Array substrates and electronic devices
By using a layered inorganic insulating layer structure, the stability problem of high-mobility oxide thin-film transistor devices is solved, and the stability of high-mobility devices is improved, making them suitable for high refresh rate and ultra-narrow bezel products.
Patent Information
- Application Number
- CN202611548438.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-03-12
- Publication Date
- 2026-11-10
AI Technical Summary
Existing high-mobility oxide thin-film transistor devices have poor stability, making it difficult to meet the requirements of high refresh rates and ultra-narrow bezel products.
The first inorganic insulating layer, which adopts a layered design, includes a thin and loose first sub-insulating layer and a thicker second sub-insulating layer. The first sub-insulating layer is in contact with the metal oxide semiconductor layer. By adjusting the film density and hydrogen content, oxygen is replenished to the high-mobility metal oxide semiconductor layer, reducing the negative bias of the threshold voltage and thus improving the stability of the device.
This improves the stability of high-mobility oxide thin-film transistors, enhances the forward bias of the threshold voltage, and improves the performance of the device.
Smart Images

Figure CN123076015A_ABST
Abstract
Description
[0001] This divisional application is a divisional application of Chinese patent application No. 202410288010.3, filed on March 12, 2024, entitled "Array Substrate and Electronic Device". Technical Field
[0002] This application relates to the field of thin-film transistor technology, and more particularly to an array substrate and electronic device. Background Technology
[0003] Oxide thin-film transistors (OTTs) have been increasingly used in display driver circuits due to their low off-state current and high mobility. However, most of the oxide semiconductors currently available for mass production are indium gallium zinc oxide (IGZO), which typically has a mobility of less than 15 cm⁻¹. 2 / Vs. In high refresh rate, ultra-narrow bezel product applications, GOA driving circuits require thin film transistors (TFTs) with higher mobility to meet the target requirements. However, the threshold and stability of current oxide devices for achieving high mobility are relatively poor. Therefore, the stability of existing high-mobility TFT devices urgently needs improvement. Summary of the Invention
[0004] This application provides an array substrate and electronic device to solve the technical problem of poor stability of existing metal oxide thin film transistors with high mobility characteristics.
[0005] To solve the above problems, the technical solution provided in this application is as follows: This application provides an array substrate, including: Substrate; A metal oxide semiconductor layer is disposed on the substrate; A gate electrode is disposed on the substrate, and a gate insulating layer is provided between the gate electrode and the metal oxide semiconductor layer; and A first inorganic insulating layer is disposed on the side of the metal oxide semiconductor layer away from the gate. The first inorganic insulating layer includes a first sub-insulating layer and a second sub-insulating layer stacked together. The first sub-insulating layer is in contact with the metal oxide semiconductor layer, and the second sub-insulating layer is disposed on the side of the first sub-insulating layer away from the metal oxide semiconductor layer. Wherein, the thickness of the first sub-insulating layer is less than the thickness of the second sub-insulating layer, and the film density of the first sub-insulating layer is less than the film density of the second sub-insulating layer.
[0006] In some embodiments of this application, the mass content of hydrogen in the first sub-insulating layer is greater than the mass content of hydrogen in the second sub-insulating layer, and / or the material of the first inorganic insulating layer includes silicon oxide, and the Si-O bond content of the first sub-insulating layer is less than the Si-O bond content in the second sub-insulating layer.
[0007] In some embodiments of this application, the first inorganic insulating layer is disposed on the substrate, the metal oxide semiconductor layer is disposed on the first inorganic insulating layer, the gate insulating layer is disposed on the metal oxide semiconductor layer, and the gate is disposed on the gate insulating layer.
[0008] In some embodiments of this application, the gate is disposed on the substrate, the gate insulating layer is disposed on the gate, the metal oxide semiconductor layer is disposed on the gate insulating layer, and the first inorganic insulating layer is disposed on the metal oxide semiconductor layer.
[0009] In some embodiments of this application, the array substrate further includes a second inorganic insulating layer, the material of which includes a silicon nitride layer, the silicon nitride layer being disposed on the side of the second sub-insulating layer near the substrate.
[0010] In some embodiments of this application, the thickness of the first inorganic insulating layer is 1000 Å-4000 Å.
[0011] In some embodiments of this application, the thickness of the first inorganic insulating layer is 2000 Å-10000 Å.
[0012] In some embodiments of this application, the thickness of the first sub-insulating layer is less than 500 Å.
[0013] In some embodiments of this application, the film density of the first sub-insulating layer is 1.83 g / cm³. 3 -2.53 g / cm 3 .
[0014] In some embodiments of this application, the material of the metal oxide semiconductor layer is indium tin oxide, indium gallium oxide, or indium zinc oxide doped with at least one metal ion, wherein the metal ion doped with the indium tin oxide is selected from Zn. 2+ Ga 3+ Sn 2+ Al 3+ and Hf 4+ At least one of the following, wherein the indium gallium oxide-doped metal ions are selected from Sn 2+ Al 3+ and Hf 4+At least one of the following, wherein the indium zinc oxide doped metal ion is selected from Sn 2+ Al 3+ and Hf 4+ At least one of them.
[0015] This application also provides an electronic device, including the array substrate in any of the above embodiments, and a light-emitting element or a sensing element.
[0016] The beneficial effects of this application are as follows: This application provides an array substrate and an electronic device, including a metal oxide semiconductor layer, a gate, and a first inorganic insulating layer disposed on a substrate. A gate insulating layer is disposed between the gate and the metal oxide semiconductor layer. The first inorganic insulating layer is disposed on the side of the metal oxide semiconductor layer away from the gate. The first inorganic insulating layer includes a first sub-insulating layer and a second sub-insulating layer stacked together. The first sub-insulating layer is in contact with the metal oxide semiconductor layer. The second sub-insulating layer is disposed on the side of the first sub-insulating layer away from the metal oxide semiconductor layer. The thickness of the first sub-insulating layer is less than the thickness of the second sub-insulating layer, and the film density of the first sub-insulating layer is less than the film density of the second sub-insulating layer. By designing the first inorganic insulating layer (a first sub-insulating layer and a second sub-insulating layer) on the side of the metal oxide semiconductor layer away from the gate and in contact with the metal oxide semiconductor layer, the thickness of the first sub-insulating layer in contact with the metal oxide semiconductor layer is designed to be smaller than that of the second sub-insulating layer. The film quality of the first sub-insulating layer is also changed so that the film quality density of the first sub-insulating layer is smaller than that of the second sub-insulating layer. This makes the film quality of the thinner first sub-insulating layer more porous, which can achieve oxygen replenishment to the high-mobility metal oxide semiconductor layer, reduce the negative bias of the threshold voltage, and thus improve the stability of the high-mobility metal oxide semiconductor device. Attached Figure Description
[0017] To more clearly illustrate the technical solutions in the embodiments or the prior art, the drawings used in the description of the embodiments or the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the application. For those skilled in the art, other drawings can be obtained based on these drawings without creative effort.
[0018] Figure 1 This is a schematic diagram of a first structure of the array substrate provided in an embodiment of this application; Figure 2 This is a schematic diagram of a second structure of the array substrate provided in an embodiment of this application; Figure 3 This is a schematic diagram of a first structure of an electronic device provided in an embodiment of this application; Figure 4This is a schematic diagram of a second structure of the electronic device provided in the embodiments of this application; Figure 5 This is a schematic diagram of a third structure of the electronic device provided in the embodiments of this application; Figure 6 A graph showing the hydrogen content of the first sub-insulating layer in Example 1; Figure 7 A graph showing the hydrogen content of the second sub-insulating layer in Example 1; Figure 8 The diagram shows the electrical test results of the thin-film transistor in Example 1. Figure 9 This is an electrical test diagram of the thin-film transistor in Comparative Example 1. Detailed Implementation
[0019] The following descriptions of the embodiments are based on the accompanying illustrations and are used to illustrate specific embodiments in which this application can be implemented. Directional terms used in this application, such as [up], [down], [front], [back], [left], [right], [inner], [outer], [side], etc., are only for reference to the accompanying drawings. Therefore, the directional terms used are for illustrative and understanding purposes and not for limiting the application. In the figures, structurally similar units are represented by the same reference numerals.
[0020] The technical solutions of the embodiments of this application will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only a part of the embodiments of this application, and not all of them. All other embodiments obtained by those skilled in the art based on the embodiments of this application without creative effort are within the scope of protection of this application.
[0021] Please see Figure 1 This application provides an array substrate 10, which includes a substrate 11, a metal oxide semiconductor layer 13, a gate insulating layer 14, a gate 15, and a first inorganic insulating layer 12.
[0022] The substrate 11 is used to support the various layers on the substrate 11. The substrate 11 can be a rigid substrate such as a glass substrate, or the substrate 11 can be a flexible substrate. The materials of the flexible substrate include, but are not limited to, polyimide (PI), polyethylene naphthalate (PEN), polyethylene terephthalate (PET), and polyetherimide (PEI). The substrate 11 can include a multilayered composite film structure. Specifically, the substrate 11 can include a first flexible substrate, an intermediate layer, and a second flexible substrate stacked sequentially. The first flexible substrate and the second flexible substrate can be formed of polyimide, and the intermediate layer can be formed of inorganic materials such as silicon nitride and silicon oxide.
[0023] The gate 15 and the metal oxide semiconductor layer 13 are stacked on the substrate 11. The gate 15 may be disposed on the side of the metal oxide semiconductor layer 13 away from the substrate 11, or on the side of the metal oxide semiconductor layer 13 closer to the substrate 11. The material of the gate 15 may include molybdenum, aluminum, platinum, palladium, silver, magnesium, gold, nickel, neodymium, iridium, chromium, titanium, tantalum, tungsten, copper, or alloys thereof. The gate 15 may include a single-layer or multi-layer metal structure.
[0024] A gate insulating layer 14 is provided between the gate 15 and the metal oxide layer. The material of the gate insulating layer 14 may include inorganic materials, such as silicon nitride, silicon oxide, etc.
[0025] The first inorganic insulating layer 12 is disposed on the side of the metal oxide semiconductor layer 13 away from the gate 15 and is in contact with the metal oxide semiconductor layer 13.
[0026] The metal oxide semiconductor layer 13 is disposed on the substrate 11, and the thickness of the metal oxide semiconductor layer 13 is 200 Å-800 Å. The material of the metal oxide semiconductor layer 13 is indium tin oxide (ITO), indium gallium oxide (IGO), or indium zinc oxide (IZO) doped with at least one metal ion, wherein the metal ion doped in ITO is selected from Zn. 2+ Ga 3+ Sn 2+ Al 3+ and Hf 4+ One of them, the IGO-doped metal ions are selected from Sn. 2+ Al 3+ and Hf 4+ One of them, the IZO-doped metal ions are selected from Sn.2+ Al 3+ and Hf 4+ One of them. The material of the metal oxide semiconductor layer 13 can be IGZTO or IZTO.
[0027] Currently, the mobility of mass-produced IGZO semiconductors is typically less than 15 cm⁻¹. 2 / VS. In electronic products with high refresh rates and extremely narrow bezels, the GOA driving circuit requires thin-film transistor devices with higher mobility to meet the target requirements. The metal oxide in this application embodiment achieves a mobility of 15cm. 2 With a mobility of / VS or higher, it exhibits higher mobility compared to IGZO, meeting the requirements. The key to controlling the characteristics of thin-film transistors lies in the channel interface. The threshold voltage and stability of high-mobility devices with abundant charge carriers are affected not only by the positive channel interface but also by the back channel interface. If high-mobility thin-film transistor devices are fabricated using the existing structure and process of IGZO thin-film transistor devices, negative bias at the threshold voltage is likely to occur. If only oxygen is added to the gate insulating layer 14 and the metal-oxide-semiconductor layer 13 for adjustment, a decrease in mobility and poor bias voltage stability are likely to occur. Therefore, this application improves the structure of high-mobility metal-oxide-semiconductor devices to solve the negative bias phenomenon of the threshold voltage and improve the stability of high-mobility metal-oxide-semiconductor devices.
[0028] Specifically, this application embodiment improves the first inorganic insulating layer 12, which includes multiple sub-layers. The first inorganic insulating layer 12 may include a first sub-insulating layer 121 and a second sub-insulating layer 122. The first sub-insulating layer 121 is in contact with the metal oxide semiconductor layer 13, and the second sub-insulating layer 122 is disposed on the side of the first sub-insulating layer 121 away from the metal oxide semiconductor layer 13. The thickness of the first sub-insulating layer 121 is less than the thickness of the second sub-insulating layer 122, and the film density of the first sub-insulating layer 121 is less than the film density of the second sub-insulating layer 122. By designing the first inorganic insulating layer 12, which is on the side of the metal oxide semiconductor layer 13 away from the gate 15 and in contact with the metal oxide semiconductor layer 13, into at least two sub-film layers (first sub-insulating layer 121 and second sub-insulating layer 122), the thickness of the first sub-insulating layer 121 in contact with the metal oxide semiconductor layer 13 is designed to be smaller than the thickness of the second sub-insulating layer 122. The film quality of the first sub-insulating layer 121 is changed so that the film quality density of the first sub-insulating layer 121 is smaller than that of the second sub-insulating layer 122. This makes the thinner first sub-insulating layer 121 more porous, enabling oxygen replenishment to the high-mobility metal oxide semiconductor layer 13, reducing the negative bias of the threshold voltage, and thus improving the stability of the high-mobility metal oxide semiconductor device.
[0029] The array substrate 10 in this embodiment may further include a source 191 and a drain 192, wherein the gate 15, the metal-oxide-semiconductor layer 13, the source 191, and the drain 192 constitute a thin-film transistor. The thin-film transistor in this embodiment may be a top-gate thin-film transistor, such as... Figure 1 As shown, Figure 1 This is a schematic diagram of a first structure of the array substrate provided in the embodiments of this application; it can also be a bottom-gate thin-film transistor, such as... Figure 2 As shown, Figure 2 This is a schematic diagram of a second structure of the array substrate provided in an embodiment of this application.
[0030] exist Figure 1 In the illustrated embodiment, the array substrate 10 may further include a light-shielding layer 16 located below the metal-oxide-semiconductor layer 13. The light-shielding layer 16 overlaps with the orthographic projection of the active layer onto the substrate 11, thereby reducing ambient light irradiation of the metal-oxide-semiconductor layer 13 and ensuring the performance stability of the thin-film transistor device. The material of the light-shielding layer 16 may include molybdenum, aluminum, platinum, palladium, silver, magnesium, gold, nickel, neodymium, iridium, chromium, titanium, tantalum, tungsten, copper, or alloys thereof. The thickness of the light-shielding layer 16 is 2000 Å-8000 Å.
[0031] Specifically, the array substrate 10 includes a light-shielding layer 16, a second inorganic insulating layer 17, and a first inorganic insulating layer 12 sequentially stacked on a substrate 11. The second inorganic insulating layer covers the light-shielding layer 16. The second inorganic insulating layer 17 can be a single-layer or multi-layer structure. The second inorganic insulating layer 17 serves to insulate against impurities and moisture, and to provide a flat surface for subsequently formed film layers. The second inorganic insulating layer 17 may include a silicon nitride layer to enhance the bonding performance between the second inorganic insulating layer 17 and other film layers. The second inorganic insulating layer 17 may also include multiple sub-layer structures. The sub-layers near the substrate 11 are formed of silicon oxide to enhance the bonding performance between the second inorganic insulating layer 17 and the substrate 11, and the sub-layers near the first inorganic insulating layer 12 are formed of silicon nitride to enhance the bonding performance between the second inorganic insulating layer 17 and the first inorganic insulating layer 12.
[0032] exist Figure 1 In the illustrated embodiment, the thickness of the first inorganic insulating layer 12 is 1000 Å-4000 Å. The material of the first inorganic insulating layer 12 includes oxides. The first inorganic insulating layer 12 is formed in two stages. The first sub-insulating layer 121, which is closer to the metal oxide semiconductor layer 13, is thinner and has a lower film density, while the second sub-insulating layer 122, which is closer to the substrate 11, is thicker and has a higher film density. With this design, the film of the first sub-insulating layer 121 is relatively porous. During the film formation process of the first sub-insulating layer 121, when the first sub-insulating layer 121 is cleaned by oxygen plasma treatment, the surface of the first sub-insulating layer 121 becomes rich in oxygen. Subsequently, the interface between the first sub-insulating layer 121 and the metal oxide semiconductor layer 13 is rich in oxygen, which plays a role in oxygen replenishment to the metal oxide semiconductor layer 13. The second sub-insulating layer 122, which has a thicker film thickness and higher film density, can be used as a buffer layer to further block impurities, moisture, and achieve planarization.
[0033] In some embodiments, the film density of the first sub-insulating layer 121 is 1.83 g / cm³. 3 -2.53 g / cm 3 Optionally, the film density of the first sub-insulating layer 121 may be 1.83 g / cm³. 3 1.85 g / cm 3 1.88 g / cm 3 1.90 g / cm 3 1.95 g / cm 3 2.0 g / cm 3 2.1 g / cm 3 2.2 g / cm 3 2.3 g / cm 3 2.4 g / cm3 2.53 g / cm 3 And the values between any two of the above values.
[0034] Specifically, the thickness of the first sub-insulating layer 121 is less than 500 Å. The thickness of the second sub-insulating layer 122 is 500 Å - 3500 Å. After formation, the layers of the first sub-insulating layer 121 and the second sub-insulating layer 122 may not be discernible to the naked eye, but can be identified by SIMS (Secondary Ion Mass Spectroscopy) or XRR (X-ray reflectivity) testing.
[0035] Please continue reading. Figure 1 The metal oxide semiconductor layer 13 is disposed on the first sub-insulating layer 121, the gate insulating layer 14 is disposed on the metal oxide semiconductor layer 13, and the gate 15 is disposed on the gate insulating layer 14. An interlayer insulating layer 18 is provided on the metal oxide semiconductor layer 13, and the interlayer insulating layer 18 covers the metal oxide semiconductor layer 13, the gate 15, and the gate insulating layer 14.
[0036] The interlayer insulating layer 18 can be made of silicon nitride, silicon oxide, or a stacked structure of silicon nitride and silicon oxide. The thickness of the interlayer insulating layer 18 is 2000 Å-10000 Å.
[0037] The source electrode 191 and the drain electrode 192 are disposed on the interlayer insulating layer 18. The materials of the source electrode 191 and the drain electrode 192 may include molybdenum, aluminum, platinum, palladium, silver, magnesium, gold, nickel, neodymium, iridium, chromium, titanium, tantalum, tungsten, copper, or alloys thereof. The thickness of the source electrode 191 and the drain electrode 192 is 2000 Å-8000 Å.
[0038] In the embodiments of this application, the hydrogen content of the first sub-insulating layer 121 is greater than that of the second sub-insulating layer 122. The material of the first inorganic insulating layer 12 may include silicon oxide, and the Si-O bond content in the first sub-insulating layer 12 is less than that in the second sub-insulating layer. The Si-O bond content can be the number of Si-O bonds per unit volume. This design allows the first sub-insulating layer 121 to have a better oxygen storage capacity than the second sub-insulating layer 122, which is more conducive to the oxygen replenishment of the metal oxide semiconductor layer 13 by the first sub-insulating layer 121. The hydrogen content can be measured by SIMS (Secondary Ion Mass Spectroscopy), and the Si-O bond content can be measured by FTIR (Fourier Transform Infrared Spectrometer).
[0039] In some embodiments of this application, the first inorganic insulating layer may further include a third sub-insulating layer, which is disposed on the side of the second sub-insulating layer 122 opposite to the first sub-insulating layer 121, and may also include more sub-insulating layers. In the multiple sub-insulating layers of the first inorganic insulating layer 12, along the direction of the first sub-insulating layer 121 away from the metal oxide semiconductor layer 13, the thickness of the multiple sub-insulating layers increases sequentially, the film density gradually increases, the hydrogen content gradually decreases, and the Si-O bond content gradually increases. This stepped design enhances the oxygen storage capacity of the sub-insulating layers near the oxide semiconductor layer, improving the oxygen replenishment effect of the first inorganic insulating layer on the metal oxide layer.
[0040] like Figure 2 As shown, in other embodiments, the thin-film transistor may be a bottom-gate structure. Specifically, the gate 15 is disposed on the substrate 11, the gate insulating layer 14 is disposed on the gate 15, the metal oxide semiconductor layer 13 is disposed on the gate insulating layer 14, the first inorganic insulating layer 12 is disposed on the metal oxide semiconductor layer 13, and the source 191 is disposed on the first inorganic insulating layer 12.
[0041] exist Figure 2 In the illustrated embodiment, the first sub-insulating layer 121 is disposed on the metal oxide semiconductor layer 13 and contacts the top surface of the metal oxide semiconductor layer 13. The second sub-insulating layer 122 is disposed on the first sub-insulating layer 122. In this embodiment, the first sub-insulating layer 121 serves as an oxygen supplement, and the second sub-insulating layer 122 serves as an interlayer insulating layer. In this embodiment, the overall thickness of the first inorganic insulating layer is relatively... Figure 1The overall thickness of the first inorganic insulating layer in the illustrated embodiment is thick, and the overall thickness of the first inorganic insulating layer 12 is 2000 Å-10000 Å. Figure 2 Other structures of the thin-film transistors shown in the embodiments can be found in reference. Figure 1 Description of the illustrated embodiment.
[0042] This application also provides an electronic device, which may be a display device, such as... Figure 3 and Figure 4 As shown, it can specifically be an organic electroluminescent display panel; it can also be an electronic sensor, such as... Figure 5 As shown, these can specifically be gas sensors, temperature sensors, biological detection sensors, etc.
[0043] like Figure 3 As shown, Figure 3 This is a schematic diagram of a first structure of an electronic device provided in an embodiment of this application. The electronic device is an organic electroluminescent display panel. The organic electroluminescent display panel includes an array substrate 10 and light-emitting elements 20 disposed on the array substrate 10. The light-emitting element 20 includes a passivation layer 21, a connecting metal 22, a planarization layer 23, an anode 24, a pixel definition layer 25, etc., stacked sequentially.
[0044] The passivation layer 21 is disposed on the source electrode 191 and the drain electrode 192. The material of the passivation layer 21 can be silicon oxide or oxynitride, which serves to isolate and protect the thin-film transistor and prevent moisture intrusion. The thickness of the passivation layer 21 is 1000 Å-5000 Å.
[0045] The connecting metal 22 is disposed on the passivation layer 21, and the connecting metal 22 is used for wiring connections between different metal layers. The material of the light-shielding layer 16 may include molybdenum, aluminum, platinum, palladium, silver, magnesium, gold, nickel, neodymium, iridium, chromium, titanium, tantalum, tungsten, copper, or alloys thereof. The thickness of the light-shielding layer 16 is 2000 Å-8000 Å.
[0046] The planarization layer 23 is disposed on the connecting metal 22, and the planarization layer 23 provides a flat surface for the subsequently formed anode 24.
[0047] The anode 24 is disposed on the planarization layer 23, and the anode 24 is made of ITO. The pixel definition layer 25 is disposed on the planarization layer 23. The pixel definition layer 25 includes a plurality of pixel grooves, and a subsequent light-emitting material layer is formed within the pixel grooves.
[0048] The light-emitting element 20 further includes a light-emitting layer and a cathode sequentially stacked on the anode 24. The light-emitting layer may include a hole injection layer, a hole transport layer, a light-emitting material layer, an electron transport layer, and an electron injection layer sequentially stacked on the anode 24.
[0049] like Figure 4 As shown, Figure 4 This is a schematic diagram of a second structure of an electronic device provided in an embodiment of this application. Figure 4 The illustrated embodiments and Figure 3 The light-emitting element 20 in the illustrated embodiment has the same structure, which will not be described again here. The difference lies in... Figure 4 In the embodiments described, the array substrate is a bottom-gate thin-film transistor, as detailed in the following reference. Figure 2 The structure of the array substrate shown is as follows: Figure 3 The array substrate in the illustrated embodiment is a top-gate thin-film transistor, which can be referred to in detail below. Figure 3 The structure of the array substrate shown.
[0050] The inventors have demonstrated the present application through specific embodiment 1 and comparative example 1. Figure 1 The structure shown forms a high-mobility IZO-doped oxide (mobility > 30 cm⁻¹). 2 Threshold bias voltage testing was performed on the top-gate thin-film transistor device (VS), as shown in the attached figure. Figure 6 , Figure 7 , Figure 8 as well as Figure 9 As shown, Figure 6 This is a graph showing the hydrogen content of the first sub-insulating layer in Example 1. Figure 7 This is a graph showing the hydrogen content of the second sub-insulating layer in Example 1. Figure 8 The diagram shows the electrical test results of the thin-film transistor in Example 1. Figure 9 The diagram shows the electrical test results of the thin-film transistor in Comparative Example 1. The top-gate thin-film transistor devices in Example 1 and Comparative Example 1 have the same structure. The difference lies in the structure of the first inorganic insulating layer 12. In Example 1, the first inorganic insulating layer 12 is a double-layer structure, and the material is SiO2. x The film density of the first sub-insulating layer 121 is 2.03 g / cm³. 3 The film density of the second insulating layer 122 is 2.42 g / cm³. 3 In Comparative Example 1, the first inorganic insulating layer 12 is a single-layer structure, and the material is SiO2. x The film density of the first inorganic insulating layer 12 is 2.42 g / cm³. 3 The test conditions for Example 1 and Example 2 are the same.
[0051] from Figure 8 and Figure 9As can be seen, the array substrate 10 provided in Example 1 significantly improves the negative bias of the threshold voltage, with the average value of the threshold voltage Vth improving from -0.87V to -0.04V. Therefore, by employing a layered deposition design for the first inorganic insulating layer 12 in contact with the back channel, the array substrate 10 provided in this application can improve the back channel interface, resulting in a positive bias of the threshold voltage Vth, and a slight increase or no effect on mobility, thereby improving the stability of high-mobility devices.
[0052] like Figure 5 As shown, Figure 5 This is a schematic diagram of a third structure of the electronic device provided in an embodiment of this application. Figure 5 In the embodiment shown, the electronic device is an electronic sensor, which includes the array substrate 10 and the sensing element 30. The array substrate 10 is provided with a passivation layer 21, and the sensing element 30 is disposed on the passivation layer 21 and electrically connected to the source 191 or drain 192 in the array substrate 10 through a via on the passivation layer 21.
[0053] The sensing element 30 can be a photoelectric detection element, a temperature sensing element, or a gas sensing element.
[0054] In summary, this application provides an array substrate 10 and an electronic device, including a metal oxide semiconductor layer 13, a gate 15, and a first inorganic insulating layer 12 disposed on a substrate 11. A gate insulating layer 14 is provided between the gate 15 and the metal oxide semiconductor layer 13. The first inorganic insulating layer 12 is disposed on the side of the metal oxide semiconductor layer 13 away from the gate 15. The first inorganic insulating layer 12 includes a first sub-insulating layer 121 and a second sub-insulating layer 122 stacked together. The first sub-insulating layer 121 is in contact with the metal oxide semiconductor layer 13. The second sub-insulating layer 122 is disposed on the side of the first sub-insulating layer 121 away from the metal oxide semiconductor layer 13. The thickness of the first sub-insulating layer 121 is less than the thickness of the second sub-insulating layer 122, and the film density of the first sub-insulating layer 121 is less than the film density of the second sub-insulating layer 122. By designing the first inorganic insulating layer 12, which is on the side of the metal oxide semiconductor layer 13 away from the gate 15 and in contact with the metal oxide semiconductor layer 13, into at least two sub-film layers (first sub-insulating layer 121 and second sub-insulating layer 122), the thickness of the first sub-insulating layer 121 in contact with the metal oxide semiconductor layer 13 is designed to be smaller than the thickness of the second sub-insulating layer 122. The film quality of the first sub-insulating layer 121 is changed so that the film quality density of the first sub-insulating layer 121 is smaller than that of the second sub-insulating layer 122. This makes the thinner first sub-insulating layer 121 more porous, enabling oxygen replenishment to the high-mobility metal oxide semiconductor layer 13, reducing the negative bias of the threshold voltage, and thus improving the stability of the high-mobility metal oxide semiconductor device.
[0055] In the above embodiments, the descriptions of each embodiment have different focuses. For parts not described in detail in a certain embodiment, please refer to the relevant descriptions in other embodiments.
[0056] The above provides a detailed description of an array substrate and electronic device provided in the embodiments of this application. Specific examples have been used to illustrate the principles and implementation methods of this application. The description of the above embodiments is only for the purpose of helping to understand the technical solutions and core ideas of this application. Those skilled in the art should understand that modifications can still be made to the technical solutions described in the foregoing embodiments, or equivalent substitutions can be made to some of the technical features. These modifications or substitutions do not cause the essence of the corresponding technical solutions to deviate from the scope of the technical solutions of the embodiments of this application.
Claims
1. An array substrate, characterized in that, include: Substrate; A first inorganic insulating layer is disposed on the substrate; A metal oxide semiconductor layer, wherein the metal oxide semiconductor layer is disposed on a surface of the first inorganic insulating layer away from the substrate; A gate, wherein the gate is disposed on the side of the metal oxide semiconductor layer away from the substrate; The first inorganic insulating layer includes a first sub-insulating layer and a second sub-insulating layer. The first sub-insulating layer is disposed on a surface of the metal oxide semiconductor layer near the substrate, and the second sub-insulating layer is disposed on the side of the first sub-insulating layer near the substrate. The thickness of the first sub-insulating layer is less than the thickness of the second sub-insulating layer, and the film density of the first sub-insulating layer is less than the film density of the second sub-insulating layer.
2. The array substrate according to claim 1, characterized in that, The mass content of hydrogen in the first sub-insulating layer is greater than that in the second sub-insulating layer, and / or the material of the first inorganic insulating layer includes silicon oxide, and the Si-O bond content in the first sub-insulating layer is less than that in the second sub-insulating layer.
3. The array substrate according to claim 1, characterized in that, The array substrate further includes a second inorganic insulating layer, the material of which includes a silicon nitride layer, the silicon nitride layer being disposed on the side of the second sub-insulating layer near the substrate.
4. The array substrate according to claim 3, characterized in that, The array substrate further includes a light-shielding layer disposed on the substrate, the light-shielding layer overlapping the orthographic projection of the metal oxide semiconductor layer on the substrate, wherein the second inorganic insulating layer covers the light-shielding layer.
5. The array substrate according to claim 1, characterized in that, The thickness of the first inorganic insulating layer is 1000 Å-4000 Å.
6. The array substrate according to claim 5, characterized in that, The thickness of the first sub-insulating layer is less than 500 Å, and / or the film density of the first sub-insulating layer is 1.83 g / cm³. 3 -2.53 g / cm 3 .
7. The array substrate according to claim 1, characterized in that, The metal oxide semiconductor layer is made of indium tin oxide, indium gallium oxide, or indium zinc oxide doped with at least one metal ion, wherein the metal ion doped in the indium tin oxide is selected from Zn. 2+ Ga 3+ Sn 2+ Al 3+ and Hf 4+ At least one of the following, wherein the indium gallium oxide-doped metal ions are selected from Sn 2+ Al 3+ and Hf 4+ At least one of the following, wherein the indium zinc oxide doped metal ion is selected from Sn 2+ Al 3+ and Hf 4+ At least one of them.
8. The array substrate according to claim 1, characterized in that, The first inorganic insulating layer further includes a third sub-insulating layer, which is disposed on the side of the second sub-insulating layer opposite to the first sub-insulating layer.
9. The array substrate according to claim 1, characterized in that, Along the direction away from the metal oxide semiconductor layer in the first sub-insulating layer, the thickness of the multilayer sub-insulating layers in the first inorganic insulating layer increases sequentially, and the film density of the multilayer sub-insulating layers in the first inorganic insulating layer gradually increases.
10. An electronic device, characterized in that, It includes the array substrate as described in any one of claims 1 to 9, and the light-emitting element or the sensing element.