A lightweight, perforated suit chest lining and its manufacturing method

By employing a three-layer composite structure and precise zoned perforation and micro-adhesive coating processes, the problems of insufficient breathability and support in the chest lining of lightweight suits have been solved, achieving a balance between high breathability and three-dimensional shaping, making it suitable for the production of high-end lightweight suits.

CN123100896APending Publication Date: 2026-11-17BEIJING SMART GARMENTS
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611547291.5
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-10-08
Publication Date
2026-11-17

AI Technical Summary

Technical Problem

Existing lightweight suits have insufficient breathability in the chest lining, resulting in severe moisture and heat buildup. It is difficult to balance lightweight design with shaping and support. After multi-layer composite, the pores are easily blocked by the adhesive layer, leading to problems such as stuffiness, lack of breathability, insufficient support, and easy deformation when worn.

Method used

A three-layer differentiated lightweight substrate composite structure is adopted, combined with precise partitioned perforation, layered micro-coating, staggered composite, low temperature setting, and softening finishing processes to prepare a high-elasticity, lightweight suit chest lining with regular breathable holes. By setting an array of breathable micropores in areas with weak stress and high breathability requirements, and using a low-permeability micro-coating process, the adhesive layer is prevented from blocking the breathable holes.

Benefits of technology

It achieves ultimate breathability (breathability ≥550mm/s), takes into account three-dimensional shaping and structural stability, solves the problem of stuffiness when wearing in summer, has strong support and is not easy to collapse, and is suitable for the production needs of high-end lightweight suits.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123100896A_ABST
    Figure CN123100896A_ABST
Patent Text Reader

Abstract

This invention discloses a lightweight, perforated suit chest lining and its manufacturing method, belonging to the field of suit accessory processing technology. The method includes the following steps: providing and pre-treating three lightweight substrate layers: a breathable knitted outer layer, a high-elastic non-woven middle layer, and a flexible linen fiber thin inner layer; precisely perforating in designated areas, leaving the central support area perforated while arraying perforations in the outer breathable areas; applying a layered micro-adhesive coating using low-permeability modified polyurethane water-based hot melt adhesive only on one side of the non-perforated areas and pre-drying to semi-curing; staggered layered lamination, with the edges of the high-elastic non-woven middle layer recessed, and the three layers of breathable perforations aligned one-to-one before roller pressing; segmented low-temperature constant-temperature shaping; softening and finishing; and inspection and storage. This invention, through the synergy of zoned perforation and micro-adhesive coating to avoid the adhesive layer blocking the breathable pores, balances lightweight breathability, three-dimensional shaping, and structural stability. The finished product has an air permeability ≥550mm / s, suitable for the mass production of high-end lightweight formal wear and summer suits.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention belongs to the field of suit accessory processing technology, specifically relating to a lightweight perforated suit chest lining and its manufacturing method. Background Technology

[0002] The chest liner is the core structural material of a suit jacket, playing a crucial role in supporting the chest shape, ensuring fabric smoothness, and creating a three-dimensional silhouette. It directly determines the suit's feel and overall appearance. With the increasing popularity of lightweight and comfortable suits, traditional heavy chest liners can no longer meet market demands, and existing lightweight chest liners still have many technical shortcomings.

[0003] Currently, most lightweight suit chest linings on the market use a multi-layer thin-material composite process. While this optimizes thickness and weight, the adhesive layer easily blocks the breathable pores of the substrate during the multi-layer composite process. This significantly reduces the overall breathability of the chest lining, making it difficult for heat and moisture to dissipate in summer, leading to sweating, stickiness, and a stuffy feeling, resulting in extremely poor wearing comfort. Furthermore, existing breathable chest linings often have holes punched haphazardly throughout, without distinguishing between the support and breathable areas. This perforation easily damages the overall structural strength of the chest lining, resulting in insufficient chest support, sagging and deformation after long-term wear, and wrinkling and loosening of the fit, failing to meet the dual requirements of high breathability and durable shape retention. In addition, conventional perforation processes lack standardized parameters for hole diameter and spacing, making the edges prone to fraying and delamination after perforation, severely affecting the lifespan and fit of the chest lining.

[0004] In summary, existing technologies lack a manufacturing process for suit chest linings that features precise perforation in different areas, excellent breathability, stable structural strength, and a balance between lightweight and shapeability. This makes it impossible to meet the production and adaptation needs of high-end lightweight suits and breathable summer suits. Therefore, there is an urgent need to develop a manufacturing method for lightweight suit chest linings with perforations. Summary of the Invention

[0005] The purpose of this invention is to provide a lightweight, perforated suit chest lining and its manufacturing method, in order to solve the problems mentioned in the background art.

[0006] To achieve the above objectives, the embodiments of the present invention provide the following technical solutions:

[0007] A method for manufacturing a lightweight, perforated suit jacket chest lining includes the following steps:

[0008] Substrate pretreatment: Three lightweight substrates are provided, namely a breathable knitted lining on the surface, a high-elastic non-woven lining in the middle, and a flexible linen fiber lining at the bottom; the three lightweight substrates are ironed flat and dust and impurities are removed to obtain the pretreated three-layer substrates;

[0009] Precise perforation in zones: Using the pre-treated three-layer substrate as raw material, each layer of substrate is divided into a central stress support area and a breathable area located around the central stress support area. The central stress support area is not perforated, while the breathable area is perforated in an array matrix to form breathable holes. After perforation, the hole debris is cleaned to obtain the perforated three-layer substrate.

[0010] Layered micro-coating: Using three-layer substrates after perforation as raw materials, low-permeability modified polyurethane water-based hot melt adhesive is used to apply adhesive to the non-porous areas of the bonding surface of each substrate, except for the vent holes. After coating, the adhesive is pre-dried to make the adhesive layer semi-cured, thus obtaining the coated three-layer substrate.

[0011] Staggered layered composite: Using three layers of substrate after adhesive coating as raw materials, the layers are stacked from top to bottom in the order of breathable knitted lining, high-elastic non-woven lining in the middle layer, and flexible hemp fiber lining in the bottom layer. The edge of the high-elastic non-woven lining in the middle layer is recessed relative to the upper and lower substrate layers. The breathable holes of the three substrate layers correspond one-to-one. The composite is rolled and laminated to obtain a composite chest lining semi-finished product.

[0012] Low-temperature constant temperature setting: The composite chest lining semi-finished product is subjected to segmented low-temperature setting to obtain the set chest lining;

[0013] Softening and finishing process: After the shaped chest lining is cooled, the four sides are sanded and rounded, the whole body is softened and kneaded, and then cut and shaped according to the pattern to obtain the chest lining blank;

[0014] Finished product inspection and storage: The chest lining blanks are inspected, qualified products are selected and stored, resulting in a lightweight, perforated suit chest lining.

[0015] Furthermore, the surface breathable knitted lining is a 75D / 144F polyester fiber knitted fabric with a warp and weft density of 120*90 and a weight of 110±5g / m². 2 The intermediate high-elastic nonwoven lining consists of 60-70 wt% polyester and 30-40 wt% viscose spunlace nonwoven lining, with a basis weight of 90 ± 5 g / m². 2 The underlying flexible linen lining is a blend of 45-55 wt% linen and 45-55 wt% cotton, with a basis weight of 80 ± 5 g / m². 2 The thickness of each substrate is 0.15-0.25mm;

[0016] The ironing temperature for smooth ironing is 80-90℃, the ironing speed is 3-5m / min, and the pressure of the hot press roller is 0.1-0.3MPa. The dust removal and impurity removal adopts an electrostatic brush dust removal and impurity removal unit with a brush rotation speed of 100-150r / min, and is coordinated with a negative pressure dust collection fan.

[0017] Furthermore, the central stress-supporting area is rectangular, the outer contour of the chest lining is (470-490)mm×(350-370)mm, the central stress-supporting area is (230-250)mm×(310-330)mm, its left and right boundaries are 110-130mm away from the left and right outer edges of the chest lining, respectively, and its upper and lower boundaries are 15-25mm away from the top and bottom outer edges of the chest lining, respectively. The area of ​​the central stress-supporting area accounts for 42%-46% of the total area of ​​the chest lining, and the area of ​​the breathable area accounts for 54%-58%.

[0018] Furthermore, the diameter of the array-type matrix punching is 0.8-1.2mm, the hole spacing is 8-12mm, and the punching speed is 200-300 times / min; after punching, the hole debris is cleaned by blowing with a high-pressure airflow of 0.05-0.15MPa; at the same time as punching, a reference positioning hole with a diameter of 1.5-2.5mm is reserved on the side of the substrate.

[0019] Furthermore, the softening point of the low-permeability modified polyurethane waterborne hot melt adhesive is 52-58℃, the dry single-layer peel strength is ≥11N / 5cm, the solid content is 42±2%, the adhesive layer penetration depth is ≤0.01mm, and the elastic elongation after curing is ≥350%.

[0020] Furthermore, the layered single-sided adhesive coating employs either CCD vision-controlled point-to-point adhesive coating or perforated mask roller coating. CCD vision-controlled point-to-point adhesive coating scans the coordinates of the ventilation holes in real time and releases adhesive only at fixed points in non-hole areas, with adhesive dots diameters of 0.5-0.7 mm and dot spacing of 4-6 mm. Perforated mask roller coating uses a metal perforated mask roller matched to the arrangement of the ventilation holes, ensuring that the adhesive is transferred only to non-hole areas. The adhesive application rate is 8-12 g / m². 2 The adhesive layer thickness is 0.02-0.05mm; the pre-drying temperature is 60-70℃, the pre-drying time is 2-3min, and the hot air velocity is 1.1-1.3m / min; the semi-cured state meets the following requirements: the degree of curing of the adhesive layer is 45%-55%, the initial tack of the adhesive surface is 0.8-1.5N / 25mm, and the adhesive film is intact and does not flow.

[0021] Furthermore, the edge of the middle layer high-elastic nonwoven lining is recessed by 1-2mm relative to the upper and lower substrate layers; the alignment of the ventilation holes of the three substrate layers is achieved by coarse positioning with side reference positioning holes and fine adjustment with CCD vision servo, with an alignment deviation of ≤0.1mm; the roll pressing composite is achieved by a double roll press with a roll pressing pressure of 0.3-0.5MPa and a roll pressing speed of 4-6m / min.

[0022] Furthermore, the segmented low-temperature setting includes a first stage of preheating and a second stage of curing; the temperature of the first stage of preheating is 75-80℃ and the time is 2-4 min; the temperature of the second stage of curing is 85-90℃ and the time is 4-6 min; the setting tension is 5-8 N.

[0023] Furthermore, the cooling process involves: standing at 20-25℃ for 5-15 minutes; rounding the four sides using a belt sander with a 1000-1500 mesh ultrafine alumina sander belt, a belt speed of 5-7 m / min, a sanding pressure of 0.05-0.15 MPa, and a corner radius of 1.5-2.5 mm; and overall softening and kneading using a horizontal silicone buffer kneading machine, with a kneading frequency of 20-30 times / min, a reciprocating stroke of 11-13 cm, and a processing time of 1-3 minutes.

[0024] Another object of the present invention is to provide a lightweight, perforated suit chest lining manufactured using the above-described method.

[0025] The present invention provides a method for manufacturing a lightweight, perforated suit chest lining. Through a combination of zoned perforation and micro-adhesive application to avoid blocking the ventilation pores, it balances lightweight breathability, three-dimensional shaping, and structural stability, achieving a finished product air permeability ≥550mm / s. The process parameters of this invention are precisely controllable, resulting in a high finished product yield, making it suitable for the large-scale production of high-end lightweight formal wear and summer casual suits. Compared with existing technologies, this invention has the following advantages:

[0026] 1. Extremely breathable and eliminates stuffiness: This invention adopts a substrate partition array perforated structure, combined with a micro-coating process without pore blockage, to form a through-type three-dimensional breathable channel; the finished product has a breathability rate of ≥550mm / s, which is more than 80% higher than that of traditional non-porous thin chest linings. It can quickly dissipate the humid heat generated when wearing the chest, completely solving the pain points of stuffiness and sticky sweat in summer, and greatly improving wearing comfort.

[0027] 2. Balancing Breathability and Shaping: This invention employs a fixed-size, zoned perforation design. The chest lining features a rectangular core support area, with its four sides 120mm from the lining edge on the left and right, and 20mm from the top and bottom, covering 44.4% of the total area. This area fully covers the chest peak, placket, and shoulder support points, preserving excellent three-dimensional support and anti-sag performance. The remaining 55.6% is precisely perforated around the perimeter for ventilation and heat dissipation, addressing areas of heat accumulation such as the armpits and sides of the chest. This overcomes the shortcomings of traditional perforated chest linings, which suffer from insufficient support and are prone to deformation and collapse. After 500 cycles of testing, there was no collapse or deformation, achieving a perfect balance between high breathability and durable shaping.

[0028] 3. Lightweight and soft, comfortable to wear: It adopts a three-layer precise weight ratio ultra-thin substrate composite and low temperature flexible shaping process, without hard adhesive layer and heavy substrate; combined with the processed smooth and burr-free microporous structure, the chest pad has excellent overall flexibility, and the human body can rotate and raise its arms without restriction of movement, and it is suitable for various slim and lightweight suit styles.

[0029] 4. Stable structure and high durability: Standardized and precise drilling process ensures that the hole edges are flat without tearing or delamination; combined with low-permeability modified polyurethane hot melt adhesive, the adhesive layer has a moderate softening point and high peel strength; combined with CCD vision / cutout masking two hole-avoiding adhesive application processes, the adhesive will not block the breathable micropores; staggered composite and segmented low-temperature shaping process eliminate internal stress; after bending resistance test, the holes do not deform, block, or delaminate after 500 cycles of bending, and the pattern has good durability.

[0030] 5. Controllable process and adaptable to mass production: All processes are equipped with standardized industrial equipment. The parameters of drilling, gluing, and shaping are quantifiable and controllable. All performance indicators of the finished product can be reproduced and verified through national standard testing methods. The finished product has high stability and high pass rate. No complex high-end customized equipment is required. It can be adapted to large-scale industrial production, with controllable production costs and wide market adaptability. Attached Figure Description

[0031] Figure 1 This is a flowchart illustrating the manufacturing method of a lightweight, perforated suit chest lining provided in an embodiment of the present invention.

[0032] Figure 2 This is a schematic diagram of the overall layer structure and perforation arrangement of the lightweight perforated suit chest lining obtained by the present invention; in the figure, 1-the outer breathable knitted lining, 2-the middle high-elastic non-woven lining, 3-the bottom flexible linen fiber thin lining, 4-micro-adhesive composite layer.

[0033] Figure 3 This is a bar chart comparing the breathability and overall performance of the present invention with that of traditional chest linings. Detailed Implementation

[0034] The technical solutions of the present invention will be clearly and completely described below with reference to the embodiments of the present invention. Obviously, the described embodiments are only some embodiments of the present invention, and not all embodiments. Based on the embodiments of the present invention, all other embodiments obtained by those of ordinary skill in the art without creative effort are within the scope of protection of the present invention.

[0035] In one embodiment of the present invention, a method for manufacturing a lightweight, perforated suit chest lining is provided. This method addresses the technical shortcomings of existing lightweight suit chest linings, such as insufficient breathability, severe moisture and heat buildup, difficulty in balancing lightweight design and shaping support, and the tendency for pores to be blocked by adhesive layers after multi-layer composite construction. It employs a three-layer differentiated lightweight substrate composite structure, combined with a precise zoned perforation, layered micro-adhesive coating, staggered composite, low-temperature setting, and softening finishing integrated process to prepare a highly elastic, lightweight suit chest lining with regularly spaced breathable perforations. By setting an array of breathable micropores in areas of the chest lining with low stress and high breathability requirements, while avoiding perforation in key stress-supporting areas, and using a low-permeability micro-adhesive coating process, the present invention completely solves the problems of stuffiness, lack of breathability, and stickiness associated with traditional chest linings, while retaining the excellent three-dimensional shaping and wrinkle-resistant resilience of the chest lining, effectively balancing breathability, lightweight, and structural stability.

[0036] Specifically, such as Figure 1 and Figure 2 As shown, the manufacturing method provided in this embodiment of the invention includes the following steps:

[0037] S1. Substrate Pretreatment: Three lightweight substrates are provided: a breathable knitted lining 1 on the surface, a high-elastic non-woven lining 2 in the middle, and a flexible linen fiber thin lining 3 at the bottom. The thickness of each substrate is controlled between 0.15-0.25mm, and the total thickness of the substrate does not exceed 0.7mm. A continuous flatbed hot ironing machine (textile ironing machine) is used to iron and flatten the three substrates respectively. The ironing temperature is 80-90℃, the ironing speed is 3-5m / min, and the hot pressure roller pressure is 0.1-0.3MPa. This thoroughly removes wrinkles and residual internal stress from the substrate, ensuring a smooth and regular surface. After ironing, an electrostatic brush dust removal and impurity removal unit is connected. The brush speed is 100-150r / min, and a negative pressure dust collection fan is used to remove fiber debris and dust impurities from the substrate surface. This prevents impurities from clogging the punching mold and affecting the subsequent punching accuracy and composite bonding effect, resulting in the pretreated three-layer substrate.

[0038] The outer breathable knitted lining 1 is made of 75D / 144F polyester fiber knitted fabric with a warp and weft density of 120*90 (120 threads / inch × 90 threads / inch) and a weight of 110±5g / m². 2 According to GB / T 5453, the air permeability is ≥300mm / s, it is thin and porous, and can quickly wick away moisture; the middle layer high-elastic nonwoven lining 2 is composed of 60-70wt% polyester and 30-40wt% viscose spunlace nonwoven lining, with a basis weight of 90±5g / m². 2 According to GB / T 3923.1, the elongation at break is ≥40%, exhibiting excellent resilience and support, and is not easily collapsed or deformed; the bottom flexible linen fiber lining 3 is a 45-55wt% linen and 45-55wt% cotton blend lining, with a basis weight of 80±5g / m². 2Each base material has a thickness of 0.15-0.25mm, combining the moisture-wicking and breathable properties of natural linen with the soft and conforming characteristics of cotton fibers, optimizing the fit and feel of the chest lining against the human body fabric.

[0039] S2, Precise Drilling in Zones: Using the pre-treated three-layer substrate as raw material, each layer of substrate is divided into a central stress support area and a breathable area located around the central stress support area. The central stress support area is not drilled, while the breathable area is formed by array-matrix drilling to create breathable holes. After drilling, the hole debris is cleaned to obtain the drilled three-layer substrate.

[0040] Specifically, the three pre-treated substrate layers are perforated in a zoned array pattern. Based on the stress characteristics of the suit's chest lining, support and ventilation zones are divided: the central support area of ​​the chest lining is left unperforated to preserve structural strength and ensure the garment's support effect; the ventilation zones around the chest lining and under the armpits are perforated using an array pattern. The perforation diameter is 0.8-1.2mm, and the hole spacing is 8-12mm, arranged evenly in a matrix. High-speed precision punching equipment is used, with a punching speed of 200-300 times / min, ensuring smooth, burr-free hole edges and no substrate delamination or tearing. After perforation, a 0.05-0.15MPa high-pressure airflow is used to blow away debris from the holes, ensuring complete permeability. Simultaneously, reference positioning holes with a diameter of 1.5-2.5mm are pre-drilled on the side of the substrate.

[0041] The central support area is rectangular, the outer contour of the chest liner is (470-490)mm×(350-370)mm, the central support area is (230-250)mm×(310-330)mm, its left and right boundaries are 110-130mm away from the left and right outer edges of the chest liner, respectively, and its upper and lower boundaries are 15-25mm away from the top and bottom outer edges of the chest liner, respectively. The area of ​​the central support area accounts for 42%-46% of the total area of ​​the chest liner, and the area of ​​the breathable area accounts for 54%-58%.

[0042] Preferably, for a standard 480mm×360mm chest pad, with the geometric center of the chest pad as the origin (X0, Y0), the rectangular boundary dimensions of the support area are: 240mm horizontal width and 320mm vertical height; the left boundary of the support area is 120mm from the outer left edge of the chest pad; the right boundary of the support area is 120mm from the outer right edge of the chest pad; the upper boundary of the support area is 20mm from the outer top edge of the chest pad; the lower boundary of the support area is 20mm from the outer bottom edge of the chest pad; corresponding points on the human body: the support area completely covers the area from below the clavicle to above the waist, including the chest peak stress point, the shoulder-chest connection stress point, and the front center placket support stress band, which is the core load-bearing area for suit shaping, and completely retains the non-porous structure of the base material to ensure long-term anti-collapse and three-dimensional shaping effect; area ratio: support area = 240mm × 320mm = 76800mm 2Total area of ​​chest lining = 480 × 360 = 172800 mm 2 The area of ​​the support zone accounts for 44.4% of the total chest lining area.

[0043] The entire area surrounding the support zone is a breathable zone, including the corresponding area under the left armpit, the corresponding area under the right armpit, the side area of ​​the top shoulder seam, and the side area of ​​the bottom hem. The total area of ​​the breathable zone accounts for 55.6% of the overall area of ​​the chest lining, covering the areas under the armpits where sweat is easily produced and the sides of the chest where moisture and heat accumulate. It is used to quickly dissipate heat and moisture, ensuring maximum breathability without compromising the overall structural strength of the chest lining.

[0044] S3, Layered Micro-coating: Using the three-layer substrate after drilling as raw material, low-permeability modified polyurethane water-based hot melt adhesive is used to apply layered single-sided adhesive to the non-porous areas of the bonding surface of each substrate except for the air pores. After coating, the adhesive layer is pre-dried to make the adhesive layer semi-cured, forming a micro-adhesive composite layer 4, and the three-layer substrate after coating is obtained.

[0045] Among them, the low-permeability modified polyurethane waterborne hot melt adhesive (model WPU-826) has a softening point of 52-58℃, a dry single-layer peel strength of ≥11N / 5cm, a solid content of 42±2%, an adhesive layer penetration depth of ≤0.01mm, and an elastic elongation of ≥350% after curing. After curing, this hot melt adhesive has high elasticity, high air permeability, and low permeability, without hard adhesive lumps, ensuring the overall flexibility and pore permeability of the chest lining.

[0046] WPU-826 is a mixture of Dispercoll Covestro's U53 and U64; specifically, it uses U53 (softening temperature 50-60℃) as the main component, blended with 10-20wt% U64 (42% solids content, good film-forming properties at room temperature), which can simultaneously adjust the softening point to the 52-58℃ range and the solids content to around 42%. Dispercoll U53 / U64 is a linear thermoplastic PUD, which, although soft after film formation, has limited water resistance, dry cleaning resistance, and peel strength.

[0047] WPU-826 can also incorporate Covestro's Bayhydur (a water-dispersible isocyanate crosslinking agent). The NCO groups react with the hydroxyl groups in the PUD to crosslink, "locking" the linear molecular chains into a network structure, which can improve dry / wet peel strength, water washability, dry cleaning resistance, and heat creep resistance. It should be noted that adding too much Bayhydur will cause the film to harden and the elongation to decrease, so the amount added must be controlled. Generally, adding 2-5 wt% Bayhydur can improve water washability and peel strength to ≥11 N / 5 cm.

[0048] The layered single-sided adhesive coating employs an independently selectable precision hole-avoiding adhesive coating process: CCD vision-controlled point-to-point adhesive coating or perforated mask roller coating. This achieves single-sided micro-adhesive coating only in non-porous areas of the substrate, fundamentally preventing adhesive flow and blockage of breathable micropores, unlike traditional full-width thick adhesive coating processes. Layered single-sided micro-adhesive coating is applied to the perforated substrate to avoid the adhesive layer blocking the breathable pores. Specifically, CCD vision-controlled point-to-point adhesive coating scans the coordinates of the breathable pores in real time and releases adhesive only at fixed points in non-porous areas, with adhesive dots diameters of 0.5-0.7mm and dot spacing of 4-6mm. Perforated mask roller coating uses a metal perforated mask roller matched to the arrangement of the breathable pores, ensuring that the adhesive is transferred only to non-porous areas. Specifically, an adhesive layer is uniformly coated on the non-porous areas of the lower surface of the surface breathable knitted lining 1, the upper and lower surfaces of the middle high-elastic nonwoven lining 2, and the upper surface of the bottom flexible hemp fiber thin lining 3, with the adhesive amount controlled at 8-12g / m². 2 The adhesive layer thickness is 0.02-0.05mm, forming a micro-adhesive composite layer 4. The pre-drying temperature is 60-70℃, the pre-drying time is 2-3min, and the hot air velocity is 1.1-1.3m / min, so that the adhesive layer forms a semi-cured state, avoiding adhesive overflow and clogging of pores during lamination. The quantitative judgment standard for the semi-cured state (which can be detected online) is as follows: the degree of cross-linking curing of the adhesive layer detected by Fourier transform infrared spectroscopy is 45%-55%, with an optimal degree of curing of 50%. The initial tack of the adhesive surface is tested using a GB / T 4851-2021 tape initial tack tester, and the initial tack of the adhesive surface is 0.8-1.5N / 25mm. There is only a slight tackiness when lightly touched with a finger, with no adhesive stringing or sticky transfer. The adhesive film is intact and does not flow, with no liquid overflow. There is no risk of sticking to rollers at room temperature, and it can be remelted and bonded to the substrate during hot pressing. Meeting the above three indicators is considered a qualified semi-cured state, avoiding adhesive overflow and clogging of pores during lamination.

[0049] S4. Staggered Layered Composite: Using the three-layer substrate after adhesive coating as raw material, the layers are stacked from top to bottom in the following order: breathable knitted lining 1, high-elastic non-woven lining 2, and flexible linen fiber thin lining 3. The edge of the high-elastic non-woven lining 2 is recessed relative to the upper and lower substrate layers. The breathable holes of the three substrate layers correspond one-to-one and are completely aligned without any misalignment or obstruction. After the stacking is completed, the layers are rolled and laminated at a uniform speed to obtain a composite chest lining semi-finished product.

[0050] Specifically, the edge of the middle layer high-elastic non-woven lining 2 is recessed by 1-2mm relative to the upper and lower substrate layers to avoid the thickening of the edges of multiple adhesive layers and eliminate the defects of thick and hardened chest lining edges; the alignment of the ventilation holes of the three substrate layers adopts coarse positioning with side reference positioning holes and fine adjustment with CCD vision servo, with an alignment deviation of ≤0.1mm; the roll pressing composite adopts a double roll press with a roll pressing pressure of 0.3-0.5MPa and a roll pressing speed of 4-6m / min to ensure that each substrate layer is tightly bonded, without bubbles or delamination, and that the holes remain transparent throughout the process.

[0051] S5. Low-temperature constant temperature shaping: The composite chest lining semi-finished product is shaped in sections at low temperature to avoid high temperature damage to the elasticity of the substrate and cause the pores to shrink and deform. At the same time, it prevents the adhesive layer from overflowing and blocking the micropores, thus obtaining the shaped chest lining.

[0052] Specifically, the segmented low-temperature setting includes a first stage of preheating and a second stage of curing. The first stage of preheating is at a temperature of 75-80℃ for 2-4 minutes to slowly release the composite stress. The second stage of curing is at a temperature of 85-90℃ for 4-6 minutes to achieve stable curing of the adhesive layer. During the setting process, flat tension is maintained, and the tension is controlled at 5-8N to prevent the chest lining from shrinking and the holes from deforming, ensuring that the substrate layers are stably bonded and that the breathable pores are intact and permeable.

[0053] S6. Softening and finishing process: Cool the shaped chest lining, then grind the four sides to round the corners (remove hard edges, burrs and residual debris from punching), soften and knead the whole chest lining (eliminate the internal composite stress of the chest lining, improve the overall flexibility and wrinkle resistance, and at the same time repair the fine rough edges of the holes), and cut and shape it according to the pattern to obtain a regular perforated chest lining blank.

[0054] Specifically, the cooling process involves standing at 20-25℃ for 5-15 minutes; the four sides are polished and rounded using a belt sander with a 1000-1500 mesh ultrafine alumina sander belt, at a belt speed of 5-7 m / min, a sanding pressure of 0.05-0.15 MPa, and a rounded corner radius of 1.5-2.5 mm; the overall softening and kneading process uses a horizontal silicone buffer kneading machine, with a kneading frequency of 20-30 times / min, a silicone bump roller reciprocating stroke of 11-13 cm, and a processing time of 1-3 minutes.

[0055] S7. Finished Product Inspection and Storage: Inspect the chest lining blanks, select qualified products and store them to obtain lightweight, perforated suit chest linings.

[0056] Specifically, the repaired chest lining undergoes comprehensive performance testing, including indicators such as substrate thickness, overall weight, pore permeability, breathability, resilience, interlayer bonding strength, and structural resistance to deformation. Qualified products without delamination, wrinkles, pore blockage, or deformation are selected and stacked flat for storage, completing the preparation of the lightweight, perforated suit chest lining. A complete set of national standard testing methods and qualification thresholds are applied: thickness, weight, breathability, pore permeability, peel strength, flexural strength, and resilience.

[0057] In practical applications, comprehensive performance testing is conducted on the modified chest lining. The testing indicators, corresponding national standards, standard-specified test conditions, and pass / fail thresholds are fully matched as follows:

[0058] 1. Substrate thickness and overall areal density; Standards GB / T 3820-1997 "Determination of Thickness of Woven Textiles" and GB / T 4669-2008 "Determination of Unit Area Mass of Woven Textiles"; Test conditions: Temperature 23℃, relative humidity 65%, conditioned at standard atmosphere for 24 hours; Thickness measurement pressure weight 5kPa; Acceptable thresholds: Single-layer substrate thickness 0.15-0.25mm, total thickness of three-layer composite ≤0.7mm, overall areal density of finished product ≤85g / m³ 2 .

[0059] 2. Pore permeability; Test method: Self-made airflow sealing fixture, stable air pressure of 0.1MPa, the fixture completely seals the non-breathable area of ​​the chest lining, and only the breathable area allows airflow; Judgment criteria: airflow rate ≥99%, with no pore blockage or fiber blockage causing airflow attenuation.

[0060] 3. Air permeability (core indicator); Standard: GB / T 5453-1997 "Textiles - Determination of Air Permeability of Fabrics"; Test conditions: Sample area 20cm² 2 Pressure difference 100Pa, 23℃, 65% RH conditioning for 24h; Qualified threshold: Overall air permeability of finished product ≥550mm / s.

[0061] 4. Resilience (Elongation at Break Recovery Rate); Standard: GB / T 3923.1-2013 "Textiles - Tensile Properties of Fabrics - Part 1: Determination of Breaking Strength and Elongation at Break (Strip Method)"; Test conditions: Specimen width 50mm, tensile clamping distance 100mm, tensile speed 100mm / min, stretched to 40% elongation, held for 10s and unloaded, left to stand for 30s to measure residual elongation; Pass threshold: Elastic recovery rate ≥95%.

[0062] 5. Interlayer bonding strength (dry peel strength); Standard: GB / T 2660-2017 "Shirts" Fuse interlining peel strength test clause; Test conditions: Sample width 50mm, tensile speed 100mm / min, 23℃ room temperature dry state; additionally, a retest is conducted after 5 steam ironing cycles; Pass threshold: room temperature dry peel strength ≥9N / 5cm; after 5 steam ironing cycles, peel strength ≥7N / 5cm, with no local delamination.

[0063] 6. Bending life (bending resistance and deformation resistance); Standard: FZ / T 01088-2020 "Textile Fabrics Bending Resistance Test" Test conditions: Bending pressure 2N, reciprocating bending frequency 30 times / min, sample width 30mm; Pass threshold: 500 consecutive reciprocating bends without delamination, hole tearing, or chest lining collapse deformation.

[0064] 7. Visual inspection of appearance; full-width visual inspection: no delamination, no wrinkles, no blocked holes, no edge deformation, no perforated burrs. Select qualified products that meet all indicators, lay them flat, cover them with film for isolation, stack and store them in a constant temperature and humidity warehouse (23℃, 65%RH) to complete the preparation of the lightweight perforated suit chest lining.

[0065] In the embodiments of the present invention, the materials, reagents or equipment used, unless otherwise specified by the manufacturer, are all conventional products that can be purchased commercially.

[0066] Example 1: This example provides a method for manufacturing a lightweight, perforated suit chest lining, specifically including the following steps:

[0067] S1. Substrate Pretreatment: Three lightweight substrates are provided: a breathable knitted lining 1 on the surface, a high-elastic non-woven lining 2 in the middle, and a flexible linen fiber thin lining 3 at the bottom. The thickness of each substrate is controlled at 0.2mm, and the total thickness of the substrate is 0.6mm. A continuous flatbed hot ironing machine (textile ironing machine) is used to iron and flatten the three substrates respectively. The ironing temperature is 85℃, the ironing speed is 4m / min, and the hot pressure roller pressure is 0.2MPa to thoroughly remove wrinkles and residual internal stress from the substrate, ensuring that the substrate surface is flat and regular. After ironing, an electrostatic brush dust removal and impurity removal unit is connected. The brush speed is 1020r / min, and a negative pressure dust collection fan is used to remove fiber debris and dust impurities from the substrate surface to avoid impurities clogging the punching mold and affecting the subsequent punching accuracy and composite bonding effect, thus obtaining the pretreated three-layer substrate.

[0068] The outer breathable knitted lining 1 is made of 75D / 144F polyester fiber knitted fabric with a warp and weft density of 120*90 (120 threads / inch × 90 threads / inch) and a weight of 110g / m². 2 According to GB / T 5453, the air permeability is ≥300mm / s, it is thin and porous, and can quickly wick away moisture; the middle layer high-elastic nonwoven lining 2 is composed of 65wt% polyester and 35wt% viscose spunlace nonwoven lining, with a basis weight of 90g / m². 2 According to GB / T 3923.1, the elongation at break is ≥40%, exhibiting excellent resilience and support, and is not easily collapsed or deformed; the bottom flexible linen fiber lining 3 is a 50wt% linen and 50wt% cotton blend lining with a weight of 80g / m². 2 .

[0069] S2, Precise Drilling in Zones: Using the pre-treated three-layer substrate as raw material, each layer of substrate is divided into a central stress support area and a breathable area located around the central stress support area. The central stress support area is not drilled, while the breathable area is formed by array-matrix drilling to create breathable holes. After drilling, the hole debris is cleaned to obtain the drilled three-layer substrate.

[0070] Specifically, the three pre-treated substrate layers are perforated in a zoned array pattern. Based on the stress characteristics of the suit's chest lining, support and ventilation zones are divided: the central support area of ​​the chest lining is left unperforated to preserve structural strength and ensure the garment's support effect; the ventilation zones around the chest lining and under the armpits are perforated using an array pattern. The perforation diameter is 1.0mm, the hole spacing is 10mm, and a uniform matrix arrangement is used. High-speed precision punching equipment is used, with a punching speed of 250 times / min, ensuring smooth, burr-free hole edges and no substrate delamination or tearing. After perforation, 0.1MPa high-pressure airflow is used to clean debris from the holes, ensuring complete permeability. Simultaneously, a 2mm diameter reference positioning hole is pre-drilled on the side of the substrate.

[0071] For a standard 480mm×360mm chest pad, with the geometric center of the chest pad as the origin (X0,Y0), the rectangular boundary dimensions of the support area are: 240mm horizontal width and 320mm vertical height; the left boundary of the support area is 120mm from the outer left edge of the chest pad; the right boundary of the support area is 120mm from the outer right edge of the chest pad; the upper boundary of the support area is 20mm from the outer top edge of the chest pad; the lower boundary of the support area is 20mm from the outer bottom edge of the chest pad; corresponding points on the human body: the support area completely covers the area from below the clavicle to above the waist, including the chest peak stress point, the shoulder-chest connection stress point, and the front center placket support band. It is the core load-bearing area for suit shaping, and the non-porous structure of the base material is fully preserved to ensure long-term anti-collapse and three-dimensional shaping effect; area ratio: support area = 240mm×320mm = 76800mm 2 Total area of ​​chest lining = 480 × 360 = 172800 mm 2 The area of ​​the support zone accounts for 44.4% of the total chest lining area.

[0072] The entire area surrounding the support zone is a breathable zone, including the corresponding area under the left armpit, the corresponding area under the right armpit, the side area of ​​the top shoulder seam, and the side area of ​​the bottom hem. The total area of ​​the breathable zone accounts for 55.6% of the overall area of ​​the chest lining, covering the areas under the armpits where sweat is easily produced and the sides of the chest where moisture and heat accumulate. It is used to quickly dissipate heat and moisture, ensuring maximum breathability without compromising the overall structural strength of the chest lining.

[0073] S3, Layered Micro-coating: Using the three-layer substrate after drilling as raw material, low-permeability modified polyurethane water-based hot melt adhesive is used to apply layered single-sided adhesive to the non-porous areas of the bonding surface of each substrate except for the air pores. After coating, the adhesive layer is pre-dried to make the adhesive layer semi-cured, forming a micro-adhesive composite layer 4, and the three-layer substrate after coating is obtained.

[0074] Among them, the low-permeability modified polyurethane waterborne hot melt adhesive (model WPU-826) has a softening point of 55℃, a dry single-layer peel strength of 12N / 5cm, a solid content of 42%, an adhesive layer penetration depth of ≤0.01mm, and an elastic elongation of ≥350% after curing. After curing, this hot melt adhesive has high elasticity, high air permeability, and low permeability characteristics, without hard adhesive lumps, ensuring the overall flexibility and pore permeability of the chest lining.

[0075] The layered single-sided adhesive coating employs an independently selectable precision hole-avoiding adhesive coating process: CCD vision-controlled point-to-point adhesive coating or perforated mask roller coating. This achieves single-sided micro-adhesive coating only in non-porous areas of the substrate, fundamentally preventing adhesive flow and blocking of breathable micropores, unlike the traditional full-width thick adhesive coating process. Layered single-sided micro-adhesive coating is applied to the perforated substrate to avoid the adhesive layer blocking the breathable pores. Specifically, CCD vision-controlled point-to-point adhesive coating scans the coordinates of the breathable pores in real time and releases adhesive only at fixed points in non-porous areas, with adhesive dots of 0.6mm in diameter and a dot spacing of 4-6mm. Perforated mask roller coating uses a metal perforated mask roller matched to the arrangement of the breathable pores, ensuring that the adhesive is transferred only to non-porous areas. Specifically, an adhesive layer is uniformly coated on the non-porous areas of the surface breathable knitted lining 1, the upper and lower surfaces of the middle high-elastic nonwoven lining 2, and the upper surface of the bottom flexible hemp fiber thin lining 3, with the adhesive amount controlled at 10g / m². 2 The adhesive layer thickness is 0.02-0.05mm, forming a micro-adhesive composite layer 4. The pre-drying temperature is 65℃, the pre-drying time is 2.5min, and the hot air velocity is 1.2m / min, so that the adhesive layer forms a semi-cured state, avoiding adhesive overflow and clogging of pores during lamination. The quantitative judgment standard for the semi-cured state (which can be detected online) is as follows: the degree of cross-linking curing of the adhesive layer is 50% as detected by Fourier transform infrared spectroscopy; the initial tack of the adhesive surface is 1.1N / 25mm as detected by the GB / T 4851-2021 tape initial tack tester; there is only a slight tackiness when lightly touched with a finger; there is no adhesive stringing or sticky transfer; the adhesive film is intact and does not flow, there is no liquid overflow, and there is no risk of sticking to the roller at room temperature; it can be remelted and bonded to the substrate during hot pressing. Meeting the above three indicators is considered a qualified semi-cured state, avoiding adhesive overflow and clogging of pores during lamination.

[0076] S4. Staggered Layered Composite: Using the three-layer substrate after adhesive coating as raw material, the layers are stacked from top to bottom in the following order: breathable knitted lining 1, high-elastic non-woven lining 2, and flexible linen fiber thin lining 3. The edge of the high-elastic non-woven lining 2 is recessed relative to the upper and lower substrate layers. The breathable holes of the three substrate layers correspond one-to-one and are completely aligned without any misalignment or obstruction. After the stacking is completed, the layers are rolled and laminated at a uniform speed to obtain a composite chest lining semi-finished product.

[0077] Specifically, the edge of the middle layer high-elastic non-woven lining 2 is recessed by 1.5mm relative to the upper and lower substrate layers to avoid the thickening of the edges of multiple adhesive layers and eliminate the defects of thick and hardened chest lining edges; the alignment of the ventilation holes of the three substrate layers adopts coarse positioning with side reference positioning holes and fine adjustment with CCD vision servo, with an alignment deviation of ≤0.1mm; the roll pressing composite adopts a double roll press with a roll pressing pressure of 0.4MPa and a roll pressing speed of 5m / min to ensure that each substrate layer is tightly bonded, without bubbles or delamination, and that the holes remain transparent throughout the process.

[0078] S5. Low-temperature constant temperature shaping: The composite chest lining semi-finished product is shaped in sections at low temperature to avoid high temperature damage to the elasticity of the substrate and cause the pores to shrink and deform. At the same time, it prevents the adhesive layer from overflowing and blocking the micropores, thus obtaining the shaped chest lining.

[0079] Specifically, the segmented low-temperature setting includes a first stage of preheating and a second stage of curing. The first stage of preheating is at a temperature of 78°C for 3 minutes to slowly release the composite stress. The second stage of curing is at a temperature of 88°C for 5 minutes to achieve stable curing of the adhesive layer. During the setting process, flat tension is maintained and controlled at 6N to prevent chest lining shrinkage and pore deformation, ensuring stable bonding of each substrate layer and complete and permeable pores.

[0080] S6. Softening and finishing process: Cool the shaped chest lining, then grind the four sides to round the corners (remove hard edges, burrs and residual debris from punching), soften and knead the whole chest lining (eliminate the internal composite stress of the chest lining, improve the overall flexibility and wrinkle resistance, and at the same time repair the fine rough edges of the holes), and cut and shape it according to the pattern to obtain a regular perforated chest lining blank.

[0081] Specifically, the cooling process involves standing at 23°C for 10 minutes; the four sides are polished and rounded using a belt sander with a 1200-mesh ultrafine alumina sander belt, at a belt speed of 6 m / min, a sanding pressure of 0.1 MPa, and a rounded corner radius of 2 mm; the overall softening and kneading process uses a horizontal silicone buffer kneading machine with a kneading frequency of 25 times / min, a silicone bump roller reciprocating stroke of 12 cm, and a processing time of 2 minutes.

[0082] S7. Finished Product Inspection and Storage: Inspect the chest lining blanks, select qualified products and store them to obtain lightweight, perforated suit chest linings.

[0083] The perforated chest liner prepared in this embodiment has a total thickness of 0.6 mm, a weight of 82 g per square meter, an overall air permeability of 580 mm / s, a pore permeability of over 99%, and exhibits no deformation, delamination, or pore blockage after 500 repeated flexing cycles. It also demonstrates a 98% resilience and provides flat, uncollapsed front chest support. The entire set of performance specifications meets national standards: thickness, weight, air permeability, pore permeability, peel strength, flexural strength, and resilience, with clearly defined qualification thresholds.

[0084] Testing and Storage: After conditioning the finished product at 23℃ and 65% RH for 24 hours, a full range of national standard tests were conducted.

[0085] 1. Thickness 0.6mm, surface density 82g / m³ 2 (GB / T3820, GB / T4669);

[0086] 2. Air permeability 580mm / s (GB / T5453, pressure difference 100Pa);

[0087] 3. Pore permeability 99.2% (0.1MPa airflow fixture test);

[0088] 4. Springback recovery rate 98% (GB / T3923.1, 40% tensile load springback test);

[0089] 5. Dry peel strength: 10.5 N / 5 cm; after 5 steam ironing cycles: 8.8 N / 5 cm (GB / T2660).

[0090] 6. No delamination, holes or tears after 500 cycles of reciprocating bending (FZ / T01088, 2N bending pressure);

[0091] 7. The product has no defects in appearance and is qualified for storage under constant temperature and humidity by being laminated and laid flat.

[0092] Comparative Example 1 (Traditional non-porous lightweight chest lining): Using a three-layer composite substrate of equal thickness and conventional micro-coating process, without a perforation process, the finished product thickness is 0.6mm, the weight per square meter is 83g, and the breathability is 320mm / s. In summer, the moisture and heat accumulate significantly, resulting in a strong feeling of stuffiness.

[0093] Comparative Example 2 (Full-area irregular perforated chest lining): The full-area random perforation process is adopted, with no zone design, a hole diameter of 1.0mm and a hole spacing of 10mm. The rest of the process is the same as Example 1. The finished product has an air permeability of 590mm / s, but the core support area is damaged by perforation. After wearing it for 1 week, the chest area has slight sagging and the shape has loosened, resulting in poor support stability.

[0094] Performance comparison of Example 1 and Comparative Examples 1-2 Figure 3 As shown.

[0095] Comparative Experiment 1: Fixing conditions: hole spacing 10mm, square matrix arrangement; support area size 240mm×320mm; CCD vision-based hole-avoiding micro-coating, coating amount 10g / m². 2 The remaining process parameters are the same as in Example 1; only the micropore diameter of the air-permeable zone is changed. Testing conditions: 23℃, 65% RH conditioning for 24h; air permeability GB / T 5453 (pressure difference 100Pa); dry peel strength GB / T 2660. The test results are shown in Table 1.

[0096] Table 1

[0097]

[0098] As shown in Table 1, the air permeability of the chest lining continuously increases with increasing pore size. However, punching cuts the substrate fibers, weakening the interlayer mechanical matrix and causing a monotonically decreasing peel strength. The pore size range of 0.8-1.2 mm represents the equilibrium range. Pores smaller than 0.8 mm result in insufficient air permeability; pore sizes exceeding 1.2 mm significantly reduce interlayer bonding strength, posing risks of hole tearing and localized delamination. A pore size of 1.0 mm is preferred, simultaneously satisfying both air permeability ≥550 mm / s and peel strength ≥9 N / 5 cm.

[0099] Comparative Experiment 2: Quantitative Influence of Different Central Support Area Dimensions on Bending Resistance:

[0100] Test conditions: pore diameter 1.0 mm, pore spacing 10 mm; CCD hole-avoiding adhesive application; other processes are the same as in Example 1; only the size of the central non-perforated support area is adjusted (the outer contour of the chest liner is uniformly 480 mm × 360 mm); testing standard: FZ / T 01088-2020, bending pressure 2 N, 30 times / min, record the critical number of bends that result in collapse / hole tearing / interlayer delamination. Test results are shown in Table 2.

[0101] Table 2

[0102]

[0103] As shown in Table 2, increasing the size of the support area can improve the bending and collapse resistance of the chest lining, but it will compress the breathable perforated area, resulting in a decrease in breathability. If the size of the support area is too small, the core stress area will be damaged by micropores, and the bending resistance will not meet the standards. This invention limits the support area to 240mm×320mm (accounting for 44.4%), achieving the optimal balance between breathable area and structural deformation resistance.

[0104] Comparative Experiment 3: Comparative Experiment on the Hole Blockage Rate with and without Hole-Avoiding Adhesive Coating Process:

[0105] Experimental conditions: Complete substrate and drilling parameters (hole diameter 1.0 mm, hole spacing 10 mm) as per Example 1; Variables: Group A used the CCD vision-based hole-avoiding coating method of Example 1; Group B used traditional undifferentiated full-width micro-coating (no hole-avoiding control, all other coating amounts, adhesive types, and drying parameters were identical); Group C used a perforated mask roller coating process to avoid holes. Test method: After the finished product cooled, a 0.1 MPa airflow fixture was used to test the permeability of the holes. The number of micropores blocked by adhesive and completely unable to pass through the permeable area was counted, and the hole blockage rate was calculated. The experimental results are shown in Table 3.

[0106] Table 3

[0107]

[0108] As shown in Table 3, conventional micro-coating processes lack pore avoidance control, and adhesive overflow and spreading easily block the array of micropores, causing the perforated structure to lose its breathability value. This invention employs a precise pore avoidance process using CCD vision-based point-to-point coating or perforated mask roller coating, controlling the pore blockage rate to within 1.5%. This ensures that the multi-layered pores are interconnected, allowing the zoned perforated structure to truly function as a breathable structure, which is an essential process feature for achieving high breathability.

[0109] To clarify the boundaries of the key process parameters of this invention, multiple sets of single-variable control experiments were set up. Except for the change of the target parameter, all other process conditions were kept consistent with those in Example 1.

[0110] 1. Performance Comparison Tests with Different Pore Size Parameters: Under the condition of a constant 10mm hole spacing, samples were prepared by drilling holes with diameters of 0.6mm, 0.8mm, 1.0mm, 1.2mm, and 1.4mm. The tests showed that as the hole diameter increased, the air permeability of the finished product gradually improved, but punching and cutting damaged the continuity of the substrate fibers, leading to a continuous decrease in interlayer peel strength. Hole diameters below 0.8mm resulted in insufficient air permeability; and pore diameters above 1.2mm caused the peel strength to fall below the acceptable threshold. A hole diameter of 0.8-1.2mm is the preferred range, while a hole diameter of 1.0mm can balance air permeability and interlayer bonding strength.

[0111] 2. Comparative Test of Bending Resistance Performance with Different Support Zone Sizes: Under the premise of a fixed outer contour of 480mm × 360mm for the chest liner, the size of the central non-perforated support zone was adjusted. A decrease in the area ratio of the support zone means that the core stress area of ​​the chest liner is covered by micropores, significantly reducing the critical number of bending cycles for the finished product and making it prone to anterior chest collapse. An excessively high support zone ratio will compress the breathable area, and the breathability index will fail to meet the standard. A support zone of 240mm × 320mm, with an area ratio of 44.4%, can simultaneously meet the requirement of 500 bending cycles and the standard of breathability ≥ 550mm / s.

[0112] 3. Comparative Test of the Hole-Avoiding Glue Coating Process: The hole-avoiding micro-coating process of this invention is compared with the traditional uncontrolled full-width glue coating. The traditional glue coating method has a hole blockage rate as high as 31.6%, and the air permeability gain brought by perforation is basically negated. By using two hole-avoiding methods, namely CCD vision point-based glue coating and hollow mask roller coating, the hole blockage rate can be controlled below 1.5%, ensuring that the multi-layer micropores form a continuous and interconnected three-dimensional air permeable channel. This proves that zoned perforation must be combined with a precise hole-avoiding glue coating process, and the two work together to solve the technical problems of stuffiness and stickiness of traditional chest linings.

[0113] Comparative data shows that this invention, through partitioned perforation and precise process parameter optimization, perfectly ensures the structural strength and shaping stability of the chest liner while maintaining extreme lightweight and high breathability, resulting in overall performance significantly superior to existing conventional products.

[0114] Based on the above-described preferred embodiments of the present invention, and through the foregoing description, those skilled in the art can make various changes and modifications without departing from the inventive concept. The technical scope of this invention is not limited to the contents of the specification.

Claims

1. A method for manufacturing a lightweight, perforated suit jacket chest lining, characterized in that, Includes the following steps: Substrate pretreatment: Three lightweight substrates are provided, namely a breathable knitted lining on the surface, a high-elastic non-woven lining in the middle, and a flexible linen fiber lining at the bottom. The three lightweight substrates were ironed flat and dust and impurities were removed to obtain the pretreated three-layer substrates. Precise perforation in zones: Using the pre-treated three-layer substrate as raw material, each layer of substrate is divided into a central stress support area and a breathable area located around the central stress support area. The central stress support area is not perforated, while the breathable area is perforated in an array matrix to form breathable holes. After perforation, the hole debris is cleaned to obtain the perforated three-layer substrate. Layered micro-coating: Using three-layer substrates after perforation as raw materials, low-permeability modified polyurethane water-based hot melt adhesive is used to apply adhesive to the non-porous areas of the bonding surface of each substrate, except for the vent holes. After coating, the adhesive is pre-dried to make the adhesive layer semi-cured, thus obtaining the coated three-layer substrate. Staggered layered composite: Using three layers of substrate after adhesive coating as raw materials, the layers are stacked from top to bottom in the order of breathable knitted lining, high-elastic non-woven lining in the middle layer, and flexible hemp fiber lining in the bottom layer. The edge of the high-elastic non-woven lining in the middle layer is recessed relative to the upper and lower substrate layers. The breathable holes of the three substrate layers correspond one-to-one. The composite is rolled and laminated to obtain a composite chest lining semi-finished product. Low-temperature constant temperature setting: The composite chest lining semi-finished product is subjected to segmented low-temperature setting to obtain the set chest lining; Softening and finishing process: After the shaped chest lining is cooled, the four sides are sanded and rounded, the whole body is softened and kneaded, and then cut and shaped according to the pattern to obtain the chest lining blank; Finished product inspection and storage: The chest lining blanks are inspected, qualified products are selected and stored, resulting in a lightweight, perforated suit chest lining.

2. The method for manufacturing a lightweight, perforated suit chest lining according to claim 1, characterized in that, The breathable knitted lining is made of 75D / 144F polyester fiber knitted fabric with a warp and weft density of 120*90 and a weight of 110±5g / m². 2 The intermediate high-elastic nonwoven lining consists of 60-70 wt% polyester and 30-40 wt% viscose spunlace nonwoven lining, with a basis weight of 90 ± 5 g / m². 2 The underlying flexible linen lining is a blend of 45-55 wt% linen and 45-55 wt% cotton, with a basis weight of 80 ± 5 g / m². 2 The thickness of each substrate is 0.15-0.25mm; The ironing temperature for smooth ironing is 80-90℃, the ironing speed is 3-5m / min, and the pressure of the hot press roller is 0.1-0.3MPa. The dust removal and impurity removal adopts an electrostatic brush dust removal and impurity removal unit with a brush rotation speed of 100-150r / min, and is coordinated with a negative pressure dust collection fan.

3. The method for manufacturing the lightweight perforated suit chest lining according to claim 1, characterized in that, The central support area is rectangular, the outer contour of the chest lining is (470-490)mm×(350-370)mm, the central support area is (230-250)mm×(310-330)mm, its left and right boundaries are 110-130mm away from the left and right outer edges of the chest lining, respectively, and its upper and lower boundaries are 15-25mm away from the top and bottom outer edges of the chest lining, respectively. The area of ​​the central support area accounts for 42%-46% of the total area of ​​the chest lining, and the area of ​​the breathable area accounts for 54%-58%.

4. The method for manufacturing the lightweight perforated suit chest lining according to claim 1, characterized in that, The array-type matrix punching has a hole diameter of 0.8-1.2mm, a hole spacing of 8-12mm, and a punching speed of 200-300 times / min. After punching, the hole debris is cleaned by blowing with a high-pressure airflow of 0.05-0.15MPa. Simultaneously, a reference positioning hole with a diameter of 1.5-2.5mm is reserved on the side of the substrate.

5. The method for manufacturing the lightweight perforated suit chest lining according to claim 1, characterized in that, The low-permeability modified polyurethane waterborne hot melt adhesive has a softening point of 52-58℃, a dry single-layer peel strength of ≥11N / 5cm, a solid content of 42±2%, an adhesive layer penetration depth of ≤0.01mm, and an elastic elongation of ≥350% after curing.

6. The method for manufacturing a lightweight, perforated suit chest lining according to claim 1, characterized in that, Layered single-sided adhesive coating is achieved using CCD vision numerical control point-to-point adhesive coating or stencil mask roller coating. CCD vision numerical control point-to-point adhesive application scans the coordinates of the ventilation holes in real time and releases adhesive only at fixed points in non-hole areas, with adhesive dot diameter of 0.5-0.7mm and adhesive dot spacing of 4-6mm; The perforated mask roller coating uses a metal perforated mask roller that matches the arrangement of the ventilation holes, ensuring that the adhesive is transferred only to the non-perforated areas; the coating amount is 8-12 g / m². 2 The adhesive layer thickness is 0.02-0.05mm; the pre-drying temperature is 60-70℃, the pre-drying time is 2-3min, and the hot air velocity is 1.1-1.3m / min; the semi-cured state meets the following requirements: the degree of curing of the adhesive layer is 45%-55%, the initial tack of the adhesive surface is 0.8-1.5N / 25mm, and the adhesive film is intact and does not flow.

7. The method for manufacturing a lightweight, perforated suit chest lining according to claim 4, characterized in that, The edge of the middle layer high-elastic nonwoven lining is recessed by 1-2mm relative to the upper and lower substrate layers; the alignment of the ventilation holes of the three substrate layers is achieved by coarse positioning with side reference positioning holes and fine adjustment with CCD vision servo, with an alignment deviation of ≤0.1mm; the roll pressing composite adopts a double roll press with a roll pressing pressure of 0.3-0.5MPa and a roll pressing speed of 4-6m / min.

8. The method for manufacturing a lightweight, perforated suit chest lining according to claim 1, characterized in that, The segmented low-temperature setting includes a first stage of preheating and a second stage of curing; the temperature of the first stage of preheating is 75-80℃ and the time is 2-4 min; the temperature of the second stage of curing is 85-90℃ and the time is 4-6 min; the setting tension is 5-8 N.

9. The method for manufacturing the lightweight perforated suit chest lining according to claim 1, characterized in that, The cooling process involves standing at 20-25℃ for 5-15 minutes; the four sides are polished and rounded using a belt sander with a 1000-1500 mesh ultrafine alumina sander belt, at a belt speed of 5-7 m / min, a sanding pressure of 0.05-0.15 MPa, and a rounded corner radius of 1.5-2.5 mm; the overall softening and kneading process uses a horizontal silicone buffer kneading machine, with a kneading frequency of 20-30 times / min, a reciprocating stroke of 11-13 cm, and a processing time of 1-3 minutes.

10. A lightweight, perforated suit chest lining manufactured using the method described in any one of claims 1-8.