A method for preparing bamboo fiber by synergistic use of microwave deep eutectic solvent and photoenzyme.
By using a microwave deep eutectic solvent and photoenzyme synergistic method, the problems of long processing cycle, heavy pollution and large loss of fiber strength in bamboo fiber preparation have been solved, realizing efficient and environmentally friendly bamboo fiber preparation.
Patent Information
- Application Number
- CN202611424796.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-09-15
- Publication Date
- 2026-11-10
AI Technical Summary
Existing bamboo fiber preparation processes have long processing cycles, heavy chemical pollution, significant fiber strength loss, and poor degumming uniformity.
The method employs a combination of microwave deep eutectic solvent and photoenzyme, including steps such as low-temperature steam explosion pretreatment, microwave-assisted deep eutectic solvent delignination, photocatalysis and composite enzyme synergistic fine degumming, ultrasonic-assisted eddy current fiber separation, plant polyphenol bleaching and softening shaping.
It shortens processing time, improves degumming efficiency, reduces chemical pollution, preserves fiber strength, achieves uniform fiber separation and chlorine-free bleaching, and enhances production efficiency and environmental friendliness.
Smart Images

Figure FT_1 
Figure FT_2 
Figure FT_3
Abstract
Description
Technical Field
[0001] This invention belongs to the field of natural plant fiber extraction technology, specifically relating to a method for preparing bamboo fiber. Background Technology
[0002] Bamboo is a rapidly growing, renewable natural biomass resource. Its fibers possess excellent mechanical properties, moisture absorption, and antibacterial properties, making it promising for applications in textiles, composite materials, and papermaking. Bamboo is primarily composed of three components: cellulose, hemicellulose, and lignin. Cellulose is the target fiber component, while hemicellulose and lignin, acting as gums, need to be removed during the preparation process.
[0003] Existing methods for preparing bamboo fiber mainly fall into three categories: chemical, biological, and physical methods. Chemical methods, represented by the alkali boiling process, use high-concentration sodium hydroxide to treat bamboo at high temperatures. While this method offers high degumming efficiency, it suffers from significant fiber strength loss, severe wastewater pollution, and high treatment costs. Biological methods employ microbial fermentation or enzymes for degumming. These methods offer milder reaction conditions and less pollution, but have a long processing cycle, typically requiring dozens of days of soaking and fermentation, and the uniformity of degumming is difficult to control. Physical methods, including mechanical pressing and steam explosion, are primarily used in the pretreatment stage; their use alone is insufficient to achieve ideal degumming results.
[0004] Among the publicly available bamboo fiber preparation technologies, one approach uses a three-stage physical pressing process combined with degumming using orange enzymes and desaccharification using radish enzymes. While this method avoids the use of chemical reagents, each degumming and desaccharification step requires a soaking time of 28 to 35 days, resulting in a total preparation cycle of over two months and low production efficiency. Another approach uses a steam explosion combined with enzyme treatment, but the enzyme treatment efficiency is limited, and residual gum is not completely removed, requiring subsequent chemical bleaching.
[0005] Eutectic solvents, as a novel type of green solvent, are composed of hydrogen bond acceptors and hydrogen bond donors mixed in a certain proportion. They possess advantages such as simple preparation, low volatility, and recyclability, and have attracted attention in the field of lignocellulose component separation. Coupled with microwave radiation, eutectic solvents can shorten reaction time and improve lignin removal efficiency. The synergistic effect of photocatalysis and bioenzymes can achieve targeted degradation of residual gums under mild conditions, reducing damage to cellulose. However, a complete process for organically coupling the above technologies and applying them to the preparation of bamboo fiber has not yet been systematically reported. Summary of the Invention
[0006] Technical issues The main technical problem to be solved by this invention is that the existing bamboo fiber preparation process has a long processing cycle, heavy chemical pollution, large loss of fiber strength, and poor degumming uniformity.
[0007] Secondary technical issues include: insufficient penetration efficiency of eutectic solvents in bamboo fiber extraction; limited ability of single-enzymatic degumming to degrade lignin; and pollution from traditional chlorine bleaching that produces adsorbable organic halides. Technical solution
[0008] To solve the above-mentioned technical problems, the present invention adopts the following technical solution: A method for preparing bamboo fiber using microwave deep eutectic solvent and photoenzyme synergy includes five steps: low-temperature steam explosion pretreatment, microwave-assisted deep eutectic solvent delignination, photocatalysis and composite enzyme synergistic fine degumming, ultrasonic-assisted eddy current fiber separation, and plant polyphenol bleaching and softening shaping.
[0009] In the low-temperature steam explosion pretreatment step, bamboo strips with the bamboo green and nodes removed are placed in a steam explosion reactor, pressurized by saturated steam, and then quickly depressurized. The explosive force generated by the sudden pressure drop breaks the dense structure of the bamboo, causing the fiber bundles to separate initially, while creating channels for subsequent solvent penetration.
[0010] In the microwave-assisted eutectic solvent delignination step, expanded bamboo fibers are mixed with a ternary eutectic solvent composed of choline chloride, lactic acid, and glycerol, and heated under microwave radiation. The bulk heating effect of microwaves lowers the diffusion barrier of the eutectic solvent, promoting solvent penetration into the bamboo. The ternary eutectic solvent selectively breaks the ether bonds of the lignin-carbohydrate complex through hydrogen bonding, dissolving lignin and hemicellulose while retaining cellulose. After the reaction, lignin is separated by precipitation with water, and the eutectic solvent is recovered for recycling.
[0011] In the photocatalytic and enzymatic synergistic degumming step, the crude deligninated fiber is placed in a treatment solution containing a visible-light-responsive photocatalyst and a complex enzyme, and undergoes enzymatic hydrolysis under visible light irradiation. The photocatalyst generates reactive oxygen species upon visible light excitation, oxidizing and degrading lignin structural units; pectinase and xylanase in the complex enzyme degrade hemicellulose gums, while laccase assists in the degradation of residual lignin. The synergistic effect of photocatalysis and enzymatic hydrolysis enables efficient and targeted removal of residual gums under mild conditions, while minimizing damage to cellulose.
[0012] In the ultrasonic-assisted vortex fiber separation step, the finely degummed fibers are placed in an ultrasonic field. The ultrasonic cavitation effect is used to loosen the fiber bundles, while a high-speed vortex airflow is introduced to separate the fibers, resulting in single fibers with uniform fineness.
[0013] In the plant polyphenol bleaching and softening / setting steps, a bleaching solution containing plant polyphenols and hydrogen peroxide is used for chlorine-free bleaching. Plant polyphenols, as natural bleaching aids, work synergistically with hydrogen peroxide to achieve bleaching effects under mild conditions, avoiding contamination from adsorbable organic halides produced by chlorine-containing bleaching agents. After bleaching, the product is treated with a softener and dried for setting, yielding the finished bamboo fiber product.
[0014] In one embodiment, the steam explosion pressure is 1.2 MPa to 1.8 MPa, the temperature is 160°C to 180°C, the pressure holding time is 3 minutes to 8 minutes, and the pressure release time does not exceed 0.1 seconds.
[0015] In one embodiment, the molar ratio of choline chloride, lactic acid and glycerol in the ternary eutectic solvent is 1:(1.5 to 2.5):(0.3 to 0.8); the mass ratio of expanded bamboo filaments to the ternary eutectic solvent is 1:(8 to 15); the microwave radiation power is 400W to 600W, the reaction temperature is 120°C to 140°C, and the reaction time is 20 minutes to 40 minutes.
[0016] In one embodiment, the visible light responsive photocatalyst is graphitic carbon nitride, and its amount is 0.5% to 2% of the mass of the treatment solution; the mass ratio of pectinase, xylanase and laccase in the composite enzyme is (2 to 4):(1 to 3):1, and the total amount of the composite enzyme is 1% to 3% of the mass of the treatment solution; the pH value of the treatment solution is 4.5 to 5.5, the reaction temperature is 40°C to 50°C, and the reaction time is 60 minutes to 90 minutes; the visible light wavelength is 420 nm to 700 nm, and the light intensity is 50 mW / cm² to 150 mW / cm².
[0017] In one embodiment, the ultrasonic frequency is 20kHz to 40kHz, the ultrasonic power density is 0.5W / cm² to 2W / cm², the wind speed of the high-speed vortex airflow is 30m / s to 60m / s, and the processing time is 10 minutes to 20 minutes.
[0018] In one embodiment, the plant polyphenol is tea polyphenol or tannic acid, and its mass concentration in the bleaching solution is 2 g / L to 5 g / L; the mass concentration of hydrogen peroxide is 5 g / L to 15 g / L; the bleaching temperature is 50°C to 70°C, and the bleaching time is 40 minutes to 80 minutes; the softener is an amino silicone oil microemulsion, and its dosage is 2% to 5% of the dry weight of the fiber; the drying and setting temperature is 60°C to 80°C, and the moisture content of the fiber after drying is controlled at 8% to 12%. Beneficial effects
[0019] First, the present invention uses a low-temperature steam explosion pretreatment step to break the dense structure of bamboo and initially separate the fiber bundles by utilizing the explosive force of the sudden pressure drop. This creates a channel for the subsequent penetration of the deep eutectic solvent, which helps to shorten the solvent treatment time and improve the delignin removal efficiency.
[0020] Secondly, this invention utilizes a microwave-assisted ternary eutectic solvent delignination step. By leveraging the bulk heating effect of microwaves to reduce the diffusion barrier of the eutectic solvent, combined with the selective cleavage of ether bonds in the lignin-carbohydrate complex by the ternary eutectic solvent, most of the lignin and hemicellulose can be removed within 20 to 40 minutes. The processing time is much shorter than the dozens of days of soaking cycle of traditional bio-enzyme methods. Furthermore, the eutectic solvent can be recycled and reused, which helps reduce chemical pollution and processing costs.
[0021] Third, this invention utilizes a photocatalytic and compound enzyme synergistic degumming step, using visible light to excite a photocatalyst to generate active oxygen species to oxidize and degrade lignin. Simultaneously, the targeted enzymatic hydrolysis of pectinase, xylanase, and laccase can remove residual gum under mild conditions of 40°C to 50°C, which helps reduce damage to cellulose and improve fiber strength retention.
[0022] Fourth, the present invention achieves fiber separation by using an ultrasonic-assisted vortex fiber separation step, which utilizes the coupling effect of ultrasonic cavitation and high-speed vortex airflow to obtain single fibers with uniform fineness and avoids fiber breakage caused by mechanical combing.
[0023] Fifth, this invention utilizes a chlorine-free bleaching step involving the synergistic effect of plant polyphenols and hydrogen peroxide. By using plant polyphenols as a natural bleaching aid, the bleaching effect can be achieved under mild conditions, avoiding the pollution of adsorbable organic halides generated by chlorine-containing bleaching agents, which is beneficial to improving the environmental friendliness of the process.
[0024] The above-mentioned technical effects are the design expectations based on the technical principles, and the actual effects need to be verified by experiments. Attached Figure Description
[0025] Figure 1 This is a flowchart of the preparation method of the present invention.
[0026] Figure 2 This is a schematic diagram of a steam explosion reactor, showing components such as the upper head, cylinder, feed inlet, bamboo material, and support legs.
[0027] Figure 3 This is a schematic diagram of a microwave reactor, showing components such as the microwave generator, reaction chamber, and stirring paddle.
[0028] Figure 4 This is a schematic diagram of a photoenzyme co-reactor, with components such as the housing, visible light source, reaction solution, fibrous material, and circulation pump labeled.
[0029] Figure 5 This is a schematic diagram of an ultrasonic vortex fiber splitting device, showing components such as the outer shell, fiber material, vortex air tube, base, and ultrasonic transducer. Detailed Implementation
[0030] The process parameters involved in the following examples are all design expectations. In actual applications, they can be adjusted according to the characteristics of raw materials and product requirements. Example 1 like Figure 1 As shown, this embodiment provides a method for preparing bamboo fiber synergistically synthesized by microwave deep melting solvent and photoenzyme, and the specific steps are as follows: S1. Low-temperature steam explosion pretreatment: Select 3-year-old moso bamboo, remove the outer green layer and nodes, and cut into bamboo strips with a thickness of 2mm and a length of 30mm. For example... Figure 2 As shown, bamboo strips were placed in a steam explosion reactor. The bamboo strips were added through the feed inlet, and saturated steam was introduced through the steam inlet. The pressure was controlled at 1.5 MPa and the temperature at 170°C. After holding the pressure for 5 minutes, the pressure relief valve was quickly opened, and the pressure was released within 0.05 seconds, resulting in expanded bamboo filaments. The exploded bamboo filaments were fluffy, with initial fiber bundle separation and a significantly increased specific surface area. S2. Microwave-assisted eutectic solvent delignination: Prepare a ternary eutectic solvent according to a molar ratio of choline chloride, lactic acid, and glycerol of 1:2:0.5. During preparation, stir choline chloride and lactic acid at 80°C until a homogeneous, transparent liquid is formed. Then add glycerol and continue stirring for 30 minutes. Cool to room temperature for later use. Figure 3 As shown, expanded bamboo fibers and a ternary eutectic solvent were mixed at a mass ratio of 1:10 and added to the reaction chamber of a microwave reactor. The mixture was heated by microwave radiation at a power of 500W to 130°C and then maintained at that temperature for 30 minutes. During the reaction, a stirrer was operated at 150 rpm. After the reaction was complete, the material was removed, diluted with deionized water, and filtered. The filter cake was washed three times with hot water to obtain crude delignin-treated fibers. The eutectic solvent was recovered from the filtrate through rotary evaporation. The recovered solvent was then recycled after adding a small amount of fresh solvent. The design anticipates that this step will achieve a lignin removal rate of over 75% and a cellulose retention rate of over 90%. S3. Photocatalysis and composite enzyme synergistic degumming: In this embodiment, the graphitic carbon nitride photocatalyst was prepared by thermal polymerization: melamine was placed in a covered crucible and heated to 550°C in a muffle furnace at a heating rate of 5°C / min, held at that temperature for 4 hours, and then ground after natural cooling to obtain a light yellow graphitic carbon nitride powder. Figure 4As shown, crude deligninated fiber was placed in a photoenzyme co-processing reactor, and a treatment solution was added, immersing the fiber material in the reaction solution. The treatment solution contained 1% by mass of graphitic carbon nitride photocatalyst and 2% by mass of a composite enzyme (pectinase:xylanase:laccase in a mass ratio of 3:2:1). The pH was adjusted to 5.0 with acetate-sodium acetate buffer, the temperature was raised to 45°C, and a visible light source (wavelength 420nm to 700nm, light intensity 100mW / cm²) was turned on. The reaction was carried out for 75 minutes under gentle stirring. During the reaction, the treatment solution was circulated using a circulation pump. After the reaction was completed, the fiber was removed and washed with warm water until neutral to obtain finely degummed fiber. The design expected that the residual gum removal rate in this step could reach over 80%. S4. Ultrasonic-assisted eddy current fiber splitting: such as... Figure 5 As shown, the finely degummed fibers are placed in the processing chamber of an ultrasonic vortex fiber separating device, and deionized water is added to completely submerge the fibers. The bottom ultrasonic transducer is turned on, and the frequency is set to 30kHz and the power density to 1W / cm². Simultaneously, a high-speed vortex airflow is introduced through the vortex air tube at a wind speed of 45m / s for 15 minutes. The ultrasonic cavitation effect loosens the fiber bundles, and the vortex airflow separates the loose fiber bundles into individual fibers. After processing, the fibers are filtered and collected to obtain bamboo fiber semi-finished product. S5. Plant Polyphenol Bleaching and Softening: The semi-finished bamboo fiber is placed in a bleaching and setting tank, and bleaching solution is added. The bleaching solution contains 3 g / L of tea polyphenols and 10 g / L of hydrogen peroxide. The pH is adjusted to 8.5 with sodium carbonate, and the temperature is raised to 60℃ and maintained for 60 minutes. After bleaching, the fiber is washed with water until neutral. Then, a softening bath with a 30 g / L amino silicone oil microemulsion is prepared. The fiber is immersed in the softening bath at a ratio of 1:15 and treated at 40℃ for 20 minutes. After removing the fiber, it is dried at 70℃ until the moisture content is 10%, yielding the finished bamboo fiber product. The design anticipates that the resulting bamboo fiber product will have a fiber length of 30mm to 60mm, a fiber fineness of 2.0dtex to 3.0dtex, a fiber breaking strength exceeding 3.5cN / dtex, and a whiteness exceeding 75%. These performance indicators are design expectations and require experimental verification. Example 2 The difference between this embodiment and Embodiment 1 lies in the adjustment of process parameters, as detailed below: In step S1, the steam explosion pressure is 1.2 MPa, the temperature is 160℃, and the pressure holding time is 8 minutes. In step S2, the molar ratio of choline chloride, lactic acid, and glycerol in the ternary eutectic solvent is 1:1.5:0.3, the mass ratio of expanded bamboo filaments to solvent is 1:8, the microwave power is 400W, the reaction temperature is 120℃, and the reaction time is 40 minutes. In step S3, the amount of graphite phase carbon nitride used is 0.5% of the mass of the treatment solution, the total amount of compound enzymes used is 1% of the mass of the treatment solution, the mass ratio of pectinase:xylanase:laccase is 2:1:1, the pH value is 4.5, the reaction temperature is 40℃, the reaction time is 90 minutes, and the light intensity is 50mW / cm². In step S4, the ultrasonic frequency is 20kHz, the power density is 0.5W / cm², the vortex airflow velocity is 30m / s, and the processing time is 20 minutes. In step S5, the plant polyphenols used are tannic acid with a mass concentration of 2 g / L, hydrogen peroxide with a mass concentration of 5 g / L, bleaching temperature of 50℃, and bleaching time of 80 minutes; the amount of amino silicone oil microemulsion used is 2% of the dry weight of the fiber, the drying temperature is 60℃, and the final moisture content is 12%. The remaining steps are the same as in Example 1. Example 3 The difference between this embodiment and Embodiment 1 lies in the adjustment of process parameters, as detailed below: In step S1, the steam explosion pressure is 1.8 MPa, the temperature is 180℃, and the pressure holding time is 3 minutes. In step S2, the molar ratio of choline chloride, lactic acid, and glycerol in the ternary eutectic solvent is 1:2.5:0.8, the mass ratio of expanded bamboo filaments to solvent is 1:15, the microwave power is 600W, the reaction temperature is 140℃, and the reaction time is 20 minutes. In step S3, the amount of graphite phase carbon nitride used is 2% of the mass of the treatment solution, the total amount of compound enzymes used is 3% of the mass of the treatment solution, the mass ratio of pectinase:xylanase:laccase is 4:3:1, the pH value is 5.5, the reaction temperature is 50℃, the reaction time is 60 minutes, and the light intensity is 150mW / cm². In step S4, the ultrasonic frequency is 40kHz, the power density is 2W / cm², the vortex airflow velocity is 60m / s, and the processing time is 10 minutes. In step S5, the plant polyphenols used are tea polyphenols with a mass concentration of 5 g / L, the hydrogen peroxide mass concentration is 15 g / L, the bleaching temperature is 70℃, and the bleaching time is 40 minutes; the amount of amino silicone oil microemulsion used is 5% of the dry weight of the fiber, the drying temperature is 80℃, and the final moisture content is 8%. The remaining steps are the same as in Example 1. In the above embodiments, the eutectic solvent recovered in step S2 can be recycled after being replenished with a small amount of fresh solvent. It is designed to maintain a delignification efficiency of over 80% after 5 cycles. The graphitic carbon nitride photocatalyst in step S3 can be recovered and reused through centrifugation.
Claims
1. A method for preparing bamboo fiber in synergy of microwave deep eutectic solvent and photoenzyme, characterized in that, Includes the following steps: S1. Low-temperature steam explosion pretreatment: Bamboo strips with the outer green layer and nodes removed are placed in a steam explosion reactor, pressurized with saturated steam, and then quickly depressurized to obtain expanded bamboo fibers; S2. Microwave-assisted deep eutectic solvent delignination: The expanded bamboo fibers are mixed with a ternary deep eutectic solvent and placed in a microwave reactor. The mixture is heated under microwave radiation to selectively separate lignin and hemicellulose from cellulose, yielding crude delignin-treated fibers; the ternary deep eutectic solvent consists of choline chloride, lactic acid, and glycerol; S3. Photocatalytic and compound enzyme synergistic degumming: The crude delignin-treated fibers are placed in… In a treatment solution containing a visible light-responsive photocatalyst and a complex enzyme, an enzymatic hydrolysis reaction is carried out under visible light irradiation to degrade residual gum and obtain finely degummed fibers; the complex enzyme includes pectinase, xylanase, and laccase; S4, ultrasonic-assisted eddy current fiber separation: the finely degummed fibers are placed in an ultrasonic field, and a high-speed eddy current is introduced to separate the fibers, resulting in bamboo raw fiber semi-finished products in a single fiber state; S5, plant polyphenol bleaching and softening: the bamboo raw fiber semi-finished products are bleached without chlorine using a bleaching solution containing plant polyphenols and hydrogen peroxide, and then treated with a softener before drying and setting to obtain the finished bamboo raw fiber products.
2. The method according to claim 1, characterized in that, In step S1, the steam explosion pressure is 1.2 MPa to 1.8 MPa, the temperature is 160°C to 180°C, the pressure holding time is 3 minutes to 8 minutes, and the pressure release time does not exceed 0.1 seconds.
3. The method according to claim 1, characterized in that, In step S2, the molar ratio of choline chloride, lactic acid and glycerol in the ternary eutectic solvent is 1:(1.5 to 2.5):(0.3 to 0.8); the mass ratio of the expanded bamboo fiber to the ternary eutectic solvent is 1:(8 to 15).
4. The method according to claim 3, characterized in that, In step S2, the microwave radiation power is 400W to 600W, the reaction temperature is 120℃ to 140℃, and the reaction time is 20 minutes to 40 minutes. After the reaction is completed, lignin is separated by adding water to precipitate and the deep eutectic solvent is recovered and recycled.
5. The method according to claim 1, characterized in that, In step S3, the visible light responsive photocatalyst is graphitic carbon nitride, and its amount is 0.5% to 2% of the mass of the treatment solution; the mass ratio of pectinase, xylanase and laccase in the composite enzyme is (2 to 4):(1 to 3):1, and the total amount of composite enzyme is 1% to 3% of the mass of the treatment solution.
6. The method according to claim 5, characterized in that, In step S3, the pH of the treatment solution is 4.5 to 5.5, the reaction temperature is 40°C to 50°C, and the reaction time is 60 minutes to 90 minutes; the visible light wavelength is 420nm to 700nm, and the light intensity is 50mW / cm² to 150mW / cm².
7. The method according to claim 1, characterized in that, In step S4, the ultrasonic frequency is 20kHz to 40kHz, the ultrasonic power density is 0.5W / cm² to 2W / cm², the wind speed of the high-speed vortex airflow is 30m / s to 60m / s, and the processing time is 10 minutes to 20 minutes.
8. The method according to claim 1, characterized in that, In step S5, the plant polyphenols are tea polyphenols or tannic acid, and their mass concentration in the bleaching solution is 2 g / L to 5 g / L; the mass concentration of hydrogen peroxide is 5 g / L to 15 g / L; the bleaching temperature is 50°C to 70°C; and the bleaching time is 40 minutes to 80 minutes.
9. The method according to claim 8, characterized in that, In step S5, the softener is an amino silicone oil microemulsion, and its dosage is 2% to 5% of the dry weight of the fiber; the drying and setting temperature is 60°C to 80°C, and the moisture content of the fiber after drying is controlled at 8% to 12%.