A sodium acetate mixture for preventing crystallization, its preparation method and application

The low-temperature crystallization problem was solved by adding anti-crystallization agents and stabilizers to the sodium acetate mixture, enabling the application of high-concentration, stable, and low-cost sodium acetate solutions, thus ensuring the stability and efficiency of wastewater treatment.

CN123105853APending Publication Date: 2026-11-17JIANGXI YUHUI ENVIRONMENTAL TECH CO LTD
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
CN202611487397.0
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-09-23
Publication Date
2026-11-17

AI Technical Summary

Technical Problem

Sodium acetate solution is prone to crystallization at low temperatures, which leads to problems such as equipment blockage, inaccurate carbon source addition, high maintenance costs, and decreased denitrification efficiency. Existing technologies also suffer from problems such as dilution of effective components, additives affecting microbial activity, complex preparation processes, and high costs.

Method used

A sodium acetate mixture with anti-crystallization properties was prepared by using sodium carboxymethyl cellulose, polyvinyl alcohol, and other anti-crystallization agents and phosphates, through simple steps such as dissolution, homogenization, and filtration. This mixture maintained a high concentration and stability, inhibited crystallization, and preserved microbial activity.

Benefits of technology

It does not crystallize below -25℃, maintains high effective concentration and COD value, reduces transportation and storage costs, ensures stable denitrification effect, and is suitable for large-scale production.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure REF-OBJ-1790066823881-000001
    Figure REF-OBJ-1790066823881-000001
  • Figure REF-OBJ-1790066823881-000002
    Figure REF-OBJ-1790066823881-000002
  • Figure REF-OBJ-1790066823881-000003
    Figure REF-OBJ-1790066823881-000003
Patent Text Reader

Abstract

This invention relates to the field of wastewater treatment technology, specifically disclosing an anti-crystallization sodium acetate mixture, which is composed of the following components by mass percentage: sodium acetate: 20-40%; anti-crystallization agent: 0.5-5%; stabilizer: 0.1-2%; water: balance; the sum of the above components is 100%. This invention provides a sodium acetate mixture with excellent anti-crystallization performance, high concentration of effective components, no impact on wastewater treatment effect, good product stability, and a simple preparation process, as well as its application as a carbon source in wastewater treatment.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of wastewater treatment technology, specifically to an anti-crystallization sodium acetate mixture, its preparation method, and its application. Background Technology

[0002] In biological nitrogen removal processes, the denitrification stage requires a sufficient carbon source as an electron donor to reduce nitrate nitrogen to nitrogen gas. However, urban domestic sewage in my country generally has a low carbon-to-nitrogen ratio (C / N ratio), and the organic carbon source contained in the sewage itself is insufficient to meet the needs of denitrification. Therefore, it is necessary to supplement the denitrification stage with an external carbon source. Sodium acetate is one of the most commonly used high-quality external carbon sources in sewage treatment due to its advantages such as fast denitrification rate, low sludge production, and non-toxicity. In sewage treatment, the main role of sodium acetate is to supplement the carbon source for denitrifying bacteria and to acclimate the denitrifying sludge. Denitrifying bacteria can over-adsorb sodium acetate, so when denitrification is carried out using sodium acetate as an external carbon source, the effluent COD value can also be maintained at a low level.

[0003] However, sodium acetate solution faces a long-standing technical challenge in practical applications – low-temperature crystallization. Sodium acetate generally exists as sodium acetate trihydrate with three molecules of water of crystallization. The crystallization problem of sodium acetate solution manifests itself in several ways: First, it easily crystallizes and clogs equipment at low temperatures: When the temperature of sodium acetate solution falls below a certain threshold (usually 10-16℃), sodium acetate trihydrate crystals precipitate. In winter, under low-temperature conditions, crystallization easily occurs in storage tanks, pipelines, metering pumps, and other equipment, severely affecting the normal addition of carbon sources. Second, crystallization leads to inaccurate carbon source addition: After sodium acetate solution crystallizes, the effective carbon source concentration in the solution changes, resulting in inaccurate carbon source addition based on volume, affecting the stability of denitrification. Third, crystallization increases equipment maintenance costs: Crystallization blockage requires frequent cleaning of pipelines and metering pumps, increasing the operation and maintenance costs and labor burden of wastewater treatment plants. Fourth, lower water temperature leads to decreased denitrification efficiency: When the water temperature is below 10℃, the enzyme activity of microorganisms decomposing sodium acetate decreases by 40%, and at 5℃, the utilization rate is less than half that at room temperature. Adding carbon sources at low temperatures is already challenging, and the crystallization problem further exacerbates the difficulties of denitrification in winter.

[0004] To address the issue of low-temperature crystallization of sodium acetate solution, several solutions have been proposed in existing technologies. For example, Hangzhou Electrochemical Group Co., Ltd. disclosed a method for producing low-temperature non-crystallizing sodium acetate (CN112174805A). This method utilizes DCS automatic control technology to add high-purity water, glacial acetic acid, sodium hydroxide, a modifier, a surfactant, and an antifreeze agent to a reaction vessel to produce a low-temperature non-crystallizing sodium acetate that does not crystallize at -30℃ and provides good carbon supply. Furthermore, studies have found that adding a certain proportion of thickener to sodium acetate trihydrate can significantly inhibit crystal precipitation in supercooled sodium acetate trihydrate solutions. Another patent discloses a method for preparing a highly efficient carbon source sodium acetate solution, made from acetic acid, soda ash or alkaline solution, methanol, glucose, and butanol, which exhibits high concentration and high COD and is not prone to crystallization.

[0005] However, existing technologies still have the following shortcomings: The effective carbon source is diluted: Some existing technologies lower the crystallization point by adding large amounts of water, but this reduces the effective concentration of sodium acetate and the COD value, increasing storage, transportation, and application costs. Additives may affect wastewater treatment effectiveness: Antifreeze, surfactants, and other components added in existing technologies may adversely affect microbial activity or increase organic residues in the effluent. Insufficient product stability: Some anti-crystallizing sodium acetate solutions still exhibit slow crystallization or stratification during long-term storage, affecting the actual application effect of the product. Complex preparation process and high cost: Existing anti-crystallizing sodium acetate preparation processes often involve complex multi-step, multi-component operations, resulting in high production costs and hindering large-scale application. Based on this, the present invention provides an anti-crystallizing sodium acetate mixture, its preparation method, and its application. Summary of the Invention

[0006] To address the shortcomings of the existing technologies, the present invention aims to provide an anti-crystallization sodium acetate mixture and its application as a carbon source for wastewater treatment. While maintaining a high effective concentration, it achieves excellent low-temperature anti-crystallization performance, featuring low anti-crystallization temperature (no crystallization below -25℃), high concentration of effective components, good product stability, no impact on denitrification effect, and simple preparation process.

[0007] In a first aspect, the present invention provides an anti-crystallization sodium acetate mixture, which is composed of the following components by mass percentage: sodium acetate: 20-40%; anti-crystallization agent: 0.5-5%; stabilizer: 0.1-2%; water: balance; the sum of the above components is 100%.

[0008] Furthermore, the sodium acetate is anhydrous sodium acetate or sodium acetate trihydrate.

[0009] Furthermore, the anti-crystallization agent is one or more of sodium carboxymethyl cellulose, polyvinyl alcohol, gelatin, and sodium polyacrylate.

[0010] Furthermore, the anti-crystallization sodium acetate mixture is composed of the following components by mass percentage: 25-35% sodium acetate, 1-3% anti-crystallization agent, 0.3-1.5% stabilizer, and water as the balance.

[0011] Furthermore, the anti-crystallization agent is a mixture of sodium carboxymethyl cellulose and polyvinyl alcohol, with a mass ratio of sodium carboxymethyl cellulose to polyvinyl alcohol of (1-3):(1-2).

[0012] Furthermore, the stabilizer is one or more of sodium dihydrogen phosphate, disodium hydrogen phosphate, sodium citrate, and disodium ethylenediaminetetraacetate.

[0013] Furthermore, the pH value of the anti-crystallization sodium acetate mixture is 6.5-8.5, and the COD value is 300,000-600,000 mg / L.

[0014] Secondly, the present invention provides a method for preparing an anti-crystallization sodium acetate mixture, comprising the following steps: S1. Ingredient preparation: Weigh out sodium acetate, anti-crystallization agent, stabilizer and water according to the formula ratio; S2. Dissolving and mixing: Add water to the reaction vessel and heat to 40-70℃. Add sodium acetate, stabilizer and anti-crystallization agent in sequence under stirring. The stirring speed is 60-150 rpm and the stirring time is 20-60 minutes to ensure that all components are fully dissolved and mixed evenly. S3. Homogenization: The mixture obtained in step S2 is homogenized using a homogenizer at a pressure of 10-30 MPa for 5-15 minutes. S4. Filtration and impurity removal: Filter the mixture obtained in step S3 through a 100-300 mesh filter. S5. Cooling and filling: Cool the filtrate obtained in step S4 to room temperature, fill and seal to obtain the anti-crystallization sodium acetate mixture as the finished product.

[0015] Furthermore, in step S2, the stirring speed is 80-120 rpm, the stirring time is 30-50 minutes, and the heating temperature is 50-65℃.

[0016] Furthermore, in step S3, the homogenization pressure is 15-25 MPa and the homogenization time is 8-12 minutes.

[0017] Thirdly, the present invention provides an application of anti-crystallization sodium acetate mixture as a carbon source for wastewater treatment. The anti-crystallization sodium acetate mixture is added as an external carbon source to the denitrification tank of the wastewater treatment system, and the addition amount is controlled according to a COD / TN ratio of 3-6.

[0018] Furthermore, the anti-crystallization sodium acetate mixture remains liquid and does not crystallize within a temperature range of -25°C to 40°C.

[0019] Furthermore, the anti-crystallization sodium acetate mixture does not crystallize out after being stored at room temperature and sealed for more than 180 days.

[0020] In summary, the present invention has the following beneficial effects: This invention effectively inhibits the formation and precipitation of sodium acetate trihydrate crystals in sodium acetate solution by adding anti-crystallization agents (such as sodium carboxymethyl cellulose and polyvinyl alcohol). The anti-crystallization agents increase solution viscosity, hinder the orderly arrangement of solute molecules and crystal nucleation, allowing the sodium acetate mixture to remain liquid and non-crystallizing even at temperatures below -25°C, thus solving the technical problem of sodium acetate solution crystallization clogging equipment under low-temperature conditions in winter.

[0021] This invention achieves excellent anti-crystallization performance while maintaining a high effective concentration of sodium acetate (20-40%) and COD value (300,000-600,000 mg / L), avoiding the problem of increased transportation and storage costs caused by excessive dilution to lower the crystallization point.

[0022] This invention further enhances the long-term storage stability of sodium acetate mixture by adding stabilizers (phosphates, citrates, etc.), and no crystallization or stratification occurs when stored at room temperature and sealed for more than 180 days.

[0023] The anti-crystallization agent and stabilizer used in this invention are all non-toxic, biodegradable or harmless to microorganisms. After being added to the sewage treatment system, they will not inhibit the activity of denitrifying bacteria and will not affect the denitrification effect.

[0024] The preparation method of the present invention only requires simple steps such as dissolution, mixing, homogenization, and filtration, without the need for complex reaction conditions and equipment, resulting in low production costs and suitability for large-scale industrial production. Detailed Implementation

[0025] The technical solution of the present invention will be clearly and completely described below. Obviously, the described embodiments are only some embodiments of the present invention, not all embodiments. Based on the embodiments of the present invention, all other embodiments obtained by those skilled in the art without creative effort are within the scope of protection of the present invention. The present invention will be further described in detail below with reference to the embodiments.

[0026] Example 1

[0027] This embodiment provides an anti-crystallization sodium acetate mixture, its preparation method, and its application.

[0028] (a) Components of the anti-crystallization sodium acetate mixture By mass percentage, the anti-crystallization sodium acetate mixture of this embodiment consists of the following components:

[0029] The sum of all the above components is 100%.

[0030] (II) Preparation method of anti-crystallization sodium acetate mixture The anti-crystallization sodium acetate mixture in this embodiment is prepared according to the following steps: S1. Ingredient preparation: Weigh out 32 kg of sodium acetate trihydrate, 1.5 kg of sodium carboxymethyl cellulose, 0.8 kg of polyvinyl alcohol, 0.5 kg of sodium dihydrogen phosphate, 0.3 kg of sodium citrate and 64.9 kg of water according to the above formula ratio; S2. Dissolving and mixing: Add water to the reaction vessel, heat to 60°C, and start stirring (100 rpm). Under stirring, add sodium acetate trihydrate, sodium dihydrogen phosphate, sodium citrate, sodium carboxymethyl cellulose and polyvinyl alcohol in sequence, and continue stirring for 40 minutes to ensure that all components are fully dissolved and mixed evenly. S3. Homogenization: The mixture obtained in step S2 is homogenized in a homogenizer at a pressure of 20 MPa for 10 minutes. S4. Filtration and impurity removal: Filter the mixture obtained in step S3 through a 200-mesh filter screen; S5. Cooling and filling: Cool the filtrate obtained in step S4 to room temperature, fill and seal to obtain the anti-crystallization sodium acetate mixture as the finished product.

[0031] Testing revealed that the finished anti-crystallization sodium acetate mixture prepared in this embodiment had a COD value of 480,000 mg / L, a pH value of 7.2, and a density of 1.18 g / cm³. 3 .

[0032] (III) Anti-crystallization performance test The anti-crystallization sodium acetate mixture samples prepared in this embodiment were placed in constant temperature environments of 25℃, 4℃, -5℃, -10℃, -15℃, -20℃, and -25℃ for observation, and the crystallization status of the samples was recorded. Meanwhile, a 32% sodium acetate aqueous solution without added anti-crystallization agent and stabilizer was used as a control sample.

[0033] Anti-crystallization performance test results:

[0034] The results showed that the anti-crystallization sodium acetate mixture of the present invention did not crystallize even after standing for 30 days at a low temperature of -25℃, while the control sample began to crystallize at 4℃, proving that the anti-crystallization performance of the present invention is excellent.

[0035] (iv) Storage stability test The anti-crystallization sodium acetate mixture prepared in this embodiment was sealed and stored at room temperature (25±5℃) for 180 days, and samples were taken every 30 days to test its appearance, COD value and pH value.

[0036] Storage stability test results:

[0037] The results showed that during the 180-day storage period, the anti-crystallization sodium acetate mixture of the present invention maintained a uniform liquid appearance, with no crystallization or stratification, a COD value decrease rate of only 3.75%, and a pH value change within 0.2, indicating good product stability.

[0038] (v) Verification of the application effect as a carbon source for wastewater treatment The anti-crystallization sodium acetate mixture prepared in this embodiment was used as an external carbon source for denitrification treatment of low C / N ratio wastewater (winter water temperature 8-10℃, influent COD=160mg / L, TN=42mg / L, C / N=3.8) in a wastewater treatment plant in a northern city. The anti-crystallization sodium acetate mixture was added to the denitrification tank at a COD / TN ratio of 4.5, with a hydraulic retention time (HRT) of 2 hours.

[0039] The results showed that after adding this anti-crystallization sodium acetate mixture, the denitrification rate reached 0.10 kg NO3. - -N / (kgVSS·d), the total nitrogen removal rate increased from 48% without the addition of carbon source to 85%, and the total nitrogen concentration in the effluent decreased from 21.8 mg / L to 6.3 mg / L, meeting the Class A standard (TN≤15 mg / L) of the "Discharge Standard of Pollutants for Municipal Wastewater Treatment Plants" (GB18918-2002).

[0040] Under the same low-temperature winter conditions, the control group, which added ordinary sodium acetate solution (32%), experienced unstable operation of the dosing system due to pipeline crystallization and blockage, resulting in an actual total nitrogen removal rate of only 72%. The anti-crystallization sodium acetate mixture of the present invention operates smoothly under low-temperature conditions, and its nitrogen removal effect is stable and reliable.

[0041] Example 2

[0042] The difference between this embodiment and Example 1 lies in the composition and preparation conditions of the anti-crystallization sodium acetate mixture.

[0043] (a) Components of the anti-crystallization sodium acetate mixture By mass percentage, the anti-crystallization sodium acetate mixture of this embodiment consists of the following components:

[0044] (II) Preparation method of anti-crystallization sodium acetate mixture S1. Ingredient preparation: Weigh each component according to the above formula proportions; S2. Dissolving and mixing: Add water to the reactor, heat to 65°C, and start stirring (120 rpm). Under stirring, add anhydrous sodium acetate, disodium hydrogen phosphate, disodium ethylenediaminetetraacetate, gelatin and sodium polyacrylate in sequence, and continue stirring for 50 minutes. S3. Homogenization: The mixture obtained in step S2 is homogenized in a homogenizer at a pressure of 25 MPa for 12 minutes. S4. Filtration and impurity removal: Filter the mixture obtained in step S3 through a 150-mesh filter screen; S5. Cooling and filling: Cool the filtrate obtained in step S4 to room temperature, then fill and seal it.

[0045] Testing showed that the finished anti-crystallization sodium acetate mixture prepared in this embodiment had a COD value of 420,000 mg / L, a pH value of 7.5, and no crystallization occurred after 30 days at -20℃.

[0046] Example 3

[0047] The difference between this embodiment and Embodiment 1 is that the anti-crystallization agent is a single component of sodium carboxymethyl cellulose.

[0048] (a) Components of the anti-crystallization sodium acetate mixture By mass percentage, the anti-crystallization sodium acetate mixture of this embodiment consists of the following components:

[0049] (II) Preparation method The preparation method is the same as in Example 1, except that the dissolution and mixing temperature is 55°C, the stirring time is 35 minutes, and the homogenization pressure is 18 MPa.

[0050] Testing showed that the finished anti-crystallization sodium acetate mixture prepared in this embodiment had a COD value of 450,000 mg / L, a pH value of 7.0, and no crystallization occurred after 30 days at -20℃.

[0051] Example 4

[0052] The difference between this embodiment and Embodiment 1 is that the anti-crystallization agent is a single component of polyvinyl alcohol.

[0053] (a) Components of the anti-crystallization sodium acetate mixture By mass percentage, the anti-crystallization sodium acetate mixture of this embodiment consists of the following components:

[0054] (II) Preparation method The preparation method is the same as in Example 1, except that the dissolution and mixing temperature is 70°C and the stirring time is 45 minutes.

[0055] Testing showed that the finished anti-crystallization sodium acetate mixture prepared in this embodiment had a COD value of 520,000 mg / L, a pH value of 7.3, and no crystallization occurred after 30 days at -18℃.

[0056] Example 5

[0057] The difference between this embodiment and Embodiment 1 is that a biological promoter was added to the anti-crystallization sodium acetate mixture to further enhance the wastewater treatment effect.

[0058] (a) Components of the anti-crystallization sodium acetate mixture By mass percentage, the anti-crystallization sodium acetate mixture of this embodiment consists of the following components:

[0059] The trace element solution consists of: FeSO4·7H2O 2g / L, MnSO4·H2O 1g / L, ZnSO4·7H2O 1g / L, and CoCl2·6H2O 0.2g / L.

[0060] (II) Application Effects When the anti-crystallization sodium acetate mixture prepared in this embodiment was used under the same wastewater treatment conditions as in Example 1, the results showed that the total nitrogen removal rate was increased to 88%, which was further improved compared to Example 1 (85%), proving that the addition of trace element solution has a promoting effect on the metabolic activity of denitrifying bacteria.

[0061] This specific embodiment is merely an explanation of the present invention and is not intended to limit the invention. After reading this specification, those skilled in the art can make modifications to this embodiment without contributing any inventive step, but such modifications are protected by patent law as long as they are within the scope of the claims of the present invention.

Claims

1. An anti-crystallized sodium acetate mixture solution, characterized by, It consists of the following components by mass percentage: sodium acetate: 20-40%; anti-crystallization agent: 0.5-5%; stabilizer: 0.1-2%; water: balance; the sum of the above components is 100%.

2. The anti-crystallized sodium acetate mixture solution according to claim 1, characterized by, The sodium acetate is anhydrous sodium acetate or sodium acetate trihydrate.

3. The anti-crystallized sodium acetate mixture solution according to claim 1, characterized by, The anti-crystallization agent is one or more of sodium carboxymethyl cellulose, polyvinyl alcohol, gelatin, and sodium polyacrylate.

4. The anti-crystallized sodium acetate mixture solution according to claim 3, characterized by, The anti-crystallization agent is a mixture of sodium carboxymethyl cellulose and polyvinyl alcohol, with a mass ratio of sodium carboxymethyl cellulose to polyvinyl alcohol of (1-3):(1-2).

5. The anti-crystallization sodium acetate mixture according to claim 1, characterized in that, The stabilizer is one or more of sodium dihydrogen phosphate, disodium hydrogen phosphate, sodium citrate, and disodium ethylenediaminetetraacetate.

6. The sodium acetate mixture against crystallization according to claim 1, characterized in that, The anti-crystallization sodium acetate mixture has a pH of 6.5-8.5 and a COD of 300,000-600,000 mg / L.

7. A method for preparing the anti-crystallization sodium acetate mixture according to any one of claims 1-6, characterized in that, Includes the following steps: S1. Ingredient preparation: Weigh out sodium acetate, anti-crystallization agent, stabilizer and water according to the formula ratio; S2. Dissolving and mixing: Add water to the reaction vessel and heat to 40-70℃. Add sodium acetate, stabilizer and anti-crystallization agent in sequence under stirring. The stirring speed is 60-150 rpm and the stirring time is 20-60 minutes to ensure that all components are fully dissolved and mixed evenly. S3. Homogenization: The mixture obtained in step S2 is homogenized using a homogenizer at a pressure of 10-30 MPa for 5-15 minutes. S4. Filtration and impurity removal: Filter the mixture obtained in step S3 through a 100-300 mesh filter. S5. Cooling and filling: Cool the filtrate obtained in step S4 to room temperature, fill and seal to obtain the anti-crystallization sodium acetate mixture as the finished product.

8. The preparation method according to claim 7, characterized in that, In step S2, the stirring speed is 80-120 rpm, the stirring time is 30-50 minutes, and the heating temperature is 50-65℃.

9. The preparation method according to claim 7, characterized in that, In step S3, the homogenization pressure is 15-25 MPa and the homogenization time is 8-12 minutes.

10. The application of the anti-crystallization sodium acetate mixture according to any one of claims 1-6 as a carbon source for wastewater treatment, characterized in that, The anti-crystallization sodium acetate mixture is added as an external carbon source to the denitrification tank of the wastewater treatment system, and the addition amount is controlled according to the COD / TN ratio of 3-6.

Citation Information

Patent Citations