ring body 8, a nozzle 9 is arranged in the bottom circumferential direction of the annular water cavity, an outer ring body 7 is arranged in the outer circumferential direction of the inner ring body 8, a cavity is left between the outer ring body 7 and the inner ring body 8, both the inner ring body 8 and the outer ring body 7 are fixedly connected to the fixed plate 11, the lower diameter of the outer ring body 7 is gradually reduced, a slit is left between the bottom end of the outer ring body 7 and the sleeve 10, the cooling medium forms a cooling liquid film 4 in the processing area of ​​the workpiece 3 through the slit, the annular water cavity is connected to a water inlet pipe 5, and the cavity is connected to a suction pipe 6.

[0036] Further optimization of the design involves using microporous sintered metal or porous ceramic materials for the nozzle 9, with nozzle orifice diameters ranging from 50μm to 100μm.

[0037] The design was further optimized so that the cavity width was 0.5mm-2mm.

[0038] Further optimization of the design resulted in an angle of 15° to 45° between the lower part of the outer ring 7 and the workpiece 3.

[0039] The scheme was further optimized so that the ratio of the inner diameter of the sleeve 10 to the thickness of the coolant film 4 was 5:1 to 20:1.

[0040] The design was further optimized so that the slit width was 0.5mm-2mm.

[0041] The control device of this invention further includes a high-speed fluid switching module, a synchronous control system, a fluid circulation processing unit, and an optical detection module. The high-speed fluid switching module connects the annular water chamber and the cavity via an inlet pipe 5 and a suction pipe 6, and includes a high-pressure precision pump, a high-frequency response solenoid valve with a response time of less than 0.5 ms, and a vacuum negative pressure generator. The synchronous control system's signal input is connected to the laser's pulse trigger signal, and its output is connected to the high-speed fluid switching module. It is used to adjust the timing of the jetting and suction actions in real time according to the laser pulse phase. The synchronous control system also includes a feedback input connected to the output of the optical detection module, forming a closed-loop control loop of liquid film morphology and jet pressure. The synchronous control system uses an FPGA or DSP controller with a pre-set timing mapping table. It can dynamically adjust the duration of the first and second time windows according to the laser pulse frequency and the thermal diffusivity of the workpiece material; the fluid circulation processing unit is connected to the outlet of the outer suction channel and is used to separate, filter and cool the recovered gas-liquid mixture at a constant temperature. Its coolant outlet is connected to the liquid inlet of the high-speed fluid switching module to form a recycling loop for the cooling medium; the optical detection module is used to acquire images of the liquid film morphology in the processing area in real time and transmit feedback signals to the synchronous control system to dynamically correct the injection pressure. The optical detection module includes a high-speed camera unit and an image processing unit. The frame rate of the high-speed camera unit is not less than 10,000 fps and is used to capture liquid film thickness fluctuations and rupture behavior; the output of the image processing unit is connected to the feedback input of the synchronous control system.

[0042] During operation, within the first time window before the pulsed laser emission, the synchronous control system controls the high-speed fluid switching module to supply cooling medium to the annular water cavity through the inlet pipe 5, based on the laser's pulse trigger signal. The cooling medium is ejected from the nozzle 9 at the bottom of the annular water cavity and forms a coolant film 4 in the workpiece 3's processing area through the slit between the bottom of the outer ring 7 and the sleeve 10. The focus of the pulsed laser is located in the central region of the coolant film 4. Subsequently, the focus of the pulsed laser passes through the coolant film 4 to process the workpiece 3's processing area, and the coolant film 4 absorbs the overflow heat generated during processing. Within the second time window after the pulsed laser processing ends, the synchronous control system controls the high-speed fluid switching module to stop spraying cooling medium and generates negative pressure through a vacuum negative pressure generator. The cooling medium and processing byproducts are extracted from the surface of workpiece 3 through the cavity and suction pipe 6. During the processing waiting period, the surface of workpiece 3 is kept dry, and there is no overlap between the first time window, the second time window, and the pulsed laser processing time. The sum of the three is less than the time of a single processing cycle. The gas-liquid mixture discharged from suction pipe 6 enters the fluid circulation processing unit. After separation, filtration, and constant temperature cooling, its coolant outlet returns to the liquid inlet of the high-speed fluid switching module, forming a recycling of the cooling medium. At the same time, the optical detection module acquires the morphological image of the coolant film 4 in real time and transmits the feedback signal to the feedback input terminal of the synchronous control system. The synchronous control system dynamically corrects the injection pressure accordingly, forming a closed-loop control loop of liquid film morphology and injection pressure.

[0043] Specific example one, such as Figure 1 As shown, the device of the present invention is installed below the laser processing head 1. The nozzle 9 of the inner ring body 8 is a porous stainless steel sintered ring with an aperture of 80 μm and a slit width of 1.5 mm. The cavity width between the inner ring body 8 and the outer ring body 7 is 1.0 mm. The suction port of the outer ring body 7 is tilted downward at 30° to optimize suction efficiency. The ratio of the inner diameter of the sleeve 10 to the thickness of the coolant film 4 is designed to be 10:1, ensuring that the coolant film 4 stably wraps the laser focus without obstructing the effective processing optical path. The optical design is based on the following: the refractive index of the coolant film 4 is 1.33@1064nm, the inner diameter of the sleeve 10 is 0.5 mm, and the thickness of the coolant film 4 is 0.05 mm, ensuring that the energy attenuation of the pulsed laser 2 is <3%.

[0044] The fluid system uses deionized water as the medium and is equipped with a 2MPa plunger pump and a high-speed solenoid valve with a response time of less than 0.5ms. The negative pressure source adopts a Venturi tube structure and uses compressed air to drive the generation of instantaneous high negative pressure. The control system is developed based on FPGA and directly reads the laser Q-switch signal. The timing logic is as follows: water spraying starts 2ms before the laser pulse leading edge, and suction starts 1ms after the pulse ends, lasting for 2ms.

[0045] Methods for determining the critical time for molten pool solidification Critical time t for molten pool solidificationcritical The physical meaning of is: the time window required from the end of the laser pulse to the complete solidification of the molten pool. If the suction lag time exceeds t... critical If the molten pool has solidified, the heat has been conducted to the matrix through the solid-liquid interface, and negative pressure suction cannot effectively cut off the heat conduction path.

[0046] The critical time for solidification of the molten pool is derived based on Stefan's heat conduction theory and estimated using a one-dimensional heat conduction model: t critical =k·(L² / α). Where: L is the size of the molten pool, usually 0.5 to 1.5 times the diameter of the laser spot, in meters; α is the thermal diffusivity of the workpiece material, α=k / ρ·cp in m² / s; k is a geometric factor, calibrated by high-speed imaging experiments on five materials: copper, aluminum, steel, titanium alloy, and soda-lime glass. The value of k ranges from 0.5 to 2.0. The calibration values ​​for each material are shown in Table 1.

[0047] Table 1: Reference values ​​for critical solidification time of typical material molten pool (laser power 20W, spot diameter 50μm) In practical applications, the suction lag time should be calculated as t. critical 10% to 50% is reserved to allow for a safety margin.

[0048] Specific Example 2: Copper Foil Processing Flow Taking the cutting of a 0.2mm thick copper foil as workpiece 3 as an example, the laser parameters are: wavelength 1064nm, pulse width 10ns, frequency 1kHz, and single pulse energy 0.2mJ. The synchronous controller timing is as follows: T=-2ms~0ms: the inner ring body 8's nozzle 9 sprays water, the coolant film 4 thickness is 0.3mm, Re<2300; T=0~10ns: laser emission, coolant film 4 temperature rise <80K; T=10ns~0.1ms: outer ring body 7 starts under negative pressure, water flow rate 10m / s, drawing in the heated coolant film 4; T=0.1ms~1ms: nitrogen gas is introduced for protection, waiting for the next pulse.

[0049] Results verification: Referring to GB / T13298-2015 metallographic sample preparation, the width of the heat-affected zone of the copper foil cut in this scheme is 8-15μm, with no oxidation discoloration; the HAZ of traditional dry processing is about 45μm and has a recast layer; continuous water cooling processing has edge corrosion.

[0050] Specific Example 3: Micropore Machining of Brittle Materials For brittle materials such as glass, quartz, and sapphire, a low surface tension fluorinated liquid is used, specifically 3MNovec7100 hydrofluoroether, with a boiling point of 61°C, viscosity of 0.38 cSt, and surface tension of 13.6 mN / m. Taking 0.5 mm thick soda-lime glass as workpiece 3 as an example, the laser parameters are: fourth harmonic ultraviolet, wavelength 266 nm, pulse width 10 ns, single pulse energy 0.5 mJ, and peak power density 2.6 × 10⁻⁶. 9 W / cm². Process parameters: Coolant film thickness 0.05mm~0.1mm, first time window T1=0.5ms~1ms, lag time 0.02ms~0.05ms, second time window T2=0.05ms~0.1ms, negative pressure suction flow rate 10m / s~15m / s.

[0051] Results: The hole diameter was Φ50μm, the hole wall roughness Ra<1.5μm, the microcrack depth was <5μm, and there was no edge chipping. Compared with traditional water-cooling processing with microcrack depth >20μm, crack propagation was significantly suppressed.

[0052] In the description of this invention, it should be understood that the terms "longitudinal", "lateral", "up", "down", "front", "rear", "left", "right", "vertical", "horizontal", "top", "bottom", "inner", "outer", etc., indicate the orientation or positional relationship based on the orientation or positional relationship shown in the accompanying drawings, and are only for the convenience of describing this invention, and are not intended to indicate or imply that the device or element referred to must have a specific orientation, or be constructed and operated in a specific orientation, and therefore should not be construed as a limitation of this invention.

[0053] The embodiments described above are merely preferred embodiments of the present invention and are not intended to limit the scope of the present invention. Various modifications and improvements made by those skilled in the art to the technical solutions of the present invention without departing from the spirit of the present invention should fall within the protection scope defined by the claims of the present invention.

Claims

1. A method for controlling the heat-affected zone in laser processing based on instantaneous liquid film jet-suction switching, characterized in that, The steps are as follows: Within the first time window before the pulsed laser is emitted, a cooling medium is sprayed onto the workpiece to be processed area by a control device and the cooling medium forms a cooling liquid film. The focus of the pulsed laser is located in the central region of the liquid film. The focal point of the pulsed laser passes through the coolant film to process the area of ​​the workpiece to be processed; During the second time window after the pulsed laser processing ends, the control device stops spraying the cooling medium and generates negative pressure to remove the cooling medium and processing byproducts from the workpiece surface. During the processing waiting period, keep the surface of the workpiece dry; There is no overlap between the first time window, the second time window, and the pulsed laser processing time, and the sum of the first time window, the second time window, and the pulsed laser processing time is less than the time of a single processing cycle.

2. The laser processing heat-affected zone control method based on instantaneous liquid film jet-suction switching according to claim 1, characterized in that, The first time window is 0.5ms to 5ms, the second time window is 0.05ms to 3ms, and there is a lag time window between the second time window and the end time of pulsed laser processing. The lag time window is smaller than the critical time for solidification of the workpiece molten pool.

3. The laser processing heat-affected zone control method based on instantaneous liquid film jet-suction switching according to claim 1, characterized in that, The Reynolds number Re of the coolant film is less than 2300, the thickness of the coolant film is 0.05 mm to 0.5 mm, and the surface fluctuation of the coolant film is less than 10% of the average thickness of the coolant film.

4. The laser processing heat-affected zone control method based on instantaneous liquid film jet-suction switching according to claim 1, characterized in that, The critical time for solidification of the workpiece molten pool is determined by the following formula: t critical =k·(L² / a) Among them, t critical This refers to the critical time for the solidification of the workpiece's molten pool. k is a geometric factor, and the value of k ranges from 0.5 to 2.0; α is the thermal diffusivity; L is the size of the molten pool.

5. A laser processing heat-affected zone control device based on instantaneous liquid film jet-suction switching, used to implement the control method according to any one of claims 1-4, characterized in that, include: A fixing plate (11) is fixedly installed below the laser processing head (1). A sleeve (10) is coaxially fixed to the bottom surface of the fixing plate (11). The sleeve (10) passes through the fixing plate (11). An inner ring body (8) is coaxially sleeved on the outer side of the sleeve (10). An annular water cavity is opened in the inner circumferential direction of the inner ring body (8). A nozzle (9) is arranged in the circumferential direction at the bottom end of the annular water cavity. An outer ring body (7) is arranged in the circumferential direction on the outer side of the inner ring body (8). (7) A cavity is left between the inner ring body (8) and the outer ring body (7). The inner ring body (8) and the outer ring body (7) are both fixedly connected to the fixing plate (11). The lower diameter of the outer ring body (7) is gradually reduced. A slit is left between the bottom end of the outer ring body (7) and the sleeve (10). The cooling medium forms a cooling liquid film (4) in the processing area of ​​the workpiece (3) through the slit. The annular water cavity is connected to the water inlet pipe (5). The cavity is connected to the suction pipe (6).

6. The laser processing heat-affected zone control device based on instantaneous liquid film jet-suction switching according to claim 5, characterized in that, The material of the nozzle (9) includes microporous sintered metal or porous ceramic structure, and the nozzle (9) has a nozzle diameter of 50μm~100μm.

7. The laser processing heat-affected zone control device based on instantaneous liquid film jet-suction switching according to claim 5, characterized in that, The width of the cavity is 0.5mm-2mm.

8. The laser processing heat-affected zone control device based on instantaneous liquid film jet-suction switching according to claim 5, characterized in that, The angle between the lower part of the outer ring (7) and the workpiece (3) is 15°~45°.

9. The laser processing heat-affected zone control device based on instantaneous liquid film jet-suction switching according to claim 5, characterized in that, The ratio of the inner diameter of the sleeve (10) to the thickness of the coolant film (4) is 5:1 to 20:

1.

10. A laser processing heat-affected zone control device based on instantaneous liquid film jet-suction switching according to claim 5, characterized in that, The width of the slit is 0.5mm-2mm.