A defoaming agent for seawater desalination and its preparation method

By synthesizing a high-temperature resistant defoamer with C18 stearamide hydrophobic group and polyoxyethylene/propylene block structure, the problem of poor defoaming performance of existing defoamers under high salt and high temperature conditions was solved, and the effects of rapid defoaming and continuous foam suppression were achieved.

CN123102007APending Publication Date: 2026-11-17JIANGSU SAIOUXINYUE DEFOAMER
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
CN202611623411.5
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-10-20
Publication Date
2026-11-17

AI Technical Summary

Technical Problem

Existing defoamers struggle to balance rapid defoaming and sustained foam suppression under high salinity and high temperature conditions, and their foam control performance is poor during seawater desalination.

Method used

A defoamer composed of stearic acid, potassium hydroxide, lauryl alcohol polyoxyethylene polyoxypropylene ether, high-temperature defoaming agent, polypropylene glycol, emulsifier, stabilizer and preservative is synthesized through a specific process. This high-temperature defoaming agent forms a C18 stearamide hydrophobic group, a central ethyl group and a double-arm inner polyoxypropylene/outer polyoxyethylene block structure, which enhances the stability of the foam interface and the migration ability of active molecules.

Benefits of technology

It improves the defoaming speed and sustained foam suppression ability of defoamer under high temperature conditions, adapts to the high salinity environment of seawater, and maintains good foam control effect.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123102007A_ABST
    Figure CN123102007A_ABST
Patent Text Reader

Abstract

This invention discloses a defoamer for seawater desalination and its preparation method, relating to the field of defoamer technology. The defoamer for seawater desalination comprises the following raw materials in parts by weight: 4-7 parts stearic acid, 0.2-0.4 parts potassium hydroxide, 16-22 parts lauryl alcohol polyoxyethylene polyoxypropylene ether, 2-5 parts high-temperature resistant defoaming agent, 5-10 parts polypropylene glycol, 0.6-1.2 parts emulsifier, 0.08-0.18 parts stabilizer, 0.02-0.05 parts preservative, and 50-70 parts deionized water. The defoamer for seawater desalination prepared by this invention exhibits excellent defoaming performance, foam suppression performance, and high-temperature resistance.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of defoamer technology, specifically to a defoamer for seawater desalination and its preparation method. Background Technology

[0002] Seawater desalination is an important technological means to solve the shortage of freshwater resources in coastal and island areas. It mainly includes thermal seawater desalination technologies such as multi-stage flash evaporation and low-temperature multi-effect distillation, as well as reverse osmosis membrane seawater desalination technology. During the thermal seawater desalination process, seawater is prone to foaming during heating, evaporation, and vapor-liquid separation. Excessive foam can affect liquid level control and vapor-liquid separation efficiency, and in severe cases, it may also cause salt droplet entrainment, reducing the quality of desalinated water. Therefore, defoamers are usually added to control foaming.

[0003] Currently, the defoamers used in seawater desalination mainly include polyether-based, organosilicon-based, and polyether-modified organosilicon-based defoamers. Compared with ordinary water systems, seawater has a higher salt concentration and contains sodium. + Cl - Ca 2+ Mg 2+ Inorganic salts, including polyether segments, affect the hydration state, hydrophilicity-hydrophobicity balance, and aggregation behavior of defoamers. This leads to changes in the dispersion state and interfacial activity of defoamers under different seawater salinity and concentration ratios, resulting in fluctuations in defoaming and foam suppression performance. Existing defoamers typically rely mainly on pre-formed polyethers, silicones, or hydrophobic particles, which are insufficient for utilizing the high salinity of seawater and metal ions. Furthermore, during thermal seawater desalination, seawater requires continuous heating. As the temperature rises, the hydration level of polyether segments decreases, and the hydrophilicity-hydrophobicity balance and aggregation state of the defoaming active phase easily change. Some active components may even aggregate or coarsen, leading to a decrease in effective interfacial activity under high-temperature conditions. Therefore, existing defoamers still suffer from difficulties in simultaneously achieving rapid defoaming and sustained foam suppression capabilities, and insufficient retention of high-temperature defoaming performance under high-temperature and long-term continuous operation conditions.

[0004] Chinese invention patent CN108499162A discloses a defoamer for seawater desalination, its preparation method, and its application. The defoamer includes silicone paste, polyether-modified organosilicon, emulsifier, thickener, and water. The silicone paste has a mass fraction of 5-20%, the polyether-modified organosilicon has a mass fraction of 10-30%, the emulsifier has a mass fraction of 2-10%, and the thickener has a mass fraction of 0.5-2%. The preparation method includes the following steps: (1) Weigh the silicone paste, polyether-modified organosilicon, and emulsifier according to the mass ratio, and mix them at 70-80℃ to obtain a mixture; (2) Prepare the thickener into an aqueous solution; (3) Inject less than 1 / 3 of the thickener aqueous solution into the mixture in step (1), mix evenly, and then add the remaining thickener aqueous solution in batches to obtain the defoamer. The defoamer prepared by this invention has the characteristics of high stability, fast defoaming rate, good foam suppression performance, and good compatibility with scale inhibitors, but its high-temperature defoaming performance is still insufficient. Therefore, it is necessary to further improve the defoaming performance retention and continuous foam suppression ability of defoamers under high salt and high temperature conditions. Summary of the Invention

[0005] To address the shortcomings of existing technologies, the purpose of this invention is to provide an antifoaming agent for seawater desalination and its preparation method.

[0006] To achieve the above objectives, the present invention provides the following technical solution:

[0007] An antifoaming agent for seawater desalination comprises the following raw materials in parts by weight:

[0008] Stearic acid 4-7 parts, potassium hydroxide 0.2-0.4 parts, lauryl alcohol polyoxyethylene polyoxypropylene ether 16-22 parts, high temperature resistant defoaming agent 2-5 parts, polypropylene glycol 5-10 parts, emulsifier 0.6-1.2 parts, stabilizer 0.08-0.18 parts, preservative 0.02-0.05 parts, deionized water 50-70 parts;

[0009] The high-temperature resistant defoaming agent is prepared by the following method:

[0010] S1: 2-Amino-2-ethyl-1,3-propanediol reacts with stearoyl chloride to give N-(1-hydroxy-2-(hydroxymethyl)but-2-yl)stearoamide;

[0011] S2: N-(1-hydroxy-2-(hydroxymethyl)but-2-yl)stearamide is obtained by reacting it with propylene oxide and then with ethylene oxide.

[0012] In step S1, the molar ratio of 2-amino-2-ethyl-1,3-propanediol to stearoyl chloride is (1.01-1.03):1.

[0013] In step S1, the reaction temperature is 25-35℃ and the time is 11-12h.

[0014] In step S2, the molar ratio of N-(1-hydroxy-2-(hydroxymethyl)but-2-yl)stearamide, propylene oxide, and ethylene oxide is 1:(17-19):(11-13).

[0015] In step S2, the reaction conditions with propylene oxide are as follows: first, add 4-6% of the total molar amount of propylene oxide, control the reaction temperature at 115-125℃, and maintain the temperature for 20-40 minutes after the addition; then, add 94-96% of the total molar amount of propylene oxide, control the reaction temperature at 115-125℃, and maintain the temperature for 0.5-1.5 hours after the addition.

[0016] In step S2, the reaction conditions with ethylene oxide are as follows: the reaction temperature is controlled at 110-120℃ during the addition of ethylene oxide, and the reaction is maintained at this temperature for 0.5-1.5h after the addition is completed.

[0017] The emulsifier is composed of sorbitan monostearate and polyoxyethylene sorbitan monostearate in a mass ratio of 1:(1.4-1.6).

[0018] The stabilizer is one of xanthan gum and hydroxyethyl cellulose.

[0019] The preservative is 1,2-benzisothiazolin-3-one.

[0020] A method for preparing an antifoaming agent for seawater desalination includes the following steps:

[0021] (1) Weigh out the following by weight: 4-7 parts stearic acid, 0.2-0.4 parts potassium hydroxide, 16-22 parts lauryl alcohol polyoxyethylene polyoxypropylene ether, 2-5 parts high temperature defoaming agent, 5-10 parts polypropylene glycol, 0.6-1.2 parts emulsifier, 0.08-0.18 parts stabilizer, 0.02-0.05 parts preservative, and 50-70 parts deionized water;

[0022] (2) Mix deionized water and stabilizer to obtain stabilizer solution; mix deionized water and stearic acid, stir and heat to 75-85℃, add potassium hydroxide and stir for 40-50 min; add lauryl alcohol polyoxyethylene polyoxypropylene ether, high temperature resistant defoaming agent, polypropylene glycol and emulsifier in sequence and stir; cool to 35-45℃, add stabilizer solution, stir and shear at high speed, add preservative, stir and defoam to obtain defoamer for seawater desalination.

[0023] Due to the adoption of the above technical solutions, the beneficial effects of the present invention include:

[0024] (1) The high-temperature resistant defoaming agent prepared in this application has a C18 stearamide hydrophobic group, a central ethyl group, and a double-arm inner polyoxypropylene / outer polyoxyethylene block structure. Among them, the C18 hydrophobic chain and amide structure enhance the anchoring and structural stability of the molecule at the bubble membrane interface, the central ethyl group regulates the core hydrophobicity and polyether segment configuration; the inner polyoxypropylene segment improves the hydrophobic interface affinity, and the outer polyoxyethylene segment maintains a moderate aqueous phase dispersion; as the temperature increases, the hydration of the polyoxyethylene segment weakens, which is conducive to the migration and enrichment of active molecules to the gas-liquid interface, while the inner polyoxypropylene segment and C18 hydrophobic structure maintain a strong bubble membrane affinity. The various structures work together to maintain a suitable balance between aqueous phase dispersion, interface migration, hydrophobic defoaming, and high-temperature aggregation, thereby improving the sustained foam suppression and high-temperature defoaming performance.

[0025] (2) This application combines lauryl alcohol polyoxyethylene polyoxypropylene ether, polypropylene glycol, and a high-temperature resistant defoaming agent to form a defoaming active phase, taking into account the dispersion, interfacial migration, spreading, and high-temperature stability of the active components; simultaneously, stearic acid is partially neutralized by potassium hydroxide to form a composite fatty acid phase composed of unneutralized stearic acid and a small amount of potassium stearate, wherein the unneutralized stearic acid enhances the hydrophobic defoaming effect, and the small amount of potassium stearate improves the dispersion state of the active components. (The text abruptly ends here, likely due to an incomplete translation or source material.) 2+ Mg 2+ After being processed in a seawater system, some potassium stearate can undergo ion exchange with divalent metal ions to form highly hydrophobic metal stearate microdomains, further enhancing the local hydrophobicity and interfacial disturbance of the bubble film. The synergistic effect of the composite polyether active phase, the partially neutralized fatty acid phase, and the emulsion stabilizing system promotes bubble film drainage, thinning, and rupture, giving the defoamer a combination of rapid defoaming speed, good sustained foam suppression ability, and high-temperature adaptability. Attached Figure Description

[0026] Figure 1 Fourier transform infrared spectra of 2-amino-2-ethyl-1,3-propanediol, N-(1-hydroxy-2-(hydroxymethyl)but-2-yl)stearamide and high-temperature defoaming agent in Example 1. Detailed Implementation

[0027] The following description, in conjunction with specific embodiments, provides further details, but the present invention is not limited to these embodiments.

[0028] Example 1: Preparation of High-Temperature Resistant Defoamer

[0029] S1: Under nitrogen protection, 120 ml of anhydrous DMF (N,N-dimethylformamide), 0.101 mol of 2-amino-2-ethyl-1,3-propanediol, and 0.11 mol of triethylamine were mixed and stirred at 300 rpm for 20 min. At 0 °C, 100 ml of anhydrous DMF solution containing 0.1 mol of stearoyl chloride was added dropwise at 300 rpm over 60 min. The mixture was then heated to 25 °C and reacted for 12 h. The mixture was then added to 500 ml of deionized water, stirred at 300 rpm for 20 min, allowed to stand for 30 min, filtered, and the filter cake was washed with deionized water until the pH of the washing solution reached 7. The mixture was then vacuum dried at 70 °C and a gauge pressure of -0.09 MPa for 6 h to obtain N-(1-hydroxy-2-(hydroxymethyl)but-2-yl)stearoamide. The reaction equation is shown below:

[0030]

[0031] Its proton NMR spectrum data are as follows: 1 H NMR (400 MHz, Chloroform-d) δ 6.59 (s, 1H), 4.14 (t, J = 5.0 Hz, 2H), 3.59 (d, J = 5.0 Hz, 4H), 2.18 (t, J = 7.6 Hz, 2H), 1.67-1.51 (m, 4H), 1.36-1.23 (m, 28H), 0.89 (t, J = 6.6 Hz, 6H); HRMS (m / z):386.3630[M+H] + .

[0032] S2: Add 0.1 mol N-(1-hydroxy-2-(hydroxymethyl)but-2-yl)stearamide and 0.003 mol anhydrous potassium hydroxide to a high-pressure reactor. Seal the reactor and purge with dry nitrogen for 30 min. Under nitrogen protection, heat to 110℃ and stir at 300 rpm for 20 min. Heat to 115℃, add 0.068 mol propylene oxide over 8 min, controlling the reaction temperature at 115℃ and the gauge pressure not exceeding 0.15 MPa during the addition. After the addition, maintain the reaction temperature for 40 min. Then add 1.632 mol propylene oxide over 2.5 h, controlling the reaction temperature at 115℃ and the gauge pressure not exceeding 0.3 MPa during the addition. After the addition, maintain the reaction temperature for 1.5 h. Cool to 110℃ and add 1.1 mol ethylene oxide over 1.5 h, controlling the reaction temperature at 110℃ and the gauge pressure not exceeding 0.25 MPa during the addition. a. After addition, maintain the temperature for 1.5 h; cool to 90℃, restore atmospheric pressure, and then distill under reduced pressure at -0.09 MPa until no obvious distillate is obtained; cool to 75℃, restore atmospheric pressure, add 0.003 mol glacial acetic acid, stir at 300 rpm for 30 min, dry at 80℃ and -0.09 MPa for 2 h, and cool to room temperature to obtain a high-temperature resistant defoaming agent; during the above reaction, the hydroxyl groups in N-(1-hydroxy-2-(hydroxymethyl)but-2-yl)stearamide form alkoxide active sites under the action of potassium hydroxide. The alkoxide active sites initiate the ring-opening addition of propylene oxide and continue to grow the chain, forming an inner polyether segment mainly composed of polyoxypropylene units; then ethylene oxide is added, and ethylene oxide continues to undergo a ring-opening addition reaction at the active sites at the end of the polyether chain, so that the polyoxyethylene units are mainly distributed on the outside of the polyether segment, thereby forming a polyether structure of polyoxypropylene / polyoxyethylene sequential addition.

[0033] Figure 1 Fourier transform infrared spectra of 2-amino-2-ethyl-1,3-propanediol, N-(1-hydroxy-2-(hydroxymethyl)but-2-yl)stearamide, and a high-temperature defoaming agent. The figure shows that 2-amino-2-ethyl-1,3-propanediol exhibits high activity in the range of approximately 3390-3240 cm⁻¹. -1 OH and NH related absorption peaks appeared at 1604 cm⁻¹. -1 The nearby peak is an amino-related absorption peak, at 1060 cm⁻¹. -1 The CO absorption peak is located near this point. N-(1-hydroxy-2-(hydroxymethyl)but-2-yl)stearamide shows an absorption peak at 1648 cm⁻¹. -1 and 1543cm -1 Amide I and Amide II bands appeared nearby, and at 2922 cm⁻¹ -1 and 2852cm -1 The absorption peak of the CH stretching vibration is enhanced near 721 cm⁻¹. -1The presence of a long-chain methylene-related absorption peak nearby indicates that the stearoyl group has been introduced into the molecule through the amide structure; simultaneously, at approximately 3390 cm⁻¹... -1 A relatively broad OH absorption peak is still retained at this point, indicating that the hydroxyl structure still exists. Compared with N-(1-hydroxy-2-(hydroxymethyl)but-2-yl)stearamide, the high-temperature resistant defoamer exhibits a higher absorption peak at 1104 cm⁻¹. -1 The absorption peak of COC in the vicinity is significantly enhanced, and at 1374 cm⁻¹... -1 Enhanced absorption associated with methyl groups on the side of the polyoxypropylene chain, 1645 cm⁻¹ -1 and 1541cm -1 The amide characteristic peaks in the vicinity are still retained. The above results indicate that the prepared high-temperature resistant defoamer contains both long-chain stearamide structures and polyoxypropylene and polyoxyethylene ether segments.

[0034] Example 2 Preparation of high-temperature resistant defoaming agent

[0035] S1: Under nitrogen protection, 120 ml of anhydrous DMF, 0.102 mol of 2-amino-2-ethyl-1,3-propanediol, and 0.11 mol of triethylamine were mixed and stirred at 300 rpm for 20 min. At 3 °C, 100 ml of anhydrous DMF solution containing 0.1 mol of stearoyl chloride was added dropwise at 300 rpm for 60 min. After the addition was completed, the temperature was raised to 30 °C and the reaction was carried out for 11.5 h. The mixture was then added to 500 ml of deionized water, stirred at 300 rpm for 20 min, allowed to stand for 30 min, filtered, and the filter cake was washed with deionized water until the pH of the washing solution reached 7. The mixture was then vacuum dried at 70 °C and a gauge pressure of -0.09 MPa for 6 h to obtain N-(1-hydroxy-2-(hydroxymethyl)but-2-yl)stearoamide.

[0036] S2: Add 0.1 mol N-(1-hydroxy-2-(hydroxymethyl)but-2-yl)stearamide and 0.003 mol anhydrous potassium hydroxide to a high-pressure reactor. Seal the reactor and purge with dry nitrogen for 30 min. Under nitrogen protection, raise the temperature to 110℃ and stir at 300 rpm for 20 min. Raise the temperature to 120℃, add 0.09 mol propylene oxide over 10 min, controlling the reaction temperature at 120℃ and the gauge pressure not exceeding 0.15 MPa during the addition. After the addition is complete, maintain the reaction temperature for 30 min, then add 1.71 mol propylene oxide over 3 h, controlling the reaction temperature at 12℃ during the addition. At 0℃ and with a gauge pressure not exceeding 0.3MPa, the reaction was maintained at this temperature for 1 hour after the addition was completed. The temperature was then lowered to 115℃, and 1.2 mol of ethylene oxide was added over a period of 2 hours, with the reaction temperature controlled at 115℃ and the gauge pressure not exceeding 0.25MPa during the addition process. The reaction was then maintained at this temperature for 1 hour after the addition was completed. The temperature was then lowered to 90℃ and restored to normal pressure. The mixture was then distilled under reduced pressure at a gauge pressure of -0.09MPa until no obvious distillate was observed. The temperature was then lowered to 75℃ and restored to normal pressure. 0.003 mol of glacial acetic acid was added, and the mixture was stirred at 300 rpm for 30 minutes. The mixture was then dried at 80℃ and a gauge pressure of -0.09MPa for 2 hours and cooled to room temperature to obtain a high-temperature resistant defoaming agent.

[0037] Example 3 Preparation of high-temperature resistant defoaming agent

[0038] S1: Under nitrogen protection, 120 ml of anhydrous DMF, 0.103 mol of 2-amino-2-ethyl-1,3-propanediol, and 0.11 mol of triethylamine were mixed and stirred at 300 rpm for 20 min. At 5 °C, 100 ml of anhydrous DMF solution containing 0.1 mol of stearoyl chloride was added dropwise at 300 rpm for 60 min. After the addition was completed, the temperature was raised to 35 °C and the reaction was carried out for 11 h. The mixture was then added to 500 ml of deionized water, stirred at 300 rpm for 20 min, allowed to stand for 30 min, filtered, and the filter cake was washed with deionized water until the pH of the washing solution reached 7. The mixture was then vacuum dried at 70 °C and a gauge pressure of -0.09 MPa for 6 h to obtain N-(1-hydroxy-2-(hydroxymethyl)but-2-yl)stearoamide.

[0039] S2: Add 0.1 mol N-(1-hydroxy-2-(hydroxymethyl)but-2-yl)stearamide and 0.003 mol anhydrous potassium hydroxide to a high-pressure reactor. Seal the reactor and purge with dry nitrogen for 30 min. Under nitrogen protection, raise the temperature to 110℃ and stir at 300 rpm for 20 min. Raise the temperature to 125℃, add 0.114 mol propylene oxide over 12 min, controlling the reaction temperature at 125℃ and the gauge pressure not exceeding 0.15 MPa during the addition. After the addition is complete, maintain the reaction temperature for 20 min, then add 1.786 mol propylene oxide over 3.5 h, controlling the reaction temperature at 125℃ during the addition. The temperature was set at 120℃, and the gauge pressure was not higher than 0.3 MPa. After the addition was completed, the reaction was kept at this temperature for 0.5 h. The temperature was then lowered to 120℃, and 1.3 mol of ethylene oxide was added over a period of 2.5 h. During the addition, the reaction temperature was controlled at 120℃ and the gauge pressure was not higher than 0.25 MPa. After the addition was completed, the reaction was kept at this temperature for 0.5 h. The temperature was then lowered to 90℃, and the pressure was restored to normal. The mixture was then distilled under reduced pressure at a gauge pressure of -0.09 MPa until no obvious distillate was obtained. The temperature was then lowered to 75℃, and the pressure was restored to normal. 0.003 mol of glacial acetic acid was added, and the mixture was stirred at 300 rpm for 30 min. The mixture was then dried at 80℃ and a gauge pressure of -0.09 MPa for 2 h. After cooling to room temperature, the high-temperature resistant defoaming agent was obtained.

[0040] Example 4: Preparation of defoamer for seawater desalination

[0041] (1) Weigh the following by weight: 4g stearic acid, 0.2g potassium hydroxide, 16g lauryl alcohol polyoxyethylene polyoxypropylene ether, 2g high temperature resistant defoaming agent (prepared in Example 1), 5g polypropylene glycol (PPG1000), 0.6g emulsifier (0.25g sorbitan monostearate, 0.35g polyoxyethylene sorbitan monostearate), 0.08g stabilizer (xanthan gum), 0.02g preservative (1,2-benzisothiazolin-3-one), and 50g deionized water;

[0042] (2) Mix 12.5g of deionized water with the stabilizer and stir at 35°C and 500rpm for 40min to obtain the stabilizer solution; mix 37.5g of deionized water and stearic acid, heat to 75°C under stirring at 500rpm, add potassium hydroxide, and stir for 50min; add lauryl alcohol polyoxyethylene polyoxypropylene ether, high temperature defoaming agent, polypropylene glycol, and emulsifier in sequence under stirring at 500rpm, and continue stirring for 30min; cool to 35°C, add the stabilizer solution, stir at 500rpm for 20min, and then shear at 4000rpm for 10min; cool to 25°C, add the preservative, stir at 500rpm for 10min, and defoam under vacuum at 25°C and gauge pressure -0.08MPa for 15min to obtain the defoamer for seawater desalination.

[0043] Example 5 Preparation of defoamer for seawater desalination

[0044] (1) Weigh the following by weight: 5.5g stearic acid, 0.3g potassium hydroxide, 20g lauryl alcohol polyoxyethylene polyoxypropylene ether, 3.5g high temperature resistant defoaming agent (prepared in Example 2), 8g polypropylene glycol (PPG1000), 0.8g emulsifier (0.32g sorbitan monostearate, 0.48g polyoxyethylene sorbitan monostearate), 0.13g stabilizer (xanthan gum), 0.04g preservative (1,2-benzisothiazolin-3-one), and 60g deionized water;

[0045] (2) Mix 15g of deionized water with the stabilizer and stir at 35°C and 500rpm for 40min to obtain the stabilizer solution; mix 45g of deionized water and stearic acid, heat to 80°C under stirring at 500rpm, add potassium hydroxide, and stir for 45min; add lauryl alcohol polyoxyethylene polyoxypropylene ether, high temperature defoaming agent, polypropylene glycol and emulsifier in sequence under stirring at 500rpm, and continue stirring for 30min; cool to 40°C, add the stabilizer solution, stir at 500rpm for 20min, and then shear at 5000rpm for 8min; cool to 25°C, add the preservative, stir at 500rpm for 10min, and vacuum defoam at 25°C and gauge pressure -0.08MPa for 15min to obtain the defoamer for seawater desalination.

[0046] Example 6 Preparation of defoamer for seawater desalination

[0047] (1) Weigh the following by weight: 7g stearic acid, 0.4g potassium hydroxide, 22g lauryl alcohol polyoxyethylene polyoxypropylene ether, 5g high-temperature defoaming agent (prepared in Example 3), 10g polypropylene glycol (PPG1000), 1.2g emulsifier (0.46g sorbitan monostearate, 0.74g polyoxyethylene sorbitan monostearate), 0.18g stabilizer (hydroxyethyl cellulose), 0.05g preservative (1,2-benzisothiazolin-3-one), and 70g deionized water;

[0048] (2) Mix 17.5g of deionized water with the stabilizer and stir at 35°C and 500rpm for 40min to obtain the stabilizer solution; separately mix 52.5g of deionized water and stearic acid, heat to 85°C under stirring at 500rpm, add potassium hydroxide, and stir for 40min; under stirring at 500rpm, add lauryl alcohol polyoxyethylene polyoxypropylene ether, high temperature defoaming agent, polypropylene glycol, and emulsifier in sequence, and continue stirring for 30min; cool down to 45°C, add the stabilizer solution, stir at 500rpm for 20min, and then shear at 6000rpm for 5min; cool down to 25°C, add the preservative, stir at 500rpm for 10min, and vacuum defoam at 25°C and gauge pressure -0.08MPa for 15min to obtain the defoamer for seawater desalination.

[0049] Comparative Example 1

[0050] The raw material composition and preparation method of the defoamer for seawater desalination are basically the same as those in Example 5, except that the high-temperature resistant defoaming agent is replaced with an equal weight of a high-temperature resistant defoaming agent prepared by the following method:

[0051] The preparation method of the high-temperature resistant defoaming agent is basically the same as that in Example 2, except that 2-amino-2-ethyl-1,3-propanediol in step S1 is replaced with an equimolar amount of tris(hydroxymethyl)aminomethane.

[0052] Comparative Example 2

[0053] The raw material composition and preparation method of the defoamer for seawater desalination are basically the same as those in Example 5, except that the high-temperature resistant defoaming agent is replaced with an equal weight of a high-temperature resistant defoaming agent prepared by the following method:

[0054] The preparation method of the high-temperature resistant defoaming agent is basically the same as that in Example 2, except that 2-amino-2-ethyl-1,3-propanediol in step S1 is replaced with an equimolar amount of 2-amino-2-ethylbutane-1-ol.

[0055] Comparative Example 3

[0056] The raw material composition and preparation method of the defoamer for seawater desalination are basically the same as those in Example 5, except that the high-temperature resistant defoaming agent is replaced with an equal weight of a high-temperature resistant defoaming agent prepared by the following method:

[0057] The preparation method of the high-temperature resistant defoaming agent is basically the same as that in Example 2, except that 2-amino-2-ethyl-1,3-propanediol in step S1 is replaced with an equimolar amount of 2-amino-2-methyl-1,3-propanediol.

[0058] Comparative Example 4

[0059] The raw material composition and preparation method of the defoamer for seawater desalination are basically the same as those in Example 5, except that the high-temperature resistant defoaming agent is replaced with an equal weight of a high-temperature resistant defoaming agent prepared by the following method:

[0060] The preparation method of the high-temperature resistant defoaming agent is basically the same as that in Example 2, except that the stearoyl chloride in step S1 is replaced with an equimolar amount of palmitoyl chloride.

[0061] Comparative Example 5

[0062] The raw material composition and preparation method of the defoamer for seawater desalination are basically the same as those in Example 5, except that the high-temperature resistant defoaming agent is replaced with an equal weight of a high-temperature resistant defoaming agent prepared by the following method:

[0063] The preparation method of the high-temperature resistant defoaming agent is basically the same as that in Example 2, except that the stearoyl chloride in step S1 is replaced with an equimolar amount of eicosanoyl chloride.

[0064] Comparative Example 6

[0065] The raw material composition and preparation method of the defoamer for seawater desalination are basically the same as those in Example 5, except that the high-temperature resistant defoaming agent is replaced with an equal weight of a high-temperature resistant defoaming agent prepared by the following method:

[0066] The preparation method of the high-temperature resistant defoaming agent is basically the same as that in Example 2, except that the preparation method of step S2 is as follows:

[0067] S2: Add 0.1 mol N-(1-hydroxy-2-(hydroxymethyl)but-2-yl)stearamide and 0.003 mol anhydrous potassium hydroxide to a high-pressure reactor. Seal the reactor and purge with dry nitrogen for 30 min. Under nitrogen protection, raise the temperature to 110℃ and stir at 300 rpm for 20 min. Raise the temperature to 120℃, add 0.12 mol propylene oxide over 10 min, controlling the reaction temperature at 120℃ and the gauge pressure not exceeding 0.15 MPa during the addition. After the addition is complete, maintain the reaction temperature for 30 min, then add 2.28 mol propylene oxide over 3 h, controlling the reaction temperature at 12℃ during the addition. At 0℃ and with a gauge pressure not exceeding 0.3 MPa, the reaction was maintained at this temperature for 1 hour after the addition was completed. The temperature was then lowered to 115℃, and 0.6 mol of ethylene oxide was added over a period of 2 hours, with the reaction temperature controlled at 115℃ and the gauge pressure not exceeding 0.25 MPa during the addition process. The reaction was then maintained at this temperature for 1 hour after the addition was completed. The temperature was then lowered to 90℃ and restored to normal pressure. The mixture was then distilled under reduced pressure at a gauge pressure of -0.09 MPa until no obvious distillate was observed. The temperature was then lowered to 75℃ and restored to normal pressure. 0.003 mol of glacial acetic acid was added, and the mixture was stirred at 300 rpm for 30 minutes. The mixture was then dried at 80℃ and a gauge pressure of -0.09 MPa for 2 hours and cooled to room temperature to obtain a high-temperature resistant defoaming agent.

[0068] Comparative Example 7

[0069] The raw material composition and preparation method of the defoamer for seawater desalination are basically the same as those in Example 5, except that the high-temperature resistant defoaming agent is replaced with an equal weight of a high-temperature resistant defoaming agent prepared by the following method:

[0070] The preparation method of the high-temperature resistant defoaming agent is basically the same as that in Example 2, except that the preparation method of step S2 is as follows:

[0071] S2: Add 0.1 mol N-(1-hydroxy-2-(hydroxymethyl)but-2-yl)stearamide and 0.003 mol anhydrous potassium hydroxide to a high-pressure reactor. Seal the reactor and purge with dry nitrogen for 30 min. Under nitrogen protection, raise the temperature to 110℃ and stir at 300 rpm for 20 min. Purge with dry nitrogen to restore atmospheric pressure and raise the temperature to 120℃. First, add 0.06 mol propylene oxide over 10 min, controlling the reaction temperature at 120℃ and the gauge pressure not exceeding 0.15 MPa during the addition. After the addition is complete, maintain the reaction temperature for 30 min. Then add 1.14 mol propylene oxide over 3 h, controlling the reaction temperature during the addition. The reaction should be carried out at 120℃ with a gauge pressure not exceeding 0.3MPa for 1 hour after the addition is completed. The temperature should then be lowered to 115℃, and 1.8 mol of ethylene oxide should be added over 2 hours, maintaining the reaction temperature at 115℃ and the gauge pressure not exceeding 0.25MPa during the addition. The reaction should be carried out for 1 hour after the addition is completed. The temperature should then be lowered to 90℃ and restored to normal pressure. The mixture should then be distilled under reduced pressure (gauge pressure -0.09MPa) until no obvious distillate is obtained. The temperature should then be lowered to 75℃ and restored to normal pressure. 0.003 mol of glacial acetic acid should be added, and the mixture should be stirred at 300 rpm for 30 minutes. The mixture should then be dried at 80℃ and gauge pressure -0.09MPa for 2 hours and cooled to room temperature to obtain a high-temperature resistant defoaming agent.

[0072] Comparative Example 8

[0073] The raw material composition and preparation method of the defoamer for seawater desalination are basically the same as those in Example 5, except that the high-temperature resistant defoaming agent is replaced with an equal weight of a high-temperature resistant defoaming agent prepared by the following method:

[0074] The preparation method of the high-temperature resistant defoaming agent is basically the same as that in Example 2, except that the preparation method of step S2 is as follows:

[0075] S2: Add 0.1 mol N-(1-hydroxy-2-(hydroxymethyl)but-2-yl)stearamide and 0.003 mol anhydrous potassium hydroxide to a high-pressure reactor. Seal the reactor and purge with dry nitrogen for 30 min. Under nitrogen protection, raise the temperature to 110℃ and stir at 300 rpm for 20 min. Raise the temperature to 115℃, add 0.06 mol ethylene oxide over 10 min, controlling the reaction temperature at 115℃ and the gauge pressure not exceeding 0.15 MPa during the addition. After the addition is complete, maintain the reaction temperature for 30 min, then add 1.14 mol ethylene oxide over 2 h, controlling the reaction temperature at 11℃ during the addition. At 5℃ and a gauge pressure not exceeding 0.25MPa, the reaction was maintained at this temperature for 1 hour after the addition was completed. The temperature was then raised to 120℃, and 1.8 mol of propylene oxide was added over a period of 3 hours, with the reaction temperature controlled at 120℃ and the gauge pressure not exceeding 0.3MPa during the addition. The reaction was then maintained at this temperature for 1 hour after the addition was completed. The temperature was lowered to 90℃ and restored to normal pressure. The mixture was then distilled under reduced pressure at a gauge pressure of -0.09MPa until no obvious distillate was obtained. The temperature was lowered to 75℃ and restored to normal pressure. 0.003 mol of glacial acetic acid was added, and the mixture was stirred at 300 rpm for 30 minutes. The mixture was then dried at 80℃ and a gauge pressure of -0.09MPa for 2 hours and cooled to room temperature to obtain a high-temperature resistant defoaming agent.

[0076] The lauryl alcohol polyoxyethylene polyoxypropylene ether used in the embodiments and comparative examples of this application is of the ALKOMOL type. ® L408 contains ethylene oxide (EO) with a degree of polymerization of 4 and propylene oxide (PO) with a degree of polymerization of 8; xanthan gum is model Ziboxan®FT, produced by Ordos Zhongxuan Biochemical Co., Ltd.; hydroxyethyl cellulose is model HS-6000S, produced by Shandong Xuanhai Chemical Co., Ltd.

[0077] The defoaming and foam-suppressing properties and high-temperature resistance of the defoamers prepared in the examples and comparative examples were tested, and the test results are shown in Table 1.

[0078] Preparation of simulated seawater: Add 23.6g sodium chloride, 11.1g magnesium chloride hexahydrate, 4.09g anhydrous sodium sulfate, 1.54g calcium chloride dihydrate, 0.7g potassium chloride, 0.2g sodium bicarbonate, and 0.1g potassium bromide to 800ml of deionized water in sequence. Stir at 300rpm for 20min. Adjust the pH to 8 using 0.1mol / L hydrochloric acid or 0.1mol / L sodium hydroxide aqueous solution. Make up the volume to 1L with deionized water to obtain simulated seawater.

[0079] Preparation of defoamer dilution: Mix defoamer with deionized water at a mass ratio of 1:999, stir at 300 rpm for 5 min to obtain a defoamer dilution with a mass fraction of 0.1 wt%, and use immediately after preparation.

[0080] Preparation of foaming solution: Sodium dodecylbenzenesulfonate and simulated seawater are mixed at a mass ratio of 1:999 and stirred at 300 rpm for 10 min to obtain a foaming solution with a mass fraction of 0.1 wt%. It should be prepared and used immediately.

[0081] Defoaming performance test: At 25℃, pour 100ml of foaming liquid into a 500ml graduated cylinder, and bubble with nitrogen gas at a flow rate of 1L / min until the 500ml mark is reached. Stop the gas flow, add 0.8g of 0.1wt% defoamer dilution, and immediately use an electronic stopwatch to record the time when the foam volume is ≤10ml. Repeat the test 3 times and take the average value as the final defoaming time.

[0082] Defoaming performance test: At 25℃, pour 100ml of foaming liquid into a 500ml graduated cylinder, add 0.2g of 0.1wt% defoamer dilution, then start introducing nitrogen gas at a flow rate of 2L / min while simultaneously timing with an electronic stopwatch. Stop timing when the bubbles reach the 500ml mark and record the defoaming time. Repeat the test 3 times and take the average value as the final defoaming time.

[0083] High-temperature resistance test: Pour 100ml of foaming liquid into a 500ml graduated cylinder, place the graduated cylinder in a 90℃ constant temperature water bath, maintain the temperature for 15min, then bubble with nitrogen gas at a flow rate of 1L / min until the 500ml mark is reached. Stop the gas flow, add 0.2g of 0.1wt% defoamer dilution, and immediately use an electronic stopwatch to record the time when the foam volume is ≤10ml. Repeat the test 3 times, and take the average value as the final defoaming time at 90℃.

[0084] Table 1. Defoamer Performance Test Data

[0085] project Defoaming time / s Defoaming time / min Defoaming time at 90℃ / s Example 4 4.6 10.9 5.2 Example 5 4.5 11.2 5.1 Example 6 4.8 10.5 5.3 Comparative Example 1 9.6 8.0 11.9 Comparative Example 2 4.8 9.8 6.2 Comparative Example 3 4.7 10.1 6.4 Comparative Example 4 6.4 8.7 8.3 Comparative Example 5 4.9 9.4 6.5 Comparative Example 6 5.1 9.3 7.0 Comparative Example 7 8.0 8.6 9.7 Comparative Example 8 4.7 9.5 6.1

[0086] As can be seen from Table 1, the defoamer for seawater desalination prepared in the embodiments of this application has good defoaming performance, foam suppression performance and high temperature resistance.

[0087] In Comparative Example 1, replacing 2-amino-2-ethyl-1,3-propanediol with tris(hydroxymethyl)aminomethane resulted in a high-temperature defoaming agent that increased from two hydroxyl initiation sites to three, while lacking a central ethyl structure. With the total amounts of propylene oxide and ethylene oxide remaining constant, the polyether segments were distributed across more initiation sites, leading to a relatively shorter single-branch polyether chain, increased molecular branching, and altered hydrophilic-hydrophobic balance and spatial configuration between the hydrophobic core and polyether segments. The higher degree of branching and weaker core hydrophobicity hindered the effective migration, spreading, and retention of active molecules at the gas-liquid interface, thus reducing both defoaming and foam-suppressing performance.

[0088] In Comparative Example 2, 2-amino-2-ethylbutane-1-ol containing only one hydroxyl group was used to form a structure mainly composed of single-arm polyether. With the total amount of propylene oxide and ethylene oxide added remaining unchanged, the length of the polyether single chain increased, and the original double-arm structure was transformed into an asymmetric single-arm structure. This structure still has strong interfacial migration and bubble film disturbance capabilities under room temperature conditions, but a single long polyether chain is difficult to form the spatial dispersion and interfacial stabilization effect of the double-arm structure. Under high salt and high temperature conditions, the aggregation state and hydrophilic-hydrophobic balance of active molecules are more likely to change, resulting in a decrease in continuous foam suppression and defoaming performance at 90℃.

[0089] In Comparative Example 3, the central ethyl group was replaced with a methyl group. Although the two-arm polyether structure was still maintained, the hydrophobicity and steric hindrance of the molecular core region were reduced, which weakened the interfacial affinity and retention ability under high temperature conditions. Therefore, the high-temperature defoaming performance was reduced.

[0090] In Comparative Example 4, the C18 stearyl group was replaced with the C16 palmitoyl group, which shortened the hydrophobic chain length, reduced the hydrophobic anchoring ability of the molecule, and reduced the ability of the active molecule to form a stable hydrophobic effect after entering the bubble film and the residence time at the gas-liquid interface. Therefore, the defoaming, sustained foam suppression and high-temperature defoaming performance all decreased.

[0091] In Comparative Example 5, C20 eicosanoyl groups were used, which further increased the hydrophobic chain length. Although this enhanced the hydrophobic interface effect of the molecules, the excessively long hydrophobic chain also reduced the dispersion ability of the active molecules in the aqueous phase and increased the tendency of association and aggregation between hydrophobic molecules. Under continuous bubbling and high temperature conditions, this aggregation effect became more obvious, which limited the continuous replenishment of effective active components to the bubble film interface, resulting in a decrease in continuous foam suppression and high temperature defoaming performance.

[0092] In Comparative Example 6, the increased proportion of polyoxypropylene and the decreased proportion of polyoxyethylene segments resulted in insufficient hydration and dispersion stability between the polyether chain and the aqueous phase. At the same time, the higher proportion of polyoxypropylene segments enhanced the tendency of hydrophobic association and aggregation between molecules, which affected the uniform dispersion and continuous interfacial replenishment of the active phase under high salt and high temperature conditions, leading to a decrease in foam suppression and defoaming performance at 90℃.

[0093] In Comparative Example 7, the increased proportion of polyoxyethylene (PE) improved the dispersibility of the aqueous phase, but also enhanced the overall hydrophilicity of the molecules, reducing their migration to the bubble membrane interface and their hydrophobic defoaming ability, thus leading to a decrease in rapid defoaming performance. At the same time, the excessive bias of active molecules towards the continuous aqueous phase was not conducive to their continuous enrichment at the newly formed bubble membrane interface and the formation of effective hydrophobic disturbances, resulting in a decrease in defoaming performance. As the temperature increased, the hydration state of the PE chain segments changed further, making it easier to alter the original hydrophilic-hydrophobic balance and aggregation state, resulting in a decrease in defoaming performance at 90℃.

[0094] In Comparative Example 8, the addition sequence of epoxy monomers was changed to form an inner polyoxyethylene / outer polyoxypropylene structure. The outer polyoxypropylene layer improved the hydrophobic interface affinity at room temperature, thus resulting in better defoaming performance at room temperature. However, the hydration capacity of the outer layer was reduced, and it was more prone to hydrophobic aggregation at high temperatures, which reduced the sustained foam suppression and high-temperature defoaming performance.

[0095] The above description is merely a preferred embodiment of the present invention and is not intended to limit the present invention. However, any modifications, alterations, and variations made by those skilled in the art without departing from the scope of the present invention based on the disclosed technical content are equivalent embodiments of the present invention. Furthermore, any modifications, alterations, and variations made to the above embodiments based on the essential technology of the present invention are still within the protection scope of the present invention.

Claims

1. A defoaming agent for seawater desalination, characterized in that, The ingredients include the following parts by weight: Stearic acid 4-7 parts, potassium hydroxide 0.2-0.4 parts, lauryl alcohol polyoxyethylene polyoxypropylene ether 16-22 parts, high temperature resistant defoaming agent 2-5 parts, polypropylene glycol 5-10 parts, emulsifier 0.6-1.2 parts, stabilizer 0.08-0.18 parts, preservative 0.02-0.05 parts, deionized water 50-70 parts; The high-temperature resistant defoaming agent is prepared by the following method: S1: 2-Amino-2-ethyl-1,3-propanediol reacts with stearoyl chloride to give N-(1-hydroxy-2-(hydroxymethyl)but-2-yl)stearoamide; S2: N-(1-hydroxy-2-(hydroxymethyl)but-2-yl)stearamide is obtained by reacting it with propylene oxide and then with ethylene oxide.

2. The defoamer for seawater desalination according to claim 1, characterized in that, In step S1, the molar ratio of 2-amino-2-ethyl-1,3-propanediol to stearoyl chloride is (1.01-1.03):

1.

3. The defoamer for seawater desalination according to claim 1, characterized in that, In step S1, the reaction temperature is 25-35℃ and the time is 11-12h.

4. The defoamer for seawater desalination according to claim 1, characterized in that, In step S2, the molar ratio of N-(1-hydroxy-2-(hydroxymethyl)but-2-yl)stearamide, propylene oxide, and ethylene oxide is 1:(17-19):(11-13).

5. The defoamer for seawater desalination according to claim 1, characterized in that, In step S2, the reaction conditions with propylene oxide are as follows: first, add 4-6% of the total molar amount of propylene oxide, control the reaction temperature at 115-125℃, and maintain the temperature for 20-40 minutes after the addition; then, add 94-96% of the total molar amount of propylene oxide, control the reaction temperature at 115-125℃, and maintain the temperature for 0.5-1.5 hours after the addition.

6. The defoamer for seawater desalination according to claim 1, characterized in that, In step S2, the reaction conditions with ethylene oxide are as follows: the reaction temperature is controlled at 110-120℃ during the addition of ethylene oxide, and the reaction is maintained at this temperature for 0.5-1.5h after the addition is completed.

7. The defoamer for seawater desalination according to claim 1, characterized in that, The emulsifier is composed of sorbitan monostearate and polyoxyethylene sorbitan monostearate in a mass ratio of 1:(1.4-1.6).

8. The defoamer for seawater desalination according to claim 1, characterized in that, The stabilizer is one of xanthan gum and hydroxyethyl cellulose.

9. The defoamer for seawater desalination according to claim 1, characterized in that, The preservative is 1,2-benzisothiazolin-3-one.

10. A method for preparing an antifoaming agent for seawater desalination according to any one of claims 1-9, characterized in that, Includes the following steps: (1) Weigh out the following by weight: 4-7 parts stearic acid, 0.2-0.4 parts potassium hydroxide, 16-22 parts lauryl alcohol polyoxyethylene polyoxypropylene ether, 2-5 parts high temperature defoaming agent, 5-10 parts polypropylene glycol, 0.6-1.2 parts emulsifier, 0.08-0.18 parts stabilizer, 0.02-0.05 parts preservative, and 50-70 parts deionized water; (2) Mix deionized water and stabilizer to obtain stabilizer solution; mix deionized water and stearic acid, stir and heat to 75-85℃, add potassium hydroxide and stir for 40-50 min; add lauryl alcohol polyoxyethylene polyoxypropylene ether, high temperature resistant defoaming agent, polypropylene glycol and emulsifier in sequence and stir; cool to 35-45℃, add stabilizer solution, stir and shear at high speed, add preservative, stir and defoam to obtain defoamer for seawater desalination.

Citation Information

Patent Citations

  • Seawater desalination de-foaming agent as well as preparation method and application thereof

    CN108499162A