A method and system for curing lamp tubes
By dividing the curing process of long-length lamp tubes into independent temperature control zones and adjusting the support height and power in real time, the deformation problem caused by uneven heating and self-weight of the lamp tubes was solved, achieving uniform curing and improved stability of the lamp tubes.
Patent Information
- Application Number
- CN202611260187.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-08-19
- Publication Date
- 2026-11-17
AI Technical Summary
Existing long-length lamp tubes suffer from inconsistent curing due to uneven heating during the curing process, as well as excessive deformation or even breakage due to their own weight and thermal stress.
A method for curing lamp tubes is provided. By obtaining initial geometric parameters and coating material characteristics before curing, multiple independent temperature control zones are divided along the lamp tube axis. During the curing process, a dynamic support matrix is used to adjust the support height and curing power in real time. Combined with stepped cooling, deformation compensation and temperature field uniformity control are achieved.
It achieves axial curing consistency and mechanical stability for long-length lamp tubes, improves curing yield, and avoids the risk of deformation and breakage.
Smart Images

Figure CN123102585A_ABST
Abstract
Description
Technical Field
[0001] This application relates to the fields of lighting device manufacturing and photocuring technology, and in particular to a method and system for curing lamp tubes. Background Technology
[0002] With the continuous development of lighting and display technologies, slender light source devices, especially long-length lamps (such as 8FT lamps, which are 8 feet long), are increasingly widely used in industrial lighting, plant lighting, and special UV curing applications. These long-length lamps typically use glass tubes as the substrate, with phosphor layers, photoluminescent materials, or protective coatings applied to their inner or outer walls. To ensure that the coating material adheres quickly and firmly to the substrate surface, thermosetting or ultraviolet (UV) curing processes are usually required to cure the coated lamp.
[0003] However, existing technologies face several significant challenges in curing ultra-long lamps such as 8FT. Firstly, due to their length and weight, 8FT lamps are prone to bending and sagging in the middle section of their axis when cured horizontally due to the combined effects of gravity and thermal softening. This thermal deformation not only causes the lamp's straightness to exceed specifications, affecting subsequent assembly, but also results in uneven coating thickness distribution on the inner wall of the lamp, creating optical dark areas. Existing curing fixtures typically use fixed-spaced support wheels or support plates. This static support cannot accommodate the varying deformation of the lamp during heating, temperature control, and cooling stages, often resulting in excessive support force leading to indentations on the lamp surface, or insufficient support force exacerbating deformation.
[0004] Secondly, the axial dimension of the 8FT lamp is much larger than that of conventional lamps, making it easy for uneven temperature or light intensity distribution to form along the lamp's axis within the curing oven or curing chamber. Typically, the ends of the curing equipment experience faster heat dissipation or end effects, resulting in lower temperature / light intensity compared to the middle region. This axial gradient leads to incomplete curing of the coating material at the lamp ends, while the middle region may experience over-curing or thermal aging, severely impacting the consistency of curing throughout the lamp and its final photoelectric performance. Existing temperature control systems mostly employ an overall temperature control strategy, which cannot provide precise, differentiated compensation for localized temperature differences along the lamp's axis.
[0005] Furthermore, during the cooling phase after curing, if the cooling rate is uncontrollable or the support system fails to release stress in a timely manner, significant residual thermal stress will be generated inside the lamp tube. This will not only reduce the mechanical strength of the lamp tube but may also lead to the risk of glass tube bursting during subsequent use. Existing curing processes often emphasize heating while neglecting cooling, lacking a closed-loop intervention mechanism for the thermodynamic state of long-length lamp tubes throughout their entire life cycle.
[0006] Therefore, there is an urgent need for a lamp curing method and system that can achieve dynamic deformation compensation, axial temperature field homogenization control, and cooling stress release to solve the current technical bottleneck of low curing yield and poor consistency of long-size lamps. Summary of the Invention
[0007] This application provides a method and system for curing lamp tubes, aiming to solve the problems of inconsistent curing degree caused by uneven heating during the curing process of existing long-length lamp tubes, as well as excessive deformation or even damage caused by self-weight and thermal stress.
[0008] To solve the above-mentioned technical problems, one technical solution adopted in this application is: to provide a lamp curing method. The lamp curing method includes: S1: Obtain the initial geometric parameters of the lamp tube and the characteristics of the coating material; S2: Based on the initial geometric parameters and the characteristics of the coating material, multiple independent temperature control zones are divided along the axial direction of the lamp tube in the curing fixture; S3: Low power is used for preheating in the early stage of curing, and the support height is adjusted in real time through the dynamic support matrix of the fixture to counteract the thermal deformation caused by the lamp tube. S4: During the mid-curing stage, real-time temperature feedback data of each area on the surface of the lamp tube is obtained, and the curing power of each independent temperature control area is dynamically adjusted to ensure that the axial curing degree of the lamp tube is consistent. S5: At the end of the curing process, a stepped cooling is performed, and during the cooling process, adaptive support adjustment and phased mechanical locking are performed through the dynamic support matrix until the lamp is completely cooled.
[0009] In some embodiments, step S2 includes: S21: Calculate the expected thermal field distribution of the lamp tube at the curing temperature based on the initial geometric parameters and the characteristics of the coating material; S22: Identify the sections in the expected thermal field distribution where the rate of change of the temperature gradient along the lamp tube axis is greater than a preset threshold as key temperature control zones; S23: Map the key temperature control area and other conventional sections onto the physical heating / light source module of the curing fixture to form the multiple independent temperature control areas that are not uniformly arranged.
[0010] In some embodiments, step S23 specifically includes: Establish a one-to-one correspondence table between the axial coordinates of the lamp tube and the physical module array position of the curing fixture; For the axial coordinates belonging to the key temperature control zone, the reference power weight value of the corresponding physical module is increased by a first proportion; For the axial coordinates belonging to the conventional section, the reference power weight value of the corresponding physical module is reduced by a second ratio. The control parameters of each physical module are configured according to the adjusted weight value to form multiple independent temperature control zones with differentiated power configurations in the non-uniform arrangement.
[0011] In some embodiments, step S21 specifically includes: Extract the coefficient of thermal expansion, specific heat capacity, and exothermic parameters of the curing reaction of the coating material; A thermo-mechanical coupled finite element analysis model was constructed by combining the initial geometric parameters of each axial section of the lamp tube; The thermal expansion coefficient, specific heat capacity, curing reaction exothermic parameters, and initial geometric parameters are input into the thermo-mechanical coupled finite element analysis model to simulate and calculate the expected thermal field distribution of the lamp tube at the target curing temperature and the thermal deformation deflection trend of each axial node.
[0012] In some embodiments, step S3 includes: S31: In the early stage of curing, the lamp tube is preheated at a preset temperature lower than the target curing temperature, and the axial bending and sagging of the lamp tube is monitored in real time. S32: When the bending sag exceeds a preset safety threshold, the required vertical compensation height for each support node in the dynamic support matrix is calculated based on the sag distribution. S33: Send a driving command to the corresponding support node in the dynamic support matrix to lift the lamp tube according to the vertical compensation height, so as to form an adaptive support surface that matches the real-time deformation curve of the lamp tube.
[0013] In some embodiments, step S33 specifically includes: The vertical compensation height is analyzed to generate the target pulse count of the micro stepper motor corresponding to each support node; The micro stepper motor drives the lead screw mechanism to lift the support wheel to contact the surface of the lamp tube; The contact pressure is collected in real time by a pressure sensor installed in the support wheel. When the contact pressure reaches the preset threshold, the lifting action stops, thus completing the closed-loop fine adjustment of the support height.
[0014] In some embodiments, step S4 includes: S41: Real-time temperature of each area on the surface of the lamp tube is collected by an infrared temperature measuring array set in an independent temperature control area; S42: Calculate the deviation value and the rate of change of deviation between the real-time temperature of each region and the preset target curing temperature; S43: Input the deviation value and deviation change rate into the fuzzy PID controller, and output the power regulation coefficient of each independent temperature control zone; S44: Adjust the light source irradiation intensity or heating element power of the corresponding area independently according to the power adjustment coefficient to eliminate the axial temperature gradient of the lamp tube.
[0015] In some embodiments, step S42 specifically includes: The collected infrared thermometer array data is processed by moving average filtering to remove environmental interference outliers; The deviation between the real-time temperature of each region and the preset target curing temperature is calculated based on the filtered data, and the time-series change rate of the deviation value is extracted as the deviation change rate. The maximum and minimum temperature values in the filtered data are extracted to calculate the extreme value of the axial temperature difference. If the extreme value of the axial temperature difference exceeds the preset tolerance zone, the preset target curing temperature is finely adjusted and compensated, and the deviation value is recalculated based on the finely adjusted and compensated target curing temperature.
[0016] In some embodiments, step S5 includes: S51: Set at least three stepped cooling temperature nodes and the corresponding heat preservation dwell time for each node; S52: During the dwell period at each stepped cooling temperature node, continuously monitor the stress change value of the support nodes in the dynamic support matrix and the deformation recovery of the lamp tube. S53: When the deformation recovery amount is detected to be less than the set minimum value per unit time, it is determined that the stress of the lamp tube has been released and the deformation tends to be stable at this temperature node. The current position of the dynamic support matrix is mechanically locked, and the mechanical lock is released before entering the next cooling step or in the early stage of cooling, so as to allow the support matrix to adaptively descend and adjust according to the shrinkage of the lamp tube.
[0017] To solve the above-mentioned technical problems, another technical solution adopted in this application is to provide a lamp curing system. The lamp curing system includes: The parameter acquisition module is used to acquire the initial geometric parameters of the lamp tube and the characteristics of the coating material; The region division module is used to divide the lamp tube into multiple independent temperature control zones along the axial direction in the curing fixture; The dynamic curing execution and control module uses low power for preheating in the early stage of curing and simultaneously adjusts the support height in real time through the dynamic support matrix of the fixture to counteract the thermal deformation caused by the lamp tube. In the middle stage of curing, it acquires real-time temperature feedback data of each area on the surface of the lamp tube and dynamically adjusts the curing power of each independent temperature control area to ensure that the axial curing degree of the lamp tube is consistent. In the final stage of curing, it performs step-by-step cooling and performs adaptive support adjustment and staged mechanical locking through the dynamic support matrix during the cooling process until the lamp tube is completely cooled.
[0018] The beneficial effects of this application are as follows: Unlike existing technologies, this application provides a method and system for curing lamp tubes. In this application, the initial geometric parameters and coating material characteristics of the lamp tube are obtained before curing, and based on this, multiple independent temperature control zones are divided along the lamp tube axis in the curing fixture, achieving predictive zone division before curing. In the initial curing stage, low-power preheating is used, and the support height is simultaneously adjusted in real-time through a dynamic support matrix, effectively offsetting the thermal deformation and self-weight sagging of the lamp tube in the initial heating stage, avoiding indentations or support failure caused by static support. In the middle stage of curing, the curing power of each independent temperature control zone is dynamically adjusted based on real-time temperature feedback, accurately eliminating the axial temperature gradient and ensuring a high degree of consistency in the axial curing degree of ultra-long lamp tubes. In the final stage of curing, stepped cooling combined with adaptive adjustment of the dynamic support matrix and staged mechanical locking ensures the stability of the support and releases thermal stress, avoiding warping or cracking caused by residual stress. This application achieves coordinated closed-loop control of mechanical deformation and thermodynamic temperature field during the curing process of long-size lamp tubes, significantly improving curing yield and product consistency. Attached Figure Description
[0019] To more clearly illustrate the technical solutions in the embodiments of this application or the prior art, the drawings used in the description of the embodiments or the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of this application. For those skilled in the art, other drawings can be obtained based on these drawings without creative effort, wherein: Figure 1 This is a schematic flowchart of an embodiment of the lamp curing method provided in this application; Figure 2 yes Figure 1 A flowchart illustrating an embodiment of step S1 in the method shown; Figure 3 yes Figure 1 A flowchart illustrating an embodiment of step S2 in the method shown; Figure 4 yes Figure 1 A flowchart illustrating an embodiment of step S3 in the method shown; Figure 5 yes Figure 1 A flowchart illustrating an embodiment of step S4 in the method shown; Figure 6 yes Figure 1 A flowchart illustrating an embodiment of step S5 in the method shown; Figure 7 This is a schematic diagram of the structural block of an embodiment of the lamp curing system provided in this application. Detailed Implementation
[0020] The technical solutions of the embodiments of this application will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only a part of the embodiments of this application, and not all of the embodiments. Based on the embodiments of this application, all other embodiments obtained by those of ordinary skill in the art without creative effort are within the scope of protection of this application.
[0021] The terms "first," "second," and "third" used in the embodiments of this application are for descriptive purposes only and should not be construed as indicating or implying relative importance or implicitly specifying the number of indicated technical features. Thus, a feature defined as "first," "second," or "third" may explicitly or implicitly include at least one of that feature. In the description of this application, "multiple" means at least two, such as two, three, etc., unless otherwise explicitly specified. Furthermore, the terms "comprising" and "having," and any variations thereof, are intended to cover non-exclusive inclusion. For example, a process, method, system, product, or device that includes a series of steps or units is not limited to the listed steps or units, but may optionally include steps or units not listed, or may optionally include other steps or units inherent to these processes, methods, products, or devices.
[0022] In this document, the term "embodiment" means that a particular feature, structure, or characteristic described in connection with an embodiment may be included in at least one embodiment of this application. The appearance of this phrase in various places throughout the specification does not necessarily refer to the same embodiment, nor is it a mutually exclusive, independent, or alternative embodiment. It will be explicitly and implicitly understood by those skilled in the art that the embodiments described herein can be combined with other embodiments.
[0023] To address the issues in existing technologies where 8FT-length lamps are prone to bending and deformation during curing due to heat and their own weight, and where uneven axial heating leads to inconsistent curing degrees, this application provides a curing scheme based on dynamic deformation compensation and adaptive thermal field control. This curing scheme pre-determines temperature control zones based on lamp characteristics before curing, intervenes in real-time mechanically through a dynamic support matrix throughout the curing cycle, achieves uniform curing by combining multi-region closed-loop temperature control, and finally ensures the geometric stability of the final product through stepped cooling and stress release mechanisms.
[0024] Specifically, this application provides a method for curing lamp tubes, see reference. Figure 1 , Figure 1 This is a schematic flowchart of an embodiment of the lamp curing method provided in this application. The lamp curing method includes: Step S1: Obtain the initial geometric parameters of the lamp tube and the characteristics of the coating material.
[0025] Before curing the lamp tube, it is necessary to collect comprehensive data on its current physical state. The lamp tube to be cured is, for example, an 8-foot-long glass tube coated with photoluminescent material. Due to the slight dimensional tolerances in the geometric dimensions of different batches and specifications of lamp tubes after the coating process, and the differences in the thermodynamic properties of the coating material formulations from batch to batch, this initial state data will serve as the basis for subsequent thermal field distribution calculations and support height adjustments.
[0026] Specifically, the initial geometric parameters include, but are not limited to, the initial straightness, cylindricity, wall thickness uniformity, and the coordinate trajectories of the center of each cross-section along the axial direction of the lamp tube. The coating material characteristics include, but are not limited to, the thickness distribution of the coating layer, the spectral reflectance and transmittance of the material, the coefficient of thermal expansion, specific heat capacity, the peak exothermic temperature and heat release of the curing reaction, and the curing shrinkage rate. These parameters are acquired using a high-precision sensor array to construct a dedicated digital twin model for this specific lamp tube.
[0027] See Figure 2 , Figure 2 yes Figure 1 The flowchart illustrates an embodiment of step S1 in the lamp curing method shown. Step S1 specifically includes: Step S11: Set multiple laser displacement sensors along the lamp tube axis to obtain initial contour data of the lamp tube in an unheated state.
[0028] Before the lamp enters the curing fixture or while it is at room temperature in the curing fixture without being heated, an array of laser displacement sensors is arranged along the lamp axis. Since the length of the 8FT lamp is approximately 2438 mm, the sensor arrangement needs to have sufficient spatial resolution to ensure the accuracy of contour fitting.
[0029] In practice, the lamp tube is placed flat on a standard reference surface, which serves as the zero-point reference for all subsequent displacement measurements. At least five measurement sections are selected at equal intervals along the lamp tube's axis; for example, seven measurement sections can be selected, with a spacing of approximately 300mm to 400mm between adjacent sections. Three sampling points are selected circumferentially at the top, left, and right sides of each measurement section. The laser displacement sensor at the top illuminates the highest point of the lamp tube vertically downwards, while the sensors on the left and right sides illuminate the sidewall generatrix of the lamp tube at specific angles.
[0030] Laser echo times were collected at each sampling point, and the relationship between light speed and time was used to convert them into displacement values. Using a multi-point data fitting algorithm, such as least squares polynomial fitting, the displacement values of each cross-section sampling point were fitted to form initial profile data characterizing the initial straightness and cylindricity of the lamp tube. This initial profile data can reflect whether the lamp tube already has defects such as pre-bending, ellipticization, or twisting at room temperature, providing a basis for the initial zero-position calibration of the subsequent dynamic support matrix.
[0031] Step S12: Based on the spectral reflectance characteristics of the coating material, use a spectral thickness gauge to obtain the thickness distribution data of the coating layer on the lamp tube surface.
[0032] Since the thickness of the coating on the inner or outer wall of the lamp tube directly determines the absorption rate of the curing light source (such as ultraviolet or infrared light) in that area, it affects the heat generation rate during the curing process. Therefore, accurately obtaining the thickness distribution of the coating is crucial for predicting the thermal field.
[0033] In practice, a broadband scanning beam is emitted towards the coating layer on the lamp tube surface, and the reflected spectral signal is acquired. Since films of different thicknesses produce interference effects on light of specific wavelengths, the phase information of interference peaks at specific characteristic wavelengths in the reflected spectral signal is extracted. This extracted interference peak phase information is then substituted into a pre-calibrated optical path-thickness mapping model to calculate the coating thickness distribution data at each axial position on the lamp tube surface. This optical path-thickness mapping model is generated by coating a material of known thickness onto a standard substrate and measuring and calibrating it using the same spectral thickness gauge. This step allows for precise identification of sections on the lamp tube surface where the coating is too thin or too thick.
[0034] Step S13: Combine the initial profile data and thickness distribution data with the curing shrinkage rate parameter of the coating material to generate a dataset of initial geometric parameters and coating material properties.
[0035] The initial contour data obtained in step S11 and the thickness distribution data obtained in step S12 are aligned and fused in spatial coordinates. Combined with the known curing shrinkage rate parameters, thermal expansion coefficients, and other material properties of this batch of coating materials, a complete dataset is generated. This dataset not only contains the geometric morphology information of the lamp tube but also couples the thermodynamic properties of the material, forming the basic input source for subsequent thermo-mechanical coupling calculations.
[0036] Step S2: Based on the initial geometric parameters and the characteristics of the coating material, divide the curing fixture into multiple independent temperature control zones along the axial direction of the lamp tube.
[0037] Traditional curing equipment typically treats the entire lamp tube as a homogeneous heated body for overall temperature control, which cannot eliminate the axial temperature difference caused by heat dissipation at the ends and heat accumulation in the middle. This embodiment, based on the aforementioned dataset, divides the heating or light source module of the curing fixture into non-uniform, differentiated regions to achieve targeted temperature control.
[0038] See Figure 3 , Figure 3 yes Figure 1 The flowchart illustrates an embodiment of step S2 in the lamp curing method shown. Step S2 specifically includes: Step S21: Calculate the expected thermal field distribution of the lamp tube at the curing temperature based on the initial geometric parameters and the characteristics of the coating material.
[0039] The initial geometric parameters and coating material properties are input into a pre-built prediction model to simulate the thermal field distribution on the surface and inside of the lamp tube when it reaches the target curing temperature.
[0040] Specifically, thermodynamic constants such as the coefficient of thermal expansion, specific heat capacity, and exothermic parameters of the curing reaction of the coating material are extracted. A thermo-mechanical coupled finite element analysis model is constructed by combining the initial geometric parameters (such as wall thickness and pipe diameter variations) of each axial section of the lamp tube. In this model, environmental boundary conditions (such as airflow velocity and ambient temperature within the curing oven) are set, and a curing heat source load (such as infrared heating power density or ultraviolet light intensity) is applied. These parameters are input into the thermo-mechanical coupled finite element analysis model, and simulation calculations are performed to obtain the expected thermal field distribution of the lamp tube at the target curing temperature and the thermal deformation deflection trend of each axial node. Since the curing reaction itself is exothermic, areas with thicker coatings release more heat during curing, and the model can accurately predict these local hot spots.
[0041] Step S22: Identify the sections in the expected thermal field distribution where the rate of change of the temperature gradient along the lamp tube axis is greater than a preset threshold as key temperature control zones.
[0042] The calculated expected thermal field distribution data is differentiated along the lamp tube axis to obtain the rate of change of temperature gradient at each axial position. A temperature gradient threshold is preset, for example, 5℃ / cm. If the rate of change of temperature gradient in a certain section exceeds this threshold, it indicates that the section is prone to sudden thermal changes during curing and is identified as a key temperature control area. Typically, the two ends of the lamp tube, due to faster heat dissipation, and areas with abrupt changes in coating thickness, due to uneven heat release, are identified as key temperature control areas.
[0043] Step S23: Map the key temperature control area and the remaining regular sections onto the physical heating / light source module of the curing fixture to form multiple independent temperature control areas that are not uniformly arranged.
[0044] Based on the identified key temperature control zones and regular sections, their axial coordinates are mapped to the actual physical heating modules or ultraviolet light source module arrays arranged on the curing fixture. To achieve precise control, the curing fixture is divided into multiple controllable units along the axial direction.
[0045] In practice, a one-to-one correspondence table is established between the axial coordinates of the lamp tubes and the positions of the physical module array in the curing fixture. For axial coordinates belonging to key temperature control zones, the base power weight value of the corresponding physical module is increased by a first percentage, for example, by 15% to 30%; for axial coordinates belonging to regular zones, the base power weight value of the corresponding physical module is decreased by a second percentage, for example, by 10% to 20%. The control parameters of each physical module are configured according to the adjusted weight values to form multiple independent temperature control zones with differentiated power configurations in a non-uniform arrangement. Through this non-uniform region division and weight preset, temperature gradients can be suppressed from the source in the early stages of curing.
[0046] Step S3: In the early stage of curing, preheating is carried out with low power, and the support height is adjusted in real time through the dynamic support matrix of the fixture to counteract the thermal deformation caused by the lamp tube.
[0047] The initial curing stage is the most sensitive period for thermal deformation of the lamp tube. If full-power curing is applied directly, the glass substrate and coating layer will experience significant temperature gradient stress due to severe thermal shock, and the creep deformation caused by the lamp tube's own weight during rapid softening will be irreversible. Therefore, a low-power, slow-heating strategy combined with dynamic support intervention is adopted in this stage.
[0048] See Figure 4 , Figure 4 yes Figure 1 The flowchart illustrates an embodiment of step S3 in the lamp curing method shown. Step S3 specifically includes: Step S31: In the early stage of curing, perform constant temperature preheating at a preset temperature lower than the target curing temperature, and monitor the axial bending and sagging of the lamp tube in real time.
[0049] Start the curing fixture and control each independent temperature control zone to perform constant preheating at a preset temperature lower than the final target curing temperature. For example, if the target temperature is 180℃, the preheating temperature is set to 80℃ to 100℃. At the same time, a displacement monitoring mechanism is arranged along the axial direction of the lamp tube. The laser displacement sensor or contact displacement probe in step S11 can be reused to monitor the bending and sagging of each section of the lamp tube along the axial direction in real time.
[0050] Step S32: When the bending sag exceeds the preset safety threshold, calculate the required vertical compensation height for each support node in the dynamic support matrix based on the sag distribution.
[0051] Because the 8FT lamp tube is extremely long, the sag in the middle section is usually the greatest. A preset safe sag threshold, such as 0.5mm, is used. When the real-time bending sag at a certain axial position exceeds this threshold, a dynamic support compensation mechanism is triggered. Based on the sag distribution curves at each measuring point, an interpolation algorithm is used to calculate the required vertical compensation height for each support node in the dynamic support matrix arranged below the lamp tube, so as to lift the lamp tube at that position to the theoretical baseline.
[0052] Step S33: Send a driving command to the corresponding support node in the dynamic support matrix to lift the lamp tube according to the vertical compensation height, so as to form an adaptive support surface that matches the real-time deformation curve of the lamp tube.
[0053] The dynamic support matrix consists of multiple support nodes arranged along the lamp tube's axis. The control system sends drive commands to the support nodes that need to move, causing them to lift the lamp tube upwards according to the calculated vertical compensation height. Since the lifting amount of each node is calculated independently based on the real-time sag, the coordinated action of multiple nodes ultimately forms an adaptive support surface that matches the real-time deformation curve of the lamp tube, thus both offsetting gravity deformation and preventing excessive support that could cause the lamp tube to bend.
[0054] More specifically, the vertical compensation height is analyzed to generate the target pulse count for the corresponding micro stepper motors at each support node; the micro stepper motors are driven to move the lead screw mechanism to lift the support wheel to contact the lamp tube surface; the contact pressure is collected in real time by a pressure sensor installed in the support wheel, and the lifting action stops when the contact pressure reaches a preset threshold, completing the closed-loop fine adjustment of the support height. This closed-loop fine adjustment based on dual feedback of displacement and pressure ensures the gentleness and precision of the support force, preventing damage to the glass tube from hard impacts.
[0055] Step S4: During the mid-curing stage, obtain real-time temperature feedback data for each area on the surface of the lamp tube, and dynamically adjust the curing power of each independent temperature control area to ensure consistent axial curing degree of the lamp tube.
[0056] After low-power preheating and deformation compensation of the dynamic support matrix during the initial curing stage, the lamp tube has entered a thermally stable state, marking the beginning of the mid-curing phase. The mid-curing phase is a critical stage where the coating material undergoes a polymer cross-linking reaction or the photocuring initiator rapidly decomposes. During this stage, all areas of the lamp tube surface need to reach the target curing temperature and maintain dynamic equilibrium. Due to the uneven distribution of the coating thickness and the randomness of the airflow distribution within the curing oven, relying solely on the non-uniform power weight preset in step S2 is insufficient to completely eliminate the axial temperature gradient. Therefore, a closed-loop dynamic adjustment mechanism based on real-time feedback must be introduced.
[0057] See Figure 5 , Figure 5 yes Figure 1The flowchart illustrates an embodiment of step S4 in the lamp curing method shown. Step S4 specifically includes: Step S41: Collect the real-time temperature of each area on the surface of the lamp tube by setting an infrared temperature measurement array in an independent temperature control area.
[0058] An array of infrared temperature sensors is arranged non-contactly above or to the side of each individual temperature-controlled zone in the curing fixture. Due to the relatively long length of the 8FT lamp, an infrared temperature sensor is typically placed every 200mm to 300mm, forming a temperature measurement array covering the entire length. The infrared temperature sensor receives the infrared energy radiated by the coating layer on the lamp surface, converts it into an electrical signal, and calibrates it as a temperature value.
[0059] In practical implementation, the response time of the infrared temperature probe must be less than 50ms to ensure that transient temperature fluctuations can be captured. Meanwhile, considering the different emissivity of different coating materials, the emissivity coefficient of the infrared probe must be calibrated online using a blackbody furnace or contact thermocouple before the probe leaves the factory or each time the product model is changed. This ensures that the collected real-time temperature accurately reflects the temperature of the coating layer on the lamp surface, rather than the ambient background temperature.
[0060] Step S42: Calculate the deviation value and the rate of change of deviation between the real-time temperature of each region and the preset target curing temperature.
[0061] After obtaining the real-time temperature, the control system compares the real-time temperature of each independent temperature control zone with the preset target curing temperature. The preset target curing temperature is set according to the optimal curing kinetics curve of the coating material. For example, for a certain acrylic ester UV-initiated coating, the optimal temperature for mid-term thermal curing initiation may be set between 160°C and 180°C.
[0062] Specifically, the collected infrared temperature array data is processed using a moving average filter to remove outliers caused by environmental interference. Due to potential fan disturbances or instantaneous hot airflow impacts within the curing oven, the raw infrared data may contain high-frequency spikes. A moving average window of length N (e.g., N=5) is used to convolve the time-series temperature data. Based on the filtered data, the deviation between the real-time temperature of each region and the preset target curing temperature is calculated, and the temporal rate of change of the deviation is extracted as the deviation rate of change. The deviation value reflects the static degree of temperature deviation, while the deviation rate of change reflects the trend and speed of temperature change.
[0063] Furthermore, to prevent yellowing or thermal aging of the coating material due to localized overheating, after calculating the deviation value, it is necessary to extract the maximum and minimum temperature values from the filtered data to calculate the extreme value of the axial temperature difference. It is then determined whether the extreme value of the axial temperature difference exceeds a preset tolerance zone, for example, ±3℃. If it does, it indicates a severe imbalance in the current thermal field distribution. In this case, a temperature equalization adjustment mechanism is triggered to fine-tune the preset target curing temperature, for example, lowering the overall target temperature by 1℃ to 2℃. The deviation value is then recalculated based on the fine-tuned target curing temperature to forcibly flatten the overall temperature envelope.
[0064] Step S43: Input the deviation value and the rate of change of deviation into the fuzzy PID controller, and output the power regulation coefficient of each independent temperature control zone.
[0065] Traditional PID controllers often struggle to balance response speed and overshoot when handling curing oven thermodynamic systems with large time lags, nonlinearity, and time-varying parameters. This application employs a fuzzy PID controller, utilizing fuzzy inference rules to adaptively tune the PID parameters online.
[0066] Specifically, the deviation value and the rate of change of deviation are used as input variables of the fuzzy controller. First, the input variables are fuzzified and mapped to the fuzzy universe of discourse, for example, divided into seven fuzzy levels: negative large (NB), negative medium (NM), negative small (NS), zero (ZO), positive small (PS), positive medium (PM), and positive large (PB).
[0067] Based on the control experience of curing thermodynamics, a fuzzy control rule table is established, for example: "If the deviation value is positive and the deviation change rate is positive, it means that the current temperature is much lower than the set value and has a continuing downward trend. The maximum heating power should be output, that is, the proportional coefficient should be large, the integral coefficient should be small, and the derivative coefficient should be medium." "If the deviation value is zero and the deviation change rate is small, it means that the temperature has reached the standard but there is a slight downward trend. The power should be increased appropriately to prevent the temperature from dropping. That is, the proportional coefficient should be the median value and the integral coefficient should be the small value."
[0068] The fuzzy inference results are defuzzified using the centroid method or the maximum membership method to obtain accurate PID parameter increments, which are then superimposed with the initial PID parameters to output the power regulation coefficients for each independent temperature control zone.
[0069] Step S44: Adjust the light source irradiation intensity or heating element power of the corresponding area independently according to the power adjustment coefficient to eliminate the axial temperature gradient of the lamp tube.
[0070] Based on the power regulation coefficient output by the fuzzy PID controller, the actuators in each independent temperature control zone respond independently. Since the curing equipment may use different heating / curing media, this application develops differentiated control strategies for different media.
[0071] Specifically, the power regulation coefficient is converted into a PWM (Pulse Width Modulation) duty cycle adjustment signal. This determines whether the corresponding area is an ultraviolet curing light source or an infrared heating element.
[0072] If the corresponding area is a UV curing light source, the PWM duty cycle adjustment signal is sent to the light source driver to adjust the pulse emission frequency and duty cycle. Since the lifespan and light intensity output of the UV lamp are greatly affected by frequent switching, high-frequency PWM dimming technology is used here, for example, with a frequency between 1kHz and 10kHz. By changing the duty cycle, the UV radiation intensity is smoothly adjusted, avoiding uneven coating curing caused by low-frequency flicker.
[0073] If the corresponding area is an infrared heating element, such as a halogen infrared lamp or a silicon carbide heating plate, a PWM duty cycle adjustment signal is sent to the solid-state relay to control the on / off time ratio of the heating element. Due to the thermal inertia of the infrared heating element, the PWM period is typically set to several seconds to tens of seconds. Simultaneously, to prevent the cold-state lamp from breaking due to thermal shock when suddenly subjected to full power, an upper limit is set on the rising slope of the power change rate in the control algorithm; for example, the power increment per second should not exceed 5% of the total rated power. The output of the solid-state relay is limited by a slope limiter to ensure a smooth power ramp-up for the heating element and avoid thermal shock.
[0074] Through the closed-loop control of S41 to S44, the temperature of each axial region of the 8FT lamp during the curing process can be precisely controlled within ±2℃ of the preset target curing temperature, which greatly suppresses the phenomenon of poor end curing or over-curing in the middle.
[0075] Step S5: At the end of the curing process, a stepped cooling process is performed, and adaptive support adjustment and phased mechanical locking are carried out through a dynamic support matrix during the cooling process until the lamp is completely cooled.
[0076] In the final stage of curing, the polymer cross-linking network of the coating material has basically formed, at which point the annealing and cooling stage begins. The cooling rate and support condition directly determine the residual stress distribution and final straightness of the lamp tube. If the cooling is too rapid, the difference in thermal expansion coefficients between the glass tube and the coating layer will generate huge shear stress, leading to coating peeling or glass tube cracking. If the support matrix remains at a rigid, fixed height during the cooling process, the local stress concentration at the support points will damage the lamp tube due to slight changes in both axial and radial dimensions as the lamp tube cools and contracts.
[0077] See Figure 6 , Figure 6 yes Figure 1 A schematic flowchart of an embodiment of step S5 in the lamp curing method shown. Step S5 specifically includes: Step S51: Set at least three stepped cooling temperature nodes and the corresponding heat preservation dwell time for each node.
[0078] Based on the glass annealing process principle and the glass transition temperature of the coating material, a stepped cooling curve is set. For example, if the target curing temperature is 180℃, the first step cooling node is set at 120℃ with a holding time of 5 minutes; the second step cooling node is set at 80℃ with a holding time of 8 minutes; and the third step cooling node is set at 40℃ with a holding time of 10 minutes. Between two adjacent nodes, the control system controls the opening of the curing oven's exhaust fan and maintains low power output of the heating elements, slowly cooling to the next node according to the set cooling slope, such as 1℃ / min to 2℃ / min. This stepped holding time allows sufficient time for the polymer chain segments to relax, effectively eliminating internal thermal stress.
[0079] Step S52: During the dwell period at each stepped cooling temperature node, continuously monitor the stress change value of the support node in the dynamic support matrix and the deformation recovery amount of the lamp tube.
[0080] During the cooling phase, the dynamic support matrix not only provides physical support but also transforms into a stress monitoring and release terminal. As the temperature decreases, the lamp tube contracts, and its deflection curve rebounds. The pressure on the support nodes, which were initially lifted during the curing stage, gradually increases. Contact pressure is collected in real time by pressure sensors within the support wheels, serving as the stress change value. Simultaneously, displacement sensors inside the support nodes or external laser displacement sensors monitor the height change of the lamp tube relative to the support nodes, serving as the deformation recovery amount.
[0081] Step S53: When the deformation recovery amount is detected to be less than the set minimum value per unit time, it is determined that the stress of the lamp tube has been released and the deformation tends to be stable at this temperature node. The current position of the dynamic support matrix is mechanically locked, and the mechanical lock is released before entering the next cooling step or in the early stage of cooling, so as to allow the support matrix to adaptively adjust its descent according to the shrinkage of the lamp tube.
[0082] During each stage of heat preservation, the system continuously assesses the stress release progress. When the absolute value of the deformation recovery change per unit time (e.g., 1 minute) is less than the set minimum value (e.g., 0.005 mm / min), and the stress change value tends to fluctuate steadily, it is determined that the polymer chain rearrangement of the lamp tube at that temperature node has been basically completed, the thermal stress has been fully released, and the deformation tends to stabilize.
[0083] At this point, in order to maintain a stable support base during the subsequent cooling process, a mechanical locking action is performed. Specifically, a locking energizing signal is sent to the electromagnetic brake device of the support node. The electromagnetic brake device actuates, locking the outer surface of the lead screw mechanism, restricting the displacement freedom of the support wheel in the Z-axis direction (vertical direction). This mechanical rigid locking eliminates the stepper motor's potential for step loss or slippage when powered on or off, providing the lamp tube with a rigid support base without elastic deformation.
[0084] However, if the locking mechanism remains locked until the next stage of cooling, the lamp's contraction and cooling will be hindered, creating new structural stress. Therefore, before entering the next stage of cooling or at the initial stage of cooling, i.e., when the temperature just begins to drop, the control system actively releases the mechanical lock. Specifically, this involves sending a power-off signal to the electromagnetic brake device to release the lead screw mechanism; simultaneously, a command is sent to cut off the holding current of the micro stepper motor, causing the stepper motor to enter a free-stepping state. At this time, the support matrix enters a follow-up and pressure-following state.
[0085] In the follow-up and pressure-based state, the support wheel maintains slight contact with the lamp tube under the action of the pre-tensioned spring or slight gravity compensation. As the lamp tube cools and contracts, it sinks, and the support wheel descends accordingly, without applying a reverse lifting force to the lamp tube. When the lamp tube reaches the temperature node again and stabilizes in the next cooling stage, the system re-engages mechanically. This "lock-release-follow-lock" cyclic strategy perfectly meets the stress relief and geometric shaping requirements of long lamp tubes under complex thermal fields.
[0086] See Figure 7 , Figure 7 This is a structural block diagram of an embodiment of the lamp curing system provided in this application. This application also provides a lamp curing system 100 for implementing the lamp curing method described in any of the above embodiments. The lamp curing system 100 includes a parameter acquisition module 10, a region division module 20, and a dynamic curing execution and control module 30, which are interconnected.
[0087] The parameter acquisition module 10 is used to acquire the initial geometric parameters of the lamp tube and the characteristics of the coating material. This module integrates a laser displacement sensor array and a spectral thickness gauge in hardware, and is connected to the host industrial control computer through a data acquisition card. It is responsible for executing the logic of the aforementioned step S1.
[0088] The region division module 20 is used to divide the curing fixture into multiple independent temperature control regions along the axial direction of the lamp tube. This module is mainly a software algorithm module running on an industrial control computer. It receives data from the parameter acquisition module 10, performs finite element simulation calculations and coordinate mapping, and generates control weight configuration files for each physical module.
[0089] The dynamic curing execution and control module 30 is the core actuator of the entire system, integrating electromechanical hardware and control algorithms. In the initial curing stage, low-power preheating is used, and the support height is simultaneously adjusted in real-time via the dynamic support matrix of the fixture to counteract thermal deformation caused by the lamp tube. In the middle curing stage, real-time temperature feedback data for each area of the lamp tube surface is acquired, and the curing power of each independent temperature control zone is dynamically adjusted to ensure consistent axial curing of the lamp tube. In the final curing stage, stepped cooling is implemented, and during the cooling process, adaptive support adjustment and phased mechanical locking are performed via the dynamic support matrix until the lamp tube is completely cooled. This module includes a PLC controller, a multi-channel PWM generator, a stepper motor driver array, an infrared temperature measurement array, a dynamic support matrix mechanism, and a UV / IR light source module.
[0090] Unlike existing technologies, this application completely solves the problem of deformation and unevenness in the curing process of ultra-long lamps such as 8FT through a full-cycle coordinated control strategy of predictive non-uniform region division, initial dynamic deformation compensation, mid-term multi-zone closed-loop temperature control, and final-term stepped cooling and stress release, which greatly improves the product yield and process consistency.
[0091] To more clearly illustrate the technical solution and effects of this application, the following detailed embodiments are described using the thermosetting process of an 8FT fluorescent tube (diameter T8, length 2438mm, wall thickness 1.2mm, coated with double-layer phosphor and protective film) as an example.
[0092] Example 1: In this embodiment, the 8FT fluorescent tubes are cured using a horizontal conveying continuous curing method. The curing oven is 12 meters long and is divided into a preheating zone, a curing zone, and a cooling zone. The system of this application is deployed in the curing zone and the cooling zone.
[0093] Step S1: Before the lamp enters the curing oven, the initial geometric parameters of the lamp and the characteristics of the coating material are obtained through online detection equipment.
[0094] S11: A laser displacement sensor is arranged at 300mm intervals along the axial direction of the lamp tube, for a total of 8 measuring points. The lamp tube is placed flat on the V-shaped reference roller conveyor, and the top displacement data is measured. Through fitting calculation, the lamp tube has an initial sag deflection of 0.8mm.
[0095] S12: Using an online spectral thickness gauge to scan the surface of the lamp tube, extract characteristic wavelength interference data, and substitute it into the optical path-thickness mapping model, the average coating thickness is found to be 25μm, but the thickness in the middle section of 2000mm-2200mm is as high as 32μm.
[0096] S13: Generate a dataset by combining parameters such as the curing shrinkage rate (0.15) and thermal expansion coefficient of the coating material.
[0097] Step S2: Divide the temperature control zone based on the above dataset.
[0098] S21: Extract parameters such as the specific heat capacity of the material, construct a thermo-mechanical coupling model, input it into simulation software, and calculate the expected thermal field distribution. The results show that, due to the thicker coating in the middle section, the temperature in this region during the curing exothermic reaction is expected to be about 12°C higher than that at both ends.
[0099] S22: Identify sections with a temperature gradient change rate greater than 5℃ / cm, and identify the middle section (2000mm-2200mm) and the section 100mm from both ends as key temperature control zones.
[0100] S23: Establish a mapping table, reduce the base power weight of the two sets of infrared heating modules corresponding to the key temperature control area in the middle section by 20%, and increase the weight of the modules corresponding to both ends by 15%, forming 10 independent temperature control areas with non-uniform arrangement.
[0101] Step S3: Deformation control during the initial curing stage.
[0102] S31: The lamp enters the curing zone and is preheated at a constant temperature of 80℃ for 5 minutes. The laser sensor monitors the lamp sag in real time.
[0103] S32: When the sagging of the middle section reaches 1.5mm, the system triggers dynamic support compensation and calculates the vertical compensation height of each support node.
[0104] S33: A pulse command is sent to the middle support node, and the micro stepper motor drives the lead screw to lift the support wheel. When the pressure sensor inside the support wheel detects a contact pressure of 2N, the lifting stops, forming an adaptive support surface. This action is completed within 0.5 seconds, effectively preventing the lamp tube from continuing to sag.
[0105] Step S4: Control of uniform curing during the mid-curing stage.
[0106] S41: The infrared temperature measurement array collects the real-time temperature of 10 areas at a frequency of 200Hz.
[0107] S42: The target curing temperature is set to 160℃. The system performs a moving average filter on the temperature data and calculates the deviation value e(t) and the rate of change ec(t). It is detected that the temperature in the middle section suddenly rises to 168℃ due to heat release from the coating, and the extreme value of the axial temperature difference exceeds the ±3℃ tolerance zone, triggering the temperature equalization mechanism to fine-tune the overall target temperature to 158℃.
[0108] S43: The fuzzy PID controller outputs a power adjustment coefficient based on e(t) and ec(t), outputting a negative adjustment coefficient for the middle range and a positive adjustment coefficient for both ends.
[0109] S44: Convert the adjustment coefficient into a PWM signal. The duty cycle of the solid-state relay for the mid-section infrared heating element is reduced to 20%, while the duty cycle at both ends is increased to 80%. Simultaneously, the power rise rate is limited to no more than 5% / s to avoid thermal shock. After 2 minutes, the temperature in each area stabilizes within 158℃±1.5℃.
[0110] Step S5: Cooling and stress release at the end of curing.
[0111] S51: Set the stepped cooling nodes as follows: 120℃ for 5 minutes, 80℃ for 8 minutes, and 40℃ for 10 minutes.
[0112] S52: During the heat preservation period at 120℃, the pressure sensor detected that the force value gradually increased to 5N, and the deformation recovery was 0.02mm / min.
[0113] S53: When the deformation recovery is less than 0.005 mm / min, the stress release is considered stable. A locking signal is sent to the electromagnetic brake device to lock the lead screw and cut off the motor holding current. In the initial stage of preparing to drop to 80℃, a power-off signal is sent to release the brake, and the support matrix enters a follow-up pressure state, allowing the lamp tube to freely contract and sink. This locking and releasing logic is then repeated at the 80℃ and 40℃ nodes. After the lamp tube comes out of the furnace, it is tested by a straightness measuring instrument. The straightness is within 0.5 mm, and there is no yellowing or peeling of the coating.
[0114] Unlike existing technologies, this application provides a method and system for curing lamp tubes. In this application, the initial geometric parameters and coating material characteristics of the lamp tube are obtained before curing, and multiple independent temperature-controlled zones are divided along the lamp tube axis in the curing fixture accordingly, achieving predictive zone division before curing. In the initial curing stage, low-power preheating is used, and the support height is simultaneously adjusted in real-time through a dynamic support matrix, effectively offsetting the thermal deformation and sagging of the lamp tube under its own weight in the initial heating stage, avoiding indentations or support failure caused by static support. In the middle stage of curing, the curing power of each independent temperature-controlled zone is dynamically adjusted based on real-time temperature feedback, accurately eliminating the axial temperature gradient and ensuring a high degree of consistency in the axial curing degree of ultra-long lamp tubes. In the final stage of curing, stepped cooling combined with adaptive adjustment of the dynamic support matrix and staged mechanical locking ensures the stability of the support and releases thermal stress, avoiding warping or cracking caused by residual stress. This application achieves coordinated closed-loop control of mechanical deformation and thermodynamic temperature field during the curing process of long-size lamp tubes, significantly improving curing yield and product consistency.
[0115] The above description is merely an embodiment of this application and does not limit the patent scope of this application. Any equivalent structural or procedural transformations made using the content of this application's specification and drawings, or direct or indirect applications in other related technical fields, are similarly included within the patent protection scope of this application.
Claims
1. A method for curing lamp tubes, characterized in that, Includes the following steps: S1: Obtain the initial geometric parameters of the lamp tube and the characteristics of the coating material; S2: Based on the initial geometric parameters and the characteristics of the coating material, multiple independent temperature control zones are divided along the axial direction of the lamp tube in the curing fixture; S3: Low power is used for preheating in the early stage of curing, and the support height is adjusted in real time through the dynamic support matrix of the fixture to counteract the thermal deformation caused by the lamp tube. S4: During the mid-curing stage, real-time temperature feedback data of each area on the surface of the lamp tube is obtained, and the curing power of each independent temperature control area is dynamically adjusted to ensure that the axial curing degree of the lamp tube is consistent. S5: At the end of the curing process, a stepped cooling is performed, and during the cooling process, adaptive support adjustment and phased mechanical locking are performed through the dynamic support matrix until the lamp is completely cooled.
2. The lamp curing method according to claim 1, characterized in that, Step S2 includes: S21: Calculate the expected thermal field distribution of the lamp tube at the curing temperature based on the initial geometric parameters and the characteristics of the coating material; S22: Identify the sections in the expected thermal field distribution where the rate of change of the temperature gradient along the lamp tube axis is greater than a preset threshold as key temperature control zones; S23: Map the key temperature control area and other conventional sections onto the physical heating / light source module of the curing fixture to form the multiple independent temperature control areas that are not uniformly arranged.
3. The lamp curing method according to claim 2, characterized in that, Step S23 specifically includes: Establish a one-to-one correspondence table between the axial coordinates of the lamp tube and the physical module array position of the curing fixture; For the axial coordinates belonging to the key temperature control zone, the reference power weight value of the corresponding physical module is increased by a first proportion; For the axial coordinates belonging to the conventional section, the reference power weight value of the corresponding physical module is reduced by a second ratio. The control parameters of each physical module are configured according to the adjusted weight value to form multiple independent temperature control zones with differentiated power configurations in the non-uniform arrangement.
4. The lamp curing method according to claim 2, characterized in that, Step S21 specifically includes: Extract the coefficient of thermal expansion, specific heat capacity, and exothermic parameters of the curing reaction of the coating material; A thermo-mechanical coupled finite element analysis model was constructed by combining the initial geometric parameters of each axial section of the lamp tube; The thermal expansion coefficient, specific heat capacity, curing reaction exothermic parameters, and initial geometric parameters are input into the thermo-mechanical coupled finite element analysis model to simulate and calculate the expected thermal field distribution of the lamp tube at the target curing temperature and the thermal deformation deflection trend of each axial node.
5. The lamp curing method according to claim 1, characterized in that, Step S3 includes: S31: In the early stage of curing, the lamp tube is preheated at a preset temperature lower than the target curing temperature, and the axial bending and sagging of the lamp tube is monitored in real time. S32: When the bending sag exceeds a preset safety threshold, the required vertical compensation height for each support node in the dynamic support matrix is calculated based on the sag distribution. S33: Send a driving command to the corresponding support node in the dynamic support matrix to lift the lamp tube according to the vertical compensation height, so as to form an adaptive support surface that matches the real-time deformation curve of the lamp tube.
6. The lamp curing method according to claim 5, characterized in that, Step S33 specifically includes: The vertical compensation height is analyzed to generate the target pulse count of the micro stepper motor corresponding to each support node; The micro stepper motor drives the lead screw mechanism to lift the support wheel to contact the surface of the lamp tube; The contact pressure is collected in real time by a pressure sensor installed in the support wheel. When the contact pressure reaches the preset threshold, the lifting action stops, thus completing the closed-loop fine adjustment of the support height.
7. The lamp curing method according to claim 1, characterized in that, Step S4 includes: S41: Real-time temperature of each area on the surface of the lamp tube is collected by an infrared temperature measuring array set in an independent temperature control area; S42: Calculate the deviation value and the rate of change of deviation between the real-time temperature of each region and the preset target curing temperature; S43: Input the deviation value and deviation change rate into the fuzzy PID controller, and output the power regulation coefficient of each independent temperature control zone; S44: Adjust the light source irradiation intensity or heating element power of the corresponding area independently according to the power adjustment coefficient to eliminate the axial temperature gradient of the lamp tube.
8. The lamp curing method according to claim 7, characterized in that, Step S42 specifically includes: The collected infrared thermometer array data is processed by moving average filtering to remove environmental interference outliers; The deviation between the real-time temperature of each region and the preset target curing temperature is calculated based on the filtered data, and the time-series change rate of the deviation value is extracted as the deviation change rate. The maximum and minimum temperature values in the filtered data are extracted to calculate the extreme value of the axial temperature difference. If the extreme value of the axial temperature difference exceeds the preset tolerance zone, the preset target curing temperature is finely adjusted and compensated, and the deviation value is recalculated based on the finely adjusted and compensated target curing temperature.
9. The lamp curing method according to claim 1, characterized in that, Step S5 includes: S51: Set at least three stepped cooling temperature nodes and the corresponding heat preservation dwell time for each node; S52: During the dwell period at each stepped cooling temperature node, continuously monitor the stress change value of the support nodes in the dynamic support matrix and the deformation recovery of the lamp tube. S53: When the deformation recovery amount is detected to be less than the set minimum value per unit time, it is determined that the stress of the lamp tube has been released and the deformation tends to be stable at this temperature node. The current position of the dynamic support matrix is mechanically locked, and the mechanical lock is released before entering the next cooling step or in the early stage of cooling, so as to allow the support matrix to adaptively descend and adjust according to the shrinkage of the lamp tube.
10. A lamp curing system for implementing the lamp curing method according to any one of claims 1 to 9, characterized in that, include: The parameter acquisition module is used to acquire the initial geometric parameters of the lamp tube and the characteristics of the coating material; The region division module is used to divide the lamp tube into multiple independent temperature control zones along the axial direction in the curing fixture; The dynamic curing execution and control module uses low power for preheating in the early stage of curing and simultaneously adjusts the support height in real time through the dynamic support matrix of the fixture to counteract the thermal deformation caused by the lamp tube. In the middle stage of curing, it acquires real-time temperature feedback data of each area on the surface of the lamp tube and dynamically adjusts the curing power of each independent temperature control area to ensure that the axial curing degree of the lamp tube is consistent. At the end of the curing process, a stepped cooling process is implemented, and during the cooling process, adaptive support adjustment and phased mechanical locking are performed through the dynamic support matrix until the lamp is completely cooled.