Stress relief device and warpage control method for packaged electronic devices

By using a stress relief device in the semiconductor packaging process and utilizing temperature and pressure control technology, the warping problem was solved, enabling rapid stress release and leveling of warped samples, and ensuring the stability and accuracy of the packaging process.

CN123076200APending Publication Date: 2026-11-10ELEAD TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611577842.2
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-10-13
Publication Date
2026-11-10

AI Technical Summary

Technical Problem

In the semiconductor packaging process, warping can be caused by internal stress introduced by materials or process parameters, affecting the uniformity and operability of the process. Existing technologies are difficult to effectively control and eliminate this problem.

Method used

A stress relief device is employed, comprising a cavity, a temperature component, a pressure component, a detection component, and a control component. By precisely controlling the temperature and pressure, rapid stress release and leveling of warped samples are achieved.

Benefits of technology

Effectively control the stress release of warped samples to avoid affecting the process and ensure the stability and accuracy of the packaging process.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123076200A_ABST
    Figure CN123076200A_ABST
Patent Text Reader

Abstract

This invention relates to a stress relief device and warpage control method for packaging electronic devices. The stress relief device includes: a cavity having a sealed cavity space for placing a warped sample; a temperature component disposed within the cavity for regulating the operating temperature; a pressure component connected to the cavity for regulating the operating pressure; a detection component disposed on the cavity for detecting the warpage state of the sample; and a control component connected to the temperature component, pressure component, and detection component for receiving information from the detection component and determining the type of residual stress in the sample, thereby controlling the temperature component and pressure component to regulate the warpage control process. This invention enables warped samples to release stress quickly and efficiently, completing warpage leveling and avoiding impact on the manufacturing process.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of semiconductor packaging technology, and in particular to a stress relief device and warpage control method for packaging electronic devices. Background Technology

[0002] In the packaging process of semiconductor electronic components, internal stress is often introduced due to material or process parameters. When these stresses cannot be balanced, it manifests macroscopically as warpage. The essence of warpage is actually uneven shrinkage or expansion of materials with different coefficients of thermal expansion (CTE) under the same / different process parameters (such as temperature, pressure, etc.). Product warpage can cause uneven thickness during "addition" (such as depositing metal / non-metal materials, laminating dry films, etc.) or "reduction" (etching / etching / resin removal, etc.) processes, thus affecting performance. When the product warpage exceeds the limits of the process equipment, the product may even become impossible to hold, hold, or detect.

[0003] To eliminate stresses in the manufacturing process (such as thermal stress, curing shrinkage stress, and residual interface stress), it is necessary to precisely control the cavity temperature, contact air pressure, and operating time of the hot press equipment, thereby controlling product warpage during the packaging process. Summary of the Invention

[0004] Therefore, it is necessary to provide a stress relief device and warpage control method for packaging electronic devices to address the aforementioned technical problems in the existing technology, so that warped samples can release stress quickly and efficiently, complete warpage leveling, and avoid affecting the process.

[0005] To solve the above technical problems, the technical solution adopted by the present invention is as follows: A stress relief device for packaging electronic devices, comprising: A cavity, having a sealed cavity space, is used to place a warped sample; A temperature control unit, located inside the cavity, is used to regulate the operating temperature. The pneumatic assembly, connected to the cavity, is used to regulate the working pressure; A detection component, mounted on the cavity, is used to detect the warping state of the sample; The control component is connected to the temperature component, the pressure component, and the detection component respectively. It is used to receive information from the detection component and determine the type of residual stress in the sample, and then control the temperature component and the pressure component to perform warpage control process regulation.

[0006] Preferably, the cavity includes a first cavity and a second cavity, and the first cavity and the second cavity can be closed to form a sealed cavity space; The first chamber includes an internally pressurized airbag; The second cavity includes a sample base for placing the warped sample. The sample base is connected to a vacuum adsorption component, which adsorbs the sample onto the sample base.

[0007] Preferably, the temperature assembly includes a heater, a cooler, and a temperature sensor, wherein the heater is used to increase the operating temperature, the cooler is used to decrease the operating temperature, and the temperature sensor is used to detect the operating temperature.

[0008] Preferably, the pneumatic assembly includes a pressure boosting assembly, a pressure relief assembly, and a pressure sensor. The pressure boosting assembly is used to increase the working pressure, the pressure relief assembly is used to reduce the working pressure, and the pressure sensor is used to detect the working pressure. The pneumatic assembly includes a first pneumatic assembly and a second pneumatic assembly. The first pneumatic assembly is connected to the airbag and is used to adjust the working pressure of the airbag. The second pressure component is connected to the cavity and the vacuum adsorption component, and is used to adjust the working pressure of the sealed cavity space and the vacuum adsorption status of the sample.

[0009] Preferably, the detection component includes a first detection component and a second detection component. The first detection component includes a visual acquisition component for acquiring visual information of the sample and sensing the size of the sample's warpage. The second detection component includes a vacuum gauge for detecting the vacuum adsorption status of the sample substrate.

[0010] Preferably, the working pressure includes the working pressure of the airbag and the working pressure of the sealed cavity space; The working pressure range of the airbag is 1-20 atm, and the working pressure range of the sealed cavity is 1×10. -10 -1 atm, the working pressure adjustment rate of the airbag and the working pressure adjustment rate of the sealed cavity are both within 1×10 -3 -2atm / s; The operating temperature is 25-400 ℃, the heating rate is 0.5-30 ℃ / min, and the cooling rate is 0.1-15 ℃ / min.

[0011] To solve the above technical problems, another technical solution adopted by the present invention is: A warpage control method for packaging electronic devices, employing the stress relief device described above, includes the following steps: The sample is adsorbed onto the sample base using a vacuum adsorption assembly; The detection component collects information about the sample and transmits it to the control component; The control component receives information from the detection component, determines the type of residual stress in the sample, and selects the process parameters and steps of the temperature and pressure components based on the type of residual stress in the sample. The first chamber and the second chamber are closed to form a sealed cavity space, and the temperature component and the pressure component operate accordingly according to the selected process parameters and steps.

[0012] Preferably, the information collected by the detection component includes visual information of the sample, observation of the size of the sample warpage, detection of the vacuum adsorption status of the sample base, and detection of the degree of sample warpage.

[0013] Preferably, the control component receives information from the detection component to determine the type of residual stress in the sample. Specifically, this includes: when the control component receives visual information and observes that the sample warpage is within 1.5 mm ± 0.5 mm or exceeds 2 mm, and the sample base cannot absorb vacuum, the control component determines that the residual stress is curing shrinkage stress; when the control component receives visual information and observes that the sample warpage is within 1.5 mm ± 0.5 mm, and the sample base can absorb vacuum, the control component determines that the residual stress is thermal stress; when the control component receives visual information and observes that the sample warpage is less than 1 mm, and the sample can be absorbed by the sample base, the control component determines that the residual stress is interfacial residual stress.

[0014] Preferably, the process parameters and steps for selecting the temperature and pressure components based on the type of residual stress in the sample include: When the control component determines that the residual stress is curing shrinkage stress, the process parameters and steps for the temperature and pressure components are as follows: Stepwise heating to the curing temperature, divided into at least two stages, each stage held for 10-60 minutes; after curing, stepwise slow cooling to room temperature or B-stage temperature; applying constant contact pressure of 2-20 atm throughout the process, maintaining a vacuum environment in the chamber of less than 1×10⁻⁶ atm throughout. - 4 atm; heating rate of 0.5-30 ℃ / min, cooling rate of 0.1-15 ℃ / min; When the control component determines that the residual stress is thermal stress, the process parameters and steps for the temperature and pressure components are as follows: During rapid heating to the glass transition temperature, a controllable cooling rate of 0.1-5 ℃ / min is used to slowly cool to room temperature; a constant contact pressure of 2-20 atm is applied throughout the process, maintaining a vacuum environment in the chamber of less than 1×10⁻⁶ throughout. - 4 atm; heating rate between 0.5 and 30 ℃ / min; When the control component determines that the residual stress is interfacial residual stress, the process parameters and steps for the temperature and pressure components are as follows: The temperature is gradually increased to the material reaction temperature of 90-150 ℃, held for a period of time to allow sufficient contact between the media and pre-bonding, then increased to 200-350 ℃; then, it is slowly cooled to room temperature at a controllable rate of 0.1-5 ℃ / min; a constant contact pressure of 2-20 atm is applied throughout the process, and the cavity vacuum environment is maintained at less than 1×10⁻⁶ throughout the process. - 4 atm; heating rate between 0.5 and 30 ℃ / min; The constant contact pressure must be applied in stages. Before reaching the maximum pressure, there should be at least three stages, each with a controllable pressure increase rate of 0.05-2 atm / s and held for 0.1-5 minutes.

[0015] Due to the adoption of the above technical solutions, the present invention has the following advantages compared with the prior art: This invention relates to a stress relief device and a warpage control method for packaging electronic devices. Different warpage control methods are used according to different situations, so that warped samples can release stress quickly and efficiently in the most effective way, complete warpage leveling, and avoid affecting the process. Attached Figure Description

[0016] To more clearly illustrate the embodiments of this specification or the technical solutions in the prior art, the drawings used in the embodiments will be briefly introduced below. Obviously, the drawings described below are only some embodiments recorded in this specification. For those skilled in the art, other drawings can be obtained from these drawings without creative effort.

[0017] Figure 1 The process curve of this invention Figure 1 ; Figure 2 The process curve of this invention Figure 2 ; Figure 3 The process curve of this invention Figure 3 ; Figure 4 A schematic diagram of the stress relief device of the present invention; Figure 5 This is a flowchart of the warp control method of the present invention.

[0018] Wherein: 100, first cavity; 110, airbag; 200, second cavity; 210, sample base; 300, first temperature component; 400, second temperature component; 500, first air pressure component; 600, second air pressure component. Detailed Implementation

[0019] To make the above-mentioned objects, features, and advantages of the present invention more apparent and understandable, specific embodiments of the present invention will be described in detail below with reference to the accompanying drawings. Many specific details are set forth in the following description to provide a thorough understanding of the present invention. However, the present invention can be practiced in many other ways different from those described herein, and those skilled in the art can make similar modifications without departing from the spirit of the present invention. Therefore, the present invention is not limited to the specific embodiments disclosed below.

[0020] In the description of this invention, it should be understood that the terms "center," "longitudinal," "lateral," "length," "width," "thickness," "upper," "lower," "front," "rear," "left," "right," "vertical," "horizontal," "top," "bottom," "inner," "outer," "clockwise," "counterclockwise," "axial," "radial," and "circumferential" indicate the orientation or positional relationship based on the orientation or positional relationship shown in the accompanying drawings. They are used only for the convenience of describing this invention and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, or be constructed and operated in a specific orientation. Therefore, they should not be construed as limitations on this invention.

[0021] Furthermore, the terms "first" and "second" are used for descriptive purposes only and should not be construed as indicating or implying relative importance or implicitly specifying the number of technical features indicated. Thus, a feature defined as "first" or "second" may explicitly or implicitly include at least one of that feature. In the description of this invention, "a plurality of" means at least two, such as two, three, etc., unless otherwise explicitly specified.

[0022] It should be noted that when an element is referred to as being "fixed to" or "set on" another element, it can be directly on the other element or there may be an intervening element. When an element is considered to be "connected to" another element, it can be directly connected to the other element or there may be an intervening element. The terms "vertical," "horizontal," "upper," "lower," "left," "right," and similar expressions used herein are for illustrative purposes only and do not represent the only possible implementation.

[0023] "Multiple" means two or more, unless otherwise explicitly specified. " / " means "or".

[0024] Unless otherwise defined, all technical and scientific terms used herein have the same meaning as commonly understood by one of ordinary skill in the art to which this invention pertains. The terminology used herein in the description of the invention is for the purpose of describing particular embodiments only and is not intended to be limiting of the invention. The term "and / or" as used herein includes any and all combinations of one or more of the associated listed items.

[0025] Techniques, methods, and equipment known to those skilled in the art may not be discussed in detail, but where appropriate, such techniques, methods, and equipment should be considered part of the specification.

[0026] In the packaging process of semiconductor electronic components, internal stress is often introduced due to material or process parameters. When these stresses cannot be balanced, they manifest as warping on a macroscopic scale. Product warping can cause uneven thickness during "addition" (such as depositing metal / non-metal materials, laminating dry films, etc.) or "reduction" (etching / etching / resin removal, etc.) processes, thus affecting performance. When the product warping exceeds the limits of the process equipment, the product may even become impossible to hold, hold, or detect.

[0027] To eliminate stresses in the manufacturing process (such as thermal stress, curing shrinkage stress, and residual interface stress), it is necessary to precisely control the cavity temperature, contact air pressure, and operating time of the hot press equipment, thereby controlling product warpage during the packaging process.

[0028] Based on this, the present invention provides a stress relief device and a warpage control method for packaging electronic devices, wherein the stress relief device includes: A cavity, having a sealed cavity space, is used to place a warped sample; A temperature control unit, located inside the cavity, is used to regulate the operating temperature. The pneumatic assembly, connected to the cavity, is used to regulate the working pressure; A detection component, mounted on the cavity, is used to detect the warping state of the sample; The control component is connected to the temperature component, the pressure component, and the detection component respectively. It is used to receive information from the detection component and determine the type of residual stress in the sample, and then control the temperature component and the pressure component to perform warpage control process regulation.

[0029] The stress relief device of this invention enables warped samples to release stress quickly and efficiently, completing warping leveling and avoiding impact on the manufacturing process.

[0030] The following is in conjunction with the appendix Figure 1 - Appendix Figure 5 The present invention will be described in detail below with reference to specific embodiments.

[0031] As attached Figure 4 As shown, this embodiment provides a stress relief device for packaging electronic devices, including a cavity, a temperature component, a pressure component, a detection component, and a control component.

[0032] In this embodiment, the cavity has a sealed cavity space for placing a warped sample. The sample can be a wafer. Specifically, the cavity includes a first cavity 100 and a second cavity 200, which can be closed to form a sealed cavity space. This sealed cavity space can be pressurized / depressurized to regulate the pressure within it. The first cavity 100 includes an internally pressure-adjustable airbag 110, meaning the airbag 110 can be pressurized or depressurized to regulate the pressure within it. The airbag 110 is detachably connected to the first cavity 100. The second cavity 200 includes a sample base 210 for placing the warped sample. The sample base 210 is connected to a vacuum adsorption assembly, which adsorbs the sample onto the sample base 210.

[0033] In this embodiment, a temperature component is disposed within the cavity and is used to regulate the operating temperature. The temperature component may include a heater, a cooler, and a temperature sensor. The heater is used to increase the operating temperature, the cooler is used to decrease the operating temperature, and the temperature sensor is used to detect the operating temperature. Specifically, the temperature component includes a first temperature component 300 and a second temperature component 400. The first temperature component 300 is connected to the airbag 110 and is used to regulate the temperature of the airbag 110. The second temperature component 400 is connected to the sample base 210 and is used to regulate the temperature of the sample base 210.

[0034] In this embodiment, a pneumatic assembly is connected to the cavity and is used to regulate the working pressure. The pneumatic assembly includes a pressure boosting component, a pressure relief component, and a pressure sensor. The pressure boosting component increases the working pressure, the pressure relief component decreases the working pressure, and the pressure sensor detects the working pressure. Specifically, the pneumatic assembly includes a first pneumatic assembly 500 and a second pneumatic assembly 600. The first pneumatic assembly 500 is connected to the airbag 110 and is used to regulate the working pressure inside the airbag 110. The second pneumatic assembly 600 is connected to both the cavity and the vacuum adsorption assembly and is used to regulate the working pressure of the sealed cavity space (e.g., performing vacuum evacuation and vacuum breaking operations on the sealed cavity space) and the vacuum adsorption status of the sample (e.g., the vacuum adsorption and vacuum breaking status of the sample). The second pneumatic assembly 600 can be connected to both the cavity and the vacuum adsorption assembly via pipelines. Valves can be installed on the pipelines to allow for individual control of the pressure states of the cavity and the vacuum adsorption assembly.

[0035] In this embodiment, a detection component is disposed on the cavity to detect the warping state of the sample. Specifically, the detection component includes a first detection component and a second detection component. The first detection component is disposed on the first cavity 100 and includes a visual acquisition component for acquiring visual information about the sample, allowing for a direct perception of the magnitude of sample warping. Alternatively, the first detection component can be disposed outside the cavity and moved above the sample via a moving device to acquire visual information about the sample. The second detection component includes a vacuum gauge for detecting the vacuum adsorption status of the sample base 210, further detecting the degree of sample warping. Combining these two methods allows for the determination of the type of residual stress in the warped sample. The vacuum gauge can be a piezoresistive pressure sensor or other types.

[0036] In this embodiment, the working pressure includes the working pressure of the airbag 110 and the working pressure of the sealed cavity space. The working pressure range of the airbag is 1-20 atm, specifically 1 atm, 2 atm, 3 atm, 4 atm, 5 atm, 7 atm, 10 atm, 12 atm, 15 atm, 17 atm, and 19 atm. The working pressure range of the sealed cavity space is 1×10 -10 -1 atm. The working pressure adjustment rate of the airbag 110 and the working pressure adjustment rate of the sealed cavity space are both within 1×10. -3 -2 atm / s, specifically 1×10 -3 atm / s, 1×10 -2 atm / s, 0.1 atm / s, 0.3 atm / s, 0.5 atm / s, 0.7 atm / s, 1 atm / s, 1.3 atm / s, 1.5 atm / s, 1.7 atm / s, 1.8 atm / s.

[0037] The operating temperature is 25-400 ℃, and can also be 50-400 ℃, 50-350 ℃, 100-300 ℃, 120-280 ℃, 120-250 ℃, 120-200 ℃, 120-180 ℃, and 120-150 ℃.

[0038] The heating rate is 0.5-30 ℃ / min, and can also be 0.5-5 ℃ / min, 5-10 ℃ / min, 10-25 ℃ / min, 25-30 ℃ / min, 12-20 ℃ / min, 12-18 ℃ / min, or 13-16 ℃ / min.

[0039] The cooling rate is 0.1-15 ℃ / min, and can also be 0.5-15 ℃ / min, 1-13 ℃ / min, 3-11 ℃ / min, 5-10 ℃ / min, 5-9 ℃ / min, or 5-8 ℃ / min.

[0040] In this embodiment, the control component is signal-connected to the temperature component, the pressure component, and the detection component, respectively. It receives information from the detection component to determine the type of residual stress in the sample, and then controls the temperature and pressure components to regulate the warpage control process. For example, for warpage problems primarily caused by thermal stress, the key lies in the uniformity of the cooling rate and machine timing control; for warpage problems primarily caused by interfacial residual stress, the key lies in the pressure and machine timing control during heating; and for warpage problems primarily caused by curing shrinkage stress, the focus is more on the staged regulation of heating and cooling rates and pressure control. The control component can be a PLC (Programmable Logic Controller) or something else.

[0041] The present invention also provides a warpage control method for packaged electronic devices, employing the stress relief device described above, as shown in the attached diagram. Figure 5 As shown, the warpage control method includes the following steps: The sample is adsorbed onto the sample base using a vacuum adsorption assembly; The detection component collects information about the sample and transmits it to the control component; The control component receives information from the detection component, determines the type of residual stress in the sample, and selects the process parameters and steps for the temperature and pressure components based on the type of residual stress in the sample; the temperature and pressure components then perform corresponding operations according to the selected process parameters and steps.

[0042] In this embodiment, the information collected by the detection component includes visual information of the sample, observation of the size of the sample warping (such as judging the warping height through images), detection of the vacuum adsorption status of the sample base (such as detecting the actual vacuum level through a vacuum gauge, and the vacuum level value will be displayed on the software interface), and detection of the degree of sample warping.

[0043] In this embodiment, the control component receives information from the detection component and determines the type of residual stress in the sample. Specifically, when the control component receives visual information and observes that the sample warpage is within 1.5 mm ± 0.5 mm or exceeds 2 mm, and the sample base cannot absorb vacuum, the control component determines that the residual stress is curing shrinkage stress, which causes sample warpage. When the control component receives visual information and observes that the sample warpage is within 1.5 mm ± 0.5 mm, and the sample base can absorb vacuum, the control component determines that the residual stress is thermal stress, which causes sample warpage. When the control component receives visual information and observes that the sample warpage is less than 1 mm, and the sample can be absorbed by the sample base, the control component determines that the residual stress is interfacial residual stress, which causes sample warpage.

[0044] The specific explanation of the above judgment is as follows: Warpage is a quantitative indicator of macroscopic deformation after stress release. It is an indirect judgment based on macroscopically observable phenomena, and this correspondence was summarized by the applicant through a large amount of experimental data. Generally, curing shrinkage stress is the largest, followed by thermal stress, and interfacial residual stress is the smallest.

[0045] During the curing process, materials undergo volume shrinkage. If constrained, the release of these constraints after curing can generate significant internal stress, leading to severe warping of the sample, either overall or locally. Thermal stress arises from the mismatch in the thermal expansion coefficients of multilayer materials, causing warping due to temperature changes (such as cooling). Residual stress at interfaces typically originates from incomplete interfacial bonding or slight mismatches between materials, and its stress level is relatively low.

[0046] In this embodiment, the process parameters and steps for selecting the temperature and pressure components based on the type of residual stress in the sample include: When the control component determines that the residual stress is curing shrinkage stress and causes sample warping, the process parameters and steps for selecting the temperature and pressure components are as follows: Figure 1 The process involves a stepped heating to the curing temperature (which varies depending on the material, generally between 90-200 °C), divided into at least two stages, each held for 10-60 minutes. After curing, the material is slowly cooled to room temperature or the B-stage temperature in a stepped manner. A constant contact pressure of 2-20 atm is applied throughout the process, maintaining a vacuum environment in the chamber of less than 1 × 10⁻⁶. -4 atm; heating rate in the range of 0.5-30 ℃ / min, also in the ranges of 5-28 ℃ / min, 5-25 ℃ / min, 7-25 ℃ / min, 10-23 ℃ / min, 12-20 ℃ / min, 12-18 ℃ / min, 13-16 ℃ / min; cooling rate in the range of 0.1-15 ℃ / min, also in the ranges of 0.5-15 ℃ / min, 1-13 ℃ / min, 3-11 ℃ / min, 5-10 ℃ / min, 5-9 ℃ / min, 5-8 ℃ / min.

[0047] The constant contact pressure is the working pressure of the airbag, which can specifically be 1 atm, 2 atm, 3 atm, 4 atm, 5 atm, 7 atm, 10 atm, 12 atm, 15 atm, 17 atm, or 19 atm. The working pressure adjustment rate of both the airbag and the sealed cavity space is within 1×10⁻⁶. -3-2 atm / s, specifically 0.1 atm / s, 0.3 atm / s, 0.5 atm / s, 0.7 atm / s, 1 atm / s, 1.3 atm / s, 1.5 atm / s, 1.7 atm / s, and 1.8 atm / s.

[0048] The specific operation time for each of the above steps can be adjusted according to actual needs, and this application does not impose any restrictions on it.

[0049] When the control component determines that the residual stress is thermal stress and causes sample warping, the process parameters and procedures for selecting the temperature and pressure components are as follows: Figure 2 The diagram shows the process of rapidly heating to the glass transition temperature (which can be understood as within ±10 °C of the glass transition temperature), followed by slow cooling to room temperature at a controllable rate of 0.1-5 °C / min; a constant contact pressure of 2-20 atm is applied throughout the process, and the cavity vacuum environment is maintained at less than 1 × 10⁻⁶ throughout. -4 atm; heating rate is 0.5-30 ℃ / min, and can also be 5-28 ℃ / min, 5-25 ℃ / min, 7-25 ℃ / min, 10-23 ℃ / min, 12-20 ℃ / min, 12-18 ℃ / min, 13-16 ℃ / min.

[0050] The constant contact pressure is the working pressure of the airbag, which can specifically be 1 atm, 2 atm, 3 atm, 4 atm, 5 atm, 7 atm, 10 atm, 12 atm, 15 atm, 17 atm, or 19 atm. The working pressure adjustment rate of both the airbag and the sealed cavity space is within 1×10⁻⁶. -3 -2 atm / s, specifically 0.1 atm / s, 0.3 atm / s, 0.5 atm / s, 0.7 atm / s, 1 atm / s, 1.3 atm / s, 1.5 atm / s, 1.7 atm / s, and 1.8 atm / s.

[0051] The specific operation time for each of the above steps can be adjusted according to actual needs, and this application does not impose any limitations on it. When the control component determines that the residual stress is interfacial residual stress and causes sample warping, the process parameters and steps for selecting the temperature and pressure components are as follows. Figure 3The process involves a phased heating to the material reaction temperature, maintaining this temperature for a period to allow sufficient contact between the media and pre-bonding (e.g., initially heating to 90-150 °C and maintaining this temperature for a period to allow sufficient contact between the media (e.g., SiO2 / SiCN) and pre-bonding), then heating to 200-350 °C; followed by slow cooling to room temperature at a controllable rate of 0.1-5 °C / min; maintaining a constant contact pressure of 2-20 atm throughout the process, and ensuring a vacuum environment of less than 1 × 10⁻⁶ throughout the process. -4 atm; heating rate is 0.5-30 ℃ / min, and can also be 5-28 ℃ / min, 5-25 ℃ / min, 7-25 ℃ / min, 10-23 ℃ / min, 12-20 ℃ / min, 12-18 ℃ / min, 13-16 ℃ / min.

[0052] The constant contact pressure is the working pressure of the airbag, which can specifically be 1 atm, 2 atm, 3 atm, 4 atm, 5 atm, 7 atm, 10 atm, 12 atm, 15 atm, 17 atm, or 19 atm. The working pressure adjustment rate of both the airbag and the sealed cavity space is within 1×10⁻⁶. -3 -2 atm / s, specifically 0.1 atm / s, 0.3 atm / s, 0.5 atm / s, 0.7 atm / s, 1 atm / s, 1.3 atm / s, 1.5 atm / s, 1.7 atm / s, and 1.8 atm / s.

[0053] The specific operation time for each of the above steps can be adjusted according to actual needs, and this application does not impose any restrictions on it.

[0054] The application of constant contact pressure throughout the process must be done in stages. Before reaching the maximum pressure, there should be at least three stages, each with a controllable pressurization rate of 0.05-2 atm / s, and each stage should be maintained for 0.1-5 minutes. This operation can reduce the risk of product shifting caused by the contact airbag.

[0055] The technical features of the above embodiments can be combined in any way. For the sake of brevity, not all possible combinations of the technical features in the above embodiments are described. However, as long as there is no contradiction in the combination of these technical features, they should be considered to be within the scope of this specification.

[0056] The embodiments described above are merely illustrative of several implementations of the present invention, and while the descriptions are relatively specific and detailed, they should not be construed as limiting the scope of the invention patent. It should be noted that those skilled in the art can make various modifications and improvements without departing from the concept of the present invention, and these all fall within the protection scope of the present invention. Therefore, the protection scope of this invention patent should be determined by the appended claims.

Claims

1. A stress relief device for packaging electronic devices, characterized in that, include: A cavity, having a sealed cavity space, is used to place a warped sample; A temperature control unit, disposed within the cavity, is used to regulate the operating temperature; A pneumatic assembly, connected to the cavity, is used to regulate the working pressure; A detection component, disposed on the cavity, is used to detect the warping state of the sample; The control component is connected to the temperature component, the pressure component and the detection component respectively, and is used to receive information from the detection component and determine the type of residual stress in the sample, thereby controlling the temperature component and the pressure component to perform warpage control process regulation.

2. The stress relief device for packaging electronic devices according to claim 1, characterized in that, The cavity includes a first cavity and a second cavity, and the first cavity and the second cavity can be closed to form the sealed cavity space; The first cavity includes an airbag with adjustable internal pressure; The second cavity includes a sample base for placing a warped sample; The sample base is connected to a vacuum adsorption component, which adsorbs the sample onto the sample base.

3. The stress relief device for packaging electronic devices according to claim 1, characterized in that, The temperature assembly includes a heater, a cooler, and a temperature sensor. The heater is used to increase the operating temperature, the cooler is used to decrease the operating temperature, and the temperature sensor is used to detect the operating temperature.

4. The stress relief device for packaging electronic devices according to claim 2, characterized in that, The pneumatic assembly includes a pressurization assembly, a pressure relief assembly, and a pressure sensor. The pressurization assembly is used to increase the working pressure, the pressure relief assembly is used to reduce the working pressure, and the pressure sensor is used to detect the working pressure. The pneumatic assembly includes a first pneumatic assembly and a second pneumatic assembly. The first pneumatic assembly is connected to the airbag and is used to adjust the working pressure of the airbag. The second air pressure component is connected to the cavity and the vacuum adsorption component, and is used to adjust the working pressure of the sealed cavity space and the vacuum adsorption status of the sample.

5. The stress relief device for packaging electronic devices according to claim 2, characterized in that, The detection component includes a first detection component and a second detection component. The first detection component includes a visual acquisition component for acquiring visual information of the sample and sensing the size of the warp of the sample. The second detection component includes a vacuum gauge for detecting the vacuum adsorption status of the sample substrate.

6. The stress relief device for packaging electronic devices according to claim 2, characterized in that, The working pressure includes the working pressure of the airbag and the working pressure of the sealed cavity space; The working pressure range of the airbag is 1-20 atm, and the working pressure range of the sealed cavity is 1×10 atm. -10 -1 atm, the working pressure adjustment rate of the airbag and the working pressure adjustment rate of the sealed cavity space are both within 1×10. -3 -2 atm / s; The operating temperature is 25-400 ℃, the heating rate is 0.5-30 ℃ / min, and the cooling rate is 0.1-15 ℃ / min.

7. A warpage control method for packaged electronic devices, characterized in that, The warpage control method, using the stress relief device as described in any one of claims 1 to 6, comprises the following steps: The sample is adsorbed onto the sample base using a vacuum adsorption assembly; The detection component collects information about the sample and transmits it to the control component; The control component receives information from the detection component, determines the type of residual stress in the sample, and selects the process parameters and steps of the temperature component and the pressure component according to the type of residual stress in the sample. The first cavity and the second cavity are closed to form a sealed cavity space, and the temperature component and the air pressure component operate accordingly according to the selected process parameters and steps.

8. The warpage control method for packaged electronic devices according to claim 7, characterized in that, The information collected by the detection component includes visual information of the sample, observation of the size of the sample warpage, detection of the vacuum adsorption status of the sample base, and detection of the degree of sample warpage.

9. The warpage control method for packaged electronic devices according to claim 8, characterized in that, The control component receives information from the detection component to determine the type of residual stress in the sample. Specifically, this includes: when the control component receives visual information and observes that the sample warpage is within 1.5 mm ± 0.5 mm or exceeds 2 mm, and the sample base cannot absorb vacuum, the control component determines that the residual stress is curing shrinkage stress; when the control component receives visual information and observes that the sample warpage is within 1.5 mm ± 0.5 mm, and the sample base can absorb vacuum, the control component determines that the residual stress is thermal stress; when the control component receives visual information and observes that the sample warpage is less than 1 mm, and the sample can be absorbed by the sample base, the control component determines that the residual stress is interfacial residual stress.

10. The warpage control method for packaged electronic devices according to claim 9, characterized in that, The control component selects the process parameters and steps for the temperature and pressure components based on the type of residual stress in the sample, including: When the control component determines that the residual stress is curing shrinkage stress, the process parameters and steps for the temperature and pressure components are as follows: Stepwise heating to the curing temperature, divided into at least two stages, each stage held for 10-60 minutes; after curing, stepwise slow cooling to room temperature or B-stage temperature; applying constant contact pressure of 2-20 atm throughout the process, maintaining a vacuum environment in the chamber of less than 1×10⁻⁶ atm throughout the process. -4 atm; heating rate is 0.5-30 ℃ / min, cooling rate is 0.1-15 ℃ / min; When the control component determines that the residual stress is thermal stress, the process parameters and steps for the temperature and pressure components are as follows: During rapid heating to the glass transition temperature, a controllable cooling rate of 0.1-5 °C / min is used to slowly cool to room temperature; a constant contact pressure of 2-20 atm is applied throughout the process, maintaining a vacuum environment in the cavity of less than 1 × 10⁻⁶. -4 atm; heating rate is 0.5-30 ℃ / min; When the control component determines that the residual stress is interfacial residual stress, the process parameters and steps of the temperature and pressure components are as follows: The temperature is gradually increased to the material reaction temperature of 90-150 °C, held for a period of time to allow sufficient contact between the media and pre-bonding, then increased to 200-350 °C; then, the temperature is slowly cooled to room temperature at a controllable rate of 0.1-5 °C / min; a constant contact pressure of 2-20 atm is applied throughout the process, and the cavity vacuum environment is maintained at less than 1 × 10⁻⁶ throughout the process. -4 atm; heating rate is 0.5-30℃ / min; The constant contact pressure must be applied in stages. Before reaching the maximum pressure, there should be at least three stages, each with a controllable pressure increase rate of 0.05-2 atm / s and held for 0.1-5 minutes.