An environmentally friendly aerosol fire extinguishing agent and its preparation method
By preparing an environmentally friendly aerosol fire extinguishing agent using an oxidant-combustible co-crystallization material and a mesoporous catalyst, the problems of high-temperature corrosion and secondary damage of thermal aerosol fire extinguishing agents have been solved, achieving more efficient fire extinguishing performance and environmental friendliness.
Patent Information
- Application Number
- CN202611195600.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-08-07
- Publication Date
- 2026-11-17
AI Technical Summary
Existing thermal aerosol fire extinguishing agents have high combustion temperatures, produce high-temperature flames during combustion that may cause secondary damage to the fire scene, and leave residues that are highly corrosive to metal surfaces after extinguishing. Therefore, it is necessary to find environmentally friendly alternatives.
An environmentally friendly aerosol fire extinguishing agent is formed by using an oxidant-combustible agent co-crystallization material and a mesoporous catalyst, preparing the oxidant-combustible agent co-crystallization material by freeze drying, preparing the mesoporous catalyst by sol-gel method, and adding hexamethylenetetramine, potassium oxalate and phenolic resin.
It improves fire extinguishing performance, lowers combustion temperature, reduces corrosive residues, and enhances the environmental friendliness and fire extinguishing efficiency of the extinguishing agent.
Smart Images

Figure SMS_2
Abstract
Description
Technical Field
[0001] This invention relates to the field of aerosol fire extinguishing technology, specifically to an environmentally friendly aerosol fire extinguishing agent and its preparation method. Background Technology
[0002] In the 1940s, halon fire extinguishing agents were widely used due to their high extinguishing efficiency, ease of use, and safety (non-corrosiveness). However, it was later discovered that halon fire extinguishing agents release Freon, which contributes to ozone layer depletion. Therefore, finding alternatives to halon fire extinguishing agents is crucial. Aerosol fire extinguishing agents have gained increasing attention due to their high efficiency, economy, and ease of maintenance. Compared to halon fire extinguishing agents, thermal aerosol fire extinguishing agents have lower ozone depletion potential and greenhouse effect potential, making them environmentally friendly products that do not contribute to global warming or ozone layer depletion.
[0003] Thermal aerosol fire extinguishing agents consist of oxidizers, reducing agents, binders, and modifiers. The extinguishing agent itself cannot extinguish fires; it requires external ignition. Once ignited, the oxidizer and combustible agent undergo a redox reaction to form aerosol particles and gases, which then rapidly fill the entire fire-extinguishing environment through irregular movement. This extinguishing mechanism, primarily based on chemical inhibition and supplemented by physical endothermic reaction, achieves high extinguishing efficiency. Potassium salts and their oxides are the main active extinguishing agents. However, after extinguishing, the potassium oxides and potassium salts in the residue dilute moisture in the air, forming alkalis. These alkaline substances adhere to the protected metal surfaces, causing significant corrosion. Therefore, strontium nitrate is often added to reduce the corrosiveness of the extinguishing agent. Furthermore, thermal aerosol fire extinguishing agents have the problem of high combustion temperatures and the potential for secondary damage to the fire scene from the high-temperature flames produced during combustion. Therefore, this invention prepares an environmentally friendly aerosol fire extinguishing agent, which improves its extinguishing performance through the synergistic effect of an oxidizer-combustible agent co-crystallization material and a mesoporous catalyst. Summary of the Invention
[0004] The purpose of this invention is to provide an environmentally friendly aerosol fire extinguishing agent and its preparation method, specifically an environmentally friendly aerosol fire extinguishing agent with good fire extinguishing performance and its preparation method.
[0005] To achieve this objective, the present invention adopts the following technical solution: In a first aspect, the present invention provides an environmentally friendly aerosol fire extinguishing agent, the environmentally friendly aerosol fire extinguishing agent comprising an oxidant-combustible agent co-crystallization material, a mesoporous catalyst, hexamethylenetetramine, potassium oxalate, and phenolic resin.
[0006] Furthermore, the oxidant-combustible agent co-crystallized material is prepared by co-crystallizing a mixture of potassium nitrate, strontium nitrate, and lactose.
[0007] Furthermore, the mesoporous catalyst is prepared by ferric nitrate nonahydrate, copper nitrate trihydrate, and propylene oxide via a sol-gel method.
[0008] Secondly, the present invention provides a method for preparing an environmentally friendly aerosol fire extinguishing agent, the method comprising the following steps: (1) Mix potassium nitrate, strontium nitrate, lactose and deionized water evenly, dissolve by ultrasonic stirring, pre-freeze, vacuum dry, grind and sieve to obtain oxidant-combustible co-crystallized material; (2) Mix ferric nitrate nonahydrate, copper nitrate trihydrate and anhydrous ethanol evenly, stir and mix at room temperature, add propylene oxide, stir and mix, let stand for aging, vacuum dry, calcine in air to obtain mesoporous catalyst; (3) Mix the oxidant-combustible agent co-crystallization material, mesoporous catalyst, hexamethylenetetramine and potassium oxalate evenly, add phenolic resin ethanol solution, sieve and granulate, vacuum dry, pour into a pressing mold and press to form, and obtain an environmentally friendly aerosol fire extinguishing agent.
[0009] Further, the mass ratio of potassium nitrate, strontium nitrate, lactose, and deionized water in step (1) is 1:(3~4):(0.6~0.7):(10~12).
[0010] Furthermore, the pre-freezing time in step (1) is 2-4 hours; the vacuum drying time is 15-20 hours.
[0011] Furthermore, the sieving in step (1) is sieving through an 80-100 mesh screen.
[0012] Further, in step (2), the mass ratio of ferric nitrate nonahydrate, copper nitrate trihydrate, anhydrous ethanol, and propylene oxide is 1:(0.06~0.12):(10~12):(1.7~1.9).
[0013] Furthermore, the static aging temperature in step (2) is room temperature, and the time is 40~60 min.
[0014] Furthermore, the calcination temperature in step (2) is 300~400℃ and the calcination time is 4~6h.
[0015] Further, the phenolic resin ethanol solution in step (3) is prepared by mixing phenolic resin and anhydrous ethanol at a mass ratio of 1:(0.5~1) and stirring to dissolve.
[0016] Further, the mass ratio of the oxidant-combustible co-crystallization material, mesoporous catalyst, hexamethylenetetramine, potassium oxalate, and phenolic resin ethanol solution in step (3) is 1: (0.02~0.04): (0.01~0.02): (0.01~0.02): (0.1~0.2).
[0017] Furthermore, the granulation in step (3) is granulation through a 50-mesh screen.
[0018] Furthermore, the lactose was purchased from Huixing Biochemical Reagent Co., Ltd. in China.
[0019] Furthermore, the phenolic resin was purchased from Shanghai Maclean Biochemical Technology Co., Ltd.
[0020] Compared with the prior art, the beneficial effects achieved by the present invention are: In preparing an environmentally friendly aerosol fire extinguishing agent, this invention involves co-crystallizing potassium nitrate, strontium nitrate, and lactose to obtain an oxidant-combustible co-crystallized material; preparing a mesoporous catalyst by sol-gel method using ferric nitrate nonahydrate, copper nitrate trihydrate, and propylene oxide; and mixing the oxidant-combustible co-crystallized material, the mesoporous catalyst, hexamethylenetetramine, potassium oxalate, and phenolic resin, followed by sieving, granulation, and pressing to obtain the environmentally friendly aerosol fire extinguishing agent.
[0021] First, using potassium nitrate and strontium nitrate as oxidants and lactose as a combustible agent, an oxidant-combustible agent co-crystallized material was prepared by freeze-drying. While the aerosol extinguishing agent prepared with potassium nitrate as the oxidant exhibited good extinguishing performance, the potassium oxides and potassium salts in the residue after extinguishing diluted moisture in the air, forming alkalis. These alkaline substances adhered to the protected metal surface, causing significant corrosion. Therefore, strontium nitrate was chosen to partially replace potassium nitrate. The decomposition products of strontium nitrate after combustion are SrO, Sr(OH)2, and SrCO3. These substances have low hygroscopicity and relatively weak corrosiveness, thus effectively protecting the metal equipment. Furthermore, the melting point of SrO is much higher than that of the extinguishing agent during combustion. The temperature is low, allowing it to remain stably in the agent, with very little SrO entering the external environment, ensuring the environmental friendliness of the extinguishing aerosol particles; lactose has low hygroscopicity, which is beneficial for processing and storage; after potassium nitrate, strontium nitrate, and lactose form a co-crystallized material, the oxidizer and combustible agent achieve a more uniform and tighter bond, enabling the material to react faster at lower temperatures and the reaction to occur more completely, resulting in less residue after combustion. Most of the extinguishing agent is completely burned to form an aerosol, reducing the amount of residual substances that could cause corrosion. In addition, the combustion products are small particles, resulting in a small corrosion area, reducing corrosion damage, and thus improving extinguishing performance.
[0022] Secondly, mesoporous catalysts were prepared by sol-gel method using ferric nitrate nonahydrate, copper nitrate trihydrate, and propylene oxide. During the combustion of the extinguishing agent, the catalyst temporarily stores oxygen from the decomposition of the oxidant, facilitating the rapid decomposition of the surrounding oxidant, reducing the activation energy of the combustion reaction, and thus promoting the combustion process. When ferric oxide is used as a catalyst, it helps to lower the reaction temperature and shorten the extinguishing time. When copper oxide is used as a catalyst, it helps to lower the flame temperature and inhibit the formation of high-temperature flames, thereby further improving the extinguishing performance of the extinguishing agent. A mesoporous Fe2O3-CuO composite catalyst was prepared by sol-gel method. The mesoporous structure has a high specific surface area and abundant mesoporous channels, providing more catalytic active sites, thereby further improving the extinguishing performance of the extinguishing agent.
[0023] Finally, the oxidant-combustible agent co-crystallization material, mesoporous catalyst, hexamethylenetetramine, potassium oxalate, and phenolic resin were mixed, sieved, granulated, and pressed into shape to obtain an environmentally friendly aerosol fire extinguishing agent. Hexamethylenetetramine is an excellent solid fuel; when used in combination with lactose, it can improve combustion performance and regulate the burning rate. Potassium oxalate, as a chemical coolant, decomposes and absorbs heat during combustion, thus lowering the system temperature. Phenolic resin, as a binder, ensures uniform mixing of the fire extinguishing agent components and facilitates processing and shaping. Detailed Implementation
[0024] The technical solutions of the present invention will be clearly and completely described below with reference to the embodiments of the present invention. Obviously, the described embodiments are only some embodiments of the present invention, and not all embodiments. Based on the embodiments of the present invention, all other embodiments obtained by those of ordinary skill in the art without creative effort are within the scope of protection of the present invention.
[0025] Example 1: A method for preparing an environmentally friendly aerosol fire extinguishing agent includes the following preparation steps: (1) Potassium nitrate, strontium nitrate, lactose and deionized water are mixed evenly in a mass ratio of 1:3:0.6:10, ultrasonically stirred and dissolved, and placed in the pre-freezing chamber of a vacuum freeze dryer for 2 hours. After taking it out, it is placed in the freeze-drying chamber of a vacuum freeze dryer for 15 hours of vacuum drying. After taking it out, it is ground and passed through an 80-mesh sieve to obtain an oxidant-combustible agent co-crystallized material. (2) Mix ferric nitrate nonahydrate, copper nitrate trihydrate, and anhydrous ethanol in a mass ratio of 1:0.06:10. Stir and mix at room temperature for 10 min. Add propylene oxide in 1.7 times the mass of ferric nitrate nonahydrate and stir for 3 min. Let stand and age at room temperature for 40 min. Dry under vacuum at 75℃ for 40 h. In air, heat to 300℃ at a heating rate of 3℃ / min and calcine for 4 h to obtain a mesoporous catalyst. (3) Phenolic resin and anhydrous ethanol are mixed evenly at a mass ratio of 1:0.5 and stirred to dissolve, thus obtaining a phenolic resin ethanol solution; oxidant-combustible agent co-crystallization material, mesoporous catalyst, hexamethylenetetramine, and potassium oxalate are mixed evenly at a mass ratio of 1:0.02:0.01:0.01, and 0.1 times the mass of oxidant-combustible agent co-crystallization material of phenolic resin ethanol solution is added. The mixture is granulated by passing it through a 50-mesh screen, dried under vacuum at 40°C for 6 hours, poured into a pressing mold and pressed to form an environmentally friendly aerosol fire extinguishing agent.
[0026] Example 2: A method for preparing an environmentally friendly aerosol fire extinguishing agent includes the following preparation steps: (1) Potassium nitrate, strontium nitrate, lactose, and deionized water were mixed evenly in a mass ratio of 1:3.5:0.65:11, and dissolved by ultrasonic stirring. The mixture was then placed in the pre-freezing chamber of a vacuum freeze dryer and pre-frozen for 3 hours. After being removed, the mixture was placed in the freeze-drying chamber of the vacuum freeze dryer and vacuum-dried for 18 hours. After being removed, the mixture was ground and passed through a 90-mesh sieve to obtain an oxidant-combustible agent co-crystallized material. (2) Mix ferric nitrate nonahydrate, copper nitrate trihydrate, and anhydrous ethanol in a mass ratio of 1:0.09:11. Stir and mix at room temperature for 15 min. Add propylene oxide in 1.8 times the mass of ferric nitrate nonahydrate and stir for 4 min. Let stand and age at room temperature for 50 min. Dry under vacuum at 80℃ for 44 h. In air, heat to 350℃ at a heating rate of 3℃ / min and calcine for 5 h to obtain a mesoporous catalyst. (3) Phenolic resin and anhydrous ethanol are mixed evenly at a mass ratio of 1:0.75 and stirred to dissolve, thus obtaining a phenolic resin ethanol solution; oxidant-combustible agent co-crystallization material, mesoporous catalyst, hexamethylenetetramine, and potassium oxalate are mixed evenly at a mass ratio of 1:0.03:0.015:0.015, and phenolic resin ethanol solution with a mass of 0.15 times that of oxidant-combustible agent co-crystallization material is added. The mixture is granulated by passing it through a 50-mesh screen, dried under vacuum at 45°C for 7 hours, poured into a pressing mold and pressed to form an environmentally friendly aerosol fire extinguishing agent.
[0027] Example 3: A method for preparing an environmentally friendly aerosol fire extinguishing agent includes the following preparation steps: (1) Potassium nitrate, strontium nitrate, lactose and deionized water were mixed evenly in a mass ratio of 1:4:0.7:12, and dissolved by ultrasonic stirring. The mixture was then placed in the pre-freezing chamber of a vacuum freeze dryer and pre-frozen for 4 hours. After being removed, the mixture was placed in the freeze-drying chamber of the vacuum freeze dryer and vacuum-dried for 20 hours. After being removed, the mixture was ground and passed through a 100-mesh sieve to obtain an oxidant-combustible agent co-crystallized material. (2) Mix ferric nitrate nonahydrate, copper nitrate trihydrate, and anhydrous ethanol in a mass ratio of 1:0.12:12. Stir and mix at room temperature for 20 min. Add propylene oxide in 1.9 times the mass of ferric nitrate nonahydrate and stir for 5 min. Let stand and age at room temperature for 60 min. Dry under vacuum at 85℃ for 48 h. In air, heat to 400℃ at a heating rate of 3℃ / min and calcine for 6 h to obtain a mesoporous catalyst. (3) Phenolic resin and anhydrous ethanol are mixed evenly at a mass ratio of 1:1 and stirred to dissolve, thus obtaining a phenolic resin ethanol solution; oxidant-combustible agent co-crystallization material, mesoporous catalyst, hexamethylenetetramine, and potassium oxalate are mixed evenly at a mass ratio of 1:0.04:0.02:0.02, and 0.2 times the mass of oxidant-combustible agent co-crystallization material of phenolic resin ethanol solution is added. The mixture is granulated by passing it through a 50-mesh screen, dried under vacuum at 50°C for 8 hours, poured into a pressing mold and pressed to form an environmentally friendly aerosol fire extinguishing agent.
[0028] Comparative Example 1: The preparation method of the environmentally friendly aerosol fire extinguishing agent in Comparative Example 1 differs from that in Example 2 in that step (1) is omitted, and step (3) is modified as follows: potassium nitrate, strontium nitrate, and lactose are mixed evenly in a mass ratio of 1:3.5:0.65 to obtain an oxidant-combustible agent mixture; phenolic resin and anhydrous ethanol are mixed evenly in a mass ratio of 1:0.75 and stirred to dissolve, thus obtaining a phenolic resin ethanol solution; the oxidant-combustible agent mixture, mesoporous catalyst, hexamethylenetetramine, and potassium oxalate are mixed evenly in a mass ratio of 1:0.03:0.015:0.015, and 0.15 times the mass of the oxidant-combustible agent mixture is added to the phenolic resin ethanol solution. The mixture is granulated through a 50-mesh sieve, vacuum dried at 45°C for 7 hours, and then pressed into a pressing mold to obtain the environmentally friendly aerosol fire extinguishing agent. The remaining steps are the same as in Example 2.
[0029] Comparative Example 2: The difference between the preparation method of the environmentally friendly aerosol fire extinguishing agent in Comparative Example 2 and Example 2 lies in step (1). Step (1) is modified as follows: potassium nitrate, strontium nitrate, lactose, and deionized water are mixed evenly in a mass ratio of 1:3.5:0.65:11, ultrasonically stirred to dissolve, and placed in a 90°C water bath for continuous stirring. When there is almost no flowing water in the mixture, it is taken out and vacuum dried at 50°C for 12 hours; then ground and passed through a 90-mesh sieve to obtain the oxidant-combustible agent co-crystallized material. The remaining steps are the same as in Example 2.
[0030] Comparative Example 3: The difference between the preparation method of the environmentally friendly aerosol fire extinguishing agent in Comparative Example 3 and Example 2 lies in step (2). Step (2) is modified as follows: Ferric nitrate nonahydrate, copper nitrate trihydrate, and anhydrous ethanol are mixed evenly at a mass ratio of 1:0.09:11, stirred and mixed at room temperature for 15 min, propylene oxide with a mass of 1.8 times that of ferric nitrate nonahydrate is added, stirred for 4 min, allowed to stand and age at room temperature for 50 min, vacuum dried at 80℃ for 44 h, and calcined in air at a heating rate of 3℃ / min to 450℃ for 5 h to obtain the mesoporous catalyst. The remaining steps are the same as in Example 2.
[0031] Comparative Example 4: The difference between the preparation method of the environmentally friendly aerosol fire extinguishing agent in Comparative Example 4 and Example 2 lies in step (2). Step (2) is modified as follows: Ferric nitrate nonahydrate, copper nitrate trihydrate, and anhydrous ethanol are mixed evenly at a mass ratio of 1:0.09:11, stirred at room temperature for 15 min, propylene oxide with a mass of 1.8 times that of ferric nitrate nonahydrate is added, stirred for 4 min, allowed to stand and age at room temperature for 50 min, vacuum dried at 80℃ for 44 h, and calcined in air at a heating rate of 3℃ / min to 500℃ for 5 h to obtain the mesoporous catalyst. The remaining steps are the same as in Example 2.
[0032] Comparative Example 5: The difference between the preparation method of the environmentally friendly aerosol fire extinguishing agent in Comparative Example 5 and Example 2 lies in step (2). Step (2) is modified as follows: Ferric nitrate nonahydrate, copper nitrate trihydrate, and anhydrous ethanol are mixed evenly at a mass ratio of 1:0.02:11, stirred and mixed at room temperature for 15 min, propylene oxide with a mass of 1.8 times that of ferric nitrate nonahydrate is added, stirred for 4 min, allowed to stand and age at room temperature for 50 min, vacuum dried at 80℃ for 44 h, and calcined in air at a heating rate of 3℃ / min to 350℃ for 5 h to obtain the mesoporous catalyst. The remaining steps are the same as in Example 2.
[0033] Comparative Example 6: The difference between the preparation method of the environmentally friendly aerosol fire extinguishing agent in Comparative Example 6 and Example 2 lies in step (2). Step (2) is modified as follows: Ferric nitrate nonahydrate, copper nitrate trihydrate, and anhydrous ethanol are mixed evenly at a mass ratio of 1:0.04:11, stirred and mixed at room temperature for 15 min, propylene oxide with a mass of 1.8 times that of ferric nitrate nonahydrate is added, stirred for 4 min, allowed to stand and age at room temperature for 50 min, vacuum dried at 80℃ for 44 h, and calcined in air at a heating rate of 3℃ / min to 350℃ for 5 h to obtain the mesoporous catalyst. The remaining steps are the same as in Example 2.
[0034] Comparative Example 7: The difference between the preparation method of the environmentally friendly aerosol fire extinguishing agent in Comparative Example 7 and Example 2 lies in step (2). Step (2) is modified as follows: Ferric nitrate nonahydrate, copper nitrate trihydrate, and anhydrous ethanol are mixed evenly at a mass ratio of 1:0.14:11, stirred and mixed at room temperature for 15 min, propylene oxide with a mass of 1.8 times that of ferric nitrate nonahydrate is added, stirred for 4 min, allowed to stand and age at room temperature for 50 min, vacuum dried at 80℃ for 44 h, and calcined in air at a heating rate of 3℃ / min to 350℃ for 5 h to obtain the mesoporous catalyst. The remaining steps are the same as in Example 2.
[0035] Comparative Example 8: The difference between the preparation method of the environmentally friendly aerosol fire extinguishing agent in Comparative Example 8 and Example 2 lies in step (2). Step (2) is modified as follows: Ferric nitrate nonahydrate, copper nitrate trihydrate, and anhydrous ethanol are mixed evenly at a mass ratio of 1:0.16:11, stirred and mixed at room temperature for 15 min, propylene oxide with a mass of 1.8 times that of ferric nitrate nonahydrate is added, stirred for 4 min, allowed to stand and age at room temperature for 50 min, vacuum dried at 80℃ for 44 h, and calcined in air at a heating rate of 3℃ / min to 350℃ for 5 h to obtain the mesoporous catalyst. The remaining steps are the same as in Example 2.
[0036] Comparative Example 9: The preparation method of the environmentally friendly aerosol fire extinguishing agent in Comparative Example 9 differs from that in Example 2 in that step (2) is omitted, and step (3) is modified as follows: Phenolic resin and anhydrous ethanol are mixed evenly at a mass ratio of 1:0.75 and stirred to dissolve, thus obtaining a phenolic resin ethanol solution; Oxidant-combustible agent co-crystallization material, iron oxide, hexamethylenetetramine, and potassium oxalate are mixed evenly at a mass ratio of 1:0.03:0.015:0.015, and 0.15 times the mass of the oxidant-combustible agent co-crystallization material in the phenolic resin ethanol solution is added. The mixture is granulated through a 50-mesh sieve, vacuum dried at 45°C for 7 hours, poured into a pressing mold, and pressed to obtain the environmentally friendly aerosol fire extinguishing agent. The remaining steps are the same as in Example 2.
[0037] Comparative Example 10: The preparation method of the environmentally friendly aerosol fire extinguishing agent in Comparative Example 10 differs from that in Example 2 in that step (2) is omitted, and step (3) is modified as follows: Phenolic resin and anhydrous ethanol are mixed evenly at a mass ratio of 1:0.75, stirred and dissolved to obtain a phenolic resin ethanol solution; oxidant-combustible agent co-crystallization material, copper oxide, hexamethylenetetramine, and potassium oxalate are mixed evenly at a mass ratio of 1:0.03:0.015:0.015, and 0.15 times the mass of the oxidant-combustible agent co-crystallization material of the phenolic resin ethanol solution is added. The mixture is granulated through a 50-mesh sieve, vacuum dried at 45°C for 7 hours, poured into a pressing mold and pressed to obtain the environmentally friendly aerosol fire extinguishing agent. The remaining steps are the same as in Example 2.
[0038] Comparative Example 11: The preparation method of the environmentally friendly aerosol fire extinguishing agent in Comparative Example 11 differs from that in Example 2 in that step (2) is omitted, and step (3) is modified as follows: Phenolic resin and anhydrous ethanol are mixed evenly at a mass ratio of 1:0.75, stirred and dissolved to obtain a phenolic resin ethanol solution; Oxidant-combustible agent co-crystallization material, iron oxide, copper oxide, hexamethylenetetramine, and potassium oxalate are mixed evenly at a mass ratio of 1:0.015:0.015:0.015:0.015, and 0.15 times the mass of the oxidant-combustible agent co-crystallization material of the phenolic resin ethanol solution is added. The mixture is granulated through a 50-mesh screen, vacuum dried at 45°C for 7 hours, poured into a pressing mold and pressed to obtain the environmentally friendly aerosol fire extinguishing agent. The remaining steps are the same as in Example 2.
[0039] Comparative Example 12: The preparation method of the environmentally friendly aerosol fire extinguishing agent in Comparative Example 12 differs from that in Example 2 in that step (2) is omitted, and step (3) is modified as follows: Phenolic resin and anhydrous ethanol are mixed evenly at a mass ratio of 1:0.75, stirred and dissolved to obtain a phenolic resin ethanol solution; oxidant-combustible agent co-crystallization material, hexamethylenetetramine, and potassium oxalate are mixed evenly at a mass ratio of 1:0.015:0.015, and 0.15 times the mass of the oxidant-combustible agent co-crystallization material in the phenolic resin ethanol solution is added. The mixture is granulated through a 50-mesh sieve, vacuum dried at 45°C for 7 hours, poured into a pressing mold and pressed to obtain the environmentally friendly aerosol fire extinguishing agent. The remaining steps are the same as in Example 2.
[0040] Test Example 1: Fire extinguishing performance test: Fire extinguishing performance tests were conducted in an acrylic fire extinguishing box measuring 22cm × 22cm × 43cm. 2g of each of the environmentally friendly aerosol fire extinguishing agents prepared in each example and comparative example was used to prepare cylindrical samples with a diameter of 2cm. Heptane was placed in a crucible with a diameter of 5cm and a height of 4cm as the ignition source. The ignition source and the environmentally friendly aerosol fire extinguishing agent sample were placed diagonally inside the fire extinguishing box. The heptane was ignited, and after pre-ignition for 30 seconds under ventilation, the fire extinguishing box door was closed, and the environmentally friendly aerosol fire extinguishing agent was ignited. The combustion time and extinguishing time of the environmentally friendly aerosol fire extinguishing agent were recorded. Each test was repeated three times, and the average value was recorded.
[0041] Corrosion test: Take a brass sheet (20mm×20mm×0.1mm), wash and dry it with anhydrous ethanol, and dry it in a 50℃ forced-air drying oven for 30 minutes. Place the treated brass sheet in a petri dish. Take 2g of each of the environmentally friendly aerosol fire extinguishing agents prepared in each example and comparative example, and prepare cylindrical samples with a diameter of 2cm. Place them together with the petri dish containing the brass sheet in a fire extinguishing chamber. After 30 minutes of burning, remove them and place them in an environment with a temperature of 30℃ and a humidity of 85% for 48 hours. After removing the surface corrosion with dilute hydrochloric acid, calculate the corrosion rate. ; Where ν is the corrosion rate, m0 is the initial mass of the brass sheet in g; m1 is the mass of the brass sheet after removing corrosion in g; and S is the surface area of the brass sheet in m². 2 t represents the corrosion time, measured in hours (h).
[0042] The results are shown in Table 1; A comparison of the experimental data from Examples 1-3 and Comparative Examples 1-12 in Table 1 shows that the environmentally friendly aerosol fire extinguishing agent prepared by the present invention has good fire extinguishing performance.
[0043] The comparison of data from Example 2 and Comparative Example 1 in the table illustrates that after potassium nitrate, strontium nitrate, and lactose form a co-crystallized material, the oxidant and combustible agent achieve a more uniform and tighter bond. This allows the material to react more quickly at lower temperatures, and the reaction is more complete, resulting in less residue after combustion. Most of the extinguishing agent is completely burned to generate aerosols, reducing the amount of residual corrosive substances. Furthermore, the combustion products are small particles, resulting in a small corrosion area and reducing corrosion damage, thereby improving fire extinguishing performance.
[0044] The comparison of data from Example 2 and Comparative Example 2 in the table demonstrates that the environmentally friendly aerosol fire extinguishing agent made from the oxidant-combustible agent co-crystallized material prepared by freeze-drying has better fire extinguishing performance. This is because, compared with the isothermal evaporation method, the co-crystallized material prepared by freeze-drying avoids the possibility of stepwise crystallization to a certain extent, making the combination of oxidant and combustible agent more uniform and compact, thus making combustion easier.
[0045] The comparison of data from Example 2 and Comparative Examples 3-4 in the table illustrates that as the calcination temperature increases, the pore size of the mesoporous catalyst increases while the specific surface area decreases; the pore walls collapse as the calcination temperature rises, forming larger pores, which leads to a decrease in fire extinguishing performance.
[0046] By comparing the data of Example 2 with those of Comparative Examples 5-8 in the table, it is shown that as the content of copper nitrate trihydrate increases, the specific surface area of the mesoporous catalyst also increases. When the mass ratio of ferric nitrate nonahydrate to copper nitrate trihydrate is 1:0.75, the specific surface area of the mesoporous catalyst is the largest. Further increasing the content of copper nitrate trihydrate will actually decrease the specific surface area, which will reduce the fire extinguishing performance of the environmentally friendly aerosol fire extinguishing agent.
[0047] By comparing the data from Example 2 with those from Comparative Examples 9-11 in the table, it is demonstrated that a mesoporous catalyst prepared by the sol-gel method using ferric nitrate nonahydrate, copper nitrate trihydrate, and propylene oxide temporarily stores oxygen from the decomposition of the oxidant in the extinguishing agent during combustion, which facilitates the rapid decomposition of the surrounding oxidant, reduces the activation energy of the combustion reaction, and promotes the combustion process of the extinguishing agent. When ferric oxide is used as a catalyst, it helps to lower the reaction temperature and shorten the extinguishing time. When copper oxide is used as a catalyst, it helps to lower the flame temperature and inhibit the formation of high-temperature flames, thereby further improving the extinguishing performance of the extinguishing agent. A mesoporous Fe2O3-CuO composite catalyst was prepared by the sol-gel method. The mesoporous structure has a high specific surface area and abundant mesoporous channels, which can provide more catalytic active sites, thereby further improving the extinguishing performance of the extinguishing agent.
[0048] The specific embodiments described above further illustrate the purpose, technical solution, and beneficial effects of the present invention. It should be understood that the above description is only a specific embodiment of the present invention and is not intended to limit the scope of protection of the present invention. Any modifications, equivalent substitutions, improvements, etc., made within the spirit and principles of the present invention should be included within the scope of protection of the present invention.
Claims
1. An environmentally friendly aerosol fire extinguishing agent, characterized in that, The environmentally friendly aerosol fire extinguishing agent includes an oxidant-combustible agent co-crystallization material, a mesoporous catalyst, hexamethylenetetramine, potassium oxalate, and phenolic resin. The oxidant-combustible agent co-crystallized material is prepared by co-crystallizing a mixture of potassium nitrate, strontium nitrate, and lactose. The mesoporous catalyst is prepared by ferric nitrate nonahydrate, copper nitrate trihydrate, and propylene oxide via a sol-gel method.
2. A method for preparing the environmentally friendly aerosol fire extinguishing agent as described in claim 1, characterized in that, The preparation method includes the following steps: (1) Mix potassium nitrate, strontium nitrate, lactose and deionized water evenly, dissolve by ultrasonic stirring, pre-freeze, vacuum dry, grind and sieve to obtain oxidant-combustible co-crystallized material; (2) Mix ferric nitrate nonahydrate, copper nitrate trihydrate and anhydrous ethanol evenly, stir and mix at room temperature, add propylene oxide, stir and mix, let stand for aging, vacuum dry, calcine in air to obtain mesoporous catalyst; (3) Mix the oxidant-combustible agent co-crystallization material, mesoporous catalyst, hexamethylenetetramine and potassium oxalate evenly, add phenolic resin ethanol solution, sieve and granulate, vacuum dry, pour into a pressing mold and press to form, and obtain an environmentally friendly aerosol fire extinguishing agent.
3. The preparation method of the environmentally friendly aerosol fire extinguishing agent according to claim 2, characterized in that, The mass ratio of potassium nitrate, strontium nitrate, lactose, and deionized water in step (1) is 1:(3~4):(0.6~0.7):(10~12).
4. The preparation method of the environmentally friendly aerosol fire extinguishing agent according to claim 2, characterized in that, The pre-freezing time in step (1) is 2-4 hours; the vacuum drying time is 15-20 hours.
5. The preparation method of the environmentally friendly aerosol fire extinguishing agent according to claim 2, characterized in that, The sieving in step (1) is sieving through an 80-100 mesh screen.
6. The preparation method of the environmentally friendly aerosol fire extinguishing agent according to claim 2, characterized in that, The mass ratio of ferric nitrate nonahydrate, copper nitrate trihydrate, anhydrous ethanol, and propylene oxide in step (2) is 1:(0.06~0.12):(10~12):(1.7~1.9).
7. The method for preparing the environmentally friendly aerosol fire extinguishing agent according to claim 2, characterized in that, The static aging process in step (2) is carried out at room temperature for 40-60 minutes.
8. The preparation method of the environmentally friendly aerosol fire extinguishing agent according to claim 2, characterized in that, The calcination temperature in step (2) is 300~400℃ and the calcination time is 4~6h.
9. The preparation method of the environmentally friendly aerosol fire extinguishing agent according to claim 2, characterized in that, The mass ratio of the oxidant-combustible co-crystallization material, mesoporous catalyst, hexamethylenetetramine, potassium oxalate, and phenolic resin ethanol solution in step (3) is 1: (0.02~0.04): (0.01~0.02): (0.01~0.02): (0.1~0.2).