A cold drawing die and cold drawing method for a tree branch-shaped tee pipe
By using a step-by-step forming method with pre-drawing and reverse-drawing dies, the problems of wrinkling and tearing in sheet metal tree branch-shaped tee pipes during the forming process were solved, thereby improving the surface quality and achieving uniform material deformation.
Patent Information
- Application Number
- CN202611379149.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-09-07
- Publication Date
- 2026-11-17
AI Technical Summary
Sheet metal tree branch-shaped tee pipes are prone to wrinkling and cracking during the forming process, especially at sharp angles where deformation is severe, and existing technologies are unable to effectively solve this problem.
The pre-drawing die and the reverse drawing die are used for step-by-step forming. The pre-drawing die is used to form a preform with triangular protrusions, and the reverse drawing die is used to further form a branch of a tree-branch tee pipe. By cooperating with the pre-drawing blank holder and the reverse drawing blank holder, the material deformation is controlled and the risk of wrinkling and cracking is reduced.
The surface quality of the tree branch-shaped tee pipe is good, the profile meets the dimensional requirements of the design drawing, the risk of wrinkling and tearing is reduced, and the forming process is ensured to be carried out within the material forming limit.
Smart Images

Figure CN123102844A_ABST
Abstract
Description
Technical Field
[0001] This application relates to the field of tree branch-shaped tee pipe forming technology, and in particular to a cold drawing mold and cold drawing method for tree branch-shaped tee pipe. Background Technology
[0002] The tree-branch tee conduit is a pipe part with three outlets. The blank thickness is 0.5–2 mm, belonging to the category of thin-walled, difficult-to-form sheet metal pipe parts. These parts are generally manufactured by directly deep drawing half of the blank using a die, then removing the drawing height allowance and the allowance at the three ends, and finally welding. The acute-angle (30°–45°) tee conduit part has three outlets connected at acute angles, resulting in a complex shape at the transition and making it difficult to form. The material for this type of part is a high-strength nickel-based superalloy, which is sensitive to work hardening and exhibits significant springback after forming, further increasing the forming difficulty.
[0003] When a die is used to deep draw half of a part blank, the transition area at the bottom of the pipe is subjected to circumferential compressive stress, making it difficult to release excess blank material and causing wrinkling at the mold surface. Meanwhile, the transition flange edge of the pipe is subjected to local tensile stress, making the blank prone to thinning and cracking, which is a weak area in the part forming process. Especially for acute-angle (30°~45°) tree branch-shaped tee pipes, the deformation at the acute-angle transition area is more severe, and the aforementioned wrinkling and cracking problems are more prominent. Summary of the Invention
[0004] In order to obtain sheet metal tree branch-shaped tee pipe blanks with good surface quality, this application provides a cold drawing die and cold drawing method for tree branch-shaped tee pipes.
[0005] In the first aspect, this application provides a cold drawing die for a tree-branch-shaped tee pipe, adopting the following technical solution: A cold drawing die for a tree branch-shaped tee pipe includes a pre-drawing die and a reverse drawing die; the pre-drawing die is used to form a preformed part with triangular protrusions, and the reverse drawing die is used to further form the preformed part into branches of a tree branch-shaped tee pipe. The pre-drawing die includes an upper pre-drawing die and a lower pre-drawing die. A pre-drawing die cavity is provided on the side of the upper pre-drawing die near the lower pre-drawing die. The upper pre-drawing die is connected to a die shank by screws. An ejector rod is slidably connected inside the die shank. A pre-drawing ejector located inside the pre-drawing die cavity is fixedly connected to the lower end of the ejector rod. A pre-drawing punch is provided on the side of the lower pre-drawing die near the upper pre-drawing die. A pre-drawing cavity is formed between the pre-drawing punch and the pre-drawing die cavity. A pre-drawing pressure ring is also provided on the lower pre-drawing die, and the pre-drawing pressure ring surrounds the outer periphery of the pre-drawing punch. The reverse drawing die includes an upper reverse drawing die and a lower reverse drawing die. A punch and a die are provided on the side of the lower reverse drawing die near the upper reverse drawing die. A reverse drawing punch and a reverse drawing die are provided on the side of the upper reverse drawing die near the lower reverse drawing die, which cooperate with the punch and die. A reverse drawing ejector is provided on the upper reverse drawing die between the reverse drawing punch and the reverse drawing die. The reverse drawing die, the reverse drawing punch, and the punch and die cooperate to form a reverse drawing cavity. A reverse drawing blank holder is also provided on the lower reverse drawing die, which surrounds the outer periphery of the punch and die.
[0006] Optionally, the top of the reverse drawing punch is a triangular protrusion, the opening shape of the reverse drawing die is an inverted convex shape, the height of the top of the punch and die is 7-10 mm higher than the radius of the tee tube than the distance between the top of the reverse drawing die (24), and the radial gap between the punch and die and the reverse drawing die is 1.1 times the thickness of the blank.
[0007] Secondly, this application provides a cold-drawing method for a tree-branch-shaped tee pipe, comprising the following steps: S1. Calculate the dimensions of the left and right blanks of the tree branch-shaped tee pipe, reserve the process pressing allowance on one side, and splice the two blanks along the symmetrical plane to obtain the symmetrical final blank. S2. Perform the first deep drawing. Place the spliced billet in the pre-drawing mold. Close the pre-drawing upper mold and the pre-drawing lower mold to symmetrically draw the acute angle transition area of the two billets. The transition flange of the two billets closes to form a local deep drawing area. The pre-drawing pressure ring presses the bottom transition of the pipe. S3: Perform the second deep drawing. Turn the pre-drawn blank over and place it in the reverse deep drawing die. Position the blank by matching the inner surface of the pre-drawn blank with the positioning surface of the reverse deep drawing punch. Then, use the reverse deep drawing die to reverse draw the outer part of the blank. S4: Remove the flange edge allowance of the billet in the drawing height direction; S5: Cut the two symmetrical blanks apart and remove the excess material from the three ends respectively; S6: Weld the two blanks together to obtain a tree branch-shaped tee pipe part.
[0008] Optionally, in step S2, during pre-drawing, the flange edges of the two blanks close to form a local drawing region, allowing the material in the acute angled junction area to flow and deform within the closed region, transforming the flange junction, which originally bore local tensile stress, into a closed local drawing deformation zone, reducing the risk of thinning and cracking; the pre-drawing pressure ring applies pressure to the bottom junction of the pipe during the drawing process to eliminate wrinkling defects.
[0009] Optionally, in step S3, the inner surface of the pre-drawn blank is used as the positioning reference during reverse drawing. The positioning surface of the reverse drawing punch is in contact with the inner surface of the blank, so that the inner surface of the blank remains fixed during the reverse drawing process, and the outer shape is gradually formed by the action of the reverse drawing die, so that the stress distribution of the drawn part is uniform.
[0010] Optionally, in step S4, the flange edge excess is removed by milling or manual processing; in step S5, the two blanks are separated and the end excess is removed by cutting; in step S6, the two blanks are welded along the mating surface to form a weld seam, thereby obtaining a tree branch-shaped tee pipe part with a smooth transition.
[0011] In summary, this application includes at least one of the following beneficial technical effects: 1. By symmetrically drawing the acute angle transition area of two billets using a pre-drawing die, the transition flange edges of the two pipes are closed to form a local drawing area, reducing the risk of thinning and cracking; at the same time, pressure is applied by the pre-drawing pressure ring to eliminate wrinkling defects at the bottom transition of the pipe. 2. By using a two-step forming process of pre-drawing and reverse drawing, the large-deformation drawing process is broken down into two smaller deformation processes. The pre-drawing process produces the sharp-angle transition surface inside the tee part, and the reverse drawing process uses the inner surface of the pre-formed part as the positioning surface to produce the outer surface of the tee part. The deformation amount in each step is within the forming limit range of the material, ensuring that the surface of the tree-shaped tee pipe part meets the dimensional requirements of the design drawing. Attached Figure Description
[0012] Figure 1 This is a schematic diagram illustrating the structure of the pre-drawing die in an embodiment of the present invention; Figure 2 yes Figure 1 Sectional view of AA; Figure 3 This is a schematic diagram illustrating the structure of the reverse drawing die in an embodiment of the present invention; Figure 4 yes Figure 3 Sectional view of BB; Figure 5 yes Figure 3 Sectional view of CC; Figure 6 This is a schematic diagram used to illustrate the welded tee conduit; Figure 7 This is a schematic diagram used to illustrate the forming blank of a three-channel tube; Figure 8 It is a schematic diagram used to illustrate the positioning of the billet during the pre-drawing process; Figure 9 It is a schematic diagram used to illustrate the shape of the billet during the pre-drawing process; Figure 10It is a schematic diagram used to illustrate the shape of the billet during the reverse drawing process; Figure 11 This is a flowchart illustrating a cold-drawing method for a tree-branch-shaped tee pipe.
[0013] Explanation of reference numerals in the attached drawings: 1. Pre-drawing die; 11. Upper pre-drawing die template; 12. Lower pre-drawing die template; 13. Pre-drawing die cavity; 14. Pre-drawing punch; 15. Pre-drawing ejector; 16. Pre-drawing blank holder; 17. Die shank; 18. Ejector pin; 2. Reverse drawing die; 21. Upper reverse drawing die template; 22. Lower reverse drawing die template; 23. Reverse drawing punch; 24. Reverse drawing die cavity; 25. Punch and die cavity; 26. Reverse drawing ejector; 27. Reverse drawing blank holder; 3. Locating pin; 4. Lifting bolt; 5. Screw. Detailed Implementation
[0014] The present application will be further described in detail below with reference to all the accompanying drawings.
[0015] Example 1 Reference Figures 1-10 A cold drawing die for a tree branch-shaped tee pipe includes a pre-drawing die 1 and a reverse drawing die 2; the pre-drawing die 1 is used to form a preformed part with triangular protrusions, and the reverse drawing die 2 is used to further form the preformed part into a tree branch-shaped tee pipe branch.
[0016] The pre-drawing die 1 includes an upper pre-drawing die 11 and a lower pre-drawing die 12. A pre-drawing die 13 is provided on the side of the upper pre-drawing die 11 near the lower pre-drawing die 12, and a pre-drawing punch 14 is provided on the side of the lower pre-drawing die 12 near the upper pre-drawing die 11. A pre-drawing cavity is formed between the pre-drawing punch 14 and the pre-drawing die 13. The upper pre-drawing die 11 and the lower pre-drawing die 12 are positioned by pre-drawing cylindrical pins and fastened together by pre-drawing screws 5. A lifting stud is provided at each of the four corners of the top of the upper pre-drawing die 11.
[0017] The top of the pre-drawing punch 14 is shaped like a triangular cone, corresponding to the acute angle transition area of the tree-branch tee pipe. The pre-drawing die 13 and the pre-drawing punch 14 cooperate to form a pre-drawing cavity, and the bottom contour of the pre-drawing die 13 matches the top shape of the pre-drawing punch 14. The single-sided clearance between the pre-drawing punch 14 and the pre-drawing die 13 is 1.1 times the thickness of the blank, ensuring that the blank can deform smoothly during the drawing process without wrinkling due to excessive clearance or tearing due to insufficient clearance.
[0018] A pre-drawing blank holder 16 is also provided on the lower pre-drawing die 12. The pre-drawing blank holder 16 is sleeved around the pre-drawing punch 14 and applies blank holder force to the blank during die closing to suppress wrinkling defects caused by circumferential compressive stress in the material. The lower end of the ejector pin 18 is fixedly connected to a pre-drawing ejector 15 located in the pre-drawing die 13. Its shape is adapted to the top shape of the pre-drawing punch 14 to ensure uniform force on the formed part during ejection. The upper pre-drawing die 11 is connected to a die shank 17 by screws 5. An ejector pin 18 connected to the pre-drawing ejector 15 is slidably connected in the die shank 17. When the die is opened, the ejector pin 15 is pushed to eject the preformed part from the pre-drawing die 13.
[0019] The reverse drawing die 2 includes a reverse drawing upper die 21 and a reverse drawing lower die 22. A punch and die 25 are provided on the side of the reverse drawing lower die 22 near the reverse drawing upper die 21. A reverse drawing punch 23 and a reverse drawing die 24 that cooperate with the punch and die 25 are provided on the side of the reverse drawing upper die 21 near the reverse drawing lower die 22. The reverse drawing die 24, the reverse drawing punch 23 and the punch and die 25 cooperate to form a reverse drawing cavity.
[0020] The outer surface of the punch and die 25 is clearance-fitted with the inner surface of the preform, realizing reverse deep drawing with the inner surface of the preform as the positioning surface. The top height of the punch and die 25 is 7-10 mm higher than the radius of the tee tube than the top distance of the reverse deep drawing die (24), ensuring that the triangular protrusion of the preform can be completely accommodated in the punch and die 25 to achieve deformation-free transfer. The reverse deep drawing punch 23 and the punch and die 25 cooperate to form a reverse deep drawing cavity, and the single-sided clearance between the reverse deep drawing punch 23 and the punch and die 25 is 1.1 times the thickness of the blank.
[0021] The lower drawing die 22 is also provided with a drawing blank holder 27, which surrounds the outer periphery of the punch and die 25 and applies a blank holder force to the edge of the preform. The upper drawing die 21 is provided with a drawing ejector 26 located between the drawing punch 23 and the drawing die 24, which is used to eject the formed part from the drawing die 24.
[0022] Example 2 Reference Figure 11 A cold-drawing method for a tree-branch tee pipe includes the following steps: S1. Calculate the dimensions of the left and right blanks of the tree branch-shaped tee pipe, reserve the process pressing allowance on one side, and splice the two blanks along the symmetrical plane to obtain the symmetrical final blank. Specifically, based on the acute angle (30°) of the tree-branch tee pipe, the pipe diameter (80mm for the main pipe and 60mm for the branch pipe), and the billet thickness (1.0mm), calculate the unfolded dimensions of the left and right billets, reserving a 10-15mm allowance for edge pressing on each side. The two billets are then joined along their symmetrical planes to obtain a symmetrical final billet. During joining, ensure that the symmetrical planes of the two billets fit tightly together without any obvious gaps at the joint, so that both billets can be subjected to stress and deformation simultaneously during the subsequent deep drawing process, utilizing symmetry to balance the deformation forces on both sides.
[0023] S2. Perform the first deep drawing. Place the spliced billet in the pre-drawing mold 1. Close the pre-drawing upper mold 11 and the pre-drawing lower mold 12 to symmetrically draw the acute angle transition area of the two billets. The transition flange edge of the two billets closes to form a local deep drawing area. The pre-drawing pressure ring 16 presses the bottom transition of the pipe.
[0024] Specifically, the spliced billet is placed in the pre-drawing die 1, the press is started, the upper pre-drawing die 11 descends and closes with the lower pre-drawing die 12, and the pre-drawing blank holder 16 first contacts the billet, applying blank holder force to the bottom transition area of the pipe. As the upper die continues to descend, the transition flange edges of the two billets close, forming a local drawing area, and the material in the acute angle transition area flows and deforms within the closed area.
[0025] In this step, because the transition flange forms a closed area after closure, the material cannot flow freely and is forced to redistribute within the closed area. In traditional single-drawing, the acute-angle transition area bears local tensile stress, resulting in severe billet thinning and easy cracking. This invention transforms the area into a closed local drawing deformation zone after the transition flange is closed. The material flows within the closed area instead of deforming freely, and the stress state changes from tensile stress to compressive stress, fundamentally eliminating the conditions for thinning and cracking. Simultaneously, the pressure applied by the pre-drawing blank holder 16 to the bottom transition point of the pipe suppresses wrinkling caused by circumferential compressive stress, allowing the material to flow orderly under the blank holder force and ensuring the quality of the profile.
[0026] S3: Perform the second drawing. Turn the pre-drawn blank over and place it in the reverse drawing die 2. Position the blank so that the inner surface of the pre-drawn blank matches the positioning surface of the reverse drawing punch 23. Then, reverse drawing die 24 reverse-draws the outer part of the blank.
[0027] Specifically, the pre-drawn billet is flipped over and placed in the reverse drawing die 2. The inner surface of the pre-drawn billet mates with the positioning surface of the reverse drawing punch 23 to ensure that the inner surface of the billet remains fixed during the reverse drawing process. The press is started, and the reverse drawing die 24 descends to reverse draw the outer part of the billet. Since the inner surface has been formed by the pre-drawing process and serves as a positioning reference, the material deforms from the inside to the outside during the reverse drawing process, resulting in uniform stress distribution and no wrinkling. The billet after reverse drawing has a smooth transition shape, good surface quality, and the surface meets the dimensional requirements of the design drawing.
[0028] S4: Remove the flange allowance of the billet in the drawing height direction.
[0029] Specifically, milling is used to remove the flange edge allowance in the drawing height direction of the blank, ensuring that the blank height meets the part's design dimensions. During milling, the inner surface of the blank is used as the positioning reference to ensure machining accuracy. For complex shapes, manual grinding can be used for auxiliary finishing to ensure a smooth transition of the surface after flange edge allowance removal.
[0030] S5: Cut the two symmetrical blanks apart and remove the excess material from the three ends respectively.
[0031] Specifically, wire EDM is used to separate the two symmetrically joined blanks along the plane of symmetry. Then, the excess material at each of the three ends of half a tee part is removed to ensure that each pipe end meets the design dimensions. After removing the end excess material, the blank's external dimensions meet the drawing requirements. Wire EDM ensures the surface quality and dimensional accuracy of the cut surface, avoiding damage to the blank's profile caused by mechanical cutting.
[0032] S6: Weld the two blanks together to obtain a tree branch-shaped tee pipe part.
[0033] Specifically, two symmetrically machined blanks are aligned along their mating surfaces and welded together using argon arc welding to form a complete tree-branch tee pipe part. After welding, the weld seam is ground and the surface is inspected to ensure a smooth transition and that the surface meets the dimensional requirements of the design drawings. During welding, heat input is carefully controlled to minimize the impact of the heat-affected zone on material properties, ensuring that the mechanical properties of the welded joint meet the requirements for aero-engine piping. After welding, the part is subjected to coordinate measuring machine (CMM) measurements to check the position, profile, and surface roughness of each pipe end, ensuring that the surface dimensions meet the design requirements. Any localized deviations found during inspection are corrected manually. Inspection checkpoints are established between each process to ensure that the next process is only allowed after the previous process has passed, achieving full-process quality control.
[0034] The above are all preferred embodiments of this application, and are not intended to limit the scope of protection of this application. Therefore, all equivalent changes made in accordance with the structure, shape and principle of this application should be covered within the scope of protection of this application.
Claims
1. A cold-drawing die for a tree-branch shaped tee pipe, characterized in that, It includes a pre-drawing die (1) and a reverse drawing die (2); the pre-drawing die (1) is used to form the blank into a preform with triangular protrusions, and the reverse drawing die (2) is used to further form the preform into a branch of a tree-shaped tee pipe. The pre-drawing die (1) includes a pre-drawing upper die plate (11) and a pre-drawing lower die plate (12). A pre-drawing die (13) is provided on the side of the pre-drawing upper die plate (11) near the pre-drawing lower die plate (12). The pre-drawing upper die plate (11) is connected to a die handle (17) by screws (5). An ejector rod (18) is slidably connected in the die handle (17). A pre-drawing ejector (15) located in the pre-drawing die (13) is fixedly connected to the lower end of the ejector rod (18). A pre-drawing punch (14) is provided on the side of the pre-drawing lower die plate (12) near the pre-drawing upper die plate (11). A pre-drawing cavity is formed between the pre-drawing punch (14) and the pre-drawing die (13). A pre-drawing pressure ring (16) is also provided on the pre-drawing lower die plate (12). The pre-drawing pressure ring (16) surrounds the outer periphery of the pre-drawing punch (14). The reverse drawing die (2) includes a reverse drawing upper template (21) and a reverse drawing lower template (22). A punch and die (25) are provided on the side of the reverse drawing lower template (22) near the reverse drawing upper template (21). A reverse drawing punch (23) and a reverse drawing die (24) that cooperate with the punch and die (25) are provided on the side of the reverse drawing upper template (21) near the reverse drawing lower template (22). A reverse drawing ejector (26) is provided on the reverse drawing upper template (21) between the reverse drawing punch (23) and the reverse drawing die (24). The reverse drawing die (24), the reverse drawing punch (23), and the punch and die (25) cooperate to form a reverse drawing cavity. A reverse drawing pressure ring (27) is also provided on the reverse drawing lower template (22). The reverse drawing pressure ring (27) surrounds the outer periphery of the punch and die (25).
2. The cold drawing die for a tree-branch tee pipe according to claim 1, characterized in that, The top of the pre-drawing punch (14) is a triangular cone. The pre-drawing die (13) is located above the pre-drawing punch (14) and cooperates with the pre-drawing punch (14) to form a bowl-shaped pre-drawing cavity. The radial gap between the pre-drawing die (13) and the pre-drawing punch (14) is 1.1 times the blank thickness. The bottom contour of the pre-drawing die (13) is adapted to the top shape of the pre-drawing punch (14). The pre-drawing ejector (15) is a triangular ejector, and its shape is adapted to the top shape of the pre-drawing punch (14). The distance between the lower end face of the pre-drawing pressure ring (16) and the top of the pre-drawing punch (14) is 7-10 mm higher than the radius of the tee pipe.
3. The cold drawing die for a tree-branch tee pipe according to claim 1, characterized in that, The top of the reverse drawing punch (23) is a triangular protrusion, the opening shape of the reverse drawing die (24) is an inverted U-shape, the height of the top of the punch and die (25) and the distance between the top of the reverse drawing die (24) are 7-10 mm higher than the radius of the tee pipe, and the radial gap between the punch and die (25) and the reverse drawing die (24) is 1.1 times the thickness of the blank.
4. A cold-drawing method for a tree-branch-shaped tee pipe, characterized in that, The cold drawing die for the tree-branch-shaped tee pipe according to any one of claims 1 to 3 is characterized by comprising the following steps: S1. Calculate the dimensions of the two blanks on the left and right sides of the tree branch-shaped tee pipe, reserve the process pressing allowance on one side, and splice the two blanks along the symmetrical plane to obtain the symmetrical final blank. S2. Perform the first deep drawing. Place the spliced billet in the pre-drawing mold (1). Close the mold with the pre-drawing upper template (11) and the pre-drawing lower template (12) to symmetrically draw the acute angle transition area of the two billets. The transition flange of the two billets closes to form a local deep drawing area. The pre-drawing pressure ring (16) presses the bottom transition of the pipe. S3: Perform the second deep drawing. Turn the pre-drawn blank over and place it in the reverse deep drawing die (2). Position the blank by matching the inner surface of the pre-drawn blank with the positioning surface of the reverse deep drawing punch (23). Use the reverse deep drawing die (24) to reverse draw the outer part of the blank. S4: Remove the flange edge allowance of the billet in the drawing height direction; S5: Cut the two symmetrical blanks apart and remove the excess material from the three ends respectively; S6: Weld the two blanks together to obtain a tree branch-shaped tee pipe part.
5. The cold drawing method for a tree-branch-shaped tee pipe according to claim 4, characterized in that, In step S2, during pre-drawing, the flange edges of the two blanks close to form a local drawing area, so that the material of the acute angled junction area flows and deforms in the closed area, transforming the flange junction that originally bears local tensile stress into a closed local drawing deformation area, reducing the risk of thinning and cracking; the pre-drawing pressure ring (16) applies pressure to the bottom junction of the pipe during the drawing process to eliminate wrinkling defects.
6. The cold drawing method for a tree-branch-shaped tee pipe according to claim 4, characterized in that, In step S3, the inner surface of the pre-drawn blank is used as the positioning reference during reverse drawing. The positioning surface of the reverse drawing punch (23) is in contact with the inner surface of the blank, so that the inner surface of the blank remains fixed during the reverse drawing process. The outer shape is gradually formed by the action of the reverse drawing die (24), so that the stress distribution of the deep-drawn parts is uniform.
7. The cold drawing method for a tree-branch-shaped tee pipe according to claim 4, characterized in that, In step S4, the flange edge excess is removed by milling or manual processing; in step S5, the two blanks are separated by cutting and the end excess is removed; in step S6, the two blanks are welded along the mating surface to form a weld seam, resulting in a tree branch-shaped tee pipe part with a smooth transition.